A method for predicting variable amplitude fatigue life of unidirectional composite materials
By constructing a simulation model of unidirectional composite materials, simulating the interface state and fiber strength of micronumerals, the problem of large error in the prediction of fatigue life of unidirectional composite materials in the prior art is solved, and more accurate life prediction is achieved.
Patent Information
- Application Number
- CN202410981004.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-22
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2044-07-22
AI Technical Summary
The existing method of predicting amplitude fatigue life of unidirectional composites under high-temperature air amplitude fatigue conditions has the problem of large error in the prediction results.
A simulation model of unidirectional composite materials is constructed, through micro-element simulation, the interface shear stress, tensile stress and fiber residual strength are calculated, the tensile strength value is updated, the proportion of the number of failed fibers is determined, and the amplitude fatigue life is predicted.
A more accurate prediction of the amplitude fatigue life of one-way composite materials is achieved, which reduces the error of the prediction results and improves the accuracy of the prediction.
Smart Images

Figure CN118506941B_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of material mechanics, and in particular to a method for predicting the variable amplitude fatigue life of a unidirectional composite material. Background Art
[0002] Unidirectional composite materials such as ceramic matrix composites have the advantages of high specific modulus, high strength, high temperature resistance, and corrosion resistance. They are ideal materials for advanced aircraft engine hot end components, such as turbine blades and combustion chambers. During the preparation process, the internal pores of unidirectional composite materials will be randomly distributed, causing local fibers to bend and misalign, and stress concentration will occur during use. Preliminary studies have shown that the fatigue life of unidirectional composite materials in the parallel fiber direction is closely related to the loading history. Different loading histories will affect the interface slip state, matrix crack spacing, fiber degradation, uneven pore distribution, etc., thereby affecting the final mechanical properties of unidirectional composite materials.
[0003] Since the late 1980s, scholars from many countries have conducted research on the microscopic failure mechanism and life prediction model of unidirectional composite materials under constant amplitude fatigue at room temperature and high temperature environments. However, there are few studies on the fatigue life prediction methods of unidirectional composite materials under variable amplitude fatigue conditions in high temperature air. In addition, the prediction results obtained using the existing variable amplitude fatigue life prediction methods for unidirectional composite materials have large errors. Summary of the invention
[0004] In view of this, one of the technical problems solved by the embodiments of the present invention is to provide a method for predicting the variable amplitude fatigue life of unidirectional composite materials, so as to overcome the problem in the prior art that the variable amplitude fatigue life prediction of unidirectional composite materials under high temperature air variable amplitude fatigue conditions has large prediction result errors.
[0005] The present application embodiment discloses a method for predicting variable amplitude fatigue life of a unidirectional composite material, the method comprising:
[0006] Constructing a simulation model of a unidirectional composite material; wherein the simulation model includes a plurality of unit cells composed of a plurality of microelements, each of the unit cells is used to simulate a fiber, a matrix wrapped outside the fiber, and an interface between the fiber and the matrix, and each of the microelements is set with a corresponding tensile strength value;
[0007] Determining the interface state of each of the micro-element at the current cycle number of the current fatigue load according to a load loading rule of a variable amplitude fatigue test on the unidirectional composite material in an air environment at a first preset temperature;
[0008] According to the interface state of each micro-element, the interface shear stress value corresponding to each micro-element is calculated;
[0009] According to the interface shear stress value corresponding to each microelement, the tensile force value and matrix crack spacing of each microelement are calculated;
[0010] Determine the residual strength value of the fiber in the oxidation zone and the residual strength value of the fiber in the non-oxidation zone corresponding to each microelement according to the interface shear stress value corresponding to each microelement;
[0011] Update the tensile strength value corresponding to each micro-element according to the residual strength value of the fiber in the oxidation zone and the residual strength value of the fiber in the non-oxidation zone corresponding to each micro-element;
[0012] Determine the percentage of failed fibers according to the tensile force values corresponding to the microelements included in all the unit cells and the updated tensile strength values;
[0013] When the proportion of the number of failed fibers is greater than or equal to a first preset proportion value, the variable amplitude fatigue life of the unidirectional composite material is determined according to the current number of cycles of the current level fatigue load.
[0014] Optionally, updating the tensile strength value corresponding to each microelement according to the residual strength value of the fiber in the oxidation zone and the residual strength value of the fiber in the non-oxidation zone corresponding to each microelement comprises:
[0015] The smaller one of the residual strength value of the fiber in the oxidation zone and the residual strength value of the fiber in the non-oxidation zone corresponding to the microelement is taken as the tensile strength value corresponding to the microelement.
[0016] Optionally, updating the tensile strength value corresponding to each microelement according to the residual strength value of the fiber in the oxidation zone and the residual strength value of the fiber in the non-oxidation zone corresponding to each microelement comprises:
[0017] When the matrix crack spacing of the microelement satisfies the matrix oxidation channel closing condition, the tensile strength value corresponding to the microelement is updated according to the residual strength value of the fiber in the non-oxidized zone corresponding to the microelement;
[0018] When the matrix crack of the microelement satisfies the interface oxidation channel closure condition, the tensile strength value corresponding to the microelement is updated according to the residual strength value of the oxidation zone fiber corresponding to the microelement.
[0019] Optionally, the method further comprises:
[0020] According to the heat treatment environment conditions in the preparation process of the unidirectional composite material, a first heat treatment is performed on the fibers included in the plurality of unidirectional composite materials;
[0021] performing a tensile test on a first preset number of the fibers after the first heat treatment, respectively, to obtain tensile strength values of the fibers after the first heat treatment;
[0022] Dividing a second preset number of the fibers after the first heat treatment into a third preset number of groups, and determining the second heat treatment duration corresponding to each group according to a load loading rule for the variable amplitude fatigue test of the unidirectional composite material;
[0023] In the air environment of the first preset temperature, performing a second heat treatment on the second preset number of the fibers after the first heat treatment according to the second heat treatment duration corresponding to each group;
[0024] Performing a tensile test on the second preset number of the fibers after the second heat treatment, respectively, to obtain a tensile strength value of the fibers corresponding to each group;
[0025] A first strength degradation model is obtained according to the second heat treatment duration and the tensile strength value of the fiber corresponding to all groups; wherein the first strength degradation model is used to characterize the corresponding relationship between the tensile strength distribution of the fiber after the second heat treatment and the tensile strength distribution of the fiber after the first heat treatment and the second heat treatment duration;
[0026] Correspondingly, determining the residual strength value of the fiber in the oxidation zone and the residual strength value of the fiber in the non-oxidation zone corresponding to each microelement according to the interface shear stress value corresponding to each microelement includes:
[0027] The residual strength value of the oxidation zone fiber corresponding to each of the microelements is determined according to the first strength degradation model and the load loading rule of the variable amplitude fatigue test of the unidirectional composite material in the air environment at the first preset temperature.
[0028] Optionally, the first strength degradation model is:
[0029] ;
[0030] in, is the tensile strength distribution of the fiber after the second heat treatment; is the average value of the tensile strength corresponding to all groups after the second heat treatment; is the tensile strength distribution of the fiber after the first heat treatment; is the duration of the second heat treatment; when the variable amplitude fatigue test is performed on the unidirectional composite material in the air environment at the first preset temperature, , is the current cycle number, is the load loading frequency of the variable amplitude fatigue test.
[0031] Optionally, the method further comprises:
[0032] According to the heat treatment environment conditions in the preparation process of the unidirectional composite material, a first heat treatment is performed on the fibers included in the plurality of unidirectional composite materials;
[0033] performing a tensile test on a first preset number of the fibers after the first heat treatment, respectively, to obtain tensile strength values of the fibers after the first heat treatment;
[0034] Correspondingly, determining the residual strength value of the fiber in the oxidation zone and the residual strength value of the fiber in the non-oxidation zone corresponding to each microelement according to the interface shear stress value corresponding to each microelement includes:
[0035] Determine the residual strength value of the fiber in the non-oxidized zone corresponding to each of the micro-elements according to the second strength degradation model and the load loading rule of the variable amplitude fatigue test of the unidirectional composite material in the air environment at the first preset temperature;
[0036] Wherein, the second strength degradation model is: ;
[0037] is the residual strength distribution of the fiber in the non-oxidized zone corresponding to the microelement; , , All are empirical parameters; For the Level load cycle The reverse slip length of the fiber corresponding to the cycle; is the level corresponding to the current level fatigue load; is the current cycle number; is the degree of material inhomogeneity of the fibers; is the tensile strength distribution of the fiber after the first heat treatment.
[0038] Optionally, the method further comprises:
[0039] Acquire a cross-sectional image of one of the fibers, and segment the region where the pores of the fiber are located from the cross-sectional image;
[0040] Dividing the cross-sectional image into a plurality of statistical regions according to size;
[0041] According to the position and number of pixels of the pore area of the fiber, the formula determining the degree of material inhomogeneity of the fibers; wherein, is the total number of statistical areas, For the The number of pore pixels contained in the statistical area.
[0042] Optionally, the method further comprises:
[0043] When the interface oxidation length of the microelement at the current number of cycles of the current level fatigue load is less than the matrix crack spacing, and the interface state corresponding to the microelement has debonding and partial slip, the reverse slip length of the fiber corresponding to the current number of cycles of the current level fatigue load is:
[0044] ,in, is the radius value of the fiber; is the stress peak value corresponding to the current level fatigue load; is the stress valley value corresponding to the current level fatigue load; is the volume percentage of the fiber of the unidirectional composite material; is the maximum force of the fibers in the bonding area of the unidirectional composite material; is the minimum force on the fibers in the bonding area of the unidirectional composite material; The interface shear stress value corresponding to the microelement at the current cycle number of the current level fatigue load;
[0045] When the interface oxidation length of the microelement at the current number of cycles of the current level of fatigue load is less than the matrix crack spacing, and the interface state corresponding to the microelement is complete debonding and complete slip, then the reverse slip length of the fiber corresponding to the current number of cycles of the current level of fatigue load is 50% of the matrix crack spacing.
[0046] Optionally, the method further comprises:
[0047] performing a first heat treatment on the fibers included in a fourth preset number of the unidirectional composite materials according to a heat treatment environment condition in a process of preparing the unidirectional composite material;
[0048] Performing a tensile test on the fourth preset number of fibers after the first heat treatment to obtain a tensile strength value corresponding to each fiber;
[0049] Dividing the tensile strength values corresponding to all the fibers into a fifth preset number of numerical intervals, and calculating the tensile strength distribution of the fibers after the first heat treatment; wherein the tensile strength distribution of the fibers is used to characterize the cumulative failure probability corresponding to all the numerical intervals;
[0050] Correspondingly, the construction of the simulation model of the unidirectional composite material includes:
[0051] Randomly generate a failure probability corresponding to each of the microelements;
[0052] According to the failure probability corresponding to each of the micro-elements and using the tensile strength distribution of the fiber after the first heat treatment, the tensile strength value corresponding to each of the micro-elements is determined.
[0053] Optionally, determining the proportion of failed fibers according to the tensile stress values corresponding to the microelements included in all the unit cells and the updated tensile strength values comprises:
[0054] Randomly selecting a target area between a sixth predetermined number of matrix crack spacings of each unit cell, and determining the micro-elements included in each target area;
[0055] When, among all the micro-elements included in the target area, the proportion of the micro-elements whose tensile force value is greater than the updated tensile strength value is greater than or equal to a second preset proportion value, it is determined that the fiber simulated by the unit cell simulation has failed.
[0056] It can be seen from the above content of the present invention that, based on the construction of a simulation model of a unidirectional composite material, the present invention determines the interface state, tensile stress value and matrix crack spacing of each microelement at the current number of cycles of the current fatigue load, as well as the residual strength value of the oxidation zone fiber and the residual strength value of the non-oxidation zone fiber corresponding to each microelement according to the load loading rule of the variable amplitude fatigue test of the unidirectional composite material in the air environment at the first preset temperature; then, according to the residual strength value of the oxidation zone fiber and the residual strength value of the non-oxidation zone fiber corresponding to each microelement, the tensile strength value corresponding to each microelement is updated; thereby, according to the tensile stress value corresponding to the microelement included in all the unit cells and the updated tensile strength value, the proportion of the number of failed fibers is determined; when the proportion of the number of failed fibers is greater than or equal to the first preset ratio value, the variable amplitude fatigue life of the unidirectional composite material is determined according to the current number of cycles of the current fatigue load. Compared with the prior art, the present invention can more accurately predict the variable amplitude fatigue life of the unidirectional composite material. BRIEF DESCRIPTION OF THE DRAWINGS
[0057] In order to more clearly illustrate the technical solutions in the embodiments of the present application, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.
[0058] Figure 1 It is a flow chart of a variable amplitude fatigue life prediction method of a unidirectional composite material disclosed in an embodiment of the present application;
[0059] Figure 2 It is a schematic flow chart of a method for obtaining the tensile strength distribution of the fiber after the first heat treatment disclosed in an embodiment of the present application;
[0060] Figure 3 It is a flow chart of the first strength degradation model construction method disclosed in the embodiment of the present application. DETAILED DESCRIPTION
[0061] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.
[0062] It should be noted that the terms "first", "second", "third" and "fourth" in the specification and claims of the present application are used to distinguish different objects rather than to describe a specific order. The terms "including" and "having" in the embodiments of the present application and any of their variations are intended to cover non-exclusive inclusions, for example, a process, method, device, product or equipment including a series of steps or units is not necessarily limited to those steps or units clearly listed, but may include other steps or units that are not clearly listed or inherent to these processes, methods, products or equipment.
[0063] like Figure 1 As shown, Figure 1 The present invention is a schematic flow chart of a method for predicting the variable amplitude fatigue life of a unidirectional composite material disclosed in an embodiment of the present invention, and the method is used to predict the variable amplitude fatigue life of the unidirectional composite material in an air environment at a first preset temperature. Specifically, the method for predicting the variable amplitude fatigue life of the unidirectional composite material includes:
[0064] Step S101, constructing a simulation model of a unidirectional composite material.
[0065] In this embodiment, the simulation model of the composite material includes a plurality of unit cells composed of a plurality of micro-elements, each unit cell is used to simulate a fiber, a matrix wrapped outside the fiber, and an interface between the fiber and the matrix, and each micro-element is set with a corresponding tensile strength value. Among them, the software for constructing the simulation model and the method for setting the tensile strength value of the micro-element are not limited, and can be reasonably selected according to actual application requirements. For example, the tensile strength value of the micro-element can be set randomly, or the tensile strength value of the micro-element can be set according to a preset strength distribution, and the tensile strength value of the micro-element can also be indirectly calculated and determined based on the tensile strength value measured by the experiment.
[0066] Optionally, considering that the tensile strengths of the fibers included in the composite material are not the same, in order to reasonably and objectively perform numerical simulation on the unidirectional composite material, before step S101, refer to Figure 2 , this embodiment may further include the following steps AC:
[0067] Step A: performing a first heat treatment on the fibers included in a fourth preset number of unidirectional composite materials according to the heat treatment environment conditions in the preparation process of the unidirectional composite materials.
[0068] Among them, step A is mainly used to prepare fiber monomers that are the same as the fibers included in the unidirectional composite material, so as to perform a tensile test on these fibers in the subsequent step B and obtain the tensile strength value corresponding to the fibers. For example, if the unidirectional composite material is prepared in an argon environment at 1000 degrees Celsius, then in step A, the environment corresponding to the first heat treatment is an argon environment, and the corresponding temperature value is 1000 degrees Celsius.
[0069] In addition, the fourth preset number needs to be at least greater than 2, and the specific value is not limited and can be reasonably selected according to actual application requirements. However, in order to ensure that the cumulative failure probability corresponding to all numerical intervals obtained in the subsequent step C can be more accurate, the fourth preset number should not be too small, for example, 100 can be preferably selected.
[0070] Step B: performing a tensile test on the fourth preset number of fibers after the first heat treatment to obtain a tensile strength value corresponding to each fiber.
[0071] Among them, the equipment used for the tensile test is not limited and can be reasonably selected according to actual application requirements.
[0072] Step C: dividing the tensile strength values corresponding to all the fibers into a fifth preset number of numerical intervals, and calculating and obtaining the tensile strength distribution of the fibers after the first heat treatment.
[0073] The specific value of the fifth preset number is not limited and can be reasonably selected according to actual application requirements. The tensile strength distribution of the fiber is used to characterize the cumulative failure probability corresponding to all numerical intervals. After determining the failure probability corresponding to a fiber, the tensile strength value corresponding to the fiber after the first heat treatment can be determined based on the tensile strength distribution of the fiber after the first heat treatment.
[0074] Correspondingly, step S101 may further include the following sub-steps S101a and S101b:
[0075] Sub-step S101a, randomly generating the failure probability corresponding to each microelement.
[0076] The failure probability corresponding to a microelement is used to characterize the failure probability of this section of fiber. There is no limit to the method of randomly generating the failure probability corresponding to each microelement, and a reasonable selection can be made according to the actual application requirements. For example, for a microelement, a random number between 0 and 1 can be randomly generated by the Monte Carlo method, and used as the failure probability corresponding to the microelement.
[0077] Sub-step S101b, according to the failure probability corresponding to each microelement, using the tensile strength distribution of the fiber after the first heat treatment, determines the tensile strength value corresponding to each microelement.
[0078] Step S102, according to the load loading rule of the variable amplitude fatigue test on the unidirectional composite material in the air environment at the first preset temperature, the interface state of each microelement at the current cycle number of the current level fatigue load is determined.
[0079] In this embodiment, the variable amplitude fatigue test is a variable amplitude loading for stretching a unidirectional composite material, which usually includes multiple levels of fatigue loads, each level of fatigue load has a corresponding stress valley value and stress peak value; each level of fatigue load includes multiple cycles. The specific load loading rules of the variable amplitude fatigue test can be reasonably set according to actual application requirements, and this embodiment does not limit this.
[0080] In this embodiment, the microelement generally has interface states such as complete debonding-complete slip, partial debonding-partial slip, complete debonding-partial slip, etc. The specific method for determining the interface state of each microelement at the current cycle number of the current level fatigue load is not limited, and can be reasonably selected according to actual application requirements.
[0081] Step S103, calculating and obtaining the interface shear stress value corresponding to each micro-element according to the interface state of each micro-element.
[0082] In this embodiment, the method for calculating the corresponding interface shear stress value according to the interface state of the microelement is not limited and can be reasonably selected according to actual application requirements.
[0083] Step S104, according to the interface shear stress value corresponding to each microelement, the tensile force value of each microelement and the matrix crack spacing are calculated.
[0084] In this embodiment, the calculation method for calculating the tensile stress value and the matrix crack spacing according to the interface shear stress value corresponding to the microelement is not limited, and can be reasonably selected according to actual application requirements. For example, the tensile stress value corresponding to the microelement can be calculated based on the interface shear stress value corresponding to the microelement using a shear lag model or other models optimized based on the shear lag model.
[0085] Optionally, in order to calculate the tensile stress value of each microelement and the matrix crack spacing more simply and accurately, step S104 may further include the following sub-steps S104a-S104c:
[0086] Sub-step S104a, obtaining the tensile force value of each micro-element according to the interface shear stress value corresponding to each micro-element.
[0087] Sub-step S104b, obtaining the matrix strain energy value of each micro-element according to the tensile force value, matrix modulus and matrix cross-sectional area of each micro-element.
[0088] The matrix modulus and the matrix cross-sectional area are obtained by pre-measurement or setting.
[0089] Sub-step S104c, when the matrix strain energy value of the micro-element exceeds the preset critical matrix strain energy value, it is determined that a new crack is generated, and the matrix crack spacing of each micro-element is obtained.
[0090] Step S105, determining the residual strength value of the fiber in the oxidation zone and the residual strength value of the fiber in the non-oxidation zone corresponding to each microelement according to the interface shear stress value corresponding to each microelement.
[0091] In this embodiment, the specific method for determining the residual strength value of the fibers in the oxidation zone and the residual strength value of the fibers in the non-oxidation zone corresponding to each microelement is not limited and can be reasonably selected according to actual application requirements.
[0092] Optionally, in order to determine the residual strength value of the oxidation zone fiber corresponding to each microelement more simply and accurately, before step S100, refer to Figure 3 , this embodiment may also include the following steps D-I:
[0093] Step D: performing a first heat treatment on the fibers included in the plurality of unidirectional composite materials according to the heat treatment environment conditions in the preparation process of the unidirectional composite materials.
[0094] The heat treatment method in step D is substantially the same or similar to that in step A, and will not be described in detail herein. The fiber after the first heat treatment in step D can be divided into at least two parts, one part for the tensile test in step E, and the other part for the second heat treatment in step G.
[0095] Step E: performing a tensile test on a first preset number of fibers after the first heat treatment to obtain tensile strength values of the fibers after the first heat treatment.
[0096] Among them, step E is basically the same or similar to the aforementioned step B, and will not be repeated here. The number of the first preset number is not limited, and can be reasonably selected according to actual application requirements, and the first preset number in step E and the fourth preset number in step B can be the same or different, which is not limited in this embodiment.
[0097] In addition, when the first preset number is greater than or equal to 2, the tensile strength value of the fiber after the first heat treatment is the average value of all tensile strength measurement values measured by the tensile test.
[0098] Step F, dividing the second preset number of fibers after the first heat treatment into a third preset number of groups, and determining the second heat treatment time corresponding to each group according to the load loading rule of the variable amplitude fatigue test of the unidirectional composite material.
[0099] The value of the third preset number needs to be at least greater than 2, and the specific value is not limited and can be reasonably selected according to actual application requirements. For example, in order to reduce the complexity of the second heat treatment process in step G while ensuring the accuracy of the calculation of the first strength degradation model, the value of the third preset number can be preferably 4.
[0100] The second heat treatment is performed on the second preset number of fibers after the first heat treatment, mainly to prepare fiber monomers identical to the fibers included in the unidirectional composite material in different stages of the variable amplitude fatigue test in the air environment at the first preset temperature. Since each group corresponds to a cycle number of a fatigue load of a specific level, the second heat treatment duration corresponding to each group can be determined according to the load loading rule of the variable amplitude fatigue test of the unidirectional composite material.
[0101] In addition, the reason why the second preset number of fibers after the first heat treatment are divided into a third preset number of groups is to have more groups of data for fitting or training to obtain the first strength degradation model.
[0102] Step G: performing a second heat treatment on a second preset number of fibers after the first heat treatment in an air environment at a first preset temperature according to the second heat treatment duration corresponding to each group.
[0103] Step H: performing a tensile test on a second preset number of fibers after the second heat treatment to obtain a tensile strength value of the fibers corresponding to each group.
[0104] When a group contains a plurality of fibers after the second heat treatment, the tensile strength value of the fibers corresponding to the group is the average value of the tensile strength measurement values of all the fibers in the group.
[0105] Step I: obtaining a first strength degradation model according to the second heat treatment duration corresponding to all groups and the tensile strength values of the fibers.
[0106] Among them, the first strength degradation model is used to characterize the correspondence between the tensile strength distribution of the fiber after the second heat treatment and the tensile strength distribution of the fiber after the first heat treatment and the duration of the second heat treatment. That is, the first strength degradation model can be used to characterize the degradation of the tensile strength of the oxidation zone of the fiber as the variable amplitude fatigue test proceeds. The first strength degradation model can be used to determine the tensile strength distribution of the oxidation zone of the fiber included in the unidirectional composite material under different cycles of different levels of fatigue loads when the variable amplitude fatigue test is carried out in an air environment at a first preset temperature according to the load loading rule.
[0107] In addition, the specific method for obtaining the first strength degradation model is not limited and can be reasonably selected according to actual application requirements. For example, numerical fitting, machine learning and other methods can be used.
[0108] Correspondingly, step S105 may also include: determining the residual strength value of the oxidation zone fiber corresponding to each microelement according to the first strength degradation model and the load loading rule of the variable amplitude fatigue test of the unidirectional composite material in an air environment at a first preset temperature.
[0109] Furthermore, in order to more accurately calculate the tensile strength distribution of the fiber after the second heat treatment, the first strength degradation model may be preferably:
[0110] .
[0111] in, is the tensile strength distribution of the fiber after the second heat treatment; is the average tensile strength corresponding to all groups after the second heat treatment; is the tensile strength distribution of the fiber after the first heat treatment; is the second heat treatment duration; when the unidirectional composite material is subjected to a variable amplitude fatigue test in an air environment at the first preset temperature, , is the current cycle number, is the loading frequency of the variable amplitude fatigue test.
[0112] Optionally, in order to simply and accurately determine the residual strength value of the fiber in the non-oxidized zone corresponding to each microelement, the length of the reverse slip zone under each cycle number can be regarded as the wear length, and step S105 can also include:
[0113] According to the second strength degradation model and the load loading rule of the variable amplitude fatigue test of the unidirectional composite material in the air environment at the first preset temperature, the residual strength value of the fiber in the non-oxidized zone corresponding to each microelement is determined;
[0114] Among them, the second strength degradation model is: ;
[0115] is the residual strength distribution of fiber in non-oxidized zone corresponding to the microelement; , , are all empirical parameters, among which and According to the residual strength test, the location and dispersion of the fiber strength peak are determined respectively; For the Level load cycle The reverse slip length of the fiber corresponding to the cycle; is the level corresponding to the current level fatigue load; is the current cycle number; is the degree of material heterogeneity of the fiber; is the tensile strength distribution of the fiber after the first heat treatment.
[0116] Furthermore, in order to more accurately and reasonably characterize the material non-uniformity of the fiber, this embodiment may further include the following steps J to L:
[0117] Step J, obtaining a cross-sectional image of a fiber, and segmenting the region where the pores of the fiber are located from the cross-sectional image.
[0118] There are no restrictions on the method of acquiring the cross-sectional image of the fiber and the method of dividing the area where the pores of the fiber are located, and they can be reasonably selected according to actual application requirements.
[0119] Step K: divide the cross-sectional image into multiple statistical regions according to their sizes.
[0120] The number of statistical regions is not limited and can be reasonably selected according to actual application requirements. It should be noted that when dividing the statistical regions, all statistical regions just completely include the region where the cross section of the fiber is located.
[0121] Step L, according to the location and number of pixels of the fiber pore area, use the formula Determine the degree of material inhomogeneity of the fibers.
[0122] In this formula, is the total number of statistical areas, For the The number of void pixels contained in a statistical area.
[0123] Furthermore, in order to more accurately determine the length of the reverse slip zone at each cycle number, this embodiment may further include:
[0124] When the interface oxidation length of the microelement at the current number of cycles of the current level fatigue load is greater than or equal to the matrix crack spacing, the reverse slip length of the fiber corresponding to the current number of cycles of the current level fatigue load is 0.
[0125] When the interface oxidation length of the microelement at the current number of cycles of the current level of fatigue load is less than the matrix crack spacing, and the interface state corresponding to the microelement has debonding (including partial debonding and complete debonding) and partial slip, the reverse slip length of the fiber corresponding to the current number of cycles of the current level of fatigue load is:
[0126] .
[0127] in, is the radius of the fiber; is the peak stress value corresponding to the current level fatigue load; is the stress valley value corresponding to the current level fatigue load; is the volume percentage of fiber in unidirectional composite materials; is the maximum force on the fibers in the bonding area of the unidirectional composite material; It is the minimum force on the fibers in the bonding area of the unidirectional composite material; It is the interface shear stress value corresponding to the microelement at the current cycle number of the current level fatigue load.
[0128] When the interface oxidation length of the microelement at the current number of cycles of the current level of fatigue load is less than the matrix crack spacing, and the interface state corresponding to the microelement is complete debonding and complete slip, the reverse slip length of the fiber corresponding to the current number of cycles of the current level of fatigue load is 50% of the matrix crack spacing.
[0129] Step S106, updating the tensile strength value corresponding to each micro-element according to the residual strength value of the fiber in the oxidation zone and the residual strength value of the fiber in the non-oxidation zone corresponding to each micro-element.
[0130] In the present embodiment, since the tensile strength values of the fibers at different positions in the unidirectional composite material may change each time loading is completed during the variable amplitude fatigue test of the unidirectional composite material, it is necessary to update the tensile strength value corresponding to each microelement set in step S101 according to the residual strength value of the fibers in the oxidation zone and the residual strength value of the fibers in the non-oxidation zone corresponding to each microelement in step S106.
[0131] Optionally, in order to more accurately determine whether the fiber is broken, step S106 may also include: taking the smaller value of the residual strength value of the fiber in the oxidation zone and the residual strength value of the fiber in the non-oxidation zone corresponding to the microelement as the tensile strength value corresponding to the microelement.
[0132] For example, when the residual strength value of the fiber in the oxidation zone corresponding to a microelement is greater than the residual strength value of the fiber in the non-oxidation zone, the residual strength value of the fiber in the non-oxidation zone corresponding to the microelement is used as the tensile strength value corresponding to the microelement.
[0133] When the residual strength value of the fiber in the oxidation zone corresponding to a microelement is less than the residual strength value of the fiber in the non-oxidation zone, the residual strength value of the fiber in the oxidation zone corresponding to the microelement is used as the tensile strength value corresponding to the microelement.
[0134] Furthermore, considering that during the variable amplitude fatigue test of the unidirectional composite material, both the matrix cracks and the interface channels may be closed due to oxidation, in order to more accurately and reasonably characterize the tensile strength value corresponding to the microelement, step S106 may also include the following sub-steps S106a and S106b:
[0135] Sub-step S106a, when the matrix crack spacing of the microelement satisfies the matrix oxidation channel closure condition, the tensile strength value corresponding to the microelement is updated according to the residual strength value of the fiber in the non-oxidized zone corresponding to the microelement.
[0136] Sub-step S106b, when the matrix crack of the microelement satisfies the interface oxidation channel closure condition, the tensile strength value corresponding to the microelement is updated according to the residual strength value of the oxidation zone fiber corresponding to the microelement.
[0137] Furthermore, the closing condition of the substrate oxidation channel can be preset as follows: the substrate crack spacing is equal to twice the thickness of the silicon dioxide growth on the substrate on both sides of the substrate crack.
[0138] And the closing condition of the interface oxidation channel can be preset as follows: the thickness of the interface is equal to the sum of the thickness of the silicon dioxide growth on the substrate and the thickness of the silicon dioxide growth on the fiber on both sides of the interface.
[0139] Step S107, determining the percentage of failed fibers according to the tensile force values corresponding to the microelements included in all unit cells and the updated tensile strength values.
[0140] In this embodiment, the tensile stress value corresponding to the microelement in step S107 is obtained by calculation in step S104. When the tensile stress value corresponding to the microelement is greater than the tensile strength value, it indicates that the fiber in the unit cell may be broken. The tensile stress value corresponding to one or more microelement included in a unit cell and the updated tensile strength value can be used to determine whether the fiber simulated by the unit cell is broken, that is, whether the fiber is failed, so as to further calculate the proportion of failed fibers.
[0141] Optionally, in order to reduce the amount of data calculation and processing while ensuring accurate judgment of whether the fiber is invalid, step S107 may further include the following sub-steps S107a-S107b:
[0142] Sub-step S107a, randomly selecting a target region between a sixth predetermined number of matrix crack spacings of each unit cell, and determining the micro-elements included in each target region.
[0143] The specific value of the sixth predetermined number is not limited and can be reasonably selected according to actual application requirements. For example, the value of the sixth predetermined number can be preferably 3 or 5.
[0144] Sub-step S107b, when the proportion of the number of micro-elements whose tensile stress values are greater than the updated tensile strength value among all micro-elements included in the target area is greater than or equal to a second preset proportion value, it is determined that the fiber simulated by the unit cell simulation has failed.
[0145] The specific value of the second preset ratio is not limited and can be reasonably selected according to actual application requirements. For example, when the value of the sixth predetermined number is 3, the second preset ratio can be preferably 66%.
[0146] Step S108, when the proportion of the number of failed fibers is greater than or equal to the first preset proportion value, the variable amplitude fatigue life of the unidirectional composite material is determined according to the current cycle number of the current level fatigue load.
[0147] In this embodiment, when the proportion of failed fibers is greater than or equal to the first preset ratio value, it indicates that the unidirectional composite material has failed, and thus the variable amplitude fatigue life of the unidirectional composite material can be determined according to the current number of cycles of the current level fatigue load. The specific value of the first preset ratio value is not limited and can be reasonably selected according to actual application requirements.
[0148] In this embodiment, step S109 may be included: when the proportion of failed fibers is less than a first preset ratio, the current number of cycles of the current level fatigue load is updated according to the load loading rule of the variable amplitude fatigue test on the unidirectional composite material in an air environment at a first preset temperature.
[0149] When the proportion of failed fibers is less than the first preset ratio, it indicates that the unidirectional composite material has not failed, and the variable amplitude fatigue life of the unidirectional composite material needs to be calculated. That is, after step S109 is completed, it is necessary to return to step S102-step S107, and step S108 or step S109.
[0150] Optionally, after updating the current number of cycles of the current level fatigue load in step S109, if the peak value of the updated current level fatigue load is greater than the peak value of the current level fatigue load before the update, it indicates that new matrix cracks may appear, and the matrix crack spacing of each microelement needs to be recalculated, that is, the matrix crack spacing of each microelement needs to be recalculated when step S104 is executed again. When the peak value of the updated current level fatigue load is less than or equal to the peak value of the current level fatigue load before the update, due to the interface wear causing the interface shear stress to decrease and the interface oxidation zone to become longer, etc., it is considered that the matrix crack spacing remains unchanged, that is, it is not necessary to recalculate the matrix crack spacing of each microelement when step S104 is executed again. Specifically, when step S104 is executed again, step S104 includes the following sub-steps S104d and S104e:
[0151] Sub-step S104d, when the updated peak value of the current level fatigue load is greater than the peak value of the current level fatigue load before updating, recalculate the matrix crack spacing of each microelement according to the load loading rule of the variable amplitude fatigue test of the unidirectional composite material in the air environment at the first preset temperature.
[0152] Sub-step S104e, when the peak value of the fatigue load of the current level after update is less than or equal to the peak value of the fatigue load of the current level before update, the matrix crack spacing of each microelement remains unchanged.
[0153] It can be seen from the above description of the embodiments of the present invention that the variable amplitude fatigue life prediction method of the unidirectional composite material of this embodiment can more accurately predict the variable amplitude fatigue life of the unidirectional composite material in a high temperature air environment; a first strength degradation model caused by oxidation is established by analyzing the oxidation time and the fiber strength degradation law; a second strength degradation model caused by wear is established by comprehensively considering the interface wear distance and the uneven degree of pores, which can more realistically simulate the fatigue strengthening phenomenon in the variable amplitude cyclic loading process and the strength degradation phenomenon caused by excessive wear of the fiber; in the preferred second strength degradation model, the uneven degree of pore distribution of the fiber material is taken into account, and the determined characterization method can take into account the material defects in the preparation process of the unidirectional composite material. The above method is helpful to accurately predict the mechanical behavior such as fatigue life and residual strength of the material, and assist in the optimization design of structural parts such as turbine blades; further, combined with the matrix crack spacing and the growth rate of silica, the matrix oxidation channel closure condition and the interface oxidation channel closure condition are established, which can more accurately and objectively determine the tensile strength value of the microelement.
[0154] So far, specific embodiments of the present application have been described. Other embodiments are within the scope of the appended claims. In some cases, the actions recorded in the claims can be performed in a different order and still achieve the desired results. In addition, the processes depicted in the accompanying drawings do not necessarily require the specific order or sequential order shown to achieve the desired results. In some embodiments, multitasking and parallel processing can be advantageous.
[0155] The present application is described with reference to the flowcharts and / or block diagrams of the methods according to the embodiments of the present application. It should be understood that each process and / or block in the flowchart and / or block diagram, as well as the combination of the processes and / or blocks in the flowchart and / or block diagram, can be implemented by computer program instructions. These computer program instructions can be provided to a processor of a general-purpose computer, a special-purpose computer, an embedded processor, or other programmable data processing device to generate a machine, so that the instructions executed by the processor of the computer or other programmable data processing device generate instructions for implementing the processes in the flowchart and / or block diagram. Figure 1 A process or multiple processes and / or boxes Figure 1 A device that provides the functions specified in a block or multiple blocks.
[0156] It should also be noted that the terms "include", "comprises" or any other variations thereof are intended to cover non-exclusive inclusion, so that a process, method, commodity or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, commodity or device. In the absence of more restrictions, the elements defined by the sentence "comprises a ..." do not exclude the existence of other identical elements in the process, method, commodity or device including the elements.
[0157] Those skilled in the art should understand that the embodiments of the present application can be provided as methods and devices. Therefore, the present application can take the form of a complete hardware embodiment, a complete software embodiment, or an embodiment combining software and hardware. Moreover, the present application can take the form of a computer program product implemented on one or more computer storage media (including but not limited to disk storage, CD-ROM, optical storage, etc.) containing computer-usable program codes.
[0158] The various embodiments in this specification are described in a progressive manner, and the same or similar parts between the various embodiments can be referenced to each other, and each embodiment focuses on the differences from other embodiments.
[0159] The above are only embodiments of the present application and are not intended to limit the present application. For those skilled in the art, the present application may have various changes and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present application should be included within the scope of the claims of the present application.
Claims
1. A method for predicting variable amplitude fatigue life of unidirectional composite materials, characterized in that: The method comprises: Constructing a simulation model of a unidirectional composite material; wherein the simulation model includes a plurality of unit cells composed of a plurality of microelements, each of the unit cells is used to simulate a fiber, a matrix wrapped outside the fiber, and an interface between the fiber and the matrix, and each of the microelements is set with a corresponding tensile strength value; Determining the interface state of each of the micro-element at the current cycle number of the current fatigue load according to a load loading rule of a variable amplitude fatigue test on the unidirectional composite material in an air environment at a first preset temperature; According to the interface state of each micro-element, the interface shear stress value corresponding to each micro-element is calculated; According to the interface shear stress value corresponding to each microelement, the tensile force value and matrix crack spacing of each microelement are calculated; Determine the residual strength value of the fiber in the oxidation zone and the residual strength value of the fiber in the non-oxidation zone corresponding to each microelement according to the interface shear stress value corresponding to each microelement; Update the tensile strength value corresponding to each micro-element according to the residual strength value of the fiber in the oxidation zone and the residual strength value of the fiber in the non-oxidation zone corresponding to each micro-element; Determine the percentage of failed fibers according to the tensile force values corresponding to the microelements included in all the unit cells and the updated tensile strength values; When the proportion of the number of failed fibers is greater than or equal to a first preset proportion value, the variable amplitude fatigue life of the unidirectional composite material is determined according to the current number of cycles of the current level fatigue load.
2. The method according to claim 1, characterized in that The updating of the tensile strength value corresponding to each microelement according to the residual strength value of the fiber in the oxidation zone and the residual strength value of the fiber in the non-oxidation zone corresponding to each microelement comprises: The smaller one of the residual strength value of the fiber in the oxidation zone and the residual strength value of the fiber in the non-oxidation zone corresponding to the microelement is taken as the tensile strength value corresponding to the microelement.
3. The method according to claim 2, characterized in that The updating of the tensile strength value corresponding to each microelement according to the residual strength value of the fiber in the oxidation zone and the residual strength value of the fiber in the non-oxidation zone corresponding to each microelement comprises: When the matrix crack spacing of the microelement satisfies the matrix oxidation channel closing condition, the tensile strength value corresponding to the microelement is updated according to the residual strength value of the fiber in the non-oxidized zone corresponding to the microelement; When the matrix crack of the microelement satisfies the interface oxidation channel closure condition, the tensile strength value corresponding to the microelement is updated according to the residual strength value of the oxidation zone fiber corresponding to the microelement.
4. The method according to claim 1, characterized in that: The method further comprises: According to the heat treatment environment conditions in the preparation process of the unidirectional composite material, a first heat treatment is performed on the fibers included in the plurality of unidirectional composite materials; performing a tensile test on a first preset number of the fibers after the first heat treatment, respectively, to obtain tensile strength values of the fibers after the first heat treatment; Dividing a second preset number of the fibers after the first heat treatment into a third preset number of groups, and determining the second heat treatment duration corresponding to each group according to a load loading rule for the variable amplitude fatigue test of the unidirectional composite material; In the air environment of the first preset temperature, performing a second heat treatment on the second preset number of the fibers after the first heat treatment according to the second heat treatment duration corresponding to each group; Performing a tensile test on the second preset number of the fibers after the second heat treatment, respectively, to obtain a tensile strength value of the fibers corresponding to each group; A first strength degradation model is obtained according to the second heat treatment duration and the tensile strength value of the fiber corresponding to all groups; wherein the first strength degradation model is used to characterize the corresponding relationship between the tensile strength distribution of the fiber after the second heat treatment and the tensile strength distribution of the fiber after the first heat treatment and the second heat treatment duration; Correspondingly, determining the residual strength value of the fiber in the oxidation zone and the residual strength value of the fiber in the non-oxidation zone corresponding to each microelement according to the interface shear stress value corresponding to each microelement includes: The residual strength value of the oxidation zone fiber corresponding to each of the microelements is determined according to the first strength degradation model and the load loading rule of the variable amplitude fatigue test of the unidirectional composite material in the air environment at the first preset temperature.
5. The method according to claim 4, characterized in that The first strength degradation model is: ; in, is the tensile strength distribution of the fiber after the second heat treatment; is the average tensile strength corresponding to all groups after the second heat treatment; is the tensile strength distribution of the fiber after the first heat treatment; is the duration of the second heat treatment; when the variable amplitude fatigue test is performed on the unidirectional composite material in the air environment at the first preset temperature, , is the current cycle number, is the load loading frequency of the variable amplitude fatigue test.
6. The method according to claim 1, characterized in that The method further comprises: According to the heat treatment environment conditions in the preparation process of the unidirectional composite material, a first heat treatment is performed on the fibers included in the plurality of unidirectional composite materials; performing a tensile test on a first preset number of the fibers after the first heat treatment, respectively, to obtain tensile strength values of the fibers after the first heat treatment; Correspondingly, determining the residual strength value of the fiber in the oxidation zone and the residual strength value of the fiber in the non-oxidation zone corresponding to each microelement according to the interface shear stress value corresponding to each microelement includes: Determine the residual strength value of the fiber in the non-oxidized zone corresponding to each of the micro-elements according to the second strength degradation model and the load loading rule of the variable amplitude fatigue test of the unidirectional composite material in the air environment at the first preset temperature; Wherein, the second strength degradation model is: ; is the residual strength distribution of the fiber in the non-oxidized zone corresponding to the microelement; , , All are empirical parameters; For the Level load cycle The reverse slip length of the fiber corresponding to the cycle; is the level corresponding to the current level fatigue load; is the current cycle number; is the degree of material inhomogeneity of the fibers; is the tensile strength distribution of the fiber after the first heat treatment.
7. The method according to claim 6, characterized in that The method further comprises: Acquire a cross-sectional image of one of the fibers, and segment the region where the pores of the fiber are located from the cross-sectional image; Dividing the cross-sectional image into a plurality of statistical regions according to size; According to the position and number of pixels of the pore area of the fiber, the formula determining the degree of material inhomogeneity of the fibers; wherein, is the total number of statistical areas, For the The number of pore pixels contained in the statistical area.
8. The method according to claim 6, characterized in that The method further comprises: When the interface oxidation length of the microelement at the current number of cycles of the current level fatigue load is less than the matrix crack spacing, and the interface state corresponding to the microelement has debonding and partial slip, the reverse slip length of the fiber corresponding to the current number of cycles of the current level fatigue load is: ,in, is the radius value of the fiber; is the stress peak value corresponding to the current level fatigue load; is the stress valley value corresponding to the current level fatigue load; is the volume percentage of the fiber of the unidirectional composite material; is the maximum force of the fibers in the bonding area of the unidirectional composite material; is the minimum force on the fibers in the bonding area of the unidirectional composite material; The interface shear stress value corresponding to the microelement at the current cycle number of the current level fatigue load; When the interface oxidation length of the microelement at the current number of cycles of the current level of fatigue load is less than the matrix crack spacing, and the interface state corresponding to the microelement is complete debonding and complete slip, then the reverse slip length of the fiber corresponding to the current number of cycles of the current level of fatigue load is 50% of the matrix crack spacing.
9. The method according to claim 1, characterized in that: The method further comprises: performing a first heat treatment on the fibers included in a fourth preset number of the unidirectional composite materials according to a heat treatment environment condition in a process of preparing the unidirectional composite material; Performing a tensile test on the fourth preset number of fibers after the first heat treatment to obtain a tensile strength value corresponding to each fiber; Dividing the tensile strength values corresponding to all the fibers into a fifth preset number of numerical intervals, and calculating the tensile strength distribution of the fibers after the first heat treatment; wherein the tensile strength distribution of the fibers is used to characterize the cumulative failure probability corresponding to all the numerical intervals; Correspondingly, the construction of the simulation model of the unidirectional composite material includes: Randomly generate a failure probability corresponding to each of the microelements; According to the failure probability corresponding to each of the micro-elements and using the tensile strength distribution of the fiber after the first heat treatment, the tensile strength value corresponding to each of the micro-elements is determined.
10. The method according to claim 1, characterized in that Determining the proportion of failed fibers according to the tensile stress values corresponding to the microelements included in all the unit cells and the updated tensile strength values includes: Randomly selecting a target area between a sixth predetermined number of matrix crack spacings of each unit cell, and determining the micro-elements included in each target area; When, among all the micro-elements included in the target area, the proportion of the micro-elements whose tensile force value is greater than the updated tensile strength value is greater than or equal to a second preset proportion value, it is determined that the fiber simulated by the unit cell simulation has failed.