Structure high-cycle fatigue increment analysis method based on internal force amplitude correction

Through the ΔF-N curve and time domain increment method based on internal force amplitude correction, the shortcomings of the existing high-cycle fatigue analysis methods are solved, and accurate high-cycle fatigue life assessment and unsteady fatigue prediction of metal structures are achieved, which is suitable for Reliability assessment of large engineering structures.

CN118761192AActive Publication Date: 2024-10-11CHONGQING UNIV

Patent Information

Application Number
CN202410644759.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-05-23
Publication Date
2024-10-11
Estimated Expiration
2044-05-23

AI Technical Summary

Technical Problem

Existing high-cycle fatigue analysis methods cannot accurately predict the initial cracking position of metal structures, obtain the true fatigue amplitude of the structure, and calculate unsteady wind-induced fatigue effects, and are difficult to be applied to high-cycle fatigue life assessment of large engineering structures.

Method used

The structural high-cycle fatigue incremental analysis method based on internal force amplitude correction is adopted, and the high-cycle fatigue pre-damage index is calculated by determining the correction factor and ΔF-N correction curve, and the time-domain incremental method is used to conduct unsteady high-cycle fatigue pre-damage. Evolution analysis, updating the fatigue performance of the structure in real time.

Benefits of technology

It achieves accurate prediction of key fatigue details of metal structures, improves the accuracy and efficiency of high-cycle fatigue life assessment, and can update the unsteady high-cycle fatigue pre-damage process of steel structures in real time, which is suitable for reliability assessment of large engineering structures. and maintenance decisions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118761192A_ABST
    Figure CN118761192A_ABST
Patent Text Reader

Abstract

The invention discloses a structure high-cycle fatigue increment analysis method based on internal force amplitude correction, and belongs to the technical field of metal structure fatigue analys.The method comprises the steps that firstly, key fatigue details of a metal structure are determined, and an S-N curve is determined according to classification of the closest fatigue details in hot spot stress method suggestions; according to the actual node construction of the key fatigue details, determining a correction factor and obtaining a correction F-N curve, and calculating a pre-damage index; filtering the unsteady-state loading original curve based on an unsteady-state high-cycle fatigue pre-damage evolution criterion of time domain increment to obtain an input unsteady-state fatigue loading system; and finally, establishing a high-cycle fatigue increment analysis model of the metal structure, and simulating a high-cycle fatigue loading test by constructing a kinematic relationship and a mechanical equilibrium relationship between a rod unit and nodes at two ends of the rod unit and establishing an elastic stiffness matrix, so as to predict the unsteady-state high-cycle fatigue pre-damage evolution process of the metal structure in real time. And the high-cycle fatigue life of metal structures such as a large-span steel bridge can be predicted more accurately.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of fatigue analysis of metal structures, and relates to a structural high-cycle fatigue incremental analysis method based on internal force amplitude correction. Background Art

[0002] Common metal structures such as steel structures and aluminum structures have been widely used in infrastructure projects such as large-span buildings, bridges, and offshore platforms because of their high strength, light weight, resource recycling, and greater environmental protection. In order to fully utilize the service performance and recycling value of metal structures, it is necessary to accurately evaluate the remaining high-cycle fatigue performance of in-service metal structure projects, especially a number of industrial infrastructure projects that have been in service for a long time. Accurately evaluating their remaining fatigue life is not only an economic and environmental protection demand, but also a necessity to protect the safety of life and property.

[0003] Although the application demand of metal structures is increasing, fatigue problems are easily overlooked. The Shenyang Institute of Metal Research, Chinese Academy of Sciences and the American Society of Civil Engineering both mentioned that "nearly 90% of failures in metal structures are caused by fatigue damage", and fatigue damage often causes brittle failure, which is not easy to detect and extremely harmful. Existing technologies still need to be improved in accurately predicting the fatigue life of metal structures in two aspects. First, there are fatigue details with complex structural structures in metal structures, which cannot strictly correspond to the relevant fatigue details of the resistance curve recommended by domestic and foreign specifications, and the benchmark curve needs to be corrected; on the other hand, the existing stress-life (SN) fatigue resistance curve system is suitable for smaller-sized components such as materials or machinery, which is difficult to match the needs of fatigue performance evaluation of large-scale engineering structures. In terms of engineering applications, it is more hoped to be expressed through intuitive axial force or curved rectangular form.

[0004] At present, the research on metal fatigue at home and abroad is concentrated in the fields of materials and mechanical structures. In the field of civil engineering, especially for metal structures such as large-span steel bridges or aluminum alloy grids, there is a lack of high-cycle fatigue life prediction models that are widely applicable and convenient for engineering applications. On the one hand, when the traditional finite element simulation method is used for fatigue analysis, it is impossible to efficiently determine the key fatigue details, and the high time cost brought by the fine grid unit analysis makes it impossible to achieve real-time updates of the high-cycle fatigue performance of steel structures in long-term service status; on the other hand, the current conventional methods still rely on the benchmark SN curve and rain flow counting method statistics when predicting high-cycle fatigue performance. The former makes it difficult to accurately consider the special structure of fatigue details, and the latter makes it impossible to predict the high-cycle fatigue performance of non-steady-state loading in real time; the existing high-cycle fatigue evaluation methods are only applicable to constant amplitude or variable amplitude loading, and cannot calculate random fatigue loading such as non-steady-state pulsating wind action. Summary of the invention

[0005] The present invention aims to provide a structural high-cycle fatigue incremental analysis method based on internal force amplitude correction, to solve the problems of existing high-cycle fatigue analysis methods that cannot locate the initial crack position, cannot obtain the true fatigue amplitude of the structure, and cannot calculate the non-steady-state wind-induced fatigue effect, and through real-time output of various state variables to characterize the high-cycle fatigue pre-damage process of key fatigue details of metal structures, more accurately predict the high-cycle fatigue life of engineering-scale metal structures.

[0006] The present invention is implemented by adopting the following technical solution: a structural high cycle fatigue incremental analysis method based on internal force amplitude correction is implemented according to the following steps:

[0007] Step A: First, determine the key fatigue details of the metal structure and determine the benchmark SN curve based on the closest fatigue detail classification recommended by the hot spot stress method;

[0008] Step B, determining the correction factor according to the actual structure of the node of the key fatigue details and obtaining the ΔF-N correction curve, and calculating the high cycle fatigue pre-damage index;

[0009] Among them, the correction factors include stress concentration, thickness, and stress ratio. When determining the ΔF-N correction curve, the following method is used:

[0010] 1) Under axial force or bending moment cyclic loading, the fatigue load amplitude is modified to consider the cross-sectional area A or cross-sectional moment W of the component and the stress concentration correction factor ψ at the welding end of the component c , thickness correction factor ψ t , and the stress ratio correction factor ψ R ;

[0011] a. Establish a refined finite element model to analyze the true stress distribution of the node fatigue details, and compare it with the preliminary experiment before the node loading, and define the maximum stress S of the fatigue detail weld max and pipe body stress S nom The ratio is the stress concentration correction factor:

[0012]

[0013] Among them, the pipe body stress S nom is the maximum nominal stress on the outer edge of the pipe wall under external force, expressed as:

[0014]

[0015] b. Thickness correction factor ψ t It is used to characterize the influence of thick steel plate on welding quality, expressed as:

[0016] ψ t =1 / f(t)=1 / (25 / t) n ;

[0017] Where f(t) is the thickness fatigue factor recommended by the International Welding Association, and n is related to the node welding method and is determined according to the node classification in the International Welding Association standard;

[0018] c. Stress ratio correction factor ψ R It is used to characterize the effect of the compressive part of the cyclic load amplitude on delaying fatigue cracking when the stress ratio R is less than 0, expressed as:

[0019]

[0020] Combining the benchmark SN curve and the correction coefficient, the corrected internal force amplitude-life relationship expression is as follows:

[0021]

[0022]

[0023] Among them, σ cr is the high cycle fatigue stress constant, The constant C is determined by the benchmark SN curve of the node; ΔF is the nominal axial force amplitude of the node subjected to fatigue load, ΔM is the nominal bending moment amplitude of the node subjected to fatigue load, and N is the fatigue life of the node;

[0024] 2) Based on the above correction strategy, the internal force amplitude-life correction curve formula of the welded steel pipe-spherical shell node is derived:

[0025] First, the stress concentration distribution of the welded steel pipe-spherical shell node and the thickness and stress ratio correction coefficients are determined. The maximum true stress S at the weld under each crane load amplitude level is calculated. max , and the pipe body stress S nom The ratio of is the stress concentration correction factor:

[0026]

[0027]

[0028] Next, the internal force amplitude-life ΔF-N correction curve expression of the most unfavorable fatigue detail of the welded steel pipe-spherical shell node is derived as follows:

[0029]

[0030] Where, ΔF 管 is the nominal axial force amplitude of the steel tube weld toe fatigue detail of the welded steel tube-spherical shell joint, A 管 is the cross-sectional area of ​​the steel tube at the welded steel tube-spherical shell node, N 管 is the fatigue life of the steel pipe at the welded steel pipe-spherical shell node, ψ c管 , t管, R管 They are the stress concentration, thickness and stress ratio correction coefficients of the welded steel pipe-spherical shell node respectively.

[0031] Furthermore, a high-cycle fatigue pre-damage index is proposed based on the ΔF-N correction curve to quantitatively characterize the high-cycle fatigue performance evolution process of the most unfavorable fatigue details. Specifically:

[0032] The calculation formula of the pre-damage index w is derived through the ΔF-N correction curve formula;

[0033]

[0034] Where N is the number of cycles of high cycle fatigue loading on the structure, F cr is the high cycle fatigue corrected axial force constant, M cr is the high cycle fatigue corrected bending moment constant, ΔF is the axial force amplitude borne by the most unfavorable fatigue detail, and ΔM is the bending moment amplitude borne by the most unfavorable fatigue detail, expressed as:

[0035]

[0036]

[0037] The accuracy of the ΔF-N correction curve was verified by simulating high cycle fatigue loading tests.

[0038] Step C, establishing a non-steady-state high-cycle fatigue pre-damage evolution criterion based on time domain increment, filtering the original non-steady-state loading curve, and obtaining the input non-steady-state fatigue loading system;

[0039] (1) For fatigue load amplitudes that are constant or change periodically, it is considered steady-state high-cycle fatigue. This type of fatigue life is directly obtained through the ΔF-N correction curve or combined with the Miners cumulative damage criterion; fatigue load amplitudes that change irregularly with time periods are considered non-steady-state high-cycle fatigue. The real-time continuous evolution analysis of structural pre-damage under non-steady-state fatigue is achieved through the time domain increment method;

[0040] Based on the pre-damage index formula, the time domain increment formula of the non-steady-state high-cycle fatigue pre-damage index is further derived and expressed as:

[0041]

[0042] Among them, w(t n ) is the structural fatigue pre-damage value at the nth incremental step, w(t n-1 ) is the structural fatigue pre-damage value at the n-1th incremental step, F(t n ) is the axial force of the structural member at the nth incremental step, F(t n-1) is the axial force of the structural member at the n-1th incremental step, M(t n ) is the structural rod end bending moment at the nth incremental step, M(t n-1 ) is the structural rod end bending moment at the n-1th incremental step;

[0043] (2) The original curve of the unsteady-state loading is filtered to obtain the equivalent loading system for unsteady-state high-cycle fatigue incremental analysis. The data filtering method is as follows:

[0044] The high-cycle fatigue increment depends on the maximum load amplitude in a cycle. The peaks and troughs of each cycle are extracted, the data points between the peaks and troughs are ignored, and the proximal end points in the obtained peak-to-trough data with a time interval less than 0.05s are deleted to obtain the incremental analysis load history equivalent to fatigue pre-damage.

[0045] Step D: Finally, a high-cycle fatigue incremental analysis model for metal structures is established. By constructing the kinematic relationship and mechanical equilibrium relationship between the rod unit and its two end nodes and establishing an elastic stiffness matrix, the evolution process of non-steady-state high-cycle fatigue pre-damage of the steel structure is predicted in real time.

[0046] Establish an incremental analysis model for high-cycle fatigue of metal structures based on internal force amplitude correction; define the initial state variable matrix: node displacement, unit deformation, unit internal force, pre-damage index, node external force and boundary conditions; achieve preliminary positioning of each fatigue detail of the structure, and analyze and predict the evolution process of non-steady-state high-cycle fatigue pre-damage of steel structures in combination with the internal force amplitude-life ΔF-N correction curve of each fatigue detail;

[0047] (1) Define the unit of the internal force amplitude-life ΔF-N correction curve, define the nodes of the target steel structure, and divide the calculation rod units;

[0048] (2) Input the displacement and force boundary conditions of each node of the structure and construct the global node displacement matrix {U(t)} and the global node external force matrix {P(t)}:

[0049] Among them, the global node displacement matrix {U(t)} is defined as:

[0050] {U(t)}=[x1(t)z1(t)r1(t),......,x k (t)z k (t)r k (t)]

[0051] Among them, x(t), z(t), and r(t) are the translational displacement time history of the node along the X-axis and Z-axis of the global coordinate system and the rotational displacement time history around the Y-axis;

[0052] The axial force F at each node along the three degrees of freedom xk 、Fzk and bending moment M k The global node external force matrix {P(t)} is constructed and described as:

[0053] {P(t)}=[F x1 (t) F z1 (t) M1(t),......,F xk (t) F zk (t) M k (t)]

[0054] (3) The deformation matrix {Φ(t)} of the structure calculation rod unit b b Including the rotational deformation of the two end nodes i and j and the axial deformation of the rod, correspondingly, the internal force matrix {m(t)} b Includes the bending moments at nodes i and j and the axial forces of the rod;

[0055] (4) Construct the kinematic relationship and mechanical equilibrium relationship between the rod unit and its two end nodes, and establish the elastic stiffness matrix:

[0056] According to the counterclockwise angle of the rod element about the x-axis in the global plane coordinate system and its actual length, the global coordination matrix is ​​determined, and then the kinematic relationship between the node displacement and the unit deformation, the mechanical equilibrium relationship between the node external force and the unit internal force are constructed, and at the same time, the elastic constitutive relationship between the unit deformation and the unit internal force is established;

[0057] The kinematic relationship, mechanical equilibrium relationship and elastic constitutive relationship of crack latent period between the rod unit and each node are established; among which, the deformation matrix of the rod unit b and the total displacement matrix of all nodes including the two end nodes i and j satisfy the kinematic equation:

[0058] {Φ(t)} b =[B b (U)]{U(t)}

[0059] Among them, [B b (U)] is the global coordination matrix;

[0060] The internal force matrix of all rod elements b and the total matrix of global node external forces satisfy the mechanical equilibrium equation:

[0061]

[0062] The deformation matrix and internal force matrix of the rod element b satisfy the high cycle fatigue elastic constitutive equation:

[0063] {m(t)} b =[E]·{Φ(t)} b

[0064] The stiffness matrix [E] during the high cycle fatigue crack latency period remains unchanged and is described as:

[0065]

[0066] (5) The quantitative index of the structural high-cycle fatigue incremental analysis process is the pre-damage index matrix {w(t)} of the calculated rod element. b , the cracks finally initiate at the nodes at both ends of the rod, so:

[0067] {w(t)}b=[w i wj ] ] b

[0068] The pre-damage index matrix is ​​obtained by iteratively calculating the unit internal force obtained in each incremental step of the TDI-FEL model by substituting it into the time domain incremental formula;

[0069] (6) Real-time prediction of the evolution of non-steady-state high-cycle fatigue pre-damage in metal structures;

[0070] Based on the ΔF-N correction curve of the fatigue details of the metal structure, the time domain incremental expression of the high-cycle fatigue pre-damage index is obtained. With the help of the high-cycle fatigue incremental analysis model TDI-FEL for metal structures, the prediction of the non-steady-state high-cycle fatigue pre-damage evolution process of steel structures is realized.

[0071] Compared with the prior art, the advantages and positive effects of the present invention are:

[0072] This scheme takes into account the actual structure of the welding nodes at the fatigue details of the metal structure, and proposes a ΔF-N correction curve between the corrected internal force amplitude and the structural life; and based on the non-steady-state high-cycle fatigue performance prediction method of the time domain increment method, the real-time update of the nominal internal force, corrected internal force and high-cycle fatigue performance is achieved through the TDI-FEL model and the pre-damage evolution criterion; it can accurately and efficiently predict the fatigue life of metal structures and key nodes subjected to high-cycle fatigue loading, and update the high-cycle pre-damage evolution process in real time, providing a basis for reliability assessment and maintenance decision-making of metal structures such as steel trusses, steel frames, and aluminum trusses, and realizing risk prediction and control throughout the life cycle of the structure. BRIEF DESCRIPTION OF THE DRAWINGS

[0073] Figure 1 A flow chart of the method for predicting high cycle fatigue performance of welded metal structures of the present invention;

[0074] Figure 2 It is a flow chart of the time domain incremental method for the non-steady-state high cycle fatigue evolution of the present invention;

[0075] Figure 3 Schematic diagram of fatigue details of steel structure of the embodiment, (a) welded steel pipe-spherical shell node (b) steel pipe weld toe and spherical shell weld toe;

[0076] Figure 4 This is a comparison diagram of the pre-experimental stress distribution results of the embodiment;

[0077] Figure 5 It is a comparison result diagram of ΔF-N correction curve of high cycle fatigue test of the embodiment;

[0078] Figure 6 The figure is a comparison result diagram of the screened data and the original data of the embodiment, wherein (a) is the original data and (b) is the screened data;

[0079] Figure 7 It is a result diagram of the non-steady-state high cycle fatigue pre-damage evolution curve of the embodiment. DETAILED DESCRIPTION

[0080] In order to more clearly understand the above-mentioned purpose, features and advantages of the present invention, the present invention is further described below in conjunction with the accompanying drawings and embodiments. It should be noted that the embodiments of the present application and the features in the embodiments can be combined with each other without conflict.

[0081] This embodiment proposes a structural high-cycle fatigue incremental analysis method based on internal force amplitude correction for key welded steel pipe-spherical shell nodes of large-span steel structures that are not included in the fatigue detail classification in the current specifications. First, the corrected internal force amplitude-life relationship of the node and the corresponding high-cycle fatigue corrected axial force constant and bending moment constant are obtained to more accurately predict the high-cycle fatigue life of such nodes. The real-time evolution process of non-steady-state high-cycle fatigue pre-damage of the key node is further analyzed by the time domain incremental method. The problems of existing prediction methods that cannot locate the initial crack position, cannot obtain the true fatigue amplitude of the structure, and cannot calculate the non-steady-state wind-induced fatigue effect are solved.

[0082] like Figure 1 As shown, a structural high cycle fatigue incremental analysis method based on internal force amplitude correction includes the following steps:

[0083] Step A: First, determine the key fatigue details of the metal structure and determine the SN curve according to the closest fatigue detail classification recommended by the hot spot stress method;

[0084] Step A1: Identify key fatigue details of welded metal structures;

[0085] Fatigue of metal structures is most likely to occur at locations where stress concentration and welds are concentrated, such as nodes where rods intersect. According to the principle of macroscopic damage mechanics, under fatigue loading, rod damage is concentrated at hinge nodes. Due to stress concentration and the complexity of connections, fatigue cracks in steel grid structures are more likely to initiate at welded steel pipe-spherical shell nodes where rods intersect. Figure 3, is a type of welded steel pipe-spherical shell node commonly used in steel structures such as large-span space trusses and grid structures. This embodiment specifically takes this node as an example to introduce the correction strategy of the benchmark stress-life (SN) curve of the key fatigue detail welded steel pipe-spherical shell node in the steel grid structure.

[0086] Step A2: Determine the reference stress-life (SN) curve based on the closest fatigue detail classification recommended by the hot spot stress method. Hot spot stress refers to the stress increase effect at the structural welding details, which is caused by the sudden change in geometric dimensions caused by the intersection of multiple components and the residual stress in the weld.

[0087] The welded nodes of metal structures are often fixed connections between components of different sizes in different directions, and the stress concentration phenomenon is obvious. For this reason, the hot spot stress method summarizes the benchmark SN curves of common engineering metal structures based on a large number of fatigue experiments. The standard grades of hot spot stress for steel structures are FAT90 and FAT100, and the standard grades of hot spot stress for aluminum structures are FAT36 and FAT40.

[0088] According to the actual structure of the welded steel pipe-spherical shell node, a closer one is selected from the SN curves of the relevant fatigue level provided by the hot spot stress method, and the high cycle fatigue coefficient C and high cycle fatigue index γ of the SN relationship expression are reversed through two data points (N1, S1) and (N2, S2) on the curve.

[0089]

[0090] This type of node includes the end of the circular tube and the spherical shell as well as the weld connecting the two. Compared with the common butt welds and fillet welds, the FAT100 series recommended by the hot spot stress method is selected from the FAT90 and FAT100 series, which is closer to the welded steel tube-spherical shell node structure. The high cycle fatigue stress coefficient C = 1.622456×10 12 and exponent γ = -2.95;

[0091] Step B, determining the correction factor according to the actual structure of the node of the key fatigue detail and obtaining the modified FN curve, and calculating the pre-damage index;

[0092] Step B1. The ΔF-N correction curve is different from the SN curve in that it not only considers the size parameters of the component, but also considers three types of correction factors: stress concentration, thickness, and stress ratio. It includes the following technical steps:

[0093] 1) Under axial force or bending moment cyclic loading, the modified fatigue load amplitude takes into account the cross-sectional area A or cross-sectional moment W of the component and the stress concentration factor ψ at the weld end of the component c , thickness correction factor ψ t , and the stress ratio correction factor ψ RThe concentrated stress at the real fatigue details is obtained by finite element analysis verified by preliminary tests. The thickness and stress ratio correction factors are used to characterize the influence of thick steel plates (>25mm) on welding quality and the influence of the compression part of the cyclic load amplitude on delaying fatigue cracking.

[0094] a. Analyze the real stress distribution of the node fatigue details by establishing a refined finite element model and compare it with the preliminary experiment before the node is loaded. Figure 4 , verify the accuracy of the stress analysis model, define the maximum stress S of the fatigue detail weld max (Concentrated stress) and pipe body stress (nominal stress) S nom The ratio is the stress concentration correction factor,

[0095]

[0096] Among them, the pipe body stress is the maximum nominal stress on the outer edge of the pipe wall under the action of external forces (including axial force F and bending moment M), which is calculated as:

[0097]

[0098] Among them, A and W are the area and section moment of the circular tube cross section respectively;

[0099] b. Thickness correction factor ψ t Used to characterize the influence of thick steel plate (>25mm) on welding quality.

[0100] ψ t =1 / f(t)=1 / (25 / t) n

[0101] Among them, f(t) is the thickness fatigue coefficient recommended by the International Welding Association, and n is related to the node welding method and is taken as 0.1 to 0.3;

[0102] c. Stress ratio correction factor ψ R It is used to characterize the effect of the compressive part of the cyclic load amplitude on delaying fatigue cracking when the stress ratio R is less than 0, and is described as:

[0103]

[0104] Combining the benchmark SN curve and various correction coefficients, the corrected internal force amplitude-life relationship expression is derived as follows:

[0105]

[0106]

[0107] Among them, σ cr is the high cycle fatigue stress constant,

[0108]

[0109] 2) According to the above correction strategy, the internal force amplitude-life correction curve formula of the welded steel pipe-spherical shell node is derived:

[0110] First, determine the stress concentration distribution and other correction factors of the welded steel pipe-spherical shell node.

[0111] Based on the maximum true stress Smax at the weld under each crane load amplitude level, the ratio to the pipe body stress (nominal stress) Snom is obtained, which is the stress concentration correction factor.

[0112]

[0113]

[0114] Furthermore, the thickness of the steel plate used in conventional welded steel pipe-spherical shell nodes is generally less than 25 mm, so the thickness correction factor ψ t is 1.0; in this embodiment, the stress ratio of the crane load is 0.4, so the stress ratio correction coefficient ψ R is 1.0; then, the internal force amplitude-life (ΔF-N) correction curve expression of the most unfavorable fatigue detail of the welded steel pipe-spherical shell node is derived as follows:

[0115]

[0116] Where, ΔF 管 is the nominal axial force amplitude of the steel tube weld toe fatigue detail of the welded steel tube-spherical shell joint, A 管 is the cross-sectional area of ​​the steel tube at the welded steel tube-spherical shell node, N 管 is the fatigue life of the steel pipe at the welded steel pipe-spherical shell node, ψ c管 , t管 , R管 They are the stress concentration, thickness and stress ratio correction coefficients of the welded steel pipe-spherical shell node respectively.

[0117] Step B2, based on the ΔF-N correction curve, a high cycle fatigue pre-damage index is proposed to quantitatively characterize the high cycle fatigue performance evolution process of the most unfavorable fatigue detail;

[0118] Since the latent period before fatigue crack initiation accounts for more than 90% of the life cycle of the structure, and the structural stiffness matrix during the latent period will not be degraded due to damage, the pre-damage index is used as the key indicator to measure the evolution of high-cycle fatigue performance. The calculation formula of the pre-damage index w is derived through the ΔF-N correction curve formula.

[0119]

[0120] Where N is the number of cycles of high cycle fatigue loading on the structure, F cr is the high cycle fatigue corrected axial force constant, M cr is the high cycle fatigue corrected bending moment constant, ΔF is the axial force amplitude borne by the most unfavorable fatigue detail, and ΔM is the bending moment amplitude borne by the most unfavorable fatigue detail, which is described as,

[0121]

[0122]

[0123] For the welded steel tube-spherical shell node in the embodiment, the crack initiation under high cycle fatigue, i.e., the pre-damage evolution process, is controlled by the internal force amplitude. A calculation expression for the pre-damage index w that characterizes the high cycle fatigue performance evolution process of the most unfavorable fatigue detail is further proposed, as follows:

[0124]

[0125] Simulate high cycle fatigue loading test to verify the accuracy of the modified FN curve;

[0126] The high cycle fatigue test data of welded steel pipe-spherical shell joint and the benchmark SN curve are plotted in the same coordinate system (refer to Figure 5 ), it can be seen that the most unfavorable fatigue detail internal force amplitude-life correction formula of steel structure proposed in the present invention is in better agreement with the experimental data.

[0127] Step C, based on the non-steady-state high-cycle fatigue pre-damage evolution criterion of time domain increment, the non-steady-state loading original curve is filtered to obtain the input non-steady-state fatigue loading system;

[0128] This embodiment proposes a non-steady-state high-cycle fatigue pre-damage evolution criterion based on time domain increment, and establishes a structural pre-damage increment analysis method under high-cycle fatigue loading, especially non-steady-state action.

[0129] Metal structures are subjected to high-cycle cyclic loads and wind loads during their regular service. Among them, the fatigue load amplitude is constant or changes periodically, which is steady-state high-cycle fatigue, such as fatigue of steel beams and nodes under the crane load of the factory building. This type of fatigue life can be directly obtained through the ΔF-N curve or combined with the Miners cumulative damage criterion. The fatigue load amplitude that changes irregularly with the time period is considered as non-steady-state high-cycle fatigue.

[0130] The present invention replaces the traditional rain flow counting method with the time domain increment method to realize the real-time continuous evolution analysis of structural pre-damage under non-steady-state fatigue; the time domain increment formula of the pre-damage index is derived from the calculation formula of the constant amplitude high cycle fatigue pre-damage index, which is described as:

[0131]

[0132] Among them, w(t n ) is the structural fatigue pre-damage value at the nth incremental step, w(t n-1 ) is the structural fatigue pre-damage value at the n-1th incremental step, F(t n ) is the axial force of the structural member at the nth incremental step, F(t n-1 ) is the axial force of the structural member at the n-1th incremental step, M(t n ) is the structural rod end bending moment at the nth incremental step, M(t n-1 ) is the structural rod end bending moment at the n-1th incremental step,

[0133] The welded steel tube-spherical shell node steel grid structure is subjected to cyclic loads such as high-cycle crane loads and non-steady-state loads such as pulsating wind during conventional service. Before cracks can be found, the pre-damage index is used to characterize the crack latent process caused by stress amplitude accumulation. When the pre-damage w of the most unfavorable tensile section reaches the critical value of 1.0, cracks initiate, indicating that the structure is not suitable for normal use. The evolution curve of the non-steady-state fatigue process is updated in real time based on the time domain increment method, and the high-cycle fatigue failure is finally controlled by the pre-damage index.

[0134] Among them, the structural high-cycle fatigue incremental analysis method includes a data filtering method for the original curve of non-steady-state loading to obtain an incremental analysis loading system equivalent to the pre-damage result, specifically:

[0135] High cycle fatigue depends on the maximum load amplitude in a cycle (period is Tc). The peaks and troughs of each cycle of the curve are extracted, and the points between the peaks and troughs are ignored. In addition, there will be some adjacent peaks (troughs) with similar time history (<0.05Tc) in the curve. At this time, the smaller ones are ignored, and finally the external load used to input the fatigue model is obtained;

[0136] Reference Figure 2 The present invention proposes a time domain increment method to replace the traditional counting method rain flow counting method. The same as the latter is that both are based on the linear elastic cumulative fatigue criterion and obtain results with consistent accuracy. The difference from the latter is that the new method can update the residual fatigue performance of the steel structure under non-steady-state high-cycle fatigue loading by real-time recording of the pre-damage index evolution curve;

[0137] For the time-domain unsteady-state fatigue analysis of the welded steel pipe-spherical shell node in this embodiment, it is first necessary to perform data screening on the original unsteady-state fatigue loading curve to accurately simplify the loading system input to the model. The data filtering method is:

[0138] like Figure 6 As shown, the original non-steady-state fatigue loading curve (2432 data points) was processed by data screening to obtain the incremental analysis load history (53 data points) equivalent to fatigue pre-damage.

[0139] Step D: Finally, a high-cycle fatigue incremental analysis model for metal structures is established. By constructing the kinematic relationship and mechanical equilibrium relationship between the rod unit and its two end nodes and establishing an elastic stiffness matrix, the evolution process of non-steady-state high-cycle fatigue pre-damage of the steel structure can be predicted in real time.

[0140] Step D1, establishing a high cycle fatigue incremental analysis model TDI-FEL for metal structures based on internal force amplitude correction;

[0141] In order to perceive the changes in the internal forces of various components at the fatigue details of metal structures during fatigue loading, preliminarily locate the fatigue details of the structure, and obtain the evolution of the pre-damage values ​​of each unfavorable fatigue detail of the structure, a high-cycle fatigue incremental analysis model TDI-FEL (Time domain incremental-Fatigue Elements) for metal structures based on internal force amplitude correction is established.

[0142] And define the initial state variable matrix: node displacement (rotation and translation), unit deformation (bending and expansion), unit internal force (bending moment and axial force), pre-damage index, node external force and boundary conditions;

[0143] (1) The unit of the internal force amplitude-life (ΔF-N) correction curve is specified as kN·m, the nodes of the target steel structure are defined, and the calculation bar units are divided.

[0144] (2) Input the displacement and force boundary conditions of each node of the structure, construct the global node displacement matrix {U(t)} and the global node external force matrix {P(t)},

[0145] Among them, the global node displacement matrix {U(t)} is defined as:

[0146] {U(t)}=[x1(t) z1(t) r1(t),......,x k (t) z k (t) r k (t)]

[0147] Among them, x k (t), z k (t), r k (t) are the time history of the node's translational displacement (m) along the X-axis and Z-axis of the global coordinate system and the time history of the rotational displacement (rad) around the Y-axis; further, the axial force F acting on each node along the three degrees of freedom xk 、F zk and bending moment M k The global node external force matrix {P(t)} is constructed and described as:

[0148] {P(t)}=[F x1(t) F z1 (t) M1(t),......,F xk (t) F zk (t) M k (t)]

[0149] (3) The deformation matrix {Φ(t)} of the structure calculation rod unit b b Including the rotational deformation of the two end nodes i and j and the axial deformation of the rod, correspondingly, the internal force matrix {m(t)} b Includes the bending moments at nodes i and j and the axial forces of the rod;

[0150] (4) Construct the kinematic relationship and mechanical equilibrium relationship between the rod unit and its two end nodes, and establish the elastic stiffness matrix.

[0151] According to the counterclockwise angle of the rod element about the x-axis in the global plane coordinate system and its actual length, the global coordination matrix is ​​determined, and then the kinematic relationship between the node displacement and the unit deformation, the mechanical equilibrium relationship between the node external force and the unit internal force are constructed, and at the same time, the elastic constitutive relationship between the unit deformation and the unit internal force is established;

[0152] The kinematic relationship, mechanical equilibrium relationship and elastic constitutive relationship of crack latent period between the rod unit and each node are established; wherein the deformation matrix of the rod unit b and the total displacement matrix of all nodes including the two end nodes i and j satisfy the kinematic equation:

[0153] {Φ(t)} b =[B b (U)]{U(t)}

[0154] Among them, [B b (U)] is the global coordination matrix.

[0155] Furthermore, the internal force matrix of all the rod units b and the total matrix of the global node external force satisfy the mechanical equilibrium equation:

[0156]

[0157] Since the latent period before fatigue crack initiation accounts for more than 90% of the life cycle of the structure, and the structural stiffness matrix during the latent period will not degrade due to plastic accumulation and damage, the deformation matrix and internal force matrix of the rod element b satisfy the high-cycle fatigue elastic constitutive equation.

[0158] {m(t)} b =[E]·{Φ(t)} b

[0159] The stiffness matrix [E] during the high cycle fatigue crack latency period remains unchanged and is described as:

[0160]

[0161] (5) The quantitative index of the structural high-cycle fatigue incremental analysis process is the pre-damage index matrix {w(t)} of the calculated rod element. b , the cracks finally initiate at the nodes at both ends of the rod, so:

[0162] {W(t)}b=[w i w j ] b

[0163] The pre-damage index matrix can be obtained by iterative calculation by substituting the unit internal force obtained in each incremental step of the TDI-FEL model proposed in step D2 into the time domain incremental formula.

[0164] Step D2: Real-time prediction of the evolution process of non-steady-state high-cycle fatigue pre-damage of metal structures; accurately analyze the initial cracking position of the target steel structure through the TDI-FEL model, and combine the ΔF-N correction curve to obtain the true internal force amplitude of the fatigue details and calculate the non-steady-state high-cycle fatigue pre-damage index

[0165] Based on the ΔF-N correction curve of the fatigue details of the metal structure, the time domain incremental expression of the high-cycle fatigue pre-damage index is obtained. With the help of the high-cycle fatigue incremental analysis model TDI-FEL for metal structures, the prediction of the non-steady-state high-cycle fatigue pre-damage evolution process of steel structures is realized.

[0166] This embodiment uses the TDI-FEL model of the welded steel tube-spherical shell node to accurately locate the most unfavorable fatigue details of this type of steel structure, namely the crack initiation site, and solves the problem that the traditional continuum finite element cannot obtain the pre-damage progress when analyzing fatigue problems, especially long-cycle fatigue assessment; First, the initial input setting of the model is mainly divided into three parts, boundary conditions, attribute constant parameters, and analysis steps. The boundary condition setting includes the displacement constraints and loading system of the node, the horizontal and vertical translational degrees of freedom of the support node, and the 1-min axial force time history under pulsating wind is applied to the loading node. The equivalent high-cycle fatigue incremental analysis loading cycle period is 1, with a total of 53 cycles.

[0167] The high-cycle fatigue incremental analysis model of the welded steel pipe-spherical shell node is a multi-rod physical system connected by potential damage nodes. In addition to the nodes where the rods intersect geometrically, it also includes concentrated loading points in the physical sense. The length of the rod unit of the fatigue analysis model and the coordinates of each node are set. In order to overcome the scale effect, the generalized internal force matrix and generalized deformation matrix of the rod unit are established. The kinematic equation, mechanical equilibrium equation and high-cycle fatigue elastic constitutive equation of the welded steel pipe-spherical shell node model are further constructed. The internal force of each rod unit of the structure at each incremental step is calculated, and the pre-damage index of each potential damage node at each moment is further obtained to realize the high-cycle fatigue incremental analysis process of the structure under the non-steady-state (pulsating wind) loading system.

[0168] The evolution of the welded steel pipe-spherical shell node during the crack initiation period determines the fatigue failure process. The node is in elasticity and gradually accumulates internal force amplitude to form a potential crack source, which in turn leads to crack initiation. In order to quantitatively characterize this process, the TDI-FEL model is used to output the pre-damage index of each incremental step of the two most unfavorable fatigue details of the potential crack source, which is described as:

[0169] The pre-damage index at each moment reflects the high-cycle fatigue incremental analysis process of the steel structure. First, the ΔF-N correction is performed on the two most unfavorable fatigue detail weld toes of the welded steel pipe-spherical shell node to obtain the pre-damage index calculation formula:

[0170]

[0171]

[0172] Among them, w 管 is the pre-damage index of the weld toe of the welded steel pipe-spherical shell node, w 球 is the pre-damage index of the spherical shell weld toe of the welded steel pipe-spherical shell node,

[0173] Furthermore, based on the pre-damage index w(t n-1 ), calculate the pre-damage index w(t n ), which is used to update the high-cycle fatigue pre-damage index of the most unfavorable fatigue details in real time. The evolution formula of the pre-damage index characterizing the crack initiation process with the total loading time is:

[0174]

[0175]

[0176] Among them, t n is the current increment time, t n-1 is the moment of the previous incremental step, and ΔF is the absolute value of the internal force difference between the current moment and the previous moment of the input.

[0177] The pre-damage evolution curves of the most unfavorable fatigue detail weld toes at the welded steel pipe-spherical shell node obtained by the high cycle fatigue incremental analysis method of the present invention are as follows: Figure 7 As shown, it can be seen that the curves describe the non-steady-state fatigue evolution process of the two weld toes in real time, reflecting the changing characteristics of the non-steady-state loading amplitude in the time domain; at the same time, the comparison of the two curves can also reflect that the pre-damage evolution process of the two weld toes at the same steel tube-spherical shell node, namely the tube body weld toe and the spherical shell weld toe, is significantly distinguished by the influence of the correction factor, and the final difference in the crack initiation rate is consistent with the difference in the true stress of the two weld toes, indicating that at this spherical shell node, the most unfavorable fatigue detail is located at the interface where the weld and the circular tube intersect, showing that the numerical simulation method of the present invention not only has the high efficiency of long-period macro analysis, but also has the accuracy of accurately describing the pre-damage evolution of the most unfavorable fatigue details.

[0178] By means of the modified fatigue internal force amplitude-life relationship of the present invention and the method for defining the evolution of high-cycle fatigue pre-damage indicators, the whole process from the stress concentrated node through the crack incubation period to fatigue cracking failure is described; according to the time domain incremental iteration process set by the loading system, the fatigue internal force amplitude and pre-damage indicators of the most unfavorable fatigue details are simulated in real time, and finally the high-cycle fatigue life is calculated, which is equivalent to the accuracy of the traditional rain flow counting method, but the method of the present invention realizes the real-time update of the high-cycle fatigue performance controlled by the modified internal force amplitude, which is used for the high-cycle fatigue performance evolution analysis of metal structures such as large-span steel bridges.

[0179] The above description is only a preferred embodiment of the present invention and does not limit the present invention in other forms. Any technician familiar with the profession may use the technical content disclosed above to change or modify it into an equivalent embodiment with equivalent changes and apply it to other fields. However, any simple modification, equivalent change and modification made to the above embodiment based on the technical essence of the present invention without departing from the content of the technical solution of the present invention still falls within the protection scope of the technical solution of the present invention.

Claims

1. Structural high cycle fatigue incremental analysis method based on internal force amplitude correction, It is characterized in that The following steps are involved: Step A: First, determine the key fatigue details of the metal structure and determine the benchmark SN curve based on the closest fatigue detail classification recommended by the hot spot stress method; Step B, determining the correction factor according to the actual structure of the node of the key fatigue details and obtaining the ΔF-N correction curve, and calculating the high cycle fatigue pre-damage index; Step C, establishing a non-steady-state high-cycle fatigue pre-damage evolution criterion based on time domain increment, filtering the original non-steady-state loading curve, and obtaining the input non-steady-state fatigue loading system; Step D: Finally, a high-cycle fatigue incremental analysis model for metal structures is established. By constructing the kinematic relationship and mechanical equilibrium relationship between the rod unit and its two end nodes and establishing an elastic stiffness matrix, the evolution process of non-steady-state high-cycle fatigue pre-damage of the steel structure can be predicted in real time.

2. The structural high cycle fatigue incremental analysis method based on internal force amplitude correction according to claim 1, Features: In step B, the correction factors include stress concentration, thickness, and stress ratio. When determining the ΔF-N correction curve, the following method is specifically used: 1) Under axial force or bending moment cyclic loading, the fatigue load amplitude is modified to consider the cross-sectional area A or cross-sectional moment W of the component and the stress concentration correction factor ψ at the welding end of the component c , thickness correction factor ψ t , and the stress ratio correction factor ψ R ; a. Establish a refined finite element model to analyze the true stress distribution of the node fatigue details, and compare it with the preliminary experiment before the node loading, and define the maximum stress S of the fatigue detail weld max and pipe body stress S nom The ratio is the stress concentration correction factor: Among them, the pipe body stress S nom is the maximum nominal stress on the outer edge of the pipe wall under external force, expressed as: b. Thickness correction factor ψ t It is used to characterize the influence of thick steel plate on welding quality, expressed as: ψ t =1 / f(t)=1 / (25 / t) n ; Where f(t) is the thickness fatigue factor recommended by the International Welding Association, and n is related to the node welding method and is determined according to the node classification in the International Welding Association standard; c. Stress ratio correction factor ψ R It is used to characterize the effect of the compressive part of the cyclic load amplitude on delaying fatigue cracking when the stress ratio R is less than 0, expressed as: Combining the benchmark SN curve and the correction coefficient, the corrected internal force amplitude-life relationship expression is as follows: Among them, σ cr is the high cycle fatigue stress constant, σ cr =(C) -1 / γ ; The constant C is determined by the reference SN curve of the node; ΔF is the nominal axial force amplitude of the node subjected to fatigue load, ΔM is the nominal bending moment amplitude of the node subjected to fatigue load, and N is the fatigue life of the node; 2) Based on the above correction strategy, the internal force amplitude-life correction curve formula of the welded steel pipe-spherical shell node is derived: First, the stress concentration distribution of the welded steel pipe-spherical shell node and the thickness and stress ratio correction coefficients are determined. The maximum true stress S at the weld under each crane load amplitude level is calculated. max , and the pipe body stress S nom The ratio of is the stress concentration correction factor: Next, the internal force amplitude-life ΔF-N correction curve expression of the most unfavorable fatigue detail of the welded steel pipe-spherical shell node is derived as follows: Where, ΔF 管 is the nominal axial force amplitude of the steel tube weld toe fatigue detail of the welded steel tube-spherical shell joint, A 管 is the cross-sectional area of ​​the steel tube at the welded steel tube-spherical shell node, N 管 is the fatigue life of the steel pipe at the welded steel pipe-spherical shell node, ψ c管 , t管 , R管 They are the stress concentration, thickness and stress ratio correction coefficients of the welded steel pipe-spherical shell node respectively.

3. The structural high cycle fatigue incremental analysis method based on internal force amplitude correction according to claim 1, Features: In the step B, a high cycle fatigue pre-damage index is proposed based on the ΔF-N correction curve to quantitatively characterize the high cycle fatigue performance evolution process of the most unfavorable fatigue detail, specifically: The calculation formula of the pre-damage index w is derived through the ΔF-N correction curve formula; Where N is the number of cycles of high cycle fatigue loading on the structure, F cr is the high cycle fatigue corrected axial force constant, M cr is the high cycle fatigue corrected bending moment constant, ΔF is the axial force amplitude borne by the most unfavorable fatigue detail, and ΔM is the bending moment amplitude borne by the most unfavorable fatigue detail, expressed as: The accuracy of the ΔF-N correction curve was verified by simulating high cycle fatigue loading tests.

4. The structural high cycle fatigue incremental analysis method based on internal force amplitude correction according to claim 1, Features: In step C, a non-steady-state high-cycle fatigue pre-damage evolution criterion based on time domain increment is proposed, and the input non-steady-state fatigue loading system is obtained by filtering the original data: (1) For fatigue load amplitudes that are constant or change periodically, it is considered steady-state high-cycle fatigue. This type of fatigue life is directly obtained through the ΔF-N correction curve or combined with the Miners cumulative damage criterion; fatigue load amplitudes that change irregularly with time periods are considered non-steady-state high-cycle fatigue. The real-time continuous evolution analysis of structural pre-damage under non-steady-state fatigue is achieved through the time domain increment method; Based on the pre-damage index formula, the time domain increment formula of the non-steady-state high-cycle fatigue pre-damage index is further derived and expressed as: Among them, w(t n ) is the structural fatigue pre-damage value at the nth incremental step, w(t n-1 ) is the structural fatigue pre-damage value at the n-1th incremental step, F(t n ) is the axial force of the structural member at the nth incremental step, F(t n-1 ) is the axial force of the structural member at the n-1th incremental step, M(t n ) is the structural rod end bending moment at the nth incremental step, M(t n-1 ) is the structural rod end bending moment at the n-1th incremental step; (2) The original curve of the unsteady-state loading is filtered to obtain the equivalent loading system for unsteady-state high-cycle fatigue incremental analysis. The data filtering method is as follows: The high-cycle fatigue increment depends on the maximum load amplitude in a cycle. The peaks and troughs of each cycle are extracted, the data points between the peaks and troughs are ignored, and the proximal end points in the obtained peak-to-trough data with a time interval less than 0.05s are deleted to obtain the incremental analysis load history equivalent to fatigue pre-damage.

5. The structural high cycle fatigue incremental analysis method based on internal force amplitude correction according to claim 1, Features: In the step D, a high-cycle fatigue incremental analysis model TDI-FEL for metal structures based on internal force amplitude correction is established; an initial state variable matrix is ​​defined: node displacement, unit deformation, unit internal force, pre-damage index, node external force and boundary conditions; Achieve preliminary positioning of each fatigue detail of the structure, and analyze and predict the evolution process of non-steady-state high-cycle fatigue pre-damage of steel structures by combining the internal force amplitude-life ΔF-N correction curve of each fatigue detail; (1) Define the unit of the internal force amplitude-life ΔF-N correction curve, define the nodes of the target steel structure, and divide the calculation rod units; (2) Input the displacement and force boundary conditions of each node of the structure and construct the global node displacement matrix {U(t)} and the global node external force matrix {P(t)}: Among them, the global node displacement matrix {U(t)} is defined as: {U(t)}=[x 1 (t) z 1 (t) r 1 (t),......,x k (t) z k (t) r k (t)] Among them, x k (t), z k (t), r k (t) are the time history of translational displacement of node k along the X-axis and Z-axis of the global coordinate system and the time history of rotational displacement around the Y-axis; The axial force F at each node along the three degrees of freedom xk 、F zk and bending moment M k The global node external force matrix {P(t)} is constructed and described as: {P(t)}=[F x1 (t) F z1 (t) M 1 (t),......,F xk (t) F zk (t) M k (t)] (3) The deformation matrix {Φ(t)} of the structure calculation rod unit b b Including the rotational deformation of the two end nodes i and j and the axial deformation of the rod, correspondingly, the internal force matrix {m(t)} b Includes the bending moments at nodes i and j and the axial forces of the rod; (4) Construct the kinematic relationship and mechanical equilibrium relationship between the rod unit and its two end nodes, and establish the elastic stiffness matrix: According to the counterclockwise angle of the rod element about the x-axis in the global plane coordinate system and its actual length, the global coordination matrix is ​​determined, and then the kinematic relationship between the node displacement and the unit deformation, the mechanical equilibrium relationship between the node external force and the unit internal force are constructed, and at the same time, the elastic constitutive relationship between the unit deformation and the unit internal force is established; The kinematic relationship, mechanical equilibrium relationship and elastic constitutive relationship of crack latent period between the rod unit and each node are established; among which, the deformation matrix of the rod unit b and the total displacement matrix of all nodes including the two end nodes i and j satisfy the kinematic equation: {Φ(t)} b =[B b (U)]{U(t)} Among them, [B b (U)] is the global coordination matrix; The internal force matrix of all rod elements b and the total matrix of global node external forces satisfy the mechanical equilibrium equation: The deformation matrix and internal force matrix of the rod element b satisfy the high cycle fatigue elastic constitutive equation: {m(t)} b =[E]·{Φ(t)} b The stiffness matrix [E] during the high cycle fatigue crack latency period remains unchanged and is described as: (5) The quantitative index of the structural high-cycle fatigue incremental analysis process is the pre-damage index matrix {w(t)} of the calculated rod element. b , the cracks finally initiate at the nodes at both ends of the rod, so: {w(t)} b =[w i w j ] b The pre-damage index matrix is ​​obtained by iteratively calculating the unit internal force obtained in each incremental step of the TDI-FEL model by substituting it into the time domain incremental formula; (6) Real-time prediction of the evolution of non-steady-state high-cycle fatigue pre-damage in metal structures; Based on the ΔF-N correction curve of the fatigue details of the metal structure, the time domain incremental expression of the high-cycle fatigue pre-damage index is obtained. With the help of the high-cycle fatigue incremental analysis model TDI-FEL for metal structures, the prediction of the non-steady-state high-cycle fatigue pre-damage evolution process of steel structures is realized.

Citation Information

Patent Citations

  • Method for evaluating wind-induced multi-axis high-cycle fatigue damage of space truss node welding seam in welding

    CN110991104A

  • Nonlinear estimation method for high-cycle fatigue crack initiation life of metal structure

    CN112580235A

  • Full-aircraft fatigue test loading design method based on internal force and life control

    CN117436186A

  • A digital twin framework of weld joint fatigue based on structural stress method

    US20230342522A1

Cited By

  • Numerical simulation method suitable for evaluating high-cycle fatigue performance of lattice structure

    CN120145627A

  • Method and system for predicting fatigue life of truss chord member composite beam

    CN120493659A

  • High-cycle fatigue strength evaluation method based on damage influence

    CN120651683A