Gluing and developing device, system and control method

By setting up the interlayer module and cooling unit in the glue coating and development equipment, the problem of long waiting time for the robot caused by the temperature difference between the liquid treatment module and the heat treatment module is solved, the utilization rate of the robot and the product yield are improved, and the glue coating and development device is improved of production capacity.

CN118732402APending Publication Date: 2024-10-01KINGSEMI CO LTD

Patent Information

Application Number
CN202411230404.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-04
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

In existing glue coating and development equipment, the temperature difference between the liquid processing module and the heat treatment module causes the robot to wait for a long time when transferring the wafer, affecting the process results and reducing the product yield.

Method used

An interlayer module is set up between the liquid processing module and the heat treatment module for temporary storage of wafers, and a cooling unit is set up in the interlayer module to ensure smooth transition of the wafers between different processing stages and shorten the time for the robot to transfer the wafers. Waiting time.

Benefits of technology

Through the setting of inter-layer modules, the utilization rate of the robot is improved, ensuring that the temperature during liquid processing meets the process requirements, and improving the production capacity and product yield of the glue coating and developing device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118732402A_ABST
    Figure CN118732402A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of gluing and developing in semiconductor manufacturing, and provides a gluing and developing device and system and a control method, and the device comprises a liquid treatment module which is used for carrying out a liquid treatment process including surface coating and developing treatment on a wafer; the heat treatment module is used for carrying out a heat treatment process including baking treatment on the wafer; and the interlayer module is positioned between the liquid treatment module and the heat treatment module and is used for storing a wafer so as to link the heat treatment process and the liquid treatment process. The device is used for improving the utilization rate of the manipulator in the gluing and developing device.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of glue coating and developing in semiconductor manufacturing, and in particular to a glue coating and developing device, system and control method. Background Art

[0002] In the prior art, the liquid treatment unit and the heat treatment unit of the glue coating and developing equipment are placed in the same module, and the working temperature of the heat treatment module is higher than that of the liquid treatment module. A robot has to take both the liquid-treated wafer and the heat-treated wafer, which may affect the process results of the liquid treatment, such as affecting the film thickness on the wafer surface, resulting in a decrease in the yield of the wafer product. Therefore, a glue coating and developing device, system and control method are urgently needed to improve the above problems. Summary of the invention

[0003] The object of the present invention is to provide a glue coating and developing device, a system and a control method, which are used to improve the utilization rate of a robot in the glue coating and developing device.

[0004] In the first aspect, the present invention provides a coating and developing device, comprising: a liquid treatment module, used to perform a liquid treatment process including surface coating and developing treatment on a wafer; a heat treatment module, used to perform a heat treatment process including baking treatment on the wafer; an interlayer module, located between the liquid treatment module and the heat treatment module, used to store the wafer to connect the heat treatment process and the liquid treatment process. The beneficial effect is that the interlayer module is provided to temporarily store the wafer between the liquid treatment module and the heat treatment module, ensuring that the wafer can smoothly transition between different processing stages, and shortening the waiting time when the robot in each module transfers the wafer as much as possible.

[0005] Optionally, each frame layer in the interlayer module is provided with a plurality of interfaces for storing wafers; each time the same wafer enters the same frame layer of the interlayer module, it is stored in different interfaces in the frame layer.

[0006] Optionally, a cooling unit is provided in at least one frame layer of the interlayer module; the cooling unit is coupled to the interface; and when the cooling unit is in contact with the wafer, it is used to cool the wafer.

[0007] Optionally, the liquid processing module includes at least one layer of wafer feeding liquid processing frame and at least one layer of wafer returning liquid processing frame; a coating component is provided in the wafer feeding liquid processing frame for coating photoresist or anti-reflective layer on the wafer surface; a robot in the wafer feeding liquid processing frame is used to move the wafer from the coating component to the interface in the interlayer module; a developing unit is provided in the wafer returning liquid processing frame for developing the wafer; and the robot in the wafer returning liquid processing frame is used to move the wafer from the interface in the interlayer module to the developing unit.

[0008] Optionally, the heat treatment module includes at least one layer of wafer feeding heat treatment frame and at least one layer of wafer returning heat treatment frame; a soft baking unit is provided in the wafer feeding heat treatment frame for pre-treating the coating on the surface of the wafer; a robot in the wafer feeding heat treatment frame is used to move the wafer from the interface in the interlayer module to the soft baking unit; a hard baking unit is provided in the wafer returning heat treatment frame for curing the coating on the surface of the wafer; and the robot in the wafer returning heat treatment frame is used to move the wafer after the surface coating is cured to the interface in the interlayer module.

[0009] Optionally, the coating component includes a glue coating unit and an anti-reflection unit; the anti-reflection unit is used to coat an anti-reflection layer on the surface of the wafer; the robot in the wafer feeding liquid processing frame is used to move the wafer from the anti-reflection unit to the interface in the interlayer module; the glue coating unit is used to coat photoresist on the surface of the wafer; the robot in the wafer feeding liquid processing frame is used to move the wafer from the interface where the cooling unit is provided in the interlayer module to the glue coating unit, and to move the wafer from the glue coating unit to the interface in the interlayer module.

[0010] Optionally, the robot in the film return liquid processing frame is used to move the wafer from the interface of the interlayer module provided with the cooling unit to the developing unit; and to move the wafer from the developing unit to the interface in the interlayer module.

[0011] Optionally, the coating and developing device is further provided with an edge exposure unit for exposing the edge of the wafer.

[0012] Optionally, an anti-reflection baking unit is also provided in the wafer feeding heat treatment frame, which is used to dry the anti-reflection layer on the surface of the wafer; the robot in the wafer feeding heat treatment frame is used to move the wafer from the interface in the interlayer module to the anti-reflection baking unit, and to move the wafer from the anti-reflection baking unit to the cooling unit in the interlayer module.

[0013] Optionally, a post-exposure baking unit is also provided in the wafer return heat treatment frame, which is used to bake the wafer after the exposure process; the robot in the wafer return heat treatment frame is used to move the wafer from the post-exposure baking unit to the cooling unit in the interlayer module.

[0014] Optionally, the coating and developing device is further provided with an optical detection unit for acquiring an image of the wafer surface.

[0015] Optionally, the cooling unit is configured as a cooling disk, the cooling disk is connected to a heat sink, and a cooling passage communicating with each other is provided in the heat sink and the cooling disk; a cooling medium is provided in the cooling passage.

[0016] Optionally, it also includes an air supply component; the air supply component is arranged on the top side of the liquid treatment module, the interlayer module and the heat treatment module, and is used to blow protective gas to the liquid treatment module, the interlayer module and the heat treatment module.

[0017] In a second aspect, the present invention provides a coating and developing system, comprising the device described in any one of the first aspects, as well as a film box module and an interface module; the film box module is connected to the liquid processing module; a film feed loading port and a film return loading port are provided in the film box module; the film feed loading port is used to store wafers to be moved to the liquid processing module; the film return loading port is used to store wafers from the liquid processing module; the interface module is connected to the heat treatment module; a front washing unit and a back washing unit are provided in the interface module; the front washing unit is used to clean the front side of the wafer, and the back washing unit is used to clean the back side of the wafer.

[0018] Optionally, corresponding to the N-layer frame in the interlayer module, the wafer box module is provided with a wafer feeding robot, a wafer return robot, an entry and exit robot, F first branch interfaces and NF second branch interfaces; the wafer return robot is used to move the wafer on the branch interface to the wafer box return main interface, and the wafer feeding robot is used to move the wafer on the wafer box feed main interface to the branch interface; the entry and exit robot is used to move the wafer on the wafer feed loading port to the wafer feed main interface, or move the wafer on the return main interface to the wafer return loading port.

[0019] Optionally, the interface module also includes a cache unit, an interface cooling unit and a lithography output interface; the cache unit is used to store wafers that have been cleaned on the back side; the interface cooling unit is used to cool wafers that have been cleaned on the back side; and the lithography output interface is used to store wafers that have undergone the lithography process.

[0020] Optionally, corresponding to the N-layer frame, the interface module is provided with a back wash robot, an interface robot, a forward wash robot, F third branch interfaces and NF fourth branch interfaces; the back wash robot is used to move the wafer from the branch interface to the back wash unit, and to move the wafer from the back wash unit to the cache unit; the forward wash robot is used to move the wafer from the cache unit to the interface cooling unit, move the wafer from the lithography output interface to the forward wash unit, and move the wafer from the forward wash unit to the branch interface; the interface robot is used to send the wafer in the cache unit into the lithography machine, and to send the wafer from the lithography machine to the lithography output interface.

[0021] In a third aspect, the present invention provides a control method for a glue coating and developing device, which is used to control the glue coating and developing device described in any one of the first aspects, including: S1, controlling a robot in a liquid treatment module to move a wafer from the liquid treatment module to an interlayer module; S2, controlling a robot in a heat treatment module to move a wafer from the interlayer module to the heat treatment module; S3, controlling a robot in the heat treatment module to move a wafer from the heat treatment module to the interlayer module; S4, controlling a robot in the liquid treatment module to move a wafer from the interlayer module to the liquid treatment module.

[0022] The beneficial effects of the present invention are as follows: by providing an interlayer module located between the liquid treatment module and the heat treatment module, the wafers that have undergone heat treatment can be stored, and after the wafers are cooled in the interlayer module, they are sent to the liquid treatment module, which can ensure that the temperature during liquid treatment meets the process requirements, and there is no need to occupy a robot for cooling, thereby improving the utilization rate of the robot, which is beneficial to improving the production capacity of the coating and developing device. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Figure 1 A schematic cross-sectional view perpendicular to the Y direction of a glue coating and developing system provided by the present invention; Figure 2 A schematic top view along the Z reverse direction of a glue coating and developing system provided by the present invention; Figure 3 The present invention provides Figure 2 Schematic diagram of CC cross section in ; Figure 4 The present invention provides Figure 2 BB cross-section diagram in FIG. Figure 5 The present invention provides Figure 2 DD cross-section diagram in ; Figure 6 The present invention provides Figure 2 AA section diagram in; Figure 7 The present invention provides Figure 2 EE cross-sectional diagram in ; Figure 8 The present invention provides Figure 2 FF cross-sectional diagram in; Fig. 9 The present invention provides Figure 2 Schematic diagram of the GG cross section; Fig.10 A schematic flow chart of a control method for a glue coating and developing device provided by the present invention.

[0024] Description of reference numerals in the figures: 100, film box module; 200, liquid processing module; 300, interlayer module; 400, heat treatment module; 500, interface module. DETAILED DESCRIPTION

[0025] In order to make the purpose, technical solutions and advantages of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, rather than all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention. Unless otherwise defined, the technical terms or scientific terms used herein should be understood by people with general skills in the field to which the present invention belongs. "Including" and similar words used in this article mean that the elements or objects appearing before the word include the elements or objects listed after the word and their equivalents, without excluding other elements or objects.

[0026] In view of the problems existing in the existing technology, such as Figure 1 As shown, the first embodiment provides a coating and developing device, including: a liquid processing module 200, used for surface coating and developing treatment of wafers; a heat treatment module 400, used for baking, edge exposure and optical inspection of wafers; an interlayer module 300, located between the liquid processing module 200 and the heat treatment module 400, for storing wafers; the liquid processing module 200, the heat treatment module 400 and the interlayer module 300 all include adjacent N-layer frames, N is a positive integer greater than 1; the N-layer frames of the liquid processing module 200 are connected to the N-layer frames of the interlayer module 300 in a one-to-one correspondence; the N-layer frames of the interlayer module 300 are connected to the N-layer frames of the liquid processing module 200 in a one-to-one correspondence; each layer frame of the liquid processing module 200 and the heat treatment module 400 is provided with an independently operating robot. In this embodiment, the interlayer module is set up to temporarily store the wafers between the liquid treatment module and the heat treatment module, so as to ensure that the wafers can smoothly transition between different treatment stages and shorten the waiting time when the robot in each module transfers the wafer as much as possible.

[0027] Reference Figure 1 , N is 6, the liquid treatment module 200 and the heat treatment module 400 are both set as 6-layer frames. The 6-layer frames are stacked along the vertical Z direction. Along the horizontal X direction, the liquid treatment module 200, the interlayer module 300 and the heat treatment module 400 are arranged in sequence.

[0028] In some examples, the six layers of frames in the liquid processing module 200 include film-input liquid processing frames C1, C2, C3 and film-return liquid processing frames D1, D2, D3. The six layers of frames in the heat processing module 400 include film-input heat processing frames H1, H2, H3 and film-return heat processing frames H4, H5, H6.

[0029] In some embodiments, each frame layer in the interlayer module 300 is provided with M interfaces for storing wafers, where M is a positive integer; each time the same wafer enters the same frame layer of the interlayer module 300, it is stored in a different interface in the frame layer. This embodiment ensures that the wafer is stored in a different interface each time, keeps the wafer flowing along the linear wafer transmission path, avoids the wafer being damaged due to the wafer transmission path passing through the same interface multiple times, and makes it easier to track the source of the wafer quality problem, so as to quickly locate and solve the problem.

[0030] In some specific embodiments, M is 3, and the same wafer is stored in three different interfaces of the frame when it enters the same frame layer three times. In other embodiments, M can be set to 1, 5, 7 or 9.

[0031] In some embodiments, at least one frame of the interlayer module 300 is provided with a cooling unit; the cooling unit is coupled to the interface; and when the cooling unit is in contact with the wafer, it is used to cool the wafer. Figure 1 As shown, the bottom frame in the interlayer module 300 includes three interfaces, two of which are PSI2 and PSI3, and the other interface with an integrated cooling unit is SCPC4. The top frame in the interlayer module 300 includes three interfaces, two of which are PSI19 and PSI20, and the other interface with an integrated cooling unit is SCPC9. In some examples, when the wafer is placed on the above-mentioned interface, the surface of the wafer is horizontally arranged. When the cooling unit in this embodiment is in direct contact with the wafer, it can effectively take away the heat generated by the wafer, avoiding the wafer after heat treatment from carrying residual heat for liquid treatment process.

[0032] In some embodiments, the cooling unit is configured as a cooling disk, the cooling disk is connected to a heat sink (not shown in the figure), the heat sink and the cooling disk are provided with a cooling passage (not shown in the figure) that is mutually conductive; a cooling medium is provided in the cooling passage. In some specific embodiments, the cooling medium is configured as a coolant. In some examples, the coolant is configured as pure water. The heat sink in this embodiment increases the heat dissipation area of ​​the cooling disk, helps to accelerate the heat dissipation, and further improves the heat dissipation effect of the cooling disk on the wafer through the circulation of the cooling medium.

[0033] In some embodiments, Figure 2As shown, each layer of the frames of the liquid treatment module 200 and the heat treatment module 400 are arranged axially symmetrically with respect to the length direction X. The length direction X, the width direction Y and the height direction Z are perpendicular to each other.

[0034] In other embodiments, Figure 1 and Figure 3 As shown, interfaces PSI2-PSI7, PSI15-PSI20 and SCPC4-SCPC9 in the interlayer module 300 are integrated into the second interface tower T2.

[0035] In some embodiments, the N-layer frame of the liquid processing module 200 includes at least one layer of wafer feeding liquid processing frame and at least one layer of wafer return liquid processing frame; a coating assembly is provided in the wafer feeding liquid processing frame for coating photoresist or anti-reflective layer on the wafer surface; a manipulator in the wafer feeding liquid processing frame is used to move the wafer from the coating assembly to the interface in the interlayer module 300; a developing unit is provided in the wafer return liquid processing frame for developing the wafer; and a manipulator in the wafer return liquid processing frame is used to move the wafer from the interface in the interlayer module 300 to the developing unit. This embodiment can realize the automation of the coating and developing process through the integrated liquid processing module, reduce the manual transfer time of wafers between different workstations, and significantly improve production efficiency.

[0036] Reference Figure 1 In some specific embodiments, the N-layer frame of the liquid processing module 200 includes 3 layers of film-feeding liquid processing frames and 3 layers of film-returning liquid processing frames.

[0037] In some embodiments, the coating assembly includes a coating unit and an anti-reflection unit; the anti-reflection unit is used to coat the anti-reflection layer on the surface of the wafer; the robot in the wafer feeding liquid processing frame is used to move the wafer from the anti-reflection unit to the interface in the interlayer module 300; the coating unit is used to coat the photoresist on the surface of the wafer; the robot in the wafer feeding liquid processing frame is used to move the wafer from the interface of the interlayer module 300 with a cooling unit to the coating unit, and to move the wafer from the coating unit to the interface in the interlayer module 300. This embodiment can ensure that the coating thickness is uniform and consistent by setting the coating unit and the anti-reflection unit to integrate the control of the coating process of the anti-reflection layer and the photoresist, and ensure the smoothness of the subsequent process of the wafer.

[0038] like Figure 4As shown, in some specific embodiments, the manipulator in the wafer feeding liquid processing frame includes a coating robot 11, which is used to move the wafer from the interface provided with the cooling unit in the interlayer module 300 to the glue coating unit, and to move the wafer from the glue coating unit to the interface in the interlayer module 300. In some examples, the coating robot is symmetrically provided with coating components COT on both sides. Specifically, the coating component COT is set as a coating unit symmetrical about the vertical plane XZ.

[0039] In some other specific embodiments, the glue coating unit SCR and the anti-reflection unit SCB are stacked. In some examples, the glue coating unit SCR and the anti-reflection unit SCB are symmetrically arranged at the same height with respect to the vertical plane, for example, the glue coating unit SCR is located on the Y direction side of the anti-reflection unit SCB. In some other examples, in the same layer of the film feeding liquid processing frame, the glue coating unit SCR is located on the top side of the anti-reflection unit SCB. In some other examples, in the same layer of the film feeding liquid processing frame, the glue coating unit SCR is located on the bottom side of the anti-reflection unit SCB.

[0040] like Figure 1 As shown, in some embodiments, the robot in the film return liquid processing frame is used to move the wafer from the interface of the interlayer module 300 provided with the cooling unit to the developing unit; and to move the wafer from the developing unit to the interface in the interlayer module 300. This embodiment can realize the automation of the developing process through the integrated developing unit, reduce the manual transfer time of the wafer between different workstations, and significantly improve the production efficiency.

[0041] like Figure 4 As shown, in some specific embodiments, the manipulator in the film return liquid processing frame includes a developing robot 16, and the developing robot 16 is used to move the wafer from the interface SCPC9 provided with a cooling unit in the interlayer module 300 to the developing unit SDC, move the wafer from the developing unit SDC to the interface PSI19, and move the wafer from the interface PSI20 to the interface PSI23. In some examples, the developing unit SDC is symmetrically provided on both sides of the developing robot. Specifically, the developing unit SDC is set to be a developing unit SDC symmetrical about the vertical plane XZ.

[0042] In some embodiments, the N-layer frame of the heat treatment module 400 includes at least one layer of wafer feeding heat treatment frame and at least one layer of wafer return heat treatment frame; a soft baking unit is provided in the wafer feeding heat treatment frame for pre-treating the coating on the surface of the wafer; the manipulator in the wafer feeding heat treatment frame is used to move the wafer from the interface in the interlayer module 300 to the soft baking unit; a hard baking unit is provided in the wafer return heat treatment frame for curing the coating on the surface of the wafer; the manipulator in the wafer return heat treatment frame is used to move the wafer after the surface coating is cured to the interface in the interlayer module 300. This embodiment can realize the automation of soft baking and hard baking processes through the integrated heat treatment module, reduce the manual transfer time of wafers between different workstations, and significantly improve production efficiency.

[0043] Reference Figure 1 In some specific embodiments, the N-layer frame of the heat treatment module 400 includes a 3-layer film-feeding heat treatment frame and a 3-layer film-returning heat treatment frame.

[0044] In some embodiments, the coating and developing device is further provided with an edge exposure unit for exposing the edge of the wafer. This embodiment controls the process parameters of edge exposure by the edge exposure unit, thereby ensuring that the photoresist performance of the wafer edge area meets the requirements and ensures the smooth progress of subsequent wafer processes.

[0045] In some specific embodiments, the edge exposure unit is disposed in the film feeding heat treatment frame, and the robot in the film feeding heat treatment frame is used to move the wafer from the soft baking unit to the edge exposure unit. In other specific embodiments, the edge exposure unit is disposed in the interface module.

[0046] In some examples, the baking robot 21 is used to move the wafer after the soft baking process to the edge exposure unit WES, and to move the wafer from the edge exposure unit WES to the interfaces PSI8, PSI9 and PSI10 respectively.

[0047] In some embodiments, an anti-reflection baking unit is further provided in the wafer feeding heat treatment frame, which is used to dry the anti-reflection layer on the surface of the wafer; the robot in the wafer feeding heat treatment frame is used to move the wafer from the interface in the interlayer module 300 to the anti-reflection baking unit, and to move the wafer from the anti-reflection baking unit to the cooling unit in the interlayer module 300. This embodiment controls the parameters in the anti-reflection layer baking process by setting the anti-reflection baking unit, which can ensure that the performance of the anti-reflection layer meets the requirements and ensure the smooth progress of the subsequent wafer processes.

[0048] like Figure 1 and Figure 5As shown, in some specific embodiments, the robot 21 located in the wafer feeding heat treatment frame at the bottom layer is used to move the wafer from the interface PSI2 to the anti-reflection baking unit BHTB, move the wafer from the anti-reflection baking unit BHTB to the interface SCPC4, and move the wafer from the interface PSI3 to the soft baking unit HLTB.

[0049] In some embodiments, a post-exposure baking unit is further provided in the wafer return heat treatment frame, which is used to bake the wafer after the exposure process; and the robot in the wafer return heat treatment frame is used to move the wafer from the post-exposure baking unit to the cooling unit in the interlayer module 300. This embodiment controls the parameters in the post-exposure baking process by the post-exposure baking unit, which can ensure that the performance of the photoresist meets the requirements and ensure the smooth progress of the subsequent wafer processes.

[0050] In some specific embodiments, the baking robot 26 located in the top-level return heat treatment frame is used to move the wafer from the interface PSI14 to the post-exposure baking unit HAEB, move the wafer from the post-exposure baking unit HAEB to the interface SCPC9, and move the wafer from the interface PSI19 to the hard baking unit DLTB.

[0051] In some embodiments, the coating and developing device is further provided with an optical detection unit for acquiring an image of the wafer surface. The optical detection unit provided in this embodiment can ensure that the quality of the wafer surface meets the standards required by the process, which is crucial to ensure the smooth progress of subsequent wafer processes.

[0052] In some specific embodiments, the optical detection unit is disposed in the wafer return heat treatment frame; the robot in the wafer return heat treatment frame is used to move the wafer from the hard baking unit to the optical detection unit, and to move the wafer from the optical detection unit to the interface in the interlayer module 300. In other specific embodiments, the optical detection unit is disposed in the wafer box module.

[0053] In some examples, the robot arm 26 located in the wafer return thermal processing frame on the top layer is used to move the wafer from the hard baking unit DLTB to the optical inspection unit AOI, and to move the wafer from the optical inspection unit AOI to the interface PSI20.

[0054] In some embodiments, an air supply member (not shown) is also included; the air supply member is disposed on the top side of the liquid processing module 200, the interlayer module 300 and the heat treatment module 400, and is used to purge protective gas to the liquid processing module 200, the interlayer module 300 and the heat treatment module 400. This embodiment can effectively reduce the contamination of the wafer by particles and impurities in the air by blowing protective gas to each module, thereby improving the purity and quality of the product. In addition, when the air supply member blows protective gas to the interlayer module, it can assist in cooling the surface of the wafer and improve the cooling efficiency.

[0055] The second embodiment provides a coating and developing system, comprising the device described in any one of the above embodiments, and a film box module 100 and an interface module 500; the film box module 100 is connected to the liquid processing module 200; the film box module 100 is provided with a film loading port and a film return loading port; the film loading port is used to store the wafer to be moved to the liquid processing module 200; the film return loading port is used to store the wafer from the liquid processing module 200; the interface module 500 is connected to the heat treatment module 400; the interface module 500 is provided with a front washing unit and a back washing unit; the front washing unit is used to clean the front of the wafer, and the back washing unit is used to clean the back of the wafer. This embodiment can realize the automation of processes such as coating, developing and cleaning through an integrated system design, reduce the manual transfer time of wafers between different workstations, and significantly improve production efficiency. Compared with traditional separate workstations, the integrated design can arrange equipment more compactly, save valuable production space, and simplify equipment configuration, which helps to reduce costs.

[0056] In some specific embodiments, reference Figure 1 As shown, it includes a first loading interface LP1 for loading unprocessed wafers and a second loading interface LP2 for loading processed wafers. In some examples, the first loading interface LP1 and the second loading interface LP2 are both set to two; the two second loading interfaces LP2 are suspended directly above the two first loading interfaces LP1.

[0057] In some embodiments, corresponding to the N layers of frames in the interlayer module, the wafer box module 100 is provided with a wafer feeding robot, a wafer return robot, an in-and-out station robot, F first branch interfaces and NF second branch interfaces; the wafer return robot is used to move the wafer on the branch interface to the wafer box return interface, and the wafer feeding robot is used to move the wafer on the wafer box feed interface to the branch interface; the in-and-out station robot is used to move the wafer on the wafer feed loading port to the wafer feed interface, or to move the wafer on the return interface to the return loading port. It is worth noting that F is a positive integer greater than 0 and less than N. This embodiment can avoid wafer accumulation in each layer of the frame by flexibly allocating the number of first branch interfaces and second branch interfaces, which is conducive to breaking through process bottlenecks and improving the overall efficiency of the wafer box module.

[0058] like Figure 1 and Figure 6 As shown, in some examples, the number of the first branch interfaces and the number of the second branch interfaces are both 3. The number of the wafer feed interface and the wafer return interface are both set to 1. The wafer on the wafer feed interface PSI1 is moved by the robot 2 to three of the first branch interfaces SCPC1, SCPC2 and SCPC3, which are provided with cooling units, and the wafer on the three second branch interfaces PSI21, PSI22 and PSI23 is moved by the robot 3 to the wafer return interface PSI24.

[0059] In some examples, a tackifying unit ADB is further provided on one side of the wafer return interface PSI24 to enhance the viscosity of the wafer surface so that the coating adheres more firmly to the wafer surface. The robot 3 is also used to move the wafer from the tackifying unit ADB to the wafer feed interface PSI1.

[0060] In other examples, the cassette module 100 is provided with an in-and-out robot 1 for moving the wafer on the first loading interface LP1 to the wafer feed interface PSI1 and moving the wafer on the wafer return interface PSI24 to the second loading interface LP2.

[0061] In some embodiments, the interface module 500 further includes a front wash robot and a back wash robot; the front wash robot is used to move the wafer from the lithography machine to the front wash unit; the back wash robot is used to send the wafer cleaned on the back side into the lithography machine.

[0062] In some embodiments, corresponding to the N-layer frame, the interface module 500 is provided with an interface robot and N branch interfaces; the interface robot is used to move the wafers on the N branch interfaces to the back wash unit, or to move the wafers in the forward wash unit to the N branch interfaces.

[0063] In some examples, N is 6, and the branch interfaces within the interface module 500 are set to PSI8, PSI9, PSI10, PSI12, PSI13, and PSI14.

[0064] like Figure 1 and Figure 7 As shown, in some specific embodiments, the backwash robot 31 is used to move the wafers on the branch interfaces PSI8, PSI9 and PSI10 to the backwash unit BS. The forward wash robot 32 is used to move the wafers on the forward wash unit PIS to the branch interfaces PSI12, PSI13 and PSI14 respectively.

[0065] In other embodiments, Figure 8 and Fig. 9 As shown, interfaces PSI1, PSI21-PSI24 and SCPC1-SCPC3 in the cassette module 100 are integrated into the first interface tower T1. Interfaces PSI8-PSI14 and CPC in the interface module 500 are integrated into the third interface tower T3.

[0066] In some embodiments, the interface module further includes a cache unit, an interface cooling unit and a photolithography output interface; the cache unit is used to store wafers that have been cleaned on the back side; the interface cooling unit is used to cool wafers that have been cleaned on the back side; and the photolithography output interface is used to store wafers that have undergone a photolithography process. The presence of the cache unit in this embodiment provides a flexible wafer storage management solution, which helps to optimize the production process and improve production flexibility.

[0067] In other embodiments, corresponding to the N-layer frame, the interface module is provided with a backwash robot, an interface robot, a forward wash robot, F third branch interfaces and NF fourth branch interfaces; the backwash robot is used to move the wafer from the branch interface to the backwash unit, and to move the wafer from the backwash unit to the cache unit; the forward wash robot is used to move the wafer from the cache unit to the interface cooling unit, to move the wafer from the lithography output interface to the forward wash unit, and to move the wafer from the forward wash unit to the branch interface; the interface robot is used to send the wafer in the cache unit into the lithography machine, and to send the wafer from the lithography machine to the lithography output interface. It is worth noting that F is a positive integer greater than 0 and less than N. This embodiment can avoid wafer accumulation in each layer of the frame by flexibly allocating the number of the third branch interface and the fourth branch interface, which is conducive to breaking through the process bottleneck and improving the overall efficiency of the interface module.

[0068] In some specific embodiments, the backwash robot 31 is also used to move the wafers that have been backwashed from the backwash unit BS to the buffer unit BF. In some examples, the buffer unit BF is configured as a 25-layer wafer storage rack.

[0069] In some other specific embodiments, the forward cleaning robot 32 is further used to move the wafers on the buffer unit BF to the interface cooling unit CPC, and to move the wafers on the interface PSI11 to the forward cleaning unit PIS.

[0070] In some further specific embodiments, the interface module 500 further includes an interface robot 33 for delivering the wafer on the interface cooling unit CPC into the lithography machine SCAN, and moving the wafer output by the lithography machine SCAN to the interface PSI11.

[0071] like Fig.10 As shown, the third embodiment provides a control method for a glue coating and developing device, which is used to control the glue coating and developing device described in any one of the above embodiments, including: S1, controlling the robot in the liquid treatment module to move the wafer from the liquid treatment module to the interlayer module; S2, controlling the robot in the heat treatment module to move the wafer from the interlayer module to the heat treatment module; S3, controlling the robot in the heat treatment module to move the wafer from the heat treatment module to the interlayer module; S4, controlling the robot in the liquid treatment module to move the wafer from the interlayer module to the liquid treatment module.

[0072] In some specific embodiments, S1 includes controlling the coating robot 11 to send the wafer on the interface SCPC1 to the anti-reflection unit SCB, and to send the wafer from the anti-reflection unit SCB to the interface PSI2. Also, it sends the wafer from the interface SCPC4 to the glue coating unit SCR, and to send the wafer from the glue coating unit SCR to the interface PSI3.

[0073] In other specific embodiments, S2 includes controlling the baking robot 21 to move the wafer from interface PSI2 to the reflective baking unit BHTB, moving the wafer from the anti-reflective baking unit BHTB to interface SCPC4, moving the wafer from interface PSI3 to the soft baking unit HLTB, moving the wafer from the soft baking unit HLTB to the edge exposure unit WES, and moving the wafer from the edge exposure unit WES to interface PSI8.

[0074] It is worth noting that S1 and S2 can be performed alternately so that the same wafer passes through interface SCPC1, anti-reflection unit SCB, interface PSI2, anti-reflection baking unit BHTB, interface SCPC4, coating unit SCR, interface PSI3, soft baking unit HLTB, edge exposure unit WES and interface PSI8 in sequence.

[0075] In other examples, the same wafer may skip the anti-reflection layer process and directly pass through the interface SCPC1, the coating unit SCR, the interface PSI3, the soft baking unit HLTB, the edge exposure unit WES and the interface PSI8 in sequence.

[0076] In some specific embodiments, S3 includes controlling the baking robot 26 to move the wafer from the interface PSI14 to the post-exposure baking unit HAEB, moving the wafer from the post-exposure baking unit HAEB to the interface SCPC9, and moving the wafer from the interface PSI19 to the hard baking unit DLTB, moving the wafer from the hard baking unit DLTB to the optical inspection unit AOI, and moving the wafer from the optical inspection unit AOI to the interface PSI20.

[0077] In other specific embodiments, S4 includes controlling the developing robot 16 to move the wafer from the interface SCPC9 provided with the cooling unit in the interlayer module to the developing unit SDC, moving the wafer from the developing unit SDC to the interface PSI19, and moving the wafer from the interface PSI20 to the interface PSI23.

[0078] It is worth noting that S3 and S4 can be performed alternately so that the same wafer passes through interface PSI14, post-exposure baking unit HAEB, interface SCPC9, developing unit SDC, interface PSI19, hard baking unit DLTB, optical inspection unit AOI, interface PSI20 and interface PSI23 in sequence.

[0079] Although the embodiments of the present invention are described in detail above, it is obvious to those skilled in the art that various modifications and variations can be made to these embodiments. However, it should be understood that such modifications and variations are within the scope and spirit of the present invention as described in the claims. Moreover, the present invention described herein may have other embodiments and may be implemented or realized in a variety of ways.

Claims

1. A coating and developing device, characterized in that: include: A liquid treatment module, used for performing a liquid treatment process including surface coating and developing treatment on the wafer; A heat treatment module, used for performing a heat treatment process including a baking process on the wafer; The interlayer module is located between the liquid treatment module and the heat treatment module and is used to store wafers to connect the heat treatment process and the liquid treatment process.

2. The device according to claim 1, characterized in that Each layer frame of the interlayer module is provided with a plurality of interfaces for storing wafers; Each time the same wafer enters the same frame of the interlayer module, it is stored in a different interface of the frame.

3. The device according to claim 2, characterized in that A cooling unit is provided in at least one frame layer of the interlayer module; the cooling unit is coupled to the interface; When the cooling unit is in contact with the wafer, it is used to cool the wafer.

4. The device according to claim 2, characterized in that The liquid processing module includes at least one layer of film feeding liquid processing frame and at least one layer of film returning liquid processing frame; A coating assembly is provided in the wafer feeding liquid processing frame, which is used to coat photoresist or anti-reflection layer on the surface of the wafer; the manipulator in the wafer feeding liquid processing frame is used to move the wafer from the coating assembly to the interface in the interlayer module; A developing unit is provided in the film return liquid processing frame for developing the wafer; The robot in the film return liquid processing frame is used to move the wafer from the interface in the interlayer module to the developing unit.

5. The device according to claim 2, characterized in that The heat treatment module comprises at least one layer of film feeding heat treatment frame and at least one layer of film returning heat treatment frame; The wafer feeding heat treatment frame is provided with a soft baking unit for pre-treating the coating on the surface of the wafer; the robot in the wafer feeding heat treatment frame is used to move the wafer from the interface in the interlayer module to the soft baking unit; A hard baking unit is provided in the wafer return heat treatment frame, and the hard baking unit is used to cure the coating on the wafer surface; The robot in the wafer return heat treatment frame is used to move the wafer after the surface coating is cured to the interface in the interlayer module.

6. The device according to claim 4, characterized in that The coating assembly includes a glue coating unit and an anti-reflection unit; The anti-reflection unit is used to apply an anti-reflection layer to the surface of the wafer; the robot in the wafer feeding liquid processing frame is used to move the wafer from the anti-reflection unit to the interface in the interlayer module; The glue coating unit is used to coat photoresist on the surface of the wafer; the robot in the wafer feeding liquid processing frame is used to move the wafer from the interface of the cooling unit in the interlayer module to the glue coating unit, and to move the wafer from the glue coating unit to the interface in the interlayer module.

7. The device according to claim 4, characterized in that The robot in the film return liquid processing frame is used to move the wafer from the interface of the interlayer module provided with the cooling unit to the developing unit; and to move the wafer from the developing unit to the interface in the interlayer module.

8. The device according to claim 5, characterized in that An anti-reflection baking unit is also provided in the wafer feeding heat treatment frame, which is used to dry the anti-reflection layer on the surface of the wafer; the robot in the wafer feeding heat treatment frame is used to move the wafer from the interface in the interlayer module to the anti-reflection baking unit, and to move the wafer from the anti-reflection baking unit to the cooling unit in the interlayer module.

9. The device according to claim 5, characterized in that The wafer return heat treatment frame is also provided with a post-exposure baking unit for baking the wafer after the exposure process; the robot in the wafer return heat treatment frame is used to move the wafer from the post-exposure baking unit to the cooling unit in the interlayer module.

10. The device according to claim 3, characterized in that The cooling unit is configured as a cooling disk, the cooling disk is connected to a heat sink, the heat sink and the cooling disk are provided with a cooling passage that is connected to each other; a cooling medium is provided in the cooling passage.

11. The device according to claim 1, characterized in that It also includes an air supply component; the air supply component is arranged on the top side of the liquid processing module, the interlayer module and the heat treatment module, and is used to blow protective gas to the liquid processing module, the interlayer module and the heat treatment module.

12. The device according to claim 1, characterized in that The liquid treatment module, the heat treatment module and the interlayer module all include adjacent N-layer frames, where N is a positive integer greater than 1; the N-layer frames of the liquid treatment module are connected one-to-one with the N-layer frames of the interlayer module; the N-layer frames of the interlayer module are connected one-to-one with the N-layer frames of the liquid treatment module; and each layer of the frames of the liquid treatment module and the heat treatment module is provided with an independently operating manipulator.

13. A coating and developing system, characterized in that: A device comprising any one of claims 1 to 12, as well as a cassette module and an interface module; The wafer box module is connected to the liquid processing module; a wafer feed loading port and a wafer return loading port are provided in the wafer box module; the wafer feed loading port is used to store wafers to be moved to the liquid processing module; the wafer return loading port is used to store wafers from the liquid processing module; The interface module is connected to the heat treatment module; a front washing unit and a back washing unit are arranged in the interface module; the front washing unit is used for washing the front side of the wafer, and the back washing unit is used for washing the back side of the wafer.

14. The system according to claim 13, characterized in that Corresponding to the N-layer frame in the interlayer module, the wafer feeding robot, the wafer returning robot, the in-and-out robot, F first branch interfaces and NF second branch interfaces are arranged in the wafer box module; the wafer returning robot is used to move the wafer on the branch interface to the wafer box returning main interface, and the wafer feeding robot is used to move the wafer on the wafer box feeding main interface to the branch interface; The in-and-out station robot is used to move the wafer on the wafer input loading port to the wafer input main interface, or to move the wafer on the wafer return main interface to the wafer return loading port.

15. The system according to claim 13, characterized in that The interface module also includes a cache unit, an interface cooling unit and a photolithography output interface; the cache unit is used to store wafers that have been cleaned on the back side; the interface cooling unit is used to cool the wafers that have been cleaned on the back side; and the photolithography output interface is used to store wafers that have undergone the photolithography process.

16. The system according to claim 15, characterized in that Corresponding to the N-layer frame, the interface module is provided with a back wash robot, an interface robot, a forward wash robot, F third branch interfaces and NF fourth branch interfaces; the back wash robot is used to move the wafer from the branch interface to the back wash unit, and to move the wafer from the back wash unit to the cache unit; the forward wash robot is used to move the wafer from the cache unit to the interface cooling unit, to move the wafer from the lithography output interface to the forward wash unit, and to move the wafer from the forward wash unit to the branch interface; the interface robot is used to send the wafer in the cache unit into the lithography machine, and to send the wafer from the lithography machine to the lithography output interface.

17. A method for controlling a gum coating and developing device, used for controlling the gum coating and developing device according to any one of claims 1 to 12, characterized in that: include: S1, controlling the robot in the liquid processing module to move the wafer from the liquid processing module to the interlayer module; S2, controlling a robot in the heat treatment module to move the wafer from the interlayer module to the heat treatment module; S3, controlling the robot in the heat treatment module to move the wafer from the heat treatment module to the interlayer module; S4, controlling the robot in the liquid processing module to move the wafer from the interlayer module to the liquid processing module.

Citation Information

Patent Citations

  • Uninterrupted chip-in and chip-out device and control method

    CN108962804A

  • Chemical mechanical polishing system

    CN115723037A

  • Gluing and developing system and gluing and developing method

    CN116627003A

  • Gluing and developing apparatus and method

    CN116736649A

  • Gluing and developing equipment and control method

    CN117878033A

Cited By

  • Control method, apparatus, medium, and program for gluing and developing device

    CN121325516A