Artificial shale uniaxial failure dynamic characteristic monitoring method based on distributed optical fiber and acoustic emission monitoring

By arranging optical fiber and acoustic emission probes at multiple angles on the rock sample, combined with the simultaneous analysis of optical fiber and acoustic emission data, the problem of insufficient distance coverage of distributed optical fiber monitoring technology in long-distance sensing is solved, and the strain of the rock sample is realized. Accurate monitoring of changes supports the stability and safety of shale gas development.

CN118758744AActive Publication Date: 2024-10-11CHENGDU UNIVERSITY OF TECHNOLOGY

Patent Information

Application Number
CN202411042232.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-31
Publication Date
2024-10-11
Estimated Expiration
2044-07-31

AI Technical Summary

Technical Problem

Existing distributed optical fiber monitoring technology has the problem of insufficient distance coverage in long-distance sensing applications, and it is difficult to meet the long-distance monitoring needs in rock uniaxial compression tests.

Method used

A method for monitoring the uniaxial damage dynamic characteristics of artificial shale based on distributed optical fiber and acoustic emission monitoring is adopted. By arranging optical fiber and acoustic emission probes on the rock sample at multiple angles, the optical fiber data and the acoustic emission data are combined for simultaneous analysis and systematic monitoring. Strain distribution and failure modes of rock samples in uniaxial compression tests.

Benefits of technology

It achieves real-time and accurate monitoring of the strain changes of rock samples in uniaxial compression tests, provides reliable data support for the stress conditions and failure mechanisms of rock samples, optimizes the construction plan for shale gas development, and ensures long-term stability. and security.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118758744A_ABST
    Figure CN118758744A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of distributed optical fiber monitoring, and discloses an artificial shale uniaxial failure dynamic characteristic monitoring method based on distributed optical fibers and acoustic emission monitoring, which comprises the following steps: step 1, rock sample preparation: injecting mixed slurry into a mold, standing, demolding, maintaining, and respectively drilling cylindrical rock samples according to four angles of 0 degree, 30 degrees, 45 degrees and 90 degrees; step 2, preparing and preprocessing optical fibers; step 3, joint arrangement of optical fibers and acoustic emission sensors: four optical fibers are attached to each cylindrical rock sample in a manner that the optical fibers are horizontally attached along the rock sample at 0 degree, 90 degrees, 180 degrees and 270 degrees, and acoustic emission probes are mounted at the upper end and the lower end of the rock sample; and 4, stress loading and detection: carrying out compression loading and simultaneous analysis of optical fiber data and acoustic emission data. By reasonably selecting the drilling angle and monitoring the crack extension direction, the design and construction scheme of the geothermal well can be optimized, and the long-term stability and safety of the geothermal well are ensured.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of distributed optical fiber monitoring, and in particular to a method for monitoring dynamic characteristics of uniaxial failure of artificial shale based on distributed optical fiber and acoustic emission monitoring. Background Art

[0002] As a basic component of geological engineering and building structures, the mechanical behavior of rock materials is crucial to understanding and predicting the stability of engineering structures. Although rocks have high intrinsic strength, they are still prone to cracking and fracture under mechanical forces such as uniaxial compression. These damage processes directly affect the safety and durability of engineering structures. Therefore, it is necessary to accurately monitor the strain and crack extension of rocks in uniaxial compression experiments. Although traditional rock mechanics experimental methods such as direct observation and acoustic emission monitoring can provide certain crack information, they are limited in capturing the formation and extension process of fine cracks inside rocks.

[0003] Optical Frequency Domain Reflectometry (OFDR) is an advanced monitoring method based on the detection of the optical fiber Rayleigh back scattering spectra (RBS) with the advantages of high measurement accuracy, high sensing spatial resolution, and long measurement distance. The high spatial resolution and sensitivity of OFDR technology enable it to capture tiny strain changes, which is of great significance for early crack detection and rock damage warning. In the field of distributed optical fiber sensing, although the temperature, vibration, stress and strain sensing technology based on OTDR technology has made significant progress in test distance, spatial resolution, sensitivity, accuracy and dynamic response, these indicators still need to be improved to meet the needs of a wider range of applications, prompting researchers to explore new methods and mechanisms. As a new technology, OFDR is superior to traditional OTDR in spatial resolution and accuracy, but its test distance is short, especially in sensing applications, it can only cover tens of meters, which is difficult to meet the needs of long-distance sensing. Summary of the invention

[0004] The present invention aims to provide a method for monitoring the dynamic characteristics of uniaxial failure of artificial shale based on distributed optical fiber and acoustic emission monitoring, so as to solve the problem in the prior art that the OFDR test distance is difficult to meet the long-distance sensing requirements.

[0005] To achieve the above object, the present invention adopts the following technical solution: a method for monitoring the dynamic characteristics of uniaxial failure of artificial shale based on distributed optical fiber and acoustic emission monitoring, comprising the following steps:

[0006] Step 1: Preparation of rock samples: Mix cement with sandstone of different particle sizes to obtain a mixed slurry, inject the mixed slurry into a mold, let it stand, demould, and maintain it, and then drill cylindrical rock samples at four angles of 0°, 30°, 45°, and 90°;

[0007] Step 2: Preparation and pretreatment of optical fiber: Use single-mode optical fiber with a diameter of 125 microns and a coating diameter of 250 microns, and perform fusion splicing and protection treatment on the optical fiber;

[0008] Step 3: Joint deployment of optical fiber and acoustic emission sensors: Four optical fibers are attached to each cylindrical rock sample. The attachment method is: attach the optical fiber horizontally along the cylindrical body of the rock sample at 0°, 90°, 180°, and 270°; install acoustic emission probes at the upper and lower ends of the rock sample respectively;

[0009] Step 4: Stress loading and testing: Pre-stress to ensure that the rock sample and experimental equipment are in a stable state, and then perform compression loading and joint analysis of optical fiber data and acoustic emission data.

[0010] Preferably, as an improvement, in step one, the mass ratio of the raw materials in the mixed slurry is cement: 260 mesh sandstone: 150 mesh sandstone: 80 mesh sandstone: 60 mesh sandstone: water = 40:6:2:20:12:15.

[0011] Preferably, as an improvement, in step two, the fusion splicing operation is: use a fiber fusion splicer to fuse one end of four optical fibers, and before fusion splicing, remove the coating on the optical fiber to expose a section of the optical fiber, and perform vertical cutting on a fiber optic cutting machine.

[0012] Preferably, as an improvement, in step 2, the pretreatment operation is: after the optical fibers are fused, a transparent sleeve is put on the fusion point, and a heat sealing treatment is performed.

[0013] Preferably, as an improvement, in step 2, a welding test is performed after the welding is completed, and a laser pen is inserted into one end of the signal receiver to emit light. If the other end emits red light, it proves that the welding is successful, otherwise it means that the welding has failed.

[0014] Preferably, as an improvement, in step three, the installation directions of the acoustic emission probes are respectively 0° to 180° and 90° to 270°.

[0015] Preferably, as an improvement, in step four, the sensitivity of the optical fiber and the acoustic emission probe is tested before detection. First, the single-mode optical fiber is pressed, the single measurement mode of the optical fiber demodulator is turned on, and the optical fiber is checked to see whether it can receive the signal normally; then different positions of the rock sample are tapped to determine whether the probe position can accurately monitor the acoustic emission signal.

[0016] Preferably, as an improvement, step three also includes dividing the rock sample into six equal parts in the 0° direction, and attaching two additional optical fibers to achieve strain monitoring of the six equal parts.

[0017] The principle and advantages of this scheme are as follows: In actual application, in this technical scheme, in view of the problem that the OFDR test distance in the existing technology is difficult to meet the long-distance sensing requirements, the distributed optical fiber monitoring technology is applied to the uniaxial compression test of rock samples, and the strain distribution and failure mode of rock samples in the uniaxial compression test are systematically analyzed by combining the preparation of rock samples, multi-angle drilling sampling and multi-angle layout of optical fiber rock samples. During the technical research and development, considering the bedding of artificial rock samples in layered casting, multi-angle sampling was carried out on artificial rock samples; in the optical fiber layout stage, a multi-angle layout method was adopted to improve the accuracy of monitoring; in the result evaluation stage, the optical fiber data inversion and acoustic emission and failure mode joint analysis were combined to ensure the accuracy of the result analysis. The experimental results show that the application of distributed optical fiber monitoring technology in the uniaxial compression test of rock samples is feasible and effective. The optical fiber sensor can collect the strain changes of rock samples in real time and accurately during the compression process, and through data analysis, clearly show the strain distribution law of rock samples under compression loading conditions. This technology provides reliable data support for in-depth understanding of the stress conditions and failure mechanisms of rock samples.

[0018] In summary, by using distributed fiber optic monitoring technology, this study has analyzed in detail the strain distribution and failure mode of rock samples at different angles in uniaxial compression tests, thereby verifying the feasibility of applying fiber optic monitoring technology in rock uniaxial mechanics. The research results show that the changes in stress and strain of rocks during uniaxial failure are significantly correlated with their drilling angles, which has important reference value for understanding the mechanical behavior and failure mechanism of rocks under failure conditions during shale gas development. This technical solution can optimize the construction plan of shale gas development and ensure the long-term stability and safety of shale development by reasonably selecting drilling angles and monitoring the direction of crack expansion. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] Figure 1 This is a schematic diagram of rock sampling according to an embodiment of the present invention.

[0020] Figure 2 Schematic diagram of rock sample cracks at 0°, 30°, 45°, and 90° in an embodiment of the present invention.

[0021] Figure 3 This is a three-dimensional positioning diagram of acoustic emission in an embodiment of the present invention 0° (left) 30° (right).

[0022] Figure 4 This is a three-dimensional positioning diagram of acoustic emission in an embodiment of the present invention at 45° (left) and 90° (right).

[0023] Figure 5It is a Y-1-0° optical fiber strain waterfall diagram in an embodiment of the present invention.

[0024] Figure 6 This is the Y-1-0° optical fiber strain diagram in an embodiment of the present invention.

[0025] Figure 7 This is the 1-second strain diagram of the 45° rock sample in the embodiment of the present invention.

[0026] Figure 8 This is the strain diagram of the 45° rock sample at 23 seconds in the embodiment of the present invention.

[0027] Fig. 9 These are the 45° rock sample acoustic emission three-dimensional positioning map (left), 45° optical fiber cylindrical strain map at 55 seconds (middle), and initial crack map (right) in an embodiment of the present invention.

[0028] Fig.10 The 45° rock sample optical fiber cylindrical strain diagram at the 65th second (left) and the 76th second (right) in the embodiment of the present invention.

[0029] Fig.11 The 45° rock sample crack diagram (left) and the 45° optical fiber cylinder strain diagram at the 79th second (middle) and the 81st second (right) in an embodiment of the present invention.

[0030] Fig.12 The 45° rock sample optical fiber cylindrical strain diagram at 84 seconds (left) and 87 seconds (right) in an embodiment of the present invention.

[0031] Fig.13 The final development diagram of the 45° rock sample crack diagram in the embodiment of the present invention (left) and the 45° optical fiber cylinder strain diagram at the 98th second (middle) and the 101st second (right). DETAILED DESCRIPTION

[0032] The following is further described in detail through specific implementations, but the implementation of the present invention is not limited thereto. Unless otherwise specified, the technical means used in the following implementations are conventional means well known to those skilled in the art; the experimental methods used are all conventional methods; the materials, reagents, etc. used can all be obtained from commercial channels.

[0033] Example 1

[0034] A method for monitoring dynamic characteristics of uniaxial failure of artificial shale based on distributed optical fiber and acoustic emission monitoring, comprising the following steps:

[0035] Step 1: Preparation of rock samples: Prepare the mold and evenly apply No. 50 general-purpose mechanical lubricant to the inner wall of the mold to prevent affecting the surface flatness of the molded specimen. When applying lubricant, disassemble the mold first to ensure even application. When reassembling the mold, align the gaps;

[0036] Place the cement mortar in a cement mortar mixer according to the mass ratio of cement: 260 mesh sandstone: 150 mesh sandstone: 80 mesh sandstone: 60 mesh sandstone: water at 40:6:2:20:12:15 and stir slowly. During the stirring process, first put in all the raw materials, then slowly add water using a measuring cylinder and stir for 2 to 3 minutes;

[0037] After mixing, inject cement slurry into the mold and vibrate it on a concrete vibrator for 2 to 3 minutes until the horizontal surface becomes flat; demould after standing for 24 hours, and spray water for maintenance;

[0038] Then, 50×100 mm cylindrical rock samples were drilled at four angles: 0°, 30°, 45°, and 90°. Figure 1 shown.

[0039] Step 2: Joint deployment of optical fiber and acoustic emission sensors: Use 22 1m long single-mode optical fibers (SMFs) with a diameter of 125 microns and a coating diameter of 250 microns. The diameter has a certain influence on the mechanical strength and installation method of the optical fiber. Its spatial resolution theoretically reaches 0.1mm or even higher. Use AB type coupling agent to horizontally fit four optical fibers along the rock sample cylinder at 0°, 90°, 180°, and 270°. The fifth rock sample will set the variable to 0° and paste six optical fibers in six equal parts. Install acoustic emission probes at the upper and lower ends of the rock sample, with installation angles (directions) of 0° to 180° and 90° to 270°.

[0040] Pre-treatment operation: Before bonding, the optical fibers are fused and protected. First, one end of the four optical fibers is fused using a fiber fusion splicer. Before fusion, the coating on the optical fiber is removed to expose about 3 cm of the optical fiber, and then cut vertically on a fiber cleaver. Then, the same operation is performed on the optical fiber connected to the signal receiver. Next, the two optical fibers are placed in the fiber fusion splicer so that they are in a horizontal docking position and fused together. Finally, a transparent sleeve is placed on the fusion point and heat-sealed to protect the optical fiber connection from external interference.

[0041] Use a laser pen to insert one end of the signal receiver to emit. If the other end emits red light, it proves that the welding is successful, otherwise it fails.

[0042] Step 3: Uniaxial compression test: Use uniaxial compression equipment for testing, which includes an axial pressure loading system, a confining pressure loading system, a seepage system, an acoustic emission system, a temperature system, etc. (existing technology). The specific test steps are as follows:

[0043] S1. Cut the rock sample at four angles of 0°, 30°, 45°, and 90°, numbered as Y-1-0°, Y-1-30°, Y-1-45°, and Y-1-90° respectively. In addition, the fifth rock sample will be divided into six equal parts in the 0° direction and numbered as Y-2 to explore the effect of loading direction on the mechanical properties of rock;

[0044] S2. Fiber optic layout: Four optical fibers are bonded to each rock sample, corresponding to the directions of 0°, 90°, 180°, and 270°, to achieve strain monitoring at the corresponding positions. For the rock sample numbered Y-2, two additional optical fibers will be bonded to achieve strain monitoring in six equal parts; acoustic emission probes are installed at the upper and lower ends of the rock sample, with installation angles (directions) of 0° to 180° and 90° to 270°;

[0045] S3. Calibration and marking: Calibrate the acoustic emission probe and optical fiber, and mark their positions for subsequent data analysis. Before the experiment begins, test the sensitivity of the optical fiber and acoustic emission probe. First, gently press the single-mode optical fiber, turn on the single measurement mode of the optical fiber demodulator, and check whether the optical fiber can receive the signal normally. Secondly, tap different positions of the rock sample to determine whether the acoustic emission probe position accurately monitors the acoustic emission signal;

[0046] S4, pre-compression stage: pre-compression is performed before the experiment to ensure that the rock sample and experimental equipment are in a stable state. The strain and acoustic emission signals during the pre-compression stage are recorded;

[0047] S5. Compression loading: The rock sample is compressed and loaded by a uniaxial loading device, and the strain and acoustic emission signals during the loading process are recorded. The loading rate should be adjusted according to the experimental requirements to ensure the accuracy and reliability of data collection, and the pressure is applied until the rock sample breaks;

[0048] S6. Fiber optic detection: Use a laser pen to insert one end of the signal receiver to emit light. If the other end emits red light, it means that the entire fiber optic cable has been tested and has not been damaged by stress.

[0049] S7. Data recording: Real-time recording of strain and acoustic emission signal data during compression loading, and storage and backup at the specified frequency for subsequent analysis and research.

[0050] Results and Analysis

[0051] 1. Rock sample stress analysis and stress law

[0052] With this technical solution, most optical fibers can detect data and obtain relatively complete rock sample fragments. The corresponding force analysis and stress law can be obtained from the reorganization of the broken fragments of the rock sample ( Figure 2) It can be seen that after uniaxial compression, the rock sample is mainly destroyed by axial splitting. The crack direction is basically parallel to the stress loading direction and the cracks are relatively developed. In addition, the existence of weak planes will induce the direction of cracks.

[0053] (1) 0 degree sample: Figure 2 Left 1)

[0054] ① A longitudinal through crack was observed at the center of the sample, and the crack ran through the entire rock sample.

[0055] ② The starting position of the crack is close to the top of the sample and gradually expands downward to the bottom.

[0056] ③ It shows that the sample suffered obvious axial tensile failure during the compression process.

[0057] (2) 30 degree sample: Figure 2 Left 2)

[0058] ① Obvious longitudinal cracks appeared on the top of the sample, starting from the top and extending downward.

[0059] ②The bottom of the sample remains intact, but cracks appear on the top.

[0060] ③This indicates that the sample is subjected to a large compressive stress at the top, causing the top material to be damaged and cracks to form.

[0061] (3) 45 degree sample: Figure 2 Left 3)

[0062] ① Obvious oblique cracks were observed on the surface of the sample, and the cracks showed a certain angle.

[0063] ② The overall structure of the sample is still maintained, but the cracks run through the surface of the sample.

[0064] ③This indicates that the sample may have undergone shear failure during the compression process, leading to the formation of oblique cracks.

[0065] (4) 90 degree sample: Figure 2 Right 1)

[0066] ①The damage to the sample is quite serious, with the cracks starting from the top of the sample and showing multiple intersecting cracks.

[0067] ② The sample broke into multiple small pieces, indicating that the sample had multiple cracks during the compression process.

[0068] ③ It may be due to the existence of initial microcracks inside the sample that the stress is concentrated at multiple points, resulting in the generation of multiple cracks.

[0069] 2. Acoustic emission data analysis

[0070] In this study, acoustic emission technology was used to monitor and analyze the initiation and development of cracks in rocks under uniaxial compression. Acoustic emission technology is a non-destructive detection method that can monitor the dynamic changes of internal defects and cracks in materials in real time. In the experiment, four channels, 1, 2, 5, and 6, were set up to collect acoustic emission signals at different angles. By recording parameters such as arrival time and amplitude, the distribution of acoustic emission events in rocks during compression was analyzed. In the experiment, we obtained data through acoustic emission technology and calculated the arrival time of sound waves for three-dimensional positioning. Figure 3 and Figure 4 , thus obtaining information about the internal cracks of the rock sample. Subsequently, we compared these 3D positioning results with the crack information obtained by distributed fiber optic monitoring to verify the accuracy and effectiveness of distributed fiber optic monitoring.

[0071] Depend on Figure 3 (a) The crack distribution of the 0-degree rock sample can be seen. The red dots indicate the locations of the cracks, and the blue dots represent the sensor locations. It can be seen that the cracks are mainly concentrated in the upper and middle parts of the rock sample, which are stress concentration points. The cracks propagate axially and laterally, showing complex bending and bifurcating paths, which show the stress distribution and transmission inside the rock. The bifurcation and complex paths of these cracks indicate that there are multiple stress concentration points inside the rock sample, causing the cracks to expand in different directions.

[0072] Figure 3 (b) shows the crack distribution of the 30-degree rock sample. Compared with the 0-degree rock sample, the cracks in the 30-degree rock sample are also mainly concentrated in the upper and middle areas, but the distribution of the cracks is more dispersed. The direction and morphology of the cracks show the stress concentration and transmission characteristics of the rock sample at a 30-degree angle. The cracks propagate axially and laterally, forming a complex path, which further illustrates the stress distribution inside the rock.

[0073] Figure 4 (a) shows the crack distribution of a 45-degree rock sample. It can be seen that the cracks are mainly concentrated in the upper and middle parts of the rock sample, which are stress concentration points. The cracks propagate axially and laterally, showing complex bending and bifurcating paths, which shows the stress distribution and transmission inside the rock. The crack distribution at a 45-degree angle is more dispersed, indicating the transmission characteristics of stress in different directions.

[0074] Figure 4 (b) shows the crack distribution of the 90-degree rock sample. Compared with the 45-degree rock sample, the cracks of the 90-degree rock sample are more concentrated in the lower and middle areas of the rock sample. The direction and morphology of the cracks show the stress concentration and transfer characteristics of the rock sample at a 90-degree angle. The cracks propagate axially and laterally, forming a complex path.

[0075] Through three-dimensional positioning, it can be found that 0°, 30°, and 45° are all monitoring the top where cracks are mainly developed, with only slight cracks developed at the bottom, and 90° shows obvious crack development both above and below.

[0076] 3. Combined with fiber optic monitoring data analysis

[0077] The distributed optical fiber monitoring system is used to collect strain data in all directions on the surface of the rock sample in real time. The collected data are analyzed and visualized through the data processing software MATLAB to obtain the strain distribution law of the rock under different loading directions.

[0078] 3.1Y-1-0° rock sample analysis

[0079] In the first fiber, it is possible to Figure 5 It can be clearly seen in the figure that the optical fiber can monitor the gradually increasing strain over time. The original data shows that the strain gradient of each increase is 25, which is consistent with the uniform pressure applied by the uniaxial compressor. This preliminarily verifies the feasibility of distributed optical fiber monitoring uniaxial strain. Since this optical fiber is not laid on the cracks of the broken rock sample, it only monitors the strain caused by the uniform pressure of the rock sample by the uniaxial compressor. It can be observed from the figure that when the axial strain reaches 4200 microstrain, a jump point appears in the curve, and when the sample is damaged, the strain drops sharply to nearly 0; the second optical fiber monitors tensile stress instead of compressive stress in the initial stage, which may be due to position errors in the pre-stressing stage, or cracks from the inside of the rock sample are monitored. Subsequently, the optical fiber begins to monitor the gradually increasing strain until the rock is damaged when the axial strain reaches 2600 microstrain. From this point on, the monitored strain gradually decreases and finally approaches 0; the third optical fiber fails to monitor effective data, which may be due to the unevenness of the upper and lower ends of the rock sample or the failure to firmly stick the optical fiber when it is laid; in the fourth optical fiber, uniformly increasing strain can be detected in the first 20 seconds. After 20 seconds, an abnormal strain suddenly increased at 30-50 mm. This is because under the action of axial compression, cracks in the rock sample began to develop until the rock sample was severely damaged. At the moment of rupture, local stress was released, which reduced the axial pressure.

[0080] In summary, the fourth optical fiber first detected the crack at 30-50 mm at 20 seconds. Figure 6 As shown in Figure 1, this indicates that the weak plane of the rock sample is located at the fourth optical fiber. The second optical fiber is located opposite the fourth optical fiber and is affected by the stress in the longitudinal direction of the crack, and the tensile stress is monitored.

[0081] Therefore, the information of this crack was also monitored at 20 seconds, but since there was no rupture at the layout position, the uniaxial compressor continued to be monitored to apply pressure evenly until the rock sample was destroyed. The first optical fiber was laid on the left and right sides of the second and fourth optical fibers, and the monitored strain increase was very uniform, with minimal impact from the crack. Therefore, it was concluded that the crack began to occur at the 30-50mm position of the fourth optical fiber at 20 seconds, and propagated horizontally to the first and second optical fibers, and vertically to the upper and lower ends.

[0082] According to the above process, the Y-1-30° rock sample, Y-1-45° rock sample, Y-1-90° rock sample and Y-2-0° rock sample were analyzed. The results showed that the general rule is that the strain detected by the optical fiber shows a uniform increase trend when the optical fiber position is from 0 to 50s, which is relatively stable and gentle. As the pressure of the compressor increases, the strain detected by the optical fiber also increases significantly. It may be that multiple cracks in the rock sample are detected by the optical fiber. In the later stage, the detected stress shows a decreasing trend. It is more scattered and unconcentrated than the first stage and decays faster. It is in the later stage that the stress change inside the rock sample cannot be detected because the rock blocks fall off after the rock sample breaks. It can be seen that at the middle position of 50-80s, the strain changes from downward pressure to upward pressure. It can be concluded that no upward pressure was received during fracturing at this position.

[0083] (1) Initial expansion phase (0-50 seconds)

[0084] In the first 50 seconds, all optical fibers showed a trend of uniform strain increase, indicating that the rock sample was uniformly stressed at this stage and the cracks had not yet expanded to the monitoring positions. From about 50 seconds on, the optical fiber strain curves in all directions showed a significant decline, indicating that the cracks began to expand and affect the optical fiber monitoring points in four directions.

[0085] (2) Further expansion stage (50-80 seconds)

[0086] After 50 seconds, the strain curves of each optical fiber showed a further decrease, indicating that the crack continued to extend outward after the initial expansion. At 80 seconds, the strain of each optical fiber dropped significantly again, indicating that the crack further expanded and reached a new monitoring range.

[0087] 1. Visual processing of distributed optical fiber monitoring data

[0088] In this study, four groups of rock samples with different sampling angles were used for uniaxial compression tests. During the experiment, distributed fiber optic sensing technology was used to monitor the strain distribution of the rock samples in real time, and acoustic emission events were recorded to assist in analyzing the crack propagation process. In order to visualize and analyze this data, we wrote MATLAB code to generate dynamic GIF images, showing the strain distribution on the surface of the rock samples at various times. The following are the key steps and explanations of the MATLAB model:

[0089] (1) Data loading and processing: First, load four sets of rock sample strain data with different sampling angles to ensure that each set of data has the same size at the same height point. This step provides the basis for the subsequent visualization of strain distribution.

[0090] (2) Create a cylindrical model: Define the parameters of the cylinder (radius 25 mm, height 100 mm) and create a cylindrical model. Use linear interpolation to map the fiber data to a specific angle area on the cylindrical surface.

[0091] (3) Dynamic visualization: By looping through the data every second, the strain distribution diagram at each moment is generated and saved in sequence as a GIF file. The image shows the distribution of strain on the cylindrical surface and its change over time, providing an intuitive visualization tool for analyzing crack propagation as shown in the figure.

[0092] Through the above method, we can visually observe the dynamic changes of strain distribution of rock samples during uniaxial compression. These changes reveal the initiation, expansion and penetration of cracks, thus providing reliable data support and visualization tools for analyzing the influence of sampling angle on crack expansion.

[0093] 4.1 Crack initiation and propagation at different sampling angles

[0094] The 45° rock sample was tested. At the initial stage of compression, Figure 7 As shown in the figure, the strain distribution of the 45° rock sample is relatively uniform, and no obvious strain concentration area appears. At this time, the microcracks inside the rock sample have not yet begun to expand. As the compression force increases, the strain in certain areas gradually increases, forming a strain concentration area. As can be seen from the right figure, there is an obvious strain concentration phenomenon in the middle area of ​​the sample (yellow area), indicating that the material there is under great pressure, while tensile strain appears in the upper and lower end areas (dark red areas).

[0095] It can be seen that at the beginning of uniaxial compression, the upper and lower ends are often subjected to tensile strain first, while the middle part is subjected to compressive strain. As time increases, the strain also increases, such as Figure 8 At this time, the first crack can be detected in the 90-100mm area of ​​the first optical fiber and spreads to the central area. Fig.13As shown, from the 45° acoustic emission three-dimensional positioning diagram ( Fig. 9 Left) It can be observed that there is a stress concentration curve between the sixth and fifth probes, so there is a crack between the two probes. Then under the optical fiber monitoring, the optical fiber cylindrical strain diagram ( Fig. 9 At 60 seconds, the first and fourth optical fibers simultaneously detected tensile strain. The fifth probe is located between the first and fourth optical fibers. Therefore, the initial crack map ( Fig. 9 Right) illustrates the crack initiation location and extension direction.

[0096] like Fig.10 As shown in the figure, at 65 seconds, the strain of the fourth optical fiber was abnormal. The initial crack was offset and spread to the third optical fiber, and it extended from top to bottom. At 76 seconds, the second and third cracks began to develop at about 20 mm from the fourth optical fiber. According to subsequent analysis, one of the two cracks extended upward and the other extended downward.

[0097] like Fig.11 As shown in the figure, at 79 seconds, it can be clearly monitored that the second crack has extended to the 30mm position of the fourth optical fiber. At the same time, it can be observed that the first crack is detected at 60 to 100mm on the upper side of the third optical fiber. Therefore, the crack starts from the acoustic emission probe No. 5 and passes through the fourth optical fiber. After reaching the monitoring range of the third optical fiber, the crack begins to spread to the upper and lower ends. At the 81st second, the third optical fiber detects the second crack from the fourth optical fiber, from which it can be inferred that the crack begins to develop horizontally to the third optical fiber.

[0098] like Fig.12 As shown, at 84 seconds, the second crack at the fourth optical fiber began to grow upward and was also expanding. The first crack at the third optical fiber monitoring location continued to grow downward to 60 mm, while the first crack developed horizontally to 80 mm at the second optical fiber. At 87 seconds, the second crack began to grow downward, the third crack had grown downward to the bottom, and the first crack grew downward to 40 mm at the third optical fiber and continued to grow upward at the second optical fiber.

[0099] like Fig.13 As shown in the figure, it has entered the late stage. From 98 seconds to 101 seconds, the second crack develops downward while the third crack develops upward, and finally the two cracks converge together. At the same time, the crack at the third optical fiber continues to develop downward, and finally converges with the second and third cracks. At this point, all cracks have been developed.

[0100] Through the analysis of the expansion of uniaxial compression cracks in the remaining three groups of rocks, it was finally concluded that the failure mode of the samples was closely related to the drilling angle. The strain distribution and failure conditions of rock samples at different angles in the uniaxial compression test were different, indicating that the drilling angle had a significant effect on the stress and failure mechanism of the rock samples. The failure mode of the 0-degree and 30-degree samples was mainly axial tension failure, with cracks starting from the top and gradually extending downward. Fiber optic monitoring showed that at these angles, the strain was mainly concentrated in the longitudinal direction, and the failure mode was relatively simple. The 45-degree sample showed shear failure, with cracks showing an oblique direction. The fiber optic monitoring data showed that the strain was evenly distributed on the surface of the sample, but changed dramatically during shear failure, indicating that the sample was more susceptible to shear stress at this angle. The 90-degree sample was the most severely damaged. The fiber optic monitoring data showed the generation of multiple cracks, complex strain distribution, and multiple ruptures in the failure mode. This shows that at this angle, there are more initial microcracks inside the sample, which causes the stress to be concentrated at multiple points, resulting in multiple ruptures in the sample during compression.

[0101] The above is only an embodiment of the present invention, and the common knowledge such as the known specific technical solutions and / or characteristics in the solution is not described in detail here. It should be pointed out that for those skilled in the art, without departing from the technical solution of the present invention, several modifications and improvements can be made, which should also be regarded as the protection scope of the present invention, and these will not affect the effect of the implementation of the present invention and the practicality of the patent. The scope of protection required by this application shall be based on the content of its claims, and the specific implementation methods and other records in the specification can be used to interpret the content of the claims.

Claims

1. A method for monitoring the dynamic characteristics of uniaxial failure of artificial shale based on distributed optical fiber and acoustic emission monitoring, characterized in that: The steps include: Step 1: Preparation of rock samples: Mix cement with sandstone of different particle sizes to obtain a mixed slurry, inject the mixed slurry into a mold, let it stand, demould, and maintain it, and then drill cylindrical rock samples at four angles of 0°, 30°, 45°, and 90°; Step 2: Preparation and pretreatment of optical fiber: Use single-mode optical fiber with a diameter of 125 microns and a coating diameter of 250 microns, and perform fusion splicing and protection treatment on the optical fiber; Step 3: Joint deployment of optical fiber and acoustic emission sensors: Four optical fibers are attached to each cylindrical rock sample. The attachment method is: attach the optical fiber horizontally along the cylindrical body of the rock sample at 0°, 90°, 180°, and 270°; install acoustic emission probes at the upper and lower ends of the rock sample respectively; Step 4: Stress loading and testing: Pre-stress to ensure that the rock sample and experimental equipment are in a stable state, and then perform compression loading and joint analysis of optical fiber data and acoustic emission data.

2. According to claim 1, a method for monitoring dynamic characteristics of uniaxial failure of artificial shale based on distributed optical fiber and acoustic emission monitoring is characterized by: In step 1, the mass ratio of each raw material in the mixed slurry is cement: 260 mesh sandstone: 150 mesh sandstone: 80 mesh sandstone: 60 mesh sandstone: water = 40:6:2:20:12:

15.

3. The method for monitoring dynamic characteristics of uniaxial failure of artificial shale based on distributed optical fiber and acoustic emission monitoring according to claim 2 is characterized by: In step 2, the fusion operation is: use a fiber fusion splicer to fuse one end of four optical fibers. Before fusion, remove the coating on the optical fiber to expose a section of the optical fiber, and then cut it vertically on a fiber optic cutting machine.

4. The method for monitoring dynamic characteristics of uniaxial failure of artificial shale based on distributed optical fiber and acoustic emission monitoring according to claim 3 is characterized by: In step 2, the pretreatment operation is: after the optical fiber is fused, a transparent sleeve is put on the fusion point and a heat sealing treatment is performed.

5. The method for monitoring dynamic characteristics of uniaxial failure of artificial shale based on distributed optical fiber and acoustic emission monitoring according to claim 4 is characterized by: In step 2, after the welding is completed, a welding test is performed by inserting a laser pen into one end of the signal receiver to emit light. If the other end emits red light, it proves that the welding is successful, otherwise it fails.

6. The method for monitoring dynamic characteristics of uniaxial failure of artificial shale based on distributed optical fiber and acoustic emission monitoring according to claim 5 is characterized by: In step three, the installation directions of the acoustic emission probes are 0° to 180° and 90° to 270° respectively.

7. The method for monitoring dynamic characteristics of uniaxial failure of artificial shale based on distributed optical fiber and acoustic emission monitoring according to claim 6 is characterized by: In step 4, the sensitivity of the optical fiber and the acoustic emission probe is tested before detection. First, the single-mode optical fiber is pressed, the single-shot measurement mode of the optical fiber demodulator is turned on, and the optical fiber is checked to see if it can receive the signal normally. Then, different positions of the rock sample are tapped to determine whether the acoustic emission probe position can accurately monitor the acoustic emission signal.

8. The method for monitoring dynamic characteristics of uniaxial failure of artificial shale based on distributed optical fiber and acoustic emission monitoring according to claim 7 is characterized by: Step three also includes dividing the rock sample into six equal parts in the 0° direction and attaching two additional optical fibers to achieve strain monitoring of the six equal parts.

Citation Information

Patent Citations

  • Structure multidirectional deformation monitoring method and system

    CN108007371A

  • Rock fracturing experimental system and experimental method

    CN108240942A

  • Rock test piece damage evolution multi-parameter combined test device and method

    CN115639343A

  • Method for simulating and dynamically monitoring expansion of T-shaped crack of reservoir interlayer

    CN115961927A

  • Unconventional rock core crustal stress prediction method and device based on acoustic emission b value

    CN118209635A

Cited By

  • Bridge crack monitoring and early warning system and method

    CN119714083A

  • Ultra-high performance concrete crack resistance testing system and dynamic monitoring method thereof

    CN120489733A

  • A system for testing the crack resistance of ultra-high performance concrete and a dynamic monitoring method thereof

    CN120489733B