Multi-source coaxial plasma welding mechanism and additive cladding equipment

By introducing a rotating seat and driving assembly into the plasma arc cladding equipment, the rotation of the cathode rod is ensured, the problem of uneven heating of the filler is solved, the quality and stability of the welded joints are improved, and the welding effect is optimized.

CN118744271AInactive Publication Date: 2024-10-08ANHUI TECHN COLLEGE OF MECHANICAL & ELECTRICAL ENG
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411055042.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-02
Publication Date
2024-10-08
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

When the filling material of existing plasma arc cladding equipment is wire, the side-axis wire feeding method causes differences in weld morphology and affects dimensional accuracy; when the filling material is powder, the powder is difficult to completely melt, resulting in low material utilization and metallurgical defects. , and increasing the plasma arc power or reducing the powder conveying speed will affect the cladding efficiency.

Method used

Designing a multi-source coaxial plasma welding mechanism, the driving assembly guides the rotating base to rotate when the filler is fed, ensuring the rotation of the cathode rod and achieving uniform heating of the filling material. The combined design of the rotating base and driving assembly is used to ensure the plasma arc Even distribution and even heating of the filler.

Benefits of technology

Through uniform heat energy distribution, the quality and stability of welded joints are improved, welding defects are reduced, welding effects are optimized, and more precise welding control is achieved by adjusting the parameters of the drive components.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118744271A_ABST
    Figure CN118744271A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of metal part forming machining, in particular to a multi-source coaxial plasma welding mechanism and additive cladding equipment. The multi-source coaxial plasma welding mechanism comprises a welding head, the welding head is provided with a feeding channel located in the center of the welding head and extending in the longitudinal direction, and a rotating base coaxial with the feeding channel is arranged in the welding head; an ion airflow channel distributed in the circumferential direction of the feeding channel is formed in the rotating base, a cathode bar is arranged in the ion airflow channel, the diameter of the cathode bar is smaller than the inner diameter of the ion airflow channel, a driving assembly is further arranged in the welding head, and through accurate control of the driving assembly, the rotating base can be guided to rotate when the filler is fed. By means of the design, the cathode bar installed on the rotating base can synchronously rotate along with the rotating base, the acting range of plasma arcs in the welding process can be expanded and changed along with rotation of the cathode bar, and therefore it is guaranteed that more uniform heat energy distribution can be borne by filling materials when the filling materials are heated.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of metal parts forming and processing, and in particular to a multi-source coaxial plasma welding mechanism and additive cladding equipment. Background Art

[0002] Plasma cladding technology is a means of repairing and remanufacturing mechanical surfaces by using a water cooling system to control the nozzle arc constraint, using the transfer arc as a heat source to obtain a high-energy density plasma arc, and using various alloy powders and wires. Existing plasma arc cladding / surfacing equipment mostly uses a single plasma arc as a heat source, and one or more filling materials are fed into the plasma arc from one side or the periphery of the plasma arc. When powder is used as the filling material, multiple powders are focused under the plasma arc; when wire is used as the filling material, a single wire is fed from one side to the bottom of the plasma arc, which is the so-called side-axis wire feeding method.

[0003] However, the existing plasma arc cladding equipment has the following shortcomings: 1. If the filling material is wire, its side-axis wire feeding method makes the morphology of the deposited weld under different movement modes have great differences, which will cause cumulative errors and affect the dimensional accuracy when performing surface cladding and additive manufacturing. When feeding the wire in the reverse and sideways direction, the end of the wire will interfere with the already formed weld, affecting the stability of wire feeding. Since the wire and the deposited weld interfere with the plasma arc during the movement, the arc length changes, which has an adverse effect on the shape and quality of the weld. 2. If the filling material is powder, since the powder enters the plasma arc from the outside to the inside, it is difficult for the powder to be completely melted. On the one hand, the material utilization rate is reduced, and on the other hand, the unmelted powder entering the molten pool may cause metallurgical defects. In order to improve the quality of the weld, the existing plasma arc cladding equipment mostly adopts the method of increasing the plasma arc power or reducing the powder conveying speed, but such operation will increase the heat input of the part substrate or reduce the cladding efficiency.

[0004] Chinese patent publication number CN111590178A discloses a multi-source coaxial plasma arc cladding process and equipment, which includes a welding gun mechanism, a feeding mechanism, a power supply mechanism and an ion gas supply device; the welding gun mechanism includes a plasma arc generating component, the plasma arc generating component includes a cathode rod and a lower gun body, the positive electrode and the negative electrode of the arc starting circuit of the power supply mechanism are electrically connected to the lower gun body and the cathode rod respectively, the lower gun body includes an ion gas flow channel and a conductive nozzle, the cathode rod is inserted in the ion gas flow channel, the welding gun mechanism includes a feeding guide nozzle and multiple cathode rods, the lower gun body includes an ion gas flow channel and a conductive nozzle arranged in a one-to-one correspondence with the cathode rods, the central axes of the injection ports of the multiple conductive nozzles intersect at one point as an intersection point, and the intersection point is located on the central axis of the feeding guide nozzle outlet and below the feeding guide nozzle outlet.

[0005] The welding gun mechanism in the equipment forms a plasma arc between the cathode rod and the workpiece through several fixed settings. Since the cathode rod is stationary and the filler is fed vertically, this may cause the filler to be subjected to uneven heat distribution during the melting process. The filler close to the cathode rod may receive more heat, while the filler far from the cathode rod may not be melted enough; due to the uneven heat distribution, the quality of the welded joint may be affected. Some areas may be over-melted, while other areas may not be fully fused, resulting in unstable strength, sealing or appearance quality of the welded joint. Summary of the invention

[0006] In view of the above problems, a multi-source coaxial plasma welding mechanism and additive cladding equipment are provided. The driving assembly can guide the rotating seat to rotate when the filler material is fed, so that the cathode rod installed on the rotating seat can be rotated, thereby ensuring that the filler material is heated more evenly, solving the problem that the filler material is easily heated unevenly during welding in the existing welding gun mechanism.

[0007] In order to solve the problems of the prior art, the present invention provides a multi-source coaxial plasma welding mechanism, including a welding head, the welding head having a feeding channel located at the center position thereof and extending longitudinally, a rotating seat coaxial with the feeding channel is provided in the welding head, an ion air flow channel distributed circumferentially along the feeding channel is provided on the rotating seat, a cathode rod is provided in the ion air flow channel, the diameter of the cathode rod is smaller than the inner diameter of the ion air flow channel, the central axis of the injection port at the bottom end of the centrifugal air flow channel intersects with the central axis of the feeding channel, and a driving component for driving the rotating support to rotate is also provided in the welding head.

[0008] Preferably, a cooling cavity for cooling the ion airflow channel is provided in the rotating seat, and a water inlet and a water outlet which can be connected with the cooling cavity are provided on the welding head.

[0009] Preferably, a water inlet ring groove and a water outlet ring groove coaxial therewith are provided on the outer circumferential surface of the rotating seat, the water inlet ring groove is connected to the water inlet, the water outlet ring groove is connected to the water outlet, a lower connecting port connected to the cooling chamber is provided in the water inlet ring groove, and an upper connecting port connected to the cooling chamber is provided in the water outlet ring groove.

[0010] Preferably, a protective gas flow cavity is also provided in the welding head, the bottom end of the protective gas flow cavity extends downward to form an annular protective gas port located outside the ion gas flow channel, and a protective gas interface connected to the protective gas flow cavity is provided on the welding head.

[0011] Preferably, the driving assembly includes a transmission cylinder coaxially arranged at the top of the rotating seat, an annular air passage is formed between the outer circumferential surface of the transmission cylinder and the inner circumferential surface of the welding head, a buffer chamber connected to the ion gas flow channel is arranged between the bottom end of the transmission cylinder and the top of the rotating seat, and an ion gas inlet connected to the annular air passage is also arranged on the welding head. The outer circumferential surface of the transmission cylinder is provided with arc blades arranged along its circumference. When the ion gas passes through the annular air passage and enters the buffer chamber, the transmission cylinder drives the rotating seat to rotate in the welding head.

[0012] Preferably, a sealing cylinder is provided on the upper part of the outer circumference of the transmission cylinder, and the sealing cylinder is rotatably connected to the top of the inner cavity of the welding head in a sealing manner, and an annular air cavity is formed between the sealing cylinder and the inner circumference of the welding head, and the annular air cavity is connected to the annular air passage.

[0013] Preferably, the top end of the cathode rod passes through the buffer cavity and extends into the inner cavity of the welding head. An annular electric sheet is provided at the top end of the inner cavity of the welding head. The annular electric sheet is connected to the power cathode, and the top end of the cathode rod abuts against the bottom end of the annular electric sheet.

[0014] Preferably, the annular electric sheet is conical, and the top of the inner cavity of the welding head is provided with an embedding groove for embedding and installing the annular electric sheet, and the annular electric sheet elastically abuts against the top of the cathode rod.

[0015] Preferably, the engaging groove is provided with an annular fulcrum, and the welding head is also provided with a connecting bolt which penetrates the welding head and extends into the engaging groove, and the connecting bolt abuts against the top surface of the annular electric sheet.

[0016] Multi-source coaxial plasma additive cladding equipment comprises a multi-source coaxial plasma welding mechanism.

[0017] Compared with the prior art, the present application has the following beneficial effects: the present application can guide the rotating seat to rotate when the filler is fed through the precise control of the drive assembly. This design enables the cathode rod installed on the rotating seat to perform synchronous rotational motion. As the cathode rod rotates, the range of action of the plasma arc in the welding process is also expanded and changed, thereby ensuring that the filler can be subjected to a more uniform distribution of heat energy when heated. The dynamic heating method has significant advantages over the traditional static heating method. First, due to the rotation of the cathode rod, the plasma arc heats the filler more evenly, avoiding the problem of uneven melting of the filler due to uneven heat distribution. Secondly, uniform heating helps to improve the overall quality and stability of the welded joint and reduce the occurrence of welding defects. In addition, by adjusting the control parameters of the drive assembly, such as rotation speed, rotation direction, etc., the welding effect can be further optimized. For example, the rotation speed and direction of the cathode rod can be adjusted according to the material, shape and welding requirements of the filler to achieve more accurate welding control. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] Figure 1 It is a stereoscopic diagram of a multi-source coaxial plasma welding mechanism.

[0019] Figure 2 It is a cross-sectional view of a multi-source coaxial plasma welding mechanism.

[0020] Figure 3 It is a schematic diagram of the internal structure of a multi-source coaxial plasma welding mechanism.

[0021] Figure 4 It is a stereoscopic diagram of the cathode rod and the rotating seat in the multi-source coaxial plasma welding mechanism.

[0022] Figure 5 It is a three-dimensional exploded view of a rotating seat in a multi-source coaxial plasma welding mechanism.

[0023] Figure 6 It is a distribution diagram of cathode rods and fillers in a multi-source coaxial plasma welding mechanism.

[0024] Figure 7 It is a schematic diagram of the internal structure of a rotating seat in a multi-source coaxial plasma welding mechanism.

[0025] The numbers in the figure are: 1. welding head; 11. feeding channel; 12. water inlet; 13. water outlet; 14. protective air flow chamber; 15. annular protective air port; 16. protective air interface; 17. ion gas inlet; 18. fitting groove; 181. annular fulcrum; 19. connecting bolt; 2. rotating seat; 21. ion air flow channel; 22. cooling chamber; 23. water inlet ring groove; 231. lower connecting port; 24. water outlet ring groove; 241. upper connecting port; 3. cathode rod; 4. driving assembly; 41. transmission cylinder; 411. arc blade; 42. annular air passage; 43. buffer chamber; 44. sealing cylinder; 45. annular air cavity; 5. annular electrode. DETAILED DESCRIPTION

[0026] In order to further understand the features, technical means, specific objectives and functions of the present invention, the present invention is further described in detail below in conjunction with the accompanying drawings and specific implementation methods.

[0027] like Figure 1 and Figure 2As shown, the present application provides a multi-source coaxial plasma welding mechanism, including a welding head 1, the welding head 1 has a feed channel 11 located at its center and extending longitudinally, a rotating seat 2 coaxial with the feed channel 11 is provided in the welding head 1, an ion gas flow channel 21 distributed circumferentially along the feed channel 11 is provided on the rotating seat 2, a cathode rod 3 is provided in the ion gas flow channel 21, the diameter of the cathode rod 3 is smaller than the inner diameter of the ion gas flow channel 21, the central axis of the injection port at the bottom end of the centrifugal gas flow channel intersects with the central axis of the feed channel 11, and a driving component 4 for driving the rotating support to rotate is also provided in the welding head 1.

[0028] The welding head 1 has a feeding channel 11 located at a central position and extending in the longitudinal direction. This feeding channel 11 is the main path for the filler to enter the welding area, and its design ensures that the filler can be stably and continuously supplied.

[0029] Secondly, a rotating seat 2 coaxial with the feeding channel 11 is provided inside the welding head 1. The rotating seat 2 carries the cathode rod 3 and allows the cathode rod 3 to rotate during the welding process. Through the rotation of the rotating seat 2, the cathode rod 3 can form multiple plasma arc sources around the feeding channel 11 to achieve multi-source welding.

[0030] On the rotating seat 2, a plurality of ion gas flow channels 21 are distributed along the circumference of the feeding channel 11. A cathode rod 3 is arranged in each ion gas flow channel 21, and the diameter of these cathode rods 3 is smaller than the inner diameter of the ion gas flow channel 21 to ensure that the cathode rod 3 can generate a stable plasma arc when rotating. When electricity is applied between the cathode rod 3 and the workpiece, a high-temperature plasma arc can be generated to melt the filler on the workpiece.

[0031] The central axis of the bottom injection port of the centrifugal gas flow channel intersects with the central axis of the feed channel 11. This design enables the plasma arc to directly act on the filler in the feed channel 11 and ensures that the filler is subjected to uniform heat energy distribution during the melting process.

[0032] Finally, the welding head 1 is also provided with a driving assembly 4 for driving the rotating seat 2 to rotate. The driving assembly 4 can adjust the rotation speed and direction of the rotating seat 2 as needed to optimize the welding effect. By accurately controlling the rotational movement of the rotating seat 2, the cathode rod 3 can be evenly distributed around the feeding channel 11 and the plasma arc can be stably generated.

[0033] This embodiment can guide the rotating seat 2 to rotate when the filler material is fed through the precise control of the driving assembly 4. This design enables the cathode rod 3 installed on the rotating seat 2 to perform synchronous rotational motion. As the cathode rod 3 rotates, the range of action of the plasma arc during the welding process is also expanded and changed, thereby ensuring that the filler material can receive a more uniform distribution of heat energy when heated.

[0034] This dynamic heating method has significant advantages over the traditional static heating method. First, due to the rotation of the cathode rod 3, the plasma arc heats the filler more evenly, avoiding the problem of uneven melting of the filler due to uneven heat distribution. Second, uniform heating helps to improve the overall quality and stability of the welded joint and reduce the occurrence of welding defects.

[0035] In addition, the welding effect can be further optimized by adjusting the control parameters of the driving assembly 4, such as the rotation speed, rotation direction, etc. For example, the rotation speed and direction of the cathode rod 3 can be adjusted according to the material, shape and welding requirements of the filler to achieve more accurate welding control.

[0036] In summary, by introducing the design of the rotating seat 2 and the driving assembly 4, the new welding gun mechanism successfully solves the problem of uneven heating of the filler during welding in the existing welding gun mechanism.

[0037] like Figure 2 As shown, a cooling chamber 22 for cooling the ion air flow channel 21 is provided in the rotating seat 2 , and a water inlet 12 and a water outlet 13 which can be connected to the cooling chamber 22 are provided on the welding head 1 .

[0038] In the rotating seat 2, a cooling chamber 22 for cooling the ion gas flow channel 21 is provided. The cathode rod 3 in the ion gas flow channel 21 will face the challenge of high temperature in the process of generating a high-temperature plasma arc. Long-term high-temperature operation will not only affect the performance and life of the cathode rod 3, but may also have an adverse effect on the welding quality. Therefore, by introducing the cooling chamber 22, the temperature of the ion gas flow channel 21 and the cathode rod 3 can be effectively reduced to maintain their stable working state.

[0039] In order to realize the cooling function of the cooling chamber 22, a water inlet 12 and a water outlet 13 are also provided on the welding head 1. These two interfaces are connected to the cooling chamber 22 to form a complete cooling cycle. During the welding process, cooling water enters the cooling chamber 22 through the water inlet 12, absorbs heat and is then discharged through the water outlet 13, and this cycle is repeated to achieve a continuous cooling effect on the ion air flow channel 21 and the cathode rod 3.

[0040] The introduction of the cooling system not only improves the stability and durability of the welding head 1, but also further ensures the stability of the welding process and the quality of the welded joint. By accurately controlling the flow and temperature of the cooling water, the temperature of the ion gas flow channel 21 and the cathode rod 3 can be accurately controlled, thereby optimizing the welding effect.

[0041] like Figure 2 and Figure 3 , Figure 4As shown, a water inlet annular groove 23 and a water outlet annular groove 24 coaxial therewith are provided on the outer circumferential surface of the rotating seat 2, the water inlet annular groove 23 is connected with the water inlet 12, the water outlet annular groove 24 is connected with the water outlet 13, a lower connecting port 231 connected with the cooling chamber 22 is provided in the water inlet annular groove 23, and an upper connecting port 241 connected with the cooling chamber 22 is provided in the water outlet annular groove 24.

[0042] The outer circumferential surface of the rotating seat 2 is provided with a coaxial water inlet groove 23 and a water outlet groove 24, which not only facilitates the circulation of cooling water, but also can be seamlessly connected with the water inlet 12 and the water outlet 13 of the welding head 1 to realize the closed cycle of the cooling system.

[0043] Specifically, the water inlet annular groove 23 is connected to the water inlet 12 of the welding head 1 through a pipeline. When cooling water flows in from the water inlet 12, it will first enter the water inlet annular groove 23. In order to effectively guide the cooling water into the cooling chamber 22, a lower connecting port 231 connected to the cooling chamber 22 is provided on the water inlet annular groove 23. In this way, the cooling water can enter the cooling chamber 22 through the lower connecting port 231 to cool the ion air flow channel 21 and the cathode rod 3.

[0044] Similarly, the water outlet annular groove 24 is connected to the water outlet 13 of the welding head 1 through a pipeline. When the cooling water completes the cooling task in the cooling chamber 22, it will flow to the water outlet annular groove 24. In order to discharge the cooling water smoothly, an upper connecting port 241 connected to the cooling chamber 22 is provided on the water outlet annular groove 24. In this way, the cooling water can flow out of the water outlet annular groove 24 through the upper connecting port 241 and finally be discharged from the water outlet 13.

[0045] This design not only ensures the unimpeded circulation of cooling water, but also realizes precise control of the cooling water flow. By adjusting the opening of the water inlet 12 and the water outlet 13, the flow rate and flow velocity of the cooling water can be controlled, thereby realizing precise control of the ion gas flow channel 21 and the temperature of the cathode rod 3.

[0046] In addition, the coaxial design of the water inlet annular groove 23 and the water outlet annular groove 24 makes the cooling water more evenly distributed on the rotating seat 2, thereby improving the cooling effect. At the same time, this design also reduces the complexity and maintenance cost of the cooling system, and improves the reliability and service life of the welding head 1.

[0047] like Figure 2 As shown, a protective gas flow chamber 14 is also provided in the welding head 1, and the bottom end of the protective gas flow chamber 14 extends downward to form an annular protective gas port 15 located outside the ion gas flow channel 21, and a protective gas interface 16 connected to the protective gas flow chamber 14 is provided on the welding head 1.

[0048] In the welding head 1, in addition to the feeding channel 11, the rotating seat 2 and the cooling system, a protective airflow chamber 14 is also specially provided. The design purpose of this protective airflow chamber 14 is to provide a layer of protective airflow for the welding area to prevent possible pollution and impurity interference during the welding process.

[0049] The bottom end of the shielding gas flow chamber 14 extends downward to form an annular shielding gas port 15 located outside the ion gas flow channel 21. The annular shielding gas port 15 can release the shielding gas flow evenly to ensure that the welding area is surrounded by a layer of stable gas flow. This design can not only prevent oxidation and contamination of the welding area, but also reduce spatter and sparks during welding, thereby improving the quality and appearance of the welded joint.

[0050] In order to conveniently inject shielding gas into the shielding gas flow chamber 14, a shielding gas interface 16 connected to the shielding gas flow chamber 14 is also provided on the welding head 1. Through this interface, a shielding gas source can be conveniently connected to inject the required gas into the shielding gas flow chamber 14. Generally, the shielding gas can be an inert gas such as argon or nitrogen, which has the characteristic of not easily reacting with metals and can effectively protect the welding area.

[0051] The introduction of the protective gas flow system enables the multi-source coaxial plasma welding mechanism to have better protection capabilities during the welding process. It can not only prevent contamination and oxidation of the welding area, but also reduce spatter and sparks during the welding process, and improve the quality and appearance of the welded joint. At the same time, this design also improves the reliability and service life of the welding head 1, making the welding process more stable and reliable.

[0052] like Figure 2 , Figure 5 , Figure 6 and Figure 7 As shown, the driving assembly 4 includes a transmission cylinder 41 coaxially arranged at the top of the rotating seat 2, an annular air passage 42 is formed between the outer circumferential surface of the transmission cylinder 41 and the inner circumferential surface of the welding head 1, a buffer chamber 43 connected to the ion gas flow channel 21 is arranged between the bottom end of the transmission cylinder 41 and the top of the rotating seat 2, and an ion gas inlet 17 connected to the annular air passage 42 is also arranged on the welding head 1, and the outer circumferential surface of the transmission cylinder 41 is provided with arc blades 411 arranged along its circumference. When the ion gas passes through the annular air passage 42 and enters the buffer chamber 43, the transmission cylinder 41 drives the rotating seat 2 to rotate in the welding head 1.

[0053] The driving assembly 4 is mainly composed of a transmission cylinder 41 coaxially arranged at the top of the rotating base 2. An annular gas passage 42 is formed between the outer circumference of the transmission cylinder 41 and the inner circumference of the welding head 1. This passage not only provides a path for the circulation of ion gas, but also ensures ventilation and heat dissipation inside the welding head 1.

[0054] A buffer chamber 43 connected to the ion gas flow channel 21 is provided between the bottom end of the transmission cylinder 41 and the top end of the rotating seat 2. The buffer chamber 43 plays a role of transition and buffering. When the ion gas enters the buffer chamber 43 through the annular gas passage 42, its flow rate and pressure are properly adjusted to ensure that the ion gas can enter the ion gas flow channel 21 smoothly and evenly.

[0055] In order to conveniently inject ion gas into the annular gas passage 42, the welding head 1 is also provided with an ion gas inlet 17 connected to the annular gas passage 42. Through this inlet, an ion gas source can be conveniently connected to inject the required ion gas into the annular gas passage 42.

[0056] The outer circumferential surface of the transmission cylinder 41 is provided with arc blades 411 arranged along the circumference thereof. The arc blades 411 can generate a rotation torque when the ion gas passes through the annular gas passage 42 and enters the buffer chamber 43, thereby driving the transmission cylinder 41 and the rotating seat 2 connected thereto to rotate in the welding head 1. This design not only realizes the effective delivery of ion gas, but also realizes the automatic rotation of the welding head 1, thereby improving the automation degree of the welding process.

[0057] By introducing the drive assembly 4 and related design optimization, the multi-source coaxial plasma welding mechanism has better stability and reliability during the welding process. It can not only ensure the cleanliness and stability of the welding area, but also realize the automatic rotation of the welding head 1, and improve the quality and appearance of the welded joint. At the same time, this design also improves the service life and reliability of the welding head 1, making the welding process more efficient, environmentally friendly and reliable.

[0058] like Figure 2 As shown, a sealing cylinder 44 is provided on the upper part of the outer circumference of the transmission cylinder 41, and the sealing cylinder 44 is rotatably connected to the top of the inner cavity of the welding head 1 in a sealing manner. An annular air cavity 45 is formed between the sealing cylinder 44 and the inner circumference of the welding head 1, and the annular air cavity 45 is connected to the annular air passage 42.

[0059] The sealing cylinder 44 is connected to the top of the inner cavity of the welding head 1 in a sealed rotational manner, and this design ensures that no gas leakage occurs during the rotation process. An annular air cavity 45 is formed between the sealing cylinder 44 and the inner circumferential surface of the welding head 1, and this air cavity is connected to the annular gas passage 42 to form a complete ion gas flow path.

[0060] The design of the annular air cavity 45 not only provides a circulation space for the ion gas, but also ensures the stability and uniformity of the ion gas during the passage. After the ion gas enters the annular gas passage 42 from the ion gas inlet 17, it will further flow into the annular air cavity 45 and be fully distributed and buffered therein. Subsequently, the ion gas enters the ion gas flow channel 21 through the buffer cavity 43, providing necessary protection for the welding process.

[0061] This design not only improves the sealing performance of the welding head 1, but also enhances its stability and reliability. During the welding process, even in the face of harsh environments such as high temperature and high pressure, the welding head 1 can maintain stable operation and ensure the consistency and reliability of welding quality.

[0062] like Figure 2 As shown, the top end of the cathode rod 3 passes through the buffer cavity 43 and extends into the inner cavity of the welding head 1. An annular electric sheet 5 is provided at the top end of the inner cavity of the welding head 1. The annular electric sheet 5 is connected to the cathode of the power supply, and the top end of the cathode rod 3 abuts against the bottom end of the annular electric sheet 5.

[0063] An annular electric sheet 5 is arranged at the top of the inner cavity of the welding head 1. This electric sheet is connected to the cathode of the power supply and is one of the key electrodes in the welding process. The top of the cathode rod 3 passes through the buffer cavity 43 and accurately abuts against the bottom end of the annular electric sheet 5. This design ensures that the cathode rod 3 can also be in good contact with the annular electric sheet 5 when rotating, thereby ensuring stable current transmission during the welding process.

[0064] like Figure 2 As shown, the annular electric sheet 5 is conical, and the top of the inner cavity of the welding head 1 is provided with an embedding groove 18 for embedding and installing the annular electric sheet 5 , and the annular electric sheet 5 elastically abuts against the top of the cathode rod 3 .

[0065] The main function of the fitting groove 18 is to fit the annular electric sheet 5. As one of the key electrodes in the welding process, the stability of the installation and the reliability of the contact of the annular electric sheet 5 directly affect the quality of welding. Therefore, the design of the fitting groove 18 has been carefully considered to ensure that the annular electric sheet 5 can be firmly fitted in the groove to avoid shaking or falling off during the welding process.

[0066] In addition, in order to further enhance the contact stability between the annular electric sheet 5 and the cathode rod 3, an elastic abutment design is adopted. Specifically, the bottom of the annular electric sheet 5 is designed with an elastic contact surface, and when the annular electric sheet 5 is installed in the fitting groove 18, this contact surface will elastically abut the top of the cathode rod 3. This design can not only ensure good contact between the annular electric sheet 5 and the cathode rod 3, but also compensate for the uneven contact surface caused by processing errors or installation errors to a certain extent, thereby ensuring stable current transmission during welding.

[0067] like Figure 2 As shown, the fitting groove 18 is provided with an annular fulcrum 181 , and the welding head 1 is also provided with a connecting bolt 19 penetrating the welding head 1 and extending into the fitting groove 18 , and the connecting bolt 19 abuts against the top surface of the annular electric sheet 5 .

[0068] An annular fulcrum 181 is provided at the bottom of the fitting groove 18. The annular fulcrum 181 not only provides additional support for the annular electric sheet 5, but also ensures the flatness and stability of the annular electric sheet 5 after installation.

[0069] In order to achieve fine adjustment of the position of the annular electric sheet 5, a connecting bolt 19 is provided on the welding head 1, which penetrates the welding head 1 and extends into the fitting groove 18. The top end of the connecting bolt 19 abuts against the top surface of the annular electric sheet 5, and the position of the annular electric sheet 5 in the fitting groove 18 can be finely adjusted by rotating the connecting bolt 19. This design makes the installation and adjustment of the annular electric sheet 5 very convenient and quick, and greatly improves the work efficiency.

[0070] Multi-source coaxial plasma additive cladding equipment comprises a multi-source coaxial plasma welding mechanism.

[0071] The above embodiments only express one or several implementation modes of the present invention, and the description thereof is relatively specific and detailed, but it cannot be understood as limiting the scope of the present invention. It should be pointed out that, for those of ordinary skill in the art, several variations and improvements can be made without departing from the concept of the present invention, and these all belong to the protection scope of the present invention. Therefore, the protection scope of the present invention shall be subject to the attached claims.

Claims

1. Multi-source coaxial plasma welding mechanism, characterized in that: The invention comprises a welding head (1), wherein the welding head (1) has a feeding channel (11) located at a central position thereof and extending in a longitudinal direction, wherein a rotating seat (2) coaxial with the feeding channel (11) is arranged in the welding head (1), wherein an ion gas flow channel (21) distributed circumferentially along the feeding channel (11) is arranged on the rotating seat (2), wherein a cathode rod (3) is arranged in the ion gas flow channel (21), wherein the diameter of the cathode rod (3) is smaller than the inner diameter of the ion gas flow channel (21), wherein the central axis of the injection port at the bottom end of the centrifugal gas flow channel intersects with the central axis of the feeding channel (11), and wherein a driving component (4) for driving the rotating support to rotate is also arranged in the welding head (1).

2. The multi-source coaxial plasma welding mechanism according to claim 1, characterized in that: A cooling chamber (22) for cooling the ion airflow channel (21) is provided in the rotating seat (2), and a water inlet (12) and a water outlet (13) that can be connected to the cooling chamber (22) are provided on the welding head (1).

3. The multi-source coaxial plasma welding mechanism according to claim 2, characterized in that: A water inlet annular groove (23) and a water outlet annular groove (24) coaxial with the rotating seat (2) are provided on the outer circumferential surface thereof; the water inlet annular groove (23) is communicated with the water inlet (12); the water outlet annular groove (24) is communicated with the water outlet (13); a lower connecting port (231) communicated with the cooling chamber (22) is provided in the water inlet annular groove (23); and an upper connecting port (241) communicated with the cooling chamber (22) is provided in the water outlet annular groove (24).

4. The multi-source coaxial plasma welding mechanism according to claim 1, characterized in that: A protective gas flow chamber (14) is also provided in the welding head (1), the bottom end of the protective gas flow chamber (14) extends downward to form an annular protective gas port (15) located outside the ion gas flow channel (21), and a protective gas interface (16) connected to the protective gas flow chamber (14) is provided on the welding head (1).

5. The multi-source coaxial plasma welding mechanism according to claim 1, characterized in that: The drive assembly (4) comprises a transmission cylinder (41) coaxially arranged at the top of the rotating seat (2); an annular air passage (42) is formed between the outer circumferential surface of the transmission cylinder (41) and the inner circumferential surface of the welding head (1); a buffer chamber (43) connected to the ion gas flow passage (21) is arranged between the bottom end of the transmission cylinder (41) and the top end of the rotating seat (2); an ion gas inlet (17) connected to the annular air passage (42) is also arranged on the welding head (1); the outer circumferential surface of the transmission cylinder (41) is provided with arc-shaped blades (411) arranged along the circumference thereof; when the ion gas passes through the annular air passage (42) and enters the buffer chamber (43), the transmission cylinder (41) drives the rotating seat (2) to rotate in the welding head (1).

6. The multi-source coaxial plasma welding mechanism according to claim 5, characterized in that: A sealing cylinder (44) is provided at the upper portion of the outer circumferential surface of the transmission cylinder (41), and the sealing cylinder (44) is rotatably connected to the top end of the inner cavity of the welding head (1) in a sealing manner. An annular air cavity (45) is formed between the sealing cylinder (44) and the inner circumferential surface of the welding head (1), and the annular air cavity (45) is in communication with the annular air passage (42).

7. The multi-source coaxial plasma welding mechanism according to claim 5, characterized in that: The top end of the cathode rod (3) passes through the buffer cavity (43) and extends into the inner cavity of the welding head (1). An annular electric sheet (5) is provided at the top end of the inner cavity of the welding head (1). The annular electric sheet (5) is connected to the cathode of the power supply. The top end of the cathode rod (3) abuts against the bottom end of the annular electric sheet (5).

8. The multi-source coaxial plasma welding mechanism according to claim 7, characterized in that: The annular electric sheet (5) is conical, and a fitting groove (18) for fitting and installing the annular electric sheet (5) is provided at the top end of the inner cavity of the welding head (1), and the annular electric sheet (5) is elastically abutted against the top end of the cathode rod (3).

9. The multi-source coaxial plasma welding mechanism according to claim 8, characterized in that: The engaging groove (18) is provided with an annular fulcrum (181), and the welding head (1) is also provided with a connecting bolt (19) penetrating the welding head (1) and extending into the engaging groove (18), wherein the connecting bolt (19) abuts against the top surface of the annular electric sheet (5).

10. Multi-source coaxial plasma additive cladding equipment, characterized in that: It comprises the multi-source coaxial plasma welding mechanism as described in any one of claims 1-9.