Method of forming bonded assembly
By using a plasma jet to clean the copper surface oxide on the semiconductor wafer in a low-oxygen environment, the bonding problem caused by oxides in the traditional bonding process is solved, high-strength and low-resistance bonding wire bonding is achieved, and the manufacturing quality is improved. and reliability.
Patent Information
- Application Number
- CN202410645461.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-06-02
- Filing Date
- 2024-05-23
- Publication Date
- 2024-10-08
AI Technical Summary
During the traditional wire bonding process, the metal surface is easily oxidized, resulting in reduced bonding strength, increased resistance, and weakened adhesion. The oxides may cause the bonding wire to break, affecting manufacturing quality.
The copper surface on the semiconductor wafer is treated using a plasma jet in a low-oxygen environment, cleaning the surface oxide to attach bonding wires directly to the copper surface, eliminating the oxide layer and ensuring metal-to-metal contact.
It achieves metal-to-metal contact without an oxide interface, improves the adhesion and bonding strength of the bonding wire, reduces the resistance, enhances the stability and reliability of the bonding wire, avoids the formation of additional gold layers, and reduces process costs. .
Smart Images

Figure CN118748152A_ABST
Abstract
Description
Technical Field
[0001] Embodiments of the present invention relate to methods of forming bonded assemblies, and more particularly, to wire bonding using plasma processing. Background Art
[0002] Traditional wire bonding processes are limited by the formation of oxides on metal surfaces. Due to concerns about oxide formation, a NiAu / Electroless Nickel Electroless Palladium Immersion Gold (ENEPIG) surface treatment is now being promoted in bonding pads to provide Au / Ag / Cu wire bonding above them. Summary of the invention
[0003] An embodiment of the present invention provides a method for forming a bonding component, comprising providing a substrate and a semiconductor chip; disposing the semiconductor chip on the substrate; performing a plasma treatment process on a copper-containing surface of a chip bonding pad on the semiconductor chip in a low-oxygen environment, wherein the plasma treatment process is performed by directing a plasma jet to the chip bonding pad; and attaching a bonding wire to the semiconductor chip and the substrate, such that a first end of the bonding wire is attached to the copper-containing surface, and a second end of the bonding wire is attached to the substrate bonding pad on the substrate.
[0004] An embodiment of the present invention provides a method for forming a bonding component, comprising depositing a semiconductor chip on a substrate in a low oxygen environment, wherein the semiconductor chip includes a plurality of chip bonding pads, the low oxygen environment having an oxygen partial pressure of less than 17 kPa, wherein the chip bonding pads include electroplated copper material, and the electroplated copper material includes copper atoms with an atomic percentage ranging from 95% to 99.9999%; performing a plasma treatment process in the low oxygen environment by directing a plasma jet to a first chip bonding pad selected from the chip bonding pads; bonding a first end of a bonding wire to the first chip bonding pad; and bonding a second end of the bonding wire to a substrate bonding pad on the substrate.
[0005] An embodiment of the present invention provides a method for forming a bonding component, comprising placing a semiconductor chip on a substrate in a low-oxygen environment, the low-oxygen environment having an oxygen partial pressure of less than 17 kPa, wherein the semiconductor chip includes a chip bonding pad having a copper-containing surface; performing a plasma treatment process by directing a plasma jet to the copper-containing surface in the low-oxygen environment; attaching a first end of a bonding wire to the copper-containing surface of the chip bonding pad via a metal ball, the metal ball and the bonding wire having the same material composition; and attaching a second end of the bonding wire to a substrate bonding pad of the substrate via a pin. BRIEF DESCRIPTION OF THE DRAWINGS
[0006] The embodiments of the present invention are best understood by the following detailed description in conjunction with the accompanying drawings. It should be noted that, in accordance with standard practice in the industry, various features are not drawn to scale and are for illustration purposes only. In fact, the sizes of various components may be arbitrarily enlarged or reduced to clearly illustrate the features of the embodiments of the present invention.
[0007] Figure 1A FIG. 4 is a schematic vertical cross-sectional view of a first exemplary semiconductor wafer including at least one semiconductor die and an interposer according to an embodiment of the present invention.
[0008] Figure 1B FIG. 4 is a schematic vertical cross-sectional view of a second exemplary semiconductor wafer composed of a single semiconductor die according to an embodiment of the present invention.
[0009] Figure 2 FIG. 4 is a vertical cross-sectional view of an exemplary bonding apparatus before bonding a bonding wire to a semiconductor wafer or substrate according to an embodiment of the present invention.
[0010] Figure 3 FIG. 4 is a vertical cross-sectional view of an exemplary bonding apparatus after bonding wires to wafer bonding pads according to an embodiment of the present invention.
[0011] Figure 4 FIG. 4 is a vertical cross-sectional view of an exemplary bonding apparatus after bonding a bonding wire to a substrate bonding pad according to an embodiment of the present invention.
[0012] Figure 5A FIG. 4 is a vertical cross-sectional view of an exemplary bonding apparatus for bonding a semiconductor wafer and a substrate according to an embodiment of the present invention.
[0013] Figure 5B According to an embodiment of the present invention, Figure 5A A top view schematic diagram of a joining assembly.
[0014] Figure 6 FIG. 4 is a first schematic flow chart illustrating steps of forming a bonding assembly according to an embodiment of the present invention.
[0015] Figure 7 FIG. 4 is a second schematic flow chart illustrating steps of forming a bonding assembly according to an embodiment of the present invention.
[0016] Figure 8 FIG. 4 is a third schematic flow chart illustrating steps of forming a bonding assembly according to an embodiment of the present invention.
[0017] The reference numerals are described as follows:
[0018] 10: Platform
[0019] 20: Substrate
[0020] 28: Substrate bonding pad
[0021] 29: Low oxygen environment
[0022] 30: Adhesive layer
[0023] 31: Chamber housing
[0024] 32: First Gate
[0025] 34: The Second Door
[0026] 40: Semiconductor chips
[0027] 48: Chip bonding pad
[0028] 60: Plasma treatment system
[0029] 61: Plasma nozzle
[0030] 70: Bonding line
[0031] 71: Free Air Balloon
[0032] 72: Sphere
[0033] 73: Pin
[0034] 76: Bonding capillary
[0035] 300: Intermediary
[0036] 360: Re-distribution of dielectric layers
[0037] 380: Rerouting Metal Interconnects
[0038] 388: Bump structure on interposer
[0039] 400: Process controller
[0040] 610, 620: Steps
[0041] 630, 640: Steps
[0042] 700: Semiconductor grains
[0043] 710, 720: Steps
[0044] 730, 740: Steps
[0045] 760: Molding Compound Matrix
[0046] 788: Bump structure on die
[0047] 792: Bottom filling material part
[0048] 810, 820: Steps
[0049] 830, 840: Steps
[0050] 990: Welding materials section
[0051] P: Plasma jet DETAILED DESCRIPTION
[0052] The following disclosure provides many embodiments or examples for implementing different elements of the subject matter provided. Specific examples of each element and its configuration are described below to simplify the description of the embodiments of the present invention. Of course, these are merely examples and are not intended to limit the embodiments of the present invention. For example, if the description mentions that a first element is formed on a second element, it may include an embodiment in which the first and second elements are in direct contact, and it may also include an embodiment in which an additional element is formed between the first and second elements so that they are not in direct contact. In addition, the embodiments of the present invention may repeat reference values and / or letters in various examples. Such repetition is for the purpose of simplicity and clarity, rather than for indicating the relationship between the different embodiments and / or configurations discussed.
[0053] Furthermore, spatially relative terms may be used, such as "under", "below", "lower", "above", "higher" and the like, to facilitate the description of the relationship between one (or some) parts or features and another (or some) parts or features in the drawings. Spatially relative terms are used to include different orientations of the device in use or operation, as well as the orientations described in the drawings. When the device is turned to a different orientation (rotated 90 degrees or other orientations), the spatially relative adjectives used therein will also be interpreted according to the orientation after the rotation. Unless otherwise expressly stated, each element with the same reference number is assumed to have the same material composition and have a thickness within the same thickness range.
[0054] Bonding a semiconductor wafer to a substrate is a critical step in manufacturing electronic devices because it ensures that the semiconductor wafer is properly connected to the substrate and functions as intended during use. Many semiconductor wafers use metal pads that are primarily composed of copper. However, the copper surface is easily oxidized, that is, a surface copper oxide layer is formed. Copper oxide is a compound that forms on the copper surface exposed to air or other oxidants. The presence of copper oxide on the copper pad may seriously reduce the adhesion and contact resistance of the stitch. Therefore, due to the presence of interfacial copper oxide, the bond between the copper pad and the stitch is usually electrically and structurally unreliable. Although surface cleaning methods can be used to temporarily remove copper oxide, additional copper oxide may still be easily grown before bonding wires to the copper pad. Therefore, the use of gold plating on the top surface of the copper pad has become a popular method for achieving reliable electrical contact in the semiconductor industry because the gold surface is not affected by oxidation.
[0055] Wire bonding is a commonly used process in semiconductor manufacturing, which is used to connect bonding wires to metal pads on semiconductor devices to form electrical connections. However, during the wire bonding process, oxides may be formed. The formation of such oxides may cause many problems. These problems may include: poor bonding strength; increased resistance, reduced bonding wire adhesion, and wire breakage. For example, oxides formed on metal pads may create barriers between bonding wires and metal pads. Such barriers may reduce the strength of the bond and may cause connection failure or device failure. Oxides may increase the resistance of the bond and may ultimately reduce the performance of the device. Oxides may also reduce the ability of bonding wires to adhere to metal pads. This may result in poor bonding wire placement and poor stability. In some embodiments, oxides may cause bonding wires to break during the bonding process. This in turn may result in manufacturing defects.
[0056] According to an embodiment of the present invention, an atmospheric pressure plasma jet (APPJ) process may be performed in-situ to clean surface contaminants from a bonding structure before and during bonding a bonding wire to a copper surface of a copper-based bonding pad. Thus, by using an in-situ APPJ cleaning process and a wire bonding process, a semiconductor wafer including a copper pad may be bonded to a substrate without forming any additional metal layer such as a gold layer. Various aspects of the present disclosure are now described with reference to the accompanying drawings.
[0057] See also Figure 1A According to an embodiment of the present invention, a first exemplary semiconductor wafer 40 is used, which can be subsequently used to form a bonded assembly of the semiconductor wafer 40 and a substrate. The first exemplary semiconductor wafer 40 can be a composite wafer, which includes an assembly of at least one semiconductor die 700 and an interposer 300, wherein the interposer 300 includes redistributed metal interconnects 380 embedded in a redistributed dielectric layer 360.
[0058] The RDL 360 includes a corresponding dielectric polymer material, such as polyimide (PI), benzocyclobutene (BCB), or polybenzo Each redistributed dielectric layer 360 may be formed by spin coating and drying a corresponding dielectric polymer material. The thickness of each redistributed dielectric layer 360 may range from 2 microns to 40 microns, such as 4 microns to 20 microns.
[0059] Each redistribution metal interconnect 380 may include a metal seed layer and a corresponding stack of electroplated metal filling materials (such as copper, nickel, or a stack of copper and nickel). The metal seed layer may include, for example, a stack of a titanium barrier layer and a copper seed layer. The titanium barrier layer may have a thickness in the range of 50nm to 300nm, and the copper seed layer may have a thickness in the range of 100nm to 500nm. The metal filling material used for the redistribution metal interconnect 380 may include copper, nickel, or copper and nickel. The thickness of each line portion of the redistribution metal interconnect 380 may range from 2 microns to 40 microns, such as 4 microns to 10 microns, but smaller or larger thicknesses may also be used. The total number of layers of wiring in the interposer 300 may range from 1 to 10.
[0060] The interposer 300 may include an on-interposer bump structure 388 for attaching at least one semiconductor die 700. The metal material of the on-interposer bump structure 388 may include copper. Other metal materials are also within the scope of consideration of the present disclosure. The on-interposer bump structure 388 may have a rectangular, rounded rectangular, or circular horizontal cross-sectional shape. Other horizontal cross-sectional shapes may be within the scope of consideration of the present disclosure. Generally speaking, the on-interposer bump structure 388 may be configured for micro-bump bonding and may have a thickness ranging from 10 microns to 100 microns, but a smaller or larger thickness may also be used. In such an embodiment, the on-interposer bump structure 388 may be formed as an array of micro-bumps (such as copper pillars) having a lateral dimension ranging from 10 microns to 50 microns and a pitch ranging from 20 microns to 100 microns.
[0061] The aforementioned at least one semiconductor die 700 may include any combination of semiconductor die known in the technical field to which the present invention belongs. In one embodiment, each of the aforementioned at least one semiconductor die 700 may include at least one system-on-chip (SoC) die and / or at least one memory die. Optionally, the aforementioned at least one semiconductor die 700 may include at least one surface mount die known in the technical field to which the present invention belongs. Each SoC die may include an application processor die, a central processing unit (CPU) die, or a graphic processing unit (GPU) die. In one embodiment, the aforementioned at least one memory die may include a high bandwidth memory (HBM) die, which includes a vertical stack of static random access memory (SRAM) die. In one embodiment, the aforementioned at least one semiconductor die 700 may include at least one system-on-chip (SoC) die and at least one high bandwidth memory (HBM) die. Each HBM die may include a vertical stack of static random access memory (SRAM) dies interconnected with each other by an array of micro-bumps and laterally surrounded by a corresponding molding material packaging frame.
[0062] Each semiconductor die 700 may include a corresponding array of on-die bump structures 788. Each array of on-die bump structures 788 may be bonded to the array of on-interposer bump structures 388 via a corresponding array of solder material portions 990. An underfill material portion 792 may laterally surround the array of solder material portions 990. A molding compound matrix 760 may laterally surround the underfill material portion 792 and at least one semiconductor die 700.
[0063] See also Figure 1A, the semiconductor chip 40 of the first embodiment may include a chip bonding pad 48. In one embodiment, the chip bonding pad 48 may be located on the redistribution dielectric layer 360 so that the surface of the chip bonding pad 48 is physically exposed. In one embodiment, the chip bonding pad 48 may include a film layer stack, which includes a metal seed layer and electroplated copper. The metal seed layer may include, for example, a stack of a titanium barrier layer and a copper seed layer. The titanium barrier layer may have a thickness in the range of 50nm to 300nm, and the copper seed layer may have a thickness in the range of 100nm to 500nm. The electroplated copper contains an atomic percentage of copper in the range of 95% to 99.9999%. The thickness of the electroplated copper material may range from 4 microns to 30 microns, such as 6 microns to 20 microns, but smaller or larger thicknesses may also be used.
[0064] See also Figure 1B , the semiconductor wafer 40 of the second embodiment is used, which is composed of semiconductor grains 700. The semiconductor grains can be Figure 1A Any of the semiconductor dies 700 discussed. A wafer bonding pad 48 may be provided directly above the semiconductor die 700 (with Figure 1A In general, the chip bonding pad 48 of the semiconductor die 700 may have the same structure as that of the redistribution dielectric layer 360 of the interposer 300 shown in FIG. Figure 1A The wafer bonding pad 48 may have the same material composition and the same thickness range as discussed above. In one embodiment, the wafer bonding pad 48 may include a film layer stack including a metal seed layer and electroplated copper. The metal seed layer may include, for example, a stack of a titanium barrier layer and a copper seed layer. The titanium barrier layer may have a thickness in the range of 50nm to 300nm, and the copper seed layer may have a thickness in the range of 100nm to 500nm. The electroplated copper includes copper in an atomic percentage range of 95% to 99.9999%. The thickness of the electroplated copper material may range from 4 microns to 30 microns, such as 6 microns to 20 microns, but lesser or greater thicknesses may also be used.
[0065] See also Figure 2, depicting an embodiment of a bonding device. An embodiment of this bonding device includes a process chamber (31, 32, 34), which includes a chamber housing 31 and an environmental control system, which is configured to provide a low oxygen environment 29 within a volume spatially defined by the chamber housing 31. As used herein, "low pressure environment" refers to an environment in which the oxygen partial pressure is lower than the oxygen partial pressure under standard atmospheric conditions (about 21.23 kPa). In one embodiment, the low oxygen environment 29 may have an oxygen partial pressure that is lower than about 80% of the oxygen partial pressure under standard atmospheric conditions, such as less than 17 kPa. The total pressure of the low oxygen environment 29 may range from 10 Pa to 120 kPa. The atmospheric pressure under standard atmospheric conditions is 101.33 kPa. In one embodiment, the oxygen partial pressure in the low oxygen environment 29 may range from 1.0×10 -6 In general, the low oxygen partial pressure in the hypoxic environment 29 can be provided by reducing the total pressure of the hypoxic environment 29 and / or by reducing the oxygen fraction in the composition of the ambient gas in the hypoxic environment 29. In one embodiment, the molecular fraction of oxygen in the hypoxic environment 29 can range from 1.0×10 -9 To 0.2095 (which is the fraction of oxygen atoms in normal atmospheric composition). Suitable mechanisms (not explicitly shown) such as ambient gas supply nozzles, exhaust ports, and / or vacuum pump ports may be provided as needed to maintain the composition and pressure of the hypoxic environment 29 at a predetermined level.
[0066] The chamber housing 31 may include a first opening and a second opening. A first door 32 may be provided at the first opening, which is provided in a manner that seals the volume enclosed by the chamber housing 31. A second door 34 may be provided at the second opening, which is provided in a manner that seals the volume enclosed by the chamber housing 31. Suitable door actuation mechanisms may be provided for the first door 32 and the second door 34 so that the first door 32 and the second door 34 can be opened and closed to provide transportation of semiconductor packages and package substrates in and out of the chamber housing 31. Although the present disclosure is described using an embodiment in which the first door 32 and the second door 34 are located on both sides of the low oxygen environment, the present disclosure explicitly contemplates embodiments in which the first door 32 and the second door 34 are arranged in different ways, or are combined into one door.
[0067] A plasma processing system 60 is provided within a process chamber (31, 32, 34). The plasma processing system 60 is configured to generate a plasma jet P. The plasma processing system 60 includes a plasma nozzle 61, which is configured to generate a corresponding atmospheric pressure plasma jet P containing ions of a reducing gas (i.e., a gas that can combine with oxygen atoms to deoxidize the surface). The plasma nozzle 61 of the plasma processing system 60 can be configured so that the plasma jet P is directed toward a wafer bonding pad 48 formed on a semiconductor wafer 40. The direction of the plasma jet P of the plasma processing system 60 may or may not be tilted relative to the vertical direction, and may be tilted relative to the horizontal direction. The tilt angle of the direction of each plasma jet P relative to the vertical direction can generally range from 0 degrees to +85 degrees, such as 15 degrees to 60 degrees, but smaller and larger tilt angles can also be used. In general, the tilt angle can be a fixed angle or an in-situ controllable variable angle.
[0068] The platform 10 is provided in a process chamber (31, 32, 34). The platform 10 is configured to mount a substrate thereon. The substrate may be a package substrate, a leadframe, or a wafer including an array of semiconductor dies. The platform 10 may include a moving mechanism configured to provide lateral movement and / or vertical movement for the platform 10.
[0069] A bonding capillary 76 containing a bonding wire 70 may be provided within the process chamber (31, 32, 34). The bonding capillary 76 may be a commercially available bonding capillary. The bonding wire 70 may be made of a highly conductive metal such as gold, silver, or aluminum. In one embodiment, the bonding wire 70 may be a gold wire having a diameter in the range of 15 microns to 75 microns (such as 30 microns to 50 microns), although smaller and larger diameters may also be used.
[0070] A free air ball 71 may be provided at the bottom end of the bonding wire 70. The free air ball 71 may be formed by applying heat and / or ultrasonic energy to the bottom end of the bonding wire 70 and by locally melting the material of the bonding wire 70. The free air ball 71 comprises the same material as the bonding wire 70 and does not comprise any welding material. The free air ball 71 may be formed without any spatial restrictions, i.e., in "free air", and without contacting any welding surface other than the remainder of the bonding wire 70.
[0071] The substrate 20 may be loaded into the process chamber (31, 32, 34). The substrate 20 may include any structure to which the semiconductor chip 40 may be attached by wire bonding. In one embodiment, the substrate 20 may include a package substrate, a lead frame, or a wafer including a two-dimensional array of semiconductor dies that may then be cut along cutting channels.
[0072] The "packaging substrate" of the present disclosure refers to any substrate to which a semiconductor chip can be attached so that the semiconductor chip can be attached to a printed circuit board (PCB) through the substrate. Examples of the packaging substrate include an organic packaging substrate, a ceramic packaging substrate, an elastic packaging substrate, a multi-core packaging substrate, a glass packaging substrate, a silicon packaging substrate, etc.
[0073] "Lead frame" as used herein refers to a thin metal frame that provides a structural basis for mounting and interconnecting semiconductor devices, such as integrated circuits (ICs) and light-emitting diodes (LEDs). A lead frame typically comprises a flat metal strip, typically formed of copper or a copper alloy, and having a number of leads or pins arranged in a pattern. The bonding wires or pins of the lead frame provide electrical connections between the semiconductor device and external electrical components, such as a printed circuit board. The lead frame also provides a means of mechanical support and protection for the device, as it can be encapsulated in a plastic or ceramic package to protect the semiconductor chip 40 and the components of the lead frame from external environmental factors, such as moisture, dust, and mechanical shock.
[0074] In embodiments where substrate 20 includes an array of semiconductor dies (eg, semiconductor dies 700 ) within a wafer such as a semiconductor die, each semiconductor die 40 may be bonded to a respective semiconductor die 700 within the wafer.
[0075] Substrate 20 includes an array of bonding pads, which are referred to in this disclosure as an array of substrate bonding pads 28. In one embodiment, each substrate bonding pad 28 may include a film layer stack of multiple metal layers including a gold layer as a topmost layer.
[0076] In the illustrated example, each substrate bonding pad 28 can include a NiAu (nickel-gold) layer stack. The NiAu stack includes a nickel layer, which can be deposited directly above the metal surface below (such as a copper surface) and used as a seed layer, diffusion barrier layer, and adhesion promoting layer for the gold layer that will be deposited thereon later. The gold layer can be deposited above or directly above the nickel layer and used as the final layer for wire bonding. The gold layer provides excellent mechanical and electrical properties and has strong oxidation and corrosion resistance. Generally speaking, the gold layer does not include a surface oxide layer, which is conducive to wire bonding. The gold layer provides a smooth, low-resistance surface that is suitable for making strong and reliable wire bonding. The nickel layer is covered and protected by the gold layer and therefore does not interact with the environment.
[0077] In another illustrative example, each substrate bonding pad 28 may include an Electroless Nickel Electroless Palladium Immersion Gold (ENEPIG) stack. The ENEPIG stack includes an electroless nickel layer that can be deposited directly above the underlying metal surface (such as a copper surface) and serves as a seed layer, diffusion barrier layer, and adhesion promoting layer for subsequently deposited film layers. The electroless palladium layer is an intermediate layer used to enhance the adhesion of the subsequent gold layer and enhance the corrosion resistance of the final surface. The immersion gold layer forms a thin, corrosion-resistant gold layer that is suitable for wire bonding and protects the underlying metal layer. The ENEPIG stack provides a surface treatment suitable for wire bonding and also provides high reliability and good corrosion resistance.
[0078] The semiconductor wafer 40 may be disposed above the substrate 20. The semiconductor wafer 40 may include Figure 1A as well as Figure 1B Any semiconductor wafer 40 discussed. The semiconductor wafer 40 may optionally be secured to the top surface of the substrate 20 using an adhesive layer 30. Generally, the semiconductor wafer 40 may be aligned over the substrate 20 such that the wafer bonding pads 48 and the substrate bonding pads 28 are physically exposed to the low oxygen environment 29.
[0079] Generally, a low oxygen environment 29 with an oxygen partial pressure of less than 17 kPa is provided in a process chamber having a chamber housing 31. A substrate 20 including a substrate bonding pad 28 and a semiconductor wafer 40 including a wafer bonding pad 48 can be provided in the low oxygen environment 29, for example, by loading into the process chamber. The semiconductor wafer 40 is disposed on the substrate 20 such that the wafer bonding pad 48 and the substrate bonding pad 28 are exposed to the low oxygen environment 29.
[0080] In one embodiment, semiconductor chip 40 may include a composite chip including at least one semiconductor die 700 and an interposer 300 component, interposer 300 including redistributed metal interconnects 380 embedded in a redistributed dielectric layer 360 , and chip bonding pads 48 may be located on the redistributed dielectric layer 360 .
[0081] In one embodiment, the wafer bonding pad 48 may have a copper-containing surface as a bonding surface. In one embodiment, the wafer bonding pad 48 may include an electroplated copper material containing copper atoms in an atomic percentage range of 95% to 99.9999%. The copper-containing surface may be a surface of the electroplated copper material.
[0082] In one embodiment, the substrate 20 may be one of a package substrate, a lead frame, and a wafer containing a two-dimensional array of semiconductor dies. In one embodiment, each substrate bonding pad 28 comprises a film layer stack of multiple metal layers, the metal layers comprising a gold layer as the topmost layer.
[0083] After semiconductor wafer 40 is disposed on substrate 20, a plasma treatment process can be performed in low oxygen environment 29 by directing a plasma jet P to at least one wafer bonding pad 48 selected from wafer bonding pads 48. According to one aspect of the present disclosure, wafer bonding pads 48 of semiconductor wafer 40 can be cleaned to remove surface oxides located on copper-containing surfaces of wafer bonding pads 48. Specifically, plasma treatment system 60 forms a reducing plasma (i.e., a de-oxidizing plasma) around wafer bonding pads 48 by generating a plasma jet P, i.e., an atmospheric pressure plasma jet (APPJ). In general, an atmospheric pressure plasma jet (APPJ) can be generated by passing a gas (such as air, argon, or helium) through a high voltage discharge. The generated plasma consists of highly reactive species, such as ions and radicals, which can be used in various industrial and research applications.
[0084] APPJ treatment is a process used in semiconductor manufacturing to clean, activate, and treat surfaces. APPJ uses low-temperature plasma generated at atmospheric pressure to change the surface chemistry of materials. Plasma is a state of matter that occurs when a gas is dissociated, or when its atoms are stripped of some of their electrons, producing a mixture of ions, electrons, and neutrons. Plasma can be generated at a variety of pressures, including atmospheric pressure.
[0085] APPJ systems typically include a plasma generator, a gas supply system, and a nozzle that directs the plasma onto the surface to be treated. Plasma can be generated by introducing a gas such as argon or oxygen into the plasma generator, where the gas is electrically discharged. The plasma generator can produce the plasma, which is then directed through the nozzle onto the surface to be treated. APPJ can be a non-contact, low temperature, and low pressure process, which makes APPJ compatible with a wide range of materials and can be easily integrated into existing semiconductor manufacturing processes.
[0086] The high-energy plasma generated by the APPJ system can remove contaminants and particles from the surface, providing a clean surface for subsequent process steps. Plasma can change the surface chemistry of materials, increase the reactivity of materials, and make materials more suitable for subsequent process steps. Plasma can also be used to deposit thin films or change the surface morphology of materials. Plasma can be used to remove or passivate surface oxides and other unwanted surface films. Plasma can also be used to change the surface energy of materials to improve the adhesion of subsequent film layers.
[0087] According to one aspect of the present disclosure, the plasma jets P from the plasma processing system 60 are used for surface cleaning. Specifically, the ions in each plasma jet P can be directed toward the wafer bonding pad 48 to clean the surface of the wafer bonding pad 48. The energetic species in the plasma interact with the surface, thereby decomposing and removing contaminants on the wafer bonding pad 48. In one embodiment, each plasma jet P uses ions of a reducing gas to reduce and / or remove contaminants (such as oxygen or water vapor) on the surface of the wafer bonding pad 48. The reducing gas is mixed with the corresponding plasma jet P, and the generated active species are directed toward the surface to be cleaned, effectively reducing and removing contaminants on the surface.
[0088] The reducing gas that can be used for each plasma jet P from the plasma processing system 60 may include, but is not limited to, hydrogen, various hydride gases (such as methane, ammonia, acetylene, etc.), carbon monoxide, and various volatile compounds containing hydrogen radicals. Hydrogen is a strong reducing agent that can be used to remove oxides, sulfates, and other contaminants on the surface. Methane is a hydrocarbon gas that can be used to remove carbon-based contaminants on the surface. Ammonia is a weak reducing agent that can be used to remove nitrides and other nitrogen-based contaminants on the surface. Carbon dioxide can be used to remove organic contaminants on the surface. Nitrogen can be used to remove oxygen-based contaminants. Propane is a hydrocarbon gas that can be used to remove carbon-based contaminants on the surface. In some other embodiments, non-reducing gases, such as argon and helium, can be optionally used to cool the plasma and / or protect the plasma jet and improve plasma characteristics. In general, any ion that is a reducing agent can be used. Each atmospheric pressure plasma jet generated by the plasma processing system 60 does not need to be at an atmospheric pressure, but can be any pressure that can be used to generate atmospheric pressure plasma jets known in the art. Generally speaking, the plasma processing process can be performed in a low oxygen environment 29, which has an oxygen partial pressure of less than 17 kPa.
[0089] A process controller 400 may be provided, which includes a processor and a memory in communication with the processor. The process controller 400 may be loaded with a program that controls the loading and positioning of the semiconductor wafer 40 and the substrate 20, and / or controls the direction, area coverage, duration, and / or intensity of the plasma jet P generated by the plasma processing system 60. Surface oxides may be removed from the copper-containing surfaces of the wafer bonding pads 48.
[0090] The plasma treatment process can be performed on the copper-containing surface of at least one wafer bonding pad 48 (including, for example, the first wafer bonding pad 48) on the semiconductor wafer 40 in the low oxygen environment 29 by directing a plasma jet P toward the wafer bonding pad 48. The plasma jet P can be generated by a plasma treatment system 60 having a plasma nozzle 61 directed toward the wafer bonding pad 48. In one embodiment, the plasma nozzle 61 is directed toward the copper-containing surface in a downward non-horizontal direction, and the copper-containing surface is directed in a horizontal direction during the plasma treatment process. The plasma jet P can simultaneously clean one of the wafer bonding pads 48 (referred to as the first wafer bonding pad 48 in the present disclosure) and one of the substrate bonding pads 28 (referred to as the first substrate bonding pad 28 in the present disclosure).
[0091] See also Figure 3 , the free air ball 71 of the bonding wire 70 is attached to the wafer bonding pad 48 (such as the first wafer bonding pad 48) to provide metal-to-metal contact. For example, the bonding capillary 76 can be moved to a position directly above the first wafer bonding pad 48. The bonding wire 70 can be pulled downwardly through the bonding capillary 76 to the first wafer bonding pad 48. As the bonding wire 70 is pulled downwardly, the bonding capillary 76 can shape the bonding wire 70 into a ring and press the free air ball 71 onto the cleaned copper surface of the first wafer bonding pad 48. The free air ball 71 solidifies after contacting the copper surface of the first wafer bonding pad 48 to provide a metal-to-metal interface without an oxide interface between the electroplated copper material in the first wafer bonding pad 48 and the material (such as gold) of the free air ball 71 that is currently solidified. After being attached to the first wafer bonding pad 48, the free air ball 71 becomes a metal ball, which is referred to as a sphere 72 in the present disclosure. The sphere 72 can have the same material composition as the bonding wire 70.
[0092] According to one aspect of the present disclosure, the ball 72 can be attached to the first wafer bonding pad 48 when a plasma treatment process is performed on the first wafer bonding pad 48 by directing a plasma jet P to the copper-containing surface of the first wafer bonding pad 48 in the low oxygen environment 29. The first end of the bonding wire 70 can be attached to the copper-containing surface of the first wafer bonding pad 48 through the ball 72. Therefore, during the plasma treatment process, the first end of the bonding wire 70 is bonded to the first wafer bonding pad 48.
[0093] It should be understood that the shape and length of the bonding wire 70 may change during the bonding process. To the extent that the shape and length of the bonding wire 70 change during the process, the bonding wire 70 may also be referred to as an in-process bonding wire 70, i.e., a bonding wire that changes during the process. Generally, a first end of the in-process bonding wire 70 may be attached to a copper-containing surface of the wafer bonding pad 48, and a portion of the in-process bonding wire 70 may subsequently be attached to a surface of the substrate bonding pad 28.
[0094] In one embodiment, the die bonding pad 48 comprises an electroplated copper material containing 95% to 99.9999% copper atoms, and the copper-containing surface is a surface of the electroplated copper material. In one embodiment, the bonding wire 70 and the ball 72 consist essentially of gold.
[0095] Subsequently, the bonding capillary 76 can be moved over the substrate bonding pad 28 (such as the first substrate bonding pad 28) while allowing the bonding wire 70 to be pulled through the bonding capillary 76. The bonding wire 70 is pulled downward toward the substrate bonding pad 28, thereby forming a small indentation called a pin. The bonding capillary 76 shapes the bonding wire into a second ring shape, which is pressed onto the gold-containing surface of the first substrate bonding pad 28. The bonding capillary 76 then applies pressure and heat to the portion of the bonding wire 70 that contacts the first substrate bonding pad 28. The portion of the bonding wire 70 that contacts the surface of the first substrate bonding pad 28 is bonded to the top surface of the first substrate bonding pad 28 by pressure and heat. The temporary heat causes the pin portion of the bonding wire 70 to melt and re-solidify on the surface of the first substrate bonding pad 28, thereby forming a metal-to-metal contact without any oxide interface therebetween. In an embodiment where the bonding wire 70 includes gold, the metal-to-metal contact can be a gold-to-gold contact. According to an embodiment of the present invention, the bonding wire 70 can be bonded to the semiconductor wafer 40 and the substrate 20 during the plasma treatment process. In other words, when the bonding wire 70 is bonded to the first substrate bonding pad 28, the plasma jet P can impinge the surface of the first substrate bonding pad 28.
[0096] In one embodiment, the plasma nozzle 61 can be laterally offset from the edge of the bonding capillary 76 by a lateral offset distance greater than 1 mm when attaching the bonding wire 70 to the substrate 20 (i.e., attached to the substrate bonding pad 28 of the substrate 20); and the plasma nozzle 61 can be vertically offset from the horizontal plane including the top surface of the substrate 20 by a vertical offset distance greater than 0.1 mm when attaching the bonding wire 70 to the substrate 20.
[0097] See also Figure 4 , the portion of the bonding wire 70 remaining in the bonding capillary 76 may be severed from the portion of the bonding wire 70 connected to the first wafer bonding pad 48 and the first substrate bonding pad 28 .
[0098] In general, the bonding wire 70 is attached to the semiconductor wafer 40 and the substrate 20 by attaching a portion of the in-process bonding wire 70 to the copper-containing surface of the wafer bonding pad 48; by attaching a portion of the in-process bonding wire 70 to the surface of the substrate bonding pad 28; and by cutting the in-process bonding wire 70; so that the remaining portion of the in-process bonding wire 70 constitutes the bonding wire 70 extending between the copper-containing surface and the surface of the substrate bonding pad 28. Thus, a first end of the bonding wire 70 can be bonded to the wafer bonding pad 48, and a second end of the bonding wire 70 can be bonded to the substrate bonding pad 28 on the substrate 20. The bonding wire 70 can be attached to the copper-containing surface by a ball 72, which has the same material composition as the bonding wire 70. The bonding wire 70 can be attached to the surface of the electroplated copper material by a pin 73. The pin 73 is a shape or pattern of the bonding wire 70 to be bonded to the surface of the first substrate bonding pad 28. When the bonding wire 70 passes through the substrate bonding pad 28 of the substrate 20, the bonding wire 70 forms a loop or pattern, which is a stitch 73. The stitch 73 can have different shapes and geometries, and can be straight, curved, spherical, or zig-zag shaped. The size, shape, and position of the stitch 73 can be selected in a manner to increase the bonding strength, tensile strength, and resistance of the bonding wire 70.
[0099] According to one aspect of the present disclosure, the substrate 20 and the semiconductor wafer 40 can be located within the chamber housing 31 during the plasma treatment process and during the bonding wire 70 being attached to the semiconductor wafer 40 and the substrate 20. The plasma jet P can clean the copper-containing surface exposed by the wafer bonding pad 48 and the surface exposed by the substrate bonding pad 28 during the plasma cleaning process, and the plasma cleaning process can start before bonding the bonding wire 70 to the wafer bonding pad 48 and end after bonding the bonding wire 70 to the substrate bonding pad 28. The first end of the bonding wire 70 can be attached to the copper-containing surface of the wafer bonding pad 48 during the plasma treatment process, and the second end of the bonding wire 70 can be attached to the substrate bonding pad 28 during the plasma treatment process.
[0100] See also Figure 5A as well as Figure 5B , with reference to Figures 2 to 4 The described processing steps may be repeated for each pair of wafer bond pads 48 and substrate bond pads 28 to be electrically connected. The semiconductor wafer 40 may be electrically connected to the substrate 20 by wire bonding. Electrical testing may be performed to ensure that all electrical connections are properly made by wire bonding between the semiconductor wafer 40 and the substrate 20. Based on the results of the electrical testing, corrective action may be taken as needed, such as removal and replacement, and / or repair of defective bonds.
[0101] See also Figure 6 , Figure 6 FIG. 4 is a first schematic flow chart illustrating steps for forming a bonding assembly according to an embodiment of the present invention.
[0102] See step 610 and Figure 1A , Figure 1B as well as Figure 2 , the substrate 20 and the semiconductor wafer 40 may be provided in a low oxygen environment 29 with an oxygen partial pressure lower than 17 kPa.
[0103] See step 620 and Figure 2 , the semiconductor chip 40 can be disposed on the substrate 20 .
[0104] See step 630 and Figure 2 The copper-containing surface of the wafer bonding pad 48 on the semiconductor wafer 40 may be subjected to a plasma treatment process by directing a plasma jet P toward the wafer bonding pad 48 in the low oxygen environment 29 .
[0105] See step 640 and Figures 3 to 5B , a bonding wire 70 may be attached to the semiconductor wafer 40 and the substrate 20 such that a first end of the bonding wire 70 is attached to the copper-containing surface and a second end of the bonding wire 70 is attached to a substrate bonding pad 28 on the substrate 20 .
[0106] In one embodiment, the wafer bonding pad 48 may include an electroplated copper material containing copper atoms in the range of 95% to 99.9999% by atomic percentage; and the copper-containing surface may be a surface of the electroplated copper material. In one embodiment, the bonding wire 70 may be attached to the copper-containing surface by a ball 72 of a metal having the same material composition as the bonding wire 70; and the bonding wire 70 may be attached to the substrate bonding pad 28 by a pin 73 having the same material composition as the bonding wire 70. In one embodiment, the plasma jet P may be generated by a plasma treatment system 60 having a plasma nozzle 61, the plasma nozzle 61 being oriented toward the wafer bonding pad 48. In one embodiment, the plasma nozzle 61 may be oriented toward the copper-containing surface in a downward non-horizontal direction, while the copper-containing surface is oriented in a horizontal direction during the plasma treatment process. In one embodiment, the plasma nozzle 61 may be laterally offset from the edge of the bonding capillary 76 by a lateral offset distance greater than 1 mm when attaching the bonding wire 70 to the substrate 20; and the plasma nozzle 61 may be vertically offset from a horizontal plane including the top surface of the substrate 20 by a vertical offset distance greater than 0.1 mm when attaching the bonding wire 70 to the substrate 20. In one embodiment, the bonding wire 70 may be bonded to the semiconductor wafer 40 and the substrate 20 during the plasma treatment process. In one embodiment, the plasma jet P cleans the exposed surface of the substrate bonding pad 28 during the plasma cleaning process. In one embodiment, the semiconductor wafer 40 may include a composite wafer including an assembly of at least one semiconductor die 700 and an interposer 300, the interposer 300 including a redistributed metal interconnect 380 embedded in a redistributed dielectric layer 360; and the wafer bonding pad 48 is located on the redistributed dielectric layer 360. In one embodiment, the substrate 20 may be one of a package substrate, a lead frame, and a wafer including a two-dimensional array of semiconductor die. In one embodiment, substrate bonding pad 28 comprises a film layer stack of multiple metal layers, the metal layers comprising a gold layer as a topmost layer. In one embodiment, bonding wire 70 may be attached to semiconductor wafer 40 and substrate 20 by: attaching a first end of in-process bonding wire 70 to a copper-containing surface of wafer bonding pad 48; attaching a portion of in-process bonding wire 70 to a surface of substrate bonding pad 28; and truncating in-process bonding wire 70 such that the remaining portion of in-process bonding wire constitutes bonding wire 70 extending between the copper-containing surface and the surface of substrate bonding pad 28. In one embodiment, low oxygen environment 29 may be provided in a process chamber (31, 32, 34) having a chamber housing 31; and substrate 20 and semiconductor wafer 40 may be located within chamber housing 31 during the plasma treatment process and during attaching bonding wire 70 to semiconductor wafer 40 and substrate 20.
[0107] See also Figure 7 , Figure 7FIG. 4 is a second schematic flow chart illustrating steps for forming a bonding assembly according to an embodiment of the present invention.
[0108] See step 710 and Figure 1A , Figure 1B as well as Figure 2 The semiconductor wafer 40 including the wafer bonding pad 48 may be disposed on the substrate 20 in the low oxygen environment 29 with an oxygen partial pressure below 17 kPa. The wafer bonding pad 48 includes an electroplated copper material containing copper atoms in a range of 95 atomic % to 99.9999 atomic % .
[0109] See step 720 and Figure 2 The plasma treatment process may be performed in the low oxygen environment 29 by directing the plasma jet P to a first wafer bonding pad 48 selected from the wafer bonding pads 48 .
[0110] See step 730 and Figure 3 , a first end of the bonding wire 70 is bonded to the first chip bonding pad 48 .
[0111] See step 740 and Figures 3 to 5B , the second end of the bonding wire 70 is bonded to the substrate bonding pad 28 on the substrate 20 .
[0112] In one embodiment, the bonding wire 70 may be attached to the surface of the electroplated copper material through a metal ball 72; and the bonding wire 70 may be attached to the substrate bonding pad 28 through a pin 73. In one embodiment, the first end of the bonding wire 70 may be bonded to the first wafer bonding pad 48 during the plasma treatment process. In one embodiment, the semiconductor wafer 40 may include a composite wafer including at least one semiconductor die 700 and an interposer 300 component, the interposer 300 including a redistribution metal interconnect 380 embedded in a redistribution dielectric layer 360; and the wafer bonding pad 48 is located on the redistribution dielectric layer 360.
[0113] See also Figure 8 , Figure 8 FIG. 4 is a third schematic flow chart illustrating steps for forming a bonding assembly according to an embodiment of the present invention.
[0114] See step 810 and Figure 1A , Figure 1B as well as Figure 2 , a semiconductor wafer 40 is disposed on a substrate 20 in a low oxygen environment 29 having an oxygen partial pressure of less than 17 kPa. The semiconductor wafer 40 includes a wafer bonding pad 48 having a copper-containing surface.
[0115] See step 820 and Figure 2 , a plasma treatment process may be performed by directing a plasma jet P onto a copper-containing surface in a low oxygen environment 29 .
[0116] See step 830 and Figure 3 , a first end of the bonding wire 70 is bonded to the copper-containing surface of the wafer bonding pad 48 via a ball 72 of a metal having the same material composition as the bonding wire 70 .
[0117] See step 840 and Figures 3 to 5B The second end of the bonding wire 70 is connected to the substrate bonding pad 28 of the substrate 20 through the stitch 73 .
[0118] In one embodiment, the wafer bonding pad 48 may include an electroplated copper material containing copper atoms in a range of 95% to 99.9999% by atomic percentage; and the copper-containing surface may be a surface of the electroplated copper material. In one embodiment, during the plasma treatment process, a first end of the bonding wire 70 may be attached to the copper-containing surface of the wafer bonding pad 48; and during the plasma treatment process, a second end of the bonding wire 70 may be attached to the substrate bonding pad 28.
[0119] Various embodiments of the present disclosure provide for direct bonding of a bonding wire onto a plated copper portion in a bonding pad, thereby eliminating the need to form a gold layer on the plated copper portion prior to the bonding process. A plasma treatment process using an atmospheric pressure plasma jet (APPJ) provides for in-situ removal of copper oxide from the physically exposed surface of the plated copper portion, thereby ensuring the elimination of any surface oxide between the copper surface and the metal material of the bonding wire. Reliable wire bonding can be provided at a lower process cost.
[0120] An embodiment of the present invention provides a method for forming a bonding component, comprising providing a substrate and a semiconductor chip; placing the semiconductor chip on the substrate; performing a plasma treatment process on a copper-containing surface of a chip bonding pad on the semiconductor chip in a low-oxygen environment, wherein the plasma treatment process is performed by directing a plasma jet to the chip bonding pad; and attaching a bonding wire to the semiconductor chip and the substrate, such that a first end of the bonding wire is attached to the copper-containing surface, and a second end of the bonding wire is attached to the substrate bonding pad on the substrate.
[0121] In some embodiments, the wafer bonding pad comprises an electroplated copper material containing copper atoms in a range of 95% to 99.9999% atomic percentage; and the copper-containing surface is a surface of the electroplated copper material. In some embodiments, the bonding wire is attached to the copper-containing surface by a metal ball having the same material composition as the bonding wire; and the bonding wire is attached to the substrate bonding pad by a pin having the same material composition as the bonding wire. In some embodiments, the plasma jet is generated by a plasma processing system having a plasma nozzle, and the plasma nozzle is oriented toward the wafer bonding pad. In some embodiments, the plasma nozzle is oriented in a downward non-horizontal direction to the copper-containing surface, and the copper-containing surface is aligned in a horizontal direction during the plasma treatment process. In some embodiments, the plasma nozzle is laterally offset from the edge of the bonding capillary by a lateral offset distance greater than 1 mm when attaching the bonding wire to the substrate; and the plasma nozzle is vertically offset from a horizontal plane containing the top surface of the substrate by a vertical offset distance greater than 0.1 mm when attaching the bonding wire to the substrate. In some embodiments, the bonding wire is bonded to the semiconductor wafer and the substrate during the plasma treatment process. In some embodiments, the plasma jet cleans the exposed surface of the substrate bonding pad during the plasma treatment process. In some embodiments, the semiconductor wafer comprises a composite wafer, which is a component comprising at least one semiconductor die and an interposer, the interposer comprising a plurality of redistributed metal interconnects embedded in a plurality of redistributed dielectric layers; and a wafer bonding pad is located on the redistributed dielectric layers. In some embodiments, the substrate is one of a package substrate, a lead frame, and a wafer comprising a plurality of semiconductor die in a two-dimensional array. In some embodiments, the substrate bonding pad comprises a film layer stack of a plurality of metal layers, the metal layers comprising a gold layer as a topmost layer. In some embodiments, the bonding wire is attached to the semiconductor wafer and the substrate by: attaching a first end of the in-process bonding wire to a copper-containing surface of the wafer bonding pad; attaching a portion of the in-process bonding wire to a surface of the substrate bonding pad; and truncating the in-process bonding wire so that the remaining portion of the in-process bonding wire constitutes a bonding wire extending between the copper-containing surface and the surface of the substrate bonding pad. In some embodiments, the plasma treatment process is performed in a low oxygen environment having an oxygen partial pressure of less than 17 kPa; the low oxygen environment is provided in a process chamber having a chamber enclosure; and the substrate and the semiconductor wafer are located within the chamber enclosure during the plasma treatment process and during attaching bonding wires to the semiconductor wafer and the substrate.
[0122] An embodiment of the present invention provides a method for forming a bonding component, comprising depositing a semiconductor wafer on a substrate in a low oxygen environment, the semiconductor wafer comprising a plurality of wafer bonding pads, the low oxygen environment having an oxygen partial pressure of less than 17 kPa, wherein the wafer bonding pad comprises an electroplated copper material, the electroplated copper material comprising copper atoms in a range of 95% to 99.9999% atomic percentage; performing a plasma treatment process in the low oxygen environment by directing a plasma jet to a first wafer bonding pad selected from the wafer bonding pads; bonding a first end of a bonding wire to the first wafer bonding pad; and bonding a second end of the bonding wire to a substrate bonding pad on the substrate. In some embodiments, the bonding wire is attached to the surface of the electroplated copper material by a metal ball; and the bonding wire is attached to the substrate bonding pad by a pin. In some embodiments, the first end of the bonding wire is bonded to the first wafer bonding pad during the plasma treatment process. In some embodiments, the semiconductor wafer comprises a composite wafer, which is a component comprising at least one semiconductor die and an interposer, the interposer comprising a plurality of redistributed metal interconnects embedded in a plurality of redistributed dielectric layers; the wafer bonding pad is located on the redistributed dielectric layer.
[0123] An embodiment of the present invention provides a method for forming a bonding component, comprising placing a semiconductor chip on a substrate in a low oxygen environment, the low oxygen environment having an oxygen partial pressure of less than 17 kPa, wherein the semiconductor chip includes a chip bonding pad having a copper-containing surface; performing a plasma treatment process by directing a plasma jet to the copper-containing surface in the low oxygen environment; attaching a first end of a bonding wire to the copper-containing surface of the chip bonding pad through a metal ball, the metal ball having the same material composition as the bonding wire; and attaching a second end of the bonding wire to a substrate bonding pad of the substrate through a pin. In some embodiments, the chip bonding pad includes an electroplated copper material containing copper atoms in a range of 95% to 99.9999% atomic percentage; and the copper-containing surface is a surface of the electroplated copper material. In some embodiments, the first end of the bonding wire is attached to the copper-containing surface of the chip bonding pad during the plasma treatment process; and the second end of the bonding wire is attached to the substrate bonding pad during the plasma treatment process.
[0124] The features of several embodiments are summarized above so that those with ordinary knowledge in the technical field to which the present invention belongs can better understand the viewpoints of the embodiments of the present invention. Those with ordinary knowledge in the technical field to which the present invention belongs should understand that other processes and structures can be easily designed or modified based on the embodiments of the present invention to achieve the same purposes and / or advantages as the embodiments introduced herein. Those with ordinary knowledge in the technical field to which the present invention belongs should also understand that such equivalent structures do not deviate from the spirit and scope of the present invention, and various changes, substitutions, and replacements can be made without violating the spirit and scope of the present invention. Therefore, the scope of protection of the present invention shall be defined as defined by the appended claims.
Claims
1. A method for forming a joint assembly, comprising: Providing a substrate and a semiconductor chip; Disposing the semiconductor chip on the substrate; performing a plasma treatment process on a copper-containing surface of a wafer bonding pad on the semiconductor wafer in a low oxygen environment, the plasma treatment process being performed by directing a plasma jet toward the wafer bonding pad; as well as A bonding wire is attached to the semiconductor wafer and the substrate such that a first end of the bonding wire is attached to the copper-containing surface and a second end of the bonding wire is attached to a substrate bonding pad on the substrate.
2. The method for forming a joint assembly according to claim 1, wherein: The chip bonding pad includes an electroplated copper material containing copper atoms in a range of 95% to 99.9999% atomic percentage; and The copper-containing surface is the surface of the electroplated copper material.
3. The method for forming a joint assembly according to claim 1, wherein: The bonding wire is attached to the copper-containing surface via a metal ball having a same material composition as the bonding wire; as well as The bonding wire is attached to the substrate bonding pad via a stitch having the same material composition as the bonding wire. 4 . The method of forming a bonding component as claimed in claim 1 , wherein the plasma jet is generated by a plasma processing system having a plasma nozzle, and the plasma nozzle is directed toward the wafer bonding pad.
5. The method of forming a bonded component of claim 4, wherein the plasma nozzle is oriented toward the copper-containing surface along a downward non-horizontal direction, and the copper-containing surface is aligned along a horizontal direction during the plasma treatment process.
6. The method for forming a joint assembly according to claim 4, wherein: The plasma nozzle is laterally offset from an edge of a bonding capillary by a lateral offset distance greater than 1 mm when attaching the bond wire to the substrate; and The plasma nozzle is vertically offset by a vertical offset distance greater than 0.1 mm from a horizontal plane including a top surface of the substrate when attaching the bonding wire to the substrate.
7. The method for forming a joint assembly according to claim 1, wherein: The semiconductor wafer includes a composite wafer, which is a component including at least one semiconductor die and an interposer, the interposer including a plurality of redistributed metal interconnects embedded in a plurality of redistributed dielectric layers; and The chip bonding pad is located on the plurality of redistributed dielectric layers.
8. The method for forming a bonding assembly as claimed in claim 1, wherein the bonding wire is attached to the semiconductor wafer and the substrate by: attaching the first end of a process bond wire to the copper-containing surface of the wafer bond pad; attaching a portion of the in-process bond wire to a surface of the substrate bond pad; and The in-process bond wire is cut so that a remaining portion of the in-process bond wire constitutes the bond wire extending between the copper-containing surface and the surface of the substrate bond pad.
9. A method for forming a joint assembly, comprising: Depositing a semiconductor wafer on a substrate in a low oxygen environment, the semiconductor wafer including a plurality of wafer bonding pads, the low oxygen environment having an oxygen partial pressure of less than 17 kPa, wherein the plurality of wafer bonding pads include an electroplated copper material, the electroplated copper material including copper atoms in an atomic percentage ranging from 95% to 99.9999%; performing a plasma treatment process in the low oxygen environment by directing a plasma jet toward a first wafer bonding pad selected from the plurality of wafer bonding pads; bonding a first end of a bonding wire to the first chip bonding pad; and A second end of the bonding wire is bonded to a substrate bonding pad on the substrate.
10. A method of forming a joint assembly, comprising: Disposing a semiconductor wafer on a substrate in a low oxygen environment, the low oxygen environment having an oxygen partial pressure of less than 17 kPa, wherein the semiconductor wafer includes a wafer bonding pad having a copper-containing surface; performing a plasma treatment process by directing a plasma jet toward the copper-containing surface in the low oxygen environment; attaching a first end of a bonding wire to the copper-containing surface of the wafer bond pad via a metal ball, the metal ball having a same material composition as the bonding wire; and A second end of the bonding wire is attached to a substrate bonding pad of the substrate through a stitch.