Semiconductor device and method for manufacturing the same

By forming and removing oxide layers in different regions in the trench of semiconductor devices, the problems of parasitic capacitance and dynamic power consumption in the prior art are solved, the reliability of the device and switching speed are improved, and the risk of breakdown is reduced.

CN118629872BActive Publication Date: 2024-11-15BEIJING ZHONGKE XINWEITE SCI & TECH DEV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411095347.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-08-09
Publication Date
2024-11-15
Estimated Expiration
2044-08-09

AI Technical Summary

Technical Problem

In semiconductor devices, the prior art is difficult to effectively improve the reliability of the device, especially to prevent the possibility of device breakdown while reducing parasitic capacitance and dynamic power consumption.

Method used

By forming a sacrificial layer and a first mask layer in different areas in the trench, and removing the sacrificial layer, the first oxidation part is prepared, and the first mask layer is removed after the first oxidation part is prepared to form a second oxidation part. , the thickness of the second oxide portion is smaller than the first oxide portion to reduce the parasitic capacitance of the gate and drain, and cover the bottom wall and the trench corners to reduce the concentration of the electric field.

Benefits of technology

It effectively reduces the parasitic capacitance and dynamic power consumption of semiconductor devices, improves the switching speed and reliability of the device, and reduces the possibility of breakdown caused by the concentration of electric fields at the corners of the trench.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118629872B_ABST
    Figure CN118629872B_ABST
Patent Text Reader

Abstract

The present application relates to a semiconductor device and a method for preparing the same. The method for preparing the semiconductor device comprises the following steps: forming a groove on one side of an epitaxial layer, the groove comprising a bottom wall and a side wall, the side wall comprising a first region and a second region, the first region being located between the second region and the bottom wall. Forming a sacrificial layer in the groove, the sacrificial layer covering the bottom wall and the first region. Forming a first mask layer on at least the surface of the second region. Removing the sacrificial layer, and forming a first oxide portion on the bottom wall and the first region. Removing the first mask layer, and forming a second oxide portion in the second region, the thickness of the first oxide portion being greater than the thickness of the second oxide portion, the first oxide portion and the second oxide portion forming a gate oxide layer. The present application can improve the reliability of semiconductor devices.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of semiconductor devices, and in particular to a semiconductor device and a method for preparing the same. Background Art

[0002] Metal Oxide Semiconductor Field Effect Transistor (MOSFET) has the characteristics of high switching speed, high withstand voltage, low on-resistance, wide safe operating area and good thermal stability. It is widely used in power integrated circuits and power integrated systems such as switching power supplies, automotive electronics, aerospace, etc.

[0003] In the development of MOSFET device technology, how to improve the reliability of semiconductor devices has always been a research direction in semiconductor device technology. Summary of the invention

[0004] The semiconductor device and the method for manufacturing the same provided by the embodiments of the present application can improve the reliability of the semiconductor device.

[0005] In the first aspect, a method for preparing a semiconductor device is proposed according to an embodiment of the present application, and the method for preparing a semiconductor device includes the following steps: forming a groove on one side of an epitaxial layer, the groove including a bottom wall and a side wall, the side wall including a first region and a second region, and the first region is located between the second region and the bottom wall; forming a sacrificial layer in the groove, the sacrificial layer covering the bottom wall and the first region; forming a first mask layer on the surface of at least the second region; removing the sacrificial layer, and forming a first oxide portion on the bottom wall and the first region; removing the first mask layer, and forming a second oxide portion on the second region, the thickness of the first oxide portion is greater than the thickness of the second oxide portion, and the first oxide portion and the second oxide portion form a gate oxide layer.

[0006] According to a first aspect of an embodiment of the present application, the step of forming a first mask layer on the surface of at least the second region includes: forming a first transition portion on the surface of the second region; forming a first prefabricated mask layer on a side of the first transition portion facing away from the second region and on a side of the sacrificial layer facing away from the bottom wall; removing the first prefabricated mask layer on a side of the sacrificial layer facing away from the bottom wall to form a first mask portion with the first prefabricated mask layer on a side of the first transition portion facing away from the second region, the first transition portion and the first mask portion forming a first mask layer, and the material of the first transition portion is different from the material of the first mask portion.

[0007] According to a first aspect of the embodiment of the present application, the material of the first transition portion includes silicon oxide, and the material of the first mask portion includes silicon nitride.

[0008] According to a first aspect of the embodiment of the present application, the thickness of the first transition portion is smaller than the thickness of the first oxidized portion.

[0009] According to a first aspect of an embodiment of the present application, the step of forming a groove on one side of the epitaxial layer includes: forming a second mask layer on a surface of one side of the epitaxial layer, the second mask layer including a second mask portion and an opening, the opening passing through the second mask layer; etching the epitaxial layer exposed by the opening to form a groove.

[0010] According to a first aspect of the embodiment of the present application, the second mask layer includes a second mask portion and a second transition portion, and the second transition portion is located between the second mask portion and the epitaxial layer.

[0011] According to the first aspect of the embodiment of the present application, it also includes: forming a doping portion on one side of the epitaxial layer, the orthographic projection of the doping portion along the first direction is located within the orthographic projection of the second region along the first direction, and the first direction is perpendicular to the thickness direction of the epitaxial layer.

[0012] According to the first aspect of the embodiment of the present application, the step of forming a doping portion on one side of the epitaxial layer includes: forming a first doping portion, a second doping portion and a third doping portion in sequence on one side of the epitaxial layer, the first doping portion covers the second doping portion and the third doping portion, the third doping portion is located on the side of the second doping portion that is away from the groove, the second doping portion and the epitaxial layer are both of the first doping type, the first doping portion and the third doping portion are both of the second doping type, and the orthographic projection of the first doping portion along the first direction is located within the orthographic projection of the second region along the first direction.

[0013] According to the first aspect of the embodiment of the present application, it also includes: forming a source conductive layer on one side of the epitaxial layer along the thickness direction of the epitaxial layer, the source conductive layer covers the groove, and the source conductive layer is electrically connected to the doped part.

[0014] According to the first aspect of the embodiment of the present application, it also includes: forming a gate on the side of the gate oxide layer facing away from the trench, and the gate is located in the trench.

[0015] In a second aspect, according to an embodiment of the present application, a semiconductor device is proposed, which is manufactured using the semiconductor device manufacturing method of any of the aforementioned embodiments.

[0016] According to the semiconductor device and its preparation method provided by the present application, a sacrificial layer and a first mask layer are formed in different regions in the groove, and a first oxide portion is prepared after removing the sacrificial layer. After the first oxide portion is prepared, the first mask layer is removed, and a second oxide portion is prepared. Since the thickness of the second oxide portion is less than the thickness of the first oxide portion, the second oxide portion has less influence on the first oxide portion during the preparation process. The first oxide portion covers the bottom wall to reduce the parasitic capacitance of the gate and the drain, and reduces the influence on the switching speed and dynamic power consumption of the semiconductor device. The first oxide portion also covers the first region, so that the first oxide portion covers the groove corner where the bottom wall and the first region are connected, thereby reducing the possibility of the semiconductor device being broken down due to the electric field concentration at the groove corner, and improving the reliability of the semiconductor device. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] The features, advantages and technical effects of exemplary embodiments of the present application will be described below with reference to the accompanying drawings.

[0018] Figure 1 A schematic cross-sectional structure diagram of a semiconductor device provided in some embodiments of the present application;

[0019] Figure 2 A flowchart of a method for manufacturing a semiconductor device provided in some embodiments of the present application;

[0020] Figures 3 to 10 A schematic diagram of the process structure of a method for manufacturing a semiconductor device provided in some embodiments of the present application.

[0021] Marking Description:

[0022] 100, epitaxial layer; 200, gate oxide layer; 300, gate; 400, drain conductive layer; 500, insulating layer; 600, source conductive layer; 700, doping part; 710, first doping part; 720, second doping part; 730, third doping part;

[0023] 10. The first oxidation section;

[0024] 20. Second oxidation section;

[0025] 30, groove; 31, bottom wall; 32, side wall; 311, first area; 312, second area;

[0026] 40. Sacrificial layer;

[0027] 50. first mask layer; 51. first transition portion; 52. first mask portion;

[0028] 60. second mask layer; 61. second transition portion; 62. second mask portion;

[0029] PM1, a first pre-mask layer;

[0030] X, first direction; Z, thickness direction.

[0031] In the drawings, the same reference numerals are used for the same components. The drawings are not drawn to scale. DETAILED DESCRIPTION

[0032] The features and exemplary embodiments of various aspects of the present invention will be described in detail below. In order to make the purpose, technical solutions and advantages of the present application clearer, the present application will be further described in detail below in conjunction with the accompanying drawings and specific embodiments. It should be understood that the specific embodiments described herein are only intended to explain the present application, rather than to limit the present application. For those skilled in the art, the present application can be implemented without the need for some of these specific details. The following description of the embodiments is only to provide a better understanding of the present application by illustrating the examples of the present application.

[0033] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, the elements defined by the statement "include..." do not exclude the presence of other identical elements in the process, method, article or device including the elements.

[0034] In order to better understand the present application, on the one hand, the following Figures 1 to 10 A semiconductor device and a method for manufacturing the same according to an embodiment of the present application are described in detail.

[0035] Figure 1 A schematic cross-sectional structure diagram of a semiconductor device provided for some embodiments of the present application.

[0036] like Figure 1As shown, an embodiment of the present application provides a semiconductor device, which includes a drain conductive layer 400, an epitaxial layer 100, and a source conductive layer 600 stacked in sequence. The side of the epitaxial layer 100 facing away from the drain conductive layer 400 includes a trench 30, a doped portion 700 located on the side of the trench 30, and a gate 300 structure located in the trench 30. The gate 300 structure includes a gate oxide layer 200 and a gate 300. The gate oxide layer 200 includes a first oxide portion 10 and a second oxide portion 20, and the first oxide portion 10 covers the bottom wall 31 of the trench 30 and the first region 311 of the side wall 32. The second oxide portion 20 covers the second region 312 of the trench 30.

[0037] Optionally, the semiconductor device may include a lateral conductive semiconductor power device and a vertical conductive semiconductor power device. The embodiments of the present application are described below by taking a vertical conductive semiconductor power device as an example. For example, a drain, an epitaxial layer 100, a gate 300, and a source are sequentially stacked along a thickness direction Z of the semiconductor device.

[0038] Optionally, the semiconductor device includes a vertical double diffusion metal-oxide-semiconductor field effect transistor (VDMOS) and an insulated gate bipolar transistor (IGBT). VDMOS includes silicon-based VDMOS and silicon carbide-based VDMOS.

[0039] Optionally, the overall shape of the semiconductor device may be a strip, a block, or other shapes. For example, the shape of the semiconductor device may be a cuboid, a cube, a pentagonal strip, or the like.

[0040] Optionally, the shape of the epitaxial layer 100 may be the same as the shape of the semiconductor device, for example, the shape of the epitaxial layer 100 is a cuboid, and the center of the epitaxial layer 100 may be the geometric center of the cuboid. Optionally, the projection shape of the epitaxial layer 100 along the thickness direction Z may include a rectangle, a square, a pentagon or other polygons, and the doped regions may be symmetrically distributed about the center point of the epitaxial layer 100. Taking the projection shape of the epitaxial layer 100 along the thickness direction Z as an example of a rectangle, the line connecting the midpoints of the two long opposite sides of the rectangle is the first straight line, and the doped portion 700 is symmetrically arranged along the first straight line, that is, the epitaxial layer 100 is divided into two parts along the first straight line, each part includes the doped portion 700, and the doped portion 700 in each part includes a first doped portion 710, a second doped portion 720 and a third doped portion 730.

[0041] Optionally, the second doping portion 720 and the third doping portion 730 are arranged side by side along the first direction X, and the contact portion between the second doping portion 720 and the third doping portion 730 forms a PN junction. The first direction X intersects with the thickness direction of the epitaxial layer 100. The third doping portion 730 is located on the side of the second doping portion 720 facing away from the trench 30.

[0042] The thickness of the first oxide portion 10 is greater than the thickness of the second oxide portion 20. It is understood that the "thickness" here refers to the minimum dimension of the first oxide portion 10 and the second oxide portion 20 perpendicular to the direction of their coverage surface. For example, the thickness of the first oxide portion 10 includes a first part and a second part, the first part of the first oxide portion 10 covers the bottom wall 31, and the second part of the first oxide portion 10 covers the first area 311. The thickness of the first part is the minimum dimension perpendicular to the direction of the bottom wall 31. The thickness of the second part is the minimum dimension perpendicular to the direction of the first area 311. The thickness of the second oxide portion 20 is the minimum dimension perpendicular to the direction of the second area 312. Optionally, the first oxide portion 10 can be a uniform film layer, that is, the first part and the second part have the same thickness. The thickness of the second oxide portion 20 is less than the thickness of the first part of the first oxide portion 10. The thickness of the second oxide portion 20 is less than the thickness of the second part of the first oxide portion 10.

[0043] Optionally, the material of the gate 300 includes polysilicon.

[0044] Optionally, an insulating layer 500 is disposed between the gate 300 and the source conductive layer 600 .

[0045] Optionally, the doping concentration of the first doping portion 710 is less than the doping concentration of the third doping portion 730 .

[0046] Optionally, the second doping portion 720 is disposed adjacent to the second oxidized portion 20 . The third doping portion 730 may be located on a side of the second doping portion 720 facing away from the second oxidized portion 20 .

[0047] Figure 2 A flowchart of a method for manufacturing a semiconductor device is provided for some embodiments of the present application. Figures 3 to 10 A schematic diagram of the process structure of a method for manufacturing a semiconductor device provided in some embodiments of the present application.

[0048] like Figure 2 As shown, an embodiment of the present application provides a method for preparing a semiconductor device, which comprises the following steps.

[0049] S100 , forming a trench 30 on one side of the epitaxial layer 100 , wherein the trench 30 includes a bottom wall 31 and a side wall 32 , wherein the side wall 32 includes a first region 311 and a second region 312 , and the first region 311 is located between the second region 312 and the bottom wall 31 .

[0050] Specifically, Figure 3 As shown, the groove 30 is formed by a depression on one side of the epitaxial layer 100. The groove 30 can be formed by etching by photolithography or other processes. The first region 311 and the second region 312 are two adjacent regions, and the first region 311 is connected to the surface of the bottom wall 31.

[0051] Optionally, the epitaxial layer 100 may be of a first doping type.

[0052] Optionally, the first doping type is opposite to the second doping type, which can be understood as the first doping type is one of N-type or P-type, and the second doping type is the other of N-type or P-type. For example, when the first doping type is N-type, the second doping type is P-type. For another example, when the first doping type is P-type, the second doping type is N-type.

[0053] The embodiment of the present application is described by taking the first doping type as N type and the second doping type as P type as an example. In other embodiments, the first doping type may be P type and the second doping type may be N type.

[0054] Optionally, in the embodiment of the present application and hereinafter, one side surface of the epitaxial layer 100 along the thickness direction Z is referred to as the first surface, and the trench 30 is formed by a depression of the first surface.

[0055] S200 , forming a sacrificial layer 40 in the trench 30 , wherein the sacrificial layer 40 covers the bottom wall 31 and the first region 311 .

[0056] Specifically, Figure 4 As shown, in the process of forming the sacrificial layer 40, the sacrificial layer 40 to be processed can be formed on the first surface and in the groove 30 first, and then the sacrificial layer 40 to be processed except the first surface and a portion of the sacrificial layer 40 to be processed in the groove 30 are removed together. Since the thickness of the sacrificial layer 40 to be processed in the groove 30 is greater than the thickness of the sacrificial layer 40 to be processed on the first surface, under the same etching rate, a portion of the sacrificial layer 40 to be processed near the bottom wall 31 of the groove 30 is retained to form the sacrificial layer 40.

[0057] Optionally, the size of the sacrificial layer 40 along the thickness direction Z of the epitaxial layer 100 and the size of the first oxide part 10 along the thickness direction Z of the epitaxial layer 100 may be the same.

[0058] Optionally, the material of the sacrificial layer 40 includes silicon oxide. For example, the material of the sacrificial layer 40 includes silicon dioxide.

[0059] S300, such as Figure 5 and Figure 6 As shown, a first mask layer 50 is formed at least on the surface of the second region 312 .

[0060] Optionally, the material of the first mask layer 50 is different from the material of the sacrificial layer 40. For example, the material of the first mask layer 50 includes silicon nitride.

[0061] S400 , removing the sacrificial layer 40 , and forming a first oxidized portion 10 on the bottom wall 31 and the first region 311 .

[0062] Specifically, Figure 7 and Figure 8 As shown, the sacrificial layer 40 can be removed by wet etching to expose the bottom wall 31 and the first region 311, and then the first oxidized portion 10 is formed on the bottom wall 31 and the first region 311 by a first thermal oxidation process. It can be understood that when the first thermal oxidation process is performed on the bottom wall 31 and the first region 311, the second region 312 is shielded by the first mask portion 52, so that the second region 312 is not in contact with the prepared material in the first thermal oxidation process, thereby reducing the possibility of the second region 312 being thermally oxidized.

[0063] S500 , removing the first mask layer 50 , and forming a second oxide portion 20 in the second region 312 , wherein the thickness of the first oxide portion 10 is greater than that of the second oxide portion 20 , and the first oxide portion 10 and the second oxide portion 20 form a gate oxide layer 200 .

[0064] Specifically, Fig. 9 and Fig.10 As shown, the first mask layer 50 can be removed by wet etching to expose the second region 312, and then the second oxide portion 20 is formed in the second region 312 by a second thermal oxidation process. It can be understood that since the first oxide portion 10 has been formed in the bottom wall 31 and the first region 311, in the process of preparing the second oxide portion 20, the first oxide portion 10 and the preparation materials in the second thermal oxidation process have little effect on the first oxide portion 10, so that the second oxide portion 20 can be prepared without shielding the first oxide portion 10.

[0065] In some other embodiments, step S500 may be performed first, and then step S400. It is understandable that when step S500 is performed first, and then step S400 is performed, after the second oxide portion 20 is prepared, the mask material may be covered on the side of the second oxide portion 20 facing away from the second region 312, and then after step S400 is performed, after the first oxide portion 10 is prepared, the mask material on the side of the second oxide portion 20 facing away from the second region 312 is removed.

[0066] Optionally, the oxide portions of different thicknesses can be achieved by changing the parameters of the first thermal oxidation process and the second thermal oxidation process. For example, the first thermal oxidation process and the second thermal oxidation process have different parameters in terms of preparation time, preparation material concentration, and preparation temperature, or a combination of several parameters.

[0067] In the embodiment of the present application, the first oxide portion 10 is prepared by forming a sacrificial layer 40 and a first mask layer 50 in different regions in the groove 30, and removing the sacrificial layer 40. After the first oxide portion 10 is prepared, the first mask layer 50 is removed, and the second oxide portion 20 is prepared. Since the thickness of the second oxide portion 20 is less than the thickness of the first oxide portion 10, the second oxide portion 20 has less influence on the first oxide portion 10 during the preparation process. The first oxide portion 10 covers the bottom wall 31 to reduce the parasitic capacitance of the gate 300 and the drain, and reduce the influence on the switching speed and dynamic power consumption of the semiconductor device. The first oxide portion 10 also covers the first region 311, so that the first oxide portion 10 covers the corner of the groove 30 where the bottom wall 31 and the first region 311 are connected, thereby reducing the possibility of the semiconductor device being broken down due to the electric field concentration at the corner of the groove 30, and improving the reliability of the semiconductor device.

[0068] In some optional embodiments, the step of forming the first mask layer 50 at least on the surface of the second region 312 includes:

[0069] S310 , forming a first transition portion 51 on the surface of the second region 312 .

[0070] Specifically, Figure 5 As shown, the material of the first transition portion 51 may be silicon oxide. For example, the material of the first transition portion 51 is silicon dioxide. The first transition portion 51 may be prepared by a thermal oxidation process.

[0071] Optionally, the orthographic projection of the first transition portion 51 in the second region 312 may be located within the first transition portion 51 .

[0072] Optionally, the orthographic projection of the first transition portion 51 and the second region 312 are arranged to overlap.

[0073] S320 , forming a first pre-mask layer PM1 on a side of the first transition portion 51 facing away from the second region 312 and on a side of the sacrificial layer 40 facing away from the bottom wall 31 .

[0074] Specifically, Figure 5 As shown, the first pre-mask layer PM1 may be covered on the first surface, the side of the sacrificial layer 40 facing away from the bottom wall 31 , and the side of the first transition portion 51 facing away from the second region 312 .

[0075] Optionally, the orthographic projection of the first transition portion 51 in the second region 312 may be located within the orthographic projection of the first pre-mask layer PM1 in the second region 312 .

[0076] Optionally, the orthographic projection of the first transition portion 51 in the second region 312 and the orthographic projection of the first pre-mask layer PM1 in the second region 312 are overlapped.

[0077] S330, remove the first pre-fabricated mask layer PM1 on the side of the sacrificial layer 40 facing away from the bottom wall 31 so that the first pre-fabricated mask layer PM1 on the side of the first transition portion 51 facing away from the second region 312 forms a first mask portion 52, and the first transition portion 51 and the first mask portion 52 form a first mask layer 50. The material of the first transition portion 51 is different from the material of the first mask portion 52.

[0078] Specifically, Figure 6 As shown, the first pre-mask layer PM1 on the side of the sacrificial layer 40 facing away from the bottom wall 31 and the first pre-mask layer PM1 on the first surface can be etched by dry etching.

[0079] It can be understood that during the etching process, since dry etching can etch the entire film layer to the same thickness, the first prefabricated mask layer PM1 covering the second area 312 protrudes from the first surface along the thickness direction Z of the epitaxial layer 100. During the etching process, the dry etching can etch away the first prefabricated mask layer PM1 covering the second area 312 protruding from the first surface along the thickness direction Z of the epitaxial layer 100, so that the formed first mask portion 52 covers the second area 312.

[0080] Optionally, the hardness of the first mask portion 52 is greater than the hardness of the first transition portion 51 .

[0081] In these optional embodiments, by providing the first transition portion 51, the combination of the first mask portion 52 and the side wall 32 of the groove 30 is facilitated, and the possibility of separation of the first mask portion 52 and the side wall 32 of the groove 30 is reduced. The first mask portion 52 can be used as a shield to reduce the possibility that other subsequent preparation processes affect the side wall 32 in the second area 312 of the groove 30, resulting in poor thickness uniformity of the oxide portion in the second area 312.

[0082] In some optional embodiments, the material of the first transition portion 51 includes silicon oxide, and the material of the first mask portion 52 includes silicon nitride.

[0083] In some optional embodiments, the thickness of the first transition portion 51 is smaller than the thickness of the first oxidized portion 10 .

[0084] Optionally, the thickness of the first transition portion 51 is d, 100 angstroms (A) ≤ d ≤ 400 angstroms (A). Exemplarily, d = 100 angstroms (A), d = 130 angstroms (A), d = 150 angstroms (A), d = 170 angstroms (A), d = 200 angstroms (A), d = 250 angstroms (A), d = 300 angstroms (A) or d = 400 angstroms (A).

[0085] Optionally, the thickness of the first oxide portion 10 is D, 2000 angstroms (A) ≤ D ≤ 3000 angstroms (A). Exemplarily, D = 2000 angstroms (A), D = 2300 angstroms (A), D = 2500 angstroms (A), D = 2700 angstroms (A) or D = 3000 angstroms (A).

[0086] In the embodiment of the present application, the above-mentioned setting is helpful to reduce the possibility that the first transition portion 51 etches the thickness of the first oxide portion 10 during the etching process, resulting in the first oxide portion 10 being too thin, thereby improving the shielding effect of the first oxide portion on the gate 300 and the drain, further reducing the parasitic capacitance between the gate 300 and the drain, and improving the switching speed and dynamic power consumption of the semiconductor device.

[0087] In some optional embodiments, the step of forming the trench 30 on one side of the epitaxial layer 100 includes:

[0088] S110, such as Figure 3 As shown, a second mask layer 60 is formed on one side surface of the epitaxial layer 100 . The second mask layer 60 includes a second mask portion 62 and an opening. The opening passes through the second mask layer 60 .

[0089] Specifically, the first surface may be covered with a second pre-mask layer, and the second pre-mask layer may be patterned to form the second mask layer 60 .

[0090] Optionally, the second mask portion 62 is disposed around the opening. Alternatively, there are two second mask portions 62 , and the opening is located between the two second mask portions 62 .

[0091] S120 , etching the exposed epitaxial layer 100 to form a trench 30 .

[0092] Specifically, Figure 3 As shown, since a second mask portion 62 is provided above the first surface, a portion of the surface blocked by the second mask portion 62 does not contact the etching material, and a portion of the surface not blocked by the second mask portion 62 (i.e., the surface exposed by the opening) contacts the etching material, and the surface in contact with the etching material is etched to form a groove 30, and the surface not in contact with the etching material is retained and can be used as a doping region of the doping portion 700 later.

[0093] In some optional embodiments, the second mask layer 60 includes a second mask portion 62 and a second transition portion 61 , and the second transition portion 61 is located between the second mask portion 62 and the epitaxial layer 100 .

[0094] Optionally, the material of the second transition portion 61 includes silicon oxide. For example, the material of the second transition portion 61 is silicon dioxide.

[0095] Optionally, the material of the second mask portion 62 includes silicon nitride.

[0096] In these optional embodiments, by providing the second transition portion 61, it is beneficial to combine the second mask portion 62 with the first surface, reduce the possibility of separation of the second mask portion 62 and the first surface, and the second mask portion 62 can be used as a shield to reduce the possibility of other subsequent preparation processes affecting the thermal oxidation of the epitaxial layer 100 below the second mask portion 62. Optionally, the preparation of the second mask layer 60 can be between step S100 and step S200.

[0097] In some optional embodiments, the method for preparing a semiconductor device further includes:

[0098] S600 , forming a doped portion 700 on one side of the epitaxial layer 100 , wherein the orthographic projection of the doped portion 700 along the first direction X is located within the orthographic projection of the second region 312 along the first direction X, and the first direction X is perpendicular to the thickness direction Z of the epitaxial layer 100 .

[0099] Specifically, a predetermined doping material can be implanted into a preset position of the epitaxial layer 100 by an ion implantation process to form a PN junction and other functional modules of the semiconductor device. Optionally, a channel can be formed in the contact area between the second region 312 and the doping portion 700. Since the thickness of the second oxide portion 20 is less than the thickness of the first oxide portion 10, the shielding effect of the second oxide portion 20 is less than the shielding effect of the first oxide portion 10, thereby improving the switching speed of the semiconductor device.

[0100] Optionally, an orthographic projection of the doped portion 700 along the first direction X and an orthographic projection of the second region 312 along the first direction X are overlapped. Optionally, the first direction X may be a direction in which the doped portion 700 and the gate 300 are arranged side by side.

[0101] In some optional embodiments, the step of forming the doped portion 700 on one side of the epitaxial layer 100 includes:

[0102] S610, a first doping portion 710, a second doping portion 720 and a third doping portion 730 are sequentially formed on one side of the epitaxial layer 100, the first doping portion 710 covers the second doping portion 720 and the third doping portion 730, the third doping portion 730 is located on the side of the second doping portion 720 that is away from the groove 30, the second doping portion 720 and the epitaxial layer 100 are both of the first doping type, the first doping portion 710 and the third doping portion 730 are both of the second doping type, and the orthographic projection of the first doping portion 710 along the first direction X is located within the orthographic projection of the second region 312 along the first direction X.

[0103] Specifically, after the gate oxide layer 200 is prepared, the second mask layer 60 can be removed first, and the first doping material can be injected into the area covered by the second mask layer 60 to form the first doping portion 710. Optionally, the first doping material can be injected into a position flush with the junction of the first oxide portion 10 and the second oxide portion 20. Optionally, the first doping material can also be injected into a specific area of ​​the second oxide portion 20 along the thickness direction Z. For example, the first doping material is injected into two-thirds of the size of the second oxide portion 20 along the thickness direction Z.

[0104] After the first doping portion 710 is prepared, the second doping material and the third doping material are respectively implanted from different positions of the area covered by the second mask layer 60 to form the second doping portion 720 and the third doping portion 730 , respectively.

[0105] Optionally, the second doping portion 720 and the third doping portion 730 may form a PN junction.

[0106] Optionally, the first doped portion 710 may form an extension region, thereby weakening the short channel effect.

[0107] In some optional embodiments, the method for preparing a semiconductor device further includes:

[0108] S700 , forming a source conductive layer 600 on one side of the epitaxial layer 100 along the thickness direction Z, wherein the source conductive layer 600 covers the trench 30 and is electrically connected to the doped portion 700 .

[0109] Specifically, before preparing the source conductive layer 600, an insulating layer 500 may be prepared first, and the insulating layer 500 covers the first surface and the gate 300 in the trench 30. Then, the source conductive layer 600 is prepared on the side of the insulating layer 500 facing away from the epitaxial layer 100. Optionally, after the insulating layer 500 is prepared, a hole may be opened in the insulating layer 500 and the epitaxial layer 100 to expose the third doped portion 730. During the preparation of the source conductive layer 600, a portion of the source conductive layer 600 is electrically connected to the third doped portion 730.

[0110] In some optional embodiments, the method for preparing a semiconductor device further includes:

[0111] S800 , forming a gate 300 on a side of the gate oxide layer 200 facing away from the trench 30 , wherein the gate 300 is located in the trench 30 .

[0112] Optionally, the gate 300 may be formed of a polysilicon material, and the gate 300 may be formed by depositing a polysilicon layer and etching the polysilicon layer.

[0113] Optionally, the preparation order of step S800 and step S600 can be prepared in sequence according to the sequence number, or can be reversed. It can be understood that step S800 is before step S700.

[0114] In a second aspect, an embodiment of the present application provides a semiconductor device, which is manufactured using the method for manufacturing a semiconductor device in any of the aforementioned embodiments.

[0115] It should be noted that the semiconductor device provided in the embodiment of the present application has the beneficial effects of the semiconductor device preparation method in any of the aforementioned embodiments. For specific details, please refer to the aforementioned description of the beneficial effects of the semiconductor device preparation method, and the embodiment of the present application will not repeat them.

[0116] Although the present application has been described with reference to preferred embodiments, various modifications may be made thereto and parts thereof may be replaced with equivalents without departing from the scope of the present application. In particular, the various technical features mentioned in the various embodiments may be combined in any manner as long as there are no structural conflicts. The present application is not limited to the specific embodiments disclosed herein, but includes all technical solutions falling within the scope of the claims.

Claims

1. A method for preparing a semiconductor device, characterized in that: include: forming a trench on one side of the epitaxial layer, the trench comprising a bottom wall and a side wall, the side wall comprising a first region and a second region, the first region being located between the second region and the bottom wall; forming a sacrificial layer in the groove, wherein the sacrificial layer covers the bottom wall and the first region; A first mask layer is formed at least on the surface of the second region, wherein a first transition portion is formed on the surface of the second region; a first prefabricated mask layer is formed on a side of the first transition portion facing away from the second region and on a side of the sacrificial layer facing away from the bottom wall; the first prefabricated mask layer on the side of the sacrificial layer facing away from the bottom wall is removed to form a first mask portion on the first prefabricated mask layer on the side of the first transition portion facing away from the second region, the first transition portion and the first mask portion form a first mask layer, and the material of the first transition portion is different from the material of the first mask portion; removing the sacrificial layer, and forming a first oxide portion on the bottom wall and the first region; The first mask layer is removed, and a second oxide portion is formed in the second region, the thickness of the first oxide portion is greater than the thickness of the second oxide portion, and the first oxide portion and the second oxide portion form a gate oxide layer.

2. The preparation method according to claim 1, characterized in that: The material of the first transition portion includes silicon oxide, and the material of the first mask portion includes silicon nitride.

3. The preparation method according to claim 1, characterized in that: The thickness of the first transition portion is smaller than the thickness of the first oxidized portion.

4. The preparation method according to claim 1, characterized in that: The step of forming a trench on one side of the epitaxial layer includes: forming a second mask layer on one side surface of the epitaxial layer, wherein the second mask layer comprises a second mask portion and an opening, wherein the opening penetrates the second mask layer; The epitaxial layer exposed by the opening is etched to form a trench.

5. The preparation method according to claim 4, characterized in that: The second mask layer includes a second mask portion and a second transition portion, and the second transition portion is located between the second mask portion and the epitaxial layer.

6. The preparation method according to claim 1, characterized in that: Also includes: A doped portion is formed on one side of the epitaxial layer, the orthographic projection of the doped portion along a first direction is located within the orthographic projection of the second region along the first direction, and the first direction is perpendicular to the thickness direction of the epitaxial layer.

7. The preparation method according to claim 6, characterized in that: The step of forming a doped portion on one side of the epitaxial layer includes: A first doping portion, a second doping portion and a third doping portion are sequentially formed on one side of the epitaxial layer, the first doping portion covers the second doping portion and the third doping portion, the third doping portion is located on the side of the second doping portion that is away from the groove, the second doping portion and the epitaxial layer are both of the first doping type, the first doping portion and the third doping portion are both of the second doping type, and the orthographic projection of the first doping portion along the first direction is located within the orthographic projection of the second region along the first direction.

8. The preparation method according to claim 6, characterized in that: Also includes: A source conductive layer is formed on one side of the epitaxial layer along a thickness direction of the epitaxial layer, the source conductive layer covers the trench, and the source conductive layer is electrically connected to the doped portion.

9. The preparation method according to claim 1, characterized in that: Also includes: A gate is formed on a side of the gate oxide layer facing away from the trench, and the gate is located in the trench.

10. A semiconductor device, characterized in that: The semiconductor device is manufactured by the method for manufacturing a semiconductor device according to any one of claims 1 to 9.