Method for manufacturing semiconductor package assembly and semiconductor package assembly obtained using same

The metal layer connection component is formed through the layer-by-layer deposition technology of metal powder layer and laser radiation, which solves the problems of easy connection failure and complex and time-consuming manufacturing of existing semiconductor packages, achieving a simple and fast packaging process and low RDS(on) characteristics, extending the life of the package.

CN118737839APending Publication Date: 2024-10-01NEXPERIA BV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410349014.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-03-29
Filing Date
2024-03-26
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

The connection components of existing semiconductor packages are prone to failure over time, and the manufacturing process is complex, time-consuming and costly, resulting in limited performance.

Method used

The layer-by-layer deposition technology that combines metal powder layers with laser radiation is used to form metal layer connection components, replacing traditional Cu clamp bonding or Cu wire bonding, simplifying manufacturing steps and reducing material stress, omitting solder and adhesion promoters.

Benefits of technology

Significantly reduces package processing time, increases connection component flexibility and durability, reduces RDS(on) characteristics, extends package life, and reduces manufacturing costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118737839A_ABST
    Figure CN118737839A_ABST
Patent Text Reader

Abstract

The present invention proposes a method for manufacturing a leaded / leadless power / MCD package or power module with simple, clear and less time-consuming processing steps, and wherein the implemented connecting elements have a simple design with reduced RDS (on) properties. The method comprises providing a lead frame in a sub-step i1), and providing at least one semiconductor die structure on the lead frame in a step i2). The step (i-3) of forming one or more connection elements between the at least one semiconductor die structure and the at least two terminals of the lead frame comprises at least one forming sequence, in which sub-step (i3-1) provides a layer of metal powder, contacting the metal powder with the at least one semiconductor die structure and one of the at least two terminals of the lead frame; and a sub-step i3-2) of selectively melting the metal powder layer with laser radiation to form a metal layer. In a final step ii), the at least one semiconductor die structure, the one or more connecting elements and the plurality of terminals are encapsulated with a molding resin such that at least a portion of the at least two terminals are exposed, thereby forming at least one encapsulated semiconductor package assembly.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to manufacturing techniques for semiconductor package assemblies and semiconductor package assemblies obtained using these techniques, wherein a semiconductor die structure is mounted to a lead frame having terminals and encapsulated with a molding resin. Background Art

[0002] In conventional leaded / leadless power / MCD packages or power modules, various connection elements are implemented for electrically and mechanically interconnecting the semiconductor die structure with the various terminals of the lead frame. Examples of such electrical and mechanical connection elements are standard wire bonding, ribbon bonding, or clip bonding, which require different processing steps to be applied during the manufacture of the power module or semiconductor package assembly.

[0003] Although these known connection elements are secured by an encapsulant, these fragile bonds are still susceptible to connection failure over time. In addition, since these known bonding techniques require pre-designed and pre-manufactured connection elements, and time-consuming processing steps are required to install these connection elements during the manufacturing process, these known bonding techniques are costly, complicated, and time-consuming. In addition, these conventional leaded / leadless power / MCD packages or power modules still exhibit high RDS (on) (Drain-Source On-Resistance), which limits the performance of the conventional leaded / leadless power / MCD package or power module.

[0004] Therefore, the object of the present disclosure is to provide a manufacturing technique which avoids the above mentioned problems, thereby obtaining a leaded / leadless power / MCD package or power module manufactured with simple well-defined and less time-consuming processing steps, and wherein the implemented connection elements have a reduced RDS (on) Direct design of features. Summary of the invention

[0005] According to a first example of the present disclosure, a method for manufacturing a leaded / leadless power / MCD package or a power module is proposed, which has simple, well-defined and less time-consuming processing steps and in which the implemented connection elements have a reduced RDS (on) Features simple design.

[0006] The method comprises the following steps: i) forming at least one semiconductor package by the following sub-steps: i1) providing a lead frame made of a metal material, the lead frame having a first frame side and a second frame side opposite to the first frame side and having at least two terminals. Subsequently, in step i2), providing at least one semiconductor die structure having a first die side and a second die side opposite to the first side, the semiconductor die structure being mounted on the first frame side of the lead frame by means of the second die side of the semiconductor die structure.

[0007] In a subsequent step i3), one or more connecting elements are provided between at least one semiconductor die structure and at least two terminals of the lead frame, and in a final step ii), at least one semiconductor die structure, one or more connecting elements and a plurality of terminals are encapsulated with a molding resin, leaving at least a portion of at least two terminals exposed, thereby forming at least one encapsulated semiconductor package component.

[0008] Specifically, step i3) of providing a number of connecting elements includes at least one forming sequence, wherein: sub-step i3-1) provides a metal powder layer so that the metal powder is in contact with at least one semiconductor core structure and one of at least two terminals of a lead frame; and sub-step i3-2) uses laser radiation to selectively melt the metal powder layer to form a metal layer.

[0009] In the sequence of two sub-steps i3-1) and i3-2), the connection element is formed layer by layer by deposition and solidification of metal powder layers, replacing the known Cu clamp bonding or Cu wire bonding and significantly reducing any processing time of the panel-level package. In addition, the manufacturing technology of the connection element is more flexible than the known wire bonding / clamp bonding forming technology that requires pre-designed and pre-manufactured components.

[0010] In addition, the implementation of layer-by-layer deposition techniques allows for better material handling, thereby reducing material stress in the connecting elements, thus reducing connectivity failures due to time and extending the life of the leaded / leadless power / MCD package or power module. Moreover, this manufacturing technique outlined in sub-steps i3-1) and i3-2) results in a reduced (lower) RDS compared to known conventional interconnection methods. (on) This is because the entire interconnect interface between the various components (semiconductor die structure and lead frame) will be the same metal layer material. Since the metal powder connection can be melted between the materials, solder and / or adhesion promoters between the semiconductor die structure and the resulting connection element and between the connection element and the lead frame can be omitted.

[0011] In a specific example, the formation sequence of steps i3 - 1) and i3 - 2) is performed alternately multiple times, thereby forming a three-dimensional stack of subsequent molten metal layers.

[0012] Contrary to known pre-designed and pre-manufactured connection elements, the method according to the present disclosure allows forming the connection element layer by layer in a more flexible manner, since the local thickness and / or local density of each metal layer formed during the formation sequence of steps i3-1) and i3-2) can be effectively controlled by adjusting one or more manufacturing parameters, the one or more manufacturing parameters being selected from the following:

[0013] -Metal powder distribution;

[0014] - the supply rate of the metal powder to be deposited;

[0015] - the metal powder deposition angle relative to the plane formed by the lead frame;

[0016] - Laser power;

[0017] -Laser frequency;

[0018] -Laser wavelength;

[0019] - Ambient processing temperature;

[0020] - Duration of metal powder deposition in step i3-1);

[0021] - Duration of melting of the metal powder in step i3-2).

[0022] Effectively, the method according to the present disclosure enables each metal layer formed in step i3-2) to have a thickness of 30 to 40 μm, preferably 35 μm.

[0023] In an example of the method according to the present disclosure, the design flexibility of the above-mentioned layer-by-layer connection element allows the surface size of the metal layer to be larger or smaller than the surface size of the metal layer formed during the previous formation sequence. Therefore, a connection element with a complex three-dimensional shape can be formed according to the functionality of the connection element.

[0024] In another example of the method, after the final formation sequence of steps i3-1) and i3-2) but before step ii), step iii) is performed, which subjects the exposed portions of at least two terminals to a surface roughening treatment, for example using a chemical agent.

[0025] Therefore, in a further step iv) after step ii) or step iii), the exposed portions of at least two terminals are plated with a metal plating material. Preferably, the metal plating material is tin.

[0026] Finally, the method according to the present disclosure comprises a step v) performed after step iv) of singulating the encapsulated semiconductor package in the lead frame to form individual semiconductor package assemblies.

[0027] Similarly, the present disclosure relates to a semiconductor package assembly, which consists of at least one semiconductor die structure, which is electrically and mechanically attached to at least two terminals through one or more connecting elements, and is encapsulated by a molded resin so that a portion of at least two terminals is exposed, wherein one or more connecting elements between the semiconductor die structure and the at least two terminals are formed according to the method steps of the present disclosure.

[0028] In a particular example, the semiconductor package assembly is a leadless semiconductor package assembly or a leaded semiconductor package assembly. BRIEF DESCRIPTION OF THE DRAWINGS

[0029] The present disclosure will now be discussed with reference to the accompanying drawings, which show:

[0030] Figure 1 are examples of processing steps according to the method of the present disclosure;

[0031] Figure 2a to Figure 2b are top and cross-sectional side views of an example of a leaded semiconductor package assembly according to the present disclosure;

[0032] Figure 3a to Figure 3b are top and detailed views of an example of a power module according to the present disclosure;

[0033] Figure 4a to Figure 4b are top and cross-sectional side views of an example of a leadless semiconductor package assembly according to the present disclosure; Figure 5a to Figure 5b are top view and cross-sectional side view of another example of a leadless semiconductor package assembly according to the present disclosure. DETAILED DESCRIPTION

[0034] For proper understanding of the present disclosure, in the following detailed description, the same reference numerals will be used in the drawings to designate corresponding elements or parts of the present disclosure.

[0035] As described above, in addition to the known weak electrical and mechanical connection elements secured by the sealant, the weak bonds are still susceptible to connection failure over time. In addition, these known bonding techniques are costly, complex, and time consuming because they require pre-designed and pre-manufactured connection elements and require time-consuming processing steps to install these connection elements during the manufacturing process. In addition, these conventional leaded / leadless power / MCD packages or power modules still exhibit high RDS (on)(Drain-Source On-Resistance), which limits the performance of the conventional leaded / leadless power / MCD package or power module.

[0036] Figure 1 A flow chart showing the process steps of a manufacturing method according to the present disclosure for manufacturing a leaded / leadless power / MCD package or power module using simple, clear and less time-consuming process steps, and wherein the implemented connection elements have a reduced RDS (on) Direct design of features.

[0037] The method comprises the following steps: i) forming at least one semiconductor package by the following sub-steps: i1) providing a lead frame made of a metal material, the lead frame having a first frame side and a second frame side opposite to the first frame side and having at least two terminals. Subsequently, in step i2), providing at least one semiconductor die structure having a first die side and a second die side opposite to the first side, the semiconductor die structure being mounted on the first frame side of the lead frame by means of the second die side of the semiconductor die structure.

[0038] In a subsequent step i3), one or more connecting elements are provided between at least one semiconductor die structure and at least two terminals of the lead frame, and in a final step ii), at least one semiconductor die structure, one or more connecting elements and a plurality of terminals are encapsulated with a molding resin, leaving at least a portion of at least two terminals exposed, thereby forming at least one encapsulated semiconductor package component.

[0039] Specifically, the step i3) of providing a plurality of connection elements comprises at least one formation sequence, wherein: a sub-step i3-1) provides a metal powder layer so that the metal powder contacts at least one semiconductor die structure and one of at least two terminals of a lead frame; and a sub-step i3-2) selectively melts the metal powder layer using laser radiation to form a metal layer. The step of providing the metal powder layer may constitute depositing powder particles, and the step of selectively melting may also include solidifying or sintering the metal powder.

[0040] In the sequence of two sub-steps i3-1) and i3-2), the connection element is formed layer by layer by deposition and solidification of metal powder layers, replacing the known Cu clamp bonding or Cu wire bonding and significantly reducing any processing time of the panel-level package. In addition, the manufacturing technology of the connection element is more flexible than the known wire bonding / clamp bonding forming technology that requires pre-designed and pre-manufactured components.

[0041] Additionally, implementation of layer-by-layer deposition techniques allows for better material handling, thereby reducing material stress in the connection elements, thus reducing connectivity failures over time and extending the life of the leaded / leadless power / MCD package or power module. Moreover, this manufacturing technique outlined in sub-steps i3-1) and i3-2) results in reduced (lower) RDS compared to known conventional interconnection methods. (on) This is because the entire interconnect interface between the various components (semiconductor die structure and lead frame) will be the same metal layer material. Since the metal powder connection can be melted between the materials, solder and / or adhesion promoters between the semiconductor die structure and the resulting connection element and between the connection element and the lead frame can be omitted.

[0042] In a specific example, the formation sequence of steps i3 - 1) and i3 - 2) is performed alternately multiple times, thereby forming a three-dimensional stack of subsequent molten metal layers.

[0043] Contrary to known pre-designed and pre-manufactured connection elements, the method according to the present disclosure allows forming the connection element layer by layer in a more flexible manner, since the local thickness and / or local density of each metal layer formed during the formation sequence of steps i3-1) and i3-2) can be effectively controlled by adjusting one or more manufacturing parameters, the one or more manufacturing parameters being selected from the following:

[0044] -Metal powder distribution;

[0045] - the supply rate of the metal powder to be deposited;

[0046] - the metal powder deposition angle relative to the plane formed by the lead frame;

[0047] - Laser power;

[0048] -Laser frequency;

[0049] -Laser wavelength;

[0050] - Ambient processing temperature;

[0051] - Duration of metal powder deposition in step i3-1);

[0052] - Duration of melting of the metal powder in step i3-2).

[0053] Effectively, the method according to the present disclosure enables each metal layer formed in step i3-2) to have a thickness of 30 to 40 μm, preferably 35 μm.

[0054] In an example of the method according to the present disclosure, the design flexibility of the above-mentioned layer-by-layer connection element allows the surface size of the metal layer to be larger or smaller than the surface size of the metal layer formed during the previous formation sequence. Therefore, a connection element with a complex three-dimensional shape can be formed according to the functionality of the connection element.

[0055] In another example of the method, after the final formation sequence of steps i3-1) and i3-2) but before step ii), step iii) is performed, which subjects the exposed portions of at least two terminals to a surface roughening treatment, for example using a chemical agent.

[0056] Therefore, in a further step iv) after step ii) or step iii), a metal plating material is plated on the exposed portions of at least two terminals. For example, electroplating can be used. Preferably, the metal plating material is different from the metal material of the terminals. In one example, the metal plating material is tin.

[0057] Finally, the method according to the present disclosure comprises a step v) performed after step iv) of singulating the encapsulated semiconductor package in the lead frame to form individual semiconductor package assemblies.

[0058] Post-processing steps may include a visual inspection step vi). Optionally, before the encapsulation step ii), a step vii) is performed, which includes providing one or more bonding wires (eg, used as gate wires) between the semiconductor die structure 2 and one of the other frame terminals.

[0059] Figure 2a to Figure 2b A top view and a cross-sectional side view of an example of a singulated leaded semiconductor package assembly 101 according to the present disclosure are shown. The leaded semiconductor package assembly 101 is formed of three components. The first component is a semiconductor die structure 2 having a first die side 2a and a second die side 2b opposite to the first die side 2a. The second component is formed as a lead frame 1 made of a metal material, the lead frame 1 having a first frame side 1a and a second frame side 1b opposite to the first frame side 1a, and also having at least two lead terminals 1z1. The semiconductor die structure 2 is mounted on the first frame side 1a of the lead frame 1 using the second die side 2b of the semiconductor die structure 2.

[0060] As a third component, a three-dimensional structured connection element 31 is mounted on the first die side 2a of the semiconductor die structure 2 and manufactured according to the method steps of the present disclosure. The three-dimensional structured connection element 31 bridges the gap or distance between the semiconductor die structure 2 and the lead terminal 1z1 and forms an electrical and mechanical connection.

[0061] Specifically, the metal powder layer 30 is provided by providing a layer-by-layer formation sequence in the sub-step i3-1), so that the metal powder contacts the first tube core side 2a of the semiconductor tube core structure 2 and the lead terminal 1z1 of the lead frame 1. After each layer is deposited according to the sub-step i3-1), the sub-step i3-2) is performed, and the sub-step i3-2) selectively melts the metal powder layer 30 using laser light radiation L to form a metal layer 30.

[0062] It should be noted that the step of providing a metal powder layer may constitute depositing powder particles, whereas the step of selectively melting may also comprise solidifying or sintering the metal powder.

[0063] Therefore, the three-dimensional structure of the connecting element 31 can be regarded as a stack of multiple metal layers 30. The formation sequence of sub-steps i3-1) and i3-2) allows the three-dimensional connecting element 31 to be constructed in the shape of a curved bridging element, which has a layered first element portion 31-a formed on the semiconductor die structure 2 and a second element portion 31-b formed on the lead terminal 1z1 and the semiconductor die structure 2 (the first die side 2a).

[0064] The specific three-dimensional shape of the connecting element 31 can be established in the layer-by-layer formation steps outlined in sub-steps i3-1) and i3-2) of the method according to the present disclosure. The local thickness and / or local material density (kg / m2) of each metal layer formed during the formation sequence of steps i3-1) and i3-2) can be effectively controlled by adjusting one or more manufacturing parameters. 3 ), wherein the one or more manufacturing parameters are selected from the following: metal powder distribution; supply speed of the metal powder to be deposited; metal powder deposition angle relative to the plane formed by the lead frame; laser power; laser frequency; laser wavelength; ambient processing temperature; metal powder deposition duration of step i3-1); metal powder melting duration of step i3-2).

[0065] Specific parameter characteristics can be:

[0066] Metal powders selected from the following public metal list;

[0067] Speed ​​of supply;

[0068] Metal powder deposition angle;

[0069] The power distribution of the laser used;

[0070] Laser frequency;

[0071] Laser wavelength;

[0072] Ambient processing temperature;

[0073] Deposition duration and melting duration.

[0074] Several metals that can be 3D printed using metal powders include: stainless steel, titanium, aluminum, cobalt chromium, chromium-nickel-inconel, copper, nickel alloy, etc. The metal powder used to form the metal connection element 3 is usually formed by atomization or gas atomization, and can have a range of particle sizes and shapes to adapt to the desired environment for forming the metal connection element 3 during sub-steps i3-1) and i3-2).

[0075] For example, using sub-steps i3-1) and i3-2), a metal connection element 3 can be manufactured having a porous metal density of, for example, 60% to 90%, particularly 75% to 85%, more particularly 80%, thereby producing a more flexible interconnection with a longer lifetime and being less brittle.

[0076] Specifically, by adjusting the above-mentioned printing parameter characteristics, the density of the metal connection element 3 can be flexibly controlled at different positions and / or different parts of the element 3 using sub-steps i3-1) and i3-2). Therefore, the metal connection element 3 can be formed to have increased conductivity (high-density metal powder) or to have reduced stress characteristics (low-density metal powder) as desired.

[0077] Figure 3a to Figure 3b 1 shows a top view and a detailed view of a power module 104 according to the present disclosure. The power module 104 is formed by several lead frame parts 11 that are electrically separated from each other and mounted on a substrate 6. A plurality of semiconductor die structures 31 are mounted to the plurality of lead frame parts 11 and are also electrically connected to each other through connecting elements 31. These connecting elements 31 are manufactured in a manner similar to that of the present invention. Figure 2a to Figure 2b The connection elements 31 in the example are manufactured in a similar manner to those in FIG.

[0078] Optionally, wire bonds 5 are provided between the semiconductor die structure 21 and other terminals 1 z 2 of the lead frame 11 .

[0079] The entire package of the substrate 6, the semiconductor die structure 21, the connecting elements 31, the bonding leads 5, the lead frame portion 11, and the plurality of terminals 1z2 is encapsulated by a mold resin 4 (not shown), with only a portion of the terminals 1z2 being exposed.

[0080] exist Figure 4a and Figure 4bIn another example shown in , the semiconductor package component 102 is a singulated leadless semiconductor package component. Similar to the examples of FIGS. 2 and 3 , the semiconductor die structure 2 has a first die side 2a and a second die side 2b opposite to the first die side 2a. The lead frame 1 made of a metal material has a first frame side 1a and a second frame side 1b opposite to the first frame side 1a, and also has at least two leadless terminals 1z2. The semiconductor die structure 2 is mounted on the first frame side 1a of the lead frame 1 using the second die side 2b of the semiconductor die structure 2.

[0081] According to the method steps of the present disclosure, the connection element 32 of the three-dimensional structure is arranged on the first die side 2a of the semiconductor die structure 2. Specifically, the connection element 32 of the three-dimensional structure is provided in a layer-by-layer manner through a formation sequence of sub-step i3-1), sub-step i3-1) provides a metal powder layer 30 so that the metal powder contacts at least one semiconductor die structure 2 of the lead frame 1 and one of at least two leadless terminals 1z2, and then sub-step i3-2) is performed to selectively melt the metal powder layer 30 using laser radiation to form a metal layer 30.

[0082] Therefore, the three-dimensional structure of the connecting element 32 can be regarded as a stack of multiple metal layers 30. The formation sequence of sub-steps i3-1) and i3-2) allows the construction of a three-dimensional connecting element 32, which is formed by a layered first element portion 32-a (main portion) formed on the semiconductor die structure 2 (and used as a heat sink) and a second element portion 32-b used as an electrical interconnection between the leadless terminal 1z2 and the semiconductor die structure 2 (first die side 2a).

[0083] Optionally, a wire bond 5 is provided between the semiconductor die structure 2 and the further leadless terminal 1 z 2 .

[0084] The entire configuration of the semiconductor die structure 2, the connection elements 32, the bonding leads 5, and the plurality of terminals 1z2 is encapsulated by the mold resin 4, with only a portion of the leadless terminals 1z2 being exposed.

[0085] The design flexibility of the connection element formed by the above-mentioned layer-by-layer production allows the formation of a metal layer with a surface dimension 30a (see Figure 4a ), the surface dimension 30a is larger than the surface dimension of the metal layer formed during the previous formation sequence. In other words, Figure 4a to Figure 4bAs shown, by forming or depositing a metal layer 30 on top of a previous metal layer having a steadily increasing surface size, a connection element 32 having a complex three-dimensional shape can be formed with a funnel shape. In such a funnel shape, the connection element 32 has a larger layer surface area on the top and the larger layer surface area is exposed at the outer surface of the package component 102, and has a smaller layer surface area at the bottom and the smaller layer surface area is located at the interface with the first die side 2a of the semiconductor die structure 2. Such a three-dimensional shape allows the connection element 32 to be used as a heat sink.

[0086] exist Figure 5a to Figure 5b An example of an inverse funnel shape of the connecting element 33 is shown in the example of FIG.

[0087] In all examples of semiconductor package components 101-102-103-104 shown in the present disclosure, each metal layer 30 formed using sub-steps i3-1) and i3-2) can have a thickness of 30 to 40 μm, preferably 35 μm. In addition, the local thickness and / or local material density (kg / m2) of each metal layer formed during this formation sequence of sub-steps i3-1) and i3-2) can be effectively controlled by adjusting one or more manufacturing parameters. 3 ), the one or more manufacturing parameters are selected from the following: metal powder distribution; supply speed of the metal powder to be deposited; metal powder deposition angle relative to the plane formed by the lead frame; laser power; laser frequency; laser wavelength; ambient process temperature; metal powder deposition duration of step i3-1); metal powder melting duration of step i3-2), and according to the combination Figure 2a to Figure 2b The examples describe the parameter ranges involved.

[0088] Since the metal powder connection can be melted between the materials, solder and / or adhesion promoters between the semiconductor die structure and the resulting connection element and between the connection element and the lead frame can be omitted.

[0089] List of reference symbols used

[0090] 10 1-2-3 (First, second, third) semiconductor package

[0091] 104 Semiconductor packaging components / power modules

[0092] 1 Lead frame

[0093] 1a First side of the lead frame

[0094] 1b Second side of the lead frame

[0095] 1z1 with lead terminal

[0096] 1z2 No lead terminal

[0097] 2-21 Semiconductor die

[0098] 2a First die side of semiconductor die

[0099] 2b Second die side of the semiconductor die

[0100] 31-32-33 (First, Second, Third Examples) Electrical / Mechanical Connection Elements

[0101] 31-a / 32-a First component

[0102] 31-b / 32-b Second component

[0103] 4 Encapsulant

[0104] 5 Additional wire-bond components

[0105] 6 substrate

[0106] 30 Metal powder layers

[0107] 30a Surface dimensions.

Claims

1. A method for manufacturing a semiconductor package assembly, the method comprising the following steps i) forming at least one semiconductor package by the following sub-steps: i1) providing a lead frame (1), the lead frame (1) comprising a first section and a second section, the first section being made of a metal material, the first section having a first frame side (1a) and a second frame side (1b) opposite to the first frame side (1a) and comprising at least one terminal (1z1), the first section being separated from the second section by a gap, the second section being made of the metal material and comprising at least one terminal (1z1); i2) providing at least one semiconductor die structure (2), the semiconductor die structure (2) having a first die side (2a) and a second die side (2b) opposite the first die side (2a), the semiconductor die structure (2) being mounted on the first frame side (1a) of the first section of the lead frame by means of the second die side (2a); i3) providing one or more connecting elements (31), the connecting elements (31) bridging the gap between the at least one semiconductor die structure (2) on the first section of the lead frame and the at least one terminal (1z1) of the second section of the lead frame, thereby forming an electrical connection and a mechanical connection; as well as ii) encapsulating the at least one semiconductor die structure (2), the one or more connection elements (3a) and the plurality of terminals (1z1) with a molding resin (4), leaving at least a portion of at least two terminals (1z1) exposed, thereby forming at least one encapsulated semiconductor package component having terminals at opposite sides; Wherein, the step i3) comprises at least one formation sequence of the following sub-steps: i3-1) providing a layer of metal powder (30) such that the metal powder is in contact with the at least one semiconductor die structure (2) and one of the at least two terminals (1z1) of the lead frame; i3-2) Using laser radiation to selectively melt the layer of metal powder to form a metal layer.

2. The method for manufacturing a semiconductor package assembly according to claim 1, wherein: The formation sequence of steps i3-1) and i3-2) is performed alternately multiple times, thereby forming a three-dimensional stack of subsequent molten metal layers.

3. The method for manufacturing a semiconductor package assembly according to claim 1 or 2, further comprising controlling the local thickness and / or local density of each metal layer formed during the formation sequence of steps i3-1) and i3-2) by adjusting one or more manufacturing parameters, wherein the one or more manufacturing parameters are selected from the following: -Metal powder distribution; - the supply rate of the metal powder to be deposited; - Angle of metal powder deposition relative to the plane formed by the lead frame; - Laser power; -Laser frequency; -Laser wavelength; - Ambient processing temperature; - Duration of the metal powder deposition in step i3-1); - Duration of melting of the metal powder in step i3-2).

4. A method for manufacturing a semiconductor package assembly according to any one or more of claims 1 to 3, wherein: Each metal layer formed in step i3-2) has a thickness of 30 to 40 μm, preferably 35 μm.

5. The method for manufacturing a semiconductor package assembly according to any one or more of claims 1 to 4, wherein: The surface dimensions of the metal layer are larger than the surface dimensions of the metal layer formed during a previous formation sequence.

6. A method for manufacturing a semiconductor package assembly according to any one or more of claims 1 to 4, wherein: The surface dimensions of the metal layer are smaller than the surface dimensions of the metal layer formed during a previous formation sequence.

7. The method for manufacturing a semiconductor package component according to any one or more of claims 1 to 6, further comprising a step iii), wherein step iii) is performed after the final formation sequence of steps i3-1) and i3-2) but before step ii), wherein step iii) roughens the surface of the exposed portions of the at least two terminals using, for example, a chemical agent.

8. The method for manufacturing a semiconductor package assembly according to any one or more of claims 1 to 7, further comprising a step iv) after step ii) or step iii), wherein the step iv) is to plate the exposed portions of the at least two terminals with a metal plating material.

9. The method for manufacturing a semiconductor package assembly according to any one or more of claims 1 to 8, further comprising a step v) after step iv), wherein the step v) singulates the encapsulated semiconductor package in the lead frame to form individual semiconductor package assemblies.

10. A semiconductor package assembly, the semiconductor package assembly consisting of a semiconductor die structure electrically and mechanically attached to at least two terminals by one or more connecting elements, and encapsulated by a molding resin so that a portion of the at least two terminals is exposed, wherein: The one or more connecting elements between the semiconductor die structure and the at least two terminals are formed according to the method steps of any one or more of claims 1 to 9.

11. The semiconductor package assembly according to claim 10, wherein: The semiconductor package assembly is a leadless semiconductor package assembly.

12. The semiconductor package assembly according to claim 10, wherein: The semiconductor package assembly is a leaded semiconductor package assembly.