Preparation method and device of prepreg
The resin and fiber are directly combined through the slit coating die and extrusion mechanism, which solves the problems of unstable areal density and space occupation of traditional hot-melt prepregs, and enables high-quality, high-speed production of low-area-density prepregs. .
Patent Information
- Application Number
- CN202411065889.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-05
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2044-08-05
AI Technical Summary
Prepregs prepared by the traditional hot-melt method suffer from large areal density fluctuations and poor stability, making it impossible to produce low-area-density resin films. The process has many steps, takes up space, and has high requirements on the storage environment.
Using a slit coating die and an extrusion mechanism, the resin is melted and flows into the slit coating die through a conduit to form a uniformly distributed resin film that is combined with the fibers. Prepreg preparation is completed through roller pressing, avoiding the need for separate Requirements for the production of resin films and low-temperature and low-humidity storage environments.
It achieves ±1% change in prepreg area density, improves product quality stability, can produce ultra-thin prepregs below 10g/m2, and has a higher production rate than traditional hot melt methods, saving storage costs.
Smart Images

Figure CN118769423A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of prepreg preparation, and in particular to a method and device for preparing a prepreg. Background Art
[0002] As a standardized intermediate material, prepreg occupies an extremely important position in the field of composite material manufacturing due to its high-precision control of resin content and simple operation.
[0003] In the prior art, the commonly used method for preparing prepreg is mainly a two-step hot melt process, which is as follows: first, a resin is prepared by a glue coating machine, and then the resin is compounded with fibers. However, the prepreg prepared by this method has the disadvantages of large fluctuations in surface density, poor stability, and inability to produce resin films with low surface density. Secondly, the hot melt method involves many process steps, and the produced resin not only occupies a certain space, but also has high requirements for the storage environment. Summary of the invention
[0004] The purpose of the present application is to propose a method and device for preparing prepreg, aiming to solve the problems of large fluctuations in surface density, difficult control of product quality, and inability to produce resin films with low surface density in the traditional hot melt method for preparing prepreg.
[0005] In a first aspect, an embodiment of the present application provides a device for preparing a prepreg, comprising a slit coating die and an extrusion mechanism, the slit coating die comprising a first cavity connected to the extrusion mechanism and a second cavity connected to the first cavity, the slit coating die is provided with a lead-out port on a side close to the second cavity, the lead-out port is connected to the second cavity, the extrusion mechanism is used to place and extrude resin, and the lead-out port is used to lead out molten or melted resin.
[0006] Preferably, at least one first through hole communicating with the first cavity is provided on one side of the slit coating die head close to the first cavity, and a second through hole is further provided inside the slit coating die head, one end of the second through hole is communicating with the first cavity, and the other end of the through hole is communicating with the second cavity;
[0007] The extrusion mechanism is connected to the first through hole through a conduit.
[0008] In a second aspect, an embodiment of the present application provides a method for preparing a prepreg, which is implemented by the above-mentioned prepreg preparation device, and the method includes:
[0009] placing a resin in an extrusion mechanism, heating the extrusion mechanism to melt or molten the resin, and pressurizing the resin by the extrusion mechanism to deliver the molten or molten resin to a slot coating die;
[0010] The molten or melted resin flows out through the first cavity, the second cavity, and the outlet in sequence to form a resin film, which is combined with the fibers and pressed by rollers to complete the impregnation to obtain a prepreg.
[0011] Preferably, the resin is a thermosetting resin, and the thermosetting resin includes at least one of thermosetting resins such as unsaturated polyester resin, epoxy resin, phenolic resin, polyurethane resin, bismaleimide resin, etc.
[0012] Preferably, the resin is a thermoplastic resin, and the thermoplastic resin includes at least one of thermoplastic resins such as polyethylene resin, polypropylene resin, polyamide resin, polycarbonate resin, polyphenylene sulfide resin, and polyaryletherketone resin.
[0013] Preferably, the surface density of the resin film is 2 to 200 g / m 2 .
[0014] Preferably, the material of the fiber includes at least one of carbon fiber, glass fiber, silicon carbide fiber, alumina fiber, ceramic fiber and other inorganic fiber, ultra-high molecular weight polyethylene fiber, ultra-high molecular weight polypropylene fiber, polyamide fiber, polyacrylonitrile fiber, aramid fiber, polyphenylene benzobisoxazole fiber, polybenzimidazole fiber, polyimide fiber and other organic fiber, cotton fiber, hemp fiber, bamboo fiber, cellulose fiber and other plant fiber, the fiber form is one of unidirectional fiber, woven fabric, knitted fabric, braided fabric, non-woven fabric, the surface density of the fiber is 3-400g / m 2 .
[0015] Preferably, the surface density of the prepreg is 5 to 600 g / m 2 The surface density variation range is ±1%, and the resin content of the prepreg is 20wt% to 50wt%.
[0016] Preferably, the extrusion mechanism comprises at least one of a screw extruder, a plunger pump and a gear pump, the heating temperature of the extrusion mechanism is room temperature to 400° C., and the applied pressure of the extrusion mechanism is 0 to 20 MPa.
[0017] Preferably, the temperature of the roller is 50-400° C., and the pressure of the roller is 1-20 MPa.
[0018] Compared with the prior art, this application has the following advantages:
[0019] 1. The present application places the resin in an extrusion mechanism through a slit coating die. In the actual production process, the resin is melted or melted and flows into the slit coating die through a conduit through the first through hole. After the resin flows into the first cavity, it is evenly distributed in the first cavity. When the liquid value in the first cavity accumulates to a certain height, it automatically flows into the second cavity through the second through hole under the influence of its own gravity and extrusion pressure, and then flows out from the guide port to form a resin film, which is then combined with the fiber to complete the preparation of the prepreg. The whole process does not require the separate production of the resin film, and at the same time, there is no need to provide a storage space for the resin film and a low-temperature and low-humidity storage environment, which can effectively save storage costs.
[0020] 2. By combining liquid resin with fiber to replace the traditional two-step hot-melt method of "coating resin film and then compounding with fiber", the surface density variation range of the prepreg is made to be ±1%, which is much lower than the error of the two-step hot-melt process, greatly improving the quality stability of the product.
[0021] 3. The prepreg surface density produced in this application is 5 to 600 g / m 2 , which can produce less than 10g / m 2 prepreg, thus meeting the production of ultra-thin prepreg.
[0022] 4. The prepreg production rate of the present application is 40-50 m / min, which is much higher than the production speed of the hot melt two-step process and has the advantage of high production efficiency.
[0023] Additional aspects and advantages of the present application will be given in part in the following description, and in part will become apparent from the following description, or will be understood through the embodiments of the present application. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] Figure 1 A schematic diagram of the structure of a slit coating die and an extrusion mechanism of an embodiment of the present application is shown;
[0025] Figure 2 A schematic structural diagram of a prepreg preparation device according to an embodiment of the present application is shown;
[0026] Figure 3 Another structural schematic diagram of a prepreg preparation device according to an embodiment of the present application is shown;
[0027] Figure 4 A flow chart of a method for preparing a prepreg according to an embodiment of the present application is shown.
[0028] Explanation of symbols: 10-slit coating die, 20-extrusion mechanism, 40-wire collecting mechanism, 70-winding mechanism, 80-fabric unwinding mechanism, 90-conduit, 101-first cavity, 102-second cavity, 103-first through hole, 104-second through hole, 105-lead-out port, 301-fixed plate, 302-yarn shaft, 501-support member, 502-yarn spreading roller, 601-PE film unwinding device, 602-release paper unwinding device, 603-first roller, 604-second roller. DETAILED DESCRIPTION
[0029] In order to facilitate understanding of the present application, the present application will be described more fully below with reference to the relevant drawings. Several embodiments of the present application are provided in the drawings. However, the present application can be implemented in many different forms and is not limited to the embodiments described herein. On the contrary, the purpose of providing these embodiments is to make the disclosure of the present application more thorough and comprehensive.
[0030] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art to which this application belongs. The terms used herein in the specification of this application are only for the purpose of describing specific embodiments and are not intended to limit this application. The term "and / or" used herein includes any and all combinations of one or more of the related listed items.
[0031] In this document, unless otherwise specified, the term "°C" means "degrees Celsius"; the term "MPa" means: megapascal; the term "μm" means: micrometer; the term "g / m 2 " means: grams per square meter; the term "min" means: minutes; the term "wt%" means: mass percentage; the term "m / min" means: meters per minute.
[0032] In this article, all defined ranges are meant to include each specific range within a given range and a combination of sub-ranges between given ranges. For example, a range of 1 to 5 specifically includes 1, 2, 3, 4 and 5, and also includes sub-ranges such as 2 to 5, 3 to 5, 2 to 3, 2 to 4, 1 to 4, etc.
[0033] <First aspect>
[0034] like Figure 1As shown, the embodiment of the present application provides a device for preparing a prepreg, the device comprising a slit coating die 10 and an extrusion mechanism 20, the slit coating die 10 comprising a first cavity 101 connected to the extrusion mechanism 20 and a second cavity 102 connected to the first cavity 101, a side of the slit coating die 10 close to the second cavity 102 is provided with a guide port 105, the guide port 105 is connected to the second cavity 102, the extrusion mechanism 20 is used to place and extrude the resin, and the guide port 105 is used to guide the molten or melted resin;
[0035] In some embodiments, at least one first through hole 103 communicating with the first cavity 101 is provided on one side of the slit coating die 10 close to the first cavity 101, and a second through hole 104 is further provided inside the slit coating die 10, one end of the second through hole 104 is communicating with the first cavity 101, and the other end of the through hole is communicating with the second cavity 102, and the extrusion mechanism 20 is connected to the first through hole 103 through the conduit 90. In the actual production process, the resin is placed in the extrusion mechanism 20, and the resin is melted or melted, and then flows into the slit coating die 10 through the conduit 90 through the first through hole 103. After the resin flows into the first cavity 101, it is evenly distributed in the first cavity 101. When the liquid value in the first cavity 101 accumulates to a certain height, it automatically flows into the second cavity 102 through the second through hole 104 under the influence of its own gravity and extrusion pressure, and then flows out from the guide port 105, and then combines with the fiber, thereby completing the preparation of the prepreg.
[0036] It should also be pointed out that the outlet 105 penetrates the bottom of the slot coating die 10 in the transverse direction, and the fibers are combined with the liquid resin coming out of the outlet 105 in the transverse direction, which can further improve the prepreg effect.
[0037] In some embodiments, the extrusion mechanism 20 is one of a plunger pump, a gear pump, and a screw extruder.
[0038] In some embodiments, Figure 2 As shown, the prepreg preparation device includes, in addition to the extrusion mechanism 20 and the slot coating die 10 , a creel mechanism, a yarn collecting mechanism 40 , a yarn spreading mechanism, a prepreg mechanism and a winding mechanism 70 .
[0039] The yarn rack mechanism includes a fixed plate 301 and a yarn shaft 302 arranged on the fixed plate 301, the yarn shaft 302 is used to place the yarn roll, the yarn unwinding mechanism includes a support member 501 and a plurality of yarn unwinding rollers 502 arranged on the support member 501, the wire collecting mechanism 40 is a wire collecting plate with a plurality of through holes, the prepreg mechanism includes a PE film unwinding device 601, a release paper unwinding device 602 and two first rollers 603 and two second rollers 604 located on both sides of the yarn, the first roller 603 is used to press the liquid resin and the fiber yarn, the PE film unwinding device 601 is used to place the PE film, the release paper unwinding device 602 is used to place the release paper, the second roller 604 is used to press the PE film and the fiber yarn pre-impregnated with the resin, and the winding mechanism 70 is used to wind up the prepared prepreg.
[0040] In the actual production process, the yarn in the yarn roll is transported to the wire collecting mechanism 40 via the yarn frame mechanism, and is transported to the yarn spreading mechanism along the same horizontal plane. The liquid resin output by the extrusion mechanism 20 and the die head 10 is then transported to the unfolded yarn, and is pressed and pre-impregnated by the upper and lower first rollers. Then, the upper surface of the fiber yarn pre-impregnated with the resin is combined with the transported PE film, and the lower surface thereof is combined with the transported release paper, and is pressed together by the upper and lower second rollers to obtain a prepreg, which is transported to the winding mechanism 70 to complete the collection of the prepreg.
[0041] In some embodiments, Figure 3 As shown, the prepreg preparation device includes, in addition to the extrusion mechanism 20 and the slot coating die 10, a fabric unwinding mechanism 80, a prepreg mechanism and a winding mechanism 70;
[0042] The fabric unwinding mechanism 80 is used to place the fabric, and the prepreg mechanism includes a PE film unwinding device 601, a release paper unwinding device 602, and two first rollers 603 and two second rollers 604 located on both sides of the yarn. The first roller 603 is used to press the liquid resin and the fiber yarn, the PE film unwinding device 601 is used to place the PE film, the release paper unwinding device 602 is used to place the release paper, the second roller 604 is used to press the PE film and the fiber yarn pre-impregnated with the resin, and the winding mechanism 70 is used to wind up the prepared prepreg.
[0043] In the actual production process, the fabric unwinding device continuously conveys the fabric, and the liquid resin output by the extrusion mechanism 20 and the die head 10 is then conveyed to the fabric, and is pressed and pre-impregnated by the upper and lower first rollers. Then, the upper surface of the fiber yarn pre-impregnated with the resin is combined with the conveyed PE film, and the lower surface is combined with the conveyed release paper, and they are pressed together by the upper and lower second rollers to obtain a prepreg, which is conveyed to the winding mechanism 70 to complete the collection of the prepreg.
[0044] In summary, according to the above-mentioned device for preparing a prepreg, the resin is placed in the extrusion mechanism through the slit coating die. In the actual production process, the resin is melted or melted, and then flows into the slit coating die through the conduit through the first through hole. After the resin flows into the first cavity, it is evenly distributed in the first cavity. When the liquid value in the first cavity accumulates to a certain height, it is automatically affected by its own gravity and extrusion pressure. It flows into the second cavity through the second through hole and then flows out from the guide port, and then combines with the fiber to complete the preparation of the prepreg. The whole process does not require the separate production of resin film, and at the same time, there is no need to provide resin storage space and a low-temperature and low-humidity storage environment, which can effectively save storage costs. In addition, by combining liquid resin with fiber to replace the traditional hot melt two-step method of "coating resin film and then compounding with fiber", the surface density of the prepreg changes by ±1%, which is much lower than the error of the hot melt two-step process, greatly improving the quality stability of the product.
[0045] like Figure 4 As shown, the embodiment of the present application provides a method for preparing a prepreg, the method comprising steps S101 to S102, wherein:
[0046] Step S101: placing a resin in an extrusion mechanism, heating the extrusion mechanism to melt or melt the resin, pressurizing the resin by the extrusion mechanism, and conveying the melted or molten resin to a slot coating die;
[0047] Step S102: The molten or melted resin flows out through the first cavity, the second cavity, and the outlet in sequence to form a resin film, which is combined with the fibers and pressed by rollers to complete the impregnation to obtain a prepreg.
[0048] In some embodiments, the resin may be a thermoplastic resin or a thermosetting resin, wherein the thermosetting resin includes at least one of thermosetting resins such as unsaturated polyester resin, epoxy resin, phenolic resin, polyurethane resin, bismaleimide resin, and the thermoplastic resin includes at least one of thermoplastic resins such as polyethylene resin, polypropylene resin, polyamide resin, polycarbonate resin, polyphenylene sulfide resin, polyaryletherketone resin, and the like.
[0049] In some embodiments, the surface density of the resin film is 2 to 200 g / m 2 That is to say, by melting or molten resin and then pre-impregnating, it can be applied to the pre-impregnation of resin with extremely low surface density, with a wide industrial range and strong applicability. For example, the surface density of the resin can be 2g / m 2 , 10g / m 2 , 50g / m 2 , 100g / m 2 , 150g / m 2 , 200g / m2 etc.
[0050] In some embodiments, the fiber material includes at least one of carbon fiber, glass fiber, silicon carbide fiber, alumina fiber, ceramic fiber and other inorganic fibers, ultra-high molecular weight polyethylene fiber, ultra-high molecular weight polypropylene fiber, polyamide fiber, polyacrylonitrile fiber, aramid fiber, polyphenylene benzobisoxazole fiber, polybenzimidazole fiber, polyimide fiber and other organic fibers, cotton fiber, hemp fiber, bamboo fiber, cellulose fiber and other plant fibers. That is, the fiber can be carbon fiber, glass fiber, silicon carbide fiber, alumina fiber, ceramic fiber and other inorganic fibers, ultra-high molecular weight polyethylene fiber, ultra-high molecular weight polypropylene fiber, polyamide fiber, polyacrylonitrile fiber, aramid fiber, polyphenylene benzobisoxazole fiber, polybenzimidazole fiber, polyimide fiber and other organic fibers. The fabric is made of a single material of plant fibers such as organic fibers, cotton fibers, hemp fibers, bamboo fibers, cellulose fibers, etc.; it can also be made of multiple materials of inorganic fibers such as carbon fibers, glass fibers, silicon carbide fibers, alumina fibers, ceramic fibers, ultra-high molecular weight polyethylene fibers, ultra-high molecular weight polypropylene fibers, polyamide fibers, polyacrylonitrile fibers, aramid fibers, polyphenylene benzobisoxazole fibers, polybenzimidazole fibers, polyimide fibers, etc., and plant fibers such as cotton fibers, hemp fibers, bamboo fibers, cellulose fibers, etc. The fiber is one of unidirectional fibers, woven fabrics, knitted fabrics, braided fabrics, and nonwoven fabrics. That is to say, the fiber is a single form such as unidirectional fibers, woven fabrics, knitted fabrics, braided fabrics, and nonwoven fabrics; the surface density of the fiber is 3 to 400 g / m 2 For example, the surface density of the fiber can be 3 g / m 2 , 5g / m 2 , 10g / m 2 , 50g / m 2 , 100g / m 2 , 150g / m 2 , 200g / m 2 , 300g / m 2 , 400g / m 2 etc.
[0051] In some embodiments, the prepreg has an area density of 5 to 600 g / m 2 For example, the surface density of the obtained prepreg can be 5g / m 2 , 10g / m 2 , 50g / m 2 , 100g / m 2 , 150g / m 2 , 200g / m 2 , 300g / m 2 , 400g / m 2 , 500g / m 2, 600g / m 2 Etc., the surface density variation range is ±1%, which is much lower than the error of the two-step hot melt process, indicating that the product quality is stable and high; in addition, the resin content of the prepreg is 20wt% to 50wt%. Exemplarily, the resin content of the prepreg can be 20wt%, 30wt%, 40wt%, 50wt% and so on.
[0052] In some embodiments, the heating temperature of the extrusion mechanism is room temperature to 400°C, so that the resin is completely melted or molten. If the heating temperature is too low, the resin will not be completely melted or molten, or even not melted or molten. If the heating temperature is too high, energy is wasted. For example, the heating temperature of the extrusion mechanism can be 50°C, 100°C, 150°C, 200°C, 250°C, 300°C, 350°C, 400°C, etc. The applied pressure of the extrusion mechanism is 0 to 20MPa. For example, the applied pressure can be 1MPa, 5MPa, 10MPa, 15MPa, 20MPa, etc.
[0053] In some embodiments, the temperature of the roller is 50-400°C, that is, the temperature of the first roller and the second roller are both 50-400°C. For example, the temperature of the roller can be 50°C, 100°C, 150°C, 200°C, 250°C, 300°C, 350°C, 400°C, so that the resin can also remain molten or melted when combined with the fiber. The pressure of the roller is 1-20MPa, that is, the pressure of the first roller and the second roller is both 1-20MPa. For example, the pressure of the roller can be 1MPa, 5MPa, 10MPa, 15MPa, 20MPa, etc.
[0054] In some embodiments, the production rate of the prepreg using the method of the present application is 40 to 50 m / min, which is much higher than the production speed of the two-step hot melt process and has the advantage of high production efficiency.
[0055] Example 1
[0056] 5 kg of epoxy resin was placed in a plunger pump, and the plunger pump was heated at 80 °C and the pressure was 3 MPa. The melted epoxy resin was introduced into the slit coating die head, and flowed out through the first cavity, the second cavity, and the outlet in sequence to coat the epoxy resin to a surface density of 97.5 g / m 2 The surface of the glass fiber yarn is then continuously pressed by a first roller and a second roller. The pressure of the first roller and the second roller are both 1MPa and the temperature is 80°C. The surface density of the glass fiber yarn is 150±1.3g / m 2 The glass fiber / epoxy prepreg has a production speed of 40m / min and a resin content of 35wt%.
[0057] Example 2
[0058] 2kg of polypropylene powder was placed in a screw extruder, and the screw heating temperature was maintained at 210°C and the pressure was maintained at 10MPa. The molten polypropylene resin was introduced into the slit coating die head, and flowed out through the first cavity, the second cavity, and the outlet in sequence to coat 3g / m 2 The surface of the carbon fiber yarn (T300-1 K) was prepared by continuous pressing of the first roller and the second roller. The pressure of the first roller and the second roller were both 10 MPa and the temperature was 210 ° C. 2 The ultra-thin prepreg has a production speed of 50m / min and a resin content of 40wt%.
[0059] Example 3
[0060] 2 kg of polypropylene powder was placed in a screw extruder, and the screw heating temperature was maintained at 210 ° C and the pressure was maintained at 10 MPa. The molten polypropylene resin was introduced into the slit coating die head, and flowed out through the first cavity, the second cavity, and the outlet in sequence to coat the surface density of 200 g / m 2 The surface of the aramid plain fabric is then continuously pressed by the first roller and the second roller. The pressure of the first roller and the second roller are both 10MPa and the temperature is 210℃. The surface density is 300±2g / m 2 The aramid plain fabric reinforced polypropylene prepreg has a production speed of 45m / min and a resin content of 33wt%.
[0061] Example 4
[0062] 2 kg of epoxy resin was placed in a gear pump, and the gear pump temperature was maintained at 70 °C and the pressure was maintained at 11.5 MPa. The melted epoxy resin was introduced into the slit coating die head, and flowed out through the first cavity, the second cavity, and the outlet in sequence to coat the epoxy resin to a surface density of 300 g / m 2 The surface of the carbon fiber yarn (T700SC-24K) was pressed by a first roller and a second roller, the pressure of the first roller and the second roller were both 10.5MPa and the temperature was 90℃, and the surface density was 400±3g / m 2 The carbon fiber / epoxy prepreg has a production speed of 45m / min and a resin content of 25wt%.
[0063] Example 5
[0064] 2kg of polyetheretherketone plastic particles were placed in a screw extruder, and the screw heating temperature was maintained at 400℃ and the pressure was maintained at 15MPa. The molten polyetheretherketone resin was introduced into the slit coating die head, and flowed out through the first cavity, the second cavity, and the outlet in sequence to coat 20g / m2 The surface of the carbon fiber yarn (T800H-6K) was prepared by continuous pressing of the first roller and the second roller. The pressure of the first roller and the second roller were both 20MPa and the temperature was 380℃. 2 The prepreg has a production speed of 40m / min and a resin content of 33wt%.
[0065] Comparative Example 1
[0066] The hot melt two-step process is used to prepare the surface density of 30g / m 2 Carbon fiber (T800H-6K) / epoxy prepreg. 2kg of epoxy resin was placed in the material tank, the roller temperature was kept at 80°C, the epoxy resin was melted, and introduced into the resin coating machine, and a resin film was formed by three-roll lamination. The resin film was then placed in a compounding machine and compounded with the carbon fiber to prepare a surface density of 30±4g / m 2 The carbon fiber / epoxy prepreg has a production speed of 20 m / min and a resin content of 33 wt%. The entire process consumes a large amount of release paper and PE film.
[0067] Comparative Example 2
[0068] 2 kg of epoxy resin was placed in the material tank, the roller temperature was maintained at 80 °C, the epoxy resin was melted, introduced into the resin coating machine, and formed into a surface density of 5 g / m by three-roll pressing. 2 The resin film is then placed in a composite machine and composited with carbon fiber (T300-1K) to prepare a carbon fiber with a surface density of 25±2g / m 2 The carbon fiber / epoxy prepreg was produced at a speed of 15 m / min and the resin content of the prepreg was 40 wt%. It was found that the limiting surface density of the resin film prepared by three rollers was 5 g / m 2 The double-sided lamination method cannot produce ultra-thin prepreg (surface density less than 10g / m 2 ).
[0069] Comparative Example 3
[0070] 2 kg of epoxy resin was placed in a gear pump, and the gear pump temperature was maintained at 40 °C and the pressure was maintained at 20 MPa. The melted epoxy resin was introduced into the slit coating die head, and flowed out through the first cavity, the second cavity, and the outlet in sequence to coat the epoxy resin to a surface density of 300 g / m 2 The surface of the carbon fiber yarn (T700SC-24K) was pressed by a first roller and a second roller, the pressure of the first roller and the second roller were both 10.5MPa and the temperature was 90℃, and the surface density was 400±5g / m 2The carbon fiber / epoxy prepreg has a production speed of 5m / min and a resin content of 25wt%.
[0071] It can be seen from Comparative Example 1 that the hot melt two-step process is used to prepare the prepreg. On the one hand, the resin film preparation consumes materials such as release paper and PE film. On the other hand, before the resin film is compounded with the fiber, the storage of the resin film requires space and a low-temperature and low-humidity environment, which consumes a lot of storage costs. The slit coating method for manufacturing prepregs provided by the technology of the present invention can avoid the separate manufacture of the resin film and save storage costs. In addition, by comparing Example 2 and Comparative Example 2, it can be seen that the technology of the present invention has great advantages in manufacturing ultra-thin prepregs and in controlling the stability of the prepreg surface density.
[0072] It can be seen from Example 4 and Comparative Example 3 that there is a suitable parameter range for the slit coating process. The resin extrusion mechanisms in Example 4 and Comparative Example 3 are both gear pumps, and the heating temperatures of the gear pumps are different. The heating temperature in Example 4 is 70°C, and the epoxy resin has good fluidity at 70°C, so it is easy to achieve good impregnation of the fiber, and the production speed can reach 45m / min. In Comparative Example 3, since the heating temperature of the gear pump is only 40°C, the viscosity of the epoxy resin at 40°C is still very large, and the fluidity is poor. Even if the resin extrusion pressure is increased to 20MPa, the production speed of the prepreg cannot be accelerated. The prepreg production speed in Comparative Example 3 is only 5m / min, which is inefficient and cannot meet industrial production.
[0073] The above-mentioned embodiments only express several implementation methods of the present application, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the scope of the present application. It should be pointed out that, for a person of ordinary skill in the art, several variations and improvements can be made without departing from the concept of the present application, and these all belong to the protection scope of the present application. Therefore, the protection scope of the present application shall be subject to the attached claims.
Claims
1. A device for preparing prepreg, characterized in that: The invention comprises a slit coating die and an extrusion mechanism, wherein the slit coating die comprises a first cavity connected to the extrusion mechanism and a second cavity connected to the first cavity, a guide outlet is provided on a side of the slit coating die close to the second cavity, the guide outlet is connected to the second cavity, the extrusion mechanism is used for placing and extruding resin, and the guide outlet is used for guiding out molten or melted resin.
2. The prepreg preparation device according to claim 1, characterized in that: At least one first through hole communicating with the first cavity is provided on one side of the slit coating die head close to the first cavity, and a second through hole is also provided inside the slit coating die head, one end of the second through hole is communicating with the first cavity, and the other end of the through hole is communicating with the second cavity; The extrusion mechanism is connected to the first through hole through a conduit.
3. A method for preparing a prepreg, which is achieved by using the prepreg preparation device according to any one of claims 1 to 2, characterized in that: The method comprises: placing a resin in an extrusion mechanism, heating the extrusion mechanism to melt or molten the resin, and pressurizing the resin by the extrusion mechanism to deliver the molten or molten resin to a slot coating die; The molten or melted resin flows out through the first cavity, the second cavity and the outlet in sequence to form a resin film, and is combined with the fibers, and is pressed by rollers to complete the impregnation to obtain a prepreg.
4. The method for preparing the prepreg according to claim 3, characterized in that: The resin is a thermosetting resin, and the thermosetting resin includes at least one of thermosetting resins such as unsaturated polyester resin, epoxy resin, phenolic resin, polyurethane resin, bismaleimide resin, and the like.
5. The method for preparing the prepreg according to claim 3, characterized in that: The resin is a thermoplastic resin, and the thermoplastic resin includes at least one of thermoplastic resins such as polyethylene resin, polypropylene resin, polyamide resin, polycarbonate resin, polyphenylene sulfide resin, and polyaryletherketone resin.
6. The method for preparing a prepreg according to claim 3, characterized in that: The surface density of the resin film is 2 to 200 g / m 2 .
7. The method for preparing a prepreg according to claim 3, characterized in that: The fiber material includes at least one of carbon fiber, glass fiber, silicon carbide fiber, alumina fiber, ceramic fiber and other inorganic fiber, ultra-high molecular weight polyethylene fiber, ultra-high molecular weight polypropylene fiber, polyamide fiber, polyacrylonitrile fiber, aramid fiber, polyphenylene benzobisoxazole fiber, polybenzimidazole fiber, polyimide fiber and other organic fiber, cotton fiber, hemp fiber, bamboo fiber, cellulose fiber and other plant fiber, the fiber form is one of unidirectional fiber, woven fabric, knitted fabric, braided fabric, non-woven fabric, the surface density of the fiber is 3-400g / m 2 .
8. The method for preparing a prepreg according to claim 3, characterized in that: The surface density of the prepreg is 5 to 600 g / m 2 The surface density variation range is ±1%, and the resin content of the prepreg is 20wt% to 50wt%.
9. The method for preparing a prepreg according to claim 3, characterized in that: The extrusion mechanism at least comprises one of a screw extruder, a plunger pump and a gear pump. The heating temperature of the extrusion mechanism is room temperature to 400° C., and the applied pressure of the extrusion mechanism is 0 to 20 MPa.
10. The method for preparing a prepreg according to claim 3, characterized in that: The temperature of the roller is 50-400° C., and the pressure of the roller is 1-20 MPa.
Citation Information
Patent Citations
Elimination of surfacing film and primer from composite substrates through the use of a co-curable paint film
CN112321868A
Preparation method of asymmetrically infiltrated high-collimation high-surface-viscosity fabric prepreg
CN114103172A
Preparation method of thermosetting resin-based high-modulus carbon fiber hot-melt prepreg
CN116674123A
Continuous fiber fabric reinforced thermoplastic composite material and preparation method thereof
CN117507189A
Method of producing thermoplastic prepreg
JP2020157568A
Cited By
Preparation method of thickening continuous short carbon fiber composite prepreg
CN119912721A