A method, device and system for intelligent packaging of lithium batteries
By analyzing the cross-sectional grayscale image of the lithium battery cell, determining the degree of diaphragm wrinkles and over-compression, and adjusting the pressure of the booster cylinder, the problem of poor hot-pressing shaping effect of the lithium battery is solved, and the packaging quality and life of the lithium battery are improved.
Patent Information
- Application Number
- CN202411001677.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-25
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2044-07-25
AI Technical Summary
During the hot-pressing shaping process of lithium batteries, if the hot-pressing shaping effect of the battery core is not good, it will cause the separator to wrinkle or be over-compressed, affecting the transmission of lithium ions and the service life of the lithium battery.
By analyzing the cross-sectional grayscale image of the lithium battery cell, the degree of wrinkles and over-compression of the diaphragm is determined, the hot pressing shaping effect coefficient is calculated, and the pressure of the booster cylinder is adjusted to achieve intelligent packaging.
It improves the evaluation accuracy of the hot-pressing shaping effect of the cell separator, ensures the optimal booster cylinder pressure, and improves the packaging quality and service life of soft-pack lithium batteries.
Smart Images

Figure CN118572202B_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of lithium battery technology, and specifically to an intelligent packaging method, device and system for lithium batteries. Background Art
[0002] Compared with traditional metal shell lithium batteries, soft-pack lithium batteries have the advantages of light weight, low internal resistance, high energy density and high charge and discharge rate. In addition, when a soft-pack lithium battery fails inside the battery, the packaging on the battery surface will only bulge and rupture at most, rather than explode like metal shell lithium batteries. Soft-pack lithium batteries have been widely used in electric vehicles, mobile devices and other fields.
[0003] The production of soft-pack lithium batteries includes multiple packaging steps, which are mainly divided into top sealing, pre-sealing and secondary sealing. In the top sealing step, the battery cell that has been subjected to hot pressing and shaping treatment needs to be placed in the aluminum-plastic film, and the tabs on the upper end of the battery cell need to be heat-sealed with the aluminum-plastic film. If the hot pressing and shaping treatment of the battery cell is not effective, the internal resistance of the lithium battery will be increased, and the transmission of lithium ions in the lithium battery will be affected, thereby reducing the service life of the lithium battery. Summary of the invention
[0004] In order to solve the above technical problems, a smart packaging method, device and system for lithium batteries are provided to solve the existing problems.
[0005] The solution to the technical problem of the present application is to provide a smart packaging method, device and system for lithium batteries, comprising the following steps:
[0006] In a first aspect, an embodiment of the present application provides a smart packaging method for a lithium battery, the method comprising the following steps:
[0007] Obtain a grayscale image of the cross section of a lithium battery cell;
[0008] Determine the degree of wrinkling of the separator in the lithium battery cell according to the distance difference and distribution of the pixels in the grayscale image of the cross section of the lithium battery cell;
[0009] Determine the degree of over-compression of the separator in the lithium battery cell according to the change of the gray value of the pixel points in the gray image of the cross-section of the lithium battery cell and the change of the number of the pixel points;
[0010] Based on the degree of diaphragm wrinkling and the degree of over-compression of the diaphragm, the thermal pressing shaping effect coefficient of the battery cell in the lithium battery is obtained, the optimal boost cylinder pressure is determined, and the soft-pack lithium battery is intelligently packaged.
[0011] Preferably, the step of determining the degree of wrinkling of the separator of the battery cell in the lithium battery comprises:
[0012] Binarization is performed on the grayscale image of the cross section of the battery cell to obtain a binary image of the battery cell to obtain the pixel points of the separator;
[0013] The skeleton line extraction algorithm is used to obtain the skeleton line of the battery cell diaphragm of the battery cell binary image;
[0014] Perform curve fitting on the core diaphragm skeleton line to obtain the peak points and valley points of the fitting curve, which are recorded as the peak and valley pixel points of the core diaphragm skeleton line;
[0015] Determine the degree of convexity and concavity of the separator in the lithium battery according to the distribution and number of peak and valley pixels in the skeleton line of the separator;
[0016] Determine the dispersion of the diaphragm thickness of the battery cell in the lithium battery according to the distance difference and dispersion degree between the diaphragm pixels;
[0017] The degree of diaphragm wrinkles of the battery cell in the lithium battery is determined by forward fusion of the diaphragm concave-convex degree and the diaphragm thickness dispersion.
[0018] Preferably, the step of determining the degree of convexity and concavity of the separator of the battery cell in the lithium battery comprises:
[0019] Calculate the mean of the ordinates of all pixels in the cell separator skeleton line, and record it as the central average value of the cell separator skeleton line;
[0020] The difference between the ordinate of each peak-valley pixel point of the cell diaphragm skeleton line and the central average value is recorded as the diaphragm skeleton line bending coefficient of each peak-valley pixel point of the cell diaphragm skeleton line;
[0021] The number of peak and valley pixel points of the battery cell diaphragm skeleton line is recorded as the peak and valley number;
[0022] The number of peaks and valleys and the bending coefficient of the membrane skeleton line are forwardly integrated to determine the degree of convexity and concavity of the membrane of the battery cell in the lithium battery.
[0023] Preferably, the step of determining the dispersion of the diaphragm thickness of the battery cell in the lithium battery comprises:
[0024] The vertical coordinate difference between any two diaphragm pixels in each column of pixel points in the battery cell binary image is recorded as the diaphragm difference;
[0025] The maximum value of all the diaphragm differences is used as the diaphragm thickness of the corresponding column in the battery cell binary image. If there is no diaphragm pixel in each column of pixels, the diaphragm thickness is assigned a value of 0;
[0026] The discrete degree of the diaphragm thickness of all columns with diaphragm pixels is determined as the discrete degree of the diaphragm thickness of the battery cell in the lithium battery.
[0027] Preferably, the step of determining the degree of over-compression of the diaphragm of the battery cell in the lithium battery comprises:
[0028] Counting all the pixels in each column whose grayscale values are not all zero in the binary image of the battery cell, and obtaining a grayscale value sequence of the pixels in each column whose grayscale values are not all zero;
[0029] Segmenting the grayscale value sequence of each column based on the membrane pixel points to obtain multiple membrane layers of each column;
[0030] All gray value sequences with the same number of diaphragm layers are combined into sets of equal-layer diaphragm sequences;
[0031] The set with the largest number of grayscale value sequences among all equal-layer diaphragm sequence sets is recorded as the maximum equal-layer diaphragm sequence set;
[0032] Determine the over-compression transparency coefficient of the separator of the battery cell in the lithium battery according to the difference in gray values between the pixels in each separator layer of each gray value sequence in the maximum equal-layer separator sequence set in the battery cell cross-sectional gray image;
[0033] Determine the over-compression factor of the separator of the battery cell in the lithium battery according to the difference in the number of pixels in each separator layer of each gray value sequence in the maximum equal-layer separator sequence set;
[0034] The membrane over-compression factor and the membrane over-compression transparency coefficient are forwardly integrated to determine the membrane over-compression degree of the battery cell in the lithium battery.
[0035] Preferably, the over-compression transparency coefficient of the diaphragm of the battery cell in the lithium battery includes:
[0036] The average of the grayscale values of the pixels corresponding to the pixels in the grayscale image of the cross-section of the battery cell in each diaphragm layer of each grayscale value sequence in the maximum equal-layer diaphragm sequence set is used as the diaphragm color feature value of each diaphragm layer of each grayscale value sequence in the maximum equal-layer diaphragm sequence set;
[0037] Arrange the diaphragm color feature values of each diaphragm layer of all gray value sequences in ascending order of the column number to form a diaphragm color change sequence of each diaphragm layer of the battery cell in the lithium battery;
[0038] Determine the color difference coefficient of the separator layer of the battery cell in the lithium battery according to the difference between the separator color change sequences of all arbitrary two separator layers;
[0039] The mean of all elements in the membrane color change sequence of all membrane layers is recorded as the first mean;
[0040] The ratio of the color difference coefficient of the diaphragm layer to the first average value is used as the over-compression transparency coefficient of the diaphragm of the battery cell in the lithium battery.
[0041] Preferably, the step of determining the over-compression factor of the diaphragm of the battery cell in the lithium battery comprises:
[0042] The number of pixels in each diaphragm layer of each gray value sequence in the maximum equal-layer diaphragm sequence set is used as the diaphragm layer thickness of each diaphragm layer of each gray value sequence;
[0043] Arrange the thickness of each diaphragm layer in all gray value sequences in ascending order of the column number to form a diaphragm thickness variation sequence of each diaphragm layer in the battery cell of the lithium battery;
[0044] The difference between the thickness variation sequences of any two diaphragm layers is used to determine the thickness variation coefficient of the diaphragm layer of the battery cell in the lithium battery;
[0045] The mean of all elements in the diaphragm color thickness sequence of all diaphragm layers is recorded as the second mean;
[0046] The ratio of the diaphragm layer thickness difference coefficient to the second mean value is used as the diaphragm over-compression factor of the battery cell in the lithium battery.
[0047] Preferably, the step of obtaining the thermal compression shaping effect coefficient of the battery cell in the lithium battery and determining the optimal boost cylinder pressure includes:
[0048] The degree of diaphragm wrinkling and the degree of diaphragm over-compression are positively integrated to determine the degree of diaphragm deformation of the battery cell in the lithium battery;
[0049] The thermal compression shaping effect coefficient of the battery cell in the lithium battery is negatively correlated with the degree of deformation of the diaphragm;
[0050] Obtain the minimum boost cylinder pressure and the maximum boost cylinder pressure of all battery cells during the hot pressing shaping process, and obtain the hot pressing shaping effect coefficient and the boost cylinder pressure of each battery cell;
[0051] Perform curve fitting on the boost cylinder pressure and thermal pressure shaping effect coefficient of each battery cell;
[0052] The boost cylinder pressure corresponding to the maximum thermal pressure shaping effect coefficient of the boost cylinder pressure of the battery cell in the fitting curve within the range of the minimum boost cylinder pressure and the maximum boost cylinder pressure is taken as the optimal boost cylinder pressure.
[0053] In a second aspect, an embodiment of the present application further provides an intelligent packaging device for lithium batteries, comprising a memory, a processor, and a computer program stored in the memory and running on the processor, wherein when the processor executes the computer program, the steps of any one of the above-mentioned intelligent packaging methods for lithium batteries are implemented.
[0054] In a third aspect, the present application also provides an intelligent packaging system for lithium batteries, including:
[0055] The battery cell data acquisition module obtains the grayscale image of the cross section of the lithium battery cell;
[0056] The hot pressing shaping analysis module determines the degree of diaphragm wrinkling of the battery cell in the lithium battery according to the distance difference and distribution between the pixels in the grayscale image of the cross-section of the battery cell of the lithium battery; determines the degree of over-compression of the diaphragm in the battery cell of the lithium battery according to the change of the grayscale value of the pixels and the change of the number of pixels in the grayscale image of the cross-section of the battery cell of the lithium battery; obtains the hot pressing shaping effect coefficient of the battery cell in the lithium battery based on the degree of diaphragm wrinkling and the degree of over-compression of the diaphragm;
[0057] The boost cylinder pressure acquisition module determines the optimal boost cylinder pressure based on the thermal compression shaping effect coefficient of the battery cells in the lithium battery, adjusts the boost cylinder pressure during the subsequent thermal compression shaping process of the battery cells, and intelligently packages the soft-pack lithium battery.
[0058] This application has at least the following beneficial effects:
[0059] The present application obtains the degree of diaphragm concavity and the dispersion of diaphragm thickness by analyzing the distance between pixels and the distribution of pixels in the grayscale image of the cross-section of the battery cell of the lithium battery, and determines the degree of diaphragm wrinkling of the battery cell in the lithium battery. The beneficial effect lies in that the degree of unevenness of the diaphragm inside the battery cell and the uniformity of the thickness of the battery cell diaphragm in each vertical direction are taken into account; according to the change of the grayscale value of the pixels and the change of the number of pixels in the grayscale image of the cross-section of the battery cell of the lithium battery, the diaphragm over-compression factor and the diaphragm over-compression transparency coefficient are obtained to determine the degree of diaphragm over-compression of the battery cell in the lithium battery. The beneficial effect lies in that the battery cell is analyzed. The color change and thickness change of the diaphragm inside the core along the horizontal direction improve the accuracy of evaluating the degree of over-compression of the diaphragm inside the battery cell that has been hot-pressed and shaped; based on the degree of diaphragm wrinkling and the degree of over-compression of the diaphragm, the hot-pressing and shaping effect coefficient of the battery cell in the lithium battery is obtained, the optimal boost cylinder pressure is determined, and the soft-pack lithium battery is intelligently packaged. The beneficial effect is that the accuracy of hot-pressing and shaping treatment effect evaluation of the battery cell that has been hot-pressed and shaped is improved, which is conducive to adjusting the accuracy of the optimal boost cylinder pressure in the hot-pressing and shaping process of the subsequent battery cell, thereby improving the packaging quality of the soft-pack lithium battery. BRIEF DESCRIPTION OF THE DRAWINGS
[0060] The following is a further detailed description of an intelligent packaging method for lithium batteries of the present application in conjunction with the accompanying drawings.
[0061] Figure 1 A flowchart of a smart packaging method for lithium batteries provided in this application;
[0062] Figure 2A flowchart of the steps of the method for obtaining the degree of convexity and concavity of the diaphragm of the battery cell in the lithium battery provided in the present application;
[0063] Figure 3 A flowchart of the steps of the method for obtaining the over-compression transparency coefficient of the diaphragm of the battery cell in the lithium battery provided in the present application;
[0064] Figure 4 A flowchart of the steps of an intelligent packaging system for lithium batteries provided in this application. DETAILED DESCRIPTION
[0065] In order to make the purpose, technical solution and advantages of the present application more clearly understood, the following is a further detailed description of a smart packaging method, device and system for lithium batteries proposed in the present application in combination with the accompanying drawings and implementation examples. It should be understood that the specific embodiments described herein are only used to explain the present application and are not used to limit the present application.
[0066] Unless defined otherwise, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art to which this application belongs.
[0067] See also Figure 1 , which shows a flowchart of a smart packaging method for lithium batteries provided by an embodiment of the present application, the method comprising the following steps:
[0068] Step 1: obtain a grayscale image of the cross-section of a lithium battery cell.
[0069] Place the wound soft-pack lithium battery cell on the template of the cell hot-pressing shaping machine, set the booster cylinder pressure and template temperature of the cell hot-pressing shaping machine, use the cell hot-pressing shaping machine to perform hot-pressing shaping on the soft-pack lithium battery cell, and use industrial CT scanning equipment to collect the cross-sectional CT scanning image of the cell after hot-pressing shaping, wherein the target cell is placed horizontally during image collection. De-noise the obtained cross-sectional CT scanning image to eliminate the influence of environmental noise during image collection, and grayscale the denoised image to obtain a cross-sectional grayscale image of the soft-pack lithium battery cell.
[0070] Preferably, as an embodiment of the present application, a Gaussian filtering denoising method is used for noise reduction processing, wherein Gaussian filtering is a well-known technology and will not be described in detail here.
[0071] At this point, a grayscale image of the cross-section of the lithium battery cell is obtained.
[0072] Step 2: Determine the degree of wrinkling of the separator of the battery cell in the lithium battery according to the distance difference and distribution between the pixels in the grayscale image of the cross-section of the battery cell of the lithium battery.
[0073] During the hot pressing and shaping process of the soft-pack lithium battery cell, if the boost cylinder pressure is too low, the diaphragm wrinkles inside the cell will not be eliminated. If the boost cylinder pressure is too high, the diaphragm inside the cell will be over-compressed, causing the diaphragm thickness to change too much and become transparent. This will cause the micropores in the diaphragm inside the cell to be blocked, thereby affecting the transmission of lithium ions in the lithium battery.
[0074] Since the battery cell is usually wound with positive electrode, negative electrode and separator in the arrangement of positive electrode-separator-negative electrode-separator, the positive electrode, negative electrode and separator appear layer by layer inside the battery cell. The material of the positive electrode is usually lithium cobalt oxide or lithium iron phosphate, and the material of the negative electrode is usually graphite or silicon, so that the positive and negative electrode are usually dark gray or black, while the material of the separator is usually polypropylene or polyethylene, usually white or milky white. There is a large color difference between the positive electrode, negative electrode and separator inside the battery cell of the soft-pack lithium battery. Based on the above analysis, the foreground and background images in the grayscale image of the cross-section of the lithium battery cell are segmented.
[0075] Binarization is performed on the grayscale image of the cross section of the battery cell to obtain a binary image of the battery cell;
[0076] The pixel points with gray value of 1 in the binary image of the battery cell are recorded as the diaphragm pixel points;
[0077] Furthermore, since the battery cell is placed horizontally when the cross-sectional image of the soft-pack lithium battery is collected, if wrinkles appear inside the battery cell, the overall thickness of the diaphragm inside the battery cell of the soft-pack lithium battery will appear uneven when changing along the horizontal direction, and the consistency of the overall thickness of the diaphragm inside the battery cell is also poor.
[0078] The skeleton line extraction algorithm is used to obtain the skeleton line of the battery cell diaphragm in the battery cell binary image;
[0079] It should be noted that the skeleton line of the cell diaphragm can reflect the bending of the diaphragm inside the cell when the diaphragm changes along the horizontal direction, wherein the skeleton line extraction algorithm is a well-known technology, and the specific process will not be repeated.
[0080] A coordinate system is constructed for each pixel point in the skeleton line of the battery cell diaphragm, and a curve fitting is performed according to the coordinate position of each pixel point to obtain the peak points and trough points of the fitting curve, which are recorded as the peak and trough pixel points of the skeleton line of the battery cell diaphragm;
[0081] Preferably, as an embodiment of the present application, the least squares method is used for curve fitting; secondly, the derivative method is used to obtain the peak points and the trough points. As other implementation methods, the implementer can also use the maximum likelihood estimation method for curve fitting, and this embodiment does not impose any special restrictions on this.
[0082] Calculate the mean of the ordinates of all pixels in the cell separator skeleton line, and record it as the central average value of the cell separator skeleton line;
[0083] The difference between the ordinate of each peak-valley pixel point of the cell diaphragm skeleton line and the central average value is recorded as the diaphragm skeleton line bending coefficient of each peak-valley pixel point of the cell diaphragm skeleton line;
[0084] Preferably, as an embodiment of the present application, the diaphragm skeleton line bending coefficient is the difference between the ordinate of each peak and valley pixel point of the battery cell diaphragm skeleton line and the central average value.
[0085] It should be noted that the diaphragm skeleton line bending coefficient is used to characterize the degree of bending of the battery cell diaphragm skeleton line at the peak and valley pixel points; the greater the degree of bending of the battery cell diaphragm skeleton line at the peak and valley pixel points, the greater the diaphragm skeleton line bending coefficient.
[0086] The number of peak and valley pixel points of the battery cell diaphragm skeleton line is recorded as the peak and valley number;
[0087] The number of peaks and valleys and the bending coefficient of the diaphragm skeleton line are forwardly integrated to determine the degree of convexity and concavity of the diaphragm of the battery cell in the lithium battery;
[0088] It is understandable that forward fusion can represent a multiplication relationship, an addition relationship, and the idempotence of an exponential function, and this application does not impose any special restrictions on this.
[0089] Preferably, as an embodiment of the present application, the mean value of the bending coefficient of the diaphragm skeleton line of all peak and valley pixel points of the battery cell diaphragm skeleton line is recorded as a first mean value, and the product of the first mean value and the number of peaks and valleys is used as the degree of diaphragm concavity of the battery cell in the lithium battery.
[0090] It should be noted that the more bending locations there are in the skeleton line of the battery cell diaphragm, the greater the number of peaks and valleys, and the greater the degree of bending at the bending locations in the skeleton line of the battery cell, the larger the first mean value, and the more likely the overall thickness of the diaphragm inside the battery cell will be uneven when changing along the horizontal direction, and the more severe the unevenness is, the greater the degree of unevenness of the diaphragm.
[0091] Further, the step flow chart of the method for obtaining the degree of convexity and concavity of the diaphragm of the battery cell in the lithium battery provided in the present application is as follows: Figure 2 shown.
[0092] The vertical coordinate difference between any two diaphragm pixels in each column of pixel points in the battery cell binary image is recorded as the diaphragm difference;
[0093] The maximum value of all the diaphragm differences is used as the diaphragm thickness of the corresponding column in the battery cell binary image. If there is no diaphragm pixel in each column of pixels, the diaphragm thickness is assigned a value of 0;
[0094] The discrete degree of the diaphragm thickness of all columns with diaphragm pixels is determined as the discrete degree of the diaphragm thickness of the battery cell in the lithium battery;
[0095] Preferably, as an embodiment of the present application, the diaphragm difference is the difference in the vertical coordinates between any two diaphragm pixels in each column of pixels in the battery cell binary image; secondly, the standard deviation of all diaphragm thicknesses with diaphragm pixels is used as the discreteness of the diaphragm thickness of the battery cell in the lithium battery.
[0096] It can be understood that the degree of dispersion in this embodiment can be measured by the standard deviation. As other implementation methods, the degree of dispersion can also be measured by the coefficient of variation, variance and information entropy. The embodiment of the present application does not impose any special restrictions on this.
[0097] It should be noted that the smaller the difference between the thickness of the diaphragm inside the battery cell in each vertical direction, the better the consistency of the overall thickness of the diaphragm inside the battery cell, and the smaller the discreteness of the diaphragm thickness of the battery cell in the lithium battery.
[0098] The degree of diaphragm wrinkles of the battery cell in the lithium battery is determined by forward fusion of the diaphragm concave-convex degree and the diaphragm thickness dispersion.
[0099] Preferably, as an embodiment of the present application, the product of the diaphragm concave-convex degree and the diaphragm thickness dispersion is used as the diaphragm wrinkle degree of the battery cell in the lithium battery.
[0100] It should be noted that the degree of diaphragm wrinkling can characterize the severity of the wrinkling phenomenon of the diaphragm inside the battery cell. The greater the degree of diaphragm concavity and the greater the dispersion of diaphragm thickness, the more severe the wrinkling phenomenon of the diaphragm inside the battery cell and the greater the degree of diaphragm wrinkling.
[0101] At this point, the degree of wrinkling of the separator in the lithium battery cell is obtained.
[0102] Step 3, determining the degree of over-compression of the separator in the lithium battery cell according to the change of the gray value of the pixel points in the gray image of the cross-section of the lithium battery cell and the change of the number of the pixel points.
[0103] If the diaphragm inside the battery cell is over-compressed during the hot pressing process, some layers of the diaphragm inside the battery cell will become thinner and transparent due to over-compression. The thickness changes of the diaphragms in different layers inside the battery cell along the horizontal direction will be greatly different, and the color changes of the diaphragms in different layers along the horizontal direction will be greatly different. Based on this analysis process, the degree of diaphragm over-compression is constructed. The specific method is:
[0104] Counting all the pixels in each column whose grayscale values are not all zero in the binary image of the battery cell, and obtaining a grayscale value sequence of the pixels in each column whose grayscale values are not all zero;
[0105] Segment the grayscale value sequence of each column based on the diaphragm pixel points to obtain multiple subsequences of each column, wherein each subsequence corresponds to a diaphragm layer in the battery cell, and obtain multiple diaphragm layers of each column;
[0106] Preferably, as an embodiment of the present application, the gray value sequence is segmented into multiple subsequences using the Bernaola Galvan segmentation algorithm; wherein the Bernaola Galvan segmentation algorithm is a well-known technology, and the specific process is not repeated here.
[0107] It is understandable that the embodiment of the present application adopts the Bernaola Galvan segmentation algorithm to obtain each subsequence. As other implementation methods, the implementer can adopt other methods in the prior art, for example, using a mutation point detection method to divide the sequence, and this embodiment does not impose any special restrictions on this.
[0108] All gray value sequences with the same number of diaphragm layers are combined into sets of equal-layer diaphragm sequences;
[0109] The set with the largest number of grayscale value sequences among all equal-layer diaphragm sequence sets is recorded as the maximum equal-layer diaphragm sequence set;
[0110] It should be noted that if all equal-layer diaphragm sequences are , among which the set of equal-layer diaphragm sequences with the largest number of gray value sequences is ,but contains the most grayscale value sequences, and the number is equal. If The number of diaphragm layers is 5, 7, 9, and 12 respectively. , as the maximum set of equal-layer diaphragm sequences.
[0111] The average of the grayscale values of the pixels corresponding to the pixels in the grayscale image of the cross-section of the battery cell in each diaphragm layer of each grayscale value sequence in the maximum equal-layer diaphragm sequence set is used as the diaphragm color feature value of each diaphragm layer of each grayscale value sequence;
[0112] The number of pixels of each diaphragm layer of each gray value sequence in the maximum equal-layer diaphragm sequence set is used as the diaphragm layer thickness of each diaphragm layer of each gray value sequence;
[0113] Arrange the diaphragm color feature values of each diaphragm layer of all gray value sequences in ascending order of the column number to form a diaphragm color change sequence of each diaphragm layer of the battery cell in the lithium battery;
[0114] For the thickness of the diaphragm layer, the same method as the diaphragm color change sequence is used to obtain the diaphragm thickness change sequence of each diaphragm layer in the battery cell of the lithium battery;
[0115] It should be noted that the diaphragm color feature value is used to characterize the diaphragm color of the diaphragm layer in the column where the gray value sequence is located; secondly, the diaphragm color change sequence and the diaphragm thickness change sequence respectively reflect the color change and thickness change of the diaphragm inside the battery cell along the horizontal direction.
[0116] Determine the color difference coefficient of the separator layer of the battery cell in the lithium battery according to the difference between the separator color change sequences of all arbitrary two separator layers;
[0117] Preferably, as an embodiment of the present application, the DTW distance between the diaphragm color change sequences of any two diaphragm layers is recorded as the diaphragm color change difference; the average of all diaphragm color change differences is used as the diaphragm layer color difference coefficient of the battery cell in the lithium battery.
[0118] It can be understood that the embodiment of the present application determines the color difference coefficient of the diaphragm layer by calculating the DTW distance between the diaphragm color change sequences of any two diaphragm layers. As other implementation methods, the implementer can also adopt other methods of the prior art, such as Euclidean distance, cosine similarity, etc. This embodiment does not impose any special restrictions on this.
[0119] The mean of all elements in the membrane color change sequence of all membrane layers is recorded as the first mean;
[0120] The ratio of the color difference coefficient of the diaphragm layer to the first average value is used as the over-compression transparency coefficient of the diaphragm of the battery cell in the lithium battery;
[0121] It should be noted that the greater the difference in the color of the diaphragms between different layers of diaphragms inside the battery cell, the larger the color difference coefficient of the diaphragm layers, and the smaller the grayscale value of the pixel points corresponding to the different layers of diaphragms inside the battery cell in the battery cell binary image, the smaller the first mean value, and the greater the degree to which the diaphragm appears transparent due to excessive compression of the diaphragm inside the target battery cell during the hot pressing process, and the larger the over-compression transparency coefficient of the diaphragm. In the process of calculating the ratio, in order to prevent the denominator from being 0, a parameter adjustment factor is preset, and the value of the parameter adjustment factor is 0.01.
[0122] Furthermore, the present application provides a flowchart of the steps of the method for obtaining the over-compression transparency coefficient of the diaphragm of the lithium battery cell as shown in FIG. Figure 3 shown.
[0123] The difference between the thickness variation sequences of any two diaphragm layers is used to determine the thickness variation coefficient of the diaphragm layer of the battery cell in the lithium battery;
[0124] Preferably, as an embodiment of the present application, the DTW distance between the membrane thickness change sequences of any two membrane layers is recorded as the membrane thickness change difference; the average of all membrane thickness change differences is used as the membrane layer thickness difference coefficient of the battery cell in the lithium battery.
[0125] Preferably, as another embodiment of the present application, the Euclidean distance between the membrane thickness change sequences of any two membrane layers is recorded as the membrane thickness change difference.
[0126] It should be noted that the diaphragm layer thickness difference coefficient is used to characterize the difference in diaphragm thickness between different diaphragm layers inside the battery cell. The greater the difference in diaphragm thickness between different diaphragm layers inside the battery cell, the greater the diaphragm layer thickness difference coefficient, and the greater the possibility that the diaphragm inside the battery cell will be over-compressed during the hot pressing process.
[0127] The mean of all elements in the diaphragm color thickness sequence of all diaphragm layers is recorded as the second mean;
[0128] The ratio of the diaphragm layer thickness difference coefficient to the second mean value is used as the diaphragm over-compression factor of the battery cell in the lithium battery;
[0129] Forward fusion of the diaphragm over-compression factor and the diaphragm over-compression transparency coefficient is performed to determine the degree of diaphragm over-compression of the battery cell in the lithium battery;
[0130] Preferably, as an embodiment of the present application, the product of the diaphragm over-compression factor and the diaphragm over-compression transparency coefficient is used as the diaphragm over-compression degree of the battery cell in the lithium battery.
[0131] It should be noted that the degree of over-compression of the diaphragm can represent the degree to which the diaphragm inside the target battery cell is over-compressed during the hot pressing and shaping process. The greater the degree of over-compression of the diaphragm, the greater the degree of over-compression.
[0132] At this point, the degree of over-compression of the diaphragm of the battery cell in the lithium battery is obtained.
[0133] Step 4, based on the degree of wrinkling of the diaphragm and the degree of over-compression of the diaphragm, obtain the thermal pressing shaping effect coefficient of the battery cell in the lithium battery, determine the optimal boost cylinder pressure, and perform intelligent packaging on the soft-pack lithium battery.
[0134] Based on the above analysis, the hot pressing shaping effect coefficient of the battery cell in the lithium battery is determined according to the degree of wrinkling of the diaphragm and the degree of over-compression of the diaphragm. The specific method is:
[0135] The degree of diaphragm wrinkling and the degree of diaphragm over-compression are positively integrated to determine the degree of diaphragm deformation of the battery cell in the lithium battery;
[0136] Preferably, as an embodiment of the present application, the product of the diaphragm wrinkle degree and the diaphragm over-compression degree is used as the diaphragm wrinkle degree and the diaphragm over-compression degree.
[0137] The thermal compression shaping effect coefficient of the battery cell in the lithium battery is negatively correlated with the degree of deformation of the diaphragm;
[0138] It can be understood that a negative relationship indicates that the dependent variable will decrease as the independent variable increases, and the dependent variable will increase as the independent variable decreases. The specific relationship can be a subtraction relationship, a division relationship, a negative exponential power, etc., which is determined by actual application and this application does not impose any special restrictions on this.
[0139] Preferably, as an embodiment of the present application, the thermal pressing shaping effect coefficient of the battery cell in the lithium battery is the inverse of the deformation degree of the diaphragm, wherein, in order to prevent the denominator from being 0, a parameter adjustment factor is preset, and the value of the parameter adjustment factor is 0.01.
[0140] Preferably, as another embodiment of the present application, the result of an exponential function with a natural constant as the base and the inverse of the degree of deformation of the diaphragm as the exponent is used as the thermal pressing shaping effect coefficient of the battery cell in the lithium battery.
[0141] It should be noted that the more severe the wrinkling of the diaphragm inside the battery cell, the greater the degree of wrinkling of the diaphragm, and the greater the degree of over-compression of the diaphragm inside the battery cell, the worse the hot pressing shaping effect of the battery cell in the lithium battery, and the smaller the hot pressing shaping effect coefficient.
[0142] Obtain the minimum boost cylinder pressure and maximum boost cylinder pressure of all battery cells during the hot pressing and shaping process;
[0143] Obtain N cross-sectional images of battery cells that have been subjected to hot pressing and shaping treatment, obtain the hot pressing and shaping effect coefficient of each battery cell using the same method as the hot pressing and shaping effect coefficient, and obtain the boost cylinder pressure of each battery cell during the hot pressing and shaping process;
[0144] The boost cylinder pressure of each battery cell is taken as the horizontal coordinate, and the thermal pressure shaping effect coefficient of each battery cell is taken as the vertical coordinate, and curve fitting is performed on all battery cells;
[0145] The boost cylinder pressure corresponding to the maximum thermal pressure shaping effect coefficient of the boost cylinder pressure of the battery cell in the fitting curve within the range of the minimum boost cylinder pressure and the maximum boost cylinder pressure is taken as the optimal boost cylinder pressure;
[0146] Preferably, as another embodiment of the present application, 50 cross-sectional images of the battery cells after hot pressing and shaping are obtained. As other implementation methods, the implementer can set them according to the actual situation.
[0147] Based on the optimal boost cylinder pressure, the boost cylinder pressure is adjusted during the subsequent hot pressing and shaping process of the battery cells.
[0148] Place the hot-pressed and shaped battery cell into the aluminum-plastic film, heat-seal the tabs on the upper end of the battery cell with the aluminum-plastic film, and then seal the aluminum-plastic film on the lower end of the roll core to complete the top seal of the soft-pack lithium battery;
[0149] After adding electrolyte into the aluminum-plastic film of the top-sealed soft-pack lithium battery, the aluminum-plastic film is packaged, so that the soft-pack lithium battery is in a sealed state. After the soft-pack lithium battery is formed, a certain amount of gas will be generated in the aluminum-plastic film due to the formation effect, completing the pre-sealing of the soft-pack lithium battery;
[0150] The air in the formed soft-pack lithium battery is extracted and the soft-pack lithium battery is re-sealed to complete the second sealing of the soft-pack lithium battery;
[0151] The soft-pack lithium battery after secondary sealing is trimmed and folded to complete the intelligent packaging of the soft-pack lithium battery.
[0152] Based on the same inventive concept as the above method, an embodiment of the present application also provides an intelligent packaging device for lithium batteries, including a memory, a processor, and a computer program stored in the memory and running on the processor, and when the processor executes the computer program, the steps of any one of the above-mentioned intelligent packaging methods for lithium batteries are implemented.
[0153] Based on the same inventive concept as the above method, the embodiment of the present application also provides an intelligent packaging system for lithium batteries, including:
[0154] The battery cell data acquisition module obtains the grayscale image of the cross section of the lithium battery cell;
[0155] The hot pressing shaping analysis module determines the degree of diaphragm wrinkling of the battery cell in the lithium battery according to the distance difference and distribution between the pixels in the grayscale image of the cross-section of the battery cell of the lithium battery; determines the degree of over-compression of the diaphragm in the battery cell of the lithium battery according to the change of the grayscale value of the pixels and the change of the number of pixels in the grayscale image of the cross-section of the battery cell of the lithium battery; obtains the hot pressing shaping effect coefficient of the battery cell in the lithium battery based on the degree of diaphragm wrinkling and the degree of over-compression of the diaphragm;
[0156] The boost cylinder pressure acquisition module determines the optimal boost cylinder pressure based on the thermal compression shaping effect coefficient of the battery cells in the lithium battery, adjusts the boost cylinder pressure during the subsequent thermal compression shaping process of the battery cells, and completes the packaging of the soft-pack lithium battery.
[0157] Furthermore, the present application provides a flow chart of the steps of a smart packaging system for lithium batteries as shown in Figure 4 shown.
[0158] It should be understood that although Figure 1 The steps in the flowchart are shown in sequence as indicated by the arrows, but these steps are not necessarily executed in the order indicated by the arrows. Unless otherwise specified in this document, there is no strict order restriction for the execution of these steps, and these steps can be executed in other orders. Moreover, Figure 1 At least part of the steps may include multiple sub-steps or multiple stages. These sub-steps or stages are not necessarily executed at the same time, but can be executed at different times. The execution order of these sub-steps or stages is not necessarily sequential, but can be executed in turn or alternately with other steps or at least part of the sub-steps or stages of other steps.
[0159] The technical features of the above embodiments may be combined arbitrarily. To make the description concise, not all possible combinations of the technical features in the above embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.
[0160] The above-mentioned embodiments only express several implementation methods of the present application, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the present application. It should be pointed out that, for those of ordinary skill in the art, several modifications and improvements can be made without departing from the concept of the present application. Therefore, any simple modification, equivalent change and modification made to the above embodiments according to the technical essence of the present application without departing from the content of the technical solution of the present application, shall fall within the protection scope of the technical solution of the present application.
Claims
1. A smart packaging method for lithium batteries, characterized in that: The method comprises the following steps: Obtain a grayscale image of the cross section of a lithium battery cell; Binarize the grayscale image of the cross section of the battery cell to obtain the binary image of the battery cell and the pixel points of the diaphragm, extract the skeleton line of the battery cell diaphragm, fit the skeleton line of the battery cell diaphragm to obtain the peak and valley pixel points, and determine the degree of diaphragm wrinkles of the battery cell in the lithium battery according to the distance difference and distribution between the pixel points in the grayscale image of the cross section of the lithium battery cell; determine the degree of diaphragm concavity of the battery cell in the lithium battery according to the distribution and number of peak and valley pixel points in the skeleton line of the battery cell diaphragm; determine the discreteness of the diaphragm thickness of the battery cell in the lithium battery according to the distance difference and discreteness between the diaphragm pixel points; forwardly fuse the diaphragm concavity and the diaphragm thickness discreteness to determine the degree of diaphragm wrinkles of the battery cell in the lithium battery; The columns of the binary image of the battery cell whose grayscale values are not all zero are recorded as grayscale value sequences, the grayscale value sequences are segmented to obtain the diaphragm layers, all grayscale value sequences with the same number of diaphragm layers are composed of each equal-layer diaphragm sequence set, and the set with the largest number of grayscale value sequences is selected and recorded as the maximum equal-layer diaphragm sequence set; according to the grayscale value changes of the pixels in the grayscale image of the cross-section of the battery cell of the lithium battery and the change in the number of pixels, the degree of over-compression of the diaphragm of the battery cell in the lithium battery is determined; all pixels in each diaphragm layer of each grayscale sequence in the maximum equal-layer diaphragm sequence set are recorded in the cross-section of the battery cell. The grayscale value mean of the cross-sectional grayscale image is sorted to obtain the diaphragm color change sequence, and the diaphragm over-compression transparency coefficient is obtained according to the difference between the diaphragm color change sequences and the mean of the diaphragm color change sequence elements; the number of pixels in the diaphragm layer in the maximum equal-layer diaphragm sequence set is sorted to obtain the diaphragm thickness change sequence; the diaphragm over-compression factor is obtained according to the difference between the diaphragm thickness change sequences and the mean of the diaphragm thickness change sequence elements; the diaphragm over-compression factor is forwardly fused with the diaphragm over-compression transparency coefficient to determine the degree of diaphragm over-compression of the battery cell in the lithium battery; Based on the degree of diaphragm wrinkles and the degree of over-compression of the diaphragm, the thermal pressing shaping effect coefficient of the battery cell in the lithium battery is obtained, the optimal booster cylinder pressure is determined, and the soft-pack lithium battery is intelligently packaged; The step of obtaining the thermal pressure shaping effect coefficient of the battery cell in the lithium battery and determining the optimal boost cylinder pressure includes: The degree of diaphragm wrinkling and the degree of diaphragm over-compression are positively integrated to determine the degree of diaphragm deformation of the battery cell in the lithium battery; The thermal compression shaping effect coefficient of the battery cell in the lithium battery is negatively correlated with the degree of deformation of the diaphragm; Obtain the minimum boost cylinder pressure and the maximum boost cylinder pressure of all battery cells during the hot pressing shaping process, and obtain the hot pressing shaping effect coefficient and the boost cylinder pressure of each battery cell; Perform curve fitting on the boost cylinder pressure and thermal pressure shaping effect coefficient of each battery cell; The boost cylinder pressure corresponding to the maximum thermal pressure shaping effect coefficient of the boost cylinder pressure of the battery cell in the fitting curve within the range of the minimum boost cylinder pressure and the maximum boost cylinder pressure is taken as the optimal boost cylinder pressure.
2. The intelligent packaging method for lithium batteries according to claim 1, characterized in that: The method of determining the degree of wrinkling of the separator of the battery cell in the lithium battery comprises: Binarization is performed on the grayscale image of the cross section of the battery cell to obtain a binary image of the battery cell to obtain the pixel points of the separator; The skeleton line extraction algorithm is used to obtain the skeleton line of the battery cell diaphragm of the battery cell binary image; Perform curve fitting on the core diaphragm skeleton line to obtain the peak points and valley points of the fitting curve, which are recorded as the peak and valley pixel points of the core diaphragm skeleton line; Determine the degree of convexity and concavity of the separator in the lithium battery according to the distribution and number of peak and valley pixels in the skeleton line of the separator; Determine the dispersion of the diaphragm thickness of the battery cell in the lithium battery according to the distance difference and dispersion degree between the diaphragm pixels; The degree of diaphragm wrinkles of the battery cell in the lithium battery is determined by forward fusion of the diaphragm concave-convex degree and the diaphragm thickness dispersion.
3. A smart packaging method for lithium batteries as claimed in claim 2, characterized in that: The method of determining the degree of convexity and concavity of the separator of the battery cell in the lithium battery comprises: Calculate the mean of the ordinates of all pixels in the cell separator skeleton line, and record it as the central average value of the cell separator skeleton line; The difference between the ordinate of each peak-valley pixel point of the cell diaphragm skeleton line and the central average value is recorded as the diaphragm skeleton line bending coefficient of each peak-valley pixel point of the cell diaphragm skeleton line; The number of peak and valley pixel points of the battery cell diaphragm skeleton line is recorded as the peak and valley number; The number of peaks and valleys and the bending coefficient of the membrane skeleton line are forwardly integrated to determine the degree of convexity and concavity of the membrane of the battery cell in the lithium battery.
4. The intelligent packaging method for lithium batteries according to claim 2, characterized in that: The method of determining the dispersion of the diaphragm thickness of the battery cell in the lithium battery comprises: The vertical coordinate difference between any two diaphragm pixels in each column of pixel points in the battery cell binary image is recorded as the diaphragm difference; The maximum value of all the diaphragm differences is used as the diaphragm thickness of the corresponding column in the battery cell binary image. If there is no diaphragm pixel in each column of pixels, the diaphragm thickness is assigned a value of 0; The discrete degree of the diaphragm thickness of all columns with diaphragm pixels is determined as the discrete degree of the diaphragm thickness of the battery cell in the lithium battery.
5. The intelligent packaging method for lithium batteries according to claim 1, characterized in that: Determining the degree of over-compression of the diaphragm of the battery cell in the lithium battery includes: Counting all the pixels in each column whose grayscale values are not all zero in the binary image of the battery cell, and obtaining a grayscale value sequence of the pixels in each column whose grayscale values are not all zero; Segmenting the grayscale value sequence of each column based on the membrane pixel points to obtain multiple membrane layers of each column; All gray value sequences with the same number of diaphragm layers are combined into sets of equal-layer diaphragm sequences; The set with the largest number of grayscale value sequences among all equal-layer diaphragm sequence sets is recorded as the maximum equal-layer diaphragm sequence set; Determine the over-compression transparency coefficient of the separator of the battery cell in the lithium battery according to the difference in gray values between the pixels in each separator layer of each gray value sequence in the maximum equal-layer separator sequence set in the battery cell cross-sectional gray image; Determine the over-compression factor of the separator of the battery cell in the lithium battery according to the difference in the number of pixels in each separator layer of each gray value sequence in the maximum equal-layer separator sequence set; The membrane over-compression factor and the membrane over-compression transparency coefficient are forwardly integrated to determine the membrane over-compression degree of the battery cell in the lithium battery.
6. A smart packaging method for lithium batteries as claimed in claim 5, characterized in that: The over-compression transparency coefficient of the diaphragm of the battery cell in the lithium battery includes: The average of the grayscale values of the pixels corresponding to the pixels in the grayscale image of the cross-section of the battery cell in each diaphragm layer of each grayscale value sequence in the maximum equal-layer diaphragm sequence set is used as the diaphragm color feature value of each diaphragm layer of each grayscale value sequence in the maximum equal-layer diaphragm sequence set; Arrange the diaphragm color feature values of each diaphragm layer of all gray value sequences in ascending order of the column number to form a diaphragm color change sequence of each diaphragm layer of the battery cell in the lithium battery; Determine the color difference coefficient of the separator layer of the battery cell in the lithium battery according to the difference between the separator color change sequences of all arbitrary two separator layers; The mean of all elements in the membrane color change sequence of all membrane layers is recorded as the first mean; The ratio of the color difference coefficient of the diaphragm layer to the first average value is used as the over-compression transparency coefficient of the diaphragm of the battery cell in the lithium battery.
7. The intelligent packaging method for lithium batteries according to claim 5, characterized in that: The method of determining the over-compression factor of the separator of the battery cell in the lithium battery comprises: The number of pixels in each diaphragm layer of each gray value sequence in the maximum equal-layer diaphragm sequence set is used as the diaphragm layer thickness of each diaphragm layer of each gray value sequence; Arrange the thickness of each diaphragm layer in all gray value sequences in ascending order of the column number to form a diaphragm thickness variation sequence of each diaphragm layer in the battery cell of the lithium battery; The difference between the thickness variation sequences of any two diaphragm layers is used to determine the thickness variation coefficient of the diaphragm layer of the battery cell in the lithium battery; The mean of all elements in the diaphragm color thickness sequence of all diaphragm layers is recorded as the second mean; The ratio of the diaphragm layer thickness difference coefficient to the second mean value is used as the diaphragm over-compression factor of the battery cell in the lithium battery.
8. An intelligent packaging device for lithium batteries, comprising a memory, a processor, and a computer program stored in the memory and running on the processor, characterized in that: When the processor executes the computer program, the steps of the intelligent packaging method for lithium batteries as described in any one of claims 1-7 are implemented.
9. An intelligent packaging system for lithium batteries, implementing the method as claimed in claim 1, characterized in that: The intelligent packaging system comprises: The battery cell data acquisition module obtains the grayscale image of the cross section of the lithium battery cell; The hot pressing shaping analysis module determines the degree of diaphragm wrinkling of the battery cell in the lithium battery according to the distance difference and distribution between the pixels in the grayscale image of the cross-section of the battery cell of the lithium battery; determines the degree of over-compression of the diaphragm in the battery cell of the lithium battery according to the change of the grayscale value of the pixels and the change of the number of pixels in the grayscale image of the cross-section of the battery cell of the lithium battery; obtains the hot pressing shaping effect coefficient of the battery cell in the lithium battery based on the degree of diaphragm wrinkling and the degree of over-compression of the diaphragm; The boost cylinder pressure acquisition module determines the optimal boost cylinder pressure based on the thermal compression shaping effect coefficient of the battery cells in the lithium battery, adjusts the boost cylinder pressure during the subsequent thermal compression shaping process of the battery cells, and intelligently packages the soft-pack lithium battery.