Lithium battery pulse current heating method, system and equipment in low-temperature environment and medium
By establishing an electric-thermal-aging model in lithium batteries and using supercapacitors for pulse charging and discharging, and adjusting the frequency and amplitude according to different temperatures, the problems of low heating efficiency and safety hazards of lithium batteries in low-temperature environments are solved, and rapid, Energy-saving and efficient heating extends battery life and is suitable for a variety of application scenarios.
Patent Information
- Application Number
- CN202411078839.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-07
- Publication Date
- 2024-10-08
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
In a low-temperature environment, the impedance of lithium batteries increases, and the peak power and available capacity drop sharply, resulting in low battery performance and accelerated aging. Existing heating methods are inefficient and pose safety risks.
By establishing the electrical-thermal-aging model of lithium batteries, supercapacitors are used for pulse charging and discharging, and according to the optimal frequency and amplitude characteristics corresponding to different temperatures, the DC/DC circuit is controlled to change the pulse frequency and amplitude to achieve efficient heating.
It improves the heating rate and temperature uniformity, extends battery life, enhances system reliability and safety, and is suitable for a variety of scenarios such as electric vehicles in cold environments.
Smart Images

Figure CN118748290A_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the field of new energy lithium batteries, and specifically relates to a method, system, equipment and medium for pulse current heating of lithium batteries in a low temperature environment. Background Art
[0002] With the continuous development and expansion of new energy fields and markets, lithium batteries have become the core power source in this field, and the demand for lithium batteries has also shown an upward trend. Whether it is a pure electric vehicle, a hybrid vehicle, or a plug-in hybrid vehicle, it is inseparable from the strong power provided by lithium batteries. The high energy density of lithium batteries enables electric vehicles to have a longer range, and its long life characteristics reduce the frequency of battery replacement and reduce vehicle maintenance costs. However, in a low temperature environment, the impedance of lithium batteries increases, and the peak power and available capacity drop sharply, which will cause a series of problems such as low battery performance, battery aging and damage, low efficiency of new energy utilization, slow equipment startup and response. Therefore, in order to solve the problem of low-temperature performance degradation of power batteries, it is necessary to heat lithium batteries at low temperatures.
[0003] According to the location of the heat source applied to the battery, the current low-temperature heating strategy is mainly divided into two categories: external battery heating and internal battery heating. External heating generates thermal power through the heating element, thereby transferring heat to the battery. When using this method, more heat is consumed, resulting in lower energy utilization. Internal heating methods are divided into AC heating, DC heating and pulse heating. For example, Zhu Jinwen, Huang Liansheng, Chen Xiaojiao, et al. Capacitor-based low-temperature discharge self-heating method for lithium batteries [J]. Power Electronics Technology, 2023, 57(10): 77-79+84. Using AC heating, capacitor-based internal heating of lithium batteries, the capacitor is charged by exchanging two groups of batteries, and the current continuously flows through the internal resistance of the lithium battery to generate heat for low-temperature heating. However, the scheme does not analyze the changes in battery performance during the low-temperature heating of lithium batteries. Heating lithium batteries in a low-temperature environment will cause lithium deposition in lithium batteries, aggravate battery aging, and seriously affect battery life. At the same time, in order to avoid overcharging and over-discharging, the current amplitude needs to be limited, which will lead to low heating efficiency of the charging heating method and certain safety hazards. Summary of the invention
[0004] In order to overcome the defects of the above-mentioned prior art, the purpose of the present invention is to provide a method, system, equipment and medium for pulse current heating of lithium batteries in a low-temperature environment. The method uses a supercapacitor to charge and discharge the lithium battery, adopts different optimal frequency and optimal amplitude characteristics corresponding to different temperatures, and establishes a lithium battery electric-thermal-aging model to obtain battery temperature, aging and SOC information in real time, thereby controlling the DC / DC circuit to change the pulse frequency and amplitude and thus improve the heating rate. The method has the advantages of high heating rate, good temperature uniformity and simple system structure.
[0005] In order to achieve the above object, the technical solution adopted by the present invention is:
[0006] A method for pulse current heating of a lithium battery in a low temperature environment, specifically comprising the following steps:
[0007] Step 1: Establish a lithium battery electrical model;
[0008] Step 2: Establish a thermal model of lithium battery;
[0009] Step 3: Establish a lithium battery aging model to predict the capacity of the lithium battery in real time during the cycle use process;
[0010] Step 4: Couple the lithium battery electrical model, lithium battery thermal model and lithium battery aging model to establish an electrical-thermal-aging model of the lithium battery;
[0011] Step 5. Through the relevant parameters of the lithium battery electric-thermal-aging model: including the capacity loss Qloss, temperature and soc of the lithium battery, a pulse heating simulation of the lithium battery in a low temperature environment of -40° to -20° is performed to obtain the optimal pulse amplitude and pulse frequency corresponding to each temperature of the lithium battery in the low temperature environment, and formulate a pulse heating strategy that can suppress capacity attenuation in the low temperature environment.
[0012] The specific method of step 1 is: using EIS sweep frequency technology to obtain lithium battery impedance information in real time, and establishing a lithium battery electrical model based on a second-order RC equivalent circuit model; the lithium battery electrical model formula is as follows:
[0013]
[0014] Among them, U L is the terminal voltage of lithium battery, U OC is the open circuit voltage of the lithium battery, I is the current, R 0 is the ohmic resistance, R 1 , R 2 is the polarization resistance, C 1 , C 2 is the polarization capacitance, U 1 ,U 2 is the polarization voltage.
[0015] The specific method of step 2 is: according to the thermal balance mechanism of lithium battery, a thermal model of lithium battery is established, and the formula is as follows:
[0016]
[0017] Where Qt is the total heat generated, R is the ohmic resistance, R p is the polarization resistance, T is the lithium battery temperature, I is the current, U ocis the open circuit voltage, h is the convection heat transfer coefficient, s is the heat exchange area on the surface of the lithium battery, T a is the air temperature.
[0018] The specific method of step 3 is: real-time prediction of the capacity of the lithium battery during the cycle use process, combining the Arrhenius equation to establish a semi-empirical model of lithium battery capacity decline, and the lithium battery aging model is expressed as follows:
[0019]
[0020] Among them, a, b, c are parameters, Q cal is the capacity attenuation caused by calendar aging, Q cyc is the capacity decay caused by cycling, Ea represents the activation energy of the chemical reaction inside the lithium battery; R is the universal gas constant, and Ah represents the cumulative charge and discharge capacity during the charge and discharge period.
[0021] The specific method of step 4 is: coupling the lithium battery electrical model, the lithium battery thermal model and the lithium battery aging model to establish the lithium battery electrical-thermal-aging model:
[0022] The internal resistance of the lithium battery is obtained by EIS sweep frequency technology, and the formula is as follows:
[0023]
[0024] Where Z is the impedance of the lithium battery, R E is the real part of impedance, R I is the imaginary part of impedance, Isin(wt+α) is the AC current signal applied to the lithium battery, and Usin(wt+β) is the voltage signal generated by the lithium battery when stimulated;
[0025] The lithium battery electrical model transfers the internal resistance to the lithium battery thermal model to obtain the lithium battery temperature parameters. The lithium battery thermal model transfers the lithium battery temperature and the SOC parameters in the lithium battery electrical model to the lithium battery aging model to obtain the lithium battery capacity attenuation and lithium battery health information, and establishes the lithium battery electrical-thermal-aging model. The formula is as follows:
[0026]
[0027] Among them, Q is the initial capacity of the lithium battery, Qloss is the capacity decay during the heating process, and SOH is the health of the lithium battery.
[0028] The heating strategy in step 5 is:
[0029] Use the pulse module to perform pulse heating on the electric-thermal-aging model of the lithium battery established in step 4. By changing the charge and discharge direction, a pulse charge and discharge current is formed. The current continuously flows through the internal resistance to generate heat, thereby heating the battery. The battery pulse heating is calculated based on a°C step change. When a>0, the frequency and amplitude are changed for every a°C increase. The changed frequency and amplitude are the optimal pulse frequency and amplitude corresponding to the temperature after the a°C increase. Each step temperature has the optimal heating rate, thereby improving the overall heating efficiency.
[0030] A pulse current heating system for lithium batteries in a low temperature environment, comprising:
[0031] Coupling module: used to couple the lithium battery electrical model established in step 1, the lithium battery thermal model established in step 2, and the lithium battery aging model established in step 3, and establish the lithium battery electrical-thermal-aging model in step 4, which can simulate the charging and discharging behavior of the battery, accurately grasp the health status of the battery under different heating conditions and aging stages, and perform battery health detection and optimization;
[0032] Lithium battery pulse current heating strategy module: In step 5, the pulse module is used to generate pulse heating for the established lithium battery electric-thermal-aging model, change the charge and discharge direction, form a pulse charge and discharge current, and the current continuously flows through the internal resistance to generate heat to heat the battery. The calculation is based on a℃ step change, a>0, and the frequency and amplitude are changed for every a℃ increase. The changed frequency and amplitude are the optimal pulse frequency and amplitude corresponding to the temperature after the a℃ increase; each step temperature has the optimal heating rate, thereby improving the overall heating efficiency.
[0033] A lithium battery pulse current heating device in a low temperature environment, comprising:
[0034] Memory for storing computer programs;
[0035] The processor is used to implement the pulse current heating method for lithium batteries in a low temperature environment described in steps 1 to 5 when executing the computer program.
[0036] A computer-readable storage medium is used to store a computer program. When the computer program is executed by a processor, it can perform pulse charging and discharging on a lithium battery based on the pulse current heating method for a lithium battery in a low temperature environment described in any one of steps 1 to 5, and use different optimal frequencies and optimal amplitude characteristics corresponding to different temperatures to heat the lithium battery and improve the heating rate.
[0037] Compared with the prior art, the beneficial effects of the present invention are:
[0038] The low-temperature lithium battery pulse heating method designed by the present invention can simulate the charging and discharging behavior of the battery based on the lithium battery electric-thermal-aging model, grasp the health status of the battery under different working conditions and aging stages, and improve the reliability of the application; utilize an isolated bidirectional DC / DC circuit to charge and discharge the lithium battery through a supercapacitor to achieve pulse current heating; and achieve rapid heating by changing the pulse current amplitude and frequency.
[0039] 1. Battery health detection and optimization can be performed: Based on the lithium battery electric-thermal-aging model, it can simulate the battery's charging and discharging behavior and accurately grasp the battery's health status under different heating conditions and aging stages. This makes it possible to monitor the battery's status in real time and optimize its use and maintenance strategies, thereby improving the battery's reliability and life. By understanding the battery's health status in real time, it is possible to effectively prevent problems that may occur during battery use, such as overheating and capacity reduction. This preventive maintenance measure helps reduce the failure rate of the battery system and improve the overall reliability of the application.
[0040] 2. Pulse current parameter adjustment: By changing the amplitude and frequency of the pulse current, the heating effect can be flexibly adjusted to adapt to different working conditions and needs. This flexibility allows the technology to be applied in a variety of scenarios, such as electric vehicles in cold environments, drones and other application fields that require rapid response.
[0041] 3. Rapid heating and energy saving: Through the use of isolated bidirectional DC / DC circuits and supercapacitors, rapid pulse current heating of lithium batteries can be achieved. Compared with traditional heating methods, this method can increase the operating temperature of the battery more quickly, and can also more effectively control energy consumption and save electricity costs.
[0042] In summary, the present invention performs pulse charging and discharging on lithium batteries, adopts different optimal frequency and optimal amplitude characteristics corresponding to different temperatures, and establishes a lithium battery electric-thermal-aging model to obtain battery temperature, aging, SOC and other information in real time, thereby controlling the lithium battery circuit to change the pulse frequency and amplitude to increase the heating rate. The invention has the advantages of high heating rate, good temperature uniformity and simple system structure. BRIEF DESCRIPTION OF THE DRAWINGS
[0043] Figure 1 This is the isolated bidirectional DC / DC converter topology of the present invention.
[0044] Figure 2 This is the lithium battery electric-thermal-aging coupling model of the present invention.
[0045] Figure 3 This is the impedance sweep frequency technology of the present invention.
[0046] Figure 4 It is the optimization control strategy of the present invention.
[0047] Figure 5 It is a flow chart of the present invention.
[0048] The present invention is described in detail below with reference to the accompanying drawings and specific embodiments.
[0049] A method for pulse current heating of a lithium battery in a low temperature environment, specifically comprising the following steps:
[0050] Step 1: Establish the electrical model of lithium battery:
[0051] The EIS sweep frequency technology is used to obtain the impedance information of the lithium battery in real time. Based on the second-order RC equivalent circuit model, the lithium battery electrical model is established; this model can accurately characterize the nonlinear dynamic characteristics of the lithium battery. The formula is as follows:
[0052]
[0053] Among them, U L is the terminal voltage of lithium battery, U OC is the open circuit voltage of the lithium battery, I is the current, R 0 is the ohmic resistance, R 1 , R 2 is the polarization resistance, C 1 , C 2 is the polarization capacitance, U 1 ,U 2 is the polarization voltage; the lithium battery terminal voltage and SOC information can be obtained through the lithium battery electrical model;
[0054] Step 2: In the actual use of lithium batteries, electrical and thermal characteristics are inseparable. For example, the heat generated by lithium batteries increases, and the temperature rises, which will lead to accelerated lithium battery reactions and increased internal resistance, thus affecting its output. When the ambient temperature is high or low, the electrical and thermal coupling performance will be more significant.
[0055] According to the thermal balance mechanism of lithium batteries, a thermal model of lithium batteries is established, and the formula is as follows:
[0056]
[0057] Where Qt is the total heat generated, R is the ohmic resistance, R p is the polarization resistance, T is the lithium battery temperature, I is the current, U oc is the open circuit voltage, h is the convection heat transfer coefficient, s is the heat exchange area on the surface of the lithium battery, T a is the air temperature; by establishing a lithium battery thermal model, the change of heating temperature during the lithium battery heating process can be obtained;
[0058] Step 3: Establish a lithium battery aging model. The phenomenon that the capacity of lithium batteries gradually declines and the internal resistance gradually increases during use is called battery aging. In order to make real-time predictions of the capacity of lithium batteries during cyclic use, current research often combines the Arrhenius equation to establish a semi-empirical model of lithium battery capacity decline. The semi-empirical formula of the lithium battery aging model is expressed as follows:
[0059]
[0060] Among them, a, b, c are parameters, Q cal is the capacity attenuation caused by calendar aging, Q cyc is the capacity decay caused by cycling, Ea is the activation energy of the chemical reaction inside the lithium battery; R is the universal gas constant, which is 8.314; Ah is the cumulative charge and discharge capacity during the charge and discharge period.
[0061] Step 4: Establish the electrical-thermal-aging model of lithium batteries
[0062] Couple the lithium battery electrical model, lithium battery thermal model and lithium battery aging model: obtain the lithium battery internal resistance through impedance sweep technology to obtain the lithium battery electrical model. The lithium battery electrical model gives the internal resistance to the lithium battery thermal model to obtain the lithium battery temperature parameters. The lithium battery thermal model gives the battery temperature and the SOC parameters in the electrical model to the aging model to obtain the lithium battery capacity attenuation and lithium battery health information, and establish the lithium battery electrical-thermal-aging model;
[0063] Step 5: Through the relevant parameters of the lithium battery electric-thermal-aging model (capacity loss Qloss, temperature and soc of the lithium battery), the pulse heating simulation of the lithium battery in a low temperature environment of -40° to -20° is carried out to obtain the optimal pulse amplitude and pulse frequency corresponding to each temperature of the lithium battery in the low temperature environment, and formulate a pulse heating strategy that can suppress capacity attenuation in the low temperature environment. See the process Figure 5 , the heating strategy is:
[0064] Use the pulse module to perform pulse heating on the electric-thermal-aging model of the lithium battery established in step 4. By changing the charge and discharge direction, a pulse charge and discharge current is formed. The current continuously flows through the internal resistance, generating a large amount of heat, thereby heating the battery. The battery pulse heating is calculated based on a°C step change, a>0, and the frequency and amplitude are changed for every a°C increase. The changed frequency and amplitude are the optimal pulse frequency and amplitude corresponding to the temperature after the a°C increase. Each step temperature has the optimal heating rate, thereby improving the overall heating efficiency.
[0065] Implementation example Figure 2 First, use EIS frequency sweep technology to obtain the impedance characteristics of lithium batteries in real time. The impedance frequency sweep flow chart is as follows: Figure 3As shown in the figure, a small-amplitude sinusoidal voltage or current signal is used as an excitation signal to actively disturb the electrochemical steady-state system. By analyzing the frequency, amplitude and phase relationship between the excitation signal and the response signal, the frequency response function of the measured system within a certain frequency range is finally obtained. The lithium battery impedance information is calculated using formula (7), and an electrical model is established based on the lithium battery internal resistance information. The lithium battery terminal voltage and SOC information can be obtained through the lithium battery electrical model.
[0066]
[0067] Then, set the initial temperature and ambient temperature of the lithium battery on the simulation platform and use formulas 3 and 4 to establish a thermal model for the lithium battery. Finally, establish a lithium battery aging model based on internal resistance information, temperature information, and SOC information. Based on the battery aging information obtained on the simulation platform, the battery health status can be obtained using formula 5. After establishing the battery electrical-thermal-aging model, use the simulation platform to obtain the optimal pulse frequency and amplitude corresponding to different temperatures. The simulation platform can also be used to obtain the lithium battery aging at the optimal frequency and amplitude. Understand the battery performance of lithium batteries under pulse heating.
[0068]
[0069] Where Q is the initial capacity of the lithium battery, Qloss is the capacity decay during heating. SOH is the health of the lithium battery. The isolated bidirectional DC / DC circuit used is Figure 1 As shown, S1-S8 in the figure are fully controlled switch tubes. The on and off of the switch tubes are controlled by driving pulses, thereby controlling the bidirectional flow of energy between the primary and secondary sides. S1-S4 form an H1 bridge, and S5-S8 form an H2 bridge. The two H bridges are connected by a high-frequency transformer. The transformer ratio is n, and L is the transformer leakage inductance. The two H bridges are coupled through L, which is the main device that can realize bidirectional energy transmission. In the main circuit topology, the eight switch tubes S1-S8 all work in a 50% duty cycle mode. The driving signals of the two switch tubes in the same bridge arm in the two full bridges on the primary and secondary sides are complementary to avoid direct conduction. The driving signals of the two diagonal switch tubes are consistent. The on and off of the switch tubes are controlled by driving pulses to generate a 50% duty cycle square wave voltage at both ends of the high-frequency transformer. The phase difference of the H bridge switch tube driving signals on both sides of the high-frequency transformer is used to generate square waves with different phases on both sides of the transformer equivalent leakage inductance. The phase difference is adjusted to control the forward and reverse flow of the converter energy.
[0070] In the main topology diagram, V1 is a supercapacitor and V2 is a lithium battery. When energy flows forward, the supercapacitor charges the lithium battery through the circuit. When energy flows backward, the lithium battery discharges the supercapacitor through the circuit. By changing the direction of charge and discharge, the lithium battery will form a pulse charge and discharge current. The current continuously flows through the internal resistance, which will generate a lot of heat, thereby heating the battery. Compared with traditional capacitors, the working mode and performance of supercapacitors are very similar. The main difference is that the capacity of supercapacitors is much larger than that of traditional capacitors, so they can be used as devices similar to batteries to store energy. Supercapacitors have better high power density characteristics. Charging and discharging batteries through supercapacitors will not cause loss of battery energy. The pulse heating method of lithium batteries is realized by quickly switching the direction of energy flow in the isolated bidirectional DC / DC circuit.
[0071] Establish an isolated bidirectional DC / DC circuit of supercapacitor-lithium battery. Figure 1 As shown in the figure, the isolated bidirectional DC / DC circuit has a supercapacitor on the left and a lithium battery on the right. The output power of the circuit is calculated according to the following formula.
[0072]
[0073] DT S is the phase shift angle between the two full bridges. In charging mode, the voltage square wave of the primary bridge leads the secondary bridge by a duty cycle DT S , so the direction of energy transfer is from the primary side to the secondary side. The primary side bridge completes the inversion, and is transferred to the secondary side through the transformer. The secondary side completes the rectification and outputs. In the discharge mode, the square wave of the primary side bridge voltage lags behind the secondary side bridge by a duty cycle DTs, so the direction of energy transfer is from the secondary side to the primary side. The secondary side bridge completes the inversion, and is transferred to the primary side through the transformer. The primary side completes the rectification and outputs.
[0074] When the charge and discharge modes are switched quickly, a pulse current will be formed on the battery. By controlling the switching speed, the pulse frequency can be changed, and by changing the voltage of the supercapacitor, the pulse amplitude can be changed.
[0075] Heating optimization strategy, detailed heating strategy such as Figure 4 As shown in the figure, the pulse heating optimization algorithm is used. In a low-temperature environment, different temperatures correspond to the optimal pulse heating frequency and amplitude. In the simulation platform, the lithium battery electric-thermal-aging model is simulated by applying pulses to obtain the optimal frequency and amplitude corresponding to different temperatures. Different temperatures correspond to different optimal amplitudes and optimal frequencies, which are calculated with a step change of 1°C. For every 1°C increase, the amplitude and frequency of the isolated bidirectional DC / DC circuit are changed. Each step temperature has an optimal heating rate, thereby improving the overall heating efficiency.
[0076] A pulse current heating system for lithium batteries in a low temperature environment, comprising:
[0077] Coupling module: used to couple the lithium battery electrical model established in step 1, the lithium battery thermal model established in step 2, and the lithium battery aging model established in step 3, and establish the lithium battery electrical-thermal-aging model in step 4, which can simulate the charging and discharging behavior of the battery, accurately grasp the health status of the battery under different heating conditions and aging stages, and perform battery health detection and optimization;
[0078] Lithium battery pulse current heating strategy module: In step 5, the pulse module is used to generate pulse heating for the established lithium battery electric-thermal-aging model, change the charge and discharge direction, form a pulse charge and discharge current, and the current continuously flows through the internal resistance to generate heat to heat the battery. The calculation is based on a℃ step change, a>0, and the frequency and amplitude are changed for every a℃ increase. The changed frequency and amplitude are the optimal pulse frequency and amplitude corresponding to the temperature after the a℃ increase; each step temperature has the optimal heating rate, thereby improving the overall heating efficiency.
[0079] A lithium battery pulse current heating device in a low temperature environment, comprising:
[0080] Memory for storing computer programs;
[0081] The processor is used to implement the pulse current heating method for lithium batteries in a low temperature environment described in steps 1 to 5 when executing the computer program.
[0082] A computer-readable storage medium is used to store a computer program. When the computer program is executed by a processor, it can perform pulse charging and discharging on a lithium battery based on the pulse current heating method for a lithium battery in a low temperature environment described in any one of steps 1 to 5, and use different optimal frequencies and optimal amplitude characteristics corresponding to different temperatures to heat the lithium battery and improve the heating rate.
Claims
1. A pulse current heating method for lithium batteries in low temperature environment, It is characterized in that The specific steps include: Step 1: Establish a lithium battery electrical model; Step 2: Establish a thermal model of lithium battery; Step 3: Establish a lithium battery aging model to predict the capacity of the lithium battery in real time during the cycle use; Step 4: Couple the lithium battery electrical model, lithium battery thermal model and lithium battery aging model to establish an electrical-thermal-aging model of the lithium battery; Step 5. According to the relevant parameters of the lithium battery electric-thermal-aging model: the capacity loss Qloss, temperature and soC of the lithium battery, a pulse heating simulation of the lithium battery in a low temperature environment of -40° to -20° is performed to obtain the optimal pulse amplitude and pulse frequency corresponding to each temperature of the lithium battery in the low temperature environment, and a pulse heating strategy that can suppress capacity attenuation in the low temperature environment is formulated.
2. According to claim 1, a pulse current heating method for lithium batteries in a low temperature environment, It is characterized in that The specific method of step 1 is: The EIS sweep frequency technology is used to obtain the impedance information of the lithium battery in real time, and the lithium battery electrical model is established according to the second-order RC equivalent circuit model; the lithium battery electrical model formula is as follows: Among them, U L is the terminal voltage of lithium battery, U 0C is the open circuit voltage of the lithium battery, I is the current, R 0 is the ohmic resistance, R 1 , R 2 is the polarization resistance, C 1 , C 2 is the polarization capacitance, U 1 , U 2 is the polarization voltage.
3. According to the pulse current heating method of lithium battery in low temperature environment of claim 1, It is characterized in that The specific method of step 2 is: According to the thermal balance mechanism of lithium batteries, a thermal model of lithium batteries is established, and the formula is as follows: Among them, Qt is the total heat generation, R is the ohmic resistance, Rp is the polarization resistance, T is the lithium battery temperature, I is the current, U OC is the open circuit voltage, h is the convection heat transfer coefficient, s is the heat exchange area on the surface of the lithium battery, T a is the air temperature.
4. A pulse current heating method for lithium batteries in a low temperature environment according to claim 1, It is characterized in that The specific method of step 3 is: The capacity of lithium batteries during the cycle is predicted in real time, and a semi-empirical model of lithium battery capacity decay is established in combination with the Arrhenius equation. The lithium battery aging model is expressed as follows: Among them, a, b, c are parameters, Q cal is the capacity attenuation caused by calendar aging, Q cyc is the capacity decay caused by cycling, Ea represents the activation energy of the chemical reaction inside the lithium battery; R is the universal gas constant, and Ah represents the cumulative charge and discharge capacity during the charge and discharge period.
5. A pulse current heating method for lithium batteries in a low temperature environment according to claim 1, It is characterized in that The specific method of step 4 is: The lithium battery electrical model, lithium battery thermal model and lithium battery aging model are coupled to establish the lithium battery electric and thermal aging model: The internal resistance of the lithium battery is obtained by EIS sweep frequency technology, and the formula is as follows: Where Z is the impedance of the lithium battery, R E is the real part of impedance, R I is the imaginary part of impedance, Isin(wt+α) is the AC current signal applied to the lithium battery, and Usin(wt++β) is the voltage signal generated by the lithium battery when stimulated; The lithium battery electrical model transfers the internal resistance to the lithium battery thermal model to obtain the lithium battery temperature parameters. The lithium battery thermal model transfers the lithium battery temperature and the SOC parameters in the lithium battery electrical model to the lithium battery aging model to obtain the lithium battery capacity attenuation and lithium battery health information, and establishes the lithium battery electric and thermal aging model. The formula is as follows: Among them, Q is the initial capacity of the lithium battery, Qloss is the capacity loss during heating, and SOH is the health of the lithium battery.
6. A pulse current heating method for lithium batteries in a low temperature environment according to claim 1, It is characterized in that The heating strategy in step 5 is: Use the pulse module to perform pulse heating on the electric-thermal-aging model of the lithium battery established in step 4. By changing the charge and discharge direction, a pulse charge and discharge current is formed. The current continuously flows through the internal resistance to generate heat, thereby heating the battery. The battery pulse heating is calculated based on a°C step change. When a>0, the frequency and amplitude are changed for every a°C increase. The changed frequency and amplitude are the optimal pulse frequency and amplitude corresponding to the temperature after the a°C increase. Each step temperature has the optimal heating rate, thereby improving the overall heating efficiency.
7. A pulse current heating system for lithium batteries in low temperature environments. It is characterized in that include: Coupling module: used to couple the lithium battery electrical model established in step 1, the lithium battery thermal model established in step 2, and the lithium battery aging model established in step 3, and establish the lithium battery electrical-thermal-aging model in step 4, which can simulate the charging and discharging behavior of the battery, accurately grasp the health status of the battery under different heating conditions and aging stages, and perform battery health detection and optimization; Lithium battery pulse current heating strategy module: In step 5, the pulse module is used to generate pulse heating for the established lithium battery electric-thermal-aging model, change the charge and discharge direction, form a pulse charge and discharge current, and the current continuously flows through the internal resistance to generate heat to heat the battery. The calculation is based on a℃ step change, a>0, and the frequency and amplitude are changed for every a℃ increase. The changed frequency and amplitude are the optimal pulse frequency and amplitude corresponding to the temperature after the a℃ increase; each step temperature has the optimal heating rate, thereby improving the overall heating efficiency.
8. A lithium battery pulse current heating device in a low temperature environment, It is characterized in that include: Memory for storing computer programs; The processor is used to implement the pulse current heating method for lithium batteries in a low temperature environment described in steps 1 to 5 when executing the computer program.
9. A computer-readable storage medium for storing a computer program. It is characterized in that When the computer program is executed by the processor, it can perform pulse charging and discharging on the lithium battery based on the pulse current heating method for lithium batteries in a low temperature environment described in any one of steps 1 to 5, and heat the lithium battery using different optimal frequencies and optimal amplitude characteristics corresponding to different temperatures to increase the heating rate.
Citation Information
Patent Citations
Alternating excitation low-temperature heating method for lithium ion battery based on temperature change
CN109786897A
Pulse current preheating parameter optimization method and system based on orthogonal test and medium
CN118226258A
Cited By
Battery replacement battery series connection heating control method and system
CN118970294A
Lithium ion battery electricity-heat-aging coupling model construction method based on EIS
CN120745395A
A Method for Constructing an Electro-Thermal-Aging Coupled Model of Lithium-ion Batteries Based on EIS
CN120745395B
Battery pulse heating method and device, vehicle and storage medium
CN120879074A