A sapphire-based multi-parameter composite optical fiber sensor and its preparation method and demodulation method
By using a sapphire multi-parameter composite sensitive chip and a three-cantilever beam structure in the optical fiber sensor, combined with dual F-P cavity interference light signal modulation and demodulation, the problem that traditional optical fiber sensors cannot simultaneously measure multiple parameters in a high-temperature environment is solved, and a high-temperature sensor is achieved. Precise measurement of temperature, pressure and three-axis vibration improves robustness and measurement accuracy.
Patent Information
- Application Number
- CN202411135563.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-19
- Publication Date
- 2024-10-25
- Estimated Expiration
- 2044-08-19
AI Technical Summary
Traditional optical fiber sensors cannot simultaneously measure the temperature, pressure and three-axis vibration signals of a single measuring point in high-temperature environments, resulting in the need for multiple sensors to measure at the same time, which increases structural intrusion and system risks, and cannot guarantee in-situ and real-time performance.
Using a multi-parameter composite sensitive chip based on all-sapphire material, combined with a three-cantilever beam structure and fiber grating, through dual F-P cavity interference light signal modulation and demodulation, a single sensor can simultaneously measure temperature, pressure and three-axis vibration. Using Ceramic cannulas and fiber optic collimators perform signal transmission and processing.
It realizes multi-parameter composite measurement of a single measuring point in a high-temperature environment, reduces the difficulty of sensor processing and packaging, improves high-temperature robustness and measurement accuracy, and adapts to the sensitivity and range requirements of different test environments.
Smart Images

Figure CN118654711B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of optical fiber sensors, and in particular to a sapphire-based multi-parameter composite optical fiber sensor and a preparation method and a demodulation method thereof. Background Art
[0002] There is a general technical demand for high-temperature sensors in the fields of aerospace, oil exploration, and automobile manufacturing, including the measurement of parameters such as high-temperature temperature, high-temperature pressure, and high-temperature vibration, which are used to achieve real-time monitoring and fault diagnosis of key components inside the structure. Fiber optic sensors are widely used in the above fields because of their advantages such as small size, low invasiveness, and resistance to electromagnetic interference, and they do not have the problems of creep and parasitic capacitance that electrical sensors are prone to in high-temperature environments.
[0003] However, for some harsh test scenarios, there are problems such as small structural space, complex flow field, large dynamic range and multi-parameter coupling. Traditional fiber optic sensors cannot achieve multi-parameter composite measurement of a single measuring point while ensuring their high-temperature robustness. Multiple sensors are required for simultaneous measurement, which increases the sensor's invasiveness to the structure and increases systemic risks. It also cannot guarantee the in-situ and real-time performance of the measuring point. Summary of the invention
[0004] In view of the above-mentioned problems, the present invention aims to provide a sapphire-based multi-parameter composite optical fiber sensor and its preparation method and demodulation method, which can meet the requirements of a single sensor for simultaneous measurement of temperature, pressure and three-axis vibration signals of a single measuring point in a high temperature environment.
[0005] In order to achieve the above object, the technical solution adopted by the present invention is as follows:
[0006] A sapphire-based multi-parameter composite optical fiber sensor comprises a packaging shell and a sapphire multi-parameter composite sensitive chip packaged in the packaging shell. The bottom of the sapphire multi-parameter composite sensitive chip is provided with three cantilever beams, and the three axes of the three cantilever beams are connected with optical fiber gratings; the bottom of the packaging shell is provided with a ceramic insert, and an optical fiber collimator is provided in the ceramic insert.
[0007] Furthermore, the sapphire multi-parameter composite sensitive chip includes an upper chip layer, a middle chip layer and a lower chip layer based on all-sapphire materials. The upper chip layer and the middle chip layer constitute a double FP cavity, and the lower chip layer is a hollow structure with three cantilever beams.
[0008] Furthermore, the upper surface of the upper layer of the chip is optically opaque to the C-band incident light, and a cavity is provided on the bottom surface of the upper layer of the chip. The middle layer of the chip is a solid structure with an outer ring and upper and lower bosses, and the upper boss of the middle layer of the chip is bonded to the cavity on the bottom surface of the upper layer of the chip to form an FP cavity.
[0009] Furthermore, the three cantilever beams include an x-axis vibration beam, a y-axis vibration beam and a z-axis vibration beam, each of which is connected to a fiber grating, and the grating regions at the ends of the fiber gratings are connected to the corresponding vibration beams.
[0010] Furthermore, a collimator socket for inserting a fiber collimator and three fiber sockets for passing fiber gratings are provided in the middle of the ceramic insert.
[0011] Furthermore, the optical fiber collimator includes a sapphire lens, a ceramic ferrule and a collimator optical fiber.
[0012] Furthermore, the present invention also includes a method for preparing the sapphire-based multi-parameter composite optical fiber sensor as described above, the preparation method comprising the following steps:
[0013] S1: Preparation of sapphire multi-parameter composite sensitive chip with three cantilever beam structure;
[0014] S2: Connect three fiber Bragg gratings to the three cantilever beam structure;
[0015] S3: Encapsulate the sapphire multi-parameter composite sensitive chip in a packaging shell;
[0016] S4: Insert the ceramic insert into the bottom of the package case and fix it.
[0017] S5: Insert the fiber collimator into the ceramic insert and fix it.
[0018] Furthermore, the specific operation of step S1 includes the following steps:
[0019] S101: Take a clean single-polished sapphire wafer, roughen the non-polished surface to be optically opaque in the C-band, and etch the polished surface of the wafer to form a cavity to obtain a chip upper structure;
[0020] S102: Take a clean double-polished sapphire wafer, and etch shallow annular grooves on the front and back sides of the wafer to form upper and lower convex solid structures to obtain a chip middle layer structure;
[0021] S103: taking another clean double-polished sapphire wafer, and engraving a three-cantilever beam structure on the wafer to obtain a chip lower layer with a three-cantilever beam structure;
[0022] S104: Bonding and dicing the three sapphire wafers in steps S101-S103 to obtain a sapphire multi-parameter composite sensitive chip with a three-cantilever beam structure.
[0023] Furthermore, the present invention also includes a demodulation method for the sapphire-based multi-parameter composite optical fiber sensor as described above, and the multi-parameter demodulation method includes the following steps:
[0024] Step 1: The c-band broadband Gaussian beam is split into four beams of the same wavelength and equal intensity by a 2×4 fiber-coupled beam splitter, and the four beams are respectively incident on a fiber collimator and three fiber gratings with different central wavelengths in the c-band;
[0025] Step 2: The parallel light beam emitted by the fiber collimator is modulated by the sapphire multi-parameter composite sensitive chip to form a double FP cavity interference light and return to the fiber collimator;
[0026] Step 3: The light beams incident on the grating area from the three fiber gratings are narrow-band filtered to obtain three different central peak wavelengths;
[0027] Step 4: Couple the four modulated lights, and then separate and decouple the coupled spectra to obtain the pressure chamber lengths and L 1 , Temperature sensitive cavity length L 2 and the central wavelengths λ of the three fiber Bragg gratings 1 , 2 , 3 ;
[0028] Step 5: Calculate the pressure chamber length L 1 , Temperature sensitive cavity length L 2 and 1 , 2 , 3 The change in pressure and vibration is compensated for by temperature.
[0029] Furthermore, the cavity length L 1 The change in ,
[0030] Cavity length L 2 The change in ,
[0031] λ 1 , 2 , 3 The change in ,
[0032] In the formula, Δ P , Δ T are the changes of external pressure and temperature, E , v , α 1 They are Young's modulus, Poisson's ratio and axial thermal expansion coefficient of sapphire material. R , h1 are the radius and thickness of the pressure sensitive diaphragm, h 2 is the initial thickness of the temperature sensitive cavity, B =1,2,3, , α 2 is the thermo-optic coefficient and thermal expansion coefficient of the fiber Bragg grating, P e is the effective elastic-optical coefficient, ε is the axial strain of the grating region caused by vibration.
[0033] The beneficial effects of the present invention are as follows: compared with the prior art, the present invention has the following improvements:
[0034] 1. The present invention adopts a sapphire multi-parameter composite sensitive chip based on three-layer bonding, and couples the pressure sensitive cavity (formed by bonding the upper and middle layers of the chip), the temperature sensitive cavity (axial thermal expansion of the middle layer of the chip) and the three-axis vibration sensitive element (three cantilever beams in the lower layer of the chip) to the same MEMS chip, which can meet the requirements of the sensor being simultaneously sensitive to temperature-pressure-vibration multi-parameters at the same point in a high temperature environment and a narrow space.
[0035] 2. The middle layer of the sapphire multi-parameter composite sensitive chip in the present invention adopts a supporting structure of an external step and an outer ring. The step is used to provide a boundary for subsequent femtosecond laser chip cutting, and the outer ring is used to provide support for the chip while providing a molten welding surface between the chip and the packaging shell. The above design can significantly reduce the difficulty of processing and packaging the sensor.
[0036] 3. The method for preparing a sapphire multi-parameter composite sensitive chip proposed in the present invention is based on MEMS micromachining. It can not only realize batch preparation of chips through wafer-level bonding to reduce processing costs, but also control the detection range of parameters such as pressure and vibration by adjusting parameters such as the thickness of the pressure-sensitive diaphragm and the size of the three cantilever beams to adapt to test environments with different sensitivity, range and other requirements.
[0037] 4. The present invention adopts a full aluminum oxide structure, and the multi-parameter composite sensitive chip, fiber grating, Bragg fiber grating, and collimator lens are all made of sapphire material (Al 2 O 3 ), the packaging shell, ceramic insert and ceramic core are all alumina ceramic structures, and the high-temperature glue used for bonding is alumina high-temperature resistant inorganic glue. The overall thermal expansion coefficient of the entire sensor probe and the packaging structure tends to be consistent, which can significantly control the thermal stress of the packaging structure and improve the overall high-temperature robustness.
[0038] 5. The sensor signal transmission part of the present invention is completed by a fiber collimator and three fiber gratings. The fiber collimator light beam is injected from the bottom of the chip, modulates the temperature-sensitive cavity and the air cavity, and then returns vertically to the fiber collimator to obtain a dual FP cavity interference signal superimposed by two cosine-like signals of different periods. The three fiber gratings respectively sense the strains in the main vibration directions of the three cantilever beams to determine the vibration size. The returned spectral signals are three different narrow-band reflection peaks, which have different signal characteristics from the dual FP cavity interference signal. The single-channel control and reception of the four-way optical signal can be realized through a 2×4 fiber-coupled beam splitter, and the separation and decoupling of multiple parameters can be realized through signal processing, thereby realizing the composite processing of multi-channel signals instead of simple system superposition, reducing the complexity of the demodulation system. BRIEF DESCRIPTION OF THE DRAWINGS
[0039] Figure 1 This is a schematic diagram of the structure of the sapphire-based multi-parameter composite optical fiber sensor of the present invention.
[0040] Figure 2 This is a bottom view of the bottom structure of the sapphire multi-parameter composite sensitive chip of the present invention.
[0041] Figure 3 This is a top view of the ceramic insert structure of the present invention.
[0042] Figure 4 This is a schematic diagram of the principle of the sapphire-based multi-parameter composite optical fiber sensor signal demodulation system of the present invention.
[0043] Figure 5 This is a coupled interference spectrum diagram of the air cavity and the temperature-sensitive cavity of the sapphire-based multi-parameter composite optical fiber sensor of the present invention.
[0044] Figure 6 This is a three-fiber Bragg grating coupling spectrum diagram of the sapphire-based multi-parameter composite optical fiber sensor of the present invention.
[0045] Figure 7 This is a spectrum diagram of the overall coupled output of four-way modulated light of the sapphire-based multi-parameter composite optical fiber sensor of the present invention.
[0046] Figure 8 Schematic diagram of the chip upper layer preparation process of the present invention.
[0047] Fig. 9 It is a schematic diagram of the middle layer preparation process of the chip of the present invention.
[0048] Fig.10 It is a schematic diagram of the preparation process of the lower layer of the chip of the present invention.
[0049] Fig.11 It is a schematic diagram of the bonding and slicing process of the three-layer sapphire wafer structure of the present invention.
[0050] Wherein: 1-sapphire multi-parameter composite sensitive chip, 101-chip upper layer, 102-chip middle layer, 103-chip lower layer, 2-package shell, 3-ceramic insert, 301-collimator socket, 302-optical fiber socket, 4-optical fiber grating, 5-three cantilever beams, 501-x-axis vibration beam, 502-y-axis vibration beam, 503-z-axis vibration beam, 6-grating area, 7-optical fiber collimator, 701-sapphire lens, 702-ceramic ferrule, 703-collimator optical fiber. DETAILED DESCRIPTION
[0051] In order to enable those skilled in the art to better understand the technical solution of the present invention, the technical solution of the present invention is further described below in conjunction with the accompanying drawings and embodiments. Embodiment 1
[0052] Embodiment 1 provides a sapphire-based multi-parameter composite optical fiber sensor, as shown in the attached Figure 1-3 The sapphire-based multi-parameter composite optical fiber sensor comprises a sapphire multi-parameter composite sensitive chip 1, a packaging shell 2, a ceramic insert 3, an optical fiber grating 4, a three-cantilever beam 5 and an optical fiber collimator 7. The sapphire multi-parameter composite sensitive chip 1 is packaged in the packaging shell 2, and a three-cantilever beam 5 structure is provided at the bottom of the sapphire multi-parameter composite sensitive chip 1. The three-axis bottoms of the three-cantilever beam 5 are all connected to the optical fiber grating 4 with a grating area 6 at the end; the ceramic insert 3 is located at the bottom of the packaging shell 2, and the optical fiber collimator 7 is inserted in the ceramic insert 3.
[0053] Specifically, the sapphire multi-parameter composite sensitive chip 1 includes a chip upper layer 101 based on all-sapphire material, a chip middle layer 102 and a chip lower layer 103; the upper surface of the chip upper layer 101 is a rough surface, which is optically opaque to the incident light of the C band, the bottom surface of the chip upper layer 101 is provided with a cavity, the top surface of the cavity is provided with a pressure-sensitive membrane, and the lower surface of the pressure-sensitive membrane is smooth and transparent; the chip middle layer 102 is a solid structure provided with an outer ring and upper and lower bosses, and the upper boss of the chip middle layer 102 is bonded to the cavity on the bottom surface of the chip upper layer 101 to form a pressure cavity, and the chip middle layer 102 is axially heated and expanded to form a temperature-sensitive cavity, so that the chip upper layer 101 and the chip middle layer 102 form a double FP cavity; the chip lower layer 103 is a hollow structure provided with three cantilever beams 5, and the chip lower layer 103 is bonded to the chip middle layer 102, and there is a movable gap between the three cantilever beams 5 and the chip middle layer 102.
[0054] The three cantilever beams 5 include an x-axis vibration beam 501, a y-axis vibration beam 502, and a z-axis vibration beam 503, wherein the x-axis vibration beam 501, the y-axis vibration beam 502, and the z-axis vibration beam 503 form a three-axis structure, and the x-axis vibration beam 501, the y-axis vibration beam 502, and the z-axis vibration beam 503 are all connected with optical fiber gratings 4, and the ends of the three optical fiber gratings 4 connected to the corresponding vibration beams are respectively provided with grating regions 6 with different central wavelengths in the c-band, and the two ends of the grating regions 6 are respectively fixed to the bottoms of the corresponding x-axis vibration beams 501, the y-axis vibration beams 502, and the z-axis vibration beams 503 by transmission femtosecond laser melting welding, refer to the attached Figure 2 shown.
[0055] The sapphire multi-parameter composite sensitive chip 1 is connected to a packaging shell 2 made of alumina ceramic material. The packaging shell 2 is provided with a groove matching the outer ring structure of the chip middle layer 102, and the lower surface of the outer ring of the chip middle layer 102 and the groove of the packaging shell 2 are fixed by full-surface melting welding using a transmitted femtosecond laser.
[0056] The fiber Bragg grating 4 is fixed to the inner wall of the packaging shell 2 using alumina high-temperature inorganic glue to reduce the interference of the structure shaking on the output signal, and the end of the fiber Bragg grating 4 away from the grating area 6 passes through the ceramic insert 3.
[0057] The ceramic insert 3 is a cross-shaped structure, and the upper vertical portion of the ceramic insert 3 is inserted from the bottom of the packaging shell 2. The top surface of the horizontal portion of the ceramic insert 3 is bonded and fixed to the bottom of the packaging shell 2 by alumina high-temperature inorganic glue to support the bottom of the packaging shell 2.
[0058] The middle part of the ceramic insert tube 3 is provided with a collimator socket 301 for inserting the fiber collimator 7. The ceramic insert tube 3 is also provided with three fiber sockets 302 for the fiber grating 4 to pass through. The three fiber sockets 302 are distributed on the periphery of the collimator socket 301. The fiber collimator 7 is inserted into the collimator socket 301, and the fiber collimator 7 is perpendicular to the bottom of the sapphire multi-parameter composite sensitive chip 1. The fiber socket 302 is provided with a horn mouth on one side close to the packaging shell 2. The three fiber gratings 4 are respectively inserted and led out from the horn mouths of the three fiber sockets 302. The three fiber gratings 4 and the fiber collimator 7 are bonded and fixed to the ceramic insert tube 3 with alumina high-temperature inorganic adhesive.
[0059] The optical fiber collimator 7 includes a sapphire lens 701 , a ceramic ferrule 702 and a collimator optical fiber 703 made of sapphire material. The collimator optical fiber 703 passes through the ceramic insert 3 .
[0060] The working principle of the sapphire-based multi-parameter composite optical fiber sensor in this embodiment is as follows: Figure 4 As shown in FIG. 1 , a broadband Gaussian beam of c-band is emitted by an ASE light source, and is divided into four beams of light with the same wavelength and equal intensity by a 2×4 fiber-coupled beam splitter, and is respectively incident on a collimator fiber 703 and three fiber gratings 4 led out by a fiber collimator 7. The parallel beam emitted by the fiber collimator 7 is modulated by the temperature-sensitive cavity of the chip middle layer 102 and the pressure cavity formed by the chip middle layer 102 and the chip upper layer 101 to form a double FP cavity multi-beam interference, and returns to the fiber collimator 7; the spectral wavelength range is 1520-1580nm, the temperature-sensitive cavity length is 400μm, the pressure cavity length is 200μm, and the modulated interference light formed is shown in the attached figure. Figure 5 The light beams incident on the grating area 6 by the three fiber gratings 4 are narrow-band filtered. The central wavelengths of the three fiber gratings 4 are 1530nm, 1550nm, and 1570nm respectively. The spectrum after modulation can be expressed as shown in the attached figure. Figure 6 As shown in the figure, four modulated lights are coupled into the spectrometer module at the signal receiving end through a 2×4 fiber-coupled beam splitter. The interference spectrum after the four modulated lights are coupled can be expressed as shown in the figure. Figure 7 Finally, the collected coupling spectrum is input into the signal processing unit, and the coupling spectrum is separated and decoupled to obtain the pressure chamber length and L 1 , Temperature sensitive cavity length L 2 and the central wavelengths λ of the three fiber Bragg gratings 4 1 , 2 , 3 ; Among them, the cavity length L 1 and L 2 Corresponding to the superposition of two cosine-like signals of low frequency and high frequency, the corresponding frequencies of the two FP cavities can be obtained by FFT fast Fourier transform, thereby obtaining the cavity length value, λ 1 , 2 , 3 It can be obtained by searching the peaks through spectral scanning.
[0061] For the composite optical fiber sensor of the present invention, the cavity length L 1 The change in can be expressed by the following formula: ,
[0062] In the formula, Δ P , Δ T are the changes of external pressure and temperature, E , v , α 1They are Young's modulus, Poisson's ratio and axial thermal expansion coefficient of sapphire material. R , h 1 are the radius and thickness of the pressure sensitive diaphragm respectively.
[0063] Cavity length L 2 The change in can be expressed by the following formula: ,
[0064] In the formula, h 2 is the initial thickness of the temperature-sensitive cavity.
[0065] The central wavelengths λ of the three fiber Bragg gratings 4 1 , 2 , 3 The change in can be expressed as: ,
[0066] In the formula, B =1,2,3, , α 2 is the thermo-optic coefficient and thermal expansion coefficient of the fiber Bragg grating, P e is the effective elastic-optical coefficient, Δ ε is the axial strain of the grating region caused by vibration.
[0067] Above , Represents the pressure chamber L 1 and temperature sensitive cavity L 2 The change of cavity length with external pressure and temperature, λ 1 , 2 , 3 The amount of change It is caused by the combined effect of the axial strain of the grating area caused by external vibration (the grating strain introduced by the bending of the cantilever beam) and the change in the grating pitch caused by temperature change. In the formula, except for the external pressure change Δ P , Temperature change Δ T and the axial strain of the grating region Δ ε Except for the other parameters, the other parameters are known. L 2 Get the temperature change value Δ T , and then Δ T Substituting the rest of the formula, we get The amount that changes only with pressure fluctuations and The change in grating strain Δ caused by vibration alone ε , the external pressure change is obtained according to the formula and the vibration-induced grating strain Δ ε , and then based on the grating strain Δ ε The corresponding relationship with the vibration magnitude can obtain the external vibration change Δ a (x, y, z axis directions), therefore, in the present invention, L 1 and L 2 , 1 , 2 , 3 Simultaneous demodulation of multiple parameters can realize real-time acquisition and perception of the sensor's external pressure, temperature, and vibration, as well as temperature compensation for pressure and vibration. Embodiment 2
[0068] Embodiment 2 provides a method for preparing the sapphire-based multi-parameter composite optical fiber sensor as described in Embodiment 1, which specifically comprises the following steps:
[0069] S1: preparing a sapphire multi-parameter composite sensitive chip 1 with a three-cantilever beam 5 structure;
[0070] Specifically, S101: Take a clean single-polished sapphire wafer, use a large-particle diamond polishing liquid to grind the non-polished surface of the wafer, and further roughen the surface to be optically opaque in the C band, as shown in the attached Figure 8 As shown in (a); electroplating metal nickel on the non-etched area of the polished surface of the single-polished sapphire wafer, as shown in the attached Figure 8 As shown in (b), using nickel as an etching mask, ICP plasma etches the polished surface of the wafer to form a cavity and a pressure sensitive film, and obtain the chip upper layer 101 structure, as shown in the attached figure. Figure 8 As shown in (c).
[0071] S102: Take a clean double-polished sapphire wafer, electroplate metal nickel on the front and back sides of the wafer, and use the metal nickel as an etching mask to etch a circular shallow groove around the corresponding etching window area of the double-polished sapphire wafer to form a solid structure of upper and lower bosses, and obtain a chip middle layer 102 structure, such as Fig. 9 As shown in (a) to (d), (a) is electroplating metal nickel on the front side of the chip, (b) is etching a shallow annular groove on the front side of the chip using metal nickel as an etching mask; (c) is electroplating metal nickel on the back side of the chip, and (d) is etching a shallow annular groove on the back side of the chip using metal nickel as an etching mask.
[0072] S103: Take another clean double-polished sapphire wafer and electroplate nickel on the front side of the wafer. Fig.10 As shown in (a), nickel is used as an etching mask to etch a movable gap on the upper surface of the wafer. Fig.10As shown in (b); the upper surface of the wafer is etched from the front side, and only the z-axis vibration beam 503 is protected in the etched area, as shown in the attached Fig.10 As shown in (c), the z-axis vibration beam 503 is etched to form a step difference with other positions in the region that is the same as the thickness of the z-axis vibration beam 503. Fig.10 Then, the upper surface of the wafer is further etched on the front side, and only the x-axis vibration beam 501 and the y-axis vibration beam 502 are protected in the etched area, as shown in the attached Fig.10 As shown in (e), the entire surface of the wafer etching window area is etched through until the remaining x-axis vibration beam 501, y-axis vibration beam 502 and z-axis vibration beam 503 thinned to a specified thickness are left. Fig.10 As shown in (f), the chip lower layer 103 and the three cantilever beam 5 structure are obtained.
[0073] S104: The three sapphire wafers in steps S101-S103 are directly bonded at high temperature and annealed to release thermal stress to form a three-layer sapphire high-strength bonding structure, as shown in the attached Fig.11 As shown in (a), a femtosecond laser is then used to cut the three-layer sapphire bonding structure. The cutting position is based on the edge of the annular shallow groove of the middle layer 102 of the chip. The inner side is cut to the step area on the upper and lower sides respectively, and the outer side is cut on the entire surface, finally forming a sapphire multi-parameter composite sensitive chip 1, as shown in the attached figure. Fig.11 As shown in (b).
[0074] S2: Connect three fiber gratings 4 to three cantilever beams 5;
[0075] Specifically, a grating region with a periodic structure, namely, a grating region 6, is formed at one end of each of the three fiber gratings 4 by etching through a femtosecond laser process, and the three fiber gratings 4 have different central wavelengths in the c-band respectively; then, one end of the three fiber gratings 4 provided with the grating region 6 is fixed to the x-axis vibration beam 501, the y-axis vibration beam 502 and the z-axis vibration beam 503 at the bottom of the chip lower layer 103 by melt welding at both ends of the grating region using a transmitted femtosecond laser.
[0076] S3: Encapsulating the sapphire multi-parameter composite sensitive chip 1 in the encapsulation shell 2;
[0077] Specifically, the outer ring lower surface of the chip middle layer 102 of the sapphire multi-parameter composite sensitive chip 1 and the groove of the packaging shell 2 are fixed by full-surface melting welding using a transmitted femtosecond laser, and three fiber gratings 4 are fixed to the inner wall of the packaging shell 2 using alumina high-temperature inorganic glue.
[0078] S4: inserting the ceramic insert 3 into the bottom of the package shell 2 and fixing it;
[0079] Specifically, the upper vertical portion of the ceramic insert 3 is inserted into the bottom of the packaging shell 2, and the top surface of the horizontal portion of the ceramic insert 3 is bonded and fixed to the bottom of the packaging shell 2 by means of alumina high-temperature inorganic glue; then the three optical fiber gratings 4 are respectively led out from the three optical fiber plug holes 302, and are bonded and fixed to the side walls of the optical fiber plug holes 302 by means of alumina high-temperature inorganic glue.
[0080] S5: inserting the optical fiber collimator 7 into the ceramic insert 3 and fixing it;
[0081] Specifically, the optical fiber collimator 7 is inserted into the collimator plug hole 301 , and is bonded and fixed to the side wall of the collimator plug hole 301 using alumina high-temperature inorganic adhesive, and the collimator optical fiber 703 is led out of the collimator plug hole 301 .
[0082] The above shows and describes the basic principles, main features and advantages of the present invention. It should be understood by those skilled in the art that the present invention is not limited to the above embodiments, and the above embodiments and descriptions are only for explaining the principles of the present invention. Without departing from the spirit and scope of the present invention, the present invention may have various changes and improvements, which fall within the scope of the present invention to be protected. The scope of protection of the present invention is defined by the attached claims and their equivalents.
Claims
1. A sapphire-based multi-parameter composite optical fiber sensor, comprising a packaging shell (2), characterized in that: It also includes a sapphire multi-parameter composite sensitive chip (1) encapsulated in a packaging shell (2); the bottom of the sapphire multi-parameter composite sensitive chip (1) is provided with three cantilever beams (5), and the three axes of the three cantilever beams (5) are all connected to optical fiber gratings (4); the bottom of the packaging shell (2) is provided with a ceramic insert (3), and an optical fiber collimator (7) is provided in the ceramic insert (3); The sapphire multi-parameter composite sensitive chip (1) comprises a chip upper layer (101), a chip middle layer (102) and a chip lower layer (103) based on all sapphire materials; the upper surface of the chip upper layer (101) is a rough surface and is optically opaque to C-band incident light; the bottom surface of the chip upper layer (101) is provided with a cavity; the top surface of the cavity is provided with a pressure sensitive membrane; and the lower surface of the pressure sensitive membrane is smooth and transparent; the chip middle layer (102) is a solid structure provided with an outer ring and upper and lower bosses; The upper boss of the chip middle layer (102) is bonded to the cavity on the bottom surface of the chip upper layer (101) to form a pressure cavity, and the chip middle layer (102) is axially heated and expanded to form a temperature-sensitive cavity, so that the chip upper layer (101) and the chip middle layer (102) form a double FP cavity; the chip lower layer (103) is a hollow structure provided with three cantilever beams (5), and the chip lower layer (103) is bonded to the chip middle layer (102), and there is a movable gap between the three cantilever beams (5) and the chip middle layer (102); The three cantilever beams (5) comprise an x-axis vibration beam (501), a y-axis vibration beam (502) and a z-axis vibration beam (503); the x-axis vibration beam (501), the y-axis vibration beam (502) and the z-axis vibration beam (503) are all connected to optical fiber gratings (4); and the grating regions (6) at the ends of the optical fiber gratings (4) are connected to the corresponding vibration beams.
2. The sapphire-based multi-parameter composite optical fiber sensor according to claim 1, characterized in that: The middle portion of the ceramic insert tube (3) is provided with a collimator insertion hole (301) for inserting the optical fiber collimator (7), and three optical fiber insertion holes (302) for the optical fiber grating (4) to pass through.
3. The sapphire-based multi-parameter composite optical fiber sensor according to claim 1, characterized in that: The optical fiber collimator (7) comprises a sapphire lens (701), a ceramic ferrule (702) and a collimator optical fiber (703).
4. The method for preparing the sapphire-based multi-parameter composite optical fiber sensor according to any one of claims 1 to 3, characterized in that: The following steps are involved: S1: preparing a sapphire multi-parameter composite sensitive chip (1) with a three-cantilever beam (5) structure; S2: connecting three fiber gratings (4) to three cantilever beams (5); S3: Encapsulating the sapphire multi-parameter composite sensitive chip (1) in a packaging shell (2); S4: inserting a ceramic insert (3) into the bottom of the packaging shell (2) and fixing it; S5: Insert the optical fiber collimator (7) into the ceramic insert (3) and fix it.
5. The method for preparing the sapphire-based multi-parameter composite optical fiber sensor according to claim 4, characterized in that: The specific operation of step S1 includes the following steps: S101: Take a clean single-polished sapphire wafer, roughen the non-polished surface to be optically opaque in the C-band, and etch the polished surface of the wafer to form a cavity to obtain the upper layer (101) structure of the chip; S102: Take a clean double-polished sapphire wafer, and etch shallow annular grooves on the front and back sides of the wafer respectively to form upper and lower convex platform solid structures to obtain a chip middle layer (102) structure; S103: taking another clean double-polished sapphire wafer, and engraving a three-cantilever beam (5) structure on the wafer to obtain a chip lower layer (103) with a three-cantilever beam (5) structure; S104: Bonding and dicing the three sapphire wafers in steps S101 to S103 to obtain a sapphire multi-parameter composite sensitive chip (1) with a three-cantilever beam (5) structure.
6. The demodulation method of the sapphire-based multi-parameter composite optical fiber sensor according to any one of claims 1 to 3, characterized in that: The following steps are involved: Step 1: split the c-band broadband Gaussian beam into four beams of the same wavelength and equal intensity through a 2×4 fiber-coupled beam splitter, and respectively inject them into a fiber collimator (7) and three fiber gratings (4) with different central wavelengths in the c-band; Step 2: The parallel light beam emitted from the optical fiber collimator (7) is modulated by the sapphire multi-parameter composite sensitive chip (1) to form a double FP cavity interference light and returns to the optical fiber collimator (7); Step 3: The light beams incident on the grating region (6) from the three fiber gratings (4) are narrow-band filtered to obtain three different central peak wavelengths; Step 4: Couple the four modulated lights, and then separate and decouple the coupled spectra to obtain the pressure chamber lengths and L 1. Length of temperature sensitive chamber L 2 and the central wavelengths λ1, λ2, λ3 of the three fiber gratings (4); Step 5: Calculate the pressure chamber length L 1. Length of temperature sensitive chamber L 2 and the changes of λ1, λ2, and λ3 are used to perform temperature compensation for pressure and vibration.
7. The demodulation method of the sapphire-based multi-parameter composite optical fiber sensor according to claim 6, characterized in that: Cavity length L The change of 1 is expressed as , Cavity length L The change in 2 is expressed as , The changes of λ1, λ2, and λ3 are expressed as , In the formula, Δ P , Δ T are the changes of external pressure and temperature, E , v , α 1 They are Young's modulus, Poisson's ratio and axial thermal expansion coefficient of sapphire material. R , h 1 are the radius and thickness of the pressure sensitive diaphragm, h 2 is the initial thickness of the temperature sensitive cavity, B =1,2,3, , α 2 is the thermo-optic coefficient and thermal expansion coefficient of the fiber Bragg grating, P e is the effective elastic-optical coefficient, is the axial strain of the grating region caused by vibration.