Tunnel lining reinforcement method based on sprayed UHPC
Through the combined technology of spraying UHPC materials and high-strength steel mesh, the tunnel lining is reinforced, which solves the problem of low reinforcement strength in the existing technology and significantly improves the bearing capacity and durability of the tunnel structure.
Patent Information
- Application Number
- CN202411002463.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-25
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2044-07-25
AI Technical Summary
Existing tunnel lining reinforcement methods have the problem of low reinforcement strength, making it difficult to effectively improve the bearing capacity and durability of the tunnel structure.
The tunnel lining reinforcement method based on spraying UHPC is used to realize the tunnel lining by configuring UHPC materials, calculating the target spray thickness, performing interface processing and cleaning of the area to be reinforced, arranging high-strength steel mesh, spraying UHPC materials to the target thickness, and performing trimming and maintenance. Reinforcement of lining.
It improves the strength of the tunnel lining after reinforcement, improves the bearing capacity and durability of the tunnel structure, and reduces the reinforcement thickness.
Smart Images

Figure CN118517287B_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of tunnel lining reinforcement, and in particular to a tunnel lining reinforcement method based on sprayed UHPC. Background Art
[0002] During the construction and operation process, the tunnel lining will be affected by factors such as geological topography, external environment, and uncertainties in the design, construction, and operation process, causing various cracks and damages to occur during the tunnel's service life, requiring reinforcement of the tunnel lining.
[0003] Tunnel lining reinforcement is a performance improvement method that takes lining concrete as the object and takes measures to increase the structural bearing capacity by adding reinforcement materials. However, the existing reinforcement methods have the defect of low reinforcement strength. Summary of the invention
[0004] The purpose of this application is to provide a tunnel lining reinforcement method based on sprayed UHPC, which can improve the strength of the tunnel lining after reinforcement to enhance the bearing capacity and durability of the tunnel structure.
[0005] The present application embodiment provides a tunnel lining reinforcement method based on sprayed UHPC, comprising:
[0006] Configure UHPC materials according to preset target material parameters;
[0007] Calculating a target spraying thickness for spraying the UHPC material;
[0008] Performing interface treatment on the area to be reinforced of the tunnel lining to obtain the treated area to be reinforced;
[0009] Cleaning the processed area to be reinforced to obtain a cleaned area to be reinforced;
[0010] Arranging a high-strength steel wire mesh on the inner surface of the cleaned area to be reinforced;
[0011] After arranging the high-strength steel wire mesh, spraying the UHPC material onto the cleaned area to be reinforced until the target spraying thickness is reached, thereby obtaining the area to be reinforced after spraying;
[0012] The surface of the area to be reinforced after the spraying is trimmed and maintained to complete the reinforcement.
[0013] In some embodiments, the UHPC material is composed of cement, mineral admixture, fine aggregate, water reducing agent, accelerating agent, steel fiber and water, and the UHPC material is configured according to the preset target material parameters, including:
[0014] According to the preset flow parameters, determining the amount of the water reducing agent, the mass ratio between the water and the accelerating setting agent, and the amount of the mineral admixture;
[0015] Determining the dosage of the accelerating agent or the maximum particle size of the fine aggregate according to the preset rebound parameter;
[0016] The amount of the steel fiber or the amount of the mineral admixture is determined according to the preset mechanical parameters; the amount of the steel fiber is not more than 3%, and the amount of the mineral admixture is not more than 35%.
[0017] In some embodiments, the UHPC material consists of 32% cement, 10% mineral admixture, 42% fine aggregate, 1% water reducer, 5% accelerating agent, 2% steel fiber and 8% water.
[0018] In some embodiments, the target spray thickness is calculated as follows:
[0019] ,
[0020] ,
[0021] in, is the compressive strain of the cracked tunnel, To strengthen the tensile strain of concrete, is the elastic modulus of the cracked tunnel, The elastic modulus of reinforced concrete; The area of cracked tunnel to be reinforced; To reinforce the concrete area, , L is the length of the area to be reinforced, is the thickness of the damaged tunnel, is the target spray thickness, For external load.
[0022] In some embodiments, the step of performing interface treatment on the area to be reinforced of the tunnel lining to obtain the treated area to be reinforced includes:
[0023] The interface roughness of the area to be reinforced of the tunnel lining is adjusted by roughening, grooving and / or sandblasting, and an interface adhesive is added to the area to be reinforced of the tunnel lining.
[0024] In some embodiments, the step of cleaning the processed area to be reinforced to obtain the cleaned area to be reinforced includes:
[0025] The treated area to be reinforced is cleaned by a scraper and / or a high-pressure water gun.
[0026] In some embodiments, before arranging the high-strength steel wire mesh, the UHPC material is sprayed onto the cleaned area to be reinforced to form a UHPC protective layer, the thickness of the high-strength steel wire mesh is 3 mm, the mesh size is 100 mm×100 mm, the laying spacing is 150 mm, and the thickness of the UHPC protective layer is not less than 20 mm.
[0027] In some embodiments, after arranging the high-strength steel wire mesh, spraying the UHPC material onto the cleaned area to be reinforced until the target spraying thickness is reached, to obtain the sprayed area to be reinforced, comprising:
[0028] Arrange a wet shotcrete device; the wet shotcrete device includes a feeding system and a spraying system;
[0029] storing the UHPC material into the feed system;
[0030] The spraying system is controlled to absorb the UHPC material from the feeding system, and the UHPC material is sprayed onto the high-strength steel wire mesh and the cleaned area to be reinforced by wet spraying until the target spraying thickness is reached.
[0031] In some embodiments, the injection system is connected to a first material delivery pipe and a second material delivery pipe, and the lumen of the first material delivery pipe is provided with a pipe connector;
[0032] The pipeline connector is provided with a discharge port and a feed port, the discharge port is communicated with the first feed pipe, the feed port is connected to the second feed pipe and is provided with a feed valve; the injection system transports the accelerator through the second feed pipe, is connected to the first feed pipe through the pipeline connector, and injects the UHPC material to the outside through the first feed pipe.
[0033] In some embodiments, the surface of the area to be reinforced after spraying is trimmed and maintained to complete the reinforcement, including:
[0034] Before the UHPC material is finally set, the surface of the area to be reinforced after the spraying is scraped and trimmed with a scraper. After the UHPC material is finally set, the surface of the area to be reinforced after the spraying is regularly wetted within a preset curing period.
[0035] The beneficial effects of the present application are as follows: UHPC materials are used to reinforce tunnel linings, UHPC materials are configured according to preset target material parameters, and the target spraying thickness of the UHPC materials is calculated. After interface treatment, cleaning, and arrangement of high-strength steel wire mesh in the area to be reinforced, UHPC materials are sprayed into the area to be reinforced until the target spraying thickness is reached, and finally finishing and maintenance are performed to achieve the reinforcement of the tunnel lining, which can reduce the reinforcement thickness and increase the strength of the area to be reinforced, increase the strength of the tunnel lining after reinforcement, and enhance the bearing capacity and durability of the tunnel structure. BRIEF DESCRIPTION OF THE DRAWINGS
[0036] Figure 1 It is a flow chart of a tunnel lining reinforcement method based on sprayed UHPC provided in an embodiment of the present application.
[0037] Figure 2 It is a schematic diagram of the connection between the first material delivery pipe and the second material delivery pipe provided in an embodiment of the present application.
[0038] Figure 3 It is a schematic diagram of the structure of the pipeline connector provided in an embodiment of the present application. DETAILED DESCRIPTION
[0039] In order to make the purpose, technical solution and advantages of the present application more clearly understood, the present application is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present application and are not used to limit the present application.
[0040] It should be noted that the terms "first", "second", "third", "fourth", etc. (if any) in the specification of the present application and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequence. It should be understood that the data used in this way can be interchangeable where appropriate, so that the embodiments of the present application described herein can be implemented in an order other than those illustrated or described herein. In addition, the terms "including" and "having" and any of their variations are intended to cover non-exclusive inclusions, for example, a process, method, system, product or device that includes a series of steps or circuits is not necessarily limited to those steps or circuits clearly listed, but may include other steps or circuits that are not clearly listed or inherent to these processes, methods, products or devices.
[0041] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art to which this application belongs. The terms used herein are only for the purpose of describing the embodiments of this application and are not intended to limit this application.
[0042] See also Figure 1 , Figure 1is a flow chart of a tunnel lining reinforcement method based on sprayed UHPC provided in an embodiment of the present application. In some embodiments of the present application, Figure 1 The method may specifically include but is not limited to steps S101 to S107. Figure 1 These seven steps are introduced in detail.
[0043] Step S101, configuring UHPC material according to preset target material parameters.
[0044] Among them, UHPC materials are composed of cement, mineral admixtures, fine aggregates, water reducers, accelerators, steel fibers and water. UHPC (Ultra-High Performance Concrete), also known as reactive powder concrete, has ultra-high durability and ultra-high mechanical properties. Compared with traditional concrete, UHPC is a building material with high strength, high density, excellent durability and high toughness.
[0045] Specifically, the UHPC material can be configured by dry-mixing cement, mineral admixtures, fine aggregates and water reducers for not less than 120 seconds, then adding water to the mixed mixture for not less than 120 seconds, and finally adding steel fibers to ensure that the steel fibers are evenly distributed and not clumped.
[0046] In a specific embodiment, step S101 specifically includes the following steps: determining the amount of water reducing agent, the mass ratio between water and accelerator and the amount of mineral admixture according to preset flow parameters; determining the amount of accelerator or the maximum particle size of fine aggregate according to preset rebound parameters; determining the amount of steel fiber or the amount of mineral admixture according to preset mechanical parameters.
[0047] For example, if the flowability of UHPC materials needs to be enhanced, the amount of water reducer, the mass ratio of water to accelerator and / or the amount of each mineral admixture can be increased; if the rebound rate of UHPC materials needs to be reduced, the amount of accelerator can be increased or the maximum particle size of fine aggregate can be reduced; if the mechanical properties of UHPC materials need to be improved, the amount of steel fiber or the amount of mineral admixture can be increased. Among them, the amount of steel fiber is not more than 3%, and the amount of mineral admixture is not more than 35%.
[0048] In a specific embodiment, the UHPC material is composed of 32% cement, 10% mineral admixture, 42% fine aggregate, 1% water reducer, 5% accelerating agent, 2% steel fiber and 8% water.
[0049] Step S102, calculating the target spraying thickness of the sprayed UHPC material.
[0050] In a specific embodiment, the target spray thickness is calculated as follows:
[0051] ,
[0052] ,
[0053] in, is the compressive strain of the cracked tunnel, To strengthen the tensile strain of concrete, is the elastic modulus of the cracked tunnel, The elastic modulus of reinforced concrete; The area of cracked tunnel to be reinforced; To reinforce the concrete area, , L is the length of the area to be reinforced, is the thickness of the damaged tunnel, is the target spray thickness, For external load.
[0054] The tunnel lining reinforcement method based on sprayed UHPC provided in this embodiment calculates the target spraying thickness of the sprayed UHPC material through the above calculation formula, and calculates the target spraying thickness of the sprayed UHPC material equivalently based on the optimization of the tunnel lining stress and the structural parameters and mechanical parameters related to the tunnel lining, clarifies the range of the target spraying thickness of the sprayed UHPC material, and improves the bearing capacity and durability of the tunnel structure.
[0055] Step S103, performing interface treatment on the area to be reinforced of the tunnel lining to obtain a treated area to be reinforced.
[0056] In a specific embodiment, step S103 specifically includes the following steps: adjusting the interface roughness of the area to be reinforced of the tunnel lining by roughening, grooving and / or sandblasting, and adding an interface adhesive to the area to be reinforced of the tunnel lining.
[0057] Specifically, the inner surface of the area to be reinforced of the tunnel lining can be roughened by an electric hammer so that coarse aggregate is exposed on the inner surface of the area to be reinforced of the tunnel lining. The roughening depth is about 1.5 mm. Then, a scraper or a water gun is used to clean the surface debris, thereby completing the interface treatment of the area to be reinforced of the tunnel lining to obtain the treated area to be reinforced.
[0058] Step S104, cleaning the processed area to be reinforced to obtain a cleaned area to be reinforced.
[0059] In a specific embodiment, step S104 specifically includes the following steps: cleaning the treated area to be reinforced by using a scraper and / or a high-pressure water gun.
[0060] Specifically, smaller debris and / or gravel are cleaned by a scraper, and larger debris and / or gravel are cleaned by a high-pressure water gun.
[0061] Step S105, arranging a high-strength steel wire mesh on the inner surface of the cleaned area to be reinforced.
[0062] In a specific embodiment, before arranging the high-strength steel wire mesh, UHPC material is sprayed onto the cleaned area to be reinforced to form a UHPC protective layer. The thickness of the high-strength steel wire mesh is 3 mm, the mesh size is 100 mm×100 mm, the laying spacing is 150 mm, and the thickness of the UHPC protective layer is not less than 20 mm.
[0063] Specifically, the high-strength steel wire mesh is cut according to the specification requirements and bent according to the geometric shape of the tunnel. A high-strength steel wire mesh with a thickness of 3mm is used, the mesh size is 100mm×100mm, and the laying spacing is 150mm. The high-strength steel wire mesh is arranged on the cleaned area to be reinforced to ensure that the high-strength steel wire mesh fits tightly with the UHPC protective layer on the surface of the cleaned area to be reinforced. In the process of laying the high-strength steel wire mesh, attention should be paid to the flatness and verticality of the high-strength steel wire mesh to ensure that it meets the requirements.
[0064] Step S106, after arranging the high-strength steel wire mesh, spraying UHPC material onto the cleaned area to be reinforced until the target spraying thickness is reached, thereby obtaining the area to be reinforced after spraying.
[0065] In a specific embodiment, step S106 specifically includes the following steps: arranging a wet spraying concrete device, the wet spraying concrete device including a feeding system and a spraying system; storing the UHPC material in the feeding system; controlling the spraying system to absorb the UHPC material from the feeding system, and using a wet spraying method to spray the UHPC material onto the high-strength steel wire mesh and the cleaned area to be reinforced until the target spraying thickness is reached.
[0066] Specifically, firstly, a suitable location is selected according to the site conditions to arrange the wet spraying concrete device, and the UHPC material is mixed in the feeding system. First, the cement, mineral admixture, fine aggregate and water reducer are dry-mixed and stirred, and then water is added to the stirred mixture and stirred. Finally, steel fiber is added, and the generated UHPC material is stored in the feeding system. Then, the spraying system is controlled to absorb the UHPC material from the feeding system, and the UHPC material is sprayed onto the high-strength steel wire mesh and the cleaned area to be reinforced by wet spraying. During spraying, the angle between the nozzle and the area to be reinforced is controlled to be 90° to reduce rebound and increase the maximum compaction of the UHP material until the target spraying thickness is reached. The feeding system may include a concrete mixer, a water tank, and additives, and the injection system may be an air compressor. After ensuring that the pipelines between the feeding system and the injection system are correctly connected and leak-free, the feeding system and the injection system are controlled to start. According to the requirements of the injection UHPC material and the characteristics of the accelerator, the output pressure and flow rate of the injection system are adjusted. For example, the working wind pressure for side wall reinforcement is 0.3MPa~0.5MPa, and the working wind pressure for arch reinforcement is 0.4MPa~0.65MPa.
[0067] See also Figure 2 In a specific embodiment, the injection system is connected with a first feed pipe 100 and a second feed pipe 200, and the lumen of the first feed pipe 100 is provided with a pipe connector 300. The pipe connector 300 is provided with a discharge port 310 and a feed port 320, the discharge port 310 is communicated with the first feed pipe 100, and the feed port 320 is connected with the second feed pipe 200 and provided with a feed valve 330. The injection system transports the accelerating agent through the second feed pipe 200, connects to the first feed pipe 100 through the pipe connector 300, and injects the UHPC material to the outside through the first feed pipe 100.
[0068] Specifically, the discharge port 310 of the pipe connector 300 is connected to the first feed pipe 100, and the feed port 320 of the pipe connector 300 is connected to the second feed pipe 200 when the feed valve 330 is opened. The feeding system supplies the UHPC material without the accelerator to the injection system through the pipeline. The injection system transports the UHPC material without the accelerator through the first feed pipe 100 and transports the accelerator through the second feed pipe 200. The accelerator in the second feed pipe 200 is connected to the first feed pipe 100 through the pipe connector 300 and mixed with the UHPC material. The UHPC material mixed with the accelerator is injected to the outside.
[0069] Step S107, trimming and maintaining the surface of the area to be reinforced after spraying to complete the reinforcement.
[0070] In a specific embodiment, step S107 specifically includes the following steps: before the UHPC material is finally set, using a scraper to flatten and trim the surface of the area to be reinforced after spraying; after the UHPC material is finally set, regularly wetting the surface of the area to be reinforced after spraying within a preset curing period.
[0071] Specifically, before the final setting of the UHPC material, preferably when the UHPC material is initially set, the UHPC material sprayed on the surface of the area to be reinforced is scraped and trimmed with a scraper to improve the density and strength of the concrete and ensure the reinforcement effect and project quality. Two hours after the final setting of the UHPC material spraying, the UHPC material on the surface of the area to be reinforced is cured for 7-14 days. During this period, the UHPC material on the surface of the area to be reinforced needs to be kept moist to ensure that the spraying performance meets the requirements.
[0072] In summary, the tunnel lining reinforcement method based on sprayed UHPC provided in the embodiment of the present application uses UHPC material to reinforce the tunnel lining, configures UHPC material according to preset target material parameters and calculates the target spraying thickness of the sprayed UHPC material, successively performs interface treatment, cleaning and arranges high-strength steel wire mesh on the area to be reinforced, and then sprays UHPC material to the area to be reinforced until the target spraying thickness is reached, and finally performs trimming and maintenance to achieve the reinforcement of the tunnel lining, which can reduce the reinforcement thickness and increase the strength of the area to be reinforced, improve the strength of the tunnel lining after reinforcement, and improve the bearing capacity and durability of the tunnel structure.
[0073] It should be understood that in the present application, "at least one (item)" means one or more, and "plurality" means two or more. "And / or" is used to describe the association relationship of associated objects, indicating that three relationships may exist. For example, "A and / or B" can mean: only A exists, only B exists, and A and B exist at the same time, where A and B can be singular or plural. The character " / " generally indicates that the objects associated before and after are in an "or" relationship. "At least one of the following" or similar expressions refers to any combination of these items, including any combination of single or plural items. For example, at least one of a, b or c can mean: a, b, c, "a and b", "a and c", "b and c", or "a and b and c", where a, b, c can be single or multiple.
[0074] The preferred embodiments of the present invention are described above with reference to the accompanying drawings, but the scope of the rights of the present invention is not limited thereto. Any modification, equivalent substitution and improvement made by a person skilled in the art without departing from the scope and essence of the present invention should be within the scope of the rights of the present invention.
Claims
1. A tunnel lining reinforcement method based on sprayed UHPC, characterized in that: include: Configure UHPC materials according to preset target material parameters; Calculating a target spraying thickness for spraying the UHPC material; Performing interface treatment on the area to be reinforced of the tunnel lining to obtain the treated area to be reinforced; Cleaning the processed area to be reinforced to obtain a cleaned area to be reinforced; Arranging a high-strength steel wire mesh on the inner surface of the cleaned area to be reinforced; After arranging the high-strength steel wire mesh, spraying the UHPC material onto the cleaned area to be reinforced until the target spraying thickness is reached, thereby obtaining the area to be reinforced after spraying; Finishing and maintaining the surface of the area to be reinforced after the spraying to complete the reinforcement; The calculation formula of the target spray thickness is: , , in, is the compressive strain of the cracked tunnel, To strengthen the tensile strain of concrete, is the elastic modulus of the cracked tunnel, The elastic modulus of reinforced concrete; The area of cracked tunnel to be reinforced; To reinforce the concrete area, , L is the length of the area to be reinforced, is the thickness of the damaged tunnel, is the target spray thickness, is the external load; The UHPC material is composed of cement, mineral admixture, fine aggregate, water reducing agent, accelerating agent, steel fiber and water. The UHPC material is configured according to the preset target material parameters, including: According to the preset flow parameters, determining the amount of the water reducing agent, the mass ratio between the water and the accelerating setting agent, and the amount of the mineral admixture; Determining the dosage of the accelerating agent or the maximum particle size of the fine aggregate according to the preset rebound parameter; The amount of the steel fiber or the amount of the mineral admixture is determined according to the preset mechanical parameters; the amount of the steel fiber is not more than 3%, and the amount of the mineral admixture is not more than 35%.
2. The method for tunnel lining reinforcement based on sprayed UHPC according to claim 1, characterized in that: The UHPC material consists of 32% cement, 10% mineral admixture, 42% fine aggregate, 1% water reducer, 5% accelerating agent, 2% steel fiber and 8% water.
3. The method for tunnel lining reinforcement based on sprayed UHPC according to claim 1, characterized in that: The method of performing interface treatment on the area to be reinforced of the tunnel lining to obtain the treated area to be reinforced comprises: The interface roughness of the area to be reinforced of the tunnel lining is adjusted by roughening, grooving and / or sandblasting, and an interface adhesive is added to the area to be reinforced of the tunnel lining.
4. The method for tunnel lining reinforcement based on sprayed UHPC according to claim 1, characterized in that: The step of cleaning the processed area to be reinforced to obtain the cleaned area to be reinforced includes: The treated area to be reinforced is cleaned by a scraper and / or a high-pressure water gun.
5. The method for tunnel lining reinforcement based on sprayed UHPC according to claim 1, characterized in that: Before arranging the high-strength steel wire mesh, the UHPC material is sprayed onto the cleaned area to be reinforced to form a UHPC protective layer. The thickness of the high-strength steel wire mesh is 3 mm, the mesh size is 100 mm×100 mm, the laying spacing is 150 mm, and the thickness of the UHPC protective layer is not less than 20 mm.
6. The method for strengthening tunnel lining based on sprayed UHPC according to claim 1, characterized in that: After arranging the high-strength steel wire mesh, spraying the UHPC material onto the cleaned area to be reinforced until the target spraying thickness is reached, thereby obtaining the area to be reinforced after spraying, including: Arrange a wet shotcrete device; the wet shotcrete device includes a feeding system and a spraying system; storing the UHPC material into the feed system; The spraying system is controlled to absorb the UHPC material from the feeding system, and the UHPC material is sprayed onto the high-strength steel wire mesh and the cleaned area to be reinforced by wet spraying until the target spraying thickness is reached.
7. The method for strengthening tunnel lining based on sprayed UHPC according to claim 6, characterized in that: The injection system is connected to a first material delivery pipe and a second material delivery pipe, and the lumen of the first material delivery pipe is provided with a pipeline connector; The pipeline connector is provided with a discharge port and a feed port, the discharge port is communicated with the first feed pipe, the feed port is connected to the second feed pipe and is provided with a feed valve; the injection system transports the accelerator through the second feed pipe, is connected to the first feed pipe through the pipeline connector, and injects the UHPC material to the outside through the first feed pipe.
8. The method for strengthening tunnel lining based on sprayed UHPC according to claim 1, characterized in that: The surface of the area to be reinforced after spraying is repaired and maintained to complete the reinforcement, including: Before the UHPC material is finally set, the surface of the area to be reinforced after the spraying is scraped and trimmed with a scraper. After the UHPC material is finally set, the surface of the area to be reinforced after the spraying is regularly wetted within a preset curing period.
Citation Information
Patent Citations
Ultrahigh-toughness cement-based composite material used in ejection, and ejection process thereof
CN104150845A
Concrete bridge reinforcing design method based on force rib stress test result
CN106638332A
Reinforcement method of shield tunnel segment
CN107035385A
Construction method of tunnel lining structure by using steel fiber concrete
CN109209438A
Method of adopting concrete with super high performance to reinforce shield tunnel lining structure
CN111648787A