Forming method of thin-wall housing with inner flanging
By using a combined process of a liquid-filled flanging deep drawing mold and an internal high-pressure forming mold in the molding process of the aero-engine casing, the problems of internal flanging height and sheet metal thinning of the parts are solved, achieving high precision and high quality. Thin-walled casing molding.
Patent Information
- Application Number
- CN202410864849.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-28
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2044-06-28
AI Technical Summary
In the existing technology, during the molding process of aero-engine casings, it is difficult to ensure the height of the inner flange of the parts to meet the required dimensions and it is easy to cause excessive thinning of the sheet metal. Moreover, the traditional process has many steps and is low in efficiency, which affects the appearance quality of the parts.
Using the deep drawing process and the internal high-pressure bulging process, the liquid-filled flanging drawing die and the internal high-pressure forming die are used to control the height of the flanging punch from the sheet material, provide space for reverse expansion, and reduce the height difference caused by liquid-filled reverse expansion. And the bulging amount is compensated during the internal high-pressure forming to ensure the accurate forming of flange fillets and flange edges.
It effectively increases the height of the inner flange, reduces further thinning of parts, improves the dimensional accuracy and surface quality of parts, reduces the load on processing equipment and molds, avoids part breakage, and improves the processing qualification rate.
Smart Images

Figure CN118768459A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of thin-walled parts molding, and in particular to a method for molding a thin-walled cover shell with an inner turn-down edge. Background Art
[0002] The cover of an aircraft engine is a sheet metal part that controls the aerodynamic shape of the aircraft engine and bears the aerodynamic load. The cross-sectional structure of the cover on a certain type of aircraft engine is shown in the attached manual. Figure 1 As shown, in order to meet the requirements of lightweight aircraft engines, the wall thickness of the cover parts is usually designed to be very small, generally within 2mm, and the material is stainless steel. Figure 1 The cover parts have inward and outward features, and the inward height is large. The bottom of the part is convex, and the convex part is at a certain angle to the center line. The flange fillet at the flange edge is small, and the flatness accuracy of the flange edge is required to be high.
[0003] The traditional forming process route of the above-mentioned aircraft engine cover is: the sheet material is first formed into a rotating cylindrical part with an inner flange structure, and then the final part structure is formed by a steel mold split expansion. Due to the high inner flange height of the cover part, three processes are required to draw it into a rotating cylindrical part with a high inner flange, that is, firstly, the steel mold is drawn into a rotating cylindrical part with a low flange height, and then the bottom hole is cut, and the inner hole is formed by the hole to increase the inner flange height. However, due to the small radius of the flange of the part, the wall thickness is greatly reduced by deep drawing, and the inner flange height of the part is large, the hole mouth is very easy to crack by the aforementioned hole-turning process, and the thinning rate is high. In addition, this traditional forming method has many processes and low processing efficiency. In the subsequent steel mold expansion, the steel mold is a split combination, and there will be parting marks on the surface of the formed part, which affects the appearance quality of the part. Moreover, the flatness of the flange edge plane is poor after deep drawing, and the subsequent steel mold expansion cannot correct the flange edge flatness, which requires manual correction by a fitter, which is time-consuming and labor-intensive.
[0004] The patent with publication number CN110434216A discloses a method for integral liquid filling forming of a large annular lip part, which includes the following steps performed in sequence: placing a blank in a transition die; setting key process parameters such as the edge clamping gap, liquid chamber pressure, and punch stroke; using a passive liquid filling forming scheme for transition forming to first form a cylindrical portion inside the integral lip; taking out the transition-shaped part after forming; checking the wall thickness reduction rate of the transition lip part without forming quality problems, and if the thinning is relatively large, heat treatment can be performed to improve the material forming limit; placing the transition lip part without any problems into a final forming die; the final forming die adopts a passive liquid filling forming scheme to flanging the formed transition lip part; taking out the final formed lip part after forming to check its key parameters such as wall thickness reduction rate, mold fit, and surface roughness; using a cutting machine to cut off unnecessary parts such as the flange edge and the internal cylindrical top of the formed lip part without any problems to obtain the final part.
[0005] The above patent is a new technology that performs multi-step liquid filling forming on the basis of ensuring the overall forming of the lip part. The overall forming of the lip part is achieved through a two-step liquid filling forming process and a one-step shaping process. However, in the passive liquid filling forming process of this technical solution, the punch continues to move downward until it enters the die to form the inner flange. As the punch moves downward and the liquid is filled simultaneously, the liquid will expand. Figure 7 As shown in the figure, a height difference of the liquid-filled "soft drawbead" is generated on the part between the punch and the flange edge of the part, which prevents the sheet material from flowing smoothly to the inner flanging structure, affecting the inner flanging forming effect of the part and may even cause the adverse effect of excessive thinning of the part. Summary of the invention
[0006] The technical problem to be solved by the present invention is to provide a method for forming a thin-walled cover with an inner flange, which can ensure the inner flange size of the part is qualified and effectively avoid excessive thinning of the sheet material, in view of the defects of the prior art.
[0007] The purpose of the present invention is achieved through the following technical solutions:
[0008] A method for forming a thin-walled cover shell with an inner flange comprises a drawing process and an internal high-pressure bulging process, wherein the cover shell has a flange and a flange fillet, wherein the drawing process is to use a liquid-filled flanging drawing die to draw a sheet material, wherein the liquid-filled flanging drawing die comprises a female die and a flanging punch, wherein the flanging punch stops moving when it descends to a height h from the sheet material, and waits for liquid to be filled into a liquid chamber formed by the female die and the sheet material and pressurized to the height of the formed inner flange, after which the flanging punch descends again to draw the sheet material into a cylindrical part having an inner flange and a drawn flange fillet, wherein the radius of the drawn flange fillet is larger than the radius of the flange fillet; the internal high-pressure bulging process is used to expand the cylindrical part into a cover shell, so that the drawn flange fillet is formed into a flange fillet.
[0009] Furthermore, the fillet radius of the drawn flange is 5 to 8 times the thickness of the sheet material.
[0010] Furthermore, the height of the cylindrical part is greater than the height of the shell. The height of the cylindrical part is determined according to the principle of equal surface area and based on the surface area of the shell, the height of the cylindrical part in the drawing process is calculated.
[0011] Furthermore, the internal high-pressure bulging process is implemented by an internal high-pressure forming mold, and the internal high-pressure forming mold includes a segmented female mold and a bulging punch, and the bulging punch includes a clamping surface that cooperates with the end face of the segmented female mold to clamp the flange edge, and a step end that cooperates with the inner ring of the segmented female mold to form the flange fillet, the step end is arranged at the clamping surface, and the end face of the step end and the cylindrical part enclose a liquid filling chamber for the internal high-pressure bulging process; a sealing ring is provided at the fitting position of the clamping surface and the end face of the segmented female mold, and the sealing ring is in contact with the flange edge.
[0012] Compared with the prior art, the present invention has the following beneficial effects:
[0013] 1) Subvert the traditional liquid filling deep drawing process. Before filling and drawing, the flanging punch is controlled to be at a certain height from the sheet material to provide a certain anti-expansion space for sheet material forming. Then, the sheet material is filled with liquid to anti-expand. After a certain inner flanging height is formed, the flanging punch is controlled to move downward to draw the sheet material. Before filling and drawing, the punch height is higher than the sheet material, which reduces the height difference of the liquid filling "soft draw ribs" generated by the liquid filling anti-expansion, facilitates the sheet material to flow to the inner flanging structure, effectively reduces the excessive thinning of the blank caused by subsequent drawing, and has the effect of increasing the inner flanging height.
[0014] 2) The height of the cylindrical part is greater than the height of the shell, which is equivalent to pre-compensating the bulging amount to the drawing height of the cylindrical part after liquid filling and flanging. During the external bulging process of the cylindrical part in the internal high-pressure process, the deformation of the material is very small, which can reduce the further thinning of the part. At the same time, it also reduces the liquid chamber pressure required for internal high-pressure molding and reduces the load on related equipment and molds.
[0015] 3) Thin-walled housing parts processed by this forming method are not prone to cracking. The processed parts have high dimensional accuracy, uniform wall thickness distribution, good flange flatness, good surface quality, and high processing qualification rate. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 A partial cross-sectional view of the processed and formed cover shell according to the present invention;
[0017] Figure 2 Schematic diagram of the liquid-filled flanging drawing die for forming a cylindrical part as described in Example 1;
[0018] Figure 3It is a schematic diagram of liquid filling and deep drawing of a sheet material when the height between the flanging punch and the sheet material described in Example 1 is h;
[0019] Figure 4 Schematic diagram of the height H of the cylindrical part after the deep drawing process described in Example 1 is completed;
[0020] Figure 5 A schematic diagram of a molded housing formed by an internal high pressure molding die as described in Example 2;
[0021] Figure 6 for Figure 5 Enlarged view of part I;
[0022] Figure 7 Schematic diagram of traditional liquid filling forming inner flange. DETAILED DESCRIPTION
[0023] In order to clearly illustrate the technical features of the present solution, the present technical solution is described in detail below through specific implementation methods and in conjunction with the accompanying drawings.
[0024] In the following description, many specific details are set forth to facilitate a full understanding of the present application. However, the present application may also be implemented in other ways different from those described herein. Therefore, the scope of protection of the present application is not limited to the specific embodiments disclosed below.
[0025] In addition, in the description of the present application, it should be understood that the terms "center", "upper", "lower", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inner", "outer", "axial", "radial", "circumferential" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present application and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present application. In addition, the terms "first" and "second" are used only for descriptive purposes, and cannot be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Thus, the features defined as "first" and "second" may explicitly or implicitly include one or more of such features. In the description of the present application, the meaning of "multiple" is two or more, unless otherwise clearly and specifically defined.
[0026] In this application, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection, an electrical connection, or a communication; it can be a direct connection, or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.
[0027] In the present application, unless otherwise clearly specified and limited, a first feature "above" or "below" a second feature may be that the first and second features are in direct contact, or the first and second features are in indirect contact through an intermediate medium. In the description of this specification, the description with reference to the terms "one embodiment", "some embodiments", "example", "specific example", or "some examples" means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present application. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in an appropriate manner in any one or more embodiments or examples.
[0028] Example 1
[0029] This embodiment is directed to processing a casing on an aircraft engine. Figure 1 The cross-sectional structure of the cover shell is shown, which has an inner flange 13 and an outer convex structure 14, a flange edge 11 and a flange fillet 12. The following is an example of the size of the cover shell: the wall thickness is 1 mm, the height of the inner flange 13 is 16.2 mm, the bottom of the part barrel is convex, the outer convex structure 14 forms an angle of 6° with the center line, the flange fillet 12 is R2, and the flatness requirement of the flange edge 11 is 0.1 mm.
[0030] Compared with the traditional forming process, this forming method is mainly used for forming a large inner flange height in one step, and at the same time solves the problems of multiple shell forming processes, poor surface quality and large wall thickness reduction. This forming method includes a drawing process and an internal high-pressure bulging process. The drawing process uses a liquid-filled flanging drawing die to draw the sheet material, and the sheet material is filled with liquid flanging and drawn into a cylindrical part with an inner flange and a flange edge. The internal high-pressure bulging process uses internal high pressure to expand the obtained cylindrical part into an outer convex structure, and at the same time, the flange fillet and flange edge are shaped.
[0031] This embodiment describes the drawing process: the cut circular sheet is placed in a Figure 2In the liquid-filled flanging drawing die shown in the figure, the die comprises a female die 21, a flanging punch 22 and a blank holder 23, and the blank holder 23 presses the sheet material (in this embodiment, the blank holder presses the sheet material with a blank holder force of about 20 tons). Figure 2 , Figure 3 As shown, the flanging punch 22 stops moving when it descends to a height h from the sheet, and the booster of the liquid filling device matched with the mold is opened to replenish liquid into the liquid chamber formed by the female mold 21 and the sheet. The liquid level is flush with the pressing surface (i.e., the sheet surface), and then the liquid filling and pressurization are continued to form a partial inner flanging height in the sheet; then the flanging punch 22 is controlled to move downward, and the liquid chamber pressure is gradually increased to about 30MPa, so that the sheet is drawn into a cylindrical part with an inner flanging 13 and a drawn flange fillet. The drawn flange fillet is the preliminary forming of the cover flange fillet 12, and the radius of the drawn flange fillet needs to be larger than the radius of the flange fillet.
[0032] The above-mentioned drawing process is different from conventional liquid filling drawing. During the liquid filling flanging drawing process, a certain height h is reserved between the flanging punch and the sheet material. This height can provide sufficient space for liquid filling to expand, reduce the height difference of the liquid filling "soft draw ribs" generated by liquid filling, facilitate the sheet material to flow to the inner flanging structure, reduce the possibility of excessive thinning of the blank caused by subsequent drawing, and also form a large inner flanging height at one time. The reserved height h in this embodiment is 5mm.
[0033] Since the final flange fillet radius of the housing is relatively small, in order to avoid cracking and excessive thinning of the wall thickness during deep drawing of the parts, the fillet radius of the deep drawing flange in the deep drawing process is set to 5 to 8 times the thickness of the sheet material, that is, the fillet radius of the female mold 21 at the flange edge is designed to be 5 to 8 times the thickness of the sheet material. In this embodiment, the fillet radius of the female mold is 8 mm. In the subsequent internal high pressure forming process, the deep drawing flange fillet is processed into the final flange fillet size by the internal high pressure.
[0034] In order to avoid further thinning of the wall thickness of the drawn parts caused by conventional pure bulging, in the process of liquid drawing and flanging, Figure 4 The height H of the cylindrical part obtained by deep drawing shown in the figure must be greater than the height of the final cover shell. The principle for determining the height of the cylindrical part is: based on the principle of equal surface area, the surface area of the cover shell after internal high-pressure forming is calculated, and this surface area is used as a reference to convert it into the height H of the liquid-filled flanging drawn cylindrical part.
[0035] The design of the height H of the cylindrical part takes into account the pre-compensation of the bulging amount to the drawing height of the cylindrical part after the liquid filling and flanging drawing. During the internal high-pressure forming and external bulging process, the deformation of the material is very small, which can reduce the further thinning of the part. At the same time, it can also reduce the liquid chamber pressure of the internal high-pressure forming required for forming, and reduce the corresponding equipment and mold load.
[0036] The specific process of the drawing process is as follows:
[0037] S1. Place the sheet on the female mold 21, and press the blank ring 23 to hold the sheet;
[0038] S2. The flanging punch 22 moves downward and stops at a certain height h from the sheet;
[0039] S3. Open the booster of the filling equipment to replenish the liquid, and the height of the replenishing liquid level is level with the sheet; thereafter, further increase the liquid chamber pressure to P1 (corresponding to 30MPa in the previous text), and the specific value of the liquid chamber pressure P1 is obtained by simulation calculation;
[0040] S4. The flanging punch 22 moves downward to draw the sheet metal to the bottom, and the mold clearance of the mold meets 1 to 1.2 times the material thickness.
[0041] Example 2
[0042] This embodiment describes the internal high pressure bulging process: the internal high pressure bulging process adopts Figure 5 The internal high pressure forming mold shown in the figure can well form the outer convex structure of the housing. The mold includes a segmented female mold 31 and a bulging punch 32. The bulging punch 32 includes a pressing surface that cooperates with the end face of the segmented female mold 31 to press the flange edge of the cylindrical part, and a step end 321 that cooperates with the inner ring of the segmented female mold 31 to form the flange fillet 12. The step end 321 is arranged at the pressing surface. The end face of the step end 321 and the cylindrical part enclose a liquid filling chamber for the internal high pressure bulging process; the pressing surface is embedded with a sealing ring 33 at the place where it cooperates with the end face of the segmented female mold 31. The sealing ring 33 contacts the flange edge 11, and the sealing ring 33 can effectively seal the entire liquid filling cavity.
[0043] The mold clearance of this internal high-pressure forming mold is 1 to 1.2 times the thickness of the sheet. After the mold is closed, there is still a gap G1 between the outer cylindrical surface of the step end 321 and the inner circle of the segmented female mold 31, and there is still a gap G2 between the clamping surface and the end surface of the segmented female mold 31. The two reserved gaps mainly function as follows: the flange fillet 12 and the flange plane at the gap can be continuously shaped by the liquid chamber pressure, so that the smaller flange fillet 12 is formed in place, and the flange flatness and surface quality are improved. The fillet radius of the segmented female mold 31 is adapted to the size of the flange fillet 12 of the housing. In this embodiment, the size of the gap G1 is 0.2 to 0.5 mm, and the size of the gap G2 is 0.5 to 3 mm.
[0044] In order to reduce the liquid filling volume of the liquid filling chamber and reduce the liquid chamber pressure of the internal high-pressure molding, the internal high-pressure molding mold of this embodiment is also provided with an expansion support block 34 between the end face of the step end 321 and the bottom of the cylindrical part. The expansion support block 34 is generally made of polyurethane. The expansion support block 34 presses the bottom of the cylindrical part with a certain pressure, and can also effectively improve the forming quality of the inner flange structure.
[0045] The specific process of internal high pressure bulging process is as follows:
[0046] S1. Control the divided female mold 31 to close the female mold cavity and place the drawn cylindrical part in the female mold cavity;
[0047] S2. The bulging support block 34 is placed on the bottom of the cylindrical member;
[0048] S3. The bulging punch 32 moves downward, pressing the flange of the cylindrical member through the sealing ring 33 with a blanking force of about 100 tons;
[0049] S4. The supercharger starts the liquid filling operation and pressurizes the liquid chamber to P2. The specific value of the liquid chamber pressure P2 is obtained by simulation calculation. In this embodiment, P2 is 60 MPa to complete the high-pressure forming of the cylindrical part.
[0050] After internal high pressure forming, according to the design size requirements of the cover, the excess size of the bottom hole and flange edge of the part is cut off to obtain the final cover part.
[0051] Example 3
[0052] In order to improve the forming limit of the material and prevent cracking during forming, this embodiment adds a solution heat treatment process between the deep drawing process of embodiment 1 and the internal high pressure forming process of embodiment 2.
[0053] The cover shell processed by this forming method has high dimensional accuracy, uniform wall thickness distribution, good flange flatness, good surface quality, the parts are not prone to cracking during the forming process, and the parts processing qualification rate is high.
[0054] Obviously, the above embodiments are merely examples for clearly illustrating the technical solutions of the present invention, and are not intended to limit the implementation methods of the present invention. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all implementation methods here. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the claims of the present invention.
Claims
1. A method for forming a thin-walled housing with an inner turning edge, characterized in that: The method comprises a drawing process and an internal high-pressure bulging process, wherein the cover shell has a flange edge and a flange fillet, wherein the drawing process is to use a liquid-filled flanging drawing die to draw the sheet metal, wherein the liquid-filled flanging drawing die comprises a female die and a flanging punch, wherein the flanging punch stops moving when it descends to a height h from the sheet metal, and waits for the liquid chamber formed by the female die and the sheet metal to be filled with liquid and pressurized to the height of the formed inner flanging portion, after which the flanging punch descends again to draw the sheet metal into a cylindrical part having an inner flanging and a drawn flange fillet, wherein the radius of the drawn flange fillet is greater than the radius of the flange fillet; the internal high-pressure bulging process is used to expand the cylindrical part into a cover shell, so that the drawn flange fillet is formed into a flange fillet.
2. The method for forming a thin-walled cover with an inner turning edge according to claim 1, characterized in that: The fillet radius of the drawn flange is 5 to 8 times the thickness of the sheet material.
3. The method for forming a thin-walled casing with an inner turning edge according to claim 1, characterized in that: The height of the cylindrical part is greater than the height of the shell. The height of the cylindrical part is determined according to the principle of equal surface area and based on the surface area of the shell, the height of the cylindrical part in the drawing process is calculated.
4. The method for forming a thin-walled casing with an inner turning edge according to claim 1, characterized in that: The clamping gap of the liquid-filled flanging drawing die is 1 to 1.2 times the thickness of the sheet material.
5. The method for forming a thin-walled casing with an inner turning edge according to claim 1, characterized in that: The internal high-pressure bulging process is implemented by an internal high-pressure forming mold, and the internal high-pressure forming mold includes a segmented female mold and a bulging punch. The bulging punch includes a clamping surface that cooperates with the end face of the segmented female mold to clamp the flange edge, and a step end that cooperates with the inner ring of the segmented female mold to form the flange fillet. The step end is arranged at the clamping surface, and the end face of the step end and the cylindrical part enclose a liquid filling chamber for the internal high-pressure bulging process; a sealing ring is provided at the joint between the clamping surface and the end face of the segmented female mold, and the sealing ring is in contact with the flange edge.
6. The method for forming a thin-walled casing with an inner turning edge according to claim 5, characterized in that: The mold clearance of the internal high pressure forming mold is 1 to 1.2 times the thickness of the sheet material.
7. The method for forming a thin-walled casing with an inner turning edge according to claim 5, characterized in that: There is a gap between the pressing surface and the end surface of the segmentation female mold.
8. The method for forming a thin-walled casing with an inner turning edge according to claim 5, characterized in that: There is a gap between the outer cylindrical surface of the step end and the inner circle of the segmented female mold.
9. The method for forming a thin-walled casing with an inner turning edge according to claim 5, characterized in that: An expansion support block is provided between the end surface of the step end and the bottom of the cylindrical member.
10. The method for forming a thin-walled casing with an inner turning edge according to claim 1, characterized in that: A solution heat treatment step is also provided between the drawing step and the internal high pressure bulging step.
Citation Information
Patent Citations
Integral liquid-filling forming method for large annular lip part
CN110434216A
Method of reducing cycle time in a hydro-mechanical forming process and a tool for hydro-mechanically forming a part
CN102658327A
Press forming method for steel plate
CN103313807A
End cone forming method, forming die and end cone
CN113210488A
Rigid-flexible composite forming device and method for improving die attaching precision of deep concave bottom part
CN113523104A
Cited By
Aero-engine lip forming method, device and system
CN121222948A