Method and equipment for determining fracture conductivity of oil reservoir
By dividing the fractures of the reservoir into segments and constructing a post-attenuation model, the conductivity of the reservoir under closure stress is determined, which solves the problem of the inability to effectively determine the conductivity of fractures in the existing technology and improves efficiency. Accuracy and production results.
Patent Information
- Application Number
- CN202410752913.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-12
- Publication Date
- 2024-10-11
AI Technical Summary
Existing technology cannot effectively determine the fracture conductivity of oil reservoirs under the action of closure stress, which affects production results.
Divide the fractures into multiple segmented fractures along the length of the reservoir, determine their initial fracture width and conductivity distribution, and determine the fracture width change and conductivity distribution under closure stress based on the post-attenuation model.
It improves the accuracy of determining fracture conductivity under the action of closing stress and helps measure and improve production results.
Smart Images

Figure CN118761346A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of oil and gas field development engineering, and in particular to a method and device for determining the fracture conductivity of an oil reservoir. Background Art
[0002] At present, in order to increase the production of oil reservoirs, reservoir transformation measures such as hydraulic fracturing are often taken. For example, for low permeability oil reservoirs, the reservoirs are dense, the pore throats are fine, and the permeability is low, which makes fluid flow difficult. Relevant reservoir transformation measures are needed to increase its production.
[0003] Specifically, after the relevant technology performs fracturing and backflow on the oil reservoir, the proppant will form propped cracks underground. During the production process, with the action of closing stresses such as formation stress and fluid stress, the cracks will close, resulting in a reduction in the fluid flow space and pore throat size, which will cause changes in the fracture conductivity and affect the production effect.
[0004] However, the relevant technology cannot effectively determine the conductivity of the fracture under the action of closure stress, which may lead to the inability to measure the impact on production results and improve production results. Summary of the invention
[0005] The present invention provides a method and device for determining the fracture conductivity of an oil reservoir, which are used to solve the defect that the fracture conductivity under the action of closure stress cannot be effectively determined in the related art, effectively determine the fracture conductivity under the action of closure stress, and improve the accuracy of the determination result.
[0006] In a first aspect, the present invention provides a method for determining fracture conductivity of an oil reservoir, comprising:
[0007] Dividing the fracture in the oil reservoir into a plurality of segmented fractures along the fracture length direction of the fracture;
[0008] For at least one of the segmented fractures, determining an initial fracture width distribution and an initial conductivity distribution of the segmented fracture along the fracture length direction, and determining a fracture width variation distribution of the segmented fracture along the fracture length direction under the action of a closing stress;
[0009] The initial fracture width distribution, the initial conductivity distribution and the fracture width variation distribution are input into the constructed fracture conductivity determination model after attenuation to determine the conductivity distribution of the segmented fracture along the fracture length direction under the action of closing stress.
[0010] Optionally, determining the initial conductivity distribution of the segmented fracture along the fracture length direction includes:
[0011] Determining a first conductivity distribution, a second conductivity distribution, and a third conductivity distribution of the segmented fracture, wherein the first conductivity distribution is an initial conductivity distribution of the segmented fracture along the fracture length direction in a linear mode, the second conductivity distribution is an initial conductivity distribution of the segmented fracture along the fracture length direction in an exponential mode, and the third conductivity distribution is an initial conductivity distribution of the segmented fracture along the fracture length direction in a logarithmic mode;
[0012] The first conductivity distribution, the second conductivity distribution and the third conductivity distribution are averaged, and the average calculation result is used as the initial conductivity distribution of the segmented fracture along the fracture length direction.
[0013] Optionally, the determining the distribution of crack width variation of the segmented crack along the crack length direction under the action of the closing stress includes:
[0014] By analogy with the relationship between stress and strain in a stress-strain model of a spring, an expression for the relationship between the change in the width of the segmented crack along the length direction of the crack and the closing stress under the action of the closing stress is determined;
[0015] Based on the closing stress and the relationship expression, the distribution of the seam width variation is determined.
[0016] Optionally, the model for determining the conductivity of the fracture after attenuation is:
[0017]
[0018] Wherein, x is the distance between the zero point position and the target position in the fracture length direction, which is used to identify the target position; w(x)1 is the initial fracture width expression of the segmented fracture along the fracture length direction; F CD (x)2 The conductivity expression of the segmented crack along the length direction of the crack under the action of closing stress, F CD (x)1 is the initial conductivity expression of the segmented fracture along the fracture length direction, V 净 is the proppant volume, L is the length of the segmented fracture, and H is the height of the segmented fracture; f(σ C ) is the fracture width deformation expression; b is a constant related to the fracturing process and proppant type.
[0019] Optionally, constructing the model for determining the conductivity of the fracture after attenuation includes:
[0020] Establish the distribution expressions of initial crack width and initial conductivity along the crack length direction;
[0021] Establishing a first relational expression between fracture conductivity and fracture permeability, and a second relational expression between the fracture width variation along the fracture length direction under the action of the closure stress and the closure stress;
[0022] Under the assumption that the proppant is not broken and the proppant volume is constant, the permeability change rate expression is established based on the Gozeny-Kalman equation and the correction coefficient.
[0023] The initial fracture width distribution expression, the initial conductivity distribution expression, the first relationship expression, the second relationship expression and the permeability change rate expression are combined to construct the post-attenuation fracture conductivity determination model.
[0024] In a second aspect, the present invention provides a device for determining fracture conductivity of an oil reservoir, comprising:
[0025] A division unit is used to divide the fracture into a plurality of segmented fractures along the fracture length direction of the fracture in the oil reservoir;
[0026] a first determining unit, configured to determine, for at least one of the segmented fractures, an initial fracture width distribution and an initial conductivity distribution of the segmented fracture along the fracture length direction, and determine a fracture width variation distribution of the segmented fracture along the fracture length direction under the action of a closing stress;
[0027] The second determination unit is used to input the initial fracture width distribution, the initial conductivity distribution and the fracture width variation distribution into the constructed fracture conductivity determination model after attenuation, so as to determine the conductivity distribution of the segmented fracture along the fracture length direction under the action of closing stress.
[0028] Optionally, the first determining unit is further configured to:
[0029] Determining a first conductivity distribution, a second conductivity distribution, and a third conductivity distribution of the segmented fracture, wherein the first conductivity distribution is an initial conductivity distribution of the segmented fracture along the fracture length direction in a linear mode, the second conductivity distribution is an initial conductivity distribution of the segmented fracture along the fracture length direction in an exponential mode, and the third conductivity distribution is an initial conductivity distribution of the segmented fracture along the fracture length direction in a logarithmic mode;
[0030] The first conductivity distribution, the second conductivity distribution and the third conductivity distribution are averaged, and the average calculation result is used as the initial conductivity distribution of the segmented fracture along the fracture length direction.
[0031] Optionally, the first determining unit is further configured to:
[0032] By analogy with the relationship between stress and strain in a stress-strain model of a spring, an expression for the relationship between the change in the width of the segmented crack along the length direction of the crack and the closing stress under the action of the closing stress is determined;
[0033] Based on the closing stress and the relationship expression, the distribution of the seam width variation is determined.
[0034] In a third aspect, the present invention provides a computer device, comprising: a memory and a processor, the memory and the processor being communicatively connected to each other, the memory storing computer instructions, and the processor executing the method for determining fracture conductivity of an oil reservoir layer according to the first aspect or any corresponding embodiment thereof by executing the computer instructions.
[0035] In a fourth aspect, the present invention provides a computer-readable storage medium having computer instructions stored thereon, the computer instructions being used to enable a computer to execute the method for determining fracture conductivity of an oil reservoir layer according to the first aspect or any corresponding embodiment thereof.
[0036] The method and device for determining the fracture conductivity of an oil reservoir provided by the present invention can divide the fracture into a plurality of segmented fractures along the fracture length direction of the fracture in the oil reservoir; determine the initial fracture width distribution and initial conductivity distribution of the segmented fracture along the fracture length direction, and determine the fracture width variation distribution of the segmented fracture along the fracture length direction under the action of closing stress; determine the conductivity distribution of the segmented fracture along the fracture length direction under the action of closing stress according to the initial fracture width distribution, initial conductivity distribution, fracture width variation distribution and the constructed fracture conductivity determination model after attenuation. The present invention can divide the fracture into a plurality of segmented fractures, determine the fracture conductivity distribution of the segmented fracture under the action of closing stress, effectively determine the fracture conductivity under the action of closing stress, and improve the accuracy of the determination result. BRIEF DESCRIPTION OF THE DRAWINGS
[0037] In order to more clearly illustrate the technical solutions in the present invention or the prior art, the following briefly introduces the drawings required for use in the embodiments or the description of the prior art. Obviously, the drawings described below are some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0038] Figure 1 A flow chart of a method for determining fracture conductivity of an oil reservoir provided by an embodiment of the present invention;
[0039] Figure 2 A schematic diagram of fracture segmentation provided by an embodiment of the present invention;
[0040] Figure 3 A schematic diagram of a curve showing the relationship between the position of a crack along the crack length direction and the crack width provided by an embodiment of the present invention;
[0041] Figure 4 A schematic diagram of fracture conductivity distribution provided by an embodiment of the present invention;
[0042] Figure 5 A schematic diagram of a crack width variation curve under different closing stresses provided by an embodiment of the present invention;
[0043] Figure 6 A curve showing the change of fracture conductivity under different closure stresses provided by an embodiment of the present invention;
[0044] Figure 7 A schematic diagram of the distribution of flow conductivity at different closing stresses and different positions provided by an embodiment of the present invention;
[0045] Figure 8 A schematic diagram of the structure of a device for determining fracture conductivity of an oil reservoir provided by an embodiment of the present invention;
[0046] Fig. 9 A schematic diagram of the structure of a computer device provided in an embodiment of the present invention. DETAILED DESCRIPTION
[0047] In order to make the purpose, technical solution and advantages of the present invention clearer, the technical solution of the present invention will be clearly and completely described below in conjunction with the drawings of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0048] Combine the following Figure 1-Figure 7 The present invention describes a method for determining fracture conductivity of an oil reservoir.
[0049] like Figure 1 As shown, this embodiment proposes a first method for determining fracture conductivity of an oil reservoir, which may include the following steps:
[0050] S101. Divide the fracture in the oil reservoir into a plurality of segmented fractures along the fracture length direction of the fracture.
[0051] The oil reservoir may be an oil reservoir for which fracture conductivity needs to be determined, and may specifically be a low permeability oil reservoir.
[0052] Specifically, the fracture may be a relatively long fracture in the oil reservoir, such as a 10-meter-long fracture.
[0053] It should be noted that since the width and conductivity of the cracks vary non-uniformly, the overall calculation method cannot be used for calculation.
[0054] like Figure 2 As shown in the schematic diagram of fracture segmentation, in this embodiment, the fracture can be first divided into multiple segmented fractures along its length direction, and then the conductivity of each segmented fracture can be determined respectively. Among them, the lengths of the multiple segmented fractures can be equal or unequal.
[0055] S102. For at least one segmented fracture, determine an initial fracture width distribution and an initial conductivity distribution of the segmented fracture along the fracture length direction, and determine a fracture width variation distribution of the segmented fracture along the fracture length direction under the action of closing stress.
[0056] Specifically, this embodiment can first determine the crack width corresponding to the position where the length of the segmented crack is 0 in the crack length direction, and determine the length of the segmented crack, and then establish the initial crack width distribution of the segmented crack along the crack length direction based on the determined crack width, length and PKN crack model.
[0057] Specifically, the initial crack width distribution can be expressed as:
[0058]
[0059] Among them, x is the distance between the zero point position and the target position in the crack length direction, which is used to identify the target position, w(x) is the crack width corresponding to x, and w(0) is the crack width corresponding to the zero point position. L is the length of the segmented crack.
[0060] This embodiment can obtain Figure 3 The relationship curve between the position of the crack along the crack length and the crack width is shown in Figure 1, where Figure 3 The m here represents the length unit meter.
[0061] Optionally, determining the initial conductivity distribution of the segmented fracture along the fracture length direction includes:
[0062] Determine a first conductivity distribution, a second conductivity distribution, and a third conductivity distribution of the segmented fracture, wherein the first conductivity distribution is an initial conductivity distribution of the segmented fracture along the fracture length direction in a linear mode, the second conductivity distribution is an initial conductivity distribution of the segmented fracture along the fracture length direction in an exponential mode, and the third conductivity distribution is an initial conductivity distribution of the segmented fracture along the fracture length direction in a logarithmic mode;
[0063] The first conductivity distribution, the second conductivity distribution and the third conductivity distribution are averaged, and the average calculation result is used as the initial conductivity distribution of the segmented fracture along the fracture length direction.
[0064] It should be noted that the fracture conductivity can be expressed as:
[0065] F cD =w*k f ----------Formula (2)
[0066] F CD is the fracture conductivity, k f is the fracture permeability.
[0067] The conductivity of the crack at different positions along the length of the crack has three changing trends: linear change, logarithmic change, and exponential change. Among them:
[0068] Straight line mode: F cD (x) = -ax + F CD (0)--------------------------Formula (3);
[0069] Exponential mode: F CD (x) = F CD (0)×exp(-bx)----------------Formula (4);
[0070] Logarithmic mode: F CD (x) = F CD (0)×[1-clog(x+1)]----------Formula (5).
[0071] Among them, a, b and c are constants related to the fracturing process and proppant type.
[0072] like Figure 4 The schematic diagram of fracture conductivity distribution shown in FIG. 1 includes conductivity distributions corresponding to the linear model, the exponential model and the logarithmic model, wherein the linear model, the exponential model and the logarithmic model correspond to the linear mode, the exponential mode and the logarithmic mode, respectively. Figure 4 The x in is the above x, which can be used to identify a certain position in the seam length direction.
[0073] Specifically, in this embodiment, the calculation results of three empirical formula fitting models, namely, the linear mode, the exponential mode and the logarithmic mode, can be averaged according to the designed fracture length of the fracture to obtain the initial fracture cracks and conductivity distribution.
[0074] Specifically, the initial fracture conductivity at different positions along the fracture length direction is calculated, and the fracture widths at different positions calculated by the PKN model are used to obtain the initial permeability distribution. Specifically, in this embodiment, the PKN model is used to calculate the fracture widths at different positions along the fracture length direction, and then the average of the calculation results of three fracture conductivity distribution calculation models, namely the linear model, the exponential model, and the logarithmic model, along the fracture length direction is taken to obtain the initial conductivity inside the fracture. Combining the fracture width calculated by the PKN model, the initial fracture permeability inside the fracture is obtained.
[0075] It can be understood that in this embodiment, the initial fracture width can be calculated by the PKN model, and the initial permeability can be calculated by the linear model, the exponential model, and the logarithmic model.
[0076] Optionally, determining the distribution of the fracture width change amount along the fracture length direction under the closing stress for the segmented fracture includes:
[0077] Based on the analogy of the relationship between stress and strain in the stress-strain model of the spring, determine the relationship expression between the fracture width change amount and the closing stress along the fracture length direction under the closing stress for the segmented fracture;
[0078] Based on the closing stress and the relationship expression, determine the distribution of the fracture width change amount.
[0079] It should be noted that during the process of compressing the spring, the spring will undergo three deformation stages under the action of an external force, namely elastic deformation, elastoplastic deformation, and plastic deformation. And the process of the supporting fracture being compacted and embedded in the formation under the closing stress also undergoes three deformation processes including elastic deformation, elastoplastic deformation, and plastic deformation. Among them, the elastoplastic model mechanism is complex and is obtained by linearly differentiating the end point of the elastic stage and the starting point of the plastic stage. By analogy, the fracture stress-strain model based on the spring model is obtained:
[0080] Elastic stage: σ C = E'd d < d1 --------------------------- Formula (6);
[0081] Elastoplastic stage: σ C = c1 + c2ln d d1 ≤ d ≤ d2 -------- Formula (7);
[0082] Plastic stage: σ C = 3σ y d2 < d -------------------------- Formula (8);
[0083] E': Generalized elastic modulus.
[0084]
[0085] c1, c2: interpolation coefficients. d is the spring deformation. σ C is the contact stress. y is the compressive strength of the proppant.
[0086] Then the spring deformation d can be expressed as stress σ C Function:
[0087] d=f(σ C )--------------------------------Formula (10);
[0088] Among them, d1 and d2 are variables related to d. Among them:
[0089]
[0090] d2=82.5d1------------------------Formula (11.2).
[0091] S103, inputting the initial fracture width distribution, the initial conductivity distribution and the fracture width variation distribution into the constructed fracture conductivity determination model after attenuation, so as to determine the conductivity distribution of the segmented fracture along the fracture length direction under the action of closing stress.
[0092] Among them, the model for determining the conductivity of fractures after attenuation is:
[0093]
[0094] Where x is the distance between the zero point and the target position in the fracture length direction, which is used to identify the target position; w(x)1 is the initial fracture width expression of the segmented fracture along the fracture length direction; F CD (x)2 The expression of the conductivity of a segmented crack along the length of the crack under the action of closing stress, F CD (x)1 is the expression of the initial conductivity of the segmented fracture along the fracture length direction, V 净 is the proppant volume, L is the length of the segmented fracture, and H is the height of the segmented fracture; f(σ C ) is the fracture width deformation expression; b is a constant related to the fracturing process and proppant type.
[0095] Optionally, a model for determining fracture conductivity after attenuation is constructed, including:
[0096] Establish the distribution expressions of initial crack width and initial conductivity along the crack length direction;
[0097] Establishing a first relational expression between fracture conductivity and fracture permeability, and a second relational expression between the fracture width variation along the fracture length direction under the action of the closure stress and the closure stress;
[0098] Under the assumption that the proppant is not broken and the proppant volume is constant, the permeability change rate expression is established based on the Gozeny-Kalman equation and the correction coefficient.
[0099] The initial fracture width distribution expression, the initial conductivity distribution expression, the first relationship expression, the second relationship expression and the permeability change rate expression are combined to construct a model for determining the conductivity of fractures after attenuation.
[0100] Specifically, in this embodiment, after establishing the above formulas (1) to (11), under the assumption that the proppant does not break in the propped fracture, the porosity in the fracture is:
[0101]
[0102] V 净 V is the volume of proppant. f is the volume of hydraulic fracture. H is the fracture height.
[0103] During the crack closure process, the volume of the proppant remains unchanged, while the volume of the hydraulic fracture shrinks, so the change in porosity inside the hydraulic fracture is .
[0104]
[0105] is the porosity change.
[0106] The stress-strain model used in this embodiment obtains the relationship between different deformation variables and fracture support stress, obtains the fracture permeability change rate based on the Gozeny-Kalman equation, and introduces a correction coefficient b to correct the model.
[0107] The Gozeny-Kalman formula:
[0108]
[0109] K is the permeability. is the porosity. r is the average capillary radius. τ is the tortuosity, ranging from 1 to 1.4.
[0110] This embodiment can obtain Figure 5 The crack width variation curve under different closing stresses is shown in Figure 2.
[0111]
[0112] a is the permeability change rate, b is the correction coefficient. The fracture permeability after attenuation is:
[0113] k2=k1a--------------------Formula (17).
[0114] Specifically, this embodiment can obtain the attenuated fracture conductivity determination model of formula (12) based on formula (1) to formula (11.1) and (11.2), and based on formula (13) to formula (17):
[0115]
[0116] It can be understood that this embodiment constructs a crack stress-strain model by analogy with the spring deformation mode, calculates the change in crack closure and crack volume under different stress conditions, and calculates the degree of change in crack conductivity by combining the Gotzeni-Kalman equation.
[0117] Specifically, this embodiment can obtain the following Figure 6 The variation curve of crack conductivity under different closing stresses is shown in FIG. Figure 7 The diagram shows the distribution of flow conductivity at different closing stresses and different positions. Figure 7 The figure includes the conductivity change curves at different positions along the fracture length when the closing stress is 0, 15, 30, 45, 60, 75, 90 and 105 MPa (i.e., megapascals). Figure 7 This is the conductivity stress sensitivity chart.
[0118] Specifically, this embodiment can calculate the distribution of the flow conductivity of each segmented fracture along the fracture length direction under the action of the closing stress for each segmented fracture obtained by division.
[0119] It is understandable that this embodiment divides the fracture into multiple segmented fractures, and obtains the stress sensitivity prediction of fracture conductivity at different positions along the fracture length by segmented calculation. This embodiment can perform quantitative prediction of conductivity attenuation considering the spatial variation of the hydraulic fracture.
[0120] The method for determining the fracture conductivity of an oil reservoir proposed in this embodiment can divide the fracture into multiple segmented fractures along the fracture length direction of the fracture in the oil reservoir; determine the initial fracture width distribution and initial conductivity distribution of the segmented fracture along the fracture length direction, and determine the fracture width variation distribution of the segmented fracture along the fracture length direction under the action of closing stress; determine the conductivity distribution of the segmented fracture along the fracture length direction under the action of closing stress according to the initial fracture width distribution, initial conductivity distribution, fracture width variation distribution and the constructed fracture conductivity determination model after attenuation. This embodiment can divide the fracture into multiple segmented fractures, determine the fracture conductivity distribution of the segmented fracture under the action of closing stress, effectively determine the fracture conductivity under the action of closing stress, and improve the accuracy of the determination result.
[0121] like Figure 8 As shown, this embodiment provides a device for determining the fracture conductivity of an oil reservoir, which may include:
[0122] A division unit is used to divide the fracture into a plurality of segmented fractures along the fracture length direction of the fracture in the oil reservoir;
[0123] A first determining unit is used to determine, for at least one segmented fracture, an initial fracture width distribution and an initial conductivity distribution of the segmented fracture along the fracture length direction, and to determine a fracture width variation distribution of the segmented fracture along the fracture length direction under the action of a closing stress;
[0124] The second determination unit is used to input the initial fracture width distribution, the initial conductivity distribution and the fracture width variation distribution into the constructed fracture conductivity determination model after attenuation to determine the conductivity distribution of the segmented fracture along the fracture length direction under the action of the closing stress.
[0125] It should be noted that the processing of the division unit, the first determination unit and the second determination unit and the beneficial effects thereof can be respectively referred to in Figure 1 Steps S101 to S103 in the above are not described in detail.
[0126] Optionally, the first determining unit is further configured to:
[0127] Determine a first conductivity distribution, a second conductivity distribution, and a third conductivity distribution of the segmented fracture, wherein the first conductivity distribution is an initial conductivity distribution of the segmented fracture along the fracture length direction in a linear mode, the second conductivity distribution is an initial conductivity distribution of the segmented fracture along the fracture length direction in an exponential mode, and the third conductivity distribution is an initial conductivity distribution of the segmented fracture along the fracture length direction in a logarithmic mode;
[0128] The first conductivity distribution, the second conductivity distribution and the third conductivity distribution are averaged, and the average calculation result is used as the initial conductivity distribution of the segmented fracture along the fracture length direction.
[0129] Optionally, the first determining unit is further configured to:
[0130] Based on the analogy between the stress and strain in the stress-strain model of the spring, the relationship expression between the change in the crack width along the crack length direction and the closing stress under the action of the closing stress is determined;
[0131] Based on the closing stress and the relational expression, the distribution of the crack width variation is determined.
[0132] Optionally, the model for determining fracture conductivity after attenuation is:
[0133]
[0134] Where x is the distance between the zero point and the target position in the fracture length direction, which is used to identify the target position; w(x)1 is the initial fracture width expression of the segmented fracture along the fracture length direction; F CD (x)2 The expression of the conductivity of a segmented crack along the length of the crack under the action of closing stress, F CD (x)1 is the expression of the initial conductivity of the segmented fracture along the fracture length direction, V 净 is the proppant volume, L is the length of the segmented fracture, and H is the height of the segmented fracture; f(σ C ) is the fracture width deformation expression; b is a constant related to the fracturing process and proppant type.
[0135] Optionally, a model for determining fracture conductivity after attenuation is constructed and set as:
[0136] Construct a model to determine the conductivity of fractures after attenuation, including:
[0137] Establish the distribution expressions of initial crack width and initial conductivity along the crack length direction;
[0138] Establishing a first relational expression between fracture conductivity and fracture permeability, and a second relational expression between the fracture width variation along the fracture length direction under the action of the closure stress and the closure stress;
[0139] Under the assumption that the proppant is not broken and the proppant volume is constant, the permeability change rate expression is established based on the Gozeny-Kalman equation and the correction coefficient.
[0140] The initial fracture width distribution expression, the initial conductivity distribution expression, the first relationship expression, the second relationship expression and the permeability change rate expression are combined to construct a model for determining fracture conductivity after attenuation.
[0141] The fracture conductivity determination device of the oil reservoir proposed in this embodiment can divide the fracture into multiple segmented fractures along the fracture length direction of the fracture in the oil reservoir; determine the initial fracture width distribution and initial conductivity distribution of the segmented fracture along the fracture length direction, and determine the fracture width variation distribution of the segmented fracture along the fracture length direction under the action of closing stress; determine the conductivity distribution of the segmented fracture along the fracture length direction under the action of closing stress according to the initial fracture width distribution, initial conductivity distribution, fracture width variation distribution and the constructed fracture conductivity determination model after attenuation. This embodiment can divide the fracture into multiple segmented fractures, determine the fracture conductivity distribution of the segmented fracture under the action of closing stress, effectively determine the fracture conductivity under the action of closing stress, and improve the accuracy of the determination result.
[0142] The device for determining the fracture conductivity of an oil reservoir in this embodiment is presented in the form of a functional unit, where the unit refers to an ASIC (Application Specific Integrated Circuit) circuit, a processor and a memory that executes one or more software or fixed programs, and / or other devices that can provide the above functions.
[0143] The embodiment of the present invention also provides a computer device having the above Figure 8 The device for determining the fracture conductivity of an oil reservoir is shown.
[0144] See also Fig. 9 , a schematic diagram of the structure of a computer device provided by an optional embodiment of the present invention, the computer device includes: one or more processors 10, a memory 20, and interfaces for connecting various components, including high-speed interfaces and low-speed interfaces. The various components are connected to each other using different buses for communication, and can be installed on a common motherboard or installed in other ways as needed. The processor can process instructions executed in the computer device, including instructions stored in or on the memory to display graphical information of the GUI on an external input / output device (such as a display device coupled to the interface). In some optional embodiments, if necessary, multiple processors and / or multiple buses can be used together with multiple memories and multiple memories. Similarly, multiple computer devices can be connected, and each device provides part of the necessary operations (for example, as a server array, a group of blade servers, or a multi-processor system). Fig. 9 A processor 10 is taken as an example.
[0145] The processor 10 may be a central processing unit, a network processor or a combination thereof. The processor 10 may further include a hardware chip. The hardware chip may be a dedicated integrated circuit, a programmable logic device or a combination thereof. The programmable logic device may be a complex programmable logic device, a field programmable gate array, a general purpose array logic or any combination thereof.
[0146] The memory 20 stores instructions executable by at least one processor 10, so that at least one processor 10 executes the method shown in the above embodiment.
[0147] The memory 20 may include a program storage area and a data storage area, wherein the program storage area may store an operating system, an application required for at least one function. The data storage area may store data created according to the use of the computer device, etc. In addition, the memory 20 may include a high-speed random access memory, and may also include a non-transient memory, such as at least one disk storage device, a flash memory device, or other non-transient solid-state storage devices. In some optional embodiments, the memory 20 may optionally include a memory remotely arranged relative to the processor 10, and these remote memories may be connected to the computer device via a network. Examples of the above-mentioned network include, but are not limited to, the Internet, an intranet, a local area network, a mobile communication network, and combinations thereof.
[0148] The memory 20 may include a volatile memory, such as a random access memory. The memory may also include a non-volatile memory, such as a flash memory, a hard disk or a solid state drive. The memory 20 may also include a combination of the above-mentioned types of memory.
[0149] The computer device further comprises a communication interface 30 for the computer device to communicate with other devices or a communication network.
[0150] The embodiment of the present invention also provides a computer-readable storage medium. The method according to the embodiment of the present invention can be implemented in hardware, firmware, or can be implemented as a computer code that can be recorded in a storage medium, or can be implemented as a computer code that is originally stored in a remote storage medium or a non-temporary machine-readable storage medium and will be stored in a local storage medium through a network download, so that the method described herein can be stored in such software processing on a storage medium using a general-purpose computer, a dedicated processor, or programmable or dedicated hardware. Among them, the storage medium can be a magnetic disk, an optical disk, a read-only storage memory, a random access memory, a flash memory, a hard disk or a solid-state hard disk, etc.; further, the storage medium can also include a combination of the above types of memories. It can be understood that a computer, a processor, a microprocessor controller, or programmable hardware includes a storage component that can store or receive software or computer code. When the software or computer code is accessed and executed by a computer, a processor, or hardware, the method shown in the above embodiment is implemented.
[0151] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present invention.
Claims
1. A method for determining the fracture conductivity of an oil reservoir. It is characterized in that include: Dividing the fracture in the oil reservoir into a plurality of segmented fractures along the fracture length direction of the fracture; For at least one of the segmented fractures, determining an initial fracture width distribution and an initial conductivity distribution of the segmented fracture along the fracture length direction, and determining a fracture width variation distribution of the segmented fracture along the fracture length direction under the action of a closing stress; The initial fracture width distribution, the initial conductivity distribution and the fracture width variation distribution are input into the constructed fracture conductivity determination model after attenuation to determine the conductivity distribution of the segmented fracture along the fracture length direction under the action of closing stress.
2. The method according to claim 1, It is characterized in that Determining the initial conductivity distribution of the segmented fracture along the fracture length direction includes: Determining a first conductivity distribution, a second conductivity distribution, and a third conductivity distribution of the segmented fracture, wherein the first conductivity distribution is an initial conductivity distribution of the segmented fracture along the fracture length direction in a linear mode, the second conductivity distribution is an initial conductivity distribution of the segmented fracture along the fracture length direction in an exponential mode, and the third conductivity distribution is an initial conductivity distribution of the segmented fracture along the fracture length direction in a logarithmic mode; The first conductivity distribution, the second conductivity distribution and the third conductivity distribution are averaged, and the average calculation result is used as the initial conductivity distribution of the segmented fracture along the fracture length direction.
3. The method according to claim 1, It is characterized in that The determining of the distribution of the crack width variation of the segmented crack along the crack length direction under the action of the closing stress comprises: By analogy with the relationship between stress and strain in a stress-strain model of a spring, an expression for the relationship between the change in the width of the segmented crack along the length direction of the crack and the closing stress under the action of the closing stress is determined; Based on the closing stress and the relationship expression, the distribution of the seam width variation is determined.
4. The method according to claim 1, It is characterized in that The model for determining the conductivity of the fracture after attenuation is: Wherein, x is the distance between the zero point position and the target position in the slit length direction, which is used to identify the target position; w(x) 1 is the initial crack width expression of the segmented crack along the crack length direction; F CD (x) 2 The conductivity expression of the segmented crack along the length direction of the crack under the action of closing stress is: CD (x) 1 is the initial conductivity expression of the segmented fracture along the fracture length direction, V 净 is the proppant volume, L is the length of the segmented fracture, and H is the height of the segmented fracture; f(σ C ) is the fracture width deformation expression; b is a constant related to the fracturing process and proppant type.
5. The method according to claim 1, It is characterized in that Constructing the model for determining the conductivity of the fracture after attenuation, including: Establish the distribution expressions of initial crack width and initial conductivity along the crack length direction; Establishing a first relational expression between fracture conductivity and fracture permeability, and a second relational expression between the fracture width variation along the fracture length direction under the action of the closure stress and the closure stress; Under the assumption that the proppant is not broken and the proppant volume is constant, the permeability change rate expression is established based on the Gozeny-Kalman equation and the correction coefficient. The initial fracture width distribution expression, the initial conductivity distribution expression, the first relationship expression, the second relationship expression and the permeability change rate expression are combined to construct the post-attenuation fracture conductivity determination model.
6. A device for determining the fracture conductivity of an oil reservoir, It is characterized in that include: A division unit is used to divide the fracture into a plurality of segmented fractures along the fracture length direction of the fracture in the oil reservoir; a first determining unit, configured to determine, for at least one of the segmented fractures, an initial fracture width distribution and an initial conductivity distribution of the segmented fracture along the fracture length direction, and determine a fracture width variation distribution of the segmented fracture along the fracture length direction under the action of a closing stress; The second determination unit is used to input the initial fracture width distribution, the initial conductivity distribution and the fracture width variation distribution into the constructed fracture conductivity determination model after attenuation, so as to determine the conductivity distribution of the segmented fracture along the fracture length direction under the action of closing stress.
7. The device according to claim 6, It is characterized in that The first determining unit is further configured to: Determining a first conductivity distribution, a second conductivity distribution, and a third conductivity distribution of the segmented fracture, wherein the first conductivity distribution is an initial conductivity distribution of the segmented fracture along the fracture length direction in a linear mode, the second conductivity distribution is an initial conductivity distribution of the segmented fracture along the fracture length direction in an exponential mode, and the third conductivity distribution is an initial conductivity distribution of the segmented fracture along the fracture length direction in a logarithmic mode; The first conductivity distribution, the second conductivity distribution and the third conductivity distribution are averaged, and the average calculation result is used as the initial conductivity distribution of the segmented fracture along the fracture length direction.
8. The device according to claim 6, It is characterized in that The first determining unit is further configured to: By analogy with the relationship between stress and strain in a stress-strain model of a spring, an expression for the relationship between the change in the width of the segmented crack along the length direction of the crack and the closing stress under the action of the closing stress is determined; Based on the closing stress and the relationship expression, the distribution of the seam width variation is determined.
9. A computer device, It is characterized in that include: A memory and a processor, wherein the memory and the processor are communicatively connected to each other, the memory stores computer instructions, and the processor executes the method for determining fracture conductivity of an oil reservoir layer according to any one of claims 1 to 6 by executing the computer instructions.
10. A computer-readable storage medium, It is characterized in that The computer-readable storage medium stores computer instructions, and the computer instructions are used to enable a computer to execute the method for determining fracture conductivity of an oil reservoir according to any one of claims 1 to 6.
Citation Information
Patent Citations
Method for testing visualized propping fracture flow conductivity
CN108571314A
A water injection induced dynamic fracture variable flow conductivity calculation method for a low-permeability reservoir
CN113743037A
Shale reservoir fracture conductivity evaluation method
CN116029107A
Method for calculating fracture conductivity based on proppant form
CN116205077A
Method for evaluating flow conductivity of proppant under consideration of stress disturbance
CN117113717A