Composite coating liquid as well as preparation method and application thereof in preservation of walnut kernels

By using a composite coating liquid prepared with ingredients such as chitosan, soybean protein peptide and sesamol, the problem of oxidative rancidity of walnut kernels is solved, its preservation effect and mechanical properties are improved, the storage period is extended and the quality is improved.

CN118765975APending Publication Date: 2024-10-15SOUTHWEST FORESTRY UNIVERSITY
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410919484.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-10
Publication Date
2024-10-15

AI Technical Summary

Technical Problem

Walnut kernels are prone to oxidative rancidity during storage, resulting in reduced economic and nutritional value. The existing natural polymer cling film has insufficient preservation effects and mechanical properties.

Method used

A composite coating liquid, including chitosan, soy protein peptide, sesamol and citric acid solution, is used to prepare a coating liquid with improved mechanical properties and antioxidant properties through a specific mass ratio and preparation method, and is applied to Walnut kernels are being preserved.

Benefits of technology

It delays the oxidation rate of walnut kernels, reduces the rate of oxidative rancidity and browning degree, improves its storage quality, enhances the antibacterial performance and fluidity of the coating liquid, and maintains the appearance quality and nutritional value of walnut kernels.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention provides a composite coating liquid, a preparation method thereof and application of the composite coating liquid in preservation of walnut kernels. The composite coating liquid comprises the following raw materials: chitosan, soybean protein peptide, sesamol, glycerol and a citric acid solution. According to the composite film coating liquid provided by the invention, the soybean protein peptide and the chitosan are adopted to prepare the composite film coating liquid, so that the mechanical property of the composite film coating liquid can be improved, mechanical damage to the surfaces of the walnut kernels can be avoided, and the appearance quality of the walnut kernels can be kept. The composite coating liquid is prepared by dissolving chitosan in citric acid, so that on one hand, the storage quality is improved; on the other hand, the sensory quality of the walnut kernels in the storage and fresh-keeping process can be maintained, and strong sour taste caused by dissolving chitosan with acetic acid is avoided. The composite coating liquid is prepared from sesamol, soybean protein peptide and chitosan, so that the composite coating liquid has excellent antioxidant and antibacterial activity, the oxidative rancidity rate and browning degree of the walnut kernels are delayed, and the storage quality of the walnut kernels is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of nut preservation, in particular to a composite coating liquid and a preparation method thereof and application thereof in walnut kernel preservation. Background Art

[0002] Walnuts are also known as Qiang peaches and walnuts. Walnut production is widely distributed around the world. Chinese walnuts are mainly grown in Yunnan, Xinjiang, Shaanxi, Sichuan and other provinces, among which the output and planting area of ​​Yunnan walnuts rank first in my country. Walnuts are rich in protein and fat, as well as trace amounts of nutrients such as vitamin E, minerals and polyphenols. Among them, unsaturated fatty acids are as high as more than 90%, especially linoleic acid content (49.3-62.3g / 100g). Studies have reported that the intake of polyunsaturated fatty acids helps to reduce atherosclerosis and prevent other cardiovascular diseases. Therefore, walnuts are popular for their unique sensory properties, rich essential fatty acid content and bioactive ingredients (such as antioxidants). Since children and the elderly cannot easily open hard-shelled nuts such as walnuts, as well as various dairy products, walnut oils, nut snacks, etc. prepared with walnut kernels as raw materials, shelled walnuts have gradually become a popular product. However, a large amount of unsaturated fatty acids in walnut kernels are sensitive to oxygen and are prone to oxidative rancidity during storage, thereby reducing economic value and nutritional value. Therefore, it is a key issue to find a method to effectively delay the oxidative rancidity of walnut kernels and improve their shelf life.

[0003] Film coating refers to a method of spraying or applying a coating liquid to form an elastic film on the surface of food to prevent food from spoiling. It has the advantages of convenient use, easy access to raw materials, and low price. In recent years, natural polymer chitosan is a renewable resource with biocompatibility, degradability and antibacterial properties, and has been increasingly used in the application of food cling film. However, a single natural material has bottlenecks in food preservation, such as poor preservation effect and poor mechanical properties. Summary of the invention

[0004] The purpose of the present invention is to solve the defects of the above-mentioned prior art and provide a composite coating liquid with improved preservation effect and mechanical properties, a preparation method thereof and an application thereof in walnut kernel preservation.

[0005] A composite coating liquid, the raw materials of which include:

[0006] Chitosan, soybean protein peptide, sesamol, glycerol and citric acid solution.

[0007] Furthermore, in the composite coating liquid as described above, the concentration of the citric acid solution is 4%.

[0008] Furthermore, in the composite coating liquid as described above, the mass ratio of citric acid to glycerol and sesamol in the citric acid solution is: 4-20:1-5:0.3-1.5.

[0009] Furthermore, in the composite coating liquid as described above, the mass ratio of citric acid to glycerol and sesamol in the citric acid solution is 10:2.5:0.75.

[0010] Furthermore, in the composite coating liquid as described above, the mass ratio of citric acid to chitosan and soybean protein peptide in the citric acid solution is 4-20:1.6-8:0.4-2.

[0011] Furthermore, in the composite coating liquid as described above, the mass ratio of citric acid to chitosan and soybean protein peptide in the citric acid solution is 10:4:1.

[0012] A method for preparing the composite coating liquid as described above comprises the following steps:

[0013] (1): Prepare citric acid solution;

[0014] (2): 1.6 g of chitosan was added to the citric acid solution in sequence and stirred to dissolve, and then 0.4 g of soybean protein peptide was added to obtain a base coating solution after the solution was completely dissolved;

[0015] (3) Add 1 g of glycerol and 0.3 g of sesamol to the base coating liquid, stir magnetically for 3 h, and stir evenly to obtain the composite coating liquid.

[0016] Furthermore, in the method as described above, step (2) comprises: adding chitosan and soybean protein peptide to the citric acid solution in sequence under magnetic stirring at 50° C. to prepare the base coating solution; before step (3), it also comprises: first cooling the base coating solution to room temperature, and then adding glycerol and sesamol under magnetic stirring at room temperature.

[0017] An application of the composite coating liquid as described above in preserving walnut kernels.

[0018] The application as described above comprises: putting walnut kernels into the composite coating liquid, stirring for 1 minute, taking them out, and drying them at room temperature to obtain walnut kernels covered with the coating.

[0019] Beneficial effects:

[0020] 1. The method provided by the present invention, since direct dissolution of chitosan and soybean protein peptide will result in the precipitation of tiny particles and the dissolution effect at room temperature is not good, the chitosan is first completely dissolved at 50°C and then the soybean protein peptide is added to dissolve it, thereby obtaining a base coating liquid; then, in order to avoid the influence of temperature on the antioxidant sesamol, the base coating liquid is cooled to room temperature and then sesamol is added, thereby effectively improving the antibacterial property of the composite coating liquid; finally, glycerol is added to make the composite coating liquid finally prepared have more elasticity and fluidity mechanical properties.

[0021] 2. The composite coating liquid provided by the present invention, on the one hand, can enhance the mechanical properties of the composite coating liquid by attaching soybean protein peptides to chitosan, which is beneficial to avoid mechanical damage to the surface of walnut kernels and maintain their appearance quality, because the soybean protein peptides can be inserted into the polymer chain of chitosan, thereby increasing the free volume and molecular fluidity of the film-forming matrix molecules; on the other hand, by selecting soybean protein peptides to add to chitosan, the nutritional value of the composite coating liquid can be improved; on the other hand, by selecting soybean protein peptides to add to chitosan, the solubility, emulsification ability and antioxidant ability of the composite coating liquid can be improved; on the other hand, because more than 70% of the soybean protein peptides are small molecule peptides composed of 2-3 amino acids, they are easily absorbed by the human body. Therefore, the composite coating liquid provided by the present invention also has the effects of improving the body's immunity, lowering blood lipids and inhibiting cholesterol.

[0022] 3. The present invention adopts citric acid to dissolve chitosan to prepare the composite coating liquid. On the one hand, using chitosan as the base membrane of the preservative film liquid is beneficial to fully wrap the surface of walnut kernels, thereby avoiding microbial contamination and insect pests on the surface of walnut kernels, and also helps to regulate the permeability of oxygen and carbon dioxide and improve storage quality. On the other hand, the present invention uses citric acid to dissolve chitosan, which can avoid the strong sour taste brought by acetic acid dissolving chitosan, which is beneficial to maintain the sensory quality of walnut kernels during storage and preservation.

[0023] 4. The present invention uses sesamol, soybean protein peptide and chitosan to prepare a composite coating liquid, so that the composite coating liquid finally prepared has excellent antibacterial and antioxidant properties, thereby delaying the oxidative rancidity rate and browning degree of walnut kernels, and ultimately improving their storage quality. DETAILED DESCRIPTION

[0024] In order to make the purpose, technical solution and advantages of the present invention clearer, the technical solution of the present invention is described clearly and completely below. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0025] Chitosan is a polycationic polysaccharide composed of β-(1-4)-linked D-glucosamine and N-acetyl-D-glucosamine units, which is prepared by alkaline deacetylation of chitin at high temperature. Chitosan is widely used in the production of edible films due to its biodegradability, biocompatibility, film-forming properties and antimicrobial properties. However, the hydrophilicity leads to low water resistance and poor mechanical properties of chitosan films, which limits its application in functional films. Soy protein peptides are pure natural nutrients extracted from soybeans, with high nutritional value and important functional properties such as good solubility, emulsification ability and antioxidant ability. Therefore, the present invention prepares a composite coating liquid by dissolving soybean protein peptides and chitosan at 50°C, which can improve the mechanical properties of the composite coating liquid, help avoid mechanical damage to the surface of walnut kernels, and maintain its appearance quality. Moreover, more than 70% of the soybean protein peptides are small molecule peptides composed of 2-3 amino acids, which are easily absorbed by the human body and have the effects of improving the body's immunity, lowering blood lipids and inhibiting cholesterol. The addition of small molecule peptides can enhance the tensile strength and elongation at break of the film-forming matrix molecules. Therefore, the composite coating liquid prepared with chitosan and soybean protein peptide can form an elastic film with good mechanical properties on the surface of the walnut kernel, avoiding mechanical damage to the surface of the walnut kernel and improving its appearance quality.

[0026] In addition, the present invention can prepare a functional composite film by adding sesamol to chitosan and soybean protein peptide, and further improves the antibacterial and antioxidant properties of the composite coating liquid on the basis of improving the mechanical properties of the chitosan film. Specifically, sesamol, also known as 3,4-methylenedioxyphenol, is an important sesame lignan, with an off-white to light gray powder crystalline powder, has strong antioxidant activity, and plays an important role in preventing other fat-soluble compounds such as oils, fat-soluble vitamins and cholesterol from being oxidized and decomposed by light and rancid. Sesamol can also inhibit the growth and reproduction of food-borne pathogenic microorganisms by making cells stay in the DNA replication preparation stage, increasing membrane permeability to destroy the microbial cell structure so that its contents flow out, and increasing the active oxygen in the bacteria to accelerate the oxidation and aging of the cells. Therefore, the present invention can further improve the antibacterial and antioxidant properties of the chitosan film on the basis of improving its mechanical properties by adding sesamol to the base coating liquid. Moreover, sesamol can be slowly released to the surface of the walnut kernel in the composite film to capture active lipid free radicals, thereby preventing the oxidation chain reaction, and can also further inhibit the growth and reproduction of microorganisms and improve the storage quality of the walnut kernel.

[0027] Embodiment 1:

[0028] This embodiment provides a composite coating liquid and a preparation method thereof, and the raw materials used are as follows:

[0029] Reagents: Chitosan (analytical grade, deacetylation degree ≥ 95%, viscosity 100-200 Pa·s), soybean protein peptide (analytical grade), sesamol (analytical grade, purity 99.9%), glycerol and citric acid (analytical grade).

[0030] Preparation method (taking the preparation of 100mL as an example):

[0031] (1): Add 4 g of citric acid to 100 mL of deionized water to prepare a 4% citric acid solution;

[0032] (2): 1.6 g of chitosan was added to the above citric acid solution and stirred to dissolve, and then 0.4 g of soybean protein peptide was added to obtain a base coating solution after the solution was completely dissolved;

[0033] (3): cooling the base coating liquid to room temperature;

[0034] (4): Under magnetic stirring conditions at room temperature, 1 g of glycerol and 0.3 g of sesamol were added to the base coating liquid, and magnetic stirring was performed for 3 hours to obtain the composite coating liquid.

[0035] Embodiment 2:

[0036] In this embodiment, the composite coating liquid prepared in Example 1 is used to preserve walnut kernels, and the specific preservation steps are as follows:

[0037] Step 1: Screening of walnut kernels: After shelling the walnuts, screen out the walnut kernels that are free of odor, mildew, and in petals;

[0038] Step 2: coating of walnut kernels: placing the selected walnut kernels into the composite coating liquid and rapidly stirring for 1 minute, then taking them out and drying them at room temperature to obtain walnut kernels covered with the coating;

[0039] Step 3: Accelerated oxidation storage of walnut kernels: Place the treated walnut kernels in a 40°C oven for accelerated oxidation.

[0040] Since the degree of crushing of walnut kernels will affect their storage quality, generally speaking, the more broken the walnut kernels are, the higher the rate of oxidation and rancidity will be. In order to avoid the influence of sample differences on the storage effect, the embodiment of the present invention first screened the walnut kernels, and then coated and baked them.

[0041] Table 1 shows the changes in peroxide value of walnut kernels during accelerated oxidation storage, Table 2 shows the changes in acid value of walnut kernels during accelerated oxidation storage, and Table 3 shows the changes in browning degree of walnut kernels during accelerated oxidation storage.

[0042] Table 1

[0043] Peroxide value Coating preservation Uncoated 24 days 0.010g / 100g 0.028g / 100g

[0044] Table 2

[0045] Acid value Coating preservation Uncoated 24 days 0.38mg / g 0.62mg / g

[0046] Table 3

[0047] Browning degree Coating preservation Uncoated 24 days 0.462 0.966

[0048] Note: Take 1g of crushed walnut kernels and add 20mL of phosphate buffer solution with a pH of 6.8. Stir at room temperature for 15 minutes and then centrifuge at 8000r / min for 10 minutes. Take the supernatant and measure the absorbance at 450nm as the browning degree of the walnut kernels.

[0049] As can be seen from Tables 1-3, the use of the composite coating liquid provided by the present invention to preserve walnut kernels can slow down the oxidation rate of the walnut kernels, reduce the oxidative rancidity rate and the degree of browning, and improve the storage quality of the walnut kernels.

[0050] Embodiment 3:

[0051] This embodiment provides a method for preparing a composite coating liquid, comprising the following steps:

[0052] (1): Add 20 g of citric acid to 500 mL of deionized water to prepare a 4% citric acid solution;

[0053] (2): 8 g of chitosan was added to the above citric acid solution in sequence, and stirred to dissolve, and then 2 g of soybean protein peptide was added to obtain a base coating solution after the solution was completely dissolved;

[0054] (3): cooling the base coating liquid to room temperature;

[0055] (4): Under magnetic stirring conditions at room temperature, 5 g of glycerol and 1.5 g of sesamol were added to the base coating liquid, and magnetic stirring was performed for 3 h to obtain the composite coating liquid.

[0056] Embodiment 4:

[0057] This embodiment provides a method for preparing a composite coating liquid, comprising the following steps:

[0058] (1): Add 20 g of citric acid to 500 mL of deionized water to prepare a 4% citric acid solution;

[0059] (2): 5 g of chitosan was added to the above citric acid solution in sequence, and stirred to dissolve, and then 2.5 g of soybean protein peptide was added to obtain a base coating solution after the solution was completely dissolved;

[0060] (3): cooling the base coating liquid to room temperature;

[0061] (4): Under magnetic stirring conditions at room temperature, 3 g of glycerol and 1 g of sesamol were added to the base coating liquid, and magnetic stirring was performed for 3 h to obtain the composite coating liquid.

[0062] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present invention.

Claims

1. A composite coating liquid, characterized in that: Its raw materials include: Chitosan, soybean protein peptide, sesamol, glycerol and citric acid solution.

2. The composite coating liquid according to claim 1, characterized in that: The concentration of the citric acid solution is 4%.

3. The composite coating liquid according to claim 1, characterized in that: The mass ratio of citric acid to glycerol and sesamol in the citric acid solution is: 4-20:1-5:0.3-1.

5.

4. The composite coating liquid according to claim 3, characterized in that: The mass ratio of citric acid to glycerol and sesamol in the citric acid solution is 10:2.5:0.

75.

5. The composite coating liquid according to claim 1, characterized in that: The mass ratio of citric acid to chitosan and soybean protein peptide in the citric acid solution is 4-20:1.6-8:0.4-2.

6. The composite coating liquid according to claim 5, characterized in that: The mass ratio of citric acid to chitosan and soybean protein peptide in the citric acid solution is 10:4:

1.

7. A method for preparing the composite coating liquid according to claim 1, characterized in that: The steps include: (1): Prepare citric acid solution; (2): 1.6 g of chitosan was added to the citric acid solution in sequence and stirred to dissolve, and then 0.4 g of soybean protein peptide was added to obtain a base coating solution after the solution was completely dissolved; (3) Add 1 g of glycerol and 0.3 g of sesamol to the base coating liquid, stir magnetically for 3 h, and stir evenly to obtain the composite coating liquid.

8. The method according to claim 7, characterized in that Step (2) comprises: adding chitosan and soybean protein peptide to the citric acid solution in sequence under magnetic stirring at 50° C. to prepare the base coating solution; before step (3), it also comprises: first cooling the base coating solution to room temperature, and then adding glycerol and sesamol under magnetic stirring at room temperature.

9. Use of the composite coating liquid according to claim 1 in preserving walnut kernels.

10. The use according to claim 9, characterized in that: include: The walnut kernels were placed in the composite coating liquid and stirred for 1 minute, then taken out and air-dried at room temperature to obtain walnut kernels covered with the coating.