Micro device substrate
By arranging micro-particle areas on the micro-device substrate of the display panel, the contact area between the light-emitting element and the adhesive layer is reduced, which solves the problem of difficulty in removing the offset light-emitting element and improves the transfer efficiency and recycling rate.
Patent Information
- Application Number
- CN202410841646.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-26
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2044-06-26
AI Technical Summary
Existing display panels are prone to misalignment during the transfer process of light-emitting elements, resulting in strong adhesion between the misaligned light-emitting elements and the receiving device, making them difficult to remove, affecting transfer efficiency and difficulty in repair.
Design a micro device substrate, including a base and a first glue layer on one side. The first glue layer along a direction parallel to the base includes a plurality of chip transfer areas and micro-particle areas located between the chip transfer areas. Within the micro-particle area The micro-particles are located on the side of the adhesive layer away from the substrate, which are used to reduce the contact area between the light-emitting element and the adhesive layer and facilitate removal by water washing.
The contact area between the light-emitting element and the adhesive layer is reduced through the spacing of the micro-particle areas, simplifying the removal process, reducing the difficulty of repair, and improving the recycling rate of the micro-device substrate and the transfer efficiency of the light-emitting element.
Smart Images

Figure CN118763166A_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to the field of display technology, and in particular to a micro-device substrate. Background Art
[0002] At present, display panels are widely used in electronic devices such as mobile phones, tablet computers, and smart wearable devices. A common display panel includes a light-emitting element and a driving circuit coupled to the light-emitting element, and the driving circuit drives the light-emitting element to emit light, and the light-emitting element includes a red light-emitting element, a green light-emitting element, and a blue light-emitting element.
[0003] In the process of preparing the existing display panel, the light-emitting elements will inevitably be misaligned during the process of transferring the light-emitting elements to the circuit substrate. These misaligned light-emitting elements are stuck to the receiving glue like normal light-emitting elements and are difficult to remove, which affects the transfer efficiency. Summary of the invention
[0004] In order to solve the above technical problems, the present disclosure provides a micro-device substrate, which can reduce the viscosity of the offset light-emitting element and the receiving glue, facilitate removal, reduce the difficulty of repair, and improve the transfer efficiency.
[0005] The present disclosure provides a micro-device substrate, comprising: a base and a first adhesive layer disposed on one side of the base;
[0006] Along a direction parallel to the plane where the substrate is located, the first adhesive layer includes a plurality of chip transfer areas and micro-particle areas located between the chip transfer areas, the light-emitting element is located in the chip transfer area, and the light-emitting element is bonded to the first adhesive layer;
[0007] The micro-particle region includes micro-particles, and the micro-particles are located on a side of the first glue layer facing away from the substrate.
[0008] The technical solution provided by the embodiment of the present disclosure has the following advantages compared with the prior art: by setting a micro-particle area outside the chip transfer area, when the transferred light-emitting element has an unregulated offset or deflection, it will cause such light-emitting element and the micro-particle area to have an overlapping area in a direction perpendicular to the first adhesive layer. The contact area between such light-emitting element and the first adhesive layer can be reduced by the spacing of the micro-particles, making it easier to be removed by water washing, reducing the difficulty of repairing the micro-device substrate, and improving the recycling rate of the micro-device substrate and the transfer efficiency of the light-emitting element. BRIEF DESCRIPTION OF THE DRAWINGS
[0009] The accompanying drawings, which are incorporated in and constitute a part of this specification, illustrate embodiments consistent with the present disclosure and, together with the description, serve to explain the principles of the present disclosure.
[0010] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, for ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative labor.
[0011] Figure 1 A top view of the micro-device substrate according to an embodiment of the present disclosure;
[0012] Figure 2 for Figure 1 Sectional view along section A-A';
[0013] Figure 3 A schematic diagram of the structure of a light-emitting element provided in an embodiment of the present disclosure;
[0014] Figure 4 for Figure 1 A diagram showing the relative position relationship between the light emitting element and the micro-particle region along the A-A' section;
[0015] Figure 5 A schematic diagram showing the relationship between the diameter of the groove of the light-emitting substrate and the diameter of the micro-particles of the light-emitting element according to the embodiment of the present disclosure;
[0016] Figure 6 A schematic diagram showing the relationship between the widths of the transfer precision zones corresponding to different light-emitting elements according to the embodiment of the present disclosure;
[0017] Figure 7 A schematic diagram showing the difference in particle sizes of micro-particles around different light-emitting elements according to the embodiments of the present disclosure;
[0018] Figure 8 A schematic diagram of a process of transferring a light-emitting element from a source substrate to a temporary substrate according to an embodiment of the present disclosure;
[0019] Fig. 9 A schematic diagram of a process of transferring a light-emitting element from a temporary substrate to a transient substrate according to an embodiment of the present disclosure;
[0020] Fig.10 It is a schematic diagram of the process of transferring the light-emitting element from the temporary substrate to the array substrate according to the embodiment of the present disclosure. DETAILED DESCRIPTION
[0021] In order to more clearly understand the above-mentioned objectives, features and advantages of the present disclosure, the scheme of the present disclosure will be further described below. It should be noted that the embodiments of the present disclosure and the features in the embodiments can be combined with each other without conflict.
[0022] In the following description, many specific details are set forth to facilitate a full understanding of the present disclosure, but the present disclosure may also be implemented in other ways different from those described herein; it is obvious that the embodiments in the specification are only part of the embodiments of the present disclosure, rather than all of the embodiments.
[0023] In the production process of a display device including a light-emitting element (such as a Micro LED), the light-emitting element needs to be transferred to a circuit substrate by mass transfer and bound to the circuit substrate. Prior to this, the light-emitting element needs to be transferred to an intermediate substrate. The micro-device substrate mentioned in the present disclosure can be regarded as an intermediate substrate carrying a number of light-emitting elements. The side of the light-emitting element without an electrode pin is fixed to the micro-device substrate by a first adhesive layer. The light-emitting element on the micro-device substrate can be transferred to the corresponding circuit substrate through the micro-device substrate, so that the electrode pins of the light-emitting element are bound to the circuit substrate. After the light-emitting element is transferred to the intermediate substrate, the light-emitting element may be positionally shifted to form a defective light-emitting element. Both the defective light-emitting element and the normal light-emitting element are attached to the intermediate substrate. It is difficult to remove the defective light-emitting element by simple water washing. If it is removed by laser, it may cause damage to the adhesive layer in the middle and cannot be repaired in situ. Therefore, the present disclosure provides a micro-device substrate for solving the above-mentioned technical problems.
[0024] Figure 1 is a top view of the micro-device substrate according to an embodiment of the present disclosure, Figure 2 for Figure 1 For the cross-sectional view along section A-A', please refer to Figure 1 and Figure 2 , the present disclosure provides a micro-device substrate 100, comprising a base 10 and a first adhesive layer 20 disposed on one side of the base 10;
[0025] Along a direction parallel to the plane where the substrate 10 is located, the first adhesive layer 20 includes a plurality of chip transfer areas 30 and micro particle areas 60 located between the chip transfer areas 30, the light emitting element 40 is located in the chip transfer area 30, and the light emitting element 40 is bonded to the first adhesive layer 20;
[0026] The micro-particle region 60 includes micro-particles 70 . The micro-particles 70 are located on a side of the first adhesive layer 20 facing away from the substrate 10 .
[0027] It should be noted that Figure 1 Only a top view structure of the micro-device substrate is illustrated, and the actual shape of the micro-device substrate is not limited. In some other embodiments of the present disclosure, the micro-device substrate can also be embodied in other shapes besides a rectangle, such as a circle. In addition, Figure 1The light-emitting elements on the micro-device substrate are only illustrated, and the number and shape of the light-emitting elements actually included on the micro-device substrate are not limited. The present disclosure only shows a scheme in which the light-emitting elements include red light-emitting elements, green light-emitting elements, and blue light-emitting elements, but does not limit this. In some other embodiments of the present disclosure, the light-emitting elements can also be set to other colors as required, or in addition to red, green and blue light-emitting elements, light-emitting elements of other colors can also be included. Of course, the arrangement of the light-emitting elements on the micro-device substrate is also only for illustration, and can also be set to other arrangements according to actual needs.
[0028] For more information, see Figure 1 and Figure 2 The micro-device substrate 100 mentioned in the present disclosure includes a substrate 10 and a first adhesive layer 20, wherein the first adhesive layer 20 is located on a surface of one side of the substrate 10, and the light-emitting element 40 is fixed on the micro-device substrate 100 through the first adhesive layer 20. In a direction parallel to the plane where the substrate 10 is located, the first adhesive layer 20 includes a plurality of chip transfer areas 30, and optionally, the plurality of chip transfer areas 30 are arranged in an array on the plane where the first adhesive layer 20 is located, wherein the light-emitting element 40 is located in the chip transfer area 30, and the light-emitting element 40 is bonded to the first adhesive layer 20 in the chip transfer area 30.
[0029] The first adhesive layer 20 further includes a micro-particle area 60, which is located between the plurality of chip transfer areas 30. All areas on the first adhesive layer 20 except the chip transfer area 30 can be regarded as the micro-particle area 60. Optionally, each chip transfer area 30 is surrounded by the micro-particle area 60, and the micro-particle area 60 includes micro-particles 70. The micro-particles 70 are located on the side of the first adhesive layer 20 away from the substrate 10, and at least part of the surface of the micro-particles 70 protrudes from the first adhesive layer 20. In this way, by providing a plurality of chip transfer areas 30 and the micro-particle area 60 located between the plurality of chip transfer areas 30 on the first adhesive layer 20 in the micro-device substrate 100, in the process of using the present disclosure, During the process of transferring the light-emitting element 40 to the micro-device substrate 100, if the light-emitting element 40 is dislocated (for example, tilted), the inclined surface of this part of the light-emitting element 40 will be able to contact the micro-particles 70 protruding from the surface of the first adhesive layer 20 in the micro-particle area 60, rather than directly contacting the first adhesive layer 20, thereby reducing the contact area between the tilted and offset light-emitting element and the first adhesive layer 20, thereby reducing the adhesion of the dislocated light-emitting element, facilitating the removal of the dislocated light-emitting element in the later process, which is beneficial to reducing the difficulty of repairing the micro-device substrate, improving the recycling rate of the micro-device substrate, and improving the transfer efficiency of the light-emitting element, thereby helping to improve production efficiency.
[0030] Please continue to refer to Figure 1 to Figure 2In an optional embodiment provided by the present disclosure, the micro-particle region 60 in the micro-device substrate 100 includes at least two micro-particles 70 of different particle sizes.
[0031] Specifically, the micro-device substrate 100 includes a base 10 and a first adhesive layer 20 located on one side of the base 10. Along the direction of the plane where the base 10 is located, the first adhesive layer 20 includes a plurality of chip transfer areas 30. The first adhesive layer 20 also includes a micro-particle area 60. The micro-particle area 60 is located between the plurality of chip transfer areas 30, and each chip transfer area 30 is surrounded by the micro-particle area 60. The micro-particles 70 of the micro-particle area 60 include at least two different particle sizes. For example, the micro-particles 70 may include 2 different particle sizes, the micro-particles 70 may include 3 different particle sizes, the micro-particles 70 may include 4 different particle sizes... They are not listed one by one here, but only It is sufficient that the micro-particles 70 include at least two or more different particle sizes. In this way, the micro-particle area 60 located on the side of the first adhesive layer 20 away from the substrate 10 includes at least two different particle sizes, so that the heights of the micro-particles 70 with different particle sizes protruding from the surface of the first adhesive layer 20 are inconsistent. When the tilted light-emitting element is at least partially located outside the chip transfer area 30, compared with the micro-particles 70 with the same diameter, the micro-particles 70 with different particle sizes protrude from the surface of the first adhesive layer 20 and present a height difference, which can further reduce the contact area between the first adhesive layer 20 and the tilted light-emitting element, and facilitate the removal of the tilted light-emitting element in the subsequent process.
[0032] Figure 3 is a schematic diagram of the structure of a light-emitting element provided in an embodiment of the present disclosure, Figure 4 for Figure 1 For the relative position relationship diagram of the light emitting element and the micro-particle area along the A-A' section, please refer to Figures 1 to 4 In an optional embodiment provided in the present disclosure, the light-emitting element 40 includes a light-emitting substrate 44 and an electrode 45, the light-emitting substrate 44 is located between the electrode 45 and the first glue layer 20, and the surface of the light-emitting substrate 44 of at least part of the light-emitting element 40 facing the first glue layer 20 includes a patterned microstructure.
[0033] Optionally, the light-emitting element 40 also includes an N-type layer 411, a light-emitting layer 412 and a P-type layer 413 located between the light-emitting substrate 44 and the electrode 45, wherein the N-type layer 411 is used to provide electrons; the P-type layer 413 is used to provide holes; the light-emitting layer 412 is the core area for generating light, and emits light through the recombination of electrons and holes; when a forward voltage is applied to the N-type layer 411 and the P-type layer 413, electrons and holes are injected from the N-type layer 411 and the P-type layer 413 into the light-emitting layer 412 respectively, and the electrons and holes meet and recombine in the light-emitting layer 412, and energy is released during the recombination process, and the energy is expressed in the form of photons, thereby generating light; the light-emitting layer 412 is usually composed of structures such as quantum wells, and the energy band structure of the quantum wells can effectively limit the movement of electrons and holes, improve the recombination efficiency, and thereby enhance the light-emitting effect.
[0034] Specifically, in the conventional technology in this field, it is usually necessary to form a light-emitting element 40 on a substrate of a special material, for example, to form a light-emitting element by epitaxial growth on a sapphire substrate. The light-emitting element 40 includes a light-emitting substrate 44 and an N-type layer 411, a light-emitting layer 412, a P-type layer 413 and an electrode 45 grown on the light-emitting substrate 44. After the light-emitting element 40 is grown, it is peeled off from the sapphire substrate and transferred to the chip transfer area 30 on the micro-device substrate 100. At this time, the light-emitting substrate 44 in the light-emitting element 40 is located between the electrode 45 and the first glue layer 20 on the micro-device substrate 100. That is, when the light-emitting element 40 is transferred to the micro-device substrate 100, the electrode 45 in the light-emitting element 40 is located on the side of the first glue layer 20 away from the substrate 10, and the light-emitting element 40 is located on the side of the first glue layer 20 away from the substrate 10. The light-emitting substrate 44 in the element 40 is located on the side of the electrode 45 facing the first adhesive layer 20 and is bonded to the first adhesive layer 20. When there is a microstructure on the surface of the sapphire substrate, the light-emitting substrate 44 of the light-emitting element 40 grown on the sapphire substrate also has a corresponding patterned microstructure, so that at least part of the light-emitting substrate 44 of the light-emitting element 40 facing the first adhesive layer 20 includes a patterned microstructure; in this way, when at least part of the light-emitting substrate 44 of the light-emitting element 40 facing the first adhesive layer 20 includes a patterned microstructure, at least part of the contact area between the ex-situ light-emitting element 90 located in the micro-particle area 60 and the micro-particle 70 is smaller, so that the bonding force between the ex-situ light-emitting element 90 and the first adhesive layer 20 is smaller, which is convenient for removal in subsequent processes.
[0035] It should be noted that the "extra-situ light-emitting element 90" refers to a light-emitting element 40 transferred to the micro-device substrate 100, which is at least partially located outside the chip transfer area 30, corresponding to the light-emitting element with tilt offset or position change mentioned above, for example, the same ex-situ light-emitting element 90 is partially located in the chip transfer area 30 and partially located in the micro-particle area 60, or the same ex-situ light-emitting element 90 is entirely located in the micro-particle area 60.
[0036] Figure 5 This is a schematic diagram of the relationship between the diameter of the light-emitting substrate groove 46 of the light-emitting element of the embodiment of the present disclosure and the diameter of the micro-particles. Please refer to Figures 1 to 5 In an optional embodiment provided in the present disclosure, the patterned microstructure includes grooves 46 arranged in an array, and the minimum particle size D1 of the microparticles 70 is greater than the maximum diameter d of the grooves 46 in the patterned microstructure.
[0037] Specifically, the light-emitting element growth substrate in the prior art usually includes protrusions arranged in an array. When the light-emitting element 40 is epitaxially grown on the light-emitting element growth substrate, the light-emitting substrate 44 of the light-emitting element 40 peeled off from the light-emitting element growth substrate usually has grooves 46 arranged in an array corresponding to the protrusions. Therefore, the patterned microstructure in the light-emitting substrate 44 includes grooves 46 arranged in an array, and the maximum diameter of the grooves 46 is d; as mentioned above, the micro-particle area 60 includes at least two micro-particles 70 with different particle sizes, wherein the maximum diameter of the micro-particle 70 is D2, the minimum particle size of the micro-particle 70 is D1, and the relationship between the diameter of the micro-particle 70 and the maximum diameter of the groove 46 is: D2>D 1>d, that is to say, the maximum diameter d of the groove 46 in the patterned microstructure of the light-emitting substrate 44 is smaller than the minimum particle size D1 of the micro-particle 70. Thus, when the light-emitting element 40 is transferred to the micro-device substrate 100, the light-emitting substrate 44 of the transferred displaced ectopic light-emitting element 90 is at least partially in contact with the micro-particle 70 in the micro-particle region 60. The maximum diameter d of the groove 46 in the patterned microstructure of the light-emitting substrate 44 is smaller than the minimum particle size D1 of the micro-particle 70. This prevents the micro-particle 70 in the micro-particle region 60 from being stuck with the patterned microstructure light-emitting substrate 44 of the ectopic light-emitting element 90, thereby reducing the difficulty of removing the ectopic light-emitting element 90 in the subsequent process and improving the recycling rate of the micro-device substrate 100.
[0038] Please continue to refer to Figures 1 to 5 In an optional embodiment provided by the present disclosure, the surface of the micro-particles 70 is smooth and non-sticky.
[0039] Specifically, the micro-particles 70 can be made by a spray printing process, the surface of the micro-particles 70 is smooth and non-sticky, the surface of the micro-particles 70 that protrude from the first adhesive layer 20 is smooth and non-sticky, and the light-emitting substrate 44 of the ectopic light-emitting element 90 that is at least partially located in the micro-particle area 60 is in contact with the micro-particles 70 with a smooth and non-sticky surface, which can further reduce the bonding strength between the ectopic light-emitting element 90 and the micro-particle area 60, which is beneficial to the removal of the ectopic light-emitting element 90 in subsequent processes and improves the reuse rate of the micro-device substrate 100.
[0040] In an optional embodiment provided in the present disclosure, the microparticle 70 has an arc-shaped surface. Preferably, the microparticle 70 is a sphere. When the ectopic light-emitting element 90 is at least partially located in the microparticle area 60, the microparticle 70 with an arc-shaped surface can reduce the risk of the light-emitting element 40 being impacted and broken. In addition, the arc-shaped surface of the microparticle 70 can further reduce the contact area with the light-emitting element 40. In this way, the microparticle 70 with an arc-shaped surface can reduce the contact area with the light-emitting element 40 while reducing the probability of the light-emitting element 40 being impacted and broken.
[0041] Please continue to refer to Figures 1 to 5 In an optional embodiment provided in the present disclosure, along a direction perpendicular to the plane where the substrate 10 is located, the height of the micro-particles 70 protruding from the first adhesive layer 20 is less than or equal to 3 μm.
[0042] Specifically, along a direction parallel to the plane where the first adhesive layer 20 is located, the micro-particle area 60 is located between the plurality of chip transfer areas 30, the micro-particle area 60 includes at least two micro-particles 70 of different particle sizes, the micro-particles 70 are located on the side of the first adhesive layer 20 away from the substrate 10, and the micro-particles 70 are at least partially sunken into the first adhesive layer 20, that is, the micro-particles 70 at least partially protrude from the surface of the first adhesive layer 20, and along a direction perpendicular to the plane where the first adhesive layer 20 is located, the height of the micro-particles 70 protruding from the surface of the first adhesive layer 20 is greater than 0 and less than or equal to 3 μm, and optionally, the height of the micro-particles 70 protruding from the surface of the first adhesive layer 20 is less than or equal to 1.5 μm; optionally, the height of the micro-particles 70 protruding from the surface of the first adhesive layer 20 is less than or equal to 2 μm; optionally, the height of the micro-particles 70 protruding from the surface of the first adhesive layer 20 is less than or equal to 2.5 μm... and so on, This will not be elaborated one by one. It is only necessary to satisfy that the height of the micro-particles 70 protruding from the first glue layer 20 is less than or equal to 3 μm in the direction perpendicular to the plane where the first glue layer 20 is located. If the height of the micro-particles 70 protruding from the first glue layer 20 is greater than 3 μm, then in the direction perpendicular to the plane where the substrate 10 is located, the height difference between the light-emitting element 40 located in the chip transfer area 30 and the height of the micro-particles 70 in the micro-particle area 60 is small. When the micro-device substrate 100 is used as a transfer substrate, it is not conducive to the secondary transfer of the light-emitting element 40. In this way, when the height of the micro-particles 70 protruding from the first glue layer 20 is less than or equal to 3 μm, the micro-particles 70 protrude from the first glue layer 20, reducing the bonding between the ectopic light-emitting element 90 and the first glue layer 20. The height of the micro-particles 70 protruding from the first glue layer 20 is less than the height of the light-emitting element 40, which is conducive to the secondary transfer of the light-emitting element 40 and reduces the difficulty of transfer.
[0043] In an optional embodiment provided by the present disclosure, the micro-particles 70 include one or more of organic particles, inorganic particles, and metal particles.
[0044] Specifically, the microparticles 70 can be one or more of organic particles (polytetrafluoroethylene, etc.), inorganic particles (quartz particles, etc.) or metal particles (gold, nickel, etc.). For example, the microparticles 70 can be all organic particles, or all inorganic particles, or all metal particles; the microparticles 70 can also be partially organic particles and partially inorganic particles, or the microparticles 70 can also be partially organic particles and partially metal particles, or the microparticles 70 can also be partially inorganic particles and partially metal particles, or the microparticles 70 can also be partially organic particles, partially inorganic particles, and partially metal particles; in this way, the richness of the types of microparticles 70 can provide the possibility of a variety of combinations of microparticles 70, thereby improving the flexibility of material selection.
[0045] Figure 6 This is a schematic diagram of the relationship between the widths of the transfer precision zones corresponding to the different light-emitting elements described in the embodiment of the present disclosure. Please refer to Figures 1 to 6 In an optional embodiment provided in the present disclosure, the micro-device substrate 100, the chip transfer area 30 also includes a transfer precision area 50, the transfer precision area 50 is located between the light emitting element 40 and the micro-particle area 60, and the width of the transfer precision area 50 is less than or equal to 10μm.
[0046] Specifically, the micro-device substrate 100 includes a substrate 10 and a first adhesive layer 20 located on one side of the substrate 10. Along a direction parallel to the plane where the first adhesive layer 20 is located, the first adhesive layer 20 includes a plurality of chip transfer areas 30 and a micro-particle area 60 located between the plurality of chip transfer areas 30, wherein the chip transfer area 30 also includes a transfer accuracy area 50, and the transfer accuracy area 50 is used to control the transfer accuracy of the light-emitting element 40. Along a direction parallel to the plane where the first adhesive layer 20 is located, each transfer accuracy area 50 surrounds the light-emitting element 40 in the chip transfer area 30, and the transfer accuracy area 50 is located between the light-emitting element 40 and the micro-particle area 60. The width L of the transfer accuracy area 50 is greater than 0 and less than or equal to 10 μm. Optionally, the width L of the transfer accuracy area 50 is 1.5 μm, and optionally Optionally, the width L of the transfer precision zone 50 is 3 μm. Optionally, the width L of the transfer precision zone 50 is 5 μm... and so on. When the width L of the transfer precision zone 50 is equal to 0, there is no gap between the light emitting element 40 of the chip transfer zone 30 and the micro-particle zone 60. When the light emitting element 40 is transferred to the micro-device substrate 100, it is very easy to shift to the micro-particle zone 60, resulting in poor transfer. When the width L of the transfer precision zone 50 is greater than 10 μm, the width L of the transfer precision zone 50 is too large, which is not conducive to the position control of the light emitting element 40 and is prone to poor contact with the circuit substrate. In this way, by setting the transfer precision zone 50 in the chip transfer zone 30, a certain allowable offset space can be provided for the light emitting element 40, thereby improving the transfer accuracy of the light emitting element 40 and thereby improving the transfer yield.
[0047] It should be noted that the “width L of the transfer precision zone 50 ” referred to herein refers to the shortest distance from the light emitting element 40 to the adjacent micro-particle zone 60 in the same chip transfer zone 30 .
[0048] Please continue to refer to Figures 1 to 6 In an optional embodiment provided in the present disclosure, the light-emitting element 40 includes a red light-emitting element 41, a green light-emitting element 42 and a blue light-emitting element 43, wherein a width L1 of a transfer precision zone 50 corresponding to the red light-emitting element 41 is smaller than a width L2 of a transfer precision zone 50 corresponding to the green light-emitting element 42, or a width L1 of a transfer precision zone 50 corresponding to the red light-emitting element 41 is smaller than a width L3 of a transfer precision zone 50 corresponding to the blue light-emitting element 43.
[0049] Specifically, the light-emitting element 40 includes a red light-emitting element 41, a green light-emitting element 42 and a blue light-emitting element 43. Taking the micro-LED display panel as an example, in the existing display panel, due to the different light-emitting materials of micro-LED devices of different colors, the structure may also be different. Due to the influence of materials and structures, the electrical characteristics may also be different, that is, light-emitting elements 40 of different colors will have different luminous efficiencies. For example, the red light-emitting element 40 has a longer wavelength and lower energy of red light, and there is more energy loss in the energy conversion process. Therefore, the luminous efficiency and luminous life of the red light-emitting element 41 are lower than those of the green light-emitting element 42 and the blue light-emitting element 43. In a micro-device substrate 100 provided in the present disclosure, the width L1 of the transfer precision zone 50 corresponding to the red light-emitting element 41 is smaller than the width L2 of the transfer precision zone 50 corresponding to the green light-emitting element 42, and the width L1 of the transfer precision zone 50 corresponding to the red light-emitting element 41 is smaller than the transfer precision zone 50 corresponding to the blue light-emitting element 43. The width L3 of the transfer area 50 is as follows: for example, the width L1 of the transfer accuracy area 50 corresponding to the red light-emitting element 41 is 1.5 μm, the width L2 of the transfer accuracy area 50 corresponding to the green light-emitting element 42 is 3 μm, and the width L3 of the transfer accuracy area 50 corresponding to the blue light-emitting element 43 is 5 μm. Since the luminous efficiency and luminous life of the red light-emitting element 41 are relatively low, the narrowing of the transfer accuracy area 50 corresponding to the red light-emitting element 41 is beneficial to improving the transfer accuracy of the red light-emitting element 41, reducing the displacement offset of the red light-emitting element 41, facilitating the subsequent docking with other elements, and improving the process yield; in this way, by setting the width L1 of the transfer accuracy area 50 corresponding to the red light-emitting element 41 to be smaller than the width L2 of the transfer accuracy area 50 corresponding to the green light-emitting element 42, or smaller than the width L3 of the transfer accuracy area 50 corresponding to the blue light-emitting element 43, the offset displacement of the red light-emitting element 41 can be reduced, the transfer accuracy of the red light-emitting element 41 can be improved, and the influence of the excessive offset of the red light-emitting element 41 on its luminous efficiency and life can be reduced.
[0050] Figure 7 This is a schematic diagram of the difference in particle size of microparticles around different light-emitting elements in the embodiments of the present disclosure. Please refer to Figures 1 to 7 In an optional embodiment provided in the present disclosure, the maximum particle size of the micro-particles 70 around the chip transfer area 30 corresponding to the red light-emitting element 41 is H1, and the minimum particle size is H2;
[0051] The maximum particle size of the micro-particles 70 around the chip transfer area 30 corresponding to the green light emitting element 42 or the blue light emitting element 43 is h1, and the minimum particle size is h2;
[0052] Among them, the absolute value of the difference between H1 and H2 is greater than the absolute value of the difference between h1 and h2.
[0053] Specifically, the first adhesive layer 20 in the micro-device substrate 100 includes a plurality of chip transfer areas 30, and the micro-particle area 60 is located between the plurality of chip transfer areas 30. The micro-particle area 60 includes at least two micro-particles 70 of different particle sizes. Generally, due to different manufacturing processes, the light-emitting substrate 44 of the red light-emitting element 41 is a rough surface, which is different from the grooves 46 arranged in an array in the light-emitting substrate 44 of the blue light-emitting element 43 or the green light-emitting element 42. The micro-particles 70 around the chip transfer area 30 corresponding to the red light-emitting element 41 include at least two different particle sizes, wherein the maximum particle size is H1 and the minimum particle size is H2; the micro-particles 70 around the chip transfer area 30 corresponding to the green light-emitting element 42 or the blue light-emitting element 43 include at least two different particle sizes, wherein the maximum particle size is h1 and the minimum particle size is h2; the absolute value of the maximum difference in particle size of the micro-particles 70 around the red light-emitting element 41 is |H1-H2| , which is greater than the absolute value of the maximum difference in particle size of the micro-particles 70 around the green light-emitting element 42 or the blue light-emitting element 43 |h1-h2|, that is, the particle size difference of the micro-particles 70 around the red light-emitting element 41 is greater than the particle size difference of the micro-particles 70 around the blue light-emitting element 43 or the green light-emitting element 42, that is, the contact area between the light-emitting substrate 44 of the red light-emitting element 41 at least partially offset to the micro-particle area 60 and the micro-particles 70 is smaller. In this way, by setting the particle size difference of the micro-particles 70 around the red light-emitting element 41 to be greater than the particle size difference of the micro-particles 70 around the blue light-emitting element 43 or the green light-emitting element 42, the contact area between the light-emitting substrate 44 of the red light-emitting element 41 and the micro-particles 70 can be reduced, and the adhesion between the red light-emitting element 41 and the micro-particles 70 can be further reduced, which is beneficial to the subsequent removal of the offset red light-emitting element 41 and improves the utilization rate of the micro-device substrate 100.
[0054] Figure 8 This is a schematic diagram of a process of transferring a light-emitting element from a source substrate to a temporary substrate according to an embodiment of the present disclosure. Fig. 9This is a schematic diagram of a process of transferring a light-emitting element from a temporary substrate to a transient substrate according to an embodiment of the present disclosure. Fig.10 FIG. 1 is a schematic diagram of a process of transferring a light emitting element from a temporary substrate to an array substrate according to an embodiment of the present disclosure. Figures 1 to 10 In an optional embodiment provided in the present disclosure, the micro device substrate 100 includes a temporary substrate 81, a transient substrate 82, and an array substrate 80. The “included” here means that the micro device substrate 100 can be embodied as a temporary substrate 81, a transient substrate 82, or an array substrate 80.
[0055] Specifically, the micro-device substrate 100 includes a temporary substrate 81 for temporarily storing the light-emitting element 40. The temporary substrate 81 includes a base 811 and a glue layer 812 located on one side of the base 811. Along a direction parallel to the plane where the glue layer 812 is located, the glue layer 812 includes a plurality of chip transfer areas 30 and micro-particle areas 60, which are used for temporarily storing the light-emitting element 40 by picking up the light-emitting element 40.
[0056] The micro-device substrate 100 also includes a temporary substrate 82 during the mass transfer of the light-emitting element 40. During the mass transfer of the light-emitting element 40, the light-emitting element 40 is epitaxially grown on the source substrate 00. The light-emitting element 40 includes a light-emitting substrate 44 and an electrode 45. The temporary substrate 81 includes a base 811 and a glue layer 812 located on one side of the base 811. In a direction parallel to the plane where the glue layer 812 is located, the glue layer 812 includes a plurality of chip transfer areas 30 and micro-particle areas 60. The temporary substrate 81 is aligned with the source substrate 00, and the light-emitting element 40 on the source substrate 00 is transferred to the chip transfer area 30 of the temporary substrate 81 through a stripping process. At this time, the electrode 45 of the light-emitting element 40 45 is located between the glue layer 812 and the light-emitting substrate 44; the temporary substrate 82 includes a substrate 822 and a glue layer 821 located on one side of the substrate 822. Along the direction parallel to the plane where the first glue layer 20 is located, the glue layer 821 includes a plurality of chip transfer areas 30 and micro-particle areas 60. The temporary substrate 82 is aligned with the temporary substrate 81, and the light-emitting element 40 on the temporary substrate 81 is transferred to the chip transfer area 30 of the temporary substrate 82. At this time, the light-emitting substrate 44 of the light-emitting element 40 is located between the glue layer 821 and the electrode 45; the array substrate 80 is aligned with the temporary substrate 82, and the light-emitting element 40 located in the chip transfer area 30 of the temporary substrate 82 can be transferred to the array substrate 80.
[0057] It should be noted that when the micro-device substrate 100 is used as the array substrate 80 , the array substrate 80 also includes a glue layer and micro-particles, which will not be described in detail.
[0058] It can be understood that the array substrate 80 is the final target substrate of the mass transfer process of the light-emitting elements 40. As mentioned above, the array substrate 80 is aligned with the temporary substrate 82, and the light-emitting elements 40 on the temporary substrate 82 can be transferred to the final array substrate 80 to achieve electrical connection between the light-emitting elements 40 and the driving devices.
[0059] It can be understood that after the micro-device substrate 100 completes a transfer of the light-emitting element as a temporary substrate 81 or a transient substrate 82, it can be determined whether there are residual ex-situ light-emitting elements 90 on the micro-device substrate 100. If so, the ex-situ light-emitting elements 90 on the micro-device substrate 100 can be removed through the water washing process in the degumming process without the need for a new process, which is conducive to the recycling of the micro-device substrate 100.
[0060] In summary, the present disclosure provides a micro-device substrate, including a substrate and a first adhesive layer located on one side of the substrate. Along a direction parallel to the plane where the substrate is located, the first adhesive layer includes a plurality of chip transfer areas and a micro-particle area located between the plurality of chip transfer areas. The micro-particle area includes at least two micro-particles with different particle sizes, which can reduce the contact area between the ex-situ light-emitting element and the first adhesive layer, thereby reducing the adhesion force and facilitating the removal of the ex-situ light-emitting element in the later process; when the light-emitting substrate of at least part of the light-emitting element includes a patterned microstructure, the contact area between the ex-situ light-emitting element and the micro-particles is smaller, further reducing the adhesion force; the maximum diameter of the groove in the patterned microstructure is smaller than the minimum particle size of the micro-particles, so that the micro-particles will not be stuck with the light-emitting substrate of the ex-situ light-emitting element, reducing the difficulty of removing the ex-situ light-emitting element and improving the recycling rate of the micro-device substrate; The micro-particles on the curved surface can reduce the probability of colliding with the light-emitting element and breaking; when the height of the micro-particles protruding from the first adhesive layer is less than or equal to 3μm, it is conducive to the secondary transfer of the light-emitting element and reduces the difficulty of transfer; setting a transfer accuracy zone in the chip transfer area can provide a certain allowable offset space and improve the transfer yield; setting the width of the transfer accuracy zone corresponding to the red light-emitting element to be smaller than the width of the transfer accuracy zone corresponding to the green light-emitting element or the blue light-emitting element can reduce the offset displacement of the red light-emitting element and reduce the impact of the excessive offset of the red light-emitting element on its luminous efficiency and life; setting the particle size difference of the micro-particles around the red light-emitting element to be larger than the particle size difference of the micro-particles around the blue light-emitting element or the green light-emitting element can reduce the contact area between the red light-emitting element and the micro-particles, and further reduce the adhesion between the red light-emitting element and the micro-particles.
[0061] It should be noted that, in this article, relational terms such as "first" and "second" are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, the elements defined by the sentence "comprise a ..." do not exclude the existence of other identical elements in the process, method, article or device including the elements.
[0062] The above description is only a specific embodiment of the present disclosure, so that those skilled in the art can understand or implement the present disclosure. Various modifications to these embodiments will be apparent to those skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present disclosure. Therefore, the present disclosure will not be limited to the embodiments described herein, but will conform to the widest scope consistent with the principles and novel features disclosed herein.
Claims
1. A micro-device substrate, characterized in that: It includes a substrate and a first adhesive layer arranged on one side of the substrate; Along a direction parallel to the plane where the substrate is located, the first adhesive layer includes a plurality of chip transfer areas and micro-particle areas located between the chip transfer areas, the light-emitting element is located in the chip transfer area, and the light-emitting element is bonded to the first adhesive layer; The micro-particle region includes micro-particles, and the micro-particles are located on a side of the first glue layer facing away from the substrate.
2. The micro-device substrate according to claim 1, characterized in that: The micro-particle zone includes at least two micro-particles of different particle sizes.
3. The micro-device substrate according to claim 1, characterized in that: The light-emitting element comprises a light-emitting substrate and an electrode, wherein the light-emitting substrate is located between the electrode and the first adhesive layer, and a surface of the light-emitting substrate of at least part of the light-emitting element facing the first adhesive layer comprises a patterned microstructure.
4. The micro-device substrate according to claim 3, characterized in that: The patterned microstructure includes grooves arranged in an array, and the minimum particle size of the microparticles is greater than the maximum diameter of the grooves in the patterned microstructure.
5. The micro-device substrate according to claim 1, characterized in that: The surface of the microparticles is smooth and non-sticky.
6. The micro-device substrate according to claim 1, characterized in that: In a direction perpendicular to the plane where the substrate is located, the height of the micro-particles protruding from the first adhesive layer is less than or equal to 3 μm.
7. The micro-device substrate according to claim 1, characterized in that: The microparticles include one or more of organic particles, inorganic particles, and metal particles.
8. The micro-device substrate according to claim 1, characterized in that: The chip transfer area further includes a transfer precision area, the transfer precision area is located between the light emitting element and the micro-particle area, and the width of the transfer precision area is less than or equal to 10 μm.
9. The micro-device substrate according to claim 8, characterized in that: The light-emitting elements include a red light-emitting element, a green light-emitting element and a blue light-emitting element, wherein a width of a transfer accuracy zone corresponding to the red light-emitting element is smaller than a width of a transfer accuracy zone corresponding to the green light-emitting element or the blue light-emitting element.
10. The micro-device substrate according to claim 1, characterized in that: The maximum particle size of the microparticles around the chip transfer area corresponding to the red light-emitting element is H1, and the minimum particle size is H2; The maximum particle size of the microparticles around the chip transfer area corresponding to the green light emitting element or the blue light emitting element is h1, and the minimum particle size is h2; Among them, the absolute value of the difference between H1 and H2 is greater than the absolute value of the difference between h1 and h2.
11. The micro-device substrate according to claim 1, characterized in that: The micro-device substrate includes a temporary substrate, a transient substrate, and an array substrate.
Citation Information
Patent Citations
Ic having wafer paste sheet adhesive tape and encapsulation method tehreof
CN101980361A
Production method for semiconductor device
CN111295738A
Chip transfer assembly, manufacturing method thereof and chip transfer method
CN112967980A
Micro LED chip transfer method and display backboard
CN114078994A
Chip transfer assembly and manufacturing method therefor, chip transfer method, and display backplane