Method for welding ceramic material by using laser reaction

Through laser reaction welding technology, high-energy-density laser beams are used for precise welding of ceramic materials, which solves the problems of high melting point and brittleness of ceramic materials in traditional welding methods, achieves efficient and low-cost ceramic welding, and improves welding quality and production. efficiency.

CN118763232APending Publication Date: 2024-10-11SHENYANG INSTITUTE OF CHEMICAL TECHNOLOGY
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410734266.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-07
Publication Date
2024-10-11

AI Technical Summary

Technical Problem

Traditional welding methods are difficult to cope with the high melting point and brittleness of ceramic materials, resulting in a decrease in the strength and quality of welded joints. The differences in chemical properties and thermal expansion coefficients between ceramics and metals make it difficult to effectively combine welding materials, increasing costs and complexity.

Method used

The laser reaction welding method is used, using high-energy-density laser beams for local heating. The RLRS method and CO2 laser are used to achieve precise welding of ceramic materials, reducing costs and improving the fine controllability of the weld.

Benefits of technology

It achieves efficient welding of ceramic materials, reduces welding costs, improves welding quality and production efficiency, solves the problems of high melting point and brittleness of ceramic materials, and improves the stability of the combination of ceramics and metals.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure FT_1
    Figure FT_1
  • Figure FT_2
    Figure FT_2
  • Figure FT_3
    Figure FT_3
Patent Text Reader

Abstract

The invention relates to a method for welding ceramic materials, in particular to a method for welding ceramic materials by using laser reaction, which comprises the following steps: heating the surface of a welding joint to high temperature, and carrying out chemical reaction on the two materials to form the welding joint at specific temperature and under specific conditions, so that reliable connection between ceramic and other materials is realized. The laser reaction ceramic welding technology solves the problem that ceramic materials are difficult to treat through a traditional welding method. The traditional method is limited by high hardness, brittleness and low thermal conductivity when being used for treating ceramic, so that effective welding cannot be realized. The laser reaction welding utilizes the high energy density and locality of laser to quickly and accurately heat the ceramic to the welding temperature so as to promote the ceramic to form reliable connection with other materials. The application range of the ceramic material is expanded, the efficiency and quality in the engineering and manufacturing fields are improved, and the method is suitable for the fields of ceramic fuel cell manufacturing, microelectronic manufacturing, medical instrument manufacturing and the like.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a method for welding ceramic materials, in particular to a method for welding ceramic materials using laser reaction. Background Art

[0002] Welding ceramic materials is a challenging technology due to their high hardness, brittleness and chemical stability. The demand for welding ceramics comes from industries such as electronics, aerospace and chemicals, where ceramics need to be repaired, assembled or manufactured.

[0003] Therefore, welding ceramic materials is particularly important for us. However, welding ceramics in traditional methods faces multiple barriers: First, the high melting point of ceramic materials is one of the challenges of traditional welding methods. Ceramics usually have a high melting point, which is much higher than the temperature range of conventional metal welding. Traditional welding equipment and technology are difficult to provide a high enough temperature to melt ceramics, so welding cannot be achieved effectively. Secondly, the brittleness and fragility of ceramic materials make them prone to cracks and fractures during welding. Traditional welding methods usually apply large thermal and mechanical stresses, which can cause breakage and damage to ceramic materials and reduce the strength and quality of welded joints. In addition, the chemical properties and thermal expansion coefficients between ceramics and metals are very different, which makes it difficult for traditional welding materials to effectively combine with ceramic materials. The stability and durability of the welded joint will be affected, and problems such as loose welds and cracking may occur. In addition, traditional welding methods often require the use of special welding materials or brazing materials in ceramic welding. The selection and processing of these materials require higher technical requirements, which increases the cost and complexity of welding. Overall, traditional welding methods have technical limitations and challenges for welding ceramic materials.

[0004] Laser reaction welding technology achieves precise heating and connection of ceramics through high energy density laser beams, solving the limitations of traditional methods. It is urgent to promote the advancement of material science and technology and meet the needs of material performance in different fields. Laser ceramic welding is widely used in fuel cell manufacturing, electronics, aerospace and medical devices. This technology achieves precise connection of ceramic materials, improves production efficiency, reduces costs, and promotes technological innovation. Summary of the invention

[0005] The purpose of the present invention is to provide a method for laser reaction welding of ceramic materials. The method uses laser as a heat source to complete the welding process in a very short time, thereby achieving precise welding of ceramic materials, reducing costs, and having fine welds and strong controllability. The method is suitable for the welding and manufacturing of ceramic parts with high requirements on welding quality.

[0006] The objective of the present invention is achieved through the following technical solutions: A method for laser reaction welding of ceramic materials, the method comprising the following steps: (1) Preparation of anode substrate.

[0007] (2) Coating of electrolyte precursor film.

[0008] (3) The dense electrolyte is welded to the anode substrate using the RLRS method.

[0009] (4) Characterization of samples.

[0010] Preferably, step (1) uses a solid state reaction sintering (SSRS) method to prepare NiO+BCZYYb (NiO+BaCe 0.7 Zr 0.1 Y 0.1 Yb 0.1 O 3-δ ) is used as the anode particle substrate. The slurry in step (1) is milled for 48 hours using isopropanol as the grinding solvent, 30wt% starch as the pore-forming agent, and 3 mm YSZ (yttrium-doped zirconium oxide) as the grinding medium. The ball-milled powder is granulated into an embryo with a diameter of 1 inch and a thickness of 5 mm. The green embryo is then fired in a furnace and finally reduced at 650°C for 20 hours in 5% H2+95% Ar. The anode substrate is successfully prepared.

[0011] Preferably, the BCZYYb slurry in step (2) is prepared according to the following method. The method is as follows: a BCZYYb+1wt%NiO precursor composed of BaCO3, CeO2, ZrO2, Y2O3, Yb2O3 and NiO is mixed by ball milling in stoichiometric amounts. The ball-milled BCZYYb+1wt%NiO electrolyte precursor powder is mixed with deionized water, a dispersant (DARVAN) and a binder (HPMC) to form a printable slurry. A thin layer of BCZYYb is cast on a reduced porous NiO+BCZYY anode substrate with a scraper. Scraper casting is performed at a gap of 200 μm between the frame and the blade, and a material of about 150 μm thickness is obtained after drying in the open air at room temperature for 24 hours. The pre-fired anode substrate is reduced before laser treatment.

[0012] Preferably, a CO2 laser is used in step (3) for laser reaction welding of ceramics. The sample is preheated to 500°C on a hot plate at 500°C to reduce thermal shock. The laser beam is focused not through a general spherical lens but through a cylindrical lens (focal length 1 inch, diameter 19.05 mm, Laser Mechanisms, Inc.) to increase the sintering area. The operating parameters of the CO2 laser are defocus: 20 mm; power: 90 W; speed: 0.1 mm / s; hot plate: 500°C; spot size: 15 mm; ED: 60J / mm 2 .

[0013] Preferably, in step (4), the sample is subjected to X-ray diffraction (XRD), and its diffraction pattern is analyzed to obtain information such as the composition of the material, the structure or morphology of atoms or molecules inside the material, etc. The sample is also subjected to scanning electron microscopy (SEM) analysis to characterize the microscopic morphology of the sample.

[0014] The advantages and effects of the present invention are: 1. The laser reaction welding of the present invention utilizes the laser beam to locally heat the welding area, achieving non-contact heating 2. The laser beam of the present invention has high energy density and can quickly raise the temperature in the welding area to a sufficiently high level to achieve local melting. This enables laser reaction welding to cope with the high melting point characteristics of ceramic materials and achieve effective welding. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] Figure 1 This is the principle diagram of the CO2 laser welding system of the present invention; Figure 2 XRD patterns of the RLRS-derived BCZYYb+1wt%NiO electrolyte and Ni(O)+BCZYYb anode substrate of the present invention before and after (furnace sintering); Figure 3 A photograph of the RLRS-derived BCZYYb electrolyte on the Ni(O)-BCZYYb substrate of the present invention; Figure 4 is a low magnification surface SEM micrograph of the RLRS-derived BCZYYb electrolyte of the present invention; Figure 5 A high magnification surface SEM micrograph of the RLRS-derived BCZYYb electrolyte of the present invention; Figure 6 This is a cross-sectional SEM micrograph of the RLRS-derived BCZYYb electrolyte on the Ni(O)-BCZYYb substrate of the present invention. DETAILED DESCRIPTION

[0016] The present invention will be described in detail below with reference to the embodiments shown in the accompanying drawings. Example

[0017] (1) An anode particle substrate composed of Ni(O)+BCZYYb was prepared using the SSRS method. Stoichiometric BaCO3, CeO2, ZrO2, Y2O3, Yb2O3, NiO and 30wt% starch (pore former) were ball-milled in isopropanol using 3 mm YSZ grinding media for 48 hours. The ball-milled powder was granulated into a 1-inch diameter and 5-mm thick embryo. The green embryo was then fired in a furnace at 1450°C for 18 hours and then reduced at 650°C in 5%H2+95%Ar for 20 hours. The anode substrate was successfully prepared.

[0018] (2) The electrolyte precursor BCZYYb+1wt%NiO was ball-milled by mixing BaCO3, CeO2, ZrO2, Y2O3, and Yb2O3 in stoichiometric amounts. The ball-milled BCZYYb+1wt%NiO electrolyte precursor powder was mixed with deionized water, a dispersant (DARVAN), and a binder (HPMC) to form a printable slurry. A thin layer of green BCZYYb was then cast on a reduced porous Ni(O)+BCZYY anode substrate using a doctor blade. Doctor blade casting was performed at a 200 μm gap between the frame and the blade, and a material of approximately 150 μm thickness was obtained after drying in the open air at room temperature for 24 h. The pre-fired anode substrate was reduced before laser treatment.

[0019] (3) The sample was preheated to 500°C on a hot plate heated to 500°C to reduce thermal shock. The laser beam was focused by a cylindrical lens instead of a general spherical lens to increase the sintering area. The operating parameters of the CO2 laser were defocus: 20 mm; power: 90 W; speed: 0.1 mm / s; hot plate: 500°C; spot size: 15 mm; ED: 60 J / mm 2 . Figure 1 Laser sintering working state diagram (4) X-ray diffraction (XRD) shows that the XRD of RLRS-derived BCZYYb+1wt%NiO electrolyte ( Figure 1 ) indicates that a pure perovskite crystal structure has been formed, which is the same as the crystal structure obtained by the SSRS method. By comparing the XRD patterns of the Ni(O)-BCZYYb anode substrate before and after RLRS operation ( Figure 1), it can be found that RLRS did not cause significant phase composition changes in the anode composite, and the anode composite still contained BCZYYb, NiO, and Ni phases. However, a deeper observation showed that the amount of NiO in the anode composite increased after RLRS operation, but this did not affect the final performance of the PCFC single cell because NiO was in situ reduced during fuel cell operation. The formation of NiO in the anode composite can explain the good bonding between the electrolyte and the anode layer (such as Figure 2 Therefore, we can conclude that the desired crystal structures of the electrolyte and anode are either obtained or successfully maintained after RLRS deposition of BCZYYb + 1wt%NiO electrolyte on reduced Ni(O) + BCZYYb anode substrate.

[0020] SEM images of RLRS-derived BCZYYb+1wt%NiO electrolyte on Ni(O)-BCZYYb substrate Figure 3 It shows that no visible macro cracks are observed on the surface of the electrolyte layer supported on the Ni(O)-BCZYYb anode substrate. Low-magnification SEM micrograph of the electrolyte Figure 4 It further shows that no microcracks are observed. High-magnification SEM micrograph of the electrolyte surface Figure 5 The electrolyte membrane is completely defect-free and fully densified. The grain size (2–5 μm) is comparable to that produced by furnace SSRS operations. SEM micrograph of a cross section of a half-cell with electrolyte loaded on an anode substrate Figure 6 It is shown that the anode is still porous after RLRS operation, which can ensure sufficient porosity after further in situ reduction during fuel cell operation. It can also be clearly seen that the bonding between the electrolyte and the anode layer is good. No discontinuity is found at the interface between the anode and the electrolyte. We can conclude that after RLRS deposition of BCZYYb+1wt%NiO electrolyte on Ni(O)-BCZYYb anode substrate, the desired dense microstructure electrolyte is obtained and the desired porous anode microstructure is maintained.

Claims

1. A method for laser reaction welding of ceramic materials, characterized in that: The method comprises the following steps: (1) Preparation of anode substrate; (2) coating of electrolyte precursor film; (3) Using rapid laser reactive sintering (RLRS) technology to weld the dense electrolyte onto the anode substrate; (4) Characterization of samples.

2. A method for laser reaction welding of ceramic materials according to claim 1, characterized in that: The step (1) uses a solid state reaction sintering (SSRS) method to prepare NiO+BCZYYb (NiO+BaCe 0.7 Zr 0.1 Y 0.1 Yb 0.1 O 3-δ ) composed of anode particle substrate; the slurry in step (1) is milled for 48 hours with isopropanol as grinding solvent, 30wt% starch as pore former, 3 mm YSZ (yttrium-doped zirconium oxide) as grinding medium. The ball-milled powder is granulated into a 1-inch diameter and 5-mm thick embryo; the green embryo is then fired in a furnace and finally reduced at 650°C in 5% H2+95% Ar for 20 hours. The anode substrate is successfully prepared.

3. The method of laser reaction welding of ceramic materials according to claim 1, characterized in that: The preparation method of the BCZYYb slurry in the step (2) is as follows: a BCZYYb+1wt%NiO precursor composed of BaCO3, CeO2, ZrO2, Y2O3, Yb2O3 and NiO is mixed by ball milling according to stoichiometric ratio; the ball-milled BCZYYb+1wt%NiO electrolyte precursor powder is mixed with deionized water, a dispersant (DARVAN) and a binder (HPMC) to form a printable slurry; a thin layer of BCZYYb is cast on a reduced porous NiO+BCZYY anode substrate using a scraper; scraper casting is performed at a gap of 200 μm between the frame and the blade, and a material of about 150 μm thickness is obtained after drying in the open air at room temperature for 24 hours; and the pre-fired anode substrate is reduced before laser treatment.

4. The method of laser reaction welding of ceramic materials according to claim 1, characterized in that: In the step (3), a CO2 laser is used to perform laser reaction welding of ceramics. The sample is preheated to 500°C on a 500°C hot plate to reduce thermal shock. The laser beam is focused by a cylindrical lens (focal length 1 inch, diameter 19.05 mm, Laser Mechanisms, Inc.) to increase the sintering area. The operating parameters of the CO2 laser are: defocus: 20 mm; power: 90 W; speed: 0.1 mm / s; hot plate: 500°C; spot size: 15 mm; ED: 60 J / mm 2 .

5. The method for welding ceramic materials using rapid laser reaction according to claim 1, characterized in that: In the step (4), the sample is subjected to X-ray diffraction (XRD) to analyze its diffraction pattern to obtain information such as the composition of the material, the structure or morphology of atoms or molecules inside the material, and the sample is subjected to scanning electron microscopy (SEM) analysis to characterize the microscopic morphology of the sample.