Display panel, display device and preparation method of display panel
By arranging multiple retaining wall openings on the retaining wall structure of the electronic paper display panel, rapid and uniform diffusion of the plasma material is achieved, which solves the problem of poor display uniformity caused by the microcup structure hindering diffusion and improves the display effect.
Patent Information
- Application Number
- CN202411081978.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-07
- Publication Date
- 2024-10-11
AI Technical Summary
The microcup structure of electronic paper display panels hinders the diffusion of electronic ink, resulting in poor display uniformity and unsatisfactory effects.
Design a display panel that separates the plasma layer into multiple plasma units by arranging multiple retaining wall openings on the retaining wall structure. Adjacent plasma units are connected through the retaining wall openings to promote the diffusion of plasma materials.
The diffusion speed and uniformity of plasma materials are improved, and the uniformity and display effect of the display panel are improved.
Smart Images

Figure CN118759775A_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to the field of display technology, and in particular to a display panel, a display device, and a method for manufacturing a display panel. Background Art
[0002] Electronic paper display technology is a display technology that combines the advantages of traditional paper and modern digital display technology. It has low power consumption and a large display viewing angle, so it is favored by users.
[0003] Electronic paper includes plasma electronic paper, which includes a microcup structure made of optical adhesive material. The microcup structure can be filled with electronic ink, such as black and white particles, multi-color particles or monochrome particles, so as to display. This electronic mode adopts the ODF (One Drop Filling) process to drop electronic ink into the microcup structure. When the electronic ink is dropped, the amount of ink at each position is uneven. The ink will diffuse to make the ink evenly covered. However, due to the existence of the microcup structure, the diffusion of the ink will be hindered, resulting in uneven diffusion. As a result, when the display panel is displayed, the uniformity of the display panel is poor and the display effect is not ideal. Summary of the invention
[0004] In order to solve the above technical problems, the present disclosure provides a display panel, a display device and a method for manufacturing the display panel.
[0005] In a first aspect, the present disclosure provides a display panel, comprising:
[0006] A first substrate and a second substrate arranged opposite to each other;
[0007] a plasma layer, located between the first substrate and the second substrate;
[0008] A retaining wall structure is arranged between the first substrate and the second substrate, the retaining wall structure divides the plasma layer into a plurality of plasma units, and a plurality of retaining wall openings are arranged on the retaining wall structure; adjacent plasma units are connected through the retaining wall openings.
[0009] In a second aspect, a display device comprises any display panel as provided in the first aspect.
[0010] In a third aspect, a method for preparing a display panel includes:
[0011] A retaining wall structure is formed on the first substrate; the retaining wall structure is provided with a plurality of retaining wall openings;
[0012] The plasma layer is formed; the retaining wall structure divides the plasma layer into a plurality of plasma units, and adjacent plasma units are connected through the retaining wall openings;
[0013] A second substrate is arranged on a side of the retaining wall structure away from the first substrate.
[0014] Compared with the prior art, the technical solution provided by the present invention has the following advantages:
[0015] The display panel provided by the present disclosure includes a first substrate and a second substrate arranged opposite to each other; a plasma layer located between the first substrate and the second substrate; a retaining wall structure arranged between the first substrate and the second substrate, the retaining wall structure divides the plasma layer into a plurality of plasma units, and a plurality of retaining wall openings are arranged on the retaining wall structure; adjacent plasma units are connected through the retaining wall openings. Thus, a plurality of retaining wall openings are arranged on the retaining wall structure, and the plasma material in the plasma unit can flow through the retaining wall openings to the plasma unit at the adjacent or other positions, and diffuse rapidly, thereby increasing the diffusion speed of the plasma material, and can diffuse evenly to each area of the plasma unit, thereby improving the uniformity of the display panel and improving the display effect. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] The accompanying drawings, which are incorporated in and constitute a part of this specification, illustrate embodiments consistent with the present disclosure and, together with the description, serve to explain the principles of the present disclosure.
[0017] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, for ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative labor.
[0018] Figure 1 A schematic diagram of a top view structure of a display panel provided in an embodiment of the present disclosure;
[0019] Figure 2 A method for providing an embodiment of the present disclosure Figure 1 Schematic diagram of the cross-sectional structure of A1A2;
[0020] Figure 3 A method for providing an embodiment of the present disclosure Figure 1 A schematic diagram of the cross-sectional structure of A3A4;
[0021] Figure 4 A schematic diagram of a top view structure of another display panel provided in an embodiment of the present disclosure;
[0022] Figure 5 A method for providing an embodiment of the present disclosure Figure 4 Schematic diagram of the cross-sectional structure of A1A2;
[0023] Figure 6 Another embodiment of the present disclosure provides a Figure 4Schematic diagram of the cross-sectional structure of A1A2;
[0024] Figure 7 Another embodiment of the present disclosure provides a Figure 4 Schematic diagram of the cross-sectional structure of A1A2;
[0025] Figure 8 A schematic diagram of a top view structure of another display panel provided in an embodiment of the present disclosure;
[0026] Fig. 9 A schematic diagram of a top view structure of another display panel provided in an embodiment of the present disclosure;
[0027] Fig.10 A method for providing an embodiment of the present disclosure Fig. 9 A schematic diagram of the cross-sectional structure of A5A6;
[0028] Fig.11 A schematic diagram of a top view structure of another display panel provided in an embodiment of the present disclosure;
[0029] Fig.12 A schematic diagram of a top view structure of another display panel provided in an embodiment of the present disclosure;
[0030] Fig.13 A schematic diagram of a top view structure of another display panel provided in an embodiment of the present disclosure;
[0031] Fig.14 A method for providing an embodiment of the present disclosure Fig.13 A schematic diagram of the cross-sectional structure of A7A8;
[0032] Fig.15 A schematic diagram of a top view structure of another display panel provided in an embodiment of the present disclosure;
[0033] Fig.16 A schematic cross-sectional view of a display panel provided in an embodiment of the present disclosure;
[0034] Fig.17 A schematic diagram of a top view structure of another display panel provided in an embodiment of the present disclosure;
[0035] Fig.18 A method for providing an embodiment of the present disclosure Fig.17 A schematic diagram of the cross-sectional structure of A9A10;
[0036] Fig.19 A schematic diagram of the structure of a display device provided in an embodiment of the present disclosure;
[0037] Fig. 20 A schematic diagram of a process for preparing a display panel provided in an embodiment of the present disclosure;
[0038] Fig.21 A schematic diagram of a manufacturing process of a display panel provided in an embodiment of the present disclosure. DETAILED DESCRIPTION
[0039] In order to more clearly understand the above-mentioned objectives, features and advantages of the present disclosure, the scheme of the present disclosure will be further described below. It should be noted that the embodiments of the present disclosure and the features in the embodiments can be combined with each other without conflict.
[0040] In the following description, many specific details are set forth to facilitate a full understanding of the present disclosure, but the present disclosure may also be implemented in other ways different from those described herein; it is obvious that the embodiments in the specification are only part of the embodiments of the present disclosure, rather than all of the embodiments.
[0041] The electronic paper display panel includes electronic ink, for example, the electronic ink includes black and white particles. When a voltage is applied to the display panel, the black particles and white particles in the electronic ink will move to the display side and the non-display side, thereby realizing the display function. When preparing the electronic paper display panel, the ODF process is usually used to drop the electronic ink into the microcup structure on the substrate. When the electronic ink is dripped, the amount of ink at each position is uneven, and the ink will diffuse to make the ink evenly covered. However, due to the presence of the microcup structure, the diffusion of the ink will be hindered, resulting in uneven diffusion. As a result, when the display panel is displayed, the uniformity of the display panel is poor and the display effect is not ideal.
[0042] In view of the above-mentioned defects, the present disclosure provides a display panel. Figure 1 A schematic diagram of a top view of a display panel provided in an embodiment of the present disclosure is shown in FIG. Figure 2 A method for providing an embodiment of the present disclosure Figure 1 The cross-sectional structure diagram of A1A2 is shown in the figure. Figure 3 A method for providing an embodiment of the present disclosure Figure 1 A3A4 cross-sectional structure diagram, see Figure 1-Figure 3 , the display panel includes:
[0043] The first substrate 10 and the second substrate 20 are arranged opposite to each other.
[0044] The plasma layer 30 is located between the first substrate 10 and the second substrate 20 .
[0045] The retaining wall structure 40 is disposed between the first substrate 10 and the second substrate 20 . The retaining wall structure 40 divides the plasma layer 30 into a plurality of plasma units 31 . A plurality of retaining wall openings 41 are disposed on the retaining wall structure 40 . Adjacent plasma units 31 are connected through the retaining wall openings 41 .
[0046] Exemplarily, the display panel includes a first substrate 10 and a second substrate 20 that are arranged opposite to each other, for example, the first substrate 10 is an array substrate, and the second substrate is a color film substrate. The plasma layer 30 is arranged between the first substrate 10 and the second substrate 20, and the plasma layer 30 is filled with plasma materials, such as color-developing particles and solvents, wherein the color-developing particles can be white particles and black particles, or can be two-color, three-color or multi-color particles to display different colors, which can be set according to actual needs. A retaining wall structure 40 is also arranged between the first substrate 10 and the second substrate 20, and the retaining wall structure 40 divides the plasma layer 30 into a plurality of plasma units 31, and each plasma unit 31 is filled with plasma materials. The retaining wall structure 40 can be provided to isolate the plasma material, and prevent the plasma layer 30 from accumulating in a certain area without obstruction, resulting in uneven distribution of plasma materials in different areas of the display panel, affecting the uniformity of the display panel. The plasma layer 30 is divided into a plurality of plasma units 31 by the retaining wall structure 40, which can block the flow of plasma materials in adjacent plasma units 31 to a certain extent and prevent the accumulation of plasma materials. However, the retaining wall structure 40 is completely closed, which also makes it impossible for the plasma materials in adjacent plasma units 31 to flow to each other. When the plasma material is dripped into each plasma unit 31, the dripping amount cannot be evenly distributed, which easily leads to too much or too little plasma material in a plasma unit 31, and there will also be uneven distribution problems, which affects the uniformity of the display panel.
[0047] Based on this, a plurality of retaining wall openings 41 are provided on the retaining wall structure 40, and adjacent plasma units 31 are connected through the retaining wall openings 41, and the plasma material in the adjacent plasma units 31 can flow through the retaining wall openings 41 and diffuse to the plasma units 31 at different other positions, thereby increasing the diffusion rate of the plasma material. However, the size of the retaining wall openings 41 is limited, and the adjacent plasma units 31 are not completely connected, but the positions of the retaining wall openings 41 allow the plasma material to flow, so that the plasma material will not be completely accumulated in a certain area, and the plasma material in different areas of the display panel can be evenly distributed, thereby improving the uniformity of the display panel.
[0048] refer to Figure 1-Figure 3 , a partial structure of a display panel is provided, wherein a plasma layer 30 includes four plasma units 31, a retaining wall structure 40 is provided between adjacent plasma units 31, and a retaining wall opening 41 is provided on the retaining wall structure 40, adjacent plasma units 31 are connected through the retaining wall opening 41, and plasma materials can flow to different plasma units 31 through the retaining wall opening 41, so that the plasma materials are evenly distributed. Wherein, D1 is a first direction, D2 is a second direction, and the first direction intersects with the second direction. Figure 1 The plasma unit 31 is actually filled with plasma material, and the color-developing particles in the plasma material include black particles and white particles. Figure 1 Not shown, please refer to Figure 3When a voltage is applied to the display panel, the black particles and white particles of the plasma layer 30 will move in the direction of different substrates. The voltage is different, and the black particles and white particles move in different directions, thereby displaying different colors. In some other embodiments, the color-developing particles can also be other colors, and the embodiments disclosed herein are only used as examples.
[0049] In the disclosed embodiment, a plurality of baffle openings are provided on the baffle structure, so that the plasma material in the plasma unit can flow through the baffle openings to the plasma units at adjacent or other locations and diffuse rapidly, thereby increasing the diffusion speed of the plasma material and being able to diffuse evenly to various areas of the plasma unit, thereby improving the uniformity of the display panel and enhancing the display effect.
[0050] In some embodiments, continue to refer to Figure 1-Figure 3 , the side of the second substrate 20 facing away from the first substrate 10 is the light emitting side;
[0051] Along a direction perpendicular to the second substrate 20 , a partial thickness of the barrier wall structure 40 is provided between the second substrate 20 and the barrier wall opening 41 .
[0052] Exemplarily, the side of the second substrate 20 facing away from the first substrate 10 is the light-emitting side, from which light is emitted to the outside. Continuing with the example that the color-developing particles in the plasma material include black particles and white particles, a voltage is applied to the display panel to control the adjacent plasma units 31 to display different colors under the action of the voltage. For example, if one plasma unit 31 displays white, the white particles in the plasma unit 31 will move toward the light-emitting side, while the other plasma unit 31 displays black, and the black particles in the plasma unit 31 will move toward the light-emitting side. Since the two plasma units 31 are adjacent, the particles at the junction are affected by the voltages on both sides, and the particles of each color will crosstalk with each other. Therefore, the color displayed at the junction may be the color displayed after the black particles and the white particles are mixed, which will affect the display effect. Therefore, in the direction perpendicular to the second substrate 20, there is a partial thickness of the retaining wall structure 40 between the second substrate 20 and the retaining wall opening 41, that is, Figure 2 The retaining wall structure 40 of the middle length L1 is provided with the region of the retaining wall opening 41, and the retaining wall structure 40 is not completely hollowed out. Even if display particles of different colors are mixed at the retaining wall opening 41, there is still a portion of the thickness of the retaining wall structure 40 on the side of the retaining wall opening 41 close to the light-emitting side, so the region where the retaining wall opening 41 is located will not display color, and will not affect the display effect of the display panel.
[0053] In some embodiments, Figure 4 A schematic diagram of a top view of another display panel provided in an embodiment of the present disclosure is shown. Figure 5 A method for providing an embodiment of the present disclosure Figure 4 Schematic diagram of the cross-section structure of A1A2, see Figure 4 and Figure 5 Along the extending direction of the retaining wall structure 40 , the retaining wall structure 40 between adjacent plasma units 31 is provided with a plurality of retaining wall openings 41 .
[0054] For example Figure 4 , four plasma units 31 are provided, namely plasma unit 311, plasma unit 312, plasma unit 313 and plasma unit 314, a retaining wall structure 40 is provided between adjacent plasma units 311 and 313, and a retaining wall structure 40 is provided between adjacent plasma units 312 and 314, wherein the D1 direction is the first direction, the D2 direction is the second direction, and the A1A2 extension direction is the extension direction (D1 direction) of the retaining wall structure 40 in this area. Along the extension direction of the retaining wall structure 40, a plurality of retaining wall openings 41 are provided on the retaining wall structure 40 between adjacent plasma units 31, for example, five retaining wall openings 41 are provided on the retaining wall structure 40 between the plasma unit 311 and the plasma unit 313, and five retaining wall openings 41 are also provided on the retaining wall structure 40 between the plasma unit 312 and the plasma unit 314. After multiple retaining wall openings 41 are provided, the number of retaining wall openings 41 through which the plasma material can flow between adjacent plasma units 31 increases, and the distribution range of the retaining wall openings 41 on the retaining wall structure 40 is wider, thereby increasing the flow rate of the plasma material. In addition, the plasma material can be diffused to different areas of the plasma unit 31, and the diffusion is more uniform, further improving the uniformity of the display panel and improving the display effect.
[0055] It should be noted that the embodiment of the present disclosure does not impose any specific limitation on the number of the retaining wall openings 41 , and the number may be one, two, three or more, and may be set according to actual needs. The above embodiment is only for illustration.
[0056] In some embodiments, Figure 6 Another embodiment of the present disclosure provides a Figure 4 Schematic diagram of the cross-section structure of A1A2, see Figure 6 Combined with Figure 4 Along the extending direction of the retaining wall structure 40 , the number density of the retaining wall openings 41 of the retaining wall structure 40 between adjacent plasma units 31 gradually decreases from the middle area to the edge area.
[0057] Considering that when preparing a display panel, the plasma layer needs to be filled with plasma material, and the plasma material is usually dripped into the plasma layer, and when the droplets fall, the plasma content in the middle area of the plasma unit 31 is higher, and the plasma content in the edge area is lower. Therefore, in order to quickly diffuse the plasma material to the surroundings, along the extension direction of the retaining wall structure 40, the number density of the retaining wall openings 41 of the retaining wall structure 40 between adjacent plasma units 31 gradually decreases from the middle area to the edge area.
[0058] Exemplarily, a plurality of baffle openings 41 are provided on the baffle structure 40 between adjacent plasma units 311 and 313, and the number density of the baffle openings 41 gradually decreases from the middle area to the edge area, that is, the number of baffle openings 41 located in the middle of the baffle structure 40 is large, and the number of baffle openings 41 located on both sides is small. Similarly, a plurality of baffle openings 41 are provided on the baffle structure 40 between adjacent plasma units 312 and 314, and the number density of the baffle openings 41 gradually decreases from the middle area to the edge area. The extension direction of A1A2 is the extension direction of the baffle structure 40 in this area. Based on this structure, the plasma material in the plasma unit 31 can quickly flow in different directions through the plurality of baffle openings 41 and diffuse evenly to improve the uniformity of the display panel.
[0059] It should be noted that the embodiments of the present disclosure do not limit the specific number density of the retaining wall openings on the retaining wall structure, which can be set according to actual needs, and the above embodiments are only used as examples.
[0060] In some embodiments, Figure 7 Another embodiment of the present disclosure provides a Figure 4 Schematic diagram of the cross-section structure of A1A2, see Figure 7 Combined with Figure 4 Along the extending direction of the retaining wall structure 40 , the length of each retaining wall opening 41 of the retaining wall structure 40 between adjacent plasma units 31 gradually decreases from the middle area to the edge area.
[0061] The lengths of the retaining wall openings 41 on adjacent retaining wall structures 40 are different, and the flow speeds of the plasma material between adjacent plasma units 31 will also be different. When the plasma material is dripped into the plasma layer, the plasma content in the middle area of the plasma unit 31 is higher, and that in the edge area is lower. Therefore, in order to allow the plasma material to diffuse quickly to the surroundings, the length of the retaining wall openings 41 of the retaining wall structure 40 between adjacent plasma units 31 gradually decreases from the middle area to the edge area along the extension direction of the retaining wall structure 40.
[0062] Exemplarily, a plurality of baffle openings 41 are provided on the baffle structure 40 between adjacent plasma units 311 and plasma units 313, and the length of the baffle openings 41 gradually decreases from the middle area to the edge area, for example, the length of the baffle opening 41 in the middle area is x1, and the lengths of the baffle openings 41 from the middle area to the edge areas on both sides are x2 and x3, respectively, wherein x1>x2>x3. The length of the baffle opening 41 in the middle area is the longest, and when the heights of the baffle openings 41 are the same, it is equivalent to increasing the opening area of the baffle opening 41 in the middle area, thereby increasing the flow rate of the plasma material here, thereby accelerating the diffusion speed of the plasma material to the surroundings, and evenly covering the plasma units 31, thereby improving the uniformity of the display panel.
[0063] It should be noted that the disclosed embodiment does not impose any specific restrictions on the length of the baffle opening on the baffle structure, but it cannot be too long. If the baffle opening is too long, the baffle structure cannot effectively separate the plasma units, and the uniformity of the display panel will also be affected. In addition, the baffle structure and the baffle opening are obtained by developing and exposing the light glue layer. If the baffle opening is too long, it is easy to cause the material to fail to be fully developed, affecting the formation of the baffle opening. Therefore, the length of the baffle opening can be set according to actual needs.
[0064] In some optional embodiments, along the extension direction of the retaining wall, the opening area of each retaining wall of the retaining wall structure between adjacent plasma units gradually decreases from the middle area to the edge area. The larger the opening area, the greater the flow rate, so the flow of plasma materials from the middle area to the adjacent plasma units can be accelerated. However, considering the actual application, the opening area of the retaining wall cannot be infinite, otherwise the plasma layer cannot be separated. Therefore, the opening area of the retaining wall can be set according to actual needs. The opening area of the retaining wall is affected by the length and height, so the length and height of the retaining wall opening can be adjusted according to the needs to change the flow rate of the retaining wall opening.
[0065] In some embodiments, Figure 8 A schematic diagram of a top view structure of another display panel provided in an embodiment of the present disclosure, referring to Figure 8 The number of retaining wall openings on the retaining wall structure 40 extending along the first direction D1 is less than the number of retaining wall openings on the retaining wall structure 40 extending along the second direction D3. The first direction D1 intersects with the second direction D2, and the second direction D2 is parallel to the gravity direction.
[0066] Exemplarily, retaining wall structures 40 are provided in the direction extending along the first direction D1 and in the direction extending along the second direction D2 , and the retaining wall structures 40 provided in different directions are interconnected to form a closed loop structure, thereby separating the plasma layer into a plurality of plasma units 31 . Figure 8 Schematic diagram of the top view of the display panel. In actual application scenarios, the direction of the display panel will change. When the display panel is usually used, the second direction D2 of the display panel will be parallel to the gravity direction, and the first direction D1 intersects the second direction D2. Under the influence of gravity, the plasma material in each plasma unit 31 will accelerate the flow speed in the direction of gravity, and the plasma material can also diffuse to adjacent plasma units 31, thereby increasing the uniformity of the display panel.
[0067] However, gravity will also cause most of the plasma material to flow rapidly in the direction of gravity, resulting in the accumulation of plasma material. In order to avoid this problem, the number of baffle openings in the first direction D1 can be adjusted. Since the plasma material will pass through the baffle openings 41 on the baffle structure 40 extending along the first direction D1 when it flows under the influence of gravity, the speed of the plasma material flowing in the direction of gravity can be slowed down by reducing the number of baffle openings in the first direction D1. The number of baffle openings on the baffle structure 40 extending along the first direction D1 is made smaller than the number of baffle openings on the baffle structure 40 extending along the second direction D3, so as to balance the diffusion speed of the plasma material in different directions, so as to achieve the purpose of uniform diffusion and improve the uniformity of the display panel.
[0068] It should be noted that the embodiment of the present disclosure does not impose any specific restriction on the number of retaining wall openings on the retaining wall structure extending in different directions, and the design can be selected according to different products and different needs.
[0069] In some embodiments, Fig. 9 A schematic diagram of a top view of another display panel provided in an embodiment of the present disclosure is shown. Fig.10 A method for providing an embodiment of the present disclosure Fig. 9 A5A6 cross-sectional structure diagram, reference Fig. 9 and Fig.10 A connecting portion 42 is provided between the retaining wall structure 40 extending along the first direction D1 and the retaining wall structure 40 extending along the second direction D2; the area of the retaining wall opening 41 close to the connecting portion 42 is smaller than the area of the retaining wall opening 41 away from the connecting portion 42.
[0070] The retaining wall structure 40 is arranged in the direction extending along the first direction D1 and the direction extending along the second direction D2. A connecting portion 42 is arranged between the retaining wall structure 40 extending along the first direction D1 and the retaining wall structure 40 extending along the second direction, so that the retaining wall structures 40 extending in different directions are connected to each other to form a closed structure, and the plasma layer is divided into a plurality of plasma units 31. The connecting portion is mostly a corner structure. The retaining wall structure 40 needs to support the second substrate 20. The connecting portion 42 is the main load-bearing area and is subjected to greater force. Therefore, the area of the retaining wall opening 41 close to the connecting portion 42 should be reduced to ensure that the connecting portion 42 will not be damaged due to the larger opening area of the surrounding retaining wall structure 40, to ensure that its supporting function is not affected by the retaining wall opening 41, and the connecting portion 42 will not be damaged. The area of the retaining wall opening 41 away from the connecting portion 42 can be larger than the area of the retaining wall opening 41 close to the connecting portion 42 to increase the flow rate of the plasma material. For example, the area of the retaining wall opening 41 far from the connecting portion 42 is S1, and the area of the retaining wall opening 41 close to the connecting portion 42 is S2, wherein S1>S2.
[0071] In some embodiments, continue to refer to Fig. 9 The connection portion 42 formed by the retaining wall structure 40 between the staggered plasma units 31 is provided with a retaining wall opening 41 .
[0072] For example, Fig. 9 Four plasma units 31 are provided, namely plasma unit 311, plasma unit 312, plasma unit 313 and plasma unit 314, wherein plasma unit 311 is adjacent to plasma unit 312 and plasma unit 314, respectively, plasma unit 312 is adjacent to plasma unit 313, and plasma unit 313 is adjacent to plasma unit 314, and a retaining wall opening 41 is provided between adjacent plasma units 31, and plasma material can flow between adjacent plasma units 312 through the retaining wall opening 41. The plasma units 311 and the plasma units 314 are located in different rows and columns and are arranged in a staggered relationship. There are also connecting parts 42 formed by retaining wall structures 40 extending in different directions between the staggered plasma units 31. Retaining wall openings 41 can be provided on the connecting parts 42 between the plasma units 311 and the plasma units 31, so that the plasma material can also flow between the staggered plasma units 31, thereby increasing the diffusion speed of the electrode material to different regions and making it diffuse evenly in all directions, so as to improve the uniformity of the display panel.
[0073] In some embodiments, continue to refer to Figure 2 , along the direction perpendicular to the first substrate 10 , the height of the blocking wall opening 41 is 20%-60% of the height of the blocking wall structure 40 .
[0074] Exemplarily, the first substrate 10 is parallel to the second substrate 20, and there is a partially thick barrier wall structure 40 between the second substrate 20 and the barrier wall opening 41 in a direction perpendicular to the first substrate 10, so as to prevent the plasma materials between adjacent plasma units 31 from crosstalking with each other at the junction, interfering with the display, and supporting the second substrate 20. Therefore, the height of the barrier wall opening 41 below this part of the barrier wall structure 40 cannot be too high, so as to prevent the barrier wall structure 40 on the side of the barrier wall opening 41 close to the second substrate 20 from being too thin and unable to support the second substrate 20. The barrier wall opening 41 cannot be too small either. If the opening is too small, the flow speed of the plasma material will be limited, the flow effect will be poor, and the plasma material cannot flow quickly to the adjacent plasma units 31, affecting the uniform diffusion of the plasma material. Considering the supporting role of the barrier wall structure 40 and the role of the barrier wall opening in accelerating the flow of the plasma material, the height of the barrier wall opening 41 in the direction perpendicular to the first substrate 10 is 20%-60% of the height of the barrier wall structure 40, so as to take into account the above requirements. For example, along the direction perpendicular to the first substrate 10, the height of the retaining wall structure 40 with a partial thickness between the second substrate 20 and the retaining wall opening 41 is L1, the height of the retaining wall opening 41 is L2, the height of the retaining wall structure 40 is L3, and 20% L3≤L2≤60% L3. If the height L1 of the plasma unit 31 is 10-30 μm, the height L2 of the retaining wall opening 41 can be 3-5 μm to meet the demand for rapid circulation of plasma materials without affecting the supporting function of the retaining wall structure 40.
[0075] In other embodiments, the height of the retaining wall opening may also be other values, which can be selected according to actual needs. The embodiments of the present disclosure do not impose specific limitations on this. The above embodiment is only an optional implementation method.
[0076] In some embodiments, continue to refer to Figure 1 and Figure 2 Along the extending direction of the retaining wall structure 40 , the length of the retaining wall opening 41 is 3%-10% of the length of the retaining wall structure 40 .
[0077] Exemplarily, the extension direction of A1A2 is the extension direction of the retaining wall structure 40 in the region, that is, it extends along the first direction D1. The retaining wall structure 40 is used to support the second substrate 20. If the length of the retaining wall opening 41 is too long, the supporting function of the retaining wall structure 40 will be affected, and if the retaining wall opening is too short, the flow effect of the plasma material is poor, which affects the uniform diffusion of the plasma material. Therefore, the length D1 of the retaining wall opening 41 should be 3%-10% of the length D2 of the retaining wall structure 40, that is, 3%D2≤D1≤10%D2. For example, the size of the plasma unit 31 is 100μm*100μm, the length D2 of the retaining wall structure 40 corresponding to the plasma unit 31 is 100μm, and the length D1 of the retaining wall opening 41 is 3-10μm.
[0078] Optionally, there is a partial thickness of the retaining wall structure 40 between the second substrate 20 and the retaining wall opening 41, which can prevent the plasma materials between adjacent plasma units 31 from crosstalking at the junction and interfering with the display, and play a role in supporting the second substrate 20. If the length of the retaining wall opening 41 is too long, the retaining wall structure 40 on the side of the retaining wall opening 41 close to the second substrate 20 has a poor load-bearing capacity and is easily damaged. Therefore, the length of the retaining wall opening 41 should be avoided to be too long, which affects the supporting effect of the retaining wall structure 40. Similarly, the length of the retaining wall opening 41 should be avoided to be too short, which leads to poor flow effect of the plasma material.
[0079] In other embodiments, the length of the retaining wall opening may also be other values, which can be selected according to actual needs. The embodiments of the present disclosure do not impose specific limitations on this, and the above embodiment is only an optional implementation method.
[0080] In some embodiments, Fig.11 A schematic diagram of a top view structure of another display panel provided in an embodiment of the present disclosure, referring to Fig.11 In a direction parallel to the first substrate 10 and perpendicular to the extending direction of the retaining wall structure 40 , the retaining wall openings 41 of adjacent retaining wall structures 40 arranged in parallel at least partially overlap.
[0081] For example, Fig.11 The present invention comprises four plasma units 31, namely, plasma unit 311, plasma unit 312, plasma unit 313 and plasma unit 314. Taking the retaining wall structure 40 whose extension direction is the second direction D2 as an example, in the extension direction parallel to the first substrate 10 and perpendicular to the retaining wall structure 40, the retaining wall openings 41 of the adjacent retaining wall structures 40 arranged in parallel are retaining wall openings 411 and retaining wall openings 412 respectively. In the first direction D1, the retaining wall openings 411 and the retaining wall openings 412 at least partially overlap, and the overlapping part is equivalent to direct communication, so that the plasma material between the plasma unit 311 and the plasma unit 312 can directly convect, reducing the path of the plasma material flow and increasing the circulation speed of the plasma material. By adjusting the overlapping area of the retaining wall openings 41 of the adjacent retaining wall structures 40 arranged in parallel, the speed of the plasma flow between the adjacent plasma units 31 can be changed.
[0082] Optional, reference Figure 4 In the direction parallel to the first substrate 10 and perpendicular to the extending direction of the retaining wall structure 40, the retaining wall openings 41 of the adjacent retaining wall structures 40 arranged in parallel completely overlap, the area of direct conduction between the plasma unit 311 and the plasma unit 312 is increased, the area of direct convection of the plasma material is increased, and the flow speed of the plasma material is faster.
[0083] In some embodiments, Fig.12 A schematic diagram of a top view structure of another display panel provided in an embodiment of the present disclosure, referring to Fig.12In a direction parallel to the first substrate 10 and perpendicular to the extending direction of the retaining wall structure 40 , the retaining wall openings 41 of adjacent retaining wall structures 40 arranged in parallel do not overlap.
[0084] For example, Fig.11 The present invention comprises four plasma units 11, namely, plasma unit 311, plasma unit 312, plasma unit 313 and plasma unit 314. Continuing to take the retaining wall structure 40 whose extension direction is the second direction D2 as an example, in the extension direction parallel to the first substrate 10 and perpendicular to the retaining wall structure 40, the retaining wall openings 41 of the adjacent retaining wall structures 40 arranged in parallel are retaining wall openings 411 and retaining wall openings 412 respectively. In the first direction D1, the retaining wall openings 411 and the retaining wall openings 412 do not overlap, which can slow down the speed of plasma flow between adjacent plasma units 31 to a certain extent to meet the current demand. The retaining wall openings 41 of the adjacent retaining wall structures 40 arranged in parallel do not overlap, and the path required for the plasma materials to flow between adjacent plasma units 31 becomes longer, and the time required also increases, so the flow speed of the plasma materials between the plasma unit 311 and the plasma unit 312 can be slowed down.
[0085] It should be noted that the above embodiment does not restrict whether the retaining wall openings of adjacent retaining wall structures arranged in parallel overlap or the size of the overlapping area, which can be selected according to actual needs, and there is no restriction on the specific shape of the retaining wall openings, such as square, trapezoidal, etc., which can be selected according to actual needs and process capabilities.
[0086] In addition, the flow rate of the plasma material is related to many factors such as the shape of the retaining wall structure, the size of the retaining wall opening, the type of plasma material, etc. The specific diffusion rate is optimal and needs to be considered and selected based on actual needs.
[0087] In some embodiments, Fig.13 A schematic diagram of a top view of another display panel provided in an embodiment of the present disclosure is shown. Fig.14 A method for providing an embodiment of the present disclosure Fig.13 A7A8 cross-sectional structure diagram, see Fig.13 and Fig.14 The display panel further includes a shielding structure 50. In a direction parallel to the first substrate 10 and perpendicular to the extending direction of the barrier wall structure 40, the shielding structure 50 at least partially overlaps with the barrier wall opening 41.
[0088] For example, taking the retaining wall structure 40 extending in the second direction D2 as an example, a shielding structure 50 is provided in the extending direction parallel to the first substrate 10 and perpendicular to the retaining wall structure 40, that is, a shielding structure 50 is provided in the first direction D1. The shielding structure 50 at least partially overlaps with the retaining wall opening 41 adjacent to it, and the shielding structure 50 can hinder the free movement of the plasma material, reduce its flow speed, and prevent the display panel from being affected by gravity during use, and the plasma material quickly diffuses in the direction of gravity, resulting in uneven distribution of the electrode material, affecting the uniformity of the display panel. After the shielding structure 50 at least partially overlaps with the retaining wall opening 41, the area of the retaining wall opening 41 directly connected between the adjacent plasma units 31 can be reduced, and part of the plasma material needs to bypass the shielding structure 50 to pass through the retaining wall opening 41, thereby slowing down the flow speed of the plasma material and avoiding its uneven distribution.
[0089] In some optional embodiments, the shielding structure and the baffle opening may overlap completely or only partially. The embodiment of the present disclosure does not limit the overlapping area and can be designed according to actual needs. The shielding structure can be prepared by optical glue, and the specific material can also be selected according to actual needs. The thinner the shielding structure is, the smaller the impact on the display effect of the display panel is. The length of the shielding structure can be selected according to needs. The length can be greater than the baffle opening, or less than the baffle opening. The difference is that the flow rate of the plasma material is different, which can be selected according to actual needs.
[0090] In some embodiments, Fig.15 A schematic diagram of a top view structure of another display panel provided in an embodiment of the present disclosure, referring to Fig.15 Along the extending direction of the retaining wall structure 40 , the overlapping area between the shielding structure 50 and the retaining wall opening 41 gradually decreases from the middle area to the edge area of the retaining wall structure 40 .
[0091] For example, taking the retaining wall structure 40 extending in the second direction D2 as an example, a shielding structure 50 is provided in the extending direction parallel to the first substrate 10 and perpendicular to the retaining wall structure 40, that is, a shielding structure 50 is provided in the first direction D1. The plasma material in the middle area of the plasma unit 31 is more and diffuses faster, while the plasma material in the edge area is less and diffuses slower, resulting in different diffusion speeds of the plasma material in each area, which affects the display of the display panel. The overlapping area between the shielding structure 50 and the retaining wall opening 41 is different, and the diffusion speed of the plasma material between adjacent plasma units 31 will also be different. Therefore, the overlapping area between the shielding structure 50 and the retaining wall opening can be adjusted to make the diffusion speed of the plasma material in each area closer and diffuse evenly into the adjacent plasma material. Thus, the overlapping area between the shielding structure 50 and the retaining wall opening 41 can be gradually reduced from the middle area to the edge area of the retaining wall structure 40, thereby reducing the diffusion rate of the plasma material in the middle area and increasing the diffusion rate of the plasma material in the edge area, making the diffusion rates of the plasma materials in different areas closer and the diffusion more uniform.
[0092] In some embodiments, the plasma layer includes a solvent and color-developing particles.
[0093] The distance between adjacent retaining wall openings and shielding structures is 5 to 10 times the diameter of the color-developing particles.
[0094] The plasma layer is filled with plasma material, and the plasma material includes solvent and display particles. The color particles can be monochrome particles, two-color particles or multiple particles. When the plasma material flows in adjacent plasma units, the solvent and the color particles will diffuse to the adjacent plasma units through the baffle openings together, wherein the solvent is a liquid and the color particles are spheres. When there is a shielding structure and the distance between the shielding structure and the baffle opening is close, the color particles may not be able to pass through the baffle opening. If the distance between the shielding structure and the baffle opening is far, the shielding structure cannot play a role in slowing down the flow rate of the color particles (plasma material). Therefore, it is necessary to limit the distance between the adjacent baffle openings and the shielding structure, for example, setting the distance to 5 to 10 times the diameter of the color particles. Within this distance, the color particles can flow into the baffle opening, and the shielding structure can play a shielding role, reducing the flow rate of the plasma material.
[0095] It should be noted that the embodiments of the present disclosure do not impose any restrictions on the specific structure, size, material, etc. of the color-developing particles, nor do they limit the specific distance between the shielding structure and the retaining wall opening, which can be selected according to actual needs.
[0096] In some embodiments, Fig.16 A cross-sectional schematic diagram of a display panel provided in an embodiment of the present disclosure, referring to Fig.16 , the first substrate 10 is an array substrate.
[0097] A pixel electrode layer 60 is disposed on one side of the array substrate facing the second substrate 20. The pixel electrode layer 60 includes a plurality of pixel electrodes 61 arranged in an array; there are gaps between adjacent pixel electrodes 61, and the retaining wall structure 40 is disposed in the gap region.
[0098] Exemplarily, the first substrate 10 is an array substrate, and the array substrate can be set as a thin film transistor array substrate, in which a plurality of thin film transistors are arranged, wherein the film layer structure of the thin film transistor can be set according to actual needs. The second substrate 20 can be a glass substrate. Among them, a pixel electrode layer 60 is arranged on the side of the array substrate facing the second substrate 20, and a retaining wall structure 40 is arranged on the side of the pixel electrode layer 60 facing the second substrate 20. The pixel definition layer 60 includes a plurality of pixel electrodes 61 arranged in an array, and there is a gap between adjacent pixel electrodes 61, and the retaining wall structure 40 is arranged in the gap area. The display panel also includes a plurality of sub-pixels arranged in an array, and the pixel electrode 61 corresponds to the sub-pixel one by one, so that by transmitting different voltage values to the pixel electrode 61, the movement of the color-developing particles in the plasma unit 31 within the sub-pixel range is controlled to realize the display function. The retaining wall structure 40 is arranged in the gap area of the pixel electrode 61, so as to avoid the retaining wall structure 40 from blocking the sub-pixel and the pixel electrode 61, so as to ensure that the display of the display panel is clear and complete.
[0099] In addition, refer to Figure 3 , four plasma units 31 are provided, each of which is provided with a retaining wall structure 40 extending along the first direction D1 and a retaining wall structure 40 extending along the second direction D2. Each plasma unit 31 may correspond to one pixel electrode and one sub-pixel; or each plasma unit 31 may correspond to multiple pixel electrodes and sub-pixels, for example, one plasma unit 31 includes two pixel electrodes and two sub-pixels, which may be set according to actual needs.
[0100] Optionally, the pixel electrode layer includes a plurality of pixel electrode groups, each of which includes a plurality of pixel electrodes. Along a direction perpendicular to the thickness of the array substrate, the projection of the pixel electrode group covers the projection of the plurality of plasma units. The retaining wall structure between adjacent plasma units corresponding to the pixel electrode group is provided with a retaining wall opening; the retaining wall structure between adjacent plasma units between different pixel electrode groups is not provided with a retaining wall opening.
[0101] For example, Fig.17 A schematic diagram of a top view of another display panel provided in an embodiment of the present disclosure is shown. Fig.18 A method for providing an embodiment of the present disclosure Fig.17 The cross-sectional structure diagram of A9A10, see Fig.17 and Fig.18, the pixel electrode group 610 includes a plurality of pixel electrodes 61. For example, each pixel electrode group 610 in the figure includes four pixel electrodes 61 ( Fig.16 The pixel electrode 61 is not shown in the figure. In the direction perpendicular to the thickness of the array substrate, the projection of the pixel electrode group 610 covers the projection of multiple plasma units 31. Among them, the retaining wall structure 40 between the adjacent plasma units 31 corresponding to the pixel electrode group 610 is provided with a retaining wall opening 41, and the retaining wall structure 40 of the adjacent plasma units 31 between different pixel electrode groups 610 is not provided with a retaining wall opening 41. Taking the pixel electrode group 611 and the pixel electrode group 612 as examples, the two are adjacent electrode groups 610, and each group includes 4 pixel electrodes 61. Among them, the adjacent plasma units corresponding to the pixel electrode group 611 include the plasma unit 3151 and the plasma unit 3152, and the retaining wall structure 40 between the plasma unit 3151 and the plasma unit 3152 is provided with a retaining wall opening 41. The pixel electrode group 611 and the pixel electrode group 612 are different pixel electrode groups 610, and the plasma unit 3152 corresponding to the pixel electrode group 611 and the plasma unit 3161 corresponding to the pixel electrode group 612 are adjacent plasma units 31, but the plasma unit 3152 and the plasma unit 3161 are located in different groups, and the retaining wall structure 40 therebetween is not provided with a retaining wall opening 41. Therefore, the plasma material can flow in each plasma unit corresponding to the same pixel electrode group.
[0102] It should be noted that the disclosed embodiment does not impose any specific restrictions on the number and position of the openings, and the plasma material flow rate can be adjusted according to actual needs to make the plasma material evenly diffuse to each area to ensure the uniformity of the display panel. In addition, there is no restriction on the number of plasma units corresponding to the pixel electrode group, that is, there is no restriction on the number of plasma units corresponding to the sub-pixels.
[0103] The present disclosure also provides a display device, Fig.19 A schematic diagram of a display device provided in an embodiment of the present disclosure is shown in FIG. Fig.19 As shown, the display device may include the display panel of any one of the above display panel embodiments.
[0104] The display device provided by the embodiment of the present disclosure may include the display panel in the above embodiment, and thus can achieve the same or at least similar technical effects as the above display panel embodiment, which will not be described in detail herein.
[0105] The present disclosure also provides a method for preparing a display panel. Fig. 20 A schematic diagram of a method for preparing a display panel provided in an embodiment of the present disclosure is shown in FIG. Fig. 20 As shown, and refer to Figures 1 to 3 , the preparation method comprises:
[0106] S110 , forming a retaining wall structure 40 on the first substrate 10 ; a plurality of retaining wall openings 41 are disposed on the retaining wall structure 40 .
[0107] First, a first substrate 10 is provided. The first substrate 10 may be an array substrate. A retaining wall structure 40 is formed on the array substrate, and retaining wall openings 41 are provided on the retaining wall structure 40. The retaining wall structure 40 may be made of optical adhesive. The number and position of the retaining wall openings 41 may be selected according to actual needs.
[0108] S120 , forming a plasma layer 30 ; the retaining wall structure 40 divides the plasma layer 30 into a plurality of plasma units 31 , and adjacent plasma units 31 are connected through the retaining wall openings 41 .
[0109] A plasma layer 30 is formed on the side of the first substrate 10 where the retaining wall structure 40 is provided. The plasma layer 30 is filled with plasma materials, such as color-developing particles and solvents. The color-developing particles can be single-color particles, such as white particles and black particles. The present disclosure is explained with this type of particles. In other embodiments, particles of other colors, or two-color, three-color, and multi-color particles can also be used.
[0110] The retaining wall structure 40 separates the plasma layer 30 into a plurality of plasma units 31, preventing the plasma layer 30 from accumulating in a certain area without obstruction, resulting in uneven distribution of plasma materials in different areas of the display panel, affecting the uniformity of the display panel. However, the retaining wall structure 40 is completely closed, which also causes the plasma materials in adjacent plasma units 31 to be unable to circulate with each other. When the plasma material is dripped into each plasma unit 31, the dripping amount cannot be evenly distributed, which can easily lead to too much or too little plasma material in a certain plasma unit 31, and there will also be uneven distribution, affecting the display. Therefore, the plasma material can flow between adjacent plasma units 31 through the retaining wall opening 41 and diffuse evenly.
[0111] S130 , disposing a second substrate 20 on a side of the retaining wall structure 40 away from the first substrate 10 .
[0112] The second substrate 20 is located on a side of the retaining wall structure 40 away from the first substrate 10. The retaining wall structure 40 supports the second substrate 20 to facilitate the flow of plasma materials in the plasma layer 30. The second substrate 20 may be a color filter substrate.
[0113] In the display panel prepared by the method provided in the embodiment of the present disclosure, a plurality of baffle openings are provided on the baffle structure, so that the plasma material in the plasma unit can flow through the baffle openings to the plasma units at adjacent or other locations and diffuse rapidly, thereby increasing the diffusion speed of the plasma material and being able to diffuse evenly to various areas of the plasma unit, thereby improving the uniformity of the display panel and improving the display effect.
[0114] In some embodiments, Fig.21 A schematic diagram of a manufacturing process of a display panel provided in an embodiment of the present disclosure, referring to Fig.21 , forming a retaining wall structure on the first substrate; a plurality of retaining wall openings are provided on the retaining wall structure, including:
[0115] A positive optical adhesive layer is formed on the first substrate.
[0116] The positive optical adhesive layer is exposed and developed to form a positive optical adhesive layer pattern corresponding to a plurality of retaining wall openings.
[0117] A negative optical adhesive layer is formed; the negative optical adhesive layer covers the positive optical adhesive layer pattern and the first substrate.
[0118] The positive optical adhesive layer pattern is removed by exposure and development, so that a plurality of retaining wall openings are arranged on the retaining wall structure.
[0119] Exemplarily, first, a positive optical adhesive layer needs to be formed on the first substrate, and the positive optical adhesive layer is coated on the entire first substrate, wherein the position where the positive optical adhesive layer receives light can be washed away by a developer, so the position where the baffle opening needs to be set can be retained, and other positions are exposed and developed, and the positive optical adhesive layer is exposed and developed to form a positive optical adhesive layer pattern corresponding to a plurality of baffle openings. Continue to form a negative optical adhesive layer, and the negative optical adhesive layer covers the positive optical adhesive layer pattern and the first substrate, wherein the position where the negative optical adhesive layer does not receive light can be washed away by a developer. Expose and develop again to form a baffle structure, and at the same time, light will pass through the negative optical adhesive layer and irradiate the position where the retained positive optical adhesive layer is located. At this time, the positive optical adhesive layer is exposed, and the exposure and development remove the positive optical adhesive layer pattern, so that a plurality of baffle openings are set on the baffle structure. In addition, a post-baking process can also be performed to solidify the retained negative optical adhesive layer to obtain a baffle structure, and a structure with a baffle opening on the side facing the first substrate. The specific material of the light adhesive layer can be selected according to actual needs, and the illumination and development materials can adopt the same conditions.
[0120] A plurality of retaining wall openings are provided on the retaining wall structure, and adjacent plasma units are connected through the retaining wall openings. The plasma material in the adjacent plasma units can flow through the retaining wall openings and diffuse to the plasma units 31 at different other positions, thereby increasing the diffusion speed of the plasma material and preventing the retaining wall structure from blocking the diffusion of the plasma material, so that the plasma material in different areas of the display panel is evenly distributed, thereby improving the uniformity of the display panel.
[0121] In some embodiments, it also includes:
[0122] A shielding structure is formed on the first substrate; in a direction parallel to the first substrate and perpendicular to the extending direction of the shielding wall structure, the shielding structure and the shielding wall opening at least partially overlap.
[0123] A shielding structure may also be formed on the first substrate, and the flow rate of the plasma material may be adjusted by setting the shielding structure to avoid excessive flow rate in some areas, which may lead to uneven diffusion of the plasma material. The shielding structure may be formed by using a positive optical adhesive layer, and the shielding structure at least partially overlaps with the baffle opening in a direction parallel to the first substrate and perpendicular to the extension direction of the baffle structure, and the shielding structure is retained during subsequent development and exposure to prevent it from being removed by development, thereby forming the shielding structure.
[0124] It should be noted that, in this article, relational terms such as "first" and "second" are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, the elements defined by the sentence "comprise a ..." do not exclude the existence of other identical elements in the process, method, article or device including the elements.
[0125] The above description is only a specific embodiment of the present disclosure, so that those skilled in the art can understand or implement the present disclosure. Various modifications to these embodiments will be apparent to those skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present disclosure. Therefore, the present disclosure will not be limited to the embodiments described herein, but will conform to the widest scope consistent with the principles and novel features disclosed herein.
Claims
1. A display panel, characterized in that: include: A first substrate and a second substrate arranged opposite to each other; a plasma layer, located between the first substrate and the second substrate; A retaining wall structure is arranged between the first substrate and the second substrate, the retaining wall structure divides the plasma layer into a plurality of plasma units, and a plurality of retaining wall openings are arranged on the retaining wall structure; adjacent plasma units are connected through the retaining wall openings.
2. The display panel according to claim 1, characterized in that: The side of the second substrate facing away from the first substrate is a light emitting side; Along a direction perpendicular to the second substrate, a blocking wall structure with a partial thickness is provided between the second substrate and the blocking wall opening.
3. The display panel according to claim 1, characterized in that: Along the extending direction of the retaining wall structure, the retaining wall structure between adjacent plasma units is provided with a plurality of retaining wall openings.
4. The display panel according to claim 3, characterized in that: Along the extending direction of the retaining wall structure, the number density of the retaining wall openings of the retaining wall structure between adjacent plasma units gradually decreases from the middle area to the edge area.
5. The display panel according to claim 3, characterized in that: Along the extending direction of the retaining wall structure, the length of each retaining wall opening of the retaining wall structure between adjacent plasma units gradually decreases from the middle area to the edge area.
6. The display panel according to claim 3, characterized in that: The number of retaining wall openings on the retaining wall structure extending along the first direction is less than the number of retaining wall openings on the retaining wall structure extending along the second direction; The first direction intersects with the second direction, and the second direction is parallel to the direction of gravity.
7. The display panel according to claim 6, characterized in that: A connecting portion is provided between the retaining wall structure extending along the first direction and the retaining wall structure extending along the second direction; the area of the retaining wall opening close to the connecting portion is smaller than the area of the retaining wall opening far from the connecting portion.
8. The display panel according to claim 7, characterized in that: The connection portion formed by the retaining wall structure between the staggered plasma units is provided with the retaining wall opening.
9. The display panel according to claim 1, characterized in that: Along a direction perpendicular to the first substrate, a height of the retaining wall opening is 20%-60% of a height of the retaining wall structure.
10. The display panel according to claim 1, characterized in that: Along the extending direction of the retaining wall structure, the length of the retaining wall opening is 3%-10% of the length of the retaining wall structure.
11. The display panel according to claim 1, characterized in that: In a direction parallel to the first substrate and perpendicular to the extending direction of the retaining wall structure, the retaining wall openings of adjacent retaining wall structures arranged in parallel at least partially overlap.
12. The display panel according to claim 1, characterized in that: In a direction parallel to the first substrate and perpendicular to the extending direction of the retaining wall structure, the retaining wall openings of adjacent retaining wall structures arranged in parallel do not overlap.
13. The display panel according to claim 1, characterized in that: It also includes a shielding structure; in a direction parallel to the first substrate and perpendicular to the extending direction of the blocking wall structure, the shielding structure at least partially overlaps with the blocking wall opening.
14. The display panel according to claim 13, characterized in that: Along the extending direction of the retaining wall structure, the overlapping area between the shielding structure and the retaining wall opening gradually decreases from the middle area to the edge area of the retaining wall structure.
15. The display panel according to claim 13, characterized in that: The plasma layer includes a solvent and color-developing particles; The distance between adjacent openings of the retaining wall and the shielding structure is 5 to 10 times the diameter of the color-developing particles.
16. The display panel according to claim 1, characterized in that: The first substrate is an array substrate; A pixel electrode layer is disposed on a side of the array substrate facing the second substrate; the pixel electrode layer includes a plurality of pixel electrodes arranged in an array; There is a gap between adjacent pixel electrodes, and the retaining wall structure is arranged in the gap area.
17. A display device, characterized in that: Comprising a display panel as described in any one of claims 1-16.
18. A method for preparing a display panel, characterized in that: include: forming a retaining wall structure on the first substrate; The retaining wall structure is provided with a plurality of retaining wall openings; forming the plasma layer; The retaining wall structure divides the plasma layer into a plurality of plasma units, and adjacent plasma units are connected through the retaining wall openings; A second substrate is arranged on a side of the retaining wall structure away from the first substrate.
19. The method for preparing a display panel according to claim 18, characterized in that: forming a retaining wall structure on the first substrate; The retaining wall structure is provided with a plurality of retaining wall openings, including: forming a positive optical adhesive layer on the first substrate; exposing and developing the positive optical adhesive layer to form a positive optical adhesive layer pattern corresponding to a plurality of retaining wall openings; Forming a negative optical adhesive layer; wherein the negative optical adhesive layer covers the positive optical adhesive layer pattern and the first substrate; The positive optical adhesive layer pattern is removed by exposure and development, so that a plurality of retaining wall openings are provided on the retaining wall structure.
20. The method for preparing a display panel according to claim 18, characterized in that: Also includes: The shielding structure is formed on the first substrate; in a direction parallel to the first substrate and perpendicular to an extension direction of the blocking wall structure, the shielding structure at least partially overlaps with the blocking wall opening.
