Wire mesh coating jig and sealing structure for plate-like member

By arranging high-rigidity clamps and sealing members on the surface of the plate-shaped member across the convex portion, and utilizing the split surface design, the problem of uneven height of the sealing member is solved and the sealing performance and uniformity of the sealing member are improved.

CN118721966AActive Publication Date: 2024-10-01HONDA MOTOR CO LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202410215919.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-03-31
Filing Date
2024-02-27
Publication Date
2024-10-01
Estimated Expiration
2044-02-27

AI Technical Summary

Technical Problem

When forming a closed space facing a plate material arranged in a concave and convex shape, it is difficult to ensure a uniform height of the sealing member in the prior art, which affects the sealing performance.

Method used

Design a screen coating jig in which the main body of the jig is composed of components with higher rigidity than the sealing member. The sealing member is provided on the surface of the plate-like member across the convex portion, and the main body of the jig is divided into multiple parts by dividing surfaces. section, ensuring that the height of the sealing member is uniform and the width narrows at the location of the convex portion to prevent overcoating.

Benefits of technology

It achieves a high degree of uniformity in screen-coating the sealing member across the convex portion on the surface of the plate-shaped member, improves the sealing performance, and prevents the sealing member from bulging and leaking at the convex portion.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118721966A_ABST
    Figure CN118721966A_ABST
Patent Text Reader

Abstract

A wire mesh coating jig (10B) for wire mesh coating a sealing member (7) on the surface of a plate-shaped member (3) having a convex portion (30) so as to straddle the convex portion (30) is provided with a jig body (11) that is configured from a member having higher rigidity than the sealing member and is placed on the surface of the plate-shaped member (3). The jig body (11) has: a first surface (11a) facing the surface of the plate-like member; a second surface (11b) on the opposite side of the first surface; and a pair of dividing surfaces (113, 113) extending from the first surface to the second surface and dividing at least a portion of the jig body into a first portion (111) and a second portion (112). The first surface has recessed portions (115, 115) that engage with the protruding portions of the plate-shaped member, starting from intersecting portions (114, 114) with the dividing surfaces. The height of the dividing surfaces from the first surface to the second surface is uniform, and the width between the pair of dividing surfaces becomes narrower at a position corresponding to the recess.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a screen coating jig for screen coating a sealing member on a plate-like member and a sealing structure of the plate-like member. Background Art

[0002] In the past, there is a known jig for screen-coating a paste-like member on a plate having a concave-convex shape, such as a separator of a fuel cell monomer. For example, in the jig described in Patent Document 1, a mating concave-convex portion capable of being embedded in the concave-convex portion formed on the coating target member is formed on the surface opposite to the coating target member in a mask provided integrally with the screen, and an opening for coating the paste is provided in at least one of the mating convex portion and the mating concave portion of the mating concave-convex portion.

[0003] Yet, when forming a confined space towards the plate material that is arranged in a concavo-convex shape, sometimes a sealing member that straddles the surface of the plate material is formed, and in such a case, in order to ensure the sealing property, it is preferred to make the height of the sealing member uniform. However, in patent document 1, there is no record of this point.

[0004] Prior art literature

[0005] Patent Literature

[0006] Patent Document 1: Japanese Patent Application Publication No. 2017-087504 (JP 2017-087504A). Summary of the invention

[0007] One technical solution of the present invention is a screen coating fixture for screen coating a sealing member on the surface of a plate-like member having a convex portion in a manner that straddles the convex portion. The screen coating fixture includes a fixture body, which is composed of a component with higher rigidity than the sealing member and is placed on the surface of the plate-like member. The fixture body has: a first surface, which is opposite to the surface of the plate-like member; a second surface on the opposite side of the first surface; and a pair of split surfaces, which extend from the first surface to the second surface and divide at least a portion of the fixture body into a first part and a second part. The first surface has a recessed portion that is engaged with the convex portion of the plate-like member with the intersection of the pair of split surfaces as a starting point. The height of the pair of split surfaces from the first surface to the second surface is uniform, and the width between the pair of split surfaces narrows at the position corresponding to the recessed portion.

[0008] A sealing structure of a plate-like member according to another technical solution of the present invention comprises: a plate-like member having a convex portion; and a sealing member provided on the surface of the plate-like member in a manner straddling the convex portion. The height of the sealing member from the surface of the plate-like member is uniform, and the width of the sealing member is narrowed at a position straddling the convex portion. BRIEF DESCRIPTION OF THE DRAWINGS

[0009] The objects, features and advantages of the present invention will be further clarified through the following description of the embodiments in conjunction with the accompanying drawings.

[0010] Figure 1 It is a perspective view schematically showing the overall structure of a fuel cell stack having a sealing structure of a plate-like member according to an embodiment of the present invention.

[0011] Figure 2 It is shown Figure 1 A three-dimensional diagram showing the schematic structure of an electrode assembly included in a fuel cell stack.

[0012] Figure 3 It is shown Figure 1 A cross-sectional view of a power generation cell along line III-III.

[0013] Figure 4 It is shown Figure 3 A front view of an example of a sealing structure near a through hole of a partition.

[0014] Figure 5 This is a front view showing an example of the screen coating jig according to the first embodiment of the present invention.

[0015] Figure 6 It is along Figure 5 VI-VI cross-sectional view.

[0016] Figure 7 It is partially shown Figure 5 A perspective view of a screen coating fixture.

[0017] Figure 8 yes Figure 4 A cross-sectional view of a sealing component.

[0018] Fig. 9 It is used to illustrate the composition Figure 4 Diagram of the characteristics of the resin material of the sealing member.

[0019] Fig.10 is to use Figure 5 A cross-sectional view of a sealing component coated by a screen coating fixture.

[0020] Fig.11 is to use Figure 5 A three-dimensional view of a sealing component coated by a screen coating fixture.

[0021] Fig.12 It is a perspective view partially showing a screen coating jig according to a second embodiment of the present invention.

[0022] Fig.13 is to use Fig.12 A cross-sectional view of a sealing component coated by a screen coating fixture.

[0023] Fig.14 is to use Fig.12 A three-dimensional view of a sealing component coated by a screen coating fixture.

[0024] Fig.15 This is a front view showing an example of a sealing structure of a plate-like member according to a second embodiment of the present invention. DETAILED DESCRIPTION

[0025] Below, refer to Figure 1 to Figure 15 The embodiments of the present invention are described. The screen coating jig of the embodiments of the present invention is a jig for screen coating a sealing member on the surface of a plate-like member having a convex portion in a manner straddling the convex portion, for example, a jig for screen coating a sealing member on a separator of a fuel cell arranged in a concave-convex shape. In addition, the sealing structure of the plate-like member of the embodiments of the present invention is a sealing structure provided on the surface of the plate-like member having a convex portion in a manner straddling the convex portion, for example, a sealing structure provided on the surface of a separator of a fuel cell arranged in a concave-convex shape. The fuel cell is mounted on a vehicle, for example, and can generate electricity for driving the vehicle. First, the overall structure of a fuel cell stack as a constituent element of the fuel cell is briefly described.

[0026] Figure 1 1 is a perspective view schematically showing the overall structure of a fuel cell stack 100 having a sealing structure of a plate-like member according to an embodiment of the present invention. For convenience, the following three mutually orthogonal axial directions are defined as the front-to-back direction, the left-to-right direction, and the up-to-down direction as shown in the figure, and the structure of each part is explained according to this definition. These directions are not necessarily the same as the front-to-back direction, the left-to-right direction, and the up-to-down direction of the vehicle. For example Figure 1 The front-to-back direction may be the front-to-back direction of the vehicle, may be the left-to-right direction, and may be the up-down direction.

[0027] like Figure 1 As shown, the fuel cell stack 100 has a battery stack 101 formed by stacking a plurality of power generation cells 1 in the front-to-back direction and end units 102 disposed at the front and rear ends of the battery stack 101, and is generally in a rectangular shape as a whole. The length of the battery stack 101 in the left-right direction is longer than the length in the up-down direction. For convenience, Figure 1 A single power generation cell 1 is shown in FIG. The power generation cell 1 has an electrode assembly 2 and separators 3, 3, wherein the electrode assembly 2 has a joint body including an electrolyte membrane and an electrode, and the separators 3, 3 are arranged on both the front and rear sides of the electrode assembly 2 and sandwich the electrode assembly 2. The electrode assembly 2 and the separators 3 are alternately arranged in the front-to-back direction.

[0028] The separator 3 has a pair of front and rear metal thin plates with a corrugated plate-like cross section, and the outer peripheries of these thin plates are joined to each other to form an integral body. The separator 3 uses a conductive material with good corrosion resistance, and can use, for example, titanium, titanium alloy, stainless steel, etc. A cooling flow channel for the flow of a cooling medium is formed inside the separator 3, and the power generation surface of the power generation cell 1 is cooled by the flow of the cooling medium. For example, water can be used as a cooling medium. The surface (front surface and rear surface) of the separator 3 opposite to the electrode assembly 2 is formed into a concave-convex shape by press molding, etc., so as to form a gas flow channel between the separator 3 and the electrode assembly 2.

[0029] The separator 3 on the front side of the electrode assembly 2 is, for example, a separator on the anode side (anode separator), and an anode flow channel for the fuel gas to flow is formed between the anode separator 3 and the joint body of the electrode assembly 2. The separator 3 on the rear side of the electrode assembly 2 is, for example, a separator on the cathode side (cathode separator), and a cathode flow channel for the oxidant gas to flow is formed between the cathode separator 3 and the joint body of the electrode assembly 2. For example, hydrogen can be used as the fuel gas, and for example, air can be used as the oxidant gas. Sometimes, the fuel gas and the oxidant gas are not distinguished, and they are referred to as reaction gases.

[0030] Figure 2 2 is a perspective view showing the schematic structure of the electrode assembly 2. Figure 2 As shown, the electrode assembly 2 has a substantially rectangular junction body 20 and a frame 21 supporting the junction body 20. The junction body 20 is a membrane electrode assembly (so-called MEA; Membrane Electrode Assembly) having an electrolyte membrane, an anode electrode provided on the front surface of the electrolyte membrane, and a cathode electrode provided on the rear surface of the electrolyte membrane.

[0031] The electrolyte membrane is, for example, a solid polymer electrolyte membrane, and a perfluorosulfonic acid membrane containing water can be used. In addition to a fluorine-based electrolyte, a hydrocarbon-based electrolyte can also be used.

[0032] The anode electrode is an electrode catalyst layer formed on the front surface of the electrolyte membrane and serving as a reaction field for the electrode reaction, and a gas diffusion layer for diffusing and supplying the reaction gas is provided on the front surface of the electrode catalyst layer. The cathode electrode is an electrode catalyst layer formed on the rear surface of the electrolyte membrane and serving as a reaction field for the electrode reaction, and a gas diffusion layer for diffusing and supplying the reaction gas is provided on the rear surface of the electrode catalyst layer. The electrode catalyst layer includes a catalytic metal that promotes the electrochemical reaction of hydrogen contained in the fuel gas and oxygen contained in the oxidant gas, an electrolyte having proton conductivity, carbon particles having electron conductivity, and the like. The gas diffusion layer is composed of a conductive member having gas permeability, such as porous carbon.

[0033] At the anode electrode, the fuel gas (hydrogen) supplied through the anode flow channel and the gas diffusion layer is ionized by the action of the catalyst and moves to the cathode electrode side through the electrolyte membrane. The electrons generated at this time are taken out as electrical energy through the external circuit. At the cathode electrode, the oxidant gas (oxygen) supplied through the cathode flow channel and the gas diffusion layer reacts with the hydrogen ions derived from the anode electrode and the electrons moved from the anode electrode to generate water. The generated water provides appropriate humidity to the electrolyte membrane, and the remaining water is discharged to the outside of the electrode assembly 2.

[0034] The frame 21 is a thin plate in a generally rectangular shape, and is made of insulating resin, rubber, etc. A generally rectangular opening 21a is provided in the central portion of the frame 21, and the joint body 20 is provided in a manner covering the entire opening 21a. On the left side of the opening 21a of the frame 21, three through holes 211 to 213 that penetrate the frame 21 in the front-to-back direction are opened in a row in the vertical direction, and on the right side of the opening 21a, three through holes 214 to 216 that penetrate the frame 21 in the front-to-back direction are opened in a row in the vertical direction.

[0035] like Figure 1 As shown, through holes 311 to 316 that penetrate the separator 3 in the front and rear directions are respectively provided at positions corresponding to the through holes 211 to 216 of the frame 21 on the front and rear of the electrode assembly 2. The through holes 311 to 316 are respectively connected to the through holes 211 to 216 of the frame 21. The collection of these interconnected through holes 211 to 216, 311 to 316 forms flow passages PA1 to PA6 (indicated by arrows for convenience) that penetrate the battery stack 101 and extend in the front and rear directions. The flow passages PA1 to PA6 are sometimes also referred to as manifolds. The flow passages PA1 to PA6 are connected to the manifold outside the fuel cell stack 100.

[0036] The flow channel PA1 (solid arrow) extending forward through the through holes 211 and 311 is the fuel gas supply flow channel. The flow channel PA6 (solid arrow) extending backward through the through holes 216 and 316 is the fuel gas exhaust flow channel. The fuel gas supply flow channel PA1 and the fuel gas exhaust flow channel PA6 are connected to the anode flow channel opposite to the front surface of the joint 20. As shown by the solid arrows, the fuel gas flows in the left and right directions in the anode flow channel via the fuel gas supply flow channel PA1 and the fuel gas exhaust flow channel PA6. The connection between the anode flow channel and the other flow channels PA2 to PA5 is provided by the sealing member 7 ( Figure 3 ) is cut off. The fuel gas flowing in the fuel gas exhaust flow channel PA6 is a portion of the fuel gas after being used in the anode electrode, and is sometimes referred to as fuel exhaust gas.

[0037] The flow channel PA4 (dashed arrow) extending forward through the through holes 214 and 314 is the oxidant gas supply flow channel. The flow channel PA3 (dashed arrow) extending backward through the through holes 213 and 313 is the oxidant gas exhaust flow channel. The oxidant gas supply flow channel PA4 and the oxidant gas exhaust flow channel PA3 are connected to the cathode flow channel opposite to the rear surface of the joint 20. As shown by the dashed arrows, the oxidant gas flows in the left and right directions in the cathode flow channel via the oxidant gas supply flow channel PA4 and the oxidant gas exhaust flow channel PA3. The connection between the cathode flow channel and the other flow channels PA1, PA2, PA5, and PA6 is provided by the sealing member 7 ( Figure 3 ) is cut off. The oxidant gas flowing in the oxidant gas exhaust flow channel PA3 is a part of the oxidant gas after being used at the cathode electrode, and is sometimes referred to as oxidant waste gas. Sometimes, fuel waste gas and oxidant waste gas are not distinguished, and they are called reaction waste gas.

[0038] The flow channel PA5 (single-dot dash arrow) extending forward through the through holes 215 and 315 is the cooling medium supply flow channel. The flow channel PA2 (single-dot dash arrow) extending backward through the through holes 212 and 312 is the cooling medium discharge flow channel. The cooling medium supply flow channel PA5 and the cooling medium discharge flow channel PA2 are connected to the cooling flow channel inside the partition 3, and the cooling medium flows in the cooling flow channel through the cooling medium supply flow channel PA5 and the cooling medium discharge flow channel PA2. The connection between the cooling flow channel and other flow channels PA1, PA3, PA4, and PA6 is provided by the sealing member 7 ( Figure 3 ) cut off.

[0039] The end units 102 disposed on the front and rear sides of the battery stack 101 respectively include a connection plate 4, an insulating plate 5, and an end plate 6. It should be noted that the front end unit 102 is sometimes referred to as a dry-side end unit, and the rear end unit 102 is sometimes referred to as a wet-side end unit. A pair of front and rear connection plates 4, 4 are disposed on the front and rear sides of the battery stack 101. A pair of front and rear insulating plates 5, 5 are disposed on the front and rear sides of the connection plates 4, 4. A pair of front and rear end plates 6, 6 are disposed on the front and rear sides of the insulating plates 5, 5.

[0040] The terminal plate 4 is a metal, generally rectangular plate-shaped member having a terminal portion for extracting the electricity generated by the electrochemical reaction in the battery stack 101. The insulating plate 5 is a non-conductive, generally rectangular plate-shaped member made of resin or rubber, and electrically insulates the terminal plate 4 from the end plate 6. The end plate 6 is a metal or high-strength resin plate-shaped member, and a connecting member elongated in the front-to-back direction, for example, that connects the front and rear end plates 6, 6 to each other, is fixed to the end plate 6 by bolts. The fuel cell stack 100 is maintained in a state where the end plates 6, 6 are pressed in the front-to-back direction by the connecting member. A shell surrounding the battery stack 101 may be used as a connecting member, or the end plates 6, 6 may be fixed to the front and rear faces of the shell, respectively.

[0041] The rear end unit 102 is provided with a plurality of through holes 102a to 102f that penetrate the end unit 102 in the front-to-back direction. It should be noted that the through holes 102a to 102f include through holes that penetrate the wiring board 4, through holes that penetrate the insulating board 5, and through holes that penetrate the end plate 6, respectively. Figure 1 In the figure, these are collectively shown as through holes 102a to 102f. The through hole 102a is opened on the extension line of the fuel gas supply flow channel PA1 and is connected to the fuel gas supply flow channel PA1. The through hole 102b is opened on the extension line of the cooling medium exhaust flow channel PA2 and is connected to the cooling medium exhaust flow channel PA2. The through hole 102c is opened on the extension line of the oxidant gas exhaust flow channel PA3 and is connected to the oxidant gas exhaust flow channel PA3. The through hole 102d is opened on the extension line of the oxidant gas supply flow channel PA4 and is connected to the oxidant gas supply flow channel PA4. The through hole 102e is opened on the extension line of the cooling medium supply flow channel PA5 and is connected to the cooling medium supply flow channel PA5. The through hole 102f is opened on the extension line of the fuel gas exhaust flow channel PA6 and is connected to the fuel gas exhaust flow channel PA6.

[0042] In more detail, a fuel gas tank storing high-pressure fuel gas is connected to the through hole 102a via an ejector, an injector, etc., and the fuel gas in the fuel gas tank is supplied to the fuel cell stack 100 via the through hole 102a. A gas-liquid separator is connected to the through hole 102f, and the fuel gas (fuel exhaust gas) discharged via the through hole 102f is separated into fuel gas and water in the gas-liquid separator. The separated fuel gas is sucked in via the ejector and then supplied to the fuel cell stack 100. The separated water is discharged to the outside via the drainage channel.

[0043] A compressor for supplying oxidant gas is connected to the through hole 102d, and the oxidant gas compressed by the compressor is supplied to the fuel cell stack 100 via the through hole 102d. The oxidant gas (oxidant exhaust gas) flows out to the outside from the through hole 102c. A pump for supplying a cooling medium is connected to the through hole 102e, and the cooling medium is supplied to the fuel cell stack 100 via the through hole 102e. The cooling medium is discharged from the through hole 102b. The discharged cooling medium is cooled by heat exchange in the radiator and is supplied to the fuel cell stack 100 again via the through hole 102e.

[0044] The above is a schematic structure of the fuel cell stack 100. The fuel cell stack 100 is accommodated in a substantially box-shaped casing and mounted on a vehicle.

[0045] Figure 3 yes Figure 1 A cross-sectional view of the power generation cell 1 along line III-III. Figure 3 As shown, an anode flow channel An is formed between the anode separator 3 and the electrode assembly 2 (joined body 20) on the front side, and a cathode flow channel Ca is formed between the cathode separator 3 and the electrode assembly 2 (joined body 20) on the rear side. Figure 4 It is a front view showing an example of a sealing structure near the through hole 311 (fuel gas supply flow path PA1) of the separator (anode separator) 3, and shows the surface (rear surface) near the through hole 311 of the separator 3 opposite to the electrode assembly 2 (frame 21).

[0046] like Figure 3 and Figure 4 As shown, a plurality of (only one is shown in the figure) semi-cylindrical convex portions 30 are provided on the surface of the separator 3 opposite to the electrode assembly 2, and the convex portions 30 form connecting channels that connect the through holes 311, 314 (reaction gas supply channels PA1, PA4) with the gas channels An, Ca. Among these connecting channels, the connecting channel that connects the fuel gas supply channel PA1 with the cathode channel Ca and the connecting channel that connects the oxidant gas supply channel PA4 with the anode channel An are closed.

[0047] A sealing member 7 is provided on the surface of the separator 3 in such a manner as to cross the convex portion 30 and surround the through holes 311 and 314. A resin material such as a thermosetting elastomer such as silicon, polyurethane, and fluorine, a thermoplastic elastomer, a synthetic rubber, and a natural rubber can be used as the sealing member 7. The top end of the sealing member 7 provided on the surface of the separator 3 is in close contact with the electrode assembly 2 (frame 21), thereby the reaction gas supply flow channels PA1 and PA4 are cut off (sealed) from the unconnected gas flow channels Ca and An and the external space EX.

[0048] More specifically, Figure 1The fuel cell stack 100 is pressed in the front-to-back direction by the end plates 6, 6 via the connecting member, thereby applying a compressive load in the front-to-back direction to the sealing member 7, and the sealing member 7 is pressed to elastically deform, and the top end of the sealing member 7 is in close contact with the electrode assembly 2 (frame 21). At this time, the compressive load applies surface pressure to the top end of the sealing member 7, thereby ensuring the sealing state of the reaction gas supply flow channels PA1, PA4.

[0049] Thus, when a closed space is formed facing a plate-like member such as a partition plate 3 having a protrusion 30, it is preferable to make the height of the sealing member 7 uniform in order to ensure the sealing property. Therefore, in the present embodiment, a screen coating jig is constructed as follows so that the surface of the partition plate 3 having a protrusion 30 is screen-coated with a sealing member 7 having a uniform height across the protrusion 30.

[0050] <First embodiment>

[0051] Figure 5 1 is a front view showing an example of a screen coating jig (hereinafter referred to as a jig) 10A according to the first embodiment of the present invention. Figure 6 It is along Figure 5 The VI-VI cross-sectional view. Figure 5 and Figure 6 As shown, the jig 10A includes a jig body 11 placed on the surface of the separator 3 as the coating surface, and a connecting portion 12 connecting a first portion 111 and a second portion 112 of the jig body 11 .

[0052] The clamp body 11 and the connecting portion 12 are composed of a member having a higher rigidity than the sealing member 7. The clamp body 11 and the connecting portion 12 can use metals such as stainless steel. The clamp body 11 and the connecting portion 12 can also use materials that have been waterproofed with resins such as Teflon (registered trademark) and silicon. Considering the material of the sealing member 7, the width of the connecting portion 12 is set to a sufficiently small value (for example, about 100 μm) to avoid generating a height difference on the surface of the sealing member 7 after coating.

[0053] The clamp body 11 has a first surface 11a opposite to the surface of the partition plate 3, a second surface 11b on the opposite side of the first surface 11a, and a pair of dividing surfaces 113, 113 extending from the first surface 11a to the second surface 11b and dividing the clamp body 11 into a first portion 111 and a second portion 112. Figure 5In the example of , the pair of dividing surfaces 113, 113 is set in an annular shape, and the clamp body 11 is completely divided into the inner first part 111 and the outer second part 112 surrounded by the pair of dividing surfaces 113, 113. The pair of dividing surfaces 113, 113 can also be set in a line segment shape or a curve segment shape to partially divide the clamp body 11 into the first part 111 and the second part 112. In this case, the connecting portion 12 connecting the first part 111 and the second part 112 can also be omitted, and the clamp 10A is composed of only the clamp body 11. Hereinafter, the space between the first part 111 and the second part 112, in other words, the space between the first surface 11a and the second surface 11b and between the pair of dividing surfaces 113, 113 is referred to as the groove portion 13.

[0054] The jig body 11 is formed by, for example, forming a lower layer 14 including a first surface 11a and an upper layer 15 including a second surface 11b as separate bodies, and joining the lower layer 14 and the upper layer 15. In this case, the lower layer 14 includes a first portion 111 and a second portion 112, and the upper layer 15 includes a first portion 111, a second portion 112, and a connecting portion 12. The jig body 11 and the connecting portion 12 may be formed integrally, and the jig body 11 may be divided into the first portion 111 and the second portion 112 and the connecting portion 12 may be formed by processing such as etching or rolling.

[0055] Figure 7 1 is a perspective view partially showing the jig 10A, schematically showing a state where the sealing member 7 is screen-coated on the surface of the partition plate 3 having the protrusion 30 in a manner straddling the protrusion 30 using the jig 10A. Figure 7 As shown, in screen coating, first, the jig 10A is placed on the surface of the partition 3 as the coating surface so that the first surface 11a of the jig body 11 faces the surface of the partition 3 having the protrusion 30. Next, a paste P of a resin material such as a thermosetting elastomer such as silicone, polyurethane, fluorine, a thermoplastic elastomer, a synthetic rubber, or a natural rubber having thixotropy is placed on the second surface 11b of the jig body 11. Then, the paste P is pushed to the second surface 11b around the groove 13 by the scraper 16, and the scraper 16 is slid to apply the paste P to the surface of the partition 3 through the groove 13, and the paste is hardened to coat and form the sealing member 7 on the surface of the partition 3. Such screen coating can be performed manually or automatically using a screen printing device having a mounting table for fixing the partition 3, the jig 10A, and the scraper 16.

[0056] The first surface 11a of the clamp body 11 has a pair of recesses 115, 115, and the pair of recesses 115, 115 are engaged with the protrusion 30 of the partition plate 3 from the intersections 114, 114 with the pair of dividing surfaces 113, 113 as starting points. One of the pair of recesses 115, 115 is provided at the first portion 111 of the clamp body 11, and the other is provided at the second portion 112 of the clamp body 11. When the clamp body 11 is made of metal, a material that has been waterproofed by resin such as Teflon (registered trademark) or silicone may be used only for the recesses 115.

[0057] By providing the concave portion 115 that fits with the convex portion 30 on the surface of the partition plate 3 on the first surface 11a of the jig body 11 opposite to the coating surface, it is possible to limit the displacement of the jig body 11 relative to the coating surface even when a pressing force is applied to the jig 10A in the sliding direction of the scraper 16 during coating. As a result, screen coating can be accurately performed on the surface of the partition plate 3.

[0058] In this way, by performing screen coating using the jig body 11 and the scraper 16 having relatively higher rigidity than the sealing member 7 , it is possible to prevent the sealing member 7 from being coated outside the groove 13 , and to coat and form the sealing member 7 in a shape along the shape of the groove 13 .

[0059] The fixture body 11 is formed so that the depth of the groove 13 is uniform, that is, the height h1 from the first surface 11a to the second surface 11b of the pair of dividing surfaces 113, 113 is uniform. Therefore, the height of the sealing member 7 coated and formed along the shape of the groove 13 defined by the pair of dividing surfaces 11313 of the fixture body 11, the first surface 11a (the surface of the partition 3) and the second surface 11b (the scraper 16) can be made substantially uniform.

[0060] Figure 8 is a cross-sectional view of a sealing member 7 coated on the surface of a partition plate 3, Fig. 9 2 is a diagram for explaining the characteristics (thixotropic characteristics) of the resin material constituting the sealing member 7. Figure 8 and Fig. 9 As shown, when the coating conditions such as the composition of the paste P are the same, the thickness d of the sealing member 7 made of the thixotropic resin material after curing is determined according to the width w of the portion in contact with the surface of the partition 3. That is, the larger (wider) the width w of the sealing member 7 is, the larger (higher) the thickness d of the sealing member 7 is, and the smaller (narrower) the width w of the sealing member 7 is, the smaller (lower) the thickness d of the sealing member 7 is. The width w of the sealing member 7 is equivalent to the width w of the groove 13 of the clamp 10A, that is, the width w between the pair of dividing surfaces 113, 113 of the clamp body 11 is equivalent.

[0061] Fig.10 is a cross-sectional view of the sealing member 7 coated by the jig 10A. Fig.11 1 is a perspective view of the sealing member 7 coated by the jig 10A. Fig.10 and Fig.11 As shown, the width w and thickness d of the sealing member 7 coated by the jig 10A are uniform in the entire extension direction of the sealing member 7. The sealing member 7 extends along the surface of the partition 3 including the protrusion 30, so the height h2 of the sealing member 7 from the surface of the partition 3 is higher than the height of the protrusion 30 at the position where the sealing member 7 crosses the protrusion 30 than at other positions.

[0062] Thus, when the height h2 of the sealing member 7 from the surface of the partition plate 3 fluctuates, Figure 4 In the extending direction of the sealing member 7, applied to Figure 3 The line pressure (sealing load) at the top of the sealing member 7 in close contact with the electrode assembly 2 (frame 21) fluctuates, and leakage may occur at the position where the line pressure is low. It should be noted that the line pressure is the average value per unit length of the surface pressure applied to the top of the sealing member 7 in close contact with the electrode assembly 2 (frame 21) by the compressive load in the extending direction of the sealing member 7.

[0063] <Second embodiment>

[0064] Fig.12 1 is a perspective view partially showing a clamp 10B according to a second embodiment of the present invention. Fig.13 is a cross-sectional view of the sealing member 7 coated by the jig 10B, Fig.14 1 is a perspective view of the sealing member 7 coated by the jig 10B. The difference from the first embodiment is described below. The jig 10B is configured such that the width w between the pair of split surfaces 113, 113 of the jig body 11 (the width w of the groove 13) is narrowed at a position corresponding to the recess 115. More specifically, as Fig.12 As shown, the width w1 of the groove portion 13 at the position corresponding to the recessed portion 115 is set to a smaller value than the width w2 of the groove portion 13 at other positions (w1<w2).

[0065] In this case, if Fig.13 and Fig.14 As shown in FIG. 1 , the height h2 of the sealing member 7 from the surface of the partition 3 applied by the jig 10B is uniform in the entire extension direction of the sealing member 7. That is, the width w1 of the sealing member 7 at the position where the sealing member 7 crosses the convex portion 30 is smaller than the width w2 of the sealing member 7 at other positions, and the thickness d of the sealing member 7 at the position where the sealing member 7 crosses the convex portion 30 is smaller than that at other positions. As a result, the height h2 of the sealing member 7 from the surface of the partition 3 is uniform in the entire extension direction of the sealing member 7, and the sealing member 7 applied to the convex portion 30 is uniform. Figure 3The fluctuation of the line pressure (sealing load) at the top of the sealing member 7 which is in close contact with the electrode assembly 2 (frame 21) is eliminated, and the sealing performance is improved.

[0066] The widths w1 and w2 of the groove 13 of the sealing member 7 and the fixture 10B are set according to the maximum pressure of the gas flowing in the gas flow path, the material of the sealing member 7, the compressive load applied to the sealing member 7, etc. The ratio of the width w1 to the width w2 can also be determined based on the coating position of the sealing member 7 on the surface of the partition plate 3, the shape of the protrusion 30, Fig. 9 The value may be determined by the properties of the resin material shown in FIG. 1 , or by trial production of the jig 10B (jig body 11 ) and the sealing member 7 .

[0067] Fig.15 1 is a front view showing an example of a sealing structure of a plate-like member according to the second embodiment, showing a sealing structure near a through hole 311 (fuel gas supply passage PA1) of a separator (anode separator) 3 facing an electrode assembly 2 (frame 21). Fig.15 As shown, the sealing structure of the plate-like member includes: a partition 3 having a convex portion 30; and a sealing member 7, which is provided on the surface of the partition 3 in a manner straddling the convex portion 30. The height h2 of the sealing member 7 from the surface of the partition 3 is uniform, and the width w (w1, w2) of the sealing member 7 is narrowed at the position straddling the convex portion 30.

[0068] Thus, in the second embodiment, unlike the first embodiment, the jig 10B is configured such that the width w between the pair of dividing surfaces 113, 113 of the jig body 11 (the width w of the groove 13) is narrowed at the position corresponding to the recess 115, thereby forming a sealing member 7 of uniform height. In addition, the height h1 of the groove 13 of the jig 10B is uniform, so that the sealing member 7 along the shape of the groove 13 can be formed by one-time screen coating using the scraper 16 as in the first embodiment.

[0069] The present embodiment can achieve the following effects.

[0070] (1) A jig 10B for screen-coating a sealing member 7 on a surface of a separator 3 having a protrusion 30 in a manner straddling the protrusion 30 includes a jig body 11 ( Fig.12). The clamp body 11 has a first surface 11a opposite to the surface of the partition 3; a second surface 11b on the opposite side of the first surface 11a; and a pair of dividing surfaces 113, 113 extending from the first surface 11a to the second surface 11b and dividing at least a portion of the clamp body 11 into a first portion 111 and a second portion 112. The first surface 11a has recesses 115, 115, and the recesses 115, 115 are engaged with the protrusion 30 of the partition 3 with the intersection 114, 114 with the pair of dividing surfaces 113, 113 as the starting point. The height h1 of the pair of dividing surfaces 113, 113 from the first surface 11a to the second surface 11b is uniform, and the width w between the pair of dividing surfaces 113, 113 is narrowed at the position corresponding to the recesses 115, 115.

[0071] In this way, by providing the recessed portion 115 that fits with the convex portion 30 on the surface of the partition 3, it is possible to limit the displacement of the jig body 11 relative to the coating surface during coating, and screen coating can be accurately performed on the surface of the partition 3. In addition, by using the jig body 11 with relatively higher rigidity than the sealing member 7 for screen coating, it is possible to prevent the sealing member 7 from being applied outside the groove portion 13, and to coat and form the sealing member 7 in a shape along the shape of the groove portion 13. In addition, by making the depth (height) h1 of the groove portion 13 uniform, it is possible to form the sealing member 7 by a single screen coating using the scraper 16. In addition, by narrowing the width w of the groove portion 13 at the position corresponding to the recessed portion 115 that fits with the convex portion 30 on the surface of the partition 3, it is possible to prevent the sealing member 7 from bulging at a position across the convex portion 30, and to form a sealing member 7 with a uniform height h2.

[0072] (2) The convex portion 30 is configured to have a curved cross-sectional shape, for example, a semi-cylindrical shape ( Fig.12 ). Even when the convex portion 30 is bent and the sealing member 7 applied on the convex portion 30 is easy to expand, by narrowing the width w of the groove portion 13 and the sealing member 7 at the position across the convex portion 30, it is possible to prevent bulging at the position across the convex portion 30, and it is possible to form a sealing member 7 with a uniform height h2.

[0073] (3) The pair of dividing surfaces 113, 113 surrounds one of the first portion 111 and the second portion 112 ( Fig.12 The jig 10B further includes a connecting portion 12 that connects the first portion 111 and the second portion 112. Even when the pair of dividing surfaces 113, 113 (groove portion 13) are provided in an annular shape and the jig body 11 is completely divided, the provision of the connecting portion 12 enables accurate screen coating.

[0074] (4) The sealing member 7 is a resin member. Even if the sealing member 7 is coated via the groove portion 13 of the fixture 10, the aspect ratio of the width w to the thickness d after curing is determined by the thixotropy of the resin material. In view of such characteristics, by narrowing the width w at the position of the convex portion 30 across which the thickness d should be reduced, the height h2 of the sealing member 7 from the surface of the partition 3 after curing can be made uniform.

[0075] (5) The sealing structure of the plate-like member comprises: a partition plate 3 having a convex portion 30; and a sealing member 7 provided on the surface of the partition plate 3 so as to straddle the convex portion 30 ( Figure 13 to Figure 15 The height h2 of the sealing member 7 from the surface of the partition 3 is uniform, and the width w of the sealing member 7 is narrowed at a position across the convex portion 30. When the sealing member 7 is used to form a sealed space facing a plate-like member such as the partition 3 having the convex portion 30, the height h2 of the sealing member 7 is made uniform, thereby ensuring the sealing property of the sealed space.

[0076] In the above-mentioned embodiment, the wire mesh coating jig and the sealing structure of the separator 3 for wire mesh coating the sealing member 7 on the surface of the separator 3 of the fuel cell in a manner spanning the convex portion 30 forming the connecting channel of the gas are described as an example, but the sealing structure of the wire mesh coating jig and the plate-like member is not limited to this. The convex portion can be any member protruding from the surface of the plate-like member on which the sealing member is coated, and is not limited to the hollow structure forming the connecting channel of the gas, etc. The sealing member can be any member spanning the convex portion, and the extension direction of the convex portion does not need to be orthogonal to the extension direction of the sealing member. The surface of the plate-like member can be any member having a convex portion and a portion other than the convex portion, and the area occupied by the convex portion does not need to be smaller than the area occupied by the portion other than the convex portion. For example, for a plate-like member having a recessed portion such as a groove in a portion, the portion other than the recessed portion can also be regarded as a convex portion to apply the present invention. In this case, by making the width of the sealing member wider at the position straddling the recessed portion of such a plate-like member, and making the width between a pair of dividing surfaces of the clamp body wider at the position corresponding to the convex portion that fits into the recessed portion of such a plate-like member, a highly uniform sealing member can be formed.

[0077] One or more of the above-described embodiments and modifications may be arbitrarily combined, and modifications may be combined with each other.

[0078] According to the present invention, a highly uniform sealing member can be formed.

[0079] The present invention has been described above in conjunction with the preferred embodiments, but it should be understood by those skilled in the art that various modifications and changes can be made without departing from the scope of the disclosure of the claims set forth below.

Claims

1. A screen coating jig (10B) for screen coating a sealing member (7) on a surface of a plate-like member (3) having a convex portion (30) in a manner straddling the convex portion (30), characterized in that: have: a clamp body (11) which is composed of a member having higher rigidity than the sealing member (7) and is placed on the surface of the plate-like member (3); The clamp body (11) has: a first surface (11a) which is opposite to a surface of the plate-like member (3); a second surface (11b) on the opposite side of the first surface (11a); and a pair of dividing surfaces (113, 113) extending from the first surface (11a) to the second surface (11b) to divide at least a portion of the clamp body (11) into a first portion (111) and a second portion (112), The first surface (11a) has recessed portions (115, 115), and the recessed portions (115, 115) are engaged with the convex portion (30) of the plate-like member (3) starting from the intersection (114, 114) with the pair of dividing surfaces (113, 113). The pair of dividing surfaces (113, 113) have a uniform height from the first surface (11a) to the second surface (11b), The width between the pair of dividing surfaces (113, 113) is narrowed at positions corresponding to the recessed portions (115, 115).

2. The screen coating fixture (10B) according to claim 1, characterized in that: The convex portion (30) has a curved cross-sectional shape.

3. The screen coating jig (10B) according to claim 1 or 2, characterized in that: The pair of dividing surfaces (113, 113) surrounds one of the first portion (111) and the second portion (112), The screen coating jig (10B) further comprises a connecting portion (12) for connecting the first portion (111) and the second portion (112).

4. The screen coating jig (10B) according to claim 3, characterized in that: The pair of dividing surfaces (113, 113) are arranged in an annular shape.

5. The screen coating jig (10B) according to claim 1 or 2, characterized in that: The sealing member (7) is a resin member.

6. The screen coating jig (10B) according to claim 5, characterized in that: The ratio of the width between the pair of dividing surfaces (113, 113) at a position corresponding to the recessed portion (115, 115) to the width between the pair of dividing surfaces (113, 113) at a position other than the position is determined according to the thixotropic property of the resin material.

7. The screen coating jig (10B) according to claim 1 or 2, characterized in that: The convex portion (30) is a hollow member that forms a fluid communication channel on the surface of the plate-like member (3).

8. A sealing structure of a plate-like member (3), characterized in that: have: a plate-like member (3) having a convex portion (30); and a sealing member (7) provided on the surface of the plate-like member (3) in a manner straddling the convex portion (30), The height of the sealing member (7) from the surface of the plate-like member (3) is uniform, The width of the sealing member (7) is narrowed at a position straddling the convex portion (30).

Citation Information

Patent Citations

  • Power generation cell

    CN109428092A

  • Metal separator

    CN113394423A

  • Printed circuit board and mask of screen printing such printed circuit bard

    CN1283954A

  • Printing plate, printing machine, printing method, and apparatus for manufacturing liquid crystal device, and method for manufacturing the same

    CN1668477A

  • SMT steel mesh

    CN208424964U