A method and device for distinguishing internal and external damage of steel pipe
The magnetic permeability disturbance of the steel pipe is detected through multiple sets of electromagnetic sensors of different sizes, and the peak size and signal difference are used to distinguish internal and external damage, which solves the problem of insufficient detection sensitivity in the existing technology and achieves accurate distinction and high performance of internal and external damage on the steel pipe. Accuracy detection.
Patent Information
- Application Number
- CN202410991045.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-23
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2044-07-23
AI Technical Summary
Existing methods for detecting internal and external damage to steel pipes cannot accurately distinguish internal and external damage, and the detection sensitivity is insufficient.
Multiple sets of electromagnetic sensors of different sizes are used to detect the magnetized steel pipe. Through the peak size of the detection results and signal disturbance conditions, it is determined whether there is internal or external damage to the steel pipe, and the signal differences of sensors of different sizes are used to distinguish.
It achieves the accurate distinction of internal and external damage on steel pipes, improves the accuracy of detection, overcomes the problems of single signal characteristics and misjudgment, and achieves fast detection speed and high accuracy.
Smart Images

Figure CN118549521B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of electromagnetic nondestructive testing, and in particular to a method and device for distinguishing internal and external damage of a steel pipe. Background Art
[0002] Steel pipes are widely used in various fields in daily production and life. During the production and use process, various defects may be formed on the inner and outer walls due to the influence of various tensile and compressive stresses, corrosion and other factors. The outer wall defects include concave defects, convex defects, mixed surface defects, etc., and the inner wall defects include pores, inclusions, shrinkage holes, cold shuts, etc., which may cause leakage or even explosion in severe cases. The hazards caused by inner and outer wall defects are different. For safety and economic considerations, it is necessary to detect and distinguish the internal and external injuries of steel pipes.
[0003] At present, the commonly used methods for detecting internal and external damage of steel pipes are ultrasonic detection and radioactive detection, but the detection sensitivity is not high enough. Therefore, how to accurately distinguish the internal and external damage of steel pipes has become a technical problem that needs to be solved urgently. Summary of the invention
[0004] In view of this, it is necessary to provide a method and device for distinguishing internal and external damage of a steel pipe, so as to solve the technical problem that the current method for detecting internal and external damage of a steel pipe cannot accurately distinguish the internal and external damage of a steel pipe.
[0005] In order to achieve the above object, the present invention provides a method for distinguishing internal and external damage of a steel pipe, comprising:
[0006] Acquire detection results of multiple groups of electromagnetic sensors of different sizes, wherein the detection results of the multiple groups of electromagnetic sensors of different sizes are obtained after the multiple groups of electromagnetic sensors of different sizes detect the magnetic permeability disturbance state of the magnetized steel pipe to be detected;
[0007] Based on the detection results of the multiple groups of electromagnetic sensors with different sizes, it is determined whether the steel pipe to be detected has internal damage or external damage.
[0008] Furthermore, the magnetized steel pipe to be inspected is obtained by magnetization based on the axial magnetization field generated by the magnetization coil.
[0009] Further, the determining whether the steel pipe to be inspected has internal damage or external damage based on the detection results of the multiple groups of electromagnetic sensors with different sizes includes:
[0010] Based on the peak values of the detection results of the multiple groups of electromagnetic sensors with different sizes, it is determined whether the steel pipe to be detected has internal damage or external damage.
[0011] Further, the determining whether the steel pipe to be detected has internal damage or external damage based on the peak values of the detection results of the multiple groups of electromagnetic sensors with different sizes includes:
[0012] When the peak value of the detection result of the electromagnetic sensor with a larger size is larger, it is determined that the steel pipe to be detected has internal damage;
[0013] In the case that the peak value of the detection result of the electromagnetic sensor with a larger size is smaller, it is determined that the steel pipe to be detected has external damage.
[0014] Further, the determining whether the steel pipe to be inspected has internal damage or external damage includes:
[0015] For the first electromagnetic sensor and the second electromagnetic sensor, the size of the first electromagnetic sensor smaller than the size of the second electromagnetic sensor , the first electromagnetic sensor and the second electromagnetic sensor are any two groups of electromagnetic sensors among the multiple groups of electromagnetic sensors with different sizes;
[0016] The peak value of the detection result of the first electromagnetic sensor is smaller than the peak value of the detection result of the second electromagnetic sensor In the case of, determining that the steel pipe to be tested has internal damage;
[0017] The peak value of the detection result of the first electromagnetic sensor is greater than the peak value of the detection result of the second electromagnetic sensor In this case, it is determined that the steel pipe to be inspected has external damage.
[0018] Further,
[0019] The method further comprises:
[0020] The detection results of the multiple groups of electromagnetic sensors with different sizes are preprocessed, and signal peak values corresponding to the detection results of the multiple groups of electromagnetic sensors with different sizes after the preprocessing are obtained.
[0021] Furthermore, the plurality of groups of electromagnetic sensors of different sizes detect the disturbance condition of the magnetic permeability of the magnetized steel pipe to be detected based on sinusoidal excitation.
[0022] Furthermore, the multiple groups of electromagnetic sensors with different sizes are at least two groups.
[0023] Furthermore, the preprocessing of the detection results of the multiple groups of electromagnetic sensors of different sizes includes:
[0024] The detection results of the multiple groups of electromagnetic sensors with different sizes are amplified and filtered.
[0025] The present invention also provides a device for distinguishing internal and external damage of a steel pipe, comprising:
[0026] An acquisition module, used to acquire detection results of multiple groups of electromagnetic sensors of different sizes, wherein the detection results of the multiple groups of electromagnetic sensors of different sizes are obtained after the multiple groups of electromagnetic sensors of different sizes detect the magnetic permeability disturbance state of the magnetized steel pipe to be detected;
[0027] The determination module is used to determine whether the steel pipe to be detected has internal damage or external damage based on the detection results of the multiple groups of electromagnetic sensors with different sizes.
[0028] Compared with the prior art, the beneficial effects of the present invention include: detecting the magnetic permeability disturbance condition of the magnetized steel pipe to be inspected by multiple groups of electromagnetic sensors of different sizes, and then determining whether the steel pipe to be inspected has internal or external injuries based on the detection results of the multiple groups of electromagnetic sensors of different sizes, thereby achieving accurate distinction between internal and external injuries of the steel pipe and improving the accuracy of distinguishing between internal and external injuries of the steel pipe. BRIEF DESCRIPTION OF THE DRAWINGS
[0029] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative work.
[0030] Figure 1 A schematic diagram of a flow chart of an embodiment of a method for distinguishing internal and external damage of a steel pipe provided by the present invention;
[0031] Figure 2 A schematic diagram of an embodiment of distinguishing internal and external damage of a steel pipe provided by the present invention;
[0032] Figure 3 A schematic diagram of a flow chart of an embodiment of a process for distinguishing internal and external damage of a steel pipe provided by the present invention;
[0033] Figure 4 An overall schematic diagram of an embodiment of the present invention for distinguishing internal and external damage of a steel pipe;
[0034] Figure 5 A schematic structural diagram of an embodiment of a device for distinguishing internal and external damage of a steel pipe provided by the present invention; DETAILED DESCRIPTION
[0035] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the accompanying drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative work are within the scope of protection of the present invention.
[0036] In the description of the present invention, the terms "first" and "second" are used for descriptive purposes only and cannot be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include at least one of the features. In addition, the meaning of "plurality" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined.
[0037] In the description of the present invention, reference to an "embodiment" means that a particular feature, structure, or characteristic described in conjunction with the embodiment may be included in at least one embodiment of the present invention. The appearance of the phrase in various places in the specification does not necessarily refer to the same embodiment, nor is it an independent or alternative embodiment that is mutually exclusive of other embodiments. It is explicitly and implicitly understood by those skilled in the art that the described embodiments may be combined with other embodiments.
[0038] Steel pipes are widely used in the fields of petroleum, natural gas, chemical industry, electricity, water conservancy, light industry, machinery manufacturing and construction in daily production and life. During the production and use process, various defects may be formed on the inner and outer walls due to the influence of various tensile and compressive stresses, corrosion and other factors. The outer wall defects include concave defects, convex defects, mixed surface defects, etc., and the inner wall defects include pores, inclusions, shrinkage holes, cold shuts, etc., which may cause leakage or even explosion in severe cases. The hazards caused by inner and outer wall defects are different. For safety and economic considerations, it is necessary to detect and distinguish the internal and external injuries of ferromagnetic pipes.
[0039] The specific embodiments are described in detail below:
[0040] The present invention provides a method for distinguishing internal and external damage of a steel pipe, combining Figure 1 Come and see, Figure 1 The schematic diagram of the flow chart of an embodiment of the method for distinguishing internal and external damage of a steel pipe provided by the present invention comprises steps S101 to S102, wherein:
[0041] In step S101, the detection results of multiple groups of electromagnetic sensors of different sizes are obtained, wherein the detection results of the multiple groups of electromagnetic sensors of different sizes are obtained after the multiple groups of electromagnetic sensors of different sizes detect the magnetic permeability disturbance state of the magnetized steel pipe to be detected;
[0042] In step S102, based on the detection results of the multiple groups of electromagnetic sensors of different sizes, it is determined whether the steel pipe to be detected has internal damage or external damage, thereby accurately distinguishing the internal and external damage of the steel pipe and improving the accuracy of distinguishing the internal and external damage of the steel pipe.
[0043] In an embodiment of the present invention, the magnetic permeability disturbance condition of the magnetized steel pipe to be inspected is detected by using multiple groups of electromagnetic sensors of different sizes, and then based on the detection results of the multiple groups of electromagnetic sensors of different sizes, it is determined whether the steel pipe to be inspected has internal or external damage, thereby achieving accurate distinction between internal and external damage of the steel pipe and improving the accuracy of distinguishing between internal and external damage of the steel pipe.
[0044] In a specific embodiment of the present invention, multiple groups of electromagnetic sensors of different sizes can be used to detect the magnetic permeability disturbance condition of the magnetized steel pipe to be inspected. The magnetic permeability of the steel pipe to be inspected will fluctuate at the defective part of the steel pipe, so that it can be determined whether the steel pipe to be inspected has internal or external damage based on the detection results of the multiple groups of electromagnetic sensors of different sizes.
[0045] As a preferred embodiment, the magnetized steel pipe to be inspected is obtained by magnetization based on the axial magnetization field generated by the magnetization coil.
[0046] In a specific embodiment of the present invention, a magnetizing coil may be used to generate an axial magnetizing field, and then the steel pipe to be inspected is placed in an effective magnetizing region of the axial magnetizing field to complete the magnetization of the steel pipe to be inspected.
[0047] As a preferred embodiment, the determining whether the steel pipe to be inspected has internal damage or external damage based on the detection results of the multiple groups of electromagnetic sensors of different sizes includes:
[0048] Based on the peak values of the detection results of the multiple groups of electromagnetic sensors with different sizes, it is determined whether the steel pipe to be detected has internal damage or external damage, and the internal and external damage distinction result of the steel pipe to be detected is obtained.
[0049] In a specific embodiment of the present invention, when determining whether the steel pipe to be inspected has internal or external damage based on the detection results of multiple groups of electromagnetic sensors of different sizes, it can be determined whether the steel pipe to be inspected has internal or external damage based on the peak values of the detection results of multiple groups of electromagnetic sensors of different sizes.
[0050] As a preferred embodiment, the determining whether the steel pipe to be detected has internal damage or external damage based on the peak values of the detection results of the multiple groups of electromagnetic sensors with different sizes includes:
[0051] When the peak value of the detection result of the electromagnetic sensor with a larger size is larger, it is determined that the steel pipe to be detected has internal damage;
[0052] In the case that the peak value of the detection result of the electromagnetic sensor with a larger size is smaller, it is determined that the steel pipe to be detected has external damage.
[0053] In a specific embodiment of the present invention, when determining whether the steel pipe to be inspected has internal or external damage based on the peak values of the detection results of multiple groups of electromagnetic sensors of different sizes, if the peak value of the detection result of the larger electromagnetic sensor has a larger size, it can be determined that the steel pipe to be inspected has internal damage; if the peak value of the detection result of the larger electromagnetic sensor has a smaller size, it can be determined that the steel pipe to be inspected has external damage.
[0054] As a preferred embodiment, the determining whether the steel pipe to be inspected has internal damage or external damage includes:
[0055] For the first electromagnetic sensor and the second electromagnetic sensor, the size of the first electromagnetic sensor smaller than the size of the second electromagnetic sensor , the first electromagnetic sensor and the second electromagnetic sensor are any two groups of electromagnetic sensors among the multiple groups of electromagnetic sensors with different sizes;
[0056] The peak value of the detection result of the first electromagnetic sensor is smaller than the peak value of the detection result of the second electromagnetic sensor In the case of, determining that the steel pipe to be tested has internal damage;
[0057] The peak value of the detection result of the first electromagnetic sensor is greater than the peak value of the detection result of the second electromagnetic sensor In this case, it is determined that the steel pipe to be inspected has external damage.
[0058] In a specific embodiment of the present invention, for any two groups of electromagnetic sensors, a first electromagnetic sensor and a second electromagnetic sensor, among the multiple groups of electromagnetic sensors with different sizes, the size of the first electromagnetic sensor Smaller than the size of the second electromagnetic sensor , the peak value of the detection result of the first electromagnetic sensor is , the peak value of the detection result of the second electromagnetic sensor is .
[0059] like , it is determined that the steel pipe to be tested has internal damage; if , it is determined that the steel pipe to be tested has external damage.
[0060] As a preferred embodiment,
[0061] The method further comprises:
[0062] The detection results of the multiple groups of electromagnetic sensors with different sizes are preprocessed, and signal peak values corresponding to the detection results of the multiple groups of electromagnetic sensors with different sizes after the preprocessing are obtained.
[0063] In a specific embodiment of the present invention, when obtaining the detection results of multiple groups of electromagnetic sensors of different sizes, the detection results of the electromagnetic sensors can be preprocessed (for example, amplification filtering and analog-to-digital conversion), and then the signal peak values corresponding to the detection results of the multiple groups of electromagnetic sensors of different sizes after the preprocessing are obtained for statistical observation.
[0064] As a preferred embodiment, the plurality of groups of electromagnetic sensors of different sizes detect the disturbance condition of the magnetic permeability of the magnetized steel pipe to be detected based on sinusoidal excitation.
[0065] In a specific embodiment of the present invention, when a plurality of groups of electromagnetic sensors of different sizes detect the magnetic permeability disturbance condition of the magnetized steel pipe to be detected, the magnetic permeability disturbance condition of the steel pipe to be detected can be detected by sinusoidal excitation.
[0066] As a preferred embodiment, the multiple groups of electromagnetic sensors with different sizes are at least two groups.
[0067] In a specific embodiment of the present invention, electromagnetic sensors of different sizes may be arranged into three groups.
[0068] As a preferred embodiment, the preprocessing of the detection results of the multiple groups of electromagnetic sensors with different sizes includes:
[0069] The detection results of the multiple groups of electromagnetic sensors with different sizes are amplified and filtered.
[0070] In a specific embodiment of the present invention, when preprocessing the detection results of multiple groups of electromagnetic sensors of different sizes, the detection results of the electromagnetic sensors may be firstly amplified and then subjected to signal filtering.
[0071] The following is a specific application scenario to better illustrate the technical solution of the present invention:
[0072] Combination Figure 2 Come and see, Figure 2 A schematic diagram of an embodiment of the steel pipe internal and external damage distinction provided by the present invention shows that after the steel pipe is magnetized, the internal and external damages have different effects on the density of the eddy current field generated by sensors of different outer diameters. As the outer diameter of the sensor increases, the disturbance of the eddy current caused by the magnetic permeability distortion caused by external defects gradually decreases, while the disturbance of the eddy current caused by the magnetic permeability distortion caused by internal defects gradually increases.
[0073] Combination Figure 3 Come and see, Figure 3A schematic diagram of a process for distinguishing internal and external damage of a steel pipe according to an embodiment of the present invention, combined with Figure 4 Come and see, Figure 4 This is an overall schematic diagram of an embodiment of the present invention for distinguishing internal and external damage of a steel pipe. The specific steps of the process of distinguishing internal and external damage of a steel pipe are as follows:
[0074] 1. A magnetizing coil is used to generate an axial magnetizing field, which acts on the steel pipe 1 to be tested in the effective magnetizing area and magnetizes it. The internal defects 4 of the steel pipe generate magnetic permeability disturbance 5, and the external defects 6 generate magnetic permeability disturbance 7.
[0075] 2. The center line of the detection probe 2 is arranged on the surface of the steel pipe along the radial direction of the steel pipe. The detection probe includes three sets of sensors 8, 9, 10 of different sizes, and the size of the outer diameter is The three sets of sensors scan along the magnetized steel pipe and output three sets of defect signals after scanning the defects.
[0076] The magnetizing coil 11 magnetizes the steel pipe 1 to be inspected, and the AC excitation source 15 provides an adjustable sinusoidal excitation to be applied to the detection probe 2. The detection probe 2 is located between the yoke coil and the outer wall of the steel pipe for scanning and inspection. When the steel pipe is located below the detection probe, the signal obtained by the detection probe passes through the amplification and filtering module 12, passes through the A / D acquisition module 13, and is transmitted to the oscilloscope 14.
[0077] Extract the peak-to-peak values of the three groups of signals displayed by the oscilloscope 14, and let the peak value of the signal received by the sensor 8 be , the peak value of the signal received by sensor 9 is , the peak value of the signal received by sensor 10 is .
[0078] If the peak values of the three defect signals , then the steel pipe has internal damage; if the peak values of the three groups of defect signals , then there is external damage to the steel pipe.
[0079] The embodiment of the present invention also provides a device for distinguishing internal and external damage of a steel pipe, Figure 5 Come and see, Figure 5 The schematic diagram of the structure of an embodiment of the device for distinguishing internal and external damage of a steel pipe provided by the present invention is as follows. The device 500 for distinguishing internal and external damage of a steel pipe comprises:
[0080] The detection module 501 is used to obtain the detection results of multiple groups of electromagnetic sensors of different sizes, wherein the detection results of the multiple groups of electromagnetic sensors of different sizes are obtained after the multiple groups of electromagnetic sensors of different sizes detect the magnetic permeability disturbance state of the magnetized steel pipe to be detected;
[0081] The determination module 502 is used to determine whether the steel pipe to be inspected has internal damage or external damage based on the detection results of the multiple groups of electromagnetic sensors with different sizes.
[0082] The more specific implementation methods of each module of the device for distinguishing internal and external damage of a steel pipe can be found in the description of the above-mentioned method for distinguishing internal and external damage of a steel pipe, and have similar beneficial effects, which will not be repeated here.
[0083] The present invention discloses a method and device for distinguishing internal and external injuries of a steel pipe. The method detects the magnetic permeability disturbance condition of a magnetized steel pipe to be detected by using multiple groups of electromagnetic sensors of different sizes. Then, based on the detection results of the multiple groups of electromagnetic sensors of different sizes, it is determined whether the steel pipe to be detected has internal injuries or external injuries, thereby achieving accurate distinction between internal and external injuries of the steel pipe and improving the accuracy of distinguishing between internal and external injuries of the steel pipe.
[0084] The technical solution of the present invention uses multiple groups of sensors of different sizes to receive defect signals, and distinguishes internal and external defects by the difference in the disturbance strength of the eddy current field generated by sensors of different sizes due to internal and external defects. This makes up for the shortcomings of the current electromagnetic nondestructive testing technology that cannot directly distinguish internal and external injuries accurately, and misses the detection of tiny internal defects of thicker ferromagnetic materials. The present invention has a simple structure, the sensor is easy to manufacture, and can be used in a portable manner. It overcomes the shortcomings of misjudgment caused by signal characteristics and single signal amplitude in the past, and has a fast detection speed and high accuracy.
[0085] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any changes or substitutions that can be easily conceived by any technician familiar with the technical field within the technical scope disclosed by the present invention should be covered within the protection scope of the present invention.
Claims
1. A method for distinguishing internal and external damage of a steel pipe. It is characterized in that include: Acquire detection results of multiple groups of electromagnetic sensors of different sizes, wherein the detection results of the multiple groups of electromagnetic sensors of different sizes are obtained after the multiple groups of electromagnetic sensors of different sizes detect the magnetic permeability disturbance conditions of the magnetized steel pipe to be detected; Based on the detection results of the multiple groups of electromagnetic sensors with different sizes, determining whether the steel pipe to be detected has internal damage or external damage; The determining whether the steel pipe to be inspected has internal damage or external damage based on the detection results of the multiple groups of electromagnetic sensors with different sizes includes: Based on the peak values of the detection results of the multiple groups of electromagnetic sensors with different sizes, determining whether the steel pipe to be detected has internal damage or external damage; The determining whether the steel pipe to be detected has internal damage or external damage based on the peak values of the detection results of the multiple groups of electromagnetic sensors with different sizes includes: When the peak value of the detection result of the electromagnetic sensor with a larger size is larger, it is determined that the steel pipe to be detected has internal damage; In the case where the peak value of the detection result of the electromagnetic sensor with a larger size is smaller, it is determined that the steel pipe to be detected has external damage; The magnetized steel pipe to be tested is obtained by magnetizing the axial magnetization field generated by the magnetizing coil; The electromagnetic sensor is an electromagnetic sensor comprising an excitation coil and capable of generating an eddy current field; The multiple groups of electromagnetic sensors with different sizes refer to multiple groups of electromagnetic sensors with different outer diameters of excitation coils; In the case where the peak value of the detection result of the electromagnetic sensor with a larger size is larger, it is determined that the steel pipe to be detected has internal damage, including: When the peak value of the detection result of the electromagnetic sensor with a larger outer diameter of the excitation coil is larger, it is determined that the steel pipe to be detected has internal damage; In the case that the peak value of the detection result of the electromagnetic sensor with a larger size is smaller, determining that the steel pipe to be detected has external damage includes: In the case that the peak value of the detection result of the electromagnetic sensor with a larger outer diameter of the excitation coil is smaller, it is determined that the steel pipe to be detected has external damage.
2. The method for distinguishing internal and external damage of a steel pipe according to claim 1, It is characterized in that The determining whether the steel pipe to be inspected has internal damage or external damage includes: For the first electromagnetic sensor and the second electromagnetic sensor, the size of the first electromagnetic sensor smaller than the size of the second electromagnetic sensor , the first electromagnetic sensor and the second electromagnetic sensor are any two groups of electromagnetic sensors among the multiple groups of electromagnetic sensors with different sizes; The peak value of the detection result of the first electromagnetic sensor is smaller than the peak value of the detection result of the second electromagnetic sensor In the case of, determining that the steel pipe to be tested has internal damage; The peak value of the detection result of the first electromagnetic sensor is greater than the peak value of the detection result of the second electromagnetic sensor In this case, it is determined that the steel pipe to be inspected has external damage.
3. The method for distinguishing internal and external damage of a steel pipe according to claim 1 or 2, It is characterized in that The method further comprises: The detection results of the multiple groups of electromagnetic sensors with different sizes are preprocessed, and signal peak values corresponding to the detection results of the multiple groups of electromagnetic sensors with different sizes after the preprocessing are obtained.
4. The method for distinguishing internal and external damage of a steel pipe according to claim 1 or 2, It is characterized in that The plurality of groups of electromagnetic sensors of different sizes detect the disturbance condition of the magnetic permeability of the magnetized steel pipe to be detected based on sinusoidal excitation.
5. The method for distinguishing internal and external damage of a steel pipe according to claim 1 or 2, It is characterized in that The plurality of groups of electromagnetic sensors with different sizes are at least two groups.
6. The method for distinguishing internal and external damage of a steel pipe according to claim 3, It is characterized in that The preprocessing of the detection results of the multiple groups of electromagnetic sensors with different sizes includes: The detection results of the multiple groups of electromagnetic sensors with different sizes are amplified and filtered.
7. A device for distinguishing internal and external damage of steel pipes, It is characterized in that include: An acquisition module, used to acquire detection results of multiple groups of electromagnetic sensors of different sizes, wherein the detection results of the multiple groups of electromagnetic sensors of different sizes are obtained after the multiple groups of electromagnetic sensors of different sizes detect the magnetic permeability disturbance state of the magnetized steel pipe to be detected; A determination module, used to determine whether the steel pipe to be detected has internal damage or external damage based on the detection results of the multiple groups of electromagnetic sensors with different sizes; The determining whether the steel pipe to be inspected has internal damage or external damage based on the detection results of the multiple groups of electromagnetic sensors with different sizes includes: Based on the peak values of the detection results of the multiple groups of electromagnetic sensors with different sizes, determining whether the steel pipe to be detected has internal damage or external damage; The determining whether the steel pipe to be detected has internal damage or external damage based on the peak values of the detection results of the multiple groups of electromagnetic sensors with different sizes includes: When the peak value of the detection result of the electromagnetic sensor with a larger size is larger, it is determined that the steel pipe to be detected has internal damage; In the case where the peak value of the detection result of the electromagnetic sensor with a larger size is smaller, it is determined that the steel pipe to be detected has external damage; The magnetized steel pipe to be tested is obtained by magnetizing the axial magnetization field generated by the magnetizing coil; The electromagnetic sensor is an electromagnetic sensor comprising an excitation coil and capable of generating an eddy current field; The multiple groups of electromagnetic sensors with different sizes refer to multiple groups of electromagnetic sensors with different outer diameters of excitation coils; In the case where the peak value of the detection result of the electromagnetic sensor with a larger size is larger, it is determined that the steel pipe to be detected has internal damage, including: When the peak value of the detection result of the electromagnetic sensor with a larger outer diameter of the excitation coil is larger, it is determined that the steel pipe to be detected has internal damage; In the case that the peak value of the detection result of the electromagnetic sensor with a larger size is smaller, determining that the steel pipe to be detected has external damage includes: In the case that the peak value of the detection result of the electromagnetic sensor with a larger outer diameter of the excitation coil is smaller, it is determined that the steel pipe to be detected has external damage.
Citation Information
Patent Citations
Eddy current testing recognition and evaluation method for defects of inner wall and outer wall of steel pipe under direct current magnetization
CN102759567A
Eddy current inspection device based on resistance transducer of gigantic magnetism
CN1959402A
Magnetic powder flaw detection device
JP1988250558A
Mutual induction type through test coil and eddy current flaw detector
JP1998062392A
Eddy-current flaw detection apparatus
JP2004028897A