Tunnel segment missing corner repair device and repair process

By drilling holes in the missing corners of the tunnel segments, filling them with reinforcement glue and pouring polymer repair mortar, combined with the concave and convex groove structures of the bottom plate and side plates, efficient and high-quality repair of the missing corners of the tunnel segments is achieved, solving the existing problem of The problem of long time consumption and low integration in technology.

CN118601626BActive Publication Date: 2024-10-01JINAN RAILWAY SEGMENT MFG CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411062780.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-08-05
Publication Date
2024-10-01
Estimated Expiration
2044-08-05

AI Technical Summary

Technical Problem

The existing method of repairing missing corners of tunnel segments is time-consuming, difficult to guarantee quality, and has low bonding at the repair interface, making it easy to fall off due to high water pressure penetration during the operation period.

Method used

A device for repairing missing corners of tunnel segments is designed, which includes drilling implant holes, tie pieces, pouring enclosure structures, grouting components and fastening components. It is repaired by drilling holes, filling reinforcement glue, and pouring polymer. The mortar is vibrated and solidified, and combined with the concave and convex groove structures of the bottom plate and side panels, rapid prototyping and high-strength repair are achieved.

Benefits of technology

It improves the construction efficiency and repair quality, ensures high bonding strength after repair, avoids repeated falling off problems, and the device can be reused.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118601626B_ABST
    Figure CN118601626B_ABST
Patent Text Reader

Abstract

The present invention discloses a tunnel segment missing corner repair device and repair process, belonging to the technical field of tunnel construction auxiliary equipment. The tunnel segment missing corner repair device includes an implantation hole, a tie piece, a casting enclosure structure, a grouting assembly and a fastening and positioning assembly. The tunnel segment missing corner repair device and repair process provided by the present invention have reasonable structures and steps, simple construction, and the repair device can be reused. It can directly cast a concave and convex shape consistent with the segment axis docking surface and the circumferential docking surface at the missing corner, without the need for manual multiple plastering, and one-time molding, with high construction efficiency; after the polymer repair mortar is fixed and formed, it is connected to the wall surface of the original missing corner through the tie piece, and the interface bonding strength is high; the side plate of the casting maintenance structure is assembled by a plurality of first unit plates and second unit plates, which is convenient for flexibly selecting the number of the first unit plates and the second unit plates according to the size of the notch, and it is also easy to make the length of the overflow trough meet the requirements.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a tunnel segment missing corner repair device and a repair process, belonging to the technical field of tunnel construction auxiliary equipment. Background Art

[0002] Subways have the advantages of being safe, fast, and environmentally friendly. Shield construction technology occupies a dominant position in urban subway construction, and tunnel segments are the main assembly components of shield tunnels. Tunnels are usually located in a complex hydrogeological environment that is dark and humid underground. As the innermost barrier of the tunnel, tunnel segments are responsible for resisting soil pressure, groundwater pressure, and some special loads. The quality of tunnel segments directly affects the waterproof performance and durability of the tunnel, and is related to the overall quality and safety of the tunnel. Therefore, tunnel segments need to meet the corresponding technical indicators such as compression resistance, impermeability, and durability. At present, tunnel segments are mainly prefabricated in factories with concrete. In the actual production process, uneven vibration of corners or bumps during hoisting and transportation may cause the segments to be missing or falling off.

[0003] The existing methods for repairing missing corners of pipe segments mainly adopt direct plastering or rebar planting and meshing repair methods according to the area of ​​the missing corners and whether there is any leakage of reinforcement. However, the circumferential and axial joint surfaces of the tunnel segments contain uneven surfaces such as grooves for fixing waterproof rubber strips. The above two methods require a long time of manual plastering operation to shape these uneven surfaces at the missing corners, which requires a lot of manpower and the final quality is difficult to guarantee, resulting in poor overall appearance quality. At the same time, the above two repair methods also have the problem of low bonding degree at the repair interface, and the repaired pipe segment will fall off again if it is bumped again or under the influence of high water pressure penetration during the subway operation period. Summary of the invention

[0004] In order to solve the problems existing in the prior art, the present invention provides a tunnel segment corner missing repair device and repair process, which has high construction efficiency and high repair quality.

[0005] The present invention achieves the above-mentioned purpose by adopting the following technical solutions:

[0006] A tunnel segment missing corner repair device, comprising:

[0007] Drilling a plurality of implantation holes on the wall surface of the missing corner;

[0008] An anchor, one end of which is placed in the implantation hole and the other end is located at the notched corner of the pipe segment, and the implantation hole is used to fill the rebar-embedded glue;

[0009] A casting enclosure structure, which is covered on the outside of the missing corner of the pipe segment and is used to enclose a casting cavity matching the shape of the pipe segment at the missing corner;

[0010] A grouting assembly, the grouting assembly is used to inject polymer repair mortar into the casting cavity;

[0011] A fastening and positioning assembly, wherein the fastening and positioning assembly is used to position the pouring enclosure structure on the pipe segment;

[0012] The pouring enclosure structure is surrounded by a bottom plate, a front side plate, a rear side plate and a side plate; the bottom plate is used to support the axial butt joint surface of the pipe segment adjacent to the missing corner, the plate surface of the bottom plate is provided with concave and convex grooves matching the axial butt joint surface of the pipe segment, and a grouting port for communicating with the grouting assembly is opened on the bottom plate;

[0013] The front side plate is used to abut against the inner arc surface of the tube segment adjacent to the notched corner, the lower end surface of the front side plate is supported on the edge of the plate surface of the bottom plate, and the front side plate is fastened to the bottom plate by bolts;

[0014] The rear side plate is used to abut against the outer arc surface of the tube segment adjacent to the notched corner, the rear end surface of the bottom plate abuts against the edge of the plate surface of the rear side plate, and the bottom plate and the rear side plate are fastened and connected by bolts;

[0015] The side plate is used to abut against the circumferential butt joint surface of the tube sheet adjacent to the notched corner. The plate surface of the side plate is provided with a concave-convex groove matching the circumferential butt joint surface of the tube sheet. The lower end surface of the side plate is supported on the plate surface edge of the bottom plate, and the side plate is fastened to the bottom plate by bolts. The front end surface and the rear end surface of the side plate are respectively abutted against the plate surface edges of the front side plate and the rear side plate, and the front end surface and the rear end surface of the side plate are both provided with a clamping protrusion, and the plate surfaces of the front side plate and the rear side plate are both provided with a clamping groove matching the clamping protrusion. The side plate is assembled and connected with the front side plate and the rear side plate respectively by matching the corresponding clamping protrusion and the clamping groove.

[0016] The side plates are formed by splicing a number of unit plates up and down, and the adjacent unit plates are fastened and connected by bolts. At least the unit plates arranged at the top are provided with overflow grooves, and the overflow grooves are used to conduct the casting cavity with the outside.

[0017] In one specific embodiment, the unit plate includes a first unit plate and a second unit plate, the first unit plate and the second unit plate are spliced ​​alternately up and down, each of the first unit plate and the second unit plate is provided with a first bolt hole and a second bolt hole, the first bolt hole passes through the upper end surface and the lower end surface of the unit plate, the second bolt hole extends downward from the upper end surface of the unit plate, the first bolt hole on the first unit plate corresponds to the position of the second bolt hole on the second unit plate, and the second bolt hole on the first unit plate corresponds to the position of the first bolt hole on the second unit plate;

[0018] The first unit plate is connected to the second unit plate below it by a first bolt, and the first bolt passes through a first bolt hole on the first unit plate and is threadedly connected to a second bolt hole on the second unit plate below it;

[0019] The first unit plate is connected to the second unit plate above it through a second bolt. The second bolt passes through a first bolt hole on the second unit plate above and is threadedly connected to a second bolt hole on the first unit plate.

[0020] In one specific embodiment, the casting enclosure structure also includes a sealing strip for embedding in the overflow trough, the sealing strip has a variety of length specifications, and after the sealing strip is embedded in the overflow trough, the surface of the sealing strip is flush with the surface of the unit board adjacent to the overflow trough.

[0021] Furthermore, the cross-sectional shape of the overflow groove is a closed trapezoid or a closed arc, and the cross-sectional shape of the sealing strip matches the cross-sectional shape of the overflow groove.

[0022] In a preferred embodiment, sealing strips are embedded on the contact surface between the front side plate and the bottom plate, on the contact surface between the rear side plate and the bottom plate, and on the contact surface between the side plate and the bottom plate.

[0023] In one specific embodiment, the grouting assembly includes an air compressor and a slurry sealing cylinder. The top of the slurry sealing cylinder is connected to the air compressor through an air inlet pipe, and the bottom of the slurry sealing cylinder is connected to the grouting port through a grouting pipe. Valves are respectively provided on the air inlet pipe and the grouting pipe.

[0024] In another specific embodiment, the tightening and positioning assembly includes a load-bearing frame and a tightening mechanism;

[0025] The load-bearing frame comprises:

[0026] An upper fixed plate, a movable plate and a lower fixed plate are arranged in sequence, the upper fixed plate and the lower fixed plate are fixedly connected by a plurality of tie rods, a through hole is provided on the movable plate, and the tie rods freely pass through the through hole on the movable plate, a plate surface of the movable plate is provided with a concave-convex groove matching the axial butt surface of the pipe segment, and a notch corresponding to the grouting port is provided on the lower fixed plate;

[0027] A hydraulic cylinder, wherein the cylinder body of the hydraulic cylinder is fixed on the movable plate, and the cylinder rod of the hydraulic cylinder is connected to the upper fixed plate; the bottom plate of the casting enclosure structure is placed on the lower fixed plate, and the pipe segment and the casting enclosure structure are clamped between the movable plate and the lower fixed plate under the thrust of the hydraulic cylinder;

[0028] The tightening mechanism comprises:

[0029] A base installed at the bottom of the pull rod, wherein the base is provided with threaded holes:

[0030] A push rod is provided with an external thread matching with a threaded hole on the base, the push rod is threadedly connected in the threaded hole on the base, and the end of the push rod abuts against a side plate of the casting enclosure structure.

[0031] Furthermore, the tunnel segment chipping repair device provided by the present invention also includes a vibrator, which is installed at the bottom of the lower fixed plate.

[0032] On the other hand, the present invention also provides a repair process based on the tunnel segment corner-cut repair device, comprising the following steps:

[0033] (1) Drill an implant hole on the wall surface of the notched corner of the segment, install an anchor in the implant hole, with the outer end of the anchor located at the notched corner of the segment, and fill the implant hole with anchor glue;

[0034] (2) Determine the size of the side panels according to the size of the missing corners, select the required number of unit panels to form the side panels, and the unit panels adjacent to the top of the missing corners must be provided with overflow grooves, through which the pouring cavity is connected to the outside. The overflow grooves of other parts must be sealed with sealing strips;

[0035] (3) Assemble the front side panel, side panel and bottom panel;

[0036] (4) The missing corner of the segment is suspended above the ground, and the load-bearing frame is pre-installed on the segment near the missing corner so that the segment is located between the movable plate and the lower fixed plate;

[0037] (5) Place the assembled bottom plate, front side plate and side plate at the missing corner, so that the front side plate is against the inner arc surface of the segment, and then assemble the rear side plate with the bottom plate, and adjust the up and down and left and right positions of the casting enclosure structure, so that the concave and convex grooves on the bottom plate are matched and engaged with the concave and convex grooves on the circumferential butt joint surface of the segment, and the concave and convex grooves on the side plate are matched and engaged with the concave and convex grooves on the circumferential butt joint surface of the segment, so that the casting enclosure structure is covered at the missing corner;

[0038] (6) Control the extension of the hydraulic cylinder rod on the load-bearing frame to move the movable plate downward relative to the lower fixed plate, and at the same time rotate the push rod of the tightening mechanism to move the push rod toward the side plate of the casting enclosure structure, so that the pipe segment and the casting enclosure structure are gradually clamped between the movable plate and the lower fixed plate, and at the same time, the casting enclosure structure is tightened laterally by the push rod;

[0039] (7) Connect the grouting pipe to the grouting port of the casting enclosure structure, inject the polymer repair mortar in the slurry sealing tube into the casting cavity through the air compressor, and stop grouting when the guide groove on the side plate overflows with the polymer repair mortar;

[0040] (8) Turning on the vibrator to vibrate the polymer repair mortar in the casting cavity to make the polymer repair mortar in the casting cavity dense, and in this process, air is discharged from the casting cavity through the overflow groove;

[0041] (9) The polymer repair mortar in the slurry sealing cylinder is injected into the pouring cavity again through the air compressor, and the grouting is stopped when the guide groove on the side plate overflows with the polymer repair mortar again;

[0042] (10) When the polymer repair mortar in the casting cavity solidifies and hardens to the required strength, remove the repair device and use an angle grinder to grind off the excess solidified body formed at the overflow groove to complete the corner repair.

[0043] The beneficial effects of this application include but are not limited to:

[0044] The tunnel pipe segment missing corner repair device and repair process provided by the present invention have reasonable structures and steps, simple construction, and the repair device can be reused. Specifically, (1) under the limitation of the concave-convex grooves on the bottom plate and the side plate of the casting maintenance structure, a concave-convex shape consistent with the axial butt joint surface and the circumferential butt joint surface of the pipe segment can be directly cast at the missing corner, without the need for multiple manual plastering, and one-time molding, with high construction efficiency; (2) after the polymer repair mortar is fixed and formed, it is connected to the wall surface of the original missing corner through the tie piece, and the interface bonding strength is high; (3) through the shape matching of the concave-convex grooves on the bottom plate and the side plate with the axial butt joint surface and the circumferential butt joint surface of the pipe segment, it is more convenient to determine the installation position of the bottom plate and the side plate; the front side plate, the rear side plate and the bottom plate are assembled and connected by the matching convex and groove, and the assembly is more convenient. (4) The side plate of the casting maintenance structure is assembled by a plurality of first unit plates and second unit plates, which is convenient to flexibly select the number of the first unit plates and the second unit plates according to the size of the notch, and it is also easy to make the length of the overflow trough meet the requirements. BRIEF DESCRIPTION OF THE DRAWINGS

[0045] The drawings described herein are used to provide a further understanding of the present application and constitute a part of the present application. The illustrative embodiments of the present application and their descriptions are used to explain the present application and do not constitute an improper limitation on the present application. In the drawings:

[0046] Figure 1 It is a schematic diagram of the segment structure when observing toward the inner curved surface of the segment;

[0047] Figure 2 It is a schematic diagram of the three-dimensional structure of the segment;

[0048] Figure 3 A schematic diagram of the structure of the tunnel segment corner-cut repair device provided by the present invention;

[0049] Figure 4 It is a schematic diagram of drilling an implantation hole on the missing corner of the pipe segment;

[0050] Figure 5 is a schematic diagram of an anchor and an implantation hole;

[0051] Figure 6Assembly drawings for pouring enclosure structures;

[0052] Figure 7 An exploded view of the poured enclosure structure;

[0053] Figure 8 It is a schematic diagram of the overflow trough on the casting enclosure structure;

[0054] Fig. 9 is a schematic diagram of a first unit board and a second unit board;

[0055] Fig.10 is a schematic diagram of a blocking strip;

[0056] Fig.11 is a schematic diagram of a fastening and positioning assembly;

[0057] Fig.12 It is a schematic diagram of the assembly structure of the bottom plate, the front side plate and the side plate;

[0058] In the figure, 1, segment; 11, missing corner; 2, inner arc surface of segment; 3, outer arc surface of segment; 4, axial butt joint surface; 5, circumferential butt joint surface; 6, rubber strip groove;

[0059] 110, implantation hole; 120, anchor;

[0060] 200, pouring enclosure structure; 210, bottom plate; 211, grouting port; 220, front side plate; 230, rear side plate; 240, side plate; 241, first unit plate; 242, second unit plate; 2401, first bolt hole; 2402, second bolt hole; 251, clamping protrusion; 252, clamping groove; 260, overflow groove; 261, sealing strip; 270, sealing strip;

[0061] 300, grouting assembly; 310, air compressor; 320, slurry sealing cylinder;

[0062] 400, fastening positioning assembly; 410, hydraulic cylinder; 420, upper fixed plate; 430, movable plate; 440, lower fixed plate; 450, pull rod; 460, base; 470, push rod; 480, vibrator. DETAILED DESCRIPTION

[0063] In order to clearly illustrate the technical features of the present solution, the present invention is described in detail below through specific implementation methods and in conjunction with the accompanying drawings.

[0064] It should be noted that many specific details are described in the following description to facilitate a full understanding of the present invention, but the present invention can also be implemented in other ways different from those described herein. Therefore, the protection scope of the present invention is not limited to the specific embodiments disclosed below.

[0065] like Figure 1 and Figure 2 As shown in FIG. 1 , it is a schematic diagram of the tube segment 1. Figure 1 The figure also shows the missing corner 11 on the segment. A single segment is an arc-shaped structure, having an inner arc surface 2 and an outer arc surface 3. During the operation of the shield machine, multiple shield segments are spliced ​​to form an annular tunnel lining. The axial butt joint 4 of the shield segment in the present invention is the butt joint between adjacent segments along the axial direction of the annular tunnel, and the circumferential butt joint 5 is the butt joint between adjacent segments in the circumferential direction of the annular tunnel. The axial butt joint 4 and the circumferential butt joint 5 are both provided with a rubber strip groove 6 for fixing the waterproof rubber strip. Bolt holes for axial connection and circumferential connection are provided on the segment, as well as marks for convenient identification of the butt joint surface.

[0066] like Figure 3-Figure 5 As shown in the figure, the tunnel segment chipping repair device provided by the present invention includes a plurality of implantation holes 110 drilled on the wall surface of the chipping part, a tie member 120, a casting enclosure structure 200, a grouting assembly 300 and a fastening positioning assembly 400, and the fastening positioning assembly 400 is used to position the casting enclosure structure 200 on the segment.

[0067] Among them, Figure 4 and Figure 5 As shown in , one end of the anchor 120 is placed in the implant hole 110, and the other end is located at the missing corner of the pipe segment. The implant hole 110 is used to fill the reinforcing bar glue. Usually, the anchor 120 has a certain configuration, such as a "J" shape, which can be made by bending a high-toughness steel wire. The "J"-shaped structure has an arched portion at the head located in the implant hole 110, so that the anchor 120 is tightened and installed in the implant hole 110.

[0068] Specifically, Figure 6 and Figure 7 As shown in the figure, the cast enclosure structure 200 is surrounded by a bottom plate 210, a front side plate 220, a rear side plate 230 and a side plate 240; the bottom plate 210 is used to support the axial butt joint surface 4 of the pipe segment adjacent to the missing corner, and the plate surface of the bottom plate 210 is provided with concave and convex grooves matching the axial butt joint surface 4 of the pipe segment, and a grouting port 211 for connecting with the grouting assembly is opened on the bottom plate 210.

[0069] The front side plate 220 is used to abut against the inner arc surface 2 of the tube segment adjacent to the notched corner. The lower end surface of the front side plate 220 is supported on the edge of the plate surface of the bottom plate 210, and the front side plate 220 and the bottom plate 210 are fastened together by bolts.

[0070] The rear side plate 230 is used to abut against the outer arc surface 3 of the tube segment adjacent to the notched corner, the rear end surface of the bottom plate 210 abuts against the plate edge of the rear side plate 230, and the bottom plate 210 and the rear side plate 230 are fastened together by bolts.

[0071] The side plate 240 is used to abut against the circumferential butt joint surface 5 of the tube segment adjacent to the notched corner. The plate surface of the side plate 240 is provided with concave-convex grooves matching the circumferential butt joint surface 5 of the tube segment. The lower end surface of the side plate 240 is supported on the plate surface edge of the bottom plate 210, and the side plate 240 and the bottom plate 210 are fastened together by bolts. The front end surface and the rear end surface of the side plate 240 abut against the plate surface edges of the front side plate 220 and the rear side plate 230 respectively.

[0072] The contact parts between the front side plate 220 and the bottom plate 210, the contact parts between the rear side plate 230 and the bottom plate 210, and the contact parts between the side plate 240 and the bottom plate 210 are fastened together by bolts, and bolt holes are provided at corresponding positions of each plate. When assembling, align the corresponding bolt holes, screw in the bolts and tighten them.

[0073] In order to facilitate the assembly of the side panel 240 with the front side panel 220 and the rear side panel 230, the present invention is provided with a protrusion 251 on the front end face and the rear end face of the side panel 240, and the plate surface of the front side panel 220 and the rear side panel 230 is provided with a groove 252 that matches the protrusion 251. The side panel 240 is assembled and connected with the front side panel 220 and the rear side panel 230 through the cooperation of the corresponding protrusion 251 and the groove 252. In actual operation, after aligning the position of the protrusion 251 and the groove 252, the protrusion 251 can be slid into the groove 252, which saves assembly time. Moreover, the connection mode of the protrusion 251 and the groove 252 can also increase the difficulty of seepage, extend the seepage path, and play a role in sealing and waterproofing.

[0074] In this way, under the limitation of the concavo-convex grooves on the bottom plate 210 and the side plate 240 of the casting maintenance structure, a concavo-convex shape consistent with the segment axis abutment surface and the circumferential abutment surface can be directly cast at the missing corner. At the same time, the bottom plate 210 and the side plate 240 can be positioned by means of the concavo-convex groove structure on the bottom plate 210 and the side plate 240, so that the bottom plate 210, the side plate 240 and the front side plate 220 and the rear side plate 230 are easier to align and assemble.

[0075] like Figure 8 As shown in the figure, the casting enclosure structure 200 is covered on the outside of the missing corner of the pipe segment, and a casting cavity matching the shape of the pipe segment is enclosed at the missing corner. The grouting assembly 300 is used to inject polymer repair mortar into the casting cavity. The polymer repair mortar can be a conventional product on the market.

[0076] The bottom plate 210, the front side plate 220, and the rear side plate 230 are highly versatile and can be processed into larger sizes. However, the upper portion of the side plate 240 needs to be provided with an overflow trough 260 that connects the casting cavity and the external environment. Figure 8 and Fig. 9As shown in , the overflow groove 260 needs to be connected to the pouring cavity at one end and to the external environment at the other end. Its function is to discharge the gas in the pouring cavity during the pouring process, and when polymer repair mortar overflows from the overflow groove 260, it is judged that the pouring cavity is full of polymer repair mortar.

[0077] For the convenience of description, the connecting length between the guide groove and the pouring cavity in the vertical direction is recorded as L1, and the distance between the length of L1 and the top of the side plate 240 is recorded as L2. Excess stone bodies will be formed in the overflow groove 260 of the length of L1 and L2. After the repair device is removed, the excess stone bodies need to be polished off. Moreover, when the length of L2 is too large, if the overflow groove 260 of the length of L2 is blocked during the pouring process, it will be difficult to clean. Therefore, in order to save the amount of polymer repair mortar and reduce the workload of handling excess consolidation bodies, the lengths of L1 and L2 should not be too large.

[0078] In order to conveniently control the length of L1 and L2, the side plate 240 in the present invention is formed by splicing a number of unit plates up and down, and the adjacent unit plates are fastened together by bolts. At least the unit plate surface arranged at the upper part is provided with an overflow groove 260, which is used to connect the casting cavity with the outside.

[0079] In actual application, according to the size of the missing corner, a required number of unit plates are selected to assemble and form the side plate 240 so that the lengths of L1 and L2 of the overflow groove 260 meet the requirements.

[0080] like Fig. 9 As shown in , in one specific embodiment, the unit plate includes a first unit plate 241 and a second unit plate 242, the first unit plate 241 and the second unit plate 242 are spliced ​​alternately up and down, each of the first unit plate 241 and the second unit plate 242 is provided with a first bolt hole 2401 and a second bolt hole 2402, the first bolt hole 2401 passes through the upper end surface and the lower end surface of the unit plate, the second bolt hole 2402 extends downward from the upper end surface of the unit plate, the first bolt hole 2401 on the first unit plate 241 corresponds to the second bolt hole 2402 on the second unit plate 242, and the second bolt hole 2402 on the first unit plate 241 corresponds to the first bolt hole 2401 on the second unit plate 242;

[0081] The first unit plate 241 is connected to the second unit plate 242 below it by a first bolt, and the first bolt passes through the first bolt hole 2401 on the first unit plate 241 and is threadedly connected to the second bolt hole 2402 on the second unit plate 242 below it;

[0082] The first unit plate 241 is connected to the second unit plate 242 above it by a second bolt. The second bolt passes through the first bolt hole 2401 on the second unit plate 242 above and is threadedly connected to the second bolt hole 2402 on the first unit plate 241 .

[0083] During assembly, the unit plate resting against the bottom plate 210 is selected as the first unit plate 241, and the first unit plate 241 is connected to the threaded hole on the bottom plate 210 by the first bolt, and then the other second unit plates 242 and the first unit plates 241 are assembled in sequence.

[0084] Typically, the bolts used for casting the enclosure structure 200 of the present invention are hexagon socket bolts, and the corresponding bolt holes are configured as countersunk holes.

[0085] In the present invention, the side plate 240 is formed by assembling a plurality of first unit plates 241 and second unit plates 242, which facilitates flexible selection of the number of first unit plates 241 and second unit plates 242 according to the size of the notch, and also facilitates making the L1 and L2 lengths of the overflow trough 260 meet the requirements.

[0086] Further, such as Fig.10 As shown in , the casting enclosure structure 200 also includes a blocking strip 261 for embedding in the overflow groove 260, and the blocking strip 261 has a variety of length specifications. When in use, the blocking strip 261 of the required length can be embedded in the overflow groove 260, so that the effective use length of the overflow groove 260 meets the length requirements of L1 and L2, thereby improving the versatility of the side plate 240. It can be understood that after the blocking strip 261 is embedded in the overflow groove 260, the surface of the blocking strip 261 should be flush with the surface of the unit board adjacent to the overflow groove 260.

[0087] Specifically, the cross-sectional shape of the overflow groove 260 is a closed trapezoid or a closed arc, and the cross-sectional shape of the blocking strip 261 matches the cross-sectional shape of the overflow groove 260. During operation, the blocking strip 261 is inserted into the overflow groove 260 from one end of the overflow groove 260, and the closed trapezoid or closed arc shape design can prevent the blocking strip 261 from falling off.

[0088] Further, such as Figure 7 As shown in , in order to improve the sealing performance on the contact surface, sealing strips 270 are preferably embedded on the contact surface between the front side plate 220 and the bottom plate 210 , the contact surface between the rear side plate 230 and the bottom plate 210 , and the contact surface between the side plate 240 and the bottom plate 210 .

[0089] like Fig.11 As shown in one specific embodiment, the fastening positioning assembly 400 includes a load-bearing frame and a tightening mechanism, and the load-bearing frame includes a hydraulic cylinder 410, and an upper fixed plate 420, a movable plate 430 and a lower fixed plate 440 arranged in sequence.

[0090] The upper fixed plate 420 and the lower fixed plate 440 are fixedly connected by a plurality of tie rods 450, for example, four tie rods 450. The plate surface of the movable plate 430 is provided with a concave-convex groove matching the axial butt joint surface 4 of the pipe segment. The movable plate 430 is provided with two through holes, and the connecting line of the two through holes is parallel to the concave-convex groove on the plate surface of the movable plate 430. The two tie rods 450 freely pass through the two through holes on the movable plate 430. The lower fixed plate 440 is provided with a notch corresponding to the grouting port 211, so that the grouting port 211 is exposed and connected to the grouting pipe.

[0091] The cylinder body of the hydraulic cylinder 410 is fixed on the movable plate 430 , and the cylinder rod of the hydraulic cylinder is connected to the upper fixed plate 420 .

[0092] The tightening mechanism includes a base 460 and a push rod 470 installed at the lower part of the pull rod 450. A threaded hole is opened on the base 460, and the push rod 470 is provided with an external thread matching the threaded hole on the base 460. The push rod 470 is threadedly connected to the threaded hole on the base 460, and the end of the push rod 470 rests on the side plate 240 of the cast enclosure structure 200.

[0093] During installation, the bottom plate 210 of the pouring enclosure 200 is placed on the lower fixed plate 440, the movable plate 430 is against the axial butt joint surface of the top of the segment, and the top rod 470 faces the side plate 240 of the maintenance structure. The pouring enclosure 200 is fixed on the segment by adjusting the hydraulic cylinder 410 and the top rod 470.

[0094] In one specific embodiment, the grouting assembly 300 includes an air compressor 310 and a slurry sealing cylinder 320. The top of the slurry sealing cylinder 320 is connected to the air compressor 310 through an air inlet pipe, and the bottom of the slurry sealing cylinder 320 is connected to the grouting port 211 through a grouting pipe. Valves are respectively provided on the air inlet pipe and the grouting pipe. When in use, a certain pressure of gas is introduced into the upper cavity of the slurry sealing cylinder 320 through the air compressor 310, and the polymer repair mortar in the slurry sealing cylinder 320 is pressed into the casting cavity by the gas pressure, so that the polymer repair mortar fills the casting cavity.

[0095] Furthermore, the repair device provided by the present invention also includes a vibrator 480, which is installed at the bottom of the lower fixed plate 440. The vibrator 480 vibrates the polymer repair mortar in the casting cavity to make the polymer repair mortar in the casting cavity dense. During this process, air is discharged from the casting cavity through the overflow groove 260.

[0096] Furthermore, the repair device provided by the present invention also includes a laser locator, which can be installed on the movable plate by magnet adsorption. The laser locator can project the position of the circumferential joint surface of the pipe segment adjacent to the missing corner onto the base plate, thereby facilitating and accurately obtaining the installation position of the base plate.

[0097] On the other hand, the present invention also provides a repair process based on the above tunnel segment corner-cut repair device, comprising the following steps:

[0098] (1) If Figure 8 As shown in , an implantation hole 110 is drilled on the wall surface of the missing corner of the pipe segment, and an anchor 120 is installed in the implantation hole 110. The outer end of the anchor 120 is located at the missing corner of the pipe segment, and the implantation hole 110 is filled with anchor glue;

[0099] (2) Determine the size of the side panel 240 according to the size of the missing corner, select the required number of unit panels to splice to form the side panel 240, the unit panel adjacent to the top of the missing corner must be provided with an overflow groove 260, and the pouring cavity is connected to the outside through the overflow groove 260, and the overflow grooves 260 of other parts must be embedded with sealing strips 261 for sealing;

[0100] (3) Assemble the front side panel 220, the side panel 240 and the bottom panel 210 as follows: Fig.12 The structure shown in;

[0101] (4) The notched corner of the pipe segment is suspended above the ground, and a load-bearing frame is pre-installed on the pipe segment near the notched corner, so that the pipe segment is located between the movable plate 430 and the lower fixed plate 440;

[0102] (5) The assembled bottom plate 210, front side plate 220 and side plate 240 are placed at the missing corner, so that the front side plate 220 is close to the inner arc surface of the segment, and then the rear side plate 230 is assembled with the bottom plate 210, and the up-down and left-right positions of the casting enclosure structure 200 are adjusted, so that the concavo-convex grooves on the bottom plate 210 are matched and engaged with the concavo-convex grooves on the circumferential butt joint surface of the segment, and the concavo-convex grooves on the side plate 240 are matched and engaged with the concavo-convex grooves on the circumferential butt joint surface of the segment, so that the casting enclosure structure 200 is covered at the missing corner;

[0103] (6) Control the extension of the rod of the hydraulic cylinder 410 on the load-bearing frame to move the movable plate 430 downward relative to the lower fixed plate 440, and at the same time rotate the push rod 470 of the tightening mechanism to move the push rod 470 toward the side plate 240 of the casting enclosure 200, so that the pipe segment and the casting enclosure 200 are gradually clamped between the movable plate 430 and the lower fixed plate 440, and at the same time, the pouring enclosure 200 is tightened laterally by the push rod 470;

[0104] (7) Connect the grouting pipe to the grouting port 211 of the casting enclosure structure 200, inject the polymer repair mortar in the slurry sealing cylinder 320 into the casting cavity through the air compressor 310, and stop grouting when the guide groove on the side plate 240 overflows the polymer repair mortar;

[0105] (8) Turning on the vibrator 480 to vibrate the polymer repair mortar in the casting cavity to make the polymer repair mortar in the casting cavity dense, during which the air is discharged from the casting cavity through the overflow groove 260;

[0106] (9) The polymer repair mortar in the slurry sealing cylinder 320 is injected into the pouring cavity again through the air compressor 310. When the guide groove on the side plate 240 overflows with the polymer repair mortar again, the grouting is stopped, the valve is closed, and the grouting system at the front end of the grouting pipe valve is removed;

[0107] (10) When the polymer repair mortar in the casting cavity solidifies and hardens to the required strength, the repair device is removed and the excess solidified body formed at the overflow groove 260 is ground off with an angle grinder to complete the corner defect repair.

[0108] In the description of the present invention, it is necessary to understand that the terms "upper", "lower", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "axial", "radial", "circumferential" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention.

[0109] In the present invention, unless otherwise clearly specified and limited, the terms "set", "install", "connect", "connect", "fix" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral one; it can be directly connected, or indirectly connected through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0110] The above specific implementation manner cannot be used as a limitation on the protection scope of the present invention. For those skilled in the art, any substitution, improvement or change made to the implementation manner of the present invention falls within the protection scope of the invention.

[0111] The matters not described in detail in the present invention are all known technologies to those skilled in the art.

Claims

1. A tunnel segment missing corner repair device, It is characterized in that include: Drilling a plurality of implantation holes on the wall surface of the missing corner; An anchor, one end of which is placed in the implantation hole and the other end is located at the notched corner of the pipe segment, and the implantation hole is used to fill the rebar glue; A casting enclosure structure, which is covered on the outside of the missing corner of the pipe segment and is used to enclose a casting cavity matching the shape of the pipe segment at the missing corner; A grouting assembly, the grouting assembly is used to inject polymer repair mortar into the casting cavity; A fastening and positioning assembly, wherein the fastening and positioning assembly is used to position the pouring enclosure structure on the pipe segment; The pouring enclosure structure is surrounded by a bottom plate, a front side plate, a rear side plate and a side plate; the bottom plate is used to support the axial butt joint surface of the pipe segment adjacent to the missing corner, the plate surface of the bottom plate is provided with concave and convex grooves matching the axial butt joint surface of the pipe segment, and a grouting port for communicating with the grouting assembly is opened on the bottom plate; The front side plate is used to abut against the inner arc surface of the tube segment adjacent to the notched corner, the lower end surface of the front side plate is supported on the edge of the plate surface of the bottom plate, and the front side plate is fastened to the bottom plate by bolts; The rear side plate is used to abut against the outer arc surface of the tube segment adjacent to the notched corner, the rear end surface of the bottom plate abuts against the edge of the plate surface of the rear side plate, and the bottom plate and the rear side plate are fastened and connected by bolts; The side plate is used to abut against the circumferential butt joint surface of the tube sheet adjacent to the notched corner. The plate surface of the side plate is provided with a concave-convex groove matching the circumferential butt joint surface of the tube sheet. The lower end surface of the side plate is supported on the plate surface edge of the bottom plate, and the side plate is fastened to the bottom plate by bolts. The front end surface and the rear end surface of the side plate are respectively abutted against the plate surface edges of the front side plate and the rear side plate, and the front end surface and the rear end surface of the side plate are both provided with a clamping protrusion, and the plate surfaces of the front side plate and the rear side plate are both provided with a clamping groove matching the clamping protrusion. The side plate is assembled and connected with the front side plate and the rear side plate respectively by matching the corresponding clamping protrusion and the clamping groove. The side plates are formed by splicing a number of unit plates up and down, and the adjacent unit plates are fastened and connected by bolts. At least the unit plates arranged at the top are provided with overflow grooves, and the overflow grooves are used to conduct the casting cavity with the outside.

2. The tunnel segment missing corner repair device according to claim 1, It is characterized in that The unit plate comprises a first unit plate and a second unit plate, the first unit plate and the second unit plate are spliced ​​alternately up and down, each of the first unit plate and the second unit plate is provided with a first bolt hole and a second bolt hole, the first bolt hole passes through the upper end surface and the lower end surface of the unit plate, the second bolt hole extends downward from the upper end surface of the unit plate, the first bolt hole on the first unit plate corresponds to the position of the second bolt hole on the second unit plate, and the second bolt hole on the first unit plate corresponds to the position of the first bolt hole on the second unit plate; The first unit plate is connected to the second unit plate below it by a first bolt, and the first bolt passes through a first bolt hole on the first unit plate and is threadedly connected to a second bolt hole on the second unit plate below it; The first unit plate is connected to the second unit plate above it through a second bolt. The second bolt passes through a first bolt hole on the second unit plate above and is threadedly connected to a second bolt hole on the first unit plate.

3. The tunnel segment corner-cut repairing device according to claim 1, It is characterized in that The casting enclosure structure also includes a blocking strip for embedding in the overflow trough. The blocking strip has various length specifications. After the blocking strip is embedded in the overflow trough, the surface of the blocking strip is flush with the surface of the unit board adjacent to the overflow trough.

4. The tunnel segment corner-cut repair device according to claim 3, It is characterized in that The cross-sectional shape of the overflow groove is a closed trapezoid or a closed arc, and the cross-sectional shape of the sealing strip matches the cross-sectional shape of the overflow groove.

5. The tunnel segment missing corner repair device according to claim 1, It is characterized in that Sealing strips are embedded on the contact surface between the front side plate and the bottom plate, on the contact surface between the rear side plate and the bottom plate, and on the contact surface between the side plate and the bottom plate.

6. The tunnel segment chipping repair device according to claim 1, It is characterized in that The grouting assembly includes an air compressor and a slurry sealing cylinder. The top of the slurry sealing cylinder is connected to the air compressor through an air inlet pipe, and the bottom of the slurry sealing cylinder is connected to the grouting port through a grouting pipe. Valves are respectively provided on the air inlet pipe and the grouting pipe.

7. The tunnel segment missing corner repair device according to claim 1, It is characterized in that The tightening and positioning assembly comprises a load-bearing frame and a tightening mechanism; The load-bearing frame comprises: An upper fixed plate, a movable plate and a lower fixed plate are arranged in sequence, the upper fixed plate and the lower fixed plate are fixedly connected by a plurality of tie rods, a through hole is provided on the movable plate, and the tie rods freely pass through the through hole on the movable plate, a plate surface of the movable plate is provided with a concave-convex groove matching the axial butt surface of the pipe segment, and a notch corresponding to the grouting port is provided on the lower fixed plate; A hydraulic cylinder, wherein the cylinder body of the hydraulic cylinder is fixed on the movable plate, and the cylinder rod of the hydraulic cylinder is connected to the upper fixed plate; the bottom plate of the casting enclosure structure is placed on the lower fixed plate, and the pipe segment and the casting enclosure structure are clamped between the movable plate and the lower fixed plate under the thrust of the hydraulic cylinder; The tightening mechanism comprises: A base installed at the bottom of the pull rod, wherein the base is provided with threaded holes: A push rod is provided with an external thread matching with a threaded hole on the base, the push rod is threadedly connected in the threaded hole on the base, and the end of the push rod abuts against a side plate of the casting enclosure structure.

8. The tunnel segment missing corner repair device according to claim 7, It is characterized in that Also included is a vibrator, which is mounted on the bottom of the lower fixing plate.

9. A repair process using the tunnel segment corner-cut repair device according to claim 7, It is characterized in that The steps include: (1) Drill an implant hole on the wall surface of the notched corner of the segment, install an anchor in the implant hole, with the outer end of the anchor located at the notched corner of the segment, and fill the implant hole with anchor glue; (2) Determine the size of the side panels according to the size of the missing corners, select the required number of unit panels to form the side panels, and the unit panels adjacent to the top of the missing corners must be provided with overflow grooves, through which the pouring cavity is connected to the outside. The overflow grooves of other parts must be sealed with sealing strips; (3) Assemble the front side panel, side panel and bottom panel; (4) The missing corner of the segment is suspended above the ground, and the load-bearing frame is pre-installed on the segment near the missing corner so that the segment is located between the movable plate and the lower fixed plate; (5) Place the assembled bottom plate, front side plate and side plate at the missing corner, so that the front side plate is against the inner arc surface of the segment, and then assemble the rear side plate with the bottom plate, and adjust the up and down and left and right positions of the casting enclosure structure, so that the concave and convex grooves on the bottom plate are matched and engaged with the concave and convex grooves on the circumferential butt joint surface of the segment, and the concave and convex grooves on the side plate are matched and engaged with the concave and convex grooves on the circumferential butt joint surface of the segment, so that the casting enclosure structure is covered at the missing corner; (6) Control the extension of the hydraulic cylinder rod on the load-bearing frame to move the movable plate downward relative to the lower fixed plate, and at the same time rotate the push rod of the tightening mechanism to move the push rod toward the side plate of the casting enclosure structure, so that the pipe segment and the casting enclosure structure are gradually clamped between the movable plate and the lower fixed plate, and at the same time, the casting enclosure structure is tightened laterally by the push rod; (7) Connect the grouting pipe to the grouting port of the casting enclosure structure, inject the polymer repair mortar in the slurry sealing tube into the casting cavity through the air compressor, and stop grouting when the guide groove on the side plate overflows with the polymer repair mortar; (8) Turning on the vibrator to vibrate the polymer repair mortar in the casting cavity to make the polymer repair mortar in the casting cavity dense, and in this process, air is discharged from the casting cavity through the overflow groove; (9) The polymer repair mortar in the slurry sealing cylinder is injected into the pouring cavity again through the air compressor, and the grouting is stopped when the guide groove on the side plate overflows with the polymer repair mortar again; (10) When the polymer repair mortar in the casting cavity solidifies and hardens to the required strength, remove the repair device and use an angle grinder to grind off the excess solidified body formed at the overflow groove to complete the corner repair.