Double-groove type SiC MOSFET device and preparation method thereof
By introducing a double trench structure and a PN junction into the SiC MOSFET device, the problem of drain-source voltage overshoot during short circuit and avalanche processes of the device is solved, the short circuit withstand capability and avalanche capability of the device are improved, and the gate oxide layer is improved reliability, reducing on-resistance and power loss.
Patent Information
- Application Number
- CN202411176648.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-26
- Publication Date
- 2024-10-18
AI Technical Summary
SiC MOSFET devices are prone to drain-source voltage overshoot, short-circuit failure and performance degradation during short circuit and avalanche processes, especially in 800V electric drive systems, leading to device short circuit failure.
A dual-trench SiC MOSFET device is designed. By introducing a trench structure in the source area, a PN junction is formed in the P+ and N+ areas to reduce the saturation current, and an isolation dielectric layer and ohmic contact are provided on the gate trench area. Alloy, suppress the peak electric field and improve the short circuit withstand capability and avalanche capability of the device.
It can effectively reduce the saturation current and heat accumulation when the device is short-circuited, improve the short-circuit tolerance and avalanche capability of the device, improve the reliability of the gate oxide layer, reduce the on-resistance, and reduce power loss.
Smart Images

Figure CN118800784A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor technology, and in particular to a double-trench SiC MOSFET device and a preparation method thereof. Background Art
[0002] As a representative of the third-generation semiconductor materials, silicon carbide devices have gradually become an indispensable mainstream product in the field of power electronics. Their wide bandgap, high thermal conductivity and other characteristics play an important role in reducing the thermal resistance of power devices, improving the breakdown voltage and increasing the current density of devices.
[0003] The extremely fast switching speed of SiC MOSFET makes it very easy for the device to have a drain-source voltage overshoot problem during the shutdown process, especially in applications such as 800V electric drive systems, which can easily cause short-term avalanche breakdown of SiC MOSFET devices and form extremely large electrothermal stress near the SiC MOSFET gate oxide, which can easily cause device performance degradation or even damage during long-term use. In addition, SiC MOSFET will have a short-circuit fault when a short circuit occurs in the electric drive system, and the instantaneous high voltage and large current can easily cause the device to fail due to short circuit.
[0004] In order to solve the above problems, it is necessary to propose a double-trench SiC MOSFET device and a preparation method thereof. Summary of the invention
[0005] The present invention designs a dual-trench SiC MOSFET device, which can reduce the saturation current of the device when it is short-circuited, improve the short-circuit withstand capability and avalanche capability, and by introducing a trench structure in the source region, suppress the peak electric field at the gate oxide layer, which can improve the reliability problem of the trench MOSFET gate oxide layer.
[0006] The technical solution of the present invention is: A method for preparing a double-trench SiC MOSFET device comprises the following steps: S100, forming an N-epitaxial layer and a PW region on the N+ substrate layer; S200, etching on the PW region to form a plurality of gate trench regions spaced apart from each other; S300, forming a P+ region on the PW region by Al ion implantation, and forming an N+ region on the side of the P+ region by ion implantation (6); S400, forming a source trench region on the P+ region by etching, and forming an ohmic contact alloy on the inner sidewall of the source trench region; S500, depositing a gate oxide layer on the sidewall and bottom of the gate trench region, and filling it with a Poly layer to be led out as a gate electrode; S600, forming an isolation dielectric layer on the N-epitaxial layer; and forming an ohmic contact alloy layer on the side of the isolation dielectric layer to form an ohmic contact with the upper part of the P+ region and the N+ region; S700, forming a front electrode metal layer on the isolation dielectric layer, the ohmic contact alloy layer and in the source trench region by Al metal sputtering to serve as a source electrode lead.
[0007] Specifically, the doping concentration range of the PW region is 1E 17 cm -2 -1E 18 cm -2 , the doping depth is 0.8-1.5um.
[0008] Specifically, the gate trench region has a depth of 1-1.8 um.
[0009] Specifically, the concentration range of P+ region is 1E 18 cm -2 -1E 19 cm -2 ; The injection depth of the P+ region is the same as the injection depth of the PW region.
[0010] Specifically, the concentration range of the N+ region is 1E 18 cm -2 -5E 18 cm -2 , the injection depth is 0.4-0.8um.
[0011] Specifically, the depth of the source trench region is 0.4-0.9 um.
[0012] Specifically, the thickness of the gate oxide layer is 60nm-70nm.
[0013] Specifically, the PW region, the P+ region and the N+ region have the same potential.
[0014] Specifically, the front electrode metal layer fills up the source trench region, and the ohmic contact alloy on both side walls of the source trench region contacts the front electrode metal layer Al.
[0015] A double-trench SiC MOSFET device, comprising an N+ substrate layer, an N-epitaxial layer, a PW region and a front electrode metal layer arranged in sequence from bottom to top; The PW region is divided into a plurality of regions by setting a plurality of gate trench regions; The PW area of each region is provided with: A P+ region extending downward from the middle of the top surface of the PW region; An N+ region extends downward from the top surface of the PW region along the side of the P+ region; a gap is provided between the bottom surface of the N+ region and the bottom surface of the PW region; An ohmic contact alloy is disposed on the inner sidewall of the source trench region in the P+ region; The inner sidewall and the bottom of the gate trench region are respectively provided with a gate oxide layer; the bottom surface of the gate oxide layer is lower than the bottom surface of the PW region; the gate trench region is filled with a Poly layer on the gate oxide layer; A plurality of isolation dielectric layers are arranged at intervals on the PW region; the bottom surfaces of the isolation dielectric layers are respectively connected to the N+ region, the gate oxide layer and the Poly layer; The side of the isolation dielectric layer is provided with an ohmic contact alloy layer connected thereto; the bottom surface of the ohmic contact alloy layer is connected to the N+ region and the P+ region respectively; The bottom of the front electrode metal layer extends into the source trench region and is respectively connected to the isolation dielectric layer, the ohmic contact alloy layer, the P+ region and the ohmic contact alloy.
[0016] Beneficial effects of the present invention: Improve the short-circuit tolerance of the device: 1. When a SiC MOSFET is short-circuited, a high drain-source voltage will cause a large saturation current to flow through the device, causing heat accumulation, which in turn causes the performance of the device to degrade or even fail. The PN junctions of the P+ and N+ regions injected into the epitaxial layer of the structure of the present invention can deplete the current channel to a great extent, greatly reducing the saturation current of the device when a short circuit occurs, thereby effectively reducing the internal heat generation and heat accumulation of the device when a short circuit occurs, and improving the short-circuit tolerance of the device.
[0017] 2. Reduce the on-resistance of the device: The on-resistance between the drain and source of SiC MOSFET in the on state directly affects the power consumption and temperature of the device; the smaller the on-resistance, the smaller the power loss of the device during operation, so reducing the on-loss is a hot topic in the research and development of power devices. The PW region on both sides of the gate of the present invention is shallowly doped to reduce the channel resistance of the device and reduce device losses. At the same time, the P+ injected into the PW region acts as a shielding structure, which can further improve the avalanche capability of the device.
[0018] 3. Improve the gate oxide reliability of the device: When manufacturing a trench MOSFET structure, a stronger breakdown field strength will lead to a decrease in the gate oxide withstand voltage performance at the bottom of the trench. The present invention introduces a trench structure in the source region to suppress the peak electric field at the gate oxide layer and improve the reliability of the trench MOSFET gate oxide layer. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] Figure 1 is a cross-sectional schematic diagram of preparing an N-epitaxial layer; Figure 2 is a schematic cross-sectional view of the preparation of the PW region; Figure 3is a schematic cross-sectional view of preparing a gate trench region; Figure 4 is a cross-sectional schematic diagram of preparing a P+ region; Figure 5 is a schematic cross-sectional view of preparing an N+ region; Figure 6 is a cross-sectional schematic diagram of preparing a source trench region; Figure 7 is a cross-sectional schematic diagram of preparing an ohmic contact alloy; Figure 8 is a cross-sectional schematic diagram of preparing a gate oxide layer; Fig. 9 is a cross-sectional schematic diagram of preparing a Poly layer; Fig.10 is a cross-sectional schematic diagram of preparing an isolation dielectric layer; Fig.11 is a cross-sectional schematic diagram of preparing an ohmic contact alloy layer; Fig.12 is a schematic diagram of the metal cross section of the preparation of the front electrode; In the figure, 1 is the N+ substrate layer, 2 is the N- epitaxial layer, 3 is the PW region, 4 is the gate trench region, 5 is the P+ region, 6 is the N+ region, 7 is the source trench region, 8 is the ohmic contact alloy, 9 is the gate oxide layer, 10 is the Poly layer, 11 is the isolation dielectric layer, 12 is the ohmic contact alloy layer, and 13 is the front electrode metal layer. DETAILED DESCRIPTION
[0020] The present invention is described in detail below in conjunction with specific implementation cases. Examples of the embodiments are shown in the accompanying drawings, and the schematic implementation methods and descriptions of the present invention are only used to explain the present invention and are not intended to limit the present invention.
[0021] A method for preparing a double-trench SiC MOSFET device comprises the following steps: S100, refer to Figure 1 As shown, an N-epitaxial layer 2 is epitaxially grown on an N+ substrate layer 1; and a shallowly doped PW region 3 is formed on the N-epitaxial layer 2 by Al ion implantation, as shown in FIG. Figure 2 As shown; PW region 3 doping concentration range 1E 17 cm -2 -1E 18 cm -2 , the doping depth is 0.8-1.5um.
[0022] S200, refer to Figure 3 As shown, a gate trench region 4 extending to below the PW region 3 is formed on the PW region 3 by etching; Specifically, the gate trench region 4 has a depth of 1-1.8 um.
[0023] S300, refer to Figure 4 As shown, a P+ region 5 is formed in the middle of the top surface of the PW region 3 by multiple implantation of Al ions; P+ zone 5 concentration range 1E 18 cm -2 -1E 19 cm -2 ; The injection depth of the P+ region 5 is the same as the injection depth of the PW region 3, that is, the injection depth of the P+ region 5 is 0.8-1.5um.
[0024] S400, refer to Figure 5 As shown, in the PW region 3, N+ regions 6 are formed by multiple N ion implantations on both sides of the P+ region 5; The concentration range of N+ region 6 is 1E 18 cm -2 -5E 18 cm -2 The implantation depth is 0.4-0.8um, and then a layer of carbon film is deposited on the surface of the device. It is annealed at a high temperature of 1650℃-1690℃ for 15 minutes to activate the implanted ions, and then the carbon film is removed; the side of the N+ region 6 is connected to the P+ region 5, and the implantation depth is less than the implantation depth of the P+ region 5.
[0025] S500, refer to Figure 6 As shown, a source trench region 7 is formed on the P+ region 5 by etching; The bottom of the source trench region 7 is higher than the bottom surface of the P+ region 5 . In this embodiment, the depth of the source trench region 7 is 0.4-0.9 um.
[0026] The depth of the source trench region 7 in step S500 is 0.5-0.6 times the implantation depth of the P+ region 5, which can reduce the on-resistance and improve the withstand voltage capability of the device. S600, refer to Figure 7 As shown, an ohmic metal is formed on the inner side wall of the source trench region 7 by sputtering and depositing Ni metal, and then annealed at a high temperature of 1000° C. for 5 minutes to form an ohmic contact alloy 8, and form an ohmic contact with the P+ region 5; The ohmic contact alloy 8 in step S600 is only deposited on the two side walls of the source trench region 7, which is beneficial to the freewheeling of the device.
[0027] S700, reference Figure 8 As shown, a gate oxide layer 9 is deposited on the sidewall and bottom of the gate trench region 4 by using the LPCVD method; The thickness of the gate oxide layer 9 in step S700 is 60 nm-70 nm, which further improves the robustness of the gate oxide layer.
[0028] S800, reference Fig. 9As shown, polysilicon is deposited in the gate trench region 4 by LPCVD to form a Poly layer 10, which is used as a gate electrode lead; S900, refer to Fig.10 As shown, an isolation dielectric layer 11 is formed on the N-epitaxial layer 2 by depositing oxide; The isolation dielectric layer 11 in the middle region overlaps the upper ends of the two N+ regions 6 on both sides, and the overlapping distance is not set and is adjusted according to actual process conditions.
[0029] S1000, refer to Fig.11 As shown, an ohmic metal layer is formed on the side of the isolation dielectric layer 11 by Ni metal sputtering deposition, and then annealed at a high temperature of 1000° C. for 5 minutes to form an ohmic contact alloy layer 12, which forms an ohmic contact with the upper part of the P+ region 5 and the N+ region 6; S1100, reference Fig.12 As shown, a front electrode metal layer 13 is formed on the isolation dielectric layer 11, the ohmic contact alloy layer 12 and in the source trench region 7 by Al metal sputtering, which is used as a source electrode lead; The front electrode metal layer 13 needs to fill the entire source trench region 7 , and the ohmic contact alloy 8 on both side walls of the source trench region 7 is in contact with the front electrode metal layer 13A1.
[0030] The PW region 3, the P+ region 5 and the N+ region 6 have the same potential, thereby enhancing the voltage resistance and short-circuit tolerance of the device.
[0031] A double-trench SiC MOSFET device, comprising, from bottom to top, an N+ substrate layer 1, an N- epitaxial layer 2, a PW region 3 and a front electrode metal layer 13; The PW region 3 is divided into several regions by the provision of a plurality of gate trench regions 4; Each area has PW zone 3 with: A P+ region 5 extends downward from the middle of the top surface of the PW region 3; The N+ region 6 extends downward from the top surface of the PW region 3 along the side of the P+ region 5; a gap is provided between the bottom surface of the N+ region 6 and the bottom surface of the PW region 3; Ohmic contact alloy 8, arranged on the inner side wall of source trench region 7 in P+ region 5; The inner sidewall and the bottom of the gate trench region 4 are provided with a gate oxide layer 9 respectively; the bottom surface of the gate oxide layer 9 is lower than the bottom surface of the PW region 3; the gate trench region 4 is filled with a Poly layer 10 on the gate oxide layer 9; A plurality of isolation dielectric layers 11 are provided on the PW region 3 at intervals; the bottom surfaces of the isolation dielectric layers 11 are connected to the N+ region 6, the gate oxide layer 9 and the Poly layer 10 respectively; An ohmic contact alloy layer 12 connected to the side of the isolation dielectric layer 11 is provided; the bottom surface of the ohmic contact alloy layer 12 is connected to the N+ region 6 and the P+ region 5 respectively; The bottom of the front electrode metal layer 13 extends into the source trench region 7 and is connected to the isolation dielectric layer 11 , the ohmic contact alloy layer 12 , the P+ region 5 and the ohmic contact alloy 8 respectively.
[0032] Regarding the contents disclosed in this case, there are a few points that need to be explained: (1) The drawings of the embodiments disclosed in this case only involve the structures involved in the embodiments disclosed in this case. For other structures, please refer to the general reference; (2) In the absence of conflict, the embodiments and features of the embodiments disclosed in this case may be combined with each other to obtain new embodiments; The above are only specific implementation methods disclosed in this case, but the protection scope of the present disclosure is not limited thereto. The protection scope disclosed in this case shall be based on the protection scope of the claims.
Claims
1. A method for preparing a double-trench SiC MOSFET device, It is characterized in that The steps include: S100, forming an N-epitaxial layer (2) and a PW region (3) on the N+ substrate layer (1); S200, etching on the PW region (3) to form a plurality of gate trench regions (4) arranged at intervals; S300, forming a P+ region (5) on the PW region (3) by Al ion implantation, and forming an N+ region (6) on the side of the P+ region (5) by ion implantation; S400, forming a source trench region (7) on the P+ region (5) by etching, and forming an ohmic contact alloy (8) on the inner side wall of the source trench region (7); S500, depositing a gate oxide layer (9) on the sidewall and bottom of the gate trench region (4), and filling it with a Poly layer (10) to serve as a gate electrode lead; S600, forming an isolation dielectric layer (11) on the N-epitaxial layer (2); and forming an ohmic contact alloy layer (12) on the side of the isolation dielectric layer (11) to form an ohmic contact with the upper part of the P+ region (5) and the N+ region (6); S700, forming a front electrode metal layer (13) on the isolation dielectric layer (11), the ohmic contact alloy layer (12) and in the source trench region (7) by means of Al metal sputtering, as a source electrode lead.
2. A method for preparing a double-trench SiC MOSFET device according to claim 1, It is characterized in that The doping concentration of the PW region (3) is in the range of 1E 17 cm -2 -1E 18 cm -2 , the doping depth is 0.8-1.5um.
3. A method for preparing a double-trench SiC MOSFET device according to claim 1, It is characterized in that The gate trench region (4) has a depth of 1-1.8 um.
4. A method for preparing a double-trench SiC MOSFET device according to claim 1, It is characterized in that The concentration range of the P+ region (5) is 1E 18 cm -2 -1E 19 cm -2 ; The implantation depth of the P+ region (5) is the same as the implantation depth of the PW region (3).
5. The method for preparing a double-trench SiC MOSFET device according to claim 1, It is characterized in that The concentration range of the N+ region (6) is 1E 18 cm -2 -5E 18 cm -2 , the injection depth is 0.4-0.8um.
6. A method for preparing a double-trench SiC MOSFET device according to claim 1, It is characterized in that The depth of the source trench region (7) is 0.4-0.9 um.
7. The method for preparing a double-trench SiC MOSFET device according to claim 1, It is characterized in that The gate oxide layer (9) has a thickness of 60nm-70nm.
8. The method for preparing a double-trench SiC MOSFET device according to claim 1, It is characterized in that The PW region (3), the P+ region (5) and the N+ region (6) have the same potential.
9. The method for preparing a double-trench SiC MOSFET device according to claim 1, It is characterized in that The front electrode metal layer (13) fills the source trench region (7), and the ohmic contact alloy (8) on the side walls of the source trench region (7) is in contact with Al of the front electrode metal layer (13).
10. A double-trench SiC MOSFET device, comprising: a double-trench SiC MOSFET device prepared according to the method for preparing a double-trench SiC MOSFET device according to any one of claims 1 to 9; It is characterized in that It comprises, from bottom to top, an N+ substrate layer (1), an N- epitaxial layer (2), a PW region (3) and a front electrode metal layer (13); The PW region (3) is divided into a plurality of regions by providing a plurality of gate trench regions (4); The PW area (3) of each region is provided with: A P+ region (5) extending downward from the middle of the top surface of the PW region (3); An N+ region (6) extends downward from the top surface of the PW region (3) along the side of the P+ region (5); a gap is provided between the bottom surface of the N+ region (6) and the bottom surface of the PW region (3); An ohmic contact alloy (8) is arranged on the inner side wall of the source trench region (7) in the P+ region (5); The inner sidewalls and the bottom of the gate trench region (4) are respectively provided with a gate oxide layer (9); the bottom surface of the gate oxide layer (9) is lower than the bottom surface of the PW region (3); and the gate trench region (4) is filled with a Poly layer (10) on the gate oxide layer (9); A plurality of isolation dielectric layers (11) are arranged at intervals on the PW region (3); the bottom surfaces of the isolation dielectric layers (11) are respectively connected to the N+ region (6), the gate oxide layer (9) and the Poly layer (10); An ohmic contact alloy layer (12) connected to the side of the isolation dielectric layer (11); the bottom surface of the ohmic contact alloy layer (12) is respectively connected to the N+ region (6) and the P+ region (5); The bottom of the front electrode metal layer (13) extends into the source trench region (7) and is respectively connected to the isolation dielectric layer (11), the ohmic contact alloy layer (12), the P+ region (5) and the ohmic contact alloy (8).