A device for measuring wet film of steel structure coating

By introducing a drive unit, a blowing unit and a pressure sensor into the wet film measurement device, efficient and accurate wet film thickness detection is achieved, solving the problems of low efficiency and inaccurate detection in the prior art, reducing costs and improving Real-time adjustment capability of wet film thickness.

CN118698823BActive Publication Date: 2024-11-01CHINA WATER CONSERVANCY & HYDROPOWER NO 9 ENG BUREAU CO LTD
View PDF 14 Cites 0 Cited by

Patent Information

Application Number
CN202411178575.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-08-27
Publication Date
2024-11-01
Estimated Expiration
2044-08-27

AI Technical Summary

Technical Problem

The existing wet film thickness measurement devices are inefficient, and the measurement card needs to be continuously adjusted to judge the wet film thickness, and the wet film thickness cannot be adjusted in real time, resulting in inaccurate detection.

Method used

A steel structure coated wet film measuring device including a driving unit, a blowing unit and a pressure sensor is designed. By driving the measurement arm movement and blowing the blowing unit, the wet film thickness is determined, and the marking liquid is sprayed through the piston and the storage cylinder. Label the wet film with standard.

Benefits of technology

It improves the efficiency and accuracy of wet film thickness measurement, can adjust the wet film thickness in real time, reduces detection errors for volatile coatings, and reduces costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118698823B_ABST
    Figure CN118698823B_ABST
Patent Text Reader

Abstract

The present invention discloses a wet film measuring device for steel structure coating, which relates to the technical field of wet film measuring devices, and includes a mounting seat, a movable block, a driving unit, and a measuring arm. The outer wall of the mounting seat is provided with a through slot for the measuring arm to pass freely; and a blowing unit is arranged on the measuring arm. The driving unit is arranged to drive the two measuring arms to move relative to each other, so that after the two measuring arms move into place, the lateral spacing between the two measuring arms corresponds to the standard steel structure wet film thickness size, and then the blowing unit is used to blow air to the wet film surface of the steel structure. When the measuring arm is completely in contact with the wet film surface of the steel structure, the air generated by the blowing unit is blocked by the wet film surface of the steel structure and cannot be blown out, thereby making it possible to determine whether the wet film thickness of the steel structure meets the standard. On the contrary, when the wet film thickness of the steel structure does not meet the standard, there is a gap between the measuring arm and the wet film surface of the steel structure, thereby making it possible to blow the air generated by the blowing unit to the outside of the measuring arm, thereby making it possible to determine that the wet film thickness of the steel structure does not meet the standard.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of wet film measuring devices, in particular to a wet film measuring device for a steel structure coating. Background Art

[0002] Coating is an important means of corrosion protection for steel structures. In the corrosion protection mechanism of coatings, the shielding effect is the most important, and the shielding effect of coatings is closely related to the thickness of coatings. The thicker the coating, the better the shielding effect; but if the coating is too thick, it will lead to a series of drawbacks such as cracking and pinholes. There are two methods for measuring the film thickness of coatings: dry film thickness measurement and wet film thickness measurement. The film thickness measurement of dry film belongs to post-inspection, while in the coating process, the wet film thickness of coatings is inspected, and the wet film thickness can be adjusted at any time during the construction process to ensure the coating thickness. Wet film thickness detection cannot be used for coatings that evaporate too quickly, which will lead to inaccurate test values. In addition to ensuring the quality of coating, coating thickness control can effectively save the use of coatings and reduce costs.

[0003] After searching, Chinese invention patent publication number CN113048896A discloses a handheld wet film measuring device for steel structure coating, which relates to the technical field of coating detection, including a measuring component, an adjusting component and a handheld component, wherein: the measuring component is arranged at the front end and is used to realize the wet film measurement of the semi-enclosed steel structure coating, and the measuring component specifically includes a mounting plate 1, a guide bar 1, a servo 1, a guide bar 2, a mounting plate 2, a servo 2, a mounting plate 3 and a pinhole camera; the adjusting component is arranged in the middle and is used to realize the spatial posture adjustment of the measuring component, and the adjusting component specifically includes a fixing plate 1, a motor 1, a spline shaft 1, a fixing plate 2 and a motor 2; the handheld component is arranged at the rear end and is used to realize the single-handed holding of the measuring component and the adjusting component, and the handheld component specifically includes a handheld rod, a telescopic rod, a mounting frame, a touch screen and a mobile power supply.

[0004] When measuring, the wet film thickness measuring device in the above-mentioned prior art mainly clamps the measuring bayonet of the wet film card on the steel structure, and determines the thickness of the wet film by observing whether there is a gap between the inner wall of the measuring bayonet and the surface of the steel structure. This method requires continuous adjustment of the wet film card so that the measuring bayonet of the wet film card alternately engages with the steel structure, and then selects the measuring bayonet engaged with the steel structure, and then determines the wet film thickness of the steel structure by the scale value on the measuring bayonet, which makes the overall measurement efficiency low. Summary of the invention

[0005] The object of the present invention is to provide a steel structure coating wet film measuring device to solve the problems raised in the above background technology.

[0006] To achieve the above object, the present invention provides the following technical solutions:

[0007] A steel structure coating wet film measuring device, comprising:

[0008] A mounting seat, wherein two movable blocks are slidably connected in the mounting seat, and the two movable blocks are driven to move relative to each other by a driving unit installed on the mounting seat;

[0009] A measuring arm fixedly connected to the movable block, wherein the outer wall of the mounting seat is provided with a through slot for the measuring arm to pass freely;

[0010] A blowing unit is arranged on the measuring arm.

[0011] Furthermore, a handle is fixedly connected to one end of the mounting base away from the measuring arm.

[0012] Furthermore, the driving unit includes a motor mounted on the mounting base, the output shaft of the motor is drivingly connected to a rotating disk, a sliding pin is fixedly connected to one end of the movable block facing the rotating disk, a waist-shaped hole for the sliding pin to be inserted into the end surface of the rotating disk, and one end of the waist-shaped hole in the length direction is inclined and extends toward the radial outer side of the rotating disk.

[0013] Furthermore, a guide column is provided on the mounting seat, and a guide hole is provided in the movable block for the guide column to pass freely.

[0014] Furthermore, the blowing unit includes a cylinder installed on the outer wall of the movable block, the cylinder rod of the cylinder is driven and connected to a piston, a connecting cavity for the piston to engage is opened in the measuring arm, the piston slides freely in the connecting cavity, and a blowing hole that penetrates the connecting cavity is opened on the outer wall of the measuring arm.

[0015] Furthermore, the piston end face is coaxially provided with a through hole for the cylinder rod to pass freely, a lower limit nut is fixedly sleeved on the cylinder rod, an upper limit nut is fixedly sleeved on the upper end of the cylinder rod, the piston is arranged between the upper limit nut and the lower limit nut, and a first spring is sleeved on the cylinder rod, and both ends of the first spring in the elastic force direction elastically press against the lower limit nut and the piston in a one-to-one corresponding manner.

[0016] Furthermore, a mounting groove is formed on one end surface of the piston facing the upper limit nut, a pressure sensor is installed in the mounting groove, and a surface of the pressure sensor abuts against a lower end surface of the upper limit nut.

[0017] Furthermore, a side of the measuring arm where the blowing hole is provided is provided with a chrome-plated layer.

[0018] Furthermore, an end face of the measuring arm away from the movable block is connected to a storage cylinder, an outer wall of the storage cylinder is provided with liquid spraying microholes, the storage cylinder is connected with the interior of the communicating cavity, and a pressurizing unit is provided in the storage cylinder.

[0019] Furthermore, the pressurizing unit includes a sliding plug coaxially engaged in the storage cylinder, the sliding plug slides freely in the storage cylinder, a second spring is provided in the storage cylinder, and both ends of the second spring in the elastic force direction elastically press against the sliding plug and the top wall of the storage cylinder respectively and one by one.

[0020] Compared with the prior art, the present invention has the following beneficial effects:

[0021] The present invention provides a driving unit to drive the two measuring arms to move relative to each other, so that after the two measuring arms move to a certain position, the lateral spacing between the two measuring arms corresponds to the standard wet film thickness size of the steel structure, and then the air blowing unit blows air to the wet film surface of the steel structure. When the measuring arms are completely in contact with the wet film surface of the steel structure, the air generated by the air blowing unit is blocked by the wet film surface of the steel structure and cannot be blown out, thereby making it possible to determine whether the wet film thickness of the steel structure meets the standard. On the contrary, when the wet film thickness of the steel structure does not meet the standard, there is a gap between the measuring arms and the wet film surface of the steel structure, thereby making it possible to blow the air generated by the air blowing unit to the outside of the measuring arms, thereby making it possible to determine whether the wet film thickness of the steel structure does not meet the standard.

[0022] The present invention sets a motor to drive the rotating disk to rotate, so that the sliding pin slides in the waist-shaped hole of the rotating disk, thereby driving the two movable blocks to move relative to each other, thereby adjusting the relative distance between the two movable blocks, that is, adjusting the distance between the two measuring arms, and thus adjusting the size range of the wet film thickness of the steel structure to be measured;

[0023] The present invention arranges a piston to move in the connecting cavity toward the storage cylinder. When the air blowing hole is blocked by the wet film surface of the steel structure, the piston moves upward, thereby compressing the air in the connecting cavity, so that the air can enter the storage cylinder and squeeze the sliding plug, so that the sliding plug generates an extrusion force on the marking liquid in the storage cylinder, so that the marking liquid can be sprayed from the liquid spraying micropores to the surface of the steel structure, and the steel structure with the wet film thickness reaching the standard can be marked. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1 It is a structural schematic diagram of a steel structure coating wet film measuring device in the present invention;

[0025] Figure 2 for Figure 1 Schematic diagram of the structure from a side view angle;

[0026] Figure 3 for Figure 2 A schematic cross-sectional view of a part of the structure;

[0027] Figure 4 for Figure 3 A magnified schematic diagram of the local structure at point A;

[0028] Figure 5 It is a schematic diagram of the structure after the cylinder and piston are assembled in the present invention;

[0029] Figure 6 for Figure 5 Schematic diagram of the explosion decomposition of the structure;

[0030] Figure 7 It is a schematic diagram of the structure after the movable block and the measuring arm are assembled in the present invention;

[0031] Figure 8 for Figure 7 A schematic cross-sectional view of the structure;

[0032] Fig. 9 It is a schematic diagram of the structure of the storage cylinder in the present invention;

[0033] Fig.10 for Fig. 9 Schematic cross-sectional view of the structure.

[0034] In the figure, the description of each figure mark is as follows: 1. handle; 2. mounting seat; 3. rotating disk; 4. guide column; 5. storage cylinder; 6. measuring arm; 7. movable block; 8. waist-shaped hole; 9. motor; 10. cylinder; 11. piston; 12. connecting chamber; 13. second spring; 14. sliding plug; 15. liquid spraying microhole; 16. blowing hole; 17. lower limit nut; 18. first spring; 19. pressure sensor; 20. upper limit nut; 21. cylinder rod; 22. sliding pin; 23. liquid filling port. DETAILED DESCRIPTION

[0035] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0036] See also Figure 1 - Fig.10The present invention provides a technical solution: a steel structure coating wet film measuring device, comprising a mounting seat 2 with a handle 1 welded at one end, the mounting seat 2 is hollow, and a guide column 4 is horizontally penetrated on the mounting seat 2, two movable blocks 7 are mounted on the guide column 4, and a guide hole for the guide column 4 to pass freely is opened on the movable block 7, a measuring arm 6 is welded on the outer wall of the movable block 7, and a through groove for the measuring arm 6 to pass freely is opened on the outer wall of the mounting seat 2;

[0037] A motor 9 is mounted on the mounting seat 2, and the output shaft of the motor 9 is connected to the rotating disk 3. A sliding pin 22 is fixedly connected to one end of the movable block 7 facing the rotating disk 3. A waist-shaped hole 8 (combined with a Figure 1 and Figure 7 ), the length direction of the waist-shaped hole 8 extends in an inclined direction that forms a certain angle with the radial outer direction. When the output shaft of the motor 9 rotates, the rotating disk 3 is driven to rotate. When the rotating disk 3 rotates, the sliding pin 22 slides in the waist-shaped hole 8, and then the movable block 7 can be driven to produce horizontal movement, thereby driving the two movable blocks 7 to move relative to each other. When the two movable blocks 7 move relative to each other, the two measuring arms 6 can be driven to move relative to each other, thereby adjusting the relative spacing between the two measuring arms 6, that is, adjusting the size range of the wet film thickness detected by the two measuring arms 6;

[0038] The outer wall of the movable block 7 is provided with a cylinder 10, and the cylinder rod 21 of the cylinder 10 is driven and connected with the piston 11. A connecting cavity 12 for the piston 11 to engage is provided in the measuring arm 6, and the piston 11 slides freely in the connecting cavity 12. The outer wall of the measuring arm 6 is provided with a blowing hole 16 that passes through the connecting cavity 12. Specifically, a through hole for the cylinder rod 21 to pass freely is coaxially provided on the end face of the piston 11. A lower limit nut 17 is fixedly sleeved on the cylinder rod 21, and an upper limit nut is fixedly sleeved on the upper end of the cylinder rod 21. 20, the piston 11 is arranged between the upper limit nut 20 and the lower limit nut 17, the first spring 18 is sleeved around the cylinder rod 21, and the two ends of the elastic force direction of the first spring 18 elastically press against the lower limit nut 17 and the piston 11 one by one, and the piston 11 is provided with a mounting groove on one end surface facing the upper limit nut 20, and a pressure sensor 19 is installed in the mounting groove, and the surface of the pressure sensor 19 presses against the lower end surface of the upper limit nut 20, and the pressure sensor 19 is connected to the external control cabinet through a wireless module;

[0039] The end face of the measuring arm 6 away from the movable block 7 is connected to a storage cylinder 5, which is filled with a marking liquid, and the outer wall of the storage cylinder 5 is provided with a liquid spraying micro hole 15 (such as Figure 4As shown), in addition, a liquid replenishing port 23 for replenishing the marking liquid into the storage cylinder 5 is provided on the outer wall of the storage cylinder 5, and a one-way valve (not shown in the figure) is installed at the mouth of the liquid replenishing port 23. The marking liquid is inserted into the one-way valve using an external injection tool, and then the marking liquid can be replenished into the storage cylinder 5 through the liquid replenishing port 23. The storage cylinder 5 is connected to the inside of the communicating cavity 12, and a sliding plug 14 is coaxially engaged in the storage cylinder 5. The sliding plug 14 slides freely in the storage cylinder 5. A second spring 13 is provided in the storage cylinder 5, and the two ends of the second spring 13 in the elastic force direction elastically press against the sliding plug 14 and the inner top wall of the storage cylinder 5 respectively, and a chrome-plated layer (not shown in the figure) is provided on one side of the measuring arm 6 where the blowing hole 16 is provided;

[0040] In the initial state, the second spring 13 generates an elastic resisting force on the sliding plug 14 in the direction of the measuring arm 6, so that the sliding plug 14 will not squeeze the marking liquid in the storage cylinder 5, so that the marking liquid in the storage cylinder 5 will not be sprayed out from the spray micropores 15. When the piston 11 moves in the direction of the storage cylinder 5, if the orifice of the blowing hole 16 is in complete contact with the wet film surface of the steel structure, the piston 11 will squeeze the air in the connecting chamber 12 when it moves. Due to the resistance of the air, the piston 11 will move in the direction away from the upper limit nut 20, so that the squeezing force of the upper limit nut 20 on the pressure sensor 19 is reduced. At the same time, part of the air in the connecting chamber 12 will enter the storage cylinder 5 and generate a thrust on the sliding plug 14 in the direction away from the measuring arm 6, so that the sliding plug 14 generates a squeezing force on the marking liquid in the storage cylinder 5, so that the marking liquid is sprayed from the spray micropores 15 to The wet film surface of the steel structure can be determined to determine whether the wet film thickness meets the standard. In this embodiment, the wire diameter of the first spring 18 is smaller than the wire diameter of the second spring 13, that is, the elastic coefficient of the first spring 18 is smaller than the elastic coefficient of the second spring 13. Therefore, when the piston 11 moves upward, the second spring 13 has an elastic resisting force on the sliding plug 14, so that the air in the connecting chamber 12 cannot enter the storage cylinder 5 in the initial stage of the piston 11 moving upward, so that the air in the connecting chamber 12 is in a compressed state, and the first spring 18 will produce compression deformation before the second spring 13, and then as the piston 11 continues to move, the air pressure in the connecting chamber 12 is greater than the elastic resisting force of the second spring 13 on the sliding plug 14. At this time, the second spring 13 begins to produce compression deformation, so that the sliding plug 14 produces an extrusion effect on the marking liquid in the storage cylinder 5, so that the marking liquid is sprayed out from the spray micropore 15.

[0041] The working principle of the present invention is as follows: the motor 9 is started, and the output shaft of the motor 9 drives the rotating disk 3 to rotate. When the rotating disk 3 rotates, the sliding pin 22 slides in the waist-shaped hole 8, thereby driving the movable block 7 to produce horizontal movement, thereby driving the two movable blocks 7 to move relative to each other. When the two movable blocks 7 move relative to each other, the two measuring arms 6 can be driven to move relative to each other, thereby adjusting the relative distance between the two measuring arms 6, that is, adjusting the size range of the wet film thickness detected by the two measuring arms 6. The rotation angle of the rotating disk 3 is measured by the angle sensor in the prior art and fed back to the control cabinet, thereby calculating the rotation angle of the rotating disk 3 and the moving stroke of the measuring arm 6.

[0042] Then hold the handle 1 and insert the two measuring arms 6 into the steel structure, so that the opposite surfaces of the two measuring arms 6 are in contact with the two surfaces of the steel structure in the thickness direction respectively. In the initial state, the second spring 13 generates an elastic resisting force on the sliding plug 14 toward the measuring arm 6, so that the sliding plug 14 will not squeeze the marking liquid in the storage tube 5, so that the marking liquid in the storage tube 5 will not be sprayed out from the spray micropore 15;

[0043] After the two measuring arms 6 move toward each other to the standard measuring distance, the steel structure is located between the two measuring arms 6, that is, the wet film layers on the outer walls on both sides of the steel structure in the thickness direction also correspond to the two measuring arms 6 respectively. The cylinder 10 is started, the cylinder rod 21 of the cylinder 10 extends, and the piston 11 is driven to move toward the storage cylinder 5. If the steel structure thickness and the wet film thickness dimensions are consistent with the distance dimension between the two measuring arms 6, the surface of the measuring arm 6 is completely in contact with the wet film surface, and the wet film surface will block the mouth of the blowing hole 16. At the same time, the cylinder rod 21 of the cylinder 10 extends. Due to the blocking of the blowing hole 16 , the cylinder rod 21 drives the lower limit nut 17 to compress the first spring 18. The cylinder rod 21 further extends, which further increases the pressure of the first spring 18. When the piston 11 is pushed to move, the air in the connecting chamber 12 is squeezed. When the piston 11 moves, the air in the connecting chamber 12 is squeezed. After being subjected to air resistance, the piston 11 moves in a direction away from the upper limit nut 20. When the cylinder rod 21 is extended, the piston 11 cannot move with the cylinder rod 21 due to the air pressure generated by the blockage of the blowing hole 16. At this time, the upper limit nut 20 and the pressure sensor 19 extend with the cylinder rod 21, and the piston 11 moves. The squeezing force of the upper limit nut 20 on the pressure sensor 19 is reduced, and the pressure signal of the pressure sensor 19 is fed back to the external control cabinet. The control cabinet determines that the wet film thickness of the steel structure meets the standard according to the change of the pressure signal. On the contrary, when the two measuring arms 6 move relative to each other to the standard measuring distance, the combined size of the steel structure thickness and the wet film thickness is smaller than the distance between the two measuring arms 6. At this time, there will be a gap between the surface of the measuring arm 6 and the wet film surface. In this way, when the piston 11 is moving, the air in the connecting cavity 12 will be able to be blown out from the blowing hole 16 and the gap, so that the air in the connecting cavity 12 will basically not affect the piston 11. The movement of the piston 11 generates resistance, so that as the piston 11 moves upward in the connecting chamber 12, the piston 11 is subjected to the elastic push force of the first spring 18, and the inside of the connecting chamber 12 is connected with the gap between the measuring arm 6 and the wet film layer. The upward movement of the piston 11 will cause the air in the connecting chamber 12 to be discharged from the blowing hole 16, and the position of the piston 11 on the cylinder rod 21 will basically not change, thereby making the pressure sensor 19 less subject to the squeezing force of the upper limit nut 20. In this way, the pressure signal fed back by the pressure sensor 19 to the external control cabinet changes less, and the control cabinet can determine that the wet film thickness does not meet the standard based on the change range of the pressure signal;

[0044] Part of the air in the communication chamber 12 is squeezed to the storage cylinder 5, and a thrust is generated on the sliding plug 14 in the direction away from the measuring arm 6, so that the sliding plug 14 generates a squeezing force on the marking liquid in the storage cylinder 5, so that the marking liquid is sprayed from the spray micropores 15 to the wet film surface of the steel structure, and then it can be determined whether the wet film thickness meets the standard. In this way, the staff does not need to observe the signal prompts of the recording control cabinet all the time, and can determine whether the wet film thickness of the steel structure meets the standard by observing whether the marking liquid is sprayed on the surface of the steel structure. In addition, when the sliding plug 14 moves in the direction away from the measuring arm 6, the second spring 13 will be compressed and accumulate elastic potential energy. In this way, when the measurement is completed, the two measuring arms 6 are separated, and the cylinder rod 21 of the cylinder 10 is reset, so that the second spring 13 drives the sliding plug 14 to move in the opposite direction and reset;

[0045] When the measuring arm 6 does not contact completely with the wet film surface of the steel structure and a gap is generated, as the piston 11 moves toward the storage cylinder 5, the air in the connecting chamber 12 will be blown out from the blowing hole 16, so that the pressure sensor 19 is subjected to a smaller pressure change by the upper limit nut 20, thereby being able to determine that the wet film thickness of the steel structure does not meet the standard.

[0046] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. Although embodiments of the present invention have been shown and described, it will be understood by those skilled in the art that various changes, modifications, substitutions and variations may be made to these embodiments without departing from the principles and spirit of the present invention, and the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A steel structure coating wet film measuring device, characterized in that: include: A mounting seat (2), wherein two movable blocks (7) are slidably connected inside the mounting seat (2), and the two movable blocks (7) are driven to move relative to each other by a driving unit mounted on the mounting seat (2), wherein the driving unit comprises a motor (9) mounted on the mounting seat (2), and the output shaft of the motor (9) is drivingly connected to a rotating disk (3), and one end of the movable block (7) facing the rotating disk (3) is fixedly connected to a sliding pin (22), and an end surface of the rotating disk (3) is provided with a waist-shaped hole (8) for inserting the sliding pin (22), and one end of the waist-shaped hole (8) in the length direction is inclined and extends toward the radial outer side of the rotating disk (3); A measuring arm (6) fixedly connected to the movable block (7), wherein the outer wall of the mounting seat (2) is provided with a through slot for the measuring arm (6) to pass freely; The mounting seat (2) is provided with a guide column (4), and the movable block (7) is provided with a guide hole for the guide column (4) to pass freely. A blowing unit is provided on the measuring arm (6), the blowing unit comprising a cylinder (10) mounted on the outer wall of the movable block (7), the cylinder rod (21) of the cylinder (10) being drivingly connected to a piston (11), a connecting cavity (12) for engaging the piston (11) being provided in the measuring arm (6), the piston (11) sliding freely in the connecting cavity (12), a blowing hole (16) penetrating the connecting cavity (12) being provided on the outer wall of the measuring arm (6), a through hole for freely passing the cylinder rod (21) being coaxially provided on the end face of the piston (11), and a lower limit nut (16) being fixedly sleeved on the cylinder rod (21) 17), the upper end of the cylinder rod (21) is fixedly sleeved with an upper limit nut (20), the piston (11) is arranged between the upper limit nut (20) and the lower limit nut (17), a first spring (18) is sleeved around the cylinder rod (21), and the two ends of the elastic force direction of the first spring (18) elastically press against the lower limit nut (17) and the piston (11) in a one-to-one correspondence, and the piston (11) is provided with a mounting groove on one end surface facing the upper limit nut (20), and a pressure sensor (19) is installed in the mounting groove, and the surface of the pressure sensor (19) presses against the lower end surface of the upper limit nut (20); After the two measuring arms (6) move towards each other to a standard measuring distance, the wet film layers on the outer walls on both sides of the steel structure in the thickness direction also correspond to the two measuring arms (6) respectively. When the sum of the steel structure thickness and the wet film thickness is consistent with the distance between the two measuring arms (6), the surface of the measuring arm (6) is completely in contact with the wet film surface, and the wet film surface will block the air hole (16). Due to the blocking of the air hole (16), the cylinder rod (21) is further extended, so that the pressure of the first spring (18) is further increased, and when the piston (11) is pushed to move, the air in the connecting chamber (12) is squeezed. After the piston (11) is subjected to air resistance, when the cylinder rod (21) is extended, the piston (11) generates air pressure due to the blocking of the air hole (16), causing the piston (11) to be unable to follow the movement of the cylinder rod (21), thereby causing the pressure sensor (11) to be unable to move with ... The extrusion force of the upper limit nut (20) on the pressure sensor (19) is reduced, and the pressure signal of the pressure sensor (19) is fed back to the external control cabinet. The control cabinet determines whether the wet film thickness of the steel structure meets the standard according to the change of the pressure signal. The combined size of the structure thickness and the wet film thickness is smaller than the distance between the two measuring arms (6). At this time, there will be a gap between the surface of the measuring arm (6) and the surface of the wet film. The upward movement of the piston (11) will cause the air in the connecting cavity (12) to be discharged from the blowing hole (16), and the position of the piston (11) on the cylinder rod (21) will basically not change. As a result, the pressure sensor (19) is subjected to a smaller change in the extrusion force of the upper limit nut (20). In this way, the pressure signal fed back by the pressure sensor (19) to the external control cabinet changes less. The control cabinet can determine that the wet film thickness does not meet the standard according to the change range of the pressure signal.

2. The steel structure coating wet film measuring device according to claim 1 is characterized in that: A handle (1) is fixedly connected to one end of the mounting seat (2) away from the measuring arm (6).

3. The steel structure coating wet film measuring device according to claim 1, characterized in that: A chrome-plated layer is provided on one side of the measuring arm (6) where the blowing hole (16) is provided.

4. The steel structure coating wet film measuring device according to claim 1, characterized in that: An end surface of the measuring arm (6) away from the movable block (7) is connected to a storage cylinder (5), an outer wall of the storage cylinder (5) is provided with a liquid spraying microhole (15), the storage cylinder (5) is connected to the interior of the communicating cavity (12), and a pressurizing unit is provided in the storage cylinder (5).

5. The steel structure coating wet film measuring device according to claim 4, characterized in that: The pressurizing unit comprises a sliding plug (14) coaxially engaged in the storage cylinder (5); the sliding plug (14) slides freely in the storage cylinder (5); a second spring (13) is provided in the storage cylinder (5); two ends of the second spring (13) in the direction of elastic force respectively and elastically press against the sliding plug (14) and the inner top wall of the storage cylinder (5) in a one-to-one correspondence.

Citation Information

Patent Citations

  • Handheld wet film measuring device for steel structure coating

    CN113048896A

  • On-line detection system for film thickness on surface of enameled wire

    CN113304940A

  • Film thickness control device and rapid film coating method thereof

    CN114107934A

  • Thickness measuring device used in building board processing process

    CN116255919A

  • Glass fiber reinforced plastic curing forming device and method thereof