Preparation method and application of electrochemical sensor based on metal cluster composite material
The electrochemical sensor based on metal cluster composite materials solves the problem of insufficient detection response sensitivity of profenofos in the existing technology, and achieves efficient, stable, and anti-interference detection effects, which is suitable for practical applications.
Patent Information
- Application Number
- CN202411057928.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-02
- Publication Date
- 2024-10-18
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing electrochemical sensors have insufficient response sensitivity when detecting organophosphorus pesticides with poor stability and difficult to volatilize, such as profenofos, and traditional detection methods have problems such as high cost and easy pollution.
Electrochemical sensors based on metal cluster composite materials are used, including glassy carbon electrodes, metal clusters@graphene, white kidney bean esterase-chitosan and Nafion membranes. Through the size aggregation synthesis of metal clusters and composites with carbon materials, enzymes Combined with chitosan, the electrochemical biosensor electrode was assembled layer by layer, and the enzyme inhibition method was used to detect the content of profenofos.
Efficient detection of profenofos residues is achieved. The sensor has good repeatability, stability and interference resistance, high response sensitivity, a linear range of 1 to 2000 μg/L, and a correlation coefficient R2 = 0.97316, making it suitable for practical applications.
Smart Images

Figure CN118795000A_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the technical field of biosensors, and in particular relates to a preparation method and application of an electrochemical sensor based on a metal cluster composite material. Background Art
[0002] As a typical organophosphorus pesticide, bromophos is widely used in modern agricultural production. It is an asymmetric organophosphorus insecticide with contact and stomach poisoning effects, a wide insecticide spectrum, and long-lasting efficacy. It can prevent and control harmful insects and mites in crops such as cotton, vegetables, and fruit trees. However, the pesticide residue problem caused by the widespread use of organophosphorus pesticides not only seriously pollutes the ecological environment, but also seriously endangers human health. For example, bromophos, which is highly toxic, is easily absorbed by the human body, which not only seriously damages important organs such as the liver and kidneys, but may also cause epilepsy, toxic shock, etc. Damage to the central nervous system, gastrointestinal perforation or bleeding, respiratory failure, damage to the liver and kidneys, etc.; ultimately endangering human health. Therefore, for environmental monitoring and governance as well as food safety, it is necessary to accurately detect and analyze pesticide residues in the environment and agricultural products.
[0003] At present, traditional detection methods mainly include gas chromatography, high performance liquid chromatography and colorimetry. Gas chromatography is widely used, but it is not suitable for detecting substances with poor stability and low volatility; high performance liquid chromatography is suitable for the detection of complex samples, but it is expensive and prone to pollution; colorimetry is simple to operate, but it has certain requirements on the absorption properties of the substance being detected.
[0004] Compared with traditional detection methods, electrochemical detection is more sensitive and more convenient. By using the constructed electrochemical biosensor to detect the inhibition rate of bromophos on enzymatic reactions, the residual amount of bromophos in the sample can be analyzed more quickly and efficiently. At present, the electrode modification materials of electrochemical biosensors mainly include carbon material carriers and metal nanomaterials. The commonly used carbon material is graphene, and the metal nanomaterial is metal nanoparticles, but there are still certain deficiencies in response sensitivity. Summary of the invention
[0005] The object of the present invention is to provide an electrochemical sensor based on a metal cluster composite material to solve the problems raised in the above background technology.
[0006] To achieve the above object, the present invention provides the following technical solutions:
[0007] An electrochemical sensor based on a metal cluster composite material comprises a glassy carbon electrode, metal cluster@graphene, white kidney bean esterase-chitosan and a Nafion membrane.
[0008] A method for preparing an electrochemical sensor based on a metal cluster composite material comprises the following steps:
[0009] S1. Synthesis of metal clusters: Weigh 0.1-10 mmol of metal precursor and surfactant, add to 5-500 mL of organic solvent and stir thoroughly to obtain a reddish brown solution; take 1-10 times the molar number of metal precursor organic ligand, add to the above solution, stir thoroughly to make it completely mixed and react; place the reaction solution in ice water, then take 0.1-2 mol / L sodium borohydride (NaBH4) solution, add to the solution, and continue stirring for 2-12 hours in an ice bath. After the reaction is terminated, the mixed solution is evaporated and concentrated, and then washed with a large amount of ice water and organic solvent for 2-3 times in turn. The obtained product is extracted with an organic solvent, and then single crystals are grown to obtain pure Au. 25 Clusters;
[0010] S2. Preparation of electrode composite materials: Ultrasonic dispersion of graphene and organic solvent, adding the newly prepared metal cluster solution, and ultrasonic treatment again to obtain Au 25 @G solution. Add white kidney bean powder to ultrapure water and stir evenly, then put it in a refrigerator for extraction. The temperature in the refrigerator is set at 4°C. After centrifugation, the supernatant is aspirated to obtain a crude enzyme solution (KbE), chitosan (CS) is added and shaken to obtain a KbE-CS solution;
[0011] S3, build NF / KbE-CS / Au 25 @G / GCE electrochemical biosensor: Au 25 @G composite solution, KbE-CS solution, and Nafion solution (NF) are sequentially dripped onto the clean bare electrode (GCE). After modification, it is dried with an infrared lamp, then rinsed with ultrapure water, and blown dry with an ear bulb to obtain NF / KbE-CS / Au. 25 @G / GCE electrochemical biosensor.
[0012] Preferably, the metal precursor in S1 includes but is not limited to chloroauric acid and triphenylphosphine gold chloride.
[0013] Preferably, the surfactant in S1 includes but is not limited to tetraoctylammonium bromide, tetrabutylammonium chloride or octadecyltrimethylammonium chloride.
[0014] Preferably, the organic solvents described in S1 and S2 include but are not limited to methanol, ethanol, acetonitrile, dichloromethane, toluene, acetone, tetrahydrofuran, isopropanol, n-butanol, and N,N-dimethylformamide.
[0015] Preferably, the organic solvent used for extraction in S1 is a mixture of toluene and methanol, and the ratio of toluene to methanol includes but is not limited to 1 / 30, 1 / 15, 1 / 10, 1 / 6, 1 / 3, 1 / 2.
[0016] Preferably, the organic ligand in S1 includes but is not limited to phenylethyl mercaptan, 4-methylthiophenol, 2,4-dimethylthiophenol, 4-tert-butylthiophenol, cyclohexanethiol, and benzyl mercaptan.
[0017] Preferably, the solvent of the NaBH4 solution described in S1 includes but is not limited to water, methanol, ethanol, acetonitrile, dichloromethane, toluene, acetone, tetrahydrofuran, isopropanol, and n-butanol.
[0018] The NF / KbE-CS / Au25@G / GCE bioelectrochemical sensor prepared by a preparation method of an electrochemical sensor based on a metal cluster composite material is applied to the detection of propyl bromide.
[0019] Compared with the prior art, the present invention has the following beneficial effects:
[0020] The present invention constructs NF / KbE-CS / Au 25 @G / GCE new electrochemical sensor, the core component of which is Au 25 @G, the preparation method includes the size aggregation synthesis of metal clusters, the composite of metal clusters and carbon materials, the composite of enzymes and chitosan, and the layer-by-layer assembly of electrochemical biosensor electrodes. The cluster is composed of gold atoms and organic ligands, the number of gold atoms is 25, and it has a precise and stable three-dimensional structure. At the same time, the metal cluster and graphene composite material have good conductivity and synergistic electrocatalytic effect, which can effectively promote electron transfer, improve the response sensitivity of the sensor of the present invention, and realize efficient detection of bromophos residue.
[0021] At the same time, the present invention uses white kidney bean esterase as an enzyme source, adopts enzyme inhibition method to detect the content of bromophos, and applies it to actual sample inspection. 25 @G / GCE has good repeatability, stability and anti-interference in the test. Under the optimal experimental conditions of Au25@G loading of 5 μL, pH of PBS buffer solution of 7.0 and inhibition time of bromophos of 15 min, the linear range of electrochemical biosensor detection of bromophos is 1-2000 μg / L, the linear equation is Y=19.8626lgc+13.3459, and the correlation coefficient R 2 =0.97316. The electrochemical biosensor of the present invention exhibits excellent response sensitivity, indicating that it has broad prospects in practical applications. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1 The Au of the present invention 25 (PET) 18 UV-visible absorption spectrum of
[0023] Figure 2 For the present invention, different Au25 @G Line graph of load and peak current I;
[0024] Figure 3 It is a line graph of different inhibition times and inhibition rates of profenofos of the present invention;
[0025] Figure 4 It is a linear relationship diagram between the mass concentration of bromophos and the inhibition rate of the present invention;
[0026] Figure 5 This is a stability diagram of repeated SWV detection of the same electrode of the present invention;
[0027] Figure 6 The interferences of the present invention on NF / KbE-CS / Au 25 @G / GCE biosensor response signal impact comparison chart. DETAILED DESCRIPTION
[0028] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0029] Example 1
[0030] Weigh 675 mg of tetraoctylammonium bromide (TOAB) and dissolve it in 30 mL of tetrahydrofuran (THF). Add HAuCl4 solution (496 mg dissolved in 5 mL of THF) dropwise, and the solution turns brown-red. After stirring for half an hour, add phenylethylmercaptan (1020 μL) ligand and continue stirring until colorless. Continue stirring for half an hour under ice bath. Then weigh 536 mg of NaBH4 and dissolve it in 8 mL of ice water, quickly add it to the flask, and the solution immediately turns black. Under ice bath conditions, the reaction lasts for 12 hours. When the reaction is completed, gradually evaporate and concentrate the reaction solution to ~30 mL under vacuum. Subsequently, wash the concentrated reaction solution with a large amount of ice water, repeat 2-3 times, and then wash with methanol 2-3 times. Finally, place the resulting product in a toluene / methanol mixture system to grow crystals. Within 1-2 days, needle-shaped Au 25 Crystals gradually precipitated.
[0031] After adding 4 mg of multilayer graphene to a 10 mL centrifuge tube, 4 mL of N,N-dimethylformamide was immediately added. Ultrasonic treatment was performed to make the multilayer graphene evenly dispersed in the solution. 25 The cluster N, N-dimethylformamide solution (concentration of 1 mg / mL) was added to the centrifuge tube and ultrasonicated again for 5 minutes.25 @G solution. Mix the white kidney bean powder in the ratio of 1 gram of powder / 5 mL of ultrapure water, stir evenly, and then put it in the refrigerator and set the temperature to 4°C for extraction overnight. After centrifugation, aspirate the supernatant (crude enzyme solution) and refrigerate. Accurately weigh 1 mg of chitosan with an analytical balance, add 5 mL of KbE crude enzyme solution supernatant to dissolve, shake well, and obtain 0.2 g / L KbE-CS solution.
[0032] Use a pipette to add 5 μL of Au 25 @G composite solution, 10μL 1g / L KbE-CS solution, and 4μL 0.5% Nafion solution were dripped on the clean bare electrode (GCE). After modification, it was dried with an infrared lamp, then rinsed with ultrapure water, and dried with an ear bulb. 25 @G / GCE electrochemical biosensor.
[0033] NF / KbE-CS / Au 25 The G / GCE electrodes were incubated in prepared solutions of different mass concentrations of bromophos for 15 minutes, and then each electrode was transferred to a PBS buffer solution containing 0.8 mmol / L 1-NA at pH = 7.0 for SWV scanning. The SWV curves at different concentrations were recorded and analyzed. The experimental results showed that within the range of 1 to 2000 μg / L, the mass concentration of bromophos (lgC) and the inhibition rate (Y) showed a good linear relationship, and the linear equation was Y = 13.3459lgc + 19.8626, and the correlation coefficient R 2 =0.97316.
[0034] First, the purple cabbage juice PBS test solution was obtained by grinding, extraction, centrifugation and dilution. The NF / KbE-CS / Au 25 @G / GCE modified electrode was tested in pH=7.00.1mol / LPBS containing 0.8mmol / L 1-NA to obtain square wave pulse voltammogram, and then I0 was obtained. 25 The G / GCE modified electrode was incubated in a PBS mixed solution containing purple cabbage juice for 15 min. After incubation, the SWV was measured in a pH = 7.00.1 mol / L PBS mixed solution containing 0.8 mmol / L 1-NA to obtain I1 and inhibition rate. Substituting the standard curve, it can be seen that the concentration of propyl bromide is lower than the residual amount specified by the national standard.
[0035] Example 2
[0036] Weigh 675 mg of tetraoctylammonium bromide (TOAB) and dissolve it in 30 mL of tetrahydrofuran (THF). Add HAuCl4 solution (496 mg dissolved in 5 mL of THF) dropwise, and the solution turns brown-red. After stirring for half an hour, add phenylethylmercaptan (1020 μL) ligand and continue stirring until colorless. Continue stirring for half an hour under ice bath. Then weigh 536 mg of NaBH4 and dissolve it in 8 mL of ice water, quickly add it to the flask, and the solution immediately turns black. Under ice bath conditions, the reaction lasts for 12 hours. When the reaction is completed, gradually evaporate and concentrate the reaction solution to ~30 mL under vacuum. Subsequently, wash the concentrated reaction solution with a large amount of ice water, repeat 2-3 times, and then wash with methanol 2-3 times. Finally, place the resulting product in a toluene / methanol mixture system to grow crystals. Within 1-2 days, needle-shaped Au 25 Crystals gradually precipitated.
[0037] After adding 4 mg of multilayer graphene to a 10 mL centrifuge tube, 4 mL of N,N-dimethylformamide was immediately added. Ultrasonic treatment was performed to make the multilayer graphene evenly dispersed in the solution. 25 The cluster N, N-dimethylformamide solution (concentration of 1 mg / mL) was added to the centrifuge tube and ultrasonicated again for 5 minutes. 25 @G solution. Mix the white kidney bean powder in the ratio of 1 gram of powder / 5 mL of ultrapure water, stir evenly, and then put it in the refrigerator and set the temperature to 4°C for extraction overnight. After centrifugation, aspirate the supernatant (crude enzyme solution) and refrigerate. Accurately weigh 1 mg of chitosan with an analytical balance, add 5 mL of KbE crude enzyme solution supernatant to dissolve, shake well, and obtain 0.2 g / L KbE-CS solution.
[0038] Use a pipette to add 5 μL of Au 25 @G composite solution, 10μL 1g / L KbE-CS solution, and 4μL 0.5% Nafion solution were dripped on the clean bare electrode (GCE). After modification, it was dried with an infrared lamp, then rinsed with ultrapure water, and dried with an ear bulb. 25 @G / GCE electrochemical biosensor.
[0039] NF / KbE-CS / Au 25The G / GCE electrodes were incubated in prepared solutions of different mass concentrations of bromophos for 15 minutes, and then each electrode was transferred to a PBS buffer solution containing 0.8 mmol / L 1-NA at pH = 7.0 for SWV scanning. The SWV curves at different concentrations were recorded and analyzed. The experimental results showed that within the range of 1 to 2000 μg / L, the mass concentration of bromophos (lgC) and the inhibition rate (Y) showed a good linear relationship, and the linear equation was Y = 13.3459lgc + 19.8626, and the correlation coefficient R 2 =0.97316. First, the leek juice PBS test solution was obtained by grinding, extraction, centrifugation and dilution. The NF / KbE-CS / Au 25 @G / GCE modified electrode was tested in pH=7.00.1mol / L PBS containing 0.8mmol / L 1-NA to obtain square wave pulse voltammogram, and then I0 was obtained. 25 The G / GCE modified electrode was incubated in a PBS mixed solution containing leek juice for 15 min. After incubation, the SWV was measured in a pH = 7.00.1 mol / L PBS mixed solution containing 0.8 mmol / L 1-NA to obtain I1 and inhibition rate. Substituting the standard curve, it can be seen that the concentration of propyl bromide is lower than the residual amount specified by the national standard.
[0040] Example 3
[0041] Weigh 675 mg of tetraoctylammonium bromide (TOAB) and dissolve it in 30 mL of tetrahydrofuran (THF). Add HAuCl4 solution (496 mg dissolved in 5 mL of THF) dropwise, and the solution turns brown-red. After stirring for half an hour, add phenylethylmercaptan (1020 μL) ligand and continue stirring until colorless. Continue stirring for half an hour under ice bath. Then weigh 536 mg of NaBH4 and dissolve it in 8 mL of ice water, quickly add it to the flask, and the solution immediately turns black. Under ice bath conditions, the reaction lasts for 12 hours. When the reaction is completed, gradually evaporate and concentrate the reaction solution to ~30 mL under vacuum. Subsequently, wash the concentrated reaction solution with a large amount of ice water, repeat 2-3 times, and then wash with methanol 2-3 times. Finally, place the resulting product in a toluene / methanol mixture system to grow crystals. Within 1-2 days, needle-shaped Au 25 Crystals gradually precipitated.
[0042] After adding 4 mg of multilayer graphene to a 10 mL centrifuge tube, 4 mL of N,N-dimethylformamide was immediately added. Ultrasonic treatment was performed to make the multilayer graphene evenly dispersed in the solution. 25The cluster N, N-dimethylformamide solution (concentration of 1 mg / mL) was added to the centrifuge tube and ultrasonicated again for 5 minutes. 25 @G solution. Mix the white kidney bean powder in the ratio of 1 gram of powder / 5 mL of ultrapure water, stir evenly, and then put it in the refrigerator and set the temperature to 4°C for extraction overnight. After centrifugation, aspirate the supernatant (crude enzyme solution) and refrigerate. Accurately weigh 1 mg of chitosan with an analytical balance, add 5 mL of KbE crude enzyme solution supernatant to dissolve, shake well, and obtain 0.2 g / L KbE-CS solution.
[0043] Use a pipette to add 5 μL of Au 25 @G composite solution, 10μL 1g / L KbE-CS solution, and 4μL 0.5% Nafion solution were dripped on the clean bare electrode (GCE). After modification, it was dried with an infrared lamp, then rinsed with ultrapure water, and dried with an ear bulb. 25 @G / GCE electrochemical biosensor.
[0044] NF / KbE-CS / Au 25 The G / GCE electrodes were incubated in prepared solutions of different mass concentrations of bromophos for 15 minutes, and then each electrode was transferred to a PBS buffer solution containing 0.8 mmol / L 1-NA at pH = 7.0 for SWV scanning. The SWV curves at different concentrations were recorded and analyzed. The experimental results showed that within the range of 1 to 2000 μg / L, the mass concentration of bromophos (lgC) and the inhibition rate (Y) showed a good linear relationship, and the linear equation was Y = 13.3459lgc + 19.8626, and the correlation coefficient R 2 =0.97316. First, the PBS test solution of millet extract was obtained by grinding, extraction, centrifugation and dilution. The NF / KbE-CS / Au 25 @G / GCE modified electrode was tested in pH=7.00.1mol / LPBS containing 0.8mmol / L 1-NA to obtain square wave pulse voltammogram, and then I0 was obtained. 25 The G / GCE modified electrode was incubated in a PBS mixed solution containing millet extract for 15 min. After incubation, SWV was measured in a pH = 7.00.1 mol / L PBS mixed solution containing 0.8 mmol / L 1-NA to obtain I1 and inhibition rate. Substituting the standard curve, it can be seen that the concentration of propyl bromide is lower than the residual amount specified by the national standard.
[0045] Example 4
[0046] Weigh 675 mg of tetraoctylammonium bromide (TOAB) and dissolve it in 30 mL of tetrahydrofuran (THF). Add HAuCl4 solution (496 mg dissolved in 5 mL of THF) dropwise, and the solution turns brown-red. After stirring for half an hour, add phenylethylmercaptan (1020 μL) ligand and continue stirring until colorless. Continue stirring for half an hour under ice bath. Then weigh 536 mg of NaBH4 and dissolve it in 8 mL of ice water, quickly add it to the flask, and the solution immediately turns black. Under ice bath conditions, the reaction lasts for 12 hours. When the reaction is completed, gradually evaporate and concentrate the reaction solution to ~30 mL under vacuum. Subsequently, wash the concentrated reaction solution with a large amount of ice water, repeat 2-3 times, and then wash with methanol 2-3 times. Finally, place the resulting product in a toluene / methanol mixture system to grow crystals. Within 1-2 days, needle-shaped Au 25 Crystals gradually precipitated.
[0047] After adding 4 mg of multilayer graphene to a 10 mL centrifuge tube, 4 mL of N,N-dimethylformamide was immediately added. Ultrasonic treatment was performed to make the multilayer graphene evenly dispersed in the solution. 25 The cluster N, N-dimethylformamide solution (concentration of 1 mg / mL) was added to the centrifuge tube and ultrasonicated again for 5 minutes. 25 @G solution. Mix the white kidney bean powder in the ratio of 1 gram of powder / 5 mL of ultrapure water, stir evenly, and then put it in the refrigerator and set the temperature to 4°C for extraction overnight. After centrifugation, aspirate the supernatant (crude enzyme solution) and refrigerate. Accurately weigh 1 mg of chitosan with an analytical balance, add 5 mL of KbE crude enzyme solution supernatant to dissolve, shake well, and obtain 0.2 g / L KbE-CS solution.
[0048] Use a pipette to add 5 μL of Au 25 @G composite solution, 10μL 1g / L KbE-CS solution, and 4μL 0.5% Nafion solution were dripped on the clean bare electrode (GCE). After modification, it was dried with an infrared lamp, then rinsed with ultrapure water, and dried with an ear bulb. 25 @G / GCE electrochemical biosensor.
[0049] NF / KbE-CS / Au 25The G / GCE electrodes were incubated in prepared solutions of different mass concentrations of bromophos for 15 minutes, and then each electrode was transferred to a PBS buffer solution containing 0.8 mmol / L 1-NA at pH = 7.0 for SWV scanning. The SWV curves at different concentrations were recorded and analyzed. The experimental results showed that within the range of 1 to 2000 μg / L, the mass concentration of bromophos (lgC) and the inhibition rate (Y) showed a good linear relationship, and the linear equation was Y = 13.3459lgc + 19.8626, and the correlation coefficient R 2 =0.97316. First, the fennel white juice PBS test solution was obtained by grinding, extraction, centrifugation and dilution. The NF / KbE-CS / Au 25 @G / GCE modified electrode was tested in pH=7.00.1mol / L PBS containing 0.8mmol / L 1-NA to obtain square wave pulse voltammogram, and then I0 was obtained. 25 The G / GCE modified electrode was incubated in a PBS mixed solution containing fennel white juice for 15 min. After incubation, the SWV was measured in a pH = 7.00.1 mol / L PBS mixed solution containing 0.8 mmol / L 1-NA to obtain I1 and inhibition rate. Substituting the standard curve, it can be seen that the concentration of propyl bromide is lower than the residual amount specified by the national standard.
[0050] The present invention prepares NF / KbE-CS / Au 25 @G / GCE electrochemical biosensor, its electrochemical biosensor is used in the detection of bromophos.
[0051] The electrochemical biosensor is composed of a glassy carbon electrode, metal clusters@graphene, white bean esterase-chitosan, and a Nafion membrane, and the number of metal atoms is 25.
[0052] In order to study the response of the electrochemical biosensor of the present invention to the residual amount of bromophos, a method based on the inhibition rate as the premise of concentration detection is proposed. The specific test steps are as follows:
[0053] (1) Establishment of standard curve: NF / KbE-CS / Au 25 The @G / GCE electrodes were incubated in prepared bromophos solutions of different mass concentrations for a period of time, and then the electrodes were transferred to PBS buffer solution containing a certain concentration of 1-NA for square wave pulse SWV scanning.
[0054] As the concentration of bromophos increases, the peak current value decreases and the inhibition rate increases. Within a certain concentration range, there is a good linear relationship between the mass concentration of bromophos (lgC) and the inhibition rate (Y), and its linear equation and standard curve are obtained.
[0055] The following are applied to crops:
[0056] (2) Testing actual samples: Accurately weigh the sample and grind it thoroughly, then add it to a PBS solution, centrifuge the mixture, and take the supernatant for testing.
[0057] Firstly, the square wave pulse method was used to 25 @G / GCE modified electrode was tested in PBS containing a certain concentration of 1-NA to obtain a square wave pulse voltammogram, and then I0 was obtained. 25 The G / GCE modified electrode was incubated in a PBS mixed solution containing the sample solution for a period of time. After incubation, SWV was measured in a PBS mixed solution containing a certain concentration of 1-NA to obtain I1. The calculated inhibition rate was put into the standard curve to obtain the concentration of bromophos.
[0058] The electrochemical detection method used in the present invention is an enzyme inhibition method, using NF / KbE-CS / Au 25 @G / GCE electrochemical sensors have good repeatability, stability and anti-interference, and can maintain working capabilities under various conditions.
[0059] The mass concentration of the bromophos solution in step (1) is 1-2000 μg / L, the incubation time is 5-25 min, the 1-NA concentration is 0.1-2.0 mmol / L, the pH of the PBS buffer solution is 5.0-8.0, and the inhibition rate is
[0060]
[0061] The test conditions described in (2) should be consistent with the preferred test conditions in (1).
[0062] The present invention uses white kidney bean esterase as an enzyme source, adopts enzyme inhibition method to detect the content of bromophos, and applies it to the inspection of actual samples. NF / KbE-CS / Au 25 @G / GCE has good repeatability, stability and anti-interference in the test. 25 @G Under the optimal experimental conditions of 5 μL loading, 7.0 pH of PBS buffer solution, and 15 min inhibition time of bromophos, the linear range of electrochemical biosensor detection of bromophos was 1-2000 μg / L, the linear equation was Y=19.8626lgc+13.3459, and the correlation coefficient R 2 =0.97316. The electrochemical biosensor has high response sensitivity and convenient practical application prospects.
[0063] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. An electrochemical sensor based on a metal cluster composite material, characterized in that: The electrochemical sensor is composed of glassy carbon electrode, metal cluster@graphene, white kidney bean esterase-chitosan and Nafion membrane.
2. A method for preparing an electrochemical sensor based on a metal cluster composite material, characterized in that: The following steps are involved: S1. Synthesis of metal clusters: Weigh 0.1-10 mmol of metal precursor and surfactant, add to 5-500 mL of organic solvent and stir thoroughly to obtain a reddish brown solution; take 1-10 times the molar number of metal precursor organic ligand, add to the above solution, stir thoroughly to make it completely mixed and react; place the reaction solution in ice water, then take 0.1-2 mol / L sodium borohydride (NaBH4) solution, add to the solution, and continue stirring for 2-12 hours in an ice bath. After the reaction is terminated, the mixed solution is evaporated and concentrated, and then washed with a large amount of ice water and organic solvent for 2-3 times in turn. The obtained product is extracted with an organic solvent, and then single crystals are grown to obtain pure Au. 25 Clusters; S2. Preparation of electrode composite materials: Ultrasonic dispersion of graphene and organic solvent, adding the newly prepared metal cluster solution, and ultrasonic treatment again to obtain Au 25 @G solution. Add white kidney bean powder to ultrapure water and stir evenly, then put it in a refrigerator for extraction. The temperature in the refrigerator is set at 4°C. After centrifugation, the supernatant is aspirated to obtain a crude enzyme solution (KbE), chitosan (CS) is added and shaken to obtain a KbE-CS solution; S3. Construction of NF / KbE-CS / Au 25 @G / GCE electrochemical biosensor: Au 25 @G composite solution, KbE-CS solution, and Nafion solution (NF) are sequentially dripped onto the clean bare electrode (GCE). After modification, it is dried with an infrared lamp, then rinsed with ultrapure water, and blown dry with an ear bulb to obtain NF / KbE-CS / Au. 25 @G / GCE electrochemical biosensor.
3. The method for preparing an electrochemical sensor based on a metal cluster composite material according to claim 1, characterized in that: The metal precursor in S1 includes but is not limited to chloroauric acid and triphenylphosphine gold chloride.
4. The method for preparing an electrochemical sensor based on a metal cluster composite material according to claim 1, characterized in that: The surfactant in S1 includes but is not limited to tetraoctylammonium bromide, tetrabutylammonium chloride or octadecyltrimethylammonium chloride.
5. The method for preparing an electrochemical sensor based on a metal cluster composite material according to claim 1, characterized in that: The organic solvents described in S1 and S2 include but are not limited to methanol, ethanol, acetonitrile, dichloromethane, toluene, acetone, tetrahydrofuran, isopropanol, n-butanol, and N,N-dimethylformamide.
6. The method for preparing an electrochemical sensor based on a metal cluster composite material according to claim 1, characterized in that: The organic solvent used for extraction in S1 is a mixture of toluene and methanol, and the ratio of toluene to methanol includes but is not limited to 1 / 30, 1 / 15, 1 / 10, 1 / 6, 1 / 3, and 1 / 2.
7. The method for preparing an electrochemical sensor based on a metal cluster composite material according to claim 1, characterized in that: The organic ligand in S1 includes but is not limited to phenylethyl mercaptan, 4-methylthiophenol, 2,4-dimethylthiophenol, 4-tert-butylthiophenol, cyclohexanethiol, and benzyl mercaptan.
8. The method for preparing an electrochemical sensor based on a metal cluster composite material according to claim 1, characterized in that: The solvent of the NaBH4 solution described in S1 includes but is not limited to water, methanol, ethanol, acetonitrile, dichloromethane, toluene, acetone, tetrahydrofuran, isopropanol, and n-butanol.
9. NF / KbE-CS / Au prepared by the method for preparing an electrochemical sensor based on a metal cluster composite material according to claim 2 25 @G / GCE bioelectrochemical sensor is used for the detection of propyl bromide.
Citation Information
Patent Citations
Reduced graphene oxide coated platinum / stannic oxide nano-particle cluster gas sensor and preparation method thereof
CN108318510A
Vertical graphene glucolase working electrode, preparation method and biosensor
CN111707724A
Method of making a metallic composite and use thereof
US20160303544A1
Cited By
Construction method and application of noble metal nanocluster electrochemical sensor
CN119224089A