Inducing mechanical stress in magnetoresistive sensing element to align axis of magnetization of reference layer system in preferred direction to improve sensor performance
By introducing a stress-inducing layer into the layer stack of the magnetoresistive sensor and tuning the orientation of the magnetization axis, the problem of changes in magnetic properties caused by mechanical stress is solved, the sensitivity and life of the sensor are improved, and the angular error is reduced.
Patent Information
- Application Number
- CN202410388822.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-04-03
- Filing Date
- 2024-04-01
- Publication Date
- 2024-10-15
AI Technical Summary
Magnetoresistive sensors are exposed to mechanical stress during manufacturing and packaging, causing changes in the magnetic properties of the layer stack, increasing sensing errors, reducing sensitivity and shortening sensing element life.
By introducing a stress-inducing layer into the layer stack of a magnetoresistive sensor, the orientation of the magnetization axis is tuned so that it is aligned parallel or perpendicular to the mechanical stress axis, thus stabilizing the reference layer system, enhancing the TMR effect and sensitivity, and extending the lifetime of the sensing element. life.
Effectively reduce sensing errors, enhance TMR effect, increase signal amplitude, extend the life of sensing elements, and improve the accuracy of angle sensors.
Smart Images

Figure CN118777951A_ABST
Abstract
Description
Background Art
[0001] Magnetic field sensors based on the magnetoresistance effect are called magnetoresistive sensors and are often used in magnetic field sensing applications, such as current sensing, position sensing, and angle sensing. Magnetoresistance is a property of a material that changes the value of the material's resistance when an external magnetic field is applied to the material. Due to the high signal level and high accuracy of magnetoresistive sensors, as well as the possibility of integrating magnetoresistive sensors into complementary metal oxide (CMOS) and bipolar CMOS (BiCMOS) technologies, magnetoresistive sensors can be a preferred choice based on Hall sensors. Some types of magnetoresistive sensors include anisotropic magnetoresistive (AMR) sensors, giant magnetoresistive (GMR) sensors, and tunneling magnetoresistive (TMR) sensors, each type utilizing a corresponding magnetoresistive effect.
[0002] A large number of different magnetoresistance effects are often abbreviated as xMR, where "x" is used as a placeholder for different magnetoresistance effects. An xMR sensor can detect the orientation of an applied magnetic field by measuring the sine angular component and the cosine angular component using a monolithic integrated magnetoresistance sensing element. Here, the abbreviations of the xMR sensors represent the magnetoresistance effects used to detect the corresponding magnetic fields, respectively. In this regard, the GMR effect is a quantum mechanical magnetoresistance effect observed in a thin film structure including alternating ferromagnetic conductive layers and non-magnetic conductive layers. The TMR effect occurs in a magnetic tunnel junction (MJT), where the magnetic tunnel junction occurs at a thin insulator that separates two ferromagnets from each other. The AMR effect is a property of a material in which the dependence of the resistance on the angle between the current direction (e.g., the sensing axis) and the magnetization direction is observed. The magnetoresistance effect can be related to the sensitivity of the xMR sensor. For example, in order to increase the sensitivity of the xMR sensor, the magnetoresistance effect can be increased. Summary of the invention
[0003] In some embodiments, a magnetoresistive sensor includes a sensing element having a layer stack, the layer stack including: a reference layer having a fixed reference magnetization aligned with a magnetization axis; a magnetically free layer having a magnetically free magnetization, wherein the magnetically free magnetization is variable in the presence of an external magnetic field; and a nonmagnetic layer disposed between the reference layer and the magnetically free layer; and a stress inducing layer coupled to the layer stack, wherein the stress inducing layer is configured to apply a force to the layer stack to induce mechanical stress in the layer stack along a mechanical stress axis so that the magnetization axis is aligned parallel to the mechanical stress axis or perpendicular to the mechanical stress axis.
[0004] In some embodiments, a magnetoresistive sensor includes a first sensing element having a first layer stack, the first layer stack including: a first reference layer having a first fixed reference magnetization aligned with a first magnetization axis; a first magnetically free layer having a first magnetically free magnetization, wherein the first magnetically free magnetization is variable in the presence of an external magnetic field; and a first non-magnetic layer disposed between the first reference layer and the first magnetically free layer; the magnetoresistive sensor includes a second sensing element having a second layer stack, the second layer stack including: a second reference layer having a second fixed reference magnetization aligned with a second magnetization axis; a second magnetically free layer having a second magnetically free magnetization; The magnetoresistive sensor comprises a first layer stack and a second layer stack, wherein the second magnetic free magnetization is changeable in the presence of an external magnetic field; and a second non-magnetic layer arranged between the second reference layer and the second magnetic free layer; the magnetoresistive sensor comprises a stress inducing layer coupled to the first layer stack and the second layer stack, wherein the stress inducing layer is configured to apply a force to the first layer stack to induce a first mechanical stress in the first layer stack along a first mechanical stress axis, so that the first magnetization axis is aligned parallel to the first mechanical stress axis or perpendicular to the first mechanical stress axis, and to apply a force to the second layer stack to induce a second mechanical stress in the second layer stack along a second mechanical stress axis, so that the second magnetization axis is aligned parallel to the second mechanical stress axis or perpendicular to the second mechanical stress axis.
[0005] In some embodiments, a magnetoresistive sensor includes a sensing element having a layer stack stacked in a vertical dimension, the layer stack including: a reference layer having a fixed reference magnetization aligned with a magnetization axis; a magnetically free layer having a magnetically free magnetization, wherein the magnetically free magnetization is variable in the presence of an external magnetic field; and a nonmagnetic layer arranged between the reference layer and the magnetically free layer; and a conductive layer coupled to the top or bottom of the layer stack, wherein the conductive layer has a first outer periphery defining a lateral edge of the conductive layer, wherein the layer stack has a second outer periphery defining a lateral edge of the layer stack, wherein a minimum distance between the first outer periphery and the second outer periphery is greater than 1 micrometer (μm). BRIEF DESCRIPTION OF THE DRAWINGS
[0006] Embodiments are described herein with reference to the accompanying drawings.
[0007] Figure 1 An example of a layer stack of a magnetoresistive sensing element according to one or more embodiments is shown.
[0008] Figure 2 Graph illustrating the inverse magnetostrictive effect according to one or more embodiments.
[0009] Figure 3 A magnetoresistive sensor system according to one or more embodiments is shown.
[0010] Figure 4A A top view of a magnetoresistive sensor according to one or more embodiments is shown.
[0011] Figure 4B According to one or more embodiments, Figure 4A Top view of the magnetoresistive sensor.
[0012] Figure 4C is a graph showing the elongation of a sensing element and the width of a stress inducing layer according to one or more embodiments.
[0013] Figure 4D is a graph showing the elongation of a sensing element and the length of a stress inducing layer according to one or more embodiments.
[0014] Figure 5 A top view of a magnetoresistive sensor system is shown in accordance with one or more embodiments.
[0015] Figure 6 A magnetoresistive sensor system according to one or more embodiments is shown.
[0016] Figure 7 A magnetoresistive sensor system according to one or more embodiments is shown.
[0017] Figure 8 A magnetoresistive sensor system according to one or more embodiments is shown.
[0018] Fig. 9 A magnetoresistive sensor system according to one or more embodiments is shown. DETAILED DESCRIPTION
[0019] In the following, details are set forth to provide a more thorough explanation of the example implementation. However, it will be apparent to those skilled in the art that these embodiments may be practiced without these specific details. In other examples, well-known structures and devices are shown in block diagram form or in schematic form rather than in detail to avoid obscuring the embodiments. In addition, unless otherwise expressly stated, the features of the different embodiments described below may be combined with each other.
[0020] In addition, equivalent or similar elements or elements having equivalent or similar functions are indicated by equivalent or similar reference numerals in the following description. Since identical or functionally equivalent elements are given the same reference numerals in the drawings, repeated descriptions of elements having the same reference numerals may be omitted. Therefore, the descriptions provided for elements having the same or similar reference numerals are mutually interchangeable.
[0021] Each of the x-axis, y-axis, and z-axis is shown to be substantially perpendicular to the other two axes. In other words, the x-axis is substantially perpendicular to the y-axis and the z-axis, the y-axis is substantially perpendicular to the x-axis and the z-axis, and the z-axis is substantially perpendicular to the x-axis and the y-axis. In some cases, a single reference numeral is shown to refer to a surface, or less than all instances of a component may be labeled with all surfaces of the component. Although not every surface is labeled, all instances of a component may include an associated surface of the component.
[0022] The orientation of various elements in the figure is shown as an example, and the example shown can be rotated relative to the depicted orientation. The description provided herein and the subsequent claims relate to any structure with the described relationship between various features, regardless of whether the structure is in the specific orientation of the figure or rotated relative to such orientation. Similarly, spatial relative terms are used herein, such as "top", "bottom", "below", "under...", "lower", "above...", "upper", "middle", "left" and "right", so as to describe the relationship between an element as shown in the figure and one or more other elements. Spatial relative terms are intended to cover different orientations of elements, structures and / or components in use or operation in addition to the orientation depicted in the figure. Structures and / or components can be oriented in addition (rotated 90 degrees or in other orientations), and the spatial relative descriptors used in this article can be interpreted accordingly. In addition, the cross-sectional view in the figure only shows the features in the plane of the cross section, and unless otherwise indicated, the material behind the plane of the cross section is not shown, so as to simplify the drawings.
[0023] It should be understood that when an element is referred to as being "connected" or "coupled" to another element, it can be directly connected or coupled to the other element, or intervening elements may be present. Conversely, when an element is referred to as being "directly connected" or "directly coupled" to another element, there are no intervening elements. Other words used to describe the relationship between elements should be interpreted in a similar manner (e.g., "between" versus "directly between," "adjacent" versus "directly adjacent," etc.).
[0024] In the embodiments described herein or shown in the accompanying drawings, any direct electrical connection or coupling (e.g., any connection or coupling without additional intermediate elements) may also be achieved through an indirect connection or coupling (e.g., a connection or coupling with one or more additional intermediate elements), or vice versa, as long as the general purpose of the connection or coupling is basically maintained (e.g., for transmitting a certain signal or transmitting certain information). Features from different embodiments may be combined to form additional embodiments. For example, unless otherwise indicated, changes or modifications described with respect to one of the embodiments may also apply to other embodiments.
[0025] As used herein, the terms "substantially" and "approximately" mean "within reasonable tolerances of manufacturing and measurement." For example, the terms "substantially" and "approximately" may be used herein to illustrate small manufacturing tolerances or other factors (e.g., within 5%) that are considered acceptable in the industry without departing from aspects of the embodiments described herein. For example, a resistor having an approximate resistance value may actually have a resistance within 5% of the approximate resistance value. As another example, an approximate signal value may actually have a signal value within 5% of the approximate signal value.
[0026] In the present disclosure, expressions including ordinal numbers, such as "first", "second", etc., may modify various elements. However, such elements are not limited by the above expressions. For example, the above expressions do not limit the order and / or importance of the elements. The above expressions are only used for the purpose of distinguishing an element from other elements. For example, a first box and a second box indicate different boxes, although both are boxes. For another example, without departing from the scope of the present disclosure, a first element may be referred to as a second element, and similarly, a second element may also be referred to as a first element.
[0027] A "sensor" may refer to a component that converts a property to be measured into an electrical signal (e.g., a current signal or a voltage signal). The property to be measured may include, for example, a magnetic field, an electric field, an electromagnetic wave (e.g., a radio wave), a pressure, a force, a current, or a voltage, but is not limited to these. For example, it should be understood that there are various sensor technologies for measuring a current flowing through a conductor or the position of an object relative to a magnetic field (e.g., a linear position, a rotational position, or an angular position).
[0028] A TMR-based sensing element comprising a layer stack of ferromagnetic layers and non-magnetic layers may be exposed to mechanical stress during manufacturing or during integration of a sensor package. Mechanical stress may cause changes in the magnetic properties of the layer stack due to the inverse magnetostrictive effect. For example, mechanical stress may cause the reference magnetization of the layer stack to deviate from an expected orientation or direction. Therefore, changes in the magnetic properties of the layer stack may result in increased sensing errors (e.g., increased angular errors), may result in a worse reference layer system with a lower TMR effect and lower sensitivity, and / or may result in faster degradation of the sensing element that reduces the life of the sensing element.
[0029] Therefore, some embodiments disclosed herein relate to magnetoresistive sensors that use the inverse magnetostrictive effect to tune the sensor performance of a sensing element (e.g., a TMR sensing element) through layout and integration. For example, a stress-inducing layer can be coupled to a layer stack of a sensing element. The stress-inducing layer can be configured to apply a force to the layer stack to induce mechanical stress in the layer stack along a mechanical stress axis so that the magnetization axis of the reference layer system of the sensing element is aligned in a desired direction. For example, the magnetization axis of the reference layer system can be aligned parallel to the mechanical stress axis or perpendicular to the mechanical stress axis. Therefore, the orientation of the magnetization axis can be tuned to reduce sensing errors, enhance the reference layer system to increase the TMR effect and sensitivity, and increase the life of the sensing element. The increase in sensitivity produces a higher signal amplitude, which can be more easily processed.
[0030] For example, the magnetic material used in the TMR layer stack generally has a positive magnetostriction constant. In other words, the magnetic properties of the magnetic material are preferably aligned along the tensile stress axis. This effect can be used to stabilize the reference layer system. By coupling a stress-inducing layer (e.g., a stress-inducing liner or film) to the layer stack, a stabilizing effect can be achieved according to the metallization layout of the magnetoresistive sensor. The stabilizing effect can be used to keep the magnetization axis of the reference layer system in a desired orientation. In addition, in some embodiments, the TMR effect can be increased by 20%. In addition, due to a more stable reference layer system, less degradation is observed, which can result in less offset and increased life of the layer stack. In addition, by adapting the layout to the reference system magnetization, the increased amplitude of the angle sensor can be achieved for both the x magnetization sensing element and the y magnetization sensing element, which produces a lower angle error.
[0031] Figure 1 An example of a layer stack of a magnetoresistive sensing element 100 according to one or more embodiments is shown. For example, the magnetoresistive sensing element 100 may be a TMR sensing element having a bottom-pinned spin-valve (BSV) configuration. In addition, the magnetoresistive sensing element 100 may be arranged on a semiconductor substrate (not shown) of a magnetoresistive sensor. If described in a Cartesian coordinate system having a pair of perpendicular coordinate axes x, y, and z, the layers of the layer stack extend laterally in a plane spanned by the x-axis and the y-axis. Therefore, a lateral dimension (e.g., a lateral length, a lateral cross-sectional area, a lateral area, a lateral extension, a lateral displacement, etc.) may refer to a dimension in the xy plane and a vertical dimension may refer to a dimension in the z direction perpendicular to the xy plane. For example, the vertical extent of a layer in the z direction may be described as a layer thickness.
[0032] The layer stack of the magnetoresistive sensing element 100 includes at least a reference layer having a reference magnetization (e.g., a reference direction in the case of GMR technology or TMR technology). The reference magnetization is a magnetization direction that provides a sensing direction, which corresponds to the sensing axis of the magnetoresistive sensing element 100. The reference layer and therefore the reference magnetization define a sensor plane. For example, the sensor plane can be defined by an xy plane. Therefore, the x-direction and the y-direction can refer to "in-plane" relative to the sensor plane and the z-direction can refer to "out-of-plane" relative to the sensor plane.
[0033] Therefore, in the case of a GMR sensing element or a TMR sensing element, if the magnetic free magnetization of the magnetic free layer happens to point in the same direction as the reference magnetization (e.g., the reference direction), the resistance of the magnetoresistive sensing element 100 is at a minimum value, and if the magnetic free magnetization of the magnetic free layer happens to point in the opposite direction to the reference magnetization, the resistance of the magnetoresistive sensing element 100 is at a maximum value. The orientation of the magnetic free magnetization of the magnetic free layer is variable in the presence of an external magnetic field. Therefore, the resistance of the magnetoresistive sensing element 100 can change based on the influence of the external magnetic field on the magnetic free magnetization of the magnetic free layer.
[0034] From the bottom up, the magnetoresistive sensing element 100 may include an optional seed layer 102 that can be used to influence and / or optimize the growth of the stack. In some embodiments, the seed layer 102 can be copper, tantalum, ruthenium, or a mixture thereof. A natural antiferromagnetic (NAF) layer 104 is formed or otherwise disposed on the seed layer 102. The NAF layer 104 can be made of platinum manganese (PtMn), iridium manganese (IrMn), nickel manganese (NiMn), etc. The film thickness of the NAF can be in the range of 5nm to 50nm.
[0035] In addition, a pinned layer (PL) 106 may be formed or otherwise placed on the NAF layer 104. The pinned layer 106 may be made of a ferromagnetic material, such as cobalt iron (CoFe) or cobalt iron boron (CoFeB). The contact between the NAF layer 104 and the pinned layer 106 may cause an effect known as an exchange bias effect, so that the magnetization of the pinned layer 106 is aligned in a preferred direction (e.g., in the x-direction, as shown). The magnetization of the pinned layer 106 may be referred to as pinned magnetization. The pinned layer 106 may include a closed flux magnetization diagram in the xy plane. This closed flux magnetization diagram of the pinned layer 106 may be generated during the manufacture of the magnetoresistive sensing element 100 and may be permanently fixed. Alternatively, the pinned layer 106 may include a permanently fixed linear magnetization diagram in the xy plane (e.g., a uniform orientation in one direction).
[0036] The magnetoresistive sensing element 100 also includes a nonmagnetic layer (NML) referred to as a coupling intermediate layer 108. For example, the coupling intermediate layer 108 may be diamagnetic and may include ruthenium, iridium, copper, a copper alloy, or the like. A magnetic (e.g., ferromagnetic) reference layer (RL) 110 may be formed or otherwise disposed on the coupling intermediate layer 108. The thickness of the pinned layer 106 and the thickness of the magnetic reference layer 110 may be in the range of 1 nm to 10 nm, respectively.
[0037] Thus, the coupling interlayer 108 may be disposed between the pinned layer 106 and the magnetic reference layer 110 to spatially separate the pinned layer 106 and the magnetic reference layer 110 in the vertical direction. In addition, the coupling interlayer 108 may provide an interlayer exchange coupling (e.g., an antiferromagnetic Ruderman–Kittel–Kasuya–Yosida (RKKY) coupling) between the pinned layer 106 and the magnetic reference layer 110 to form an artificial antiferromagnet. Thus, the magnetization of the magnetic reference layer 110 may be aligned and maintained in a direction antiparallel to or opposite to the magnetization of the pinned layer 106 (e.g., in the x-direction, as shown). The magnetization of the magnetic reference layer 110 may be referred to as a reference magnetization.
[0038] Since the NAF layer 104 is configured so that the magnetization of the pinned layer 106 is aligned and fixed in a certain direction, and the coupling intermediate layer 108 is configured so that the magnetization of the magnetic reference layer 110 is aligned and fixed in the opposite direction, it can be said that the NAF layer 104 is configured to maintain the magnetization of the pinned layer 106 in a first magnetic orientation (e.g., fixed pinned magnetization) and maintain the magnetization of the magnetic reference layer 110 in a second magnetic orientation (e.g., fixed reference magnetization). For example, if the pinned layer 106 includes a clockwise closed flux magnetization pattern in the xy plane, the magnetic reference layer 110 can include a counterclockwise closed flux magnetization pattern in the xy plane (or vice versa). In this way, the magnetic reference layer 110 can have a permanent closed flux magnetization pattern. In addition, when the pinned layer 106 includes a linear magnetization pattern in a certain direction in the xy plane, the magnetic reference layer 110 can include a linear magnetization pattern in an antiparallel direction. Therefore, the NAF layer 104 , the pinned layer 106 , the coupling interlayer 108 , and the magnetic reference layer 110 form a magnetic reference layer system 112 of the magnetoresistive sensing element 100 .
[0039] The magnetoresistive sensing element 100 further includes a barrier layer 114 (e.g., a tunnel barrier layer) that is vertically arranged between the reference layer system 112 and the magnetically free (FL) layer 116. For example, the barrier layer 114 can be formed or otherwise placed on the magnetic reference (RL) layer 110 of the reference layer system 112, and the magnetically free layer 116 can be formed or otherwise placed on the barrier layer 114.
[0040] The barrier layer 114 may be made of a non-magnetic material. In some embodiments, the barrier layer 114 may be an electrically insulating tunnel barrier. For example, the barrier layer 114 may be a tunnel barrier for generating a TMR effect. The barrier layer 114 may include magnesium oxide (MgO) or other materials having similar properties.
[0041] The material of the magnetic free layer 116 can be an alloy of ferromagnetic materials, such as CoFe, CoFeB, or NiFe. The magnetic free layer 116 has a magnetic free magnetization, which is variable in the presence of an external magnetic field. Therefore, the magnetic free layer 116 can be called a sensor layer because the change in the magnetic free magnetization is used to determine the measured variable. In addition, the magnetic free magnetization has a default magnetic orientation at the ground state. The ground state is a state in which the influence of the external magnetic field on the magnetic free layer 116 does not exist or is negligibly small. In some embodiments, the magnetoresistive sensing element 100 may include a magnetic free system, which includes multiple layers (e.g., two or more magnetic free layers), which are used in combination as magnetic free layers. In this case, the magnetic free layers of the magnetic free system are magnetically coupled to each other. Therefore, the magnetic free system can be used as a magnetic free layer, but can include multiple layers. The magnetic free system has a magnetic free magnetization, wherein the magnetic free magnetization is variable in the presence of an external magnetic field.
[0042] A cap layer 118 made of, for example, tantalum (Ta), tantalum nitride (TaN), ruthenium (Ru), titanium (Ti), titanium nitride (TiN), platinum (Pt), etc. may be formed or otherwise placed on the magnetic free layer 116 to form an upper layer of the magnetoresistive sensing element 100 .
[0043] The seed layer 102 may serve as a bottom electrode or may provide electrical contact with a bottom electrode of the magnetoresistive sensing element 100. The cap layer 118 may provide electrical contact with a top electrode (not shown) of the magnetoresistive sensing element 100. The barrier layer 114 may be designed to allow electrons to tunnel between the reference layer system 112 and the magnetically free layer 116 when a bias voltage is applied to an electrode of the magnetoresistive sensing element 100 (not shown) to provide a magnetoresistive effect (e.g., a TMR effect).
[0044] As indicated above, Figure 1 Provided as an example only. Other examples may be found in Figure 1 The examples described are different. Figure 1 The numbers and arrangements of the components shown in FIG. 1 are provided as examples. In practice, the magnetoresistive sensing element 100 may include additional elements, fewer elements, different elements, or different components. Figure 1 Elements arranged differently as shown in FIG.
[0045] Figure 2A diagram 200 is shown of an inverse magnetostrictive effect according to one or more embodiments. For example, the diagram 200 shows an inverse magnetostrictive effect for a pinned layer 106. A force may be applied to the pinned layer 106, which induces a mechanical stress in the pinned layer 106 along a mechanical stress axis 202, which may be a compressive force or a decompressive force, which causes the pinned layer 106 to deform in a dimension parallel to the mechanical stress axis 202. For a positive magnetostriction constant, the magnetization tends to align with the tensile stress. In this example, the induced mechanical stress causes the magnetization axis 204 of the pinned layer 106 to shift to align parallel to the mechanical stress axis 202. Thus, the pinned magnetization of the pinned layer 106 aligned with the magnetization axis 204 is aligned parallel to the mechanical stress axis 202. Thus, by controlling the manner in which the force is applied to the pinned layer 106 and the direction of the induced mechanical stress, the orientation of the magnetization axis 204 can be controlled to align in a desired direction without orientation error.
[0046] In addition, since the reference magnetization of the magnetic reference layer 110 is anti-parallel coupled to the pinned magnetization through the coupling intermediate layer 108, the orientation of the reference magnetization is also aligned with the mechanical stress axis 202. In other words, the reference magnetization is aligned parallel or anti-parallel to the mechanical stress axis 202. In addition, since the force is applied to the entire layer stack of the sensing element, mechanical stress can be induced in each layer of the layer stack. Therefore, as a result of the mechanical stress induced within the magnetic reference layer 110, the reference magnetization of the magnetic reference layer 110 can also be aligned with the mechanical stress axis 202.
[0047] In some embodiments, the magnetization axis 204 can be oriented in different directions with respect to the mechanical stress axis 202. For example, the magnetization axis 204 can be oriented perpendicular to the mechanical stress axis 202. The orientation of the magnetization axis 204 with respect to the mechanical stress axis 202 can depend on the material (e.g., magnetostriction constant) of the magnetic reference layer 110. The mechanical stress axis 202 can be controlled based on the magnetostriction constant to control the orientation of the magnetization axis 204.
[0048] As indicated above, Figure 2 Provided as an example only. Other examples may be found in Figure 2 The examples described are different.
[0049] Figure 3 1 shows a magnetoresistive sensor system 300 according to one or more embodiments. The magnetoresistive sensor system 300 includes a first magnetoresistive sensing element 302 (e.g., a first TMR magnetoresistive sensing element) and a second magnetoresistive sensing element 304 (e.g., a second TMR magnetoresistive sensing element). The first magnetoresistive sensing element 302 and the second magnetoresistive sensing element 304 may be associated with a Figure 1The described magnetoresistive sensing element 100 is similar. Thus, the first magnetoresistive sensing element 302 and the second magnetoresistive sensing element 304 each have a corresponding layer stack.
[0050] The magnetoresistive sensor system 300 also includes a bottom conductor 306 (e.g., a bottom metal layer), a top conductor 308 (e.g., a top metal layer), and a bottom electrode 310, the top conductor 308 serving as a top electrode for the first magnetoresistive sensing element 302 and the second magnetoresistive sensing element 304, and the bottom electrode 310 serving as a bottom electrode for the first magnetoresistive sensing element 302 and the second magnetoresistive sensing element 304. The bottom electrode 310 may be a seed layer (e.g., the seed layer 102) that provides a conductive path between the first magnetoresistive sensing element 302 and the second magnetoresistive sensing element 304. Thus, the bottom electrode 310 may be part of a layer stack of the first magnetoresistive sensing element 302 and the second magnetoresistive sensing element 304. The bottom conductor 306 includes a first power supply contact 306-1 and a second power supply contact 306-2. A bias voltage may be supplied to the first power supply contact 306-1 and the second power supply contact 306-2 to generate a current I. Current I flows through the first portion 308 - 1 of the top conductor 308 , through the first magnetoresistive sensing element 302 to the bottom electrode 310 , through the bottom electrode 310 to the second magnetoresistive sensing element 304 , through the second magnetoresistive sensing element 304 , through the second portion 308 - 2 of the top conductor 308 , to the second power contact 306 - 2 .
[0051] In addition, the magnetoresistive sensor system 300 may include a stress inducing layer 312 coupled to the layer stack of the first magnetoresistive sensing element 302 and the second magnetoresistive sensing element 304. The stress inducing layer 312 may be a conductive layer or a non-conductive layer. For example, the stress inducing layer 312 may include titanium nitride (TiN), tantalum nitride (TaN), tungsten (W), titanium tungsten (TiW), or silicon nitride (SiN), but is not limited to these. In some embodiments, the stress inducing layer 312 may be arranged between the top conductor 308 and the first magnetoresistive sensing element 302. Alternatively, or in addition, the stress inducing layer 312 may be arranged between the top conductor 308 and the second magnetoresistive sensing element 304. In some embodiments, the stress inducing layer 312 may be arranged between the bottom conductor 306 and the bottom electrode 310. In some embodiments, the top conductor 308 may be a stress inducing layer. In some embodiments, two stress inducing layers may be provided such that one stress inducing layer is coupled to the top of the layer stack and the other stress inducing layer is coupled to the bottom of the layer stack. Thus, the two stress inducing layers may be configured to induce a corresponding mechanical stress in each layer stack along a mechanical stress axis such that a magnetization axis of each layer stack is aligned parallel to the mechanical stress axis or perpendicular to the mechanical stress axis.
[0052] The stress inducing layer 312 may be configured to apply a first force to the layer stack of the first magnetoresistive sensing element 302 to induce mechanical stress in the layer stack along a first mechanical stress axis, so that the magnetization axis of the first magnetoresistive sensing element 302 is aligned parallel to the first mechanical stress axis or perpendicular to the first mechanical stress axis, depending on, for example, the magnetostriction constant of the first magnetoresistive sensing element 302. Therefore, the pinned magnetization and the reference magnetization of the first magnetoresistive sensing element 302 may be oriented in a predetermined direction about the first mechanical stress axis based on the induced mechanical stress. In addition, the stress inducing layer 312 may be configured to apply a second force to the layer stack of the second magnetoresistive sensing element 304 to induce mechanical stress in the layer stack along a second mechanical stress axis, so that the magnetization axis of the second magnetoresistive sensing element 304 is aligned parallel to the second mechanical stress axis or perpendicular to the second mechanical stress axis, depending on, for example, the magnetostriction constant of the second magnetoresistive sensing element 304. Therefore, the pinned magnetization and the reference magnetization of the second magnetoresistive sensing element 304 can be oriented in a predetermined direction about the second mechanical stress axis based on the induced mechanical stress. In some embodiments, the first mechanical stress axis is parallel to the second mechanical stress axis.
[0053] The first force and the second force may be generated by the film growth conditions of the stress inducing layer 312 and the size of the stress inducing layer 312. In some embodiments, the stress inducing layer 312 may be configured to apply the first force and the second force to the layer stack to induce elongation and compression of the layer stack parallel to the mechanical stress axis or perpendicular to the mechanical stress axis. In some embodiments, the first force and the second force are compressive forces that induce tensile stress in the layer stack parallel to the mechanical stress axis or perpendicular to the mechanical stress axis. For example, the first force may be a first compressive force that induces a first tensile stress in the reference layer of the first magnetoresistive sensing element 302 parallel to the first mechanical stress axis and aligns the magnetization axis of the first magnetoresistive sensing element 302 parallel to the first mechanical stress axis or perpendicular to the first mechanical stress axis. The second force may be a second compressive force that induces a second tensile stress in the reference layer of the second magnetoresistive sensing element 304 parallel to the second mechanical stress axis and aligns the magnetization axis of the second magnetoresistive sensing element 304 parallel to the second mechanical stress axis or perpendicular to the second mechanical stress axis.
[0054] In some embodiments, the stress-inducing layer 312 is a compression layer that extends the layer pair in a dimension parallel to the mechanical stress axis. In some embodiments, wherein the stress-inducing layer 312 is configured to deform, induce mechanical stress in the layer stack and cause deformation of the layer stack parallel to the mechanical stress axis. For example, the stress-inducing layer 312 can be configured to bend or bend upward, so that the first force and the second force are decompression forces applied to the first magnetoresistive sensing element 302 and the second magnetoresistive sensing element 304, which induce mechanical stress in the layer stack along the mechanical stress axis. Alternatively, the stress-inducing layer 312 can be configured to bend or bend downward, so that the first force and the second force are compression forces applied to the first magnetoresistive sensing element 302 and the second magnetoresistive sensing element 304, which induce mechanical stress in the layer stack along the mechanical stress axis. Therefore, the stress-inducing layer 312 can be configured to bend in a dimension parallel to the mechanical stress axis, so that the first force and the second force are applied to the layer stack as a compression force and a decompression force, respectively. Thus, the mechanical stress axis can be predefined based on the designed deformation of the stress inducing layer 312 to control the orientation of the magnetization axis. In other words, rather than preventing mechanical stress from affecting the layer stack, the stress inducing layer 312 is designed to purposefully induce mechanical stress in a controllable and definable manner to control the orientation of the magnetization axis of the layer stack. Thus, the orientation of the magnetization axis can be tuned to reduce sensing errors, enhance the reference layer system to increase the TMR effect and sensitivity, and increase the lifetime of the sensing element. The increase in sensitivity produces a higher signal amplitude, which can be more easily processed.
[0055] As indicated above, Figure 3 Provided as an example only. Other examples may be found in Figure 3 The examples described are different. Figure 3 The numbers and arrangements of the components shown in FIG. 3 are provided as examples. In practice, magnetoresistive sensor system 300 may include additional elements, fewer elements, different elements, or different components. Figure 3 Elements arranged differently as shown in FIG.
[0056] FIG. 4 illustrates a top view of a magnetoresistive sensor 400 according to one or more implementations. Figure 4B FIG. 4 shows a cross-sectional view of a magnetoresistive sensor 400 according to one or more embodiments. The magnetoresistive sensor 400 may be a Figure 3 As described above, the magnetoresistive sensor system 300 is a portion of the magnetoresistive sensor system 300. Thus, the magnetoresistive sensor 400 may include a first magnetoresistive sensing element 302, a top conductor 308, a bottom electrode 310, and a stress inducing layer 312. In addition, a via 314 may be provided between the stress inducing layer 312 and the first magnetoresistive sensing element 302 to provide an electrical path for the current I.
[0057] The first magnetoresistive sensing element 302 includes a sensor plane (e.g., an XY plane) defined by a first axis (e.g., an x-axis) and a second axis (e.g., a y-axis). The layers of the layer stack are stacked along a third axis (e.g., a z-axis) perpendicular to the sensor plane. In this example, the mechanical stress axis is collinear with the first axis. In other words, the mechanical stress axis is aligned with the first axis (e.g., the x-axis). Additionally, the stress-inducing layer 312 has a size in the XY plane that is substantially similar to the size of the top conductor 308 in the XY plane. For example, the stress-inducing layer 312 has a first dimension D1 and a second dimension D2, the first dimension D1 defining the width of the stress-inducing layer 312 along the first axis and the second dimension D2 defining the length of the stress-inducing layer 312 along the second axis. Therefore, the first dimension D1 is smaller than the second dimension D2. The deformation of the stress-inducing layer 312 can be configured to occur along a smaller dimension (e.g., the first dimension) of the stress-inducing layer 312. Therefore, the mechanical stress axis of the induced mechanical stress can be aligned with the first axis (e.g., the x-axis).
[0058] Thus, the first dimension D1 (e.g., a width dimension) is defined by the distance between the first lateral edge 402 and the second lateral edge 404 of the stress inducing layer 312, and the second dimension D2 (e.g., a length dimension) is defined by the distance between the third lateral edge 406 and the fourth lateral edge 408 of the stress inducing layer 312. The first magnetoresistive sensing element 302 is disposed between the first lateral edge 402 and the second lateral edge 404, and the first magnetoresistive sensing element 302 is disposed between the third lateral edge 406 and the fourth lateral edge 408.
[0059] The amount of force applied to the first magnetoresistive sensing element 302 by the stress-inducing layer 312 decreases from the edge (e.g., exponentially). For example, the applied force that induces mechanical stress along the x-axis decreases with the distance between the first lateral edge 402 and the second lateral edge 404. Therefore, the first dimension D1 should be small enough to increase or maximize the mechanical stress induced along the x-axis. For example, the first dimension D1 should be small enough so that the first magnetoresistive sensing element 302 can be placed close to both the first lateral edge 402 and the second lateral edge 404 to increase the stress induced along the x-axis. In addition, the applied force that induces mechanical stress along the y-axis decreases with the distance between the third lateral edge 406 and the fourth lateral edge 408. Therefore, the second dimension D2 should be large enough to reduce or minimize the mechanical stress induced along the y-axis. For example, the second dimension D2 should be large enough so that the first magnetoresistive sensing element 302 can be placed far enough from both the third lateral edge 406 and the fourth lateral edge 408 to minimize the stress induced along the y-axis.
[0060] In some embodiments, the stress-inducing layer 312 is configured to induce elongation or compression of the layer stack in the dimension of the layer stack corresponding to the first axis. For example, the stress-inducing layer 312 can be under compressive stress, so that the layers of the layer stack can expand or elongate in both the positive x-axis direction and the negative x-axis direction. In other words, the width of the layer stack can increase due to the expansion force applied to the layer stack. Additionally, in some embodiments, the first magnetoresistive sensing element 302 is arranged far enough away from the third lateral edge 406 and the fourth lateral edge 408 so that the stress-inducing layer 312 does not substantially induce elongation or compression of the layer stack in the dimension corresponding to the second axis (e.g., the y-axis). Therefore, since the magnetic properties of the layer stack are preferably aligned along the tensile stress axis, the position of the first magnetoresistive sensing element 302 with respect to the first lateral edge 402, the second lateral edge 404, the third lateral edge 406, and the fourth lateral edge 408, combined with the dimensions of the first dimension D1 and the second dimension D2, can ensure that the mechanical stress axis (e.g., the tensile stress axis) is aligned in a desired direction so that the magnetization axis is aligned with that desired direction.
[0061] As indicated above, Figure 4A and Figure 4B Provided as an example only. Other examples may be found in Figure 4A and Figure 4B The examples described are different.
[0062] Figure 4C 400C is a graph showing the elongation of a sensing element and the width of a stress inducing layer according to one or more embodiments. Figure 4A and Figure 4B Described magnetoresistive sensor 400. Graph 400C plots the elongation of the sensing element in both the x-direction and the y-direction, where the width of the stress inducing layer along the x-axis (e.g., first dimension D1) varies and the length of the stress inducing layer along the y-axis (e.g., second dimension D2) is fixed (e.g., at 5.25 μm). The x-direction may be a desired direction for the magnetization axis.
[0063] The elongation of the sensing element is measured in nanometers (nm) and the width of the stress-inducing layer is measured in micrometers (μm) in the x-direction. Figure 400C is for a sensing element with a diameter of 1 μm, because the layer stack of the sensing element is usually disc-shaped or cylindrical. A higher number of induced mechanical stresses produces a larger number of elongations of the sensing element, resulting in a stronger influence on the orientation of the magnetization axis in the desired direction. Therefore, the induced mechanical stress or elongation should be maximized in the x-direction and minimized in the y-direction. In other words, the aspect ratio of the elongation in the x-direction to the elongation in the y-direction should be maximized to produce the maximum anisotropy of magnetization. Anisotropy increases with aspect ratio. Aspect ratio can be defined as the amount of change in the layer stack along the x-axis relative to the amount of change in the layer stack along the y-axis.
[0064] According to graph 400C , for a width of the stress inducing layer of about 1.5 μm, maximum anisotropy is achieved, where the aspect ratio of the elongation in the x-direction to the elongation in the y-direction is maximized and is greater than 4.
[0065] Thus, the stress-inducing layer is configured to induce the layer stack to stretch by a first percentage in a dimension corresponding to the x-axis (e.g., the x-direction) and to induce the layer stack to stretch by a second percentage in a dimension corresponding to the y-axis (e.g., the y-direction). The first percentage is at least twice the second percentage to increase the anisotropy of the magnetization of the reference layer and the pinned layer. In some embodiments, the first percentage is at least four times the second percentage. In some embodiments, the first percentage is at least ten times the second percentage.
[0066] In some embodiments, the sensing element has a diameter in the range of 0.5-1.5 μm and the mechanical stress axis is collinear with the x-axis. The stress inducing layer can have a first dimension D1 corresponding to the x-axis and a second dimension D2 corresponding to the y-axis. The second dimension D2 can be at least twice as large as the first dimension D1, wherein the first dimension is in the range of 1.0-3.0 μm to produce an aspect ratio large enough to orient the magnetization axis in the x-direction.
[0067] In some embodiments, the stress-inducing layer has a width dimension defined by the first lateral edge 402 and the second lateral edge 404 within a range of 1-3 μm, and has a length dimension defined by the third lateral edge 406 and the fourth lateral edge 408. The layer stack is arranged between the first lateral edge 402 and the second lateral edge 404 in the x-direction and the layer stack is arranged between the third lateral edge 406 and the fourth lateral edge 408 in the y-direction. The layer stack has an outer perimeter that can have a first distance of no more than 2 μm from the first lateral edge 402 and the second lateral edge 404, respectively. In other words, the layer stack of the first magnetoresistive sensing element 302, for example, can be no more than 2 μm away from the first lateral edge 402 and the second lateral edge 404. Therefore, the closest point of the layer stack to the first lateral edge 402 is no more than 2 μm, and the closest point of the layer stack to the second lateral edge 404 is no more than 2 μm. The sensing element may have a diameter in the range of 0.5-1.5 μm so that the case suffices for the stress inducing layer to have a width dimension in the range of 1-3 μm.
[0068] In addition, the outer perimeter of the layer stack has a second distance greater than 2 μm from the third lateral edge 406 and the fourth lateral edge 408. In other words, the layer stack of the first magnetoresistive sensing element 302 is, for example, at least 2 μm from the third lateral edge 406 and at least 2 μm from the fourth lateral edge 408. Therefore, the closest point of the layer stack to the third lateral edge 406 is greater than 2 μm, and the closest point of the layer stack to the fourth lateral edge 408 is greater than 2 μm.
[0069] Furthermore, the minimum distance of the second distance is at least twice as large as the maximum distance of the first distance.
[0070] As a result of this configuration, a sufficiently large aspect ratio can be produced to orient the magnetization axis along the x-axis.
[0071] As indicated above, Figure 4C Provided as an example only. Other examples may be found in Figure 4C The examples described are different.
[0072] Figure 4D is a graph 400D showing the elongation of the sensing element and the length (y) of the stress inducing layer according to one or more embodiments. Graph 400D may correspond to a graph with respect to Figure 4A and Figure 4BDescribed magnetoresistive sensor 400. Graph 400D plots the elongation of the sensing element in both the x-direction and the y-direction, where the length of the stress inducing layer along the y-axis (e.g., the second dimension D2) varies and the length of the stress inducing layer along the x-axis (e.g., the first dimension D1) is fixed (e.g., at 1.5 μm). The x-direction may be a desired direction for the magnetization axis.
[0073] The elongation of the sensing element is measured in nanometers (nm) and the length of the stress-inducing layer is measured in micrometers (μm) in the y direction. Figure 400D is for a sensing element with a diameter of 1 μm. A higher number of induced mechanical stresses produces a greater number of elongations of the sensing element, resulting in a stronger effect on the orientation of the magnetization axis in the desired direction. Therefore, the induced mechanical stress or elongation should be maximized in the x direction and minimized in the y direction. In other words, the aspect ratio of the elongation in the x direction to the elongation in the y direction should be maximized to produce the maximum anisotropy of magnetization. Anisotropy increases with aspect ratio. The aspect ratio can be defined as the amount of change in the layer stack along the x axis relative to the amount of change in the layer stack along the y axis. Figure 400D shows that the aspect ratio increases with the increase in the length of the stress-inducing layer. Therefore, the length of the stress-inducing layer should be long enough so that the aspect ratio is at least greater than two, or at least greater than four. The anisotropy of the magnetic reference layer and the pinning layer increases with the aspect ratio.
[0074] In some embodiments, the sensing element has a diameter in the range of 0.5-1.5 μm and the mechanical stress axis is collinear with the x-axis. The stress inducing layer can have a first dimension D1 corresponding to the x-axis and a second dimension D2 corresponding to the y-axis. The second dimension D2 can be at least twice as large as the first dimension D1, wherein the first dimension is in the range of 1.0-3.0 μm to produce an aspect ratio large enough to orient the magnetization axis in the x-direction.
[0075] In some embodiments, the stress-inducing layer has a width dimension defined by the first lateral edge 402 and the second lateral edge 404 within a range of 1-3 μm and has a length dimension defined by the third lateral edge 406 and the fourth lateral edge 408. The layer stack is arranged between the first lateral edge 402 and the second lateral edge 404 in the x-direction and the layer stack is arranged between the third lateral edge 406 and the fourth lateral edge 408 in the y-direction. The layer stack has an outer perimeter that can have a first distance of no more than 2 μm from the first lateral edge 402 and the second lateral edge 404, respectively. In other words, the layer stack of the first magnetoresistive sensing element 302, for example, can be no more than 2 μm away from the first lateral edge 402 and the second lateral edge 404. Therefore, the closest point of the layer stack to the first lateral edge 402 is no more than 2 μm, and the closest point of the layer stack to the second lateral edge 404 is no more than 2 μm. The sensing element may have a diameter in the range of 0.5-1.5 μm so that the case suffices for the stress inducing layer to have a width dimension in the range of 1-3 μm.
[0076] In addition, the outer perimeter of the layer stack has a second distance greater than 2 μm from the third lateral edge 406 and the fourth lateral edge 408. In other words, the layer stack of the first magnetoresistive sensing element 302 is, for example, at least 2 μm from the third lateral edge 406 and at least 2 μm from the fourth lateral edge 408. Therefore, the closest point of the layer stack to the third lateral edge 406 is greater than 2 μm, and the closest point of the layer stack to the fourth lateral edge 408 is greater than 2 μm.
[0077] Furthermore, the minimum distance of the second distance is at least twice as large as the maximum distance of the first distance.
[0078] As a result of this configuration, a sufficiently large aspect ratio can be produced to orient the magnetization axis along the x-axis.
[0079] As indicated above, Figure 4D Provided as an example only. Other examples may be found in Figure 4D The examples described are different.
[0080] Figure 5 1 shows a top view of a magnetoresistive sensor system 500 according to one or more embodiments. The magnetoresistive sensor system 500 includes a plurality of sensing elements 502 arranged between respective top conductors 504 (e.g., top metal layers) and respective bottom conductors 506 (e.g., bottom electrodes). The stress-inducing layer may also be formed with respect to Figure 3A plurality of sensing elements 502 may be coupled to the top conductor 504 in a similar manner as described above (e.g., between the sensing element 502 and the corresponding top conductor 504), such that the stress inducing layer and the top conductor 504 have similar lateral dimensions. Alternatively, the top conductor 504 may be a stress inducing layer. The stress inducing layer may have a shape that satisfies the requirements of Figure 4A-4D The above aspect ratio configures the lateral dimensions. Therefore, the mechanical stress in each layer stack of the plurality of sensing elements 502 can be induced along a mechanical stress axis oriented along the x-axis, and the pinned magnetization and the reference magnetization of each sensing element 502 can be aligned parallel to the mechanical stress axis or perpendicular to the mechanical stress axis, depending on the magnetostriction constant of each sensing element 502.
[0081] Thus, each stress-inducing layer can be a straight structure having a first dimension D1 extending in the x-direction and a second dimension D2 extending in the y-direction perpendicular to the x-direction. The first dimension D1 can be smaller than the second dimension D2, and the first dimension D1 subjected to bending stress generates a force applied to each layer stack of the sensing element 502. The sensing elements 502 coupled to the same stress-inducing layer are spaced apart in the y-direction. In addition, the x-direction is parallel to the mechanical stress axis of the sensing element 502.
[0082] As indicated above, Figure 5 Provided as an example only. Other examples may be found in Figure 5 The examples described are different.
[0083] Figure 6 A magnetoresistive sensor system 600 is shown according to one or more embodiments. The magnetoresistive sensor system 600 includes a first sensing element 602 and a second sensing element 604 disposed between a top conductor 606 (e.g., a top metal layer) and a corresponding bottom conductor 608 (e.g., a bottom electrode). The magnetoresistive sensor system 600 may also include a stress inducing layer 610. Additionally, or alternatively, the top conductor 606 may be a stress inducing layer. A first via 612 may couple the first sensing element 602 to the top conductor 606, and a second via 614 may couple the second sensing element 604 to the top conductor 606.
[0084] The lateral dimensions of the stress inducing layer 610 are configured such that the stress inducing layer 610 bends in the y-direction, induces a first mechanical stress in the first sensing element 602 in the y-direction and induces a second mechanical stress in the second sensing element 604 in the y-direction. For example, the stress inducing layer 610 may have a lateral dimension that satisfies the above requirements except that the width dimension of the stress inducing layer 610 extends in the y-direction and the length dimension of the stress inducing layer 610 extends in the x-direction. Figure 4A-4DThe lateral dimensions of the similarly described aspect ratio configurations. Thus, the pinned magnetizations and the reference magnetizations of the first sense element 602 and the second sense element 604 may be aligned along the y-axis.
[0085] As indicated above, Figure 6 Provided as an example only. Other examples may be found in Figure 6 The examples described are different.
[0086] Figure 7 1 shows a magnetoresistive sensor system 700 according to one or more embodiments. The magnetoresistive sensor system 700 includes a plurality of sensing elements 702 arranged between respective top conductors 704 (e.g., top metal layers) and respective bottom conductors 706 (e.g., bottom electrodes). The stress-inducing layer 708 may also be formed with respect to Figure 3 The stress-inducing layer 708 and the top conductor 704 may be coupled to the plurality of sensing elements 702 in a similar manner as described above (e.g., between the sensing elements 702 and the corresponding top conductors 704), such that the stress-inducing layer 708 and the top conductor 704 have similar lateral dimensions. Alternatively, the top conductor 704 may be a stress-inducing layer. The stress-inducing layer 708 may have a shape that satisfies the above-described Figure 4A-4D Describes the lateral dimensions of the aspect ratio configuration.
[0087] The lateral dimensions of the stress inducing layers 708 are configured such that each stress inducing layer 708 is bent in the x-direction, inducing a corresponding mechanical stress in the x-direction on each stress inducing layer 708. Therefore, mechanical stress in each layer stack of the plurality of sensing elements 702 can be induced along a mechanical stress axis oriented along the x-axis, and the pinned magnetization and the reference magnetization of each sensing element 702 can be aligned along the mechanical stress axis (e.g., along the x-axis).
[0088] Thus, each stress-inducing layer 708 can be a straight structure having a first dimension extending in the x-direction and a second dimension extending in the y-direction perpendicular to the x-direction. The first dimension can be smaller than the second dimension, and the first dimension subjected to bending stress can generate a force applied to each layer stack of the sensing element 702. The sensing elements 702 coupled to the same stress-inducing layer are spaced apart in the y-direction. In addition, the x-direction is parallel to the mechanical stress axis of the sensing element 702.
[0089] As indicated above, Figure 7 Provided as an example only. Other examples may be found in Figure 7 The examples described are different.
[0090] Figure 8A magnetoresistive sensor system 800 is shown in accordance with one or more implementations. The magnetoresistive sensor system 800 includes a first sensing element 802 and a second sensing element 804 disposed between a top conductor 806 (e.g., a top metal layer) and a corresponding bottom conductor 808 (e.g., a bottom electrode). The top conductor 806 may have a U-shape to align the pinned magnetization and the reference magnetization of the first sensing element 802 and the second sensing element 804 along the x-axis. The magnetoresistive sensor system 800 may also include a stress inducing layer 810 having a U-shape similar to the U-shape of the top conductor 806. Additionally, or alternatively, the top conductor 806 may be a stress inducing layer.
[0091] The lateral dimensions of the stress inducing layer 810 are configured so that a first portion 812 of the stress inducing layer 810 coupled to the first sensing element 802 is bent in the x-direction to induce a first mechanical stress in the first sensing element 802 in the x-direction. For example, the first portion 812 of the stress inducing layer 810 may have a shape that satisfies the above-mentioned Figure 4A-4D In addition, the lateral dimensions of the stress inducing layer 810 are configured so that the second portion 814 of the stress inducing layer 810 coupled to the second sensing element 804 is bent in the x-direction, inducing a second mechanical stress in the second sensing element 804 in the x-direction. For example, the second portion 814 of the stress inducing layer 810 may have a lateral dimension that satisfies the above aspect ratio. Figure 4A-4D The lateral dimensions of the similarly described aspect ratio configurations. Thus, the pinned magnetizations and the reference magnetizations of the first sense element 802 and the second sense element 804 may be aligned along the x-axis.
[0092] As indicated above, Figure 8 Provided as an example only. Other examples may be found in Figure 8 The examples described are different.
[0093] Fig. 9A magnetoresistive sensor system 900 is shown according to one or more embodiments. The magnetoresistive sensor system 900 includes a plurality of sensing elements 902 (e.g., sensing elements 902-1, 902-2, 902-3, and 902-4) arranged between a top conductor 904 (e.g., a top metal layer) and a corresponding bottom conductor 906 (e.g., a bottom electrode). Thus, the top conductor 904 is a conductive layer coupled to the top of the layer stack. The top conductor 904 has a first outer perimeter 908 defining a lateral edge of the top conductor 904. In addition, the layer stack of each sensing element 902 has a second outer perimeter 910 defining a lateral edge of the layer stack. Each of the sensing elements 902-1, 902-2, 902-3, and 902-4 has at least a minimum distance Dmin between the first outer perimeter 908 and the second outer perimeter 910 that is greater than 1 μm. In other words, each of the sensing elements 902-1, 902-2, 902-3, and 902-4 is located at least 1 μm from the first outer perimeter 908. Since the amount of force applied by the top conductor 904 to any sensing element 902 decreases (e.g., exponentially) as the distance from the first outer perimeter 908 increases, the amount of force applied to the sensing element 902 can be minimized by positioning the sensing element 902 away from the first outer perimeter 908. Therefore, the preferred magnetization anisotropy of the pinned magnetization and the reference magnetization of the sensing element 902 is substantially unaffected by the top conductor 904. In other words, rather than inducing mechanical stress in each sensing element 902, the top conductor 904 can be large enough and the sensing element 902 can be positioned sufficiently far from the first outer perimeter 908 to reduce or prevent the mechanical stress from affecting the orientation of the sensing element 902.
[0094] As indicated above, Fig. 9 Provided as an example only. Other examples may be found in Fig. 9 The examples described are different.
[0095] The following provides an overview of some aspects of the disclosure:
[0096] Aspect 1: A magnetoresistive sensor, comprising: a sensing element having a layer stack, the layer stack comprising: a reference layer having a fixed reference magnetization aligned with a magnetization axis; a magnetically free layer having a magnetically free magnetization, wherein the magnetically free magnetization is variable in the presence of an external magnetic field; and a non-magnetic layer arranged between the reference layer and the magnetically free layer; and a stress inducing layer coupled to the layer stack, wherein the stress inducing layer is configured to apply a force to the layer stack to induce mechanical stress in the layer stack along a mechanical stress axis so that the magnetization axis is aligned parallel to the mechanical stress axis or perpendicular to the mechanical stress axis.
[0097] Aspect 2: The magnetoresistive sensor according to aspect 1, wherein the stress inducing layer is configured to apply a force to the layer stack to induce an extension or compression of the layer stack parallel to the mechanical stress axis or perpendicular to the mechanical stress axis.
[0098] Aspect 3: The magnetoresistive sensor according to any one of aspects 1 to 2, wherein the force is a compressive force that induces a tensile stress in the layer stack parallel to the mechanical stress axis or perpendicular to the mechanical stress axis.
[0099] Aspect 4: The magnetoresistive sensor according to any one of aspects 1 to 3, wherein the stress-inducing layer is a compressive layer that extends the layer stack in a dimension parallel to the mechanical stress axis.
[0100] Aspect 5: The magnetoresistive sensor according to any one of aspects 1 to 4, wherein the stress inducing layer is configured to deform, induce mechanical stress in the layer stack and deform the layer stack parallel to the mechanical stress axis.
[0101] Aspect 6: The magnetoresistive sensor according to any one of Aspects 1 to 5, wherein the mechanical stress axis is predefined to control the orientation of the magnetization axis.
[0102] Aspect 7: The magnetoresistive sensor according to any one of Aspects 1 to 6 further includes: a first conductive layer configured to conduct current; and a second conductive layer configured to conduct current, wherein a layer stack is arranged between the first conductive layer and the second conductive layer, and wherein a stress inducing layer is arranged between the first conductive layer and the layer stack.
[0103] Aspect 8: The magnetoresistive sensor according to Aspect 7 further includes: a second stress inducing layer arranged between the second conductive layer and the layer stack, wherein the second stress inducing layer is configured to induce a second mechanical stress in the layer stack along the mechanical stress axis so that the magnetization axis is aligned parallel to the mechanical stress axis or perpendicular to the mechanical stress axis.
[0104] Aspect 9: The magnetoresistive sensor according to any one of aspects 1 to 8, wherein the stress inducing layer is configured to bend in a dimension parallel to the mechanical stress axis so that the force is applied to the layer stack as a compressive force or a decompressive force.
[0105] Aspect 10: A magnetoresistive sensor according to any one of Aspects 1 to 9, wherein the sensing element includes a sensor plane defined by a first axis and a second axis, wherein the layers of the layer stack are stacked along a third axis perpendicular to the first axis and the second axis, wherein the mechanical stress axis is aligned with the first axis, wherein the stress inducing layer has a first dimension extending parallel to the first axis and a second dimension extending parallel to the second axis, and wherein the first dimension is smaller than the second dimension.
[0106] Aspect 11: A magnetoresistive sensor according to any one of Aspects 1 to 10, wherein the layer stack includes a reference layer system, the reference layer system including: a pinned layer having a pinned magnetization via coupled to an antiferromagnet; a reference layer having a fixed reference magnetization oriented to be antiparallel to the pinned magnetization; and a coupling intermediate layer arranged between the pinned layer and the reference layer and configured to couple the fixed reference magnetization to be antiparallel to the pinned magnetization, wherein the stress inducing layer is configured to apply a force to the layer stack along the mechanical stress axis so that the pinned magnetization is aligned with or perpendicular to the mechanical stress axis.
[0107] Aspect 12: The magnetoresistive sensor according to aspect 11, wherein the stress inducing layer is configured to apply a force to the layer stack to induce an elongation of the layer stack parallel to the mechanical stress axis.
[0108] Aspect 13: A magnetoresistive sensor according to any one of Aspects 1 to 12, wherein the sensing element includes a sensor plane defined by a first axis and a second axis, wherein the layers of the layer stack are stacked along a third axis perpendicular to the sensor plane, wherein the mechanical stress axis is colinear with the first axis, wherein the stress inducing layer is configured to induce elongation or compression of the layer stack in a first dimension corresponding to the first axis, and substantially not induce elongation or compression of the layer stack in a second dimension corresponding to the second axis.
[0109] Aspect 14: A magnetoresistive sensor according to any one of Aspects 1 to 13, wherein the sensing element includes a sensor plane defined by a first axis and a second axis, wherein the layers of the layer stack are stacked along a third axis perpendicular to the sensor plane, wherein the mechanical stress axis is aligned with the first axis, wherein the stress inducing layer is configured to induce the reference layer to stretch by a first percentage in a first dimension corresponding to the first axis and to induce the reference layer to stretch by a second percentage in a second dimension corresponding to the second axis, and wherein the first percentage is at least twice the second percentage to increase the anisotropy of the magnetization of the reference layer.
[0110] Aspect 15: The magnetoresistive sensor of aspect 14, wherein the first percentage is at least four times the second percentage.
[0111] Aspect 16: A magnetoresistive sensor according to any one of Aspects 1 to 15, wherein the sensing element includes a sensor plane defined by a first axis and a second axis, wherein the sensing element has a diameter of 0.5-1.5 microns (μm) in the sensor plane, wherein the layers of the layer stack are stacked along a third axis perpendicular to the sensor plane, wherein the mechanical stress axis is collinear with the first axis, wherein the stress inducing layer has a first dimension corresponding to the first axis and a second dimension corresponding to the second axis, wherein the second dimension is at least twice as large as the first dimension, and wherein the first dimension is 1.0-3.0 μm.
[0112] Aspect 17: A magnetoresistive sensor according to any one of Aspects 1 to 16, wherein the stress inducing layer has a width dimension of 1-3 microns (μm) defined by a first lateral edge and a second lateral edge and a length dimension defined by a third lateral edge and a fourth lateral edge, wherein the layer stack is arranged between the first lateral edge and the second lateral edge and the layer stack is arranged between the third lateral edge and the fourth lateral edge, wherein the layer stack has an outer periphery having a first distance of no more than 2 μm from the first lateral edge and the second lateral edge, respectively, and having a second distance of more than 2 μm from the third lateral edge and the fourth lateral edge, respectively, wherein a minimum distance of the second distance is at least twice as large as a maximum distance of the first distance.
[0113] Aspect 18: The magnetoresistive sensor according to any one of Aspects 1 to 17, wherein the mechanical stress increases the magnetoresistive effect of the sensing element.
[0114] Aspect 19: A magnetoresistive sensor comprising: a first sensing element having a first layer stack, the first layer stack comprising: a first reference layer having a first fixed reference magnetization aligned with a first magnetization axis; a first magnetically free layer having a first magnetically free magnetization, wherein the first magnetically free magnetization is variable in the presence of an external magnetic field; and a first non-magnetic layer, the first non-magnetic layer being arranged between the first reference layer and the first magnetically free layer; a second sensing element having a second layer stack, the second layer stack comprising: a second reference layer having a second fixed reference magnetization aligned with a second magnetization axis; a second magnetically free layer having a second magnetically free magnetization, wherein The second magnetic free magnetization is changeable in the presence of an external magnetic field; and a second non-magnetic layer, which is arranged between the second reference layer and the second magnetic free layer; and a stress inducing layer, which is coupled to the first layer stack and the second layer stack, wherein the stress inducing layer is configured to apply a first force to the first layer stack to induce a first mechanical stress in the first layer stack along a first mechanical stress axis, so that the first magnetization axis is aligned parallel to the first mechanical stress axis or perpendicular to the first mechanical stress axis, and apply a second force to the second layer stack to induce a second mechanical stress in the second layer stack along a second mechanical stress axis, so that the second magnetization axis is aligned parallel to the second mechanical stress axis or perpendicular to the second mechanical stress axis.
[0115] Aspect 20: The magnetoresistive sensor according to Aspect 19, wherein the first mechanical stress axis is parallel to the second magnetization axis.
[0116] Aspect 21: A magnetoresistive sensor according to any one of Aspects 19 to 20, wherein the first force is a first compressive force that induces a first tensile stress in the first reference layer parallel to the first mechanical stress axis and aligns the first magnetization axis parallel to or perpendicular to the first mechanical stress axis, and wherein the second force is a second compressive force that induces a second tensile stress in the second reference layer parallel to the second mechanical stress axis and aligns the second magnetization axis parallel to or perpendicular to the second mechanical stress axis.
[0117] Aspect 22: A magnetoresistive sensor according to any one of Aspects 19 to 21, wherein the stress inducing layer is a straight structure having a first dimension extending in a first direction and a second dimension extending in a second direction perpendicular to the first direction, wherein the first dimension is smaller than the second dimension and the first dimension is subjected to bending stress, generating a first force applied to the first layer stack and a second force applied to the second layer stack, wherein the first sensing element and the second sensing element are spaced apart in the second direction, and wherein the first dimension is parallel to the first mechanical stress axis and the second mechanical stress axis.
[0118] Aspect 23: A magnetoresistive sensor according to any one of Aspects 19 to 22, wherein the stress inducing layer is a U-shaped structure having a first segment coupled to a first layer stack, a second segment coupled to a second layer stack, and a third segment coupled to the first segment and the second segment and extending in a lateral direction between the first segment and the second segment, wherein the lateral direction is parallel to a first mechanical stress axis and a second mechanical stress axis, wherein the first segment is configured to apply a first force to the first layer stack, thereby inducing a first mechanical stress along the first mechanical stress axis, and wherein the second segment is configured to apply a second force to the second layer stack, thereby inducing a second mechanical stress along the second mechanical stress axis.
[0119] Aspect 24: A magnetoresistive sensor comprising: a sensing element having a layer stack in a vertical dimension, the layer stack comprising: a reference layer having a fixed reference magnetization aligned with a magnetization axis; a magnetically free layer having a magnetically free magnetization, wherein the magnetically free magnetization is variable in the presence of an external magnetic field; and a non-magnetic layer arranged between the reference layer and the magnetically free layer; and a conductive layer coupled to the top and bottom of the layer stack, wherein the conductive layer has a first outer periphery defining a lateral edge of the conductive layer, wherein the layer stack has a second outer periphery defining a lateral edge of the layer stack, wherein a minimum distance between the first outer periphery and the second outer periphery is greater than 1 micrometer (μm).
[0120] Aspect 25: The magnetoresistive sensor of aspect 24, wherein the preferred magnetic anisotropy of the fixed reference magnetization is substantially unaffected by the conductive layer.
[0121] The foregoing disclosure provides illustration and description, but is not intended to be exhaustive or to limit the implementation to the precise form disclosed. Modifications and variations are possible in light of the above disclosure or may be acquired from practice of implementation.
[0122] Although the specific combination of features is disclosed in the claims and / or in the specification, these combinations are not intended to limit the disclosure of the implementation described herein. Many of these features can be combined in a manner not specifically described in the claims and / or disclosed in the specification. For example, the disclosure includes the combination of each dependent claim in the claim set and every other independent claim in the claim set and each combination of multiple claims in the claim set. As used herein, the phrase "at least one" referring to the list of items refers to any combination of those items including a single member. As an example, "at least one of a, b, or c" is intended to cover a, b, c, a+b, a+c, b+c, and a+b+c, and any combination of multiple identical elements (for example, a+a, a+a+a, a+a+b, a+a+c, a+b+b, a+c+c, b+b, b+b+b, b+b+c, c+c, and c+c+c, or any other ordering of a, b, and c).
[0123] In addition, it should be understood that the disclosure of multiple actions or functions disclosed in the specification or claims may not be interpreted as being in a specific order. Therefore, the disclosure of multiple actions or functions will not limit these to a specific order, unless such actions or functions are not interchangeable for technical reasons. In addition, in some embodiments, a single action may include or may be divided into multiple sub-actions. Unless explicitly excluded, these sub-actions may be included and are part of the disclosure of the single action.
[0124] Unless so clearly described, the elements, actions or instructions used herein should not be interpreted as critical or necessary. In addition, as used herein, the articles "one" and "an" are intended to include one or more items and can be used interchangeably with "one or more". Further, as used herein, the article "the" is intended to include one or more items quoted in conjunction with the article "the", and can be used interchangeably with "one or more". Wherein only one item is used, using phrases "only one", "single" or similar language. In addition, as used herein, the terms "have (has)", "have (have)", "have (having)" etc. are intended to be open terms (for example, element "has" A can also have B) of the elements that do not limit their modification. Further, unless otherwise clearly stated, the phrase "based on" is intended to mean "based at least in part". As used herein, the term "multiple" can be replaced with "multiple" and vice versa. Furthermore, as used herein, the term "or" is intended to be inclusive and interchangeable with "and / or" when used in a serial manner unless expressly stated otherwise (eg, if used in conjunction with "either" or "only one").
Claims
1. A magnetoresistive sensor, comprising: A sensing element having a layer stack, the layer stack comprising: a reference layer having a fixed reference magnetization aligned with the magnetization axis; a magnetically free layer having a magnetically free magnetization, wherein the magnetically free magnetization is changeable in the presence of an external magnetic field; and a nonmagnetic layer disposed between the reference layer and the magnetic free layer; and A stress inducing layer is coupled to the layer stack, wherein the stress inducing layer is configured to apply a force to the layer stack to induce mechanical stress in the layer stack along a mechanical stress axis so that the magnetization axis is aligned parallel to the mechanical stress axis or perpendicular to the mechanical stress axis. 2 . The magnetoresistive sensor according to claim 1 , wherein the stress inducing layer is configured to apply the force to the layer stack to induce an elongation or compression of the layer stack parallel to the mechanical stress axis or perpendicular to the mechanical stress axis. 3 . The magnetoresistive sensor of claim 1 , wherein the force is a compressive force that induces a tensile stress in the layer stack parallel to the mechanical stress axis or perpendicular to the mechanical stress axis. 4 . The magnetoresistive sensor of claim 1 , wherein the stress-inducing layer is a compressive layer that extends the layer stack in a dimension parallel to the mechanical stress axis. 5 . The magnetoresistive sensor of claim 1 , wherein the stress inducing layer is configured to deform, induce the mechanical stress in the layer stack and deform the layer stack parallel to the mechanical stress axis. 6 . The magnetoresistive sensor of claim 1 , wherein the mechanical stress axis is predefined to control the orientation of the magnetization axis.
7. The magnetoresistive sensor according to claim 1, further comprising: a first conductive layer configured to conduct electric current; as well as a second conductive layer configured to conduct the current, wherein the layer stack is arranged between the first conductive layer and the second conductive layer, Wherein the stress inducing layer is arranged between the first conductive layer and the layer stack.
8. The magnetoresistive sensor according to claim 7, further comprising: a second stress inducing layer arranged between the second conductive layer and the layer stack, The second stress inducing layer is configured to induce a second mechanical stress in the layer stack along the mechanical stress axis so that the magnetization axis is aligned parallel to the mechanical stress axis or perpendicular to the mechanical stress axis.
9. The magnetoresistive sensor of claim 1, wherein the stress inducing layer is configured to bend in a dimension parallel to the mechanical stress axis such that the force is applied to the layer stack as a compressive force or a decompressive force.
10. The magnetoresistive sensor of claim 1 , wherein the sensing element comprises a sensor plane defined by a first axis and a second axis, wherein the layers of the layer stack are stacked along a third axis perpendicular to the first axis and the second axis, wherein the mechanical stress axis is aligned with the first axis, wherein the stress inducing layer has a first dimension extending parallel to the first axis and a second dimension extending parallel to the second axis, and The first size is smaller than the second size.
11. The magnetoresistive sensor according to claim 1 , wherein the layer stack comprises a reference layer system comprising: a pinned layer having a pinned magnetized via coupled to the antiferromagnet; the reference layer having the fixed reference magnetization oriented antiparallel to the pinned magnetization; as well as a coupling intermediate layer disposed between the pinned layer and the reference layer and configured to couple the fixed reference magnetization to be antiparallel to the pinned magnetization, The stress inducing layer is configured to apply the force to the layer stack along the mechanical stress axis so that the pinned magnetization is aligned with or perpendicular to the mechanical stress axis. 12 . The magnetoresistive sensor of claim 11 , wherein the stress inducing layer is configured to apply the force to the layer stack to induce an elongation of the layer stack parallel to the mechanical stress axis.
13. The magnetoresistive sensor of claim 1 , wherein the sensing element comprises a sensor plane defined by a first axis and a second axis, wherein the layers of the layer stack are stacked along a third axis perpendicular to the sensor plane, wherein the mechanical stress axis is collinear with the first axis, The stress inducing layer is configured to induce elongation or compression of the layer stack in a first dimension corresponding to the first axis, and substantially not induce elongation or compression of the layer stack in a second dimension corresponding to the second axis.
14. The magnetoresistive sensor of claim 1 , wherein the sensing element comprises a sensor plane defined by a first axis and a second axis, wherein the layers of the layer stack are stacked along a third axis perpendicular to the sensor plane, wherein the mechanical stress axis is aligned with the first axis, wherein the stress inducing layer is configured to: induce the reference layer to stretch by a first percentage in a first dimension corresponding to the first axis, and induce the reference layer to stretch by a second percentage in a second dimension corresponding to the second axis, and The first percentage is at least twice the second percentage to increase the anisotropy of the magnetization of the reference layer.
15. The magnetoresistive sensor of claim 14, wherein the first percentage is at least four times the second percentage.
16. The magnetoresistive sensor of claim 1 , wherein the sensing element comprises a sensor plane defined by a first axis and a second axis, wherein the sensing element has a diameter in the sensor plane of 0.5 micrometers to 1.5 micrometers, wherein the layers of the layer stack are stacked along a third axis perpendicular to the sensor plane, wherein the mechanical stress axis is collinear with the first axis, Wherein the stress inducing layer has a first dimension corresponding to the first axis and a second dimension corresponding to the second axis, wherein the second dimension is at least twice as large as the first dimension, and wherein the first dimension is between 1.0 microns and 3.0 microns.
17. The magnetoresistive sensor of claim 1 , wherein the stress inducing layer has a width dimension of 1 μm to 3 μm defined by the first lateral edge and the second lateral edge and a length dimension defined by the third lateral edge and the fourth lateral edge, wherein the layer stack is arranged between the first transverse edge and the second transverse edge, and the layer stack is arranged between the third transverse edge and the fourth transverse edge, wherein the layer stack has an outer perimeter having a first distance of no more than 2 micrometers from the first lateral edge and the second lateral edge, respectively, and having a second distance of more than 2 micrometers from the third lateral edge and the fourth lateral edge, respectively, The minimum distance of the second distance is at least twice as large as the maximum distance of the first distance.
18. The magnetoresistive sensor of claim 1, wherein the mechanical stress increases a magnetoresistive effect of the sensing element.
19. A magnetoresistive sensor, comprising: The first sensing element has a first stacked body, wherein the first stacked body comprises: a first reference layer having a first fixed reference magnetization aligned with a first magnetization axis; a first magnetically free layer having a first magnetically free magnetization, wherein the first magnetically free magnetization is changeable in the presence of an external magnetic field; and a first non-magnetic layer disposed between the first reference layer and the first magnetic free layer; The second sensing element has a second stacked body, wherein the second stacked body comprises: a second reference layer having a second fixed reference magnetization aligned with the second magnetization axis; a second magnetically free layer having a second magnetically free magnetization, wherein the second magnetically free magnetization is changeable in the presence of an external magnetic field; and a second nonmagnetic layer disposed between the second reference layer and the second magnetic free layer; and A stress inducing layer is coupled to the first layer stack and the second layer stack, wherein the stress inducing layer is configured to: apply a first force to the first layer stack to induce a first mechanical stress in the first layer stack along a first mechanical stress axis, so that the first magnetization axis is aligned parallel to the first mechanical stress axis or perpendicular to the first mechanical stress axis, and apply a second force to the second layer stack to induce a second mechanical stress in the second layer stack along a second mechanical stress axis, so that the second magnetization axis is aligned parallel to the second mechanical stress axis or perpendicular to the second mechanical stress axis.
20. The magnetoresistive sensor of claim 19, wherein the first mechanical stress axis is parallel to the second magnetization axis.
21. The magnetoresistive sensor of claim 19, wherein the first force is a first compressive force that induces a first tensile stress in the first reference layer parallel to the first mechanical stress axis and aligns the first magnetization axis parallel to or perpendicular to the first mechanical stress axis, and The second force is a second compressive force, which induces a second tensile stress in the second reference layer parallel to the second mechanical stress axis and aligns the second magnetization axis parallel to or perpendicular to the second mechanical stress axis.
22. The magnetoresistive sensor of claim 19, wherein the stress-inducing layer is a straight structure having a first dimension extending in a first direction and a second dimension extending in a second direction perpendicular to the first direction, wherein the first dimension is smaller than the second dimension, and the first dimension is subject to bending stress resulting in the first force being applied to the first layer stack and the second force being applied to the second layer stack, wherein the first sensing element and the second sensing element are spaced apart in the second direction, and The first dimension is parallel to the first mechanical stress axis and the second mechanical stress axis.
23. The magnetoresistive sensor of claim 19 , wherein the stress-inducing layer is a U-shaped structure having a first segment coupled to the first layer stack, a second segment coupled to the second layer stack, and a third segment coupled to the first segment and the second segment and extending in a lateral direction between the first segment and the second segment, wherein the lateral direction is parallel to the first mechanical stress axis and the second mechanical stress axis, wherein the first segment is configured to apply the first force to the first layer stack so as to induce the first mechanical stress along the first mechanical stress axis, and The second segment is configured to apply the second force to the second layer stack, thereby inducing the second mechanical stress along the second mechanical stress axis.
24. A magnetoresistive sensor, comprising: A sensing element having a layer stack stacked in a vertical dimension, the layer stack comprising: a reference layer having a fixed reference magnetization aligned with the magnetization axis; a magnetically free layer having a magnetically free magnetization, wherein the magnetically free magnetization is changeable in the presence of an external magnetic field; and a nonmagnetic layer disposed between the reference layer and the magnetic free layer; and a conductive layer coupled to the top and bottom of the layer stack, wherein the conductive layer has a first outer perimeter defining a lateral edge of the conductive layer, Wherein the layer stack has a second outer perimeter defining a lateral edge of the layer stack, wherein a minimum distance between the first outer perimeter and the second outer perimeter is greater than 1 micrometer.
25. The magnetoresistive sensor of claim 24, wherein the preferred magnetic anisotropy of the fixed reference magnetization is substantially unaffected by the conductive layer.