Manufacturing method of golden finger structure

Through improved vacuum lamination and etching steps, the wet film step is omitted, and the manufacturing method of the golden finger structure is optimized, which solves the problem of long and high cost in the existing technology, and achieves the effect of process shortening and cost reduction.

CN118804502AActive Publication Date: 2024-10-18JIANDING (HUBEI) ELECTRONICS CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202410606429.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-05-15
Publication Date
2024-10-18
Estimated Expiration
2044-05-15

AI Technical Summary

Technical Problem

In the existing gold finger structure manufacturing method, repeated wet film and dry film steps result in low production efficiency and high cost. There is a need for a method that can shorten the process and save production time.

Method used

An improved manufacturing method is adopted, including a pre-step, a first vacuum lamination step, a gold plating step, a first removal step, a second vacuum lamination step and an etching step, eliminating the wet film step and using vacuum lamination technology. Optimize the processing of metal lines to form a golden finger structure.

Benefits of technology

It effectively shortens the manufacturing process, saves production time, reduces production costs, and improves production efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118804502A_ABST
    Figure CN118804502A_ABST
Patent Text Reader

Abstract

The invention discloses a manufacturing method of a golden finger structure, which comprises a preposition step of providing a board body and a circuit layer, and the circuit layer comprises a metal circuit with a main body circuit section and a tail end circuit section; a first vacuum film pressing step: performing vacuum film pressing on the part of the tail end circuit section by a first shielding film, so that the tail end circuit section comprises a first tail end circuit part and a second tail end circuit part, and the second tail end circuit part is covered by the first shielding film; a gold plating step: plating a gold plating film on the outer surfaces of the main body circuit section and the first tail end circuit part; a first removing step: removing the first shielding film; a second vacuum film pressing step: performing vacuum film pressing on a second shielding film on the part of the metal circuit, so that the part of the second tail end circuit part is exposed out of the second shielding film; and an etching step: removing a part of the second tail end circuit part. Therefore, the manufacturing method of the golden finger structure can completely omit the execution of a wet film step, so that the manufacturing process is shortened, the production time is saved, and the production cost is further reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a method for manufacturing a gold finger structure, and in particular to a method for manufacturing a gold finger structure which can effectively shorten the manufacturing process. Background Art

[0002] In the existing manufacturing method of the gold finger structure, it is necessary to repeatedly perform the wet film step and the dry film step to form the existing gold finger structure. However, the process of repeating the wet film step and the dry film step takes a long time, thereby causing the problems of low production efficiency and high production cost. Therefore, how to provide a method that can shorten the process and save production time, thereby reducing production costs, and improve the defects of the existing manufacturing method of the gold finger structure has become one of the important issues that the industry wants to solve.

[0003] Therefore, the inventors believe that the above defects can be improved, and have devoted themselves to research and applied scientific principles, and finally proposed the present invention which has a reasonable design and effectively improves the above defects. Summary of the invention

[0004] The embodiment of the present invention provides a method for manufacturing a gold finger structure, which can effectively improve the defects that may occur in the existing gold finger structure.

[0005] The embodiment of the present invention discloses a method for manufacturing a gold finger structure, which comprises: a pre-step: providing a board and a circuit layer formed on the board; wherein the circuit layer comprises: a plurality of metal circuits, each of which comprises a main circuit segment and an end circuit segment connected to the main circuit segment; a first vacuum lamination step: vacuum laminating a first shielding film on a portion of the end circuit segment of each metal circuit, so that the end circuit segment of each metal circuit comprises a first end circuit portion connected to the main circuit segment and a second end circuit portion connected to the first end circuit portion; wherein the second end circuit portion is covered by the first shielding film. The invention relates to a method of covering a metal circuit with a gold-plated film; a gold-plating step: plating a gold-plated film on the outer surface of the main circuit segment of each metal circuit and the outer surface of the first end circuit portion of the end circuit segment; a first removing step: removing the first shielding film to expose the second end circuit portion to the gold-plated film; a second vacuum lamination step: vacuum laminating a second shielding film on the main circuit segment and part of the end circuit segment of each metal circuit to expose part of the second end circuit portion of the end circuit segment of each metal circuit to the second shielding film; and an etching step: removing the part of the second end circuit portion exposed to the second shielding film to form a gold finger structure.

[0006] Preferably, in the preliminary step, each metal circuit also includes a connecting circuit segment; and in the first vacuum lamination step, a first shielding film is also vacuum-laminated to cover a portion of the connecting circuit segment of each metal circuit, so that the connecting circuit segment of each metal circuit includes a first connecting circuit portion connected to the main circuit segment and a second connecting circuit portion connected to the first connecting circuit portion; wherein the second connecting circuit portion is covered by the first shielding film.

[0007] Preferably, in the gold plating step, a gold plating film is also plated on the outer surface of the first connecting line portion of the connecting line segment of each metal line.

[0008] Preferably, in the first removing step, the first masking film is removed so that the second connecting circuit portion and the second terminal circuit portion are exposed to the gold-plated film.

[0009] Preferably, in the second vacuum lamination step, a second masking film is also vacuum-laminated to cover the connecting line section of each metal line.

[0010] Preferably, after the etching step, a second removing step is further included to remove the second masking film.

[0011] Preferably, in the preceding step, an insulating outer layer covering the local circuit layer is further provided; wherein each of the plurality of metal circuits includes an inner circuit buried in the insulating outer layer, and the inner circuit is electrically coupled to the connecting circuit segment.

[0012] Preferably, after the etching step, there is a distance between the end line segment of each metal line and the edge of the board along a longitudinal direction.

[0013] Preferably, after the etching step, a length of the end line segment in a longitudinal direction is 0.1 mm to 0.15 mm.

[0014] Preferably, in the first vacuum lamination step, the first masking film is vacuum-laminated at a lamination temperature of 60 to 70 degrees at the end line segment of each metal line, a pressurization time is between 15 seconds and 20 seconds, and a vacuuming time is between 10 seconds and 30 seconds.

[0015] Preferably, in the second vacuum lamination step, the second masking film is vacuum laminated on the main line segment and the end line segment of each metal line at a lamination temperature between 60 degrees and 70 degrees, a pressurization time between 15 seconds and 20 seconds, and a vacuuming time between 10 seconds and 30 seconds.

[0016] In summary, the manufacturing method of the gold finger structure disclosed in the embodiment of the present invention is improved compared to the existing manufacturing method of the gold finger structure by a first vacuum lamination step and a second vacuum lamination step, and the execution of the wet film step is completely omitted, thereby providing a manufacturing method of the gold finger structure that can shorten the process and save production time, thereby reducing production costs.

[0017] To further understand the features and technical contents of the present invention, please refer to the following detailed description and drawings of the present invention. However, such description and drawings are only used to illustrate the present invention and are not intended to limit the protection scope of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] Figure 1 It is a top view schematic diagram of the gold finger structure of an embodiment of the present invention.

[0019] Figure 2 for Figure 1 Schematic cross-section along section line II-II.

[0020] Figure 3 The figure is a flow chart of a method for manufacturing a gold finger structure according to an embodiment of the present invention.

[0021] Figure 4 Schematic diagram of the preparatory steps of the method for manufacturing the gold finger structure according to an embodiment of the present invention.

[0022] Figure 5 Schematic diagram of the first vacuum lamination step of the method for manufacturing the gold finger structure according to an embodiment of the present invention.

[0023] Figure 6 Schematic diagram of the gold plating steps of the method for manufacturing the gold finger structure according to an embodiment of the present invention.

[0024] Figure 7 It is a schematic diagram of the first removing step of the method for manufacturing the gold finger structure according to an embodiment of the present invention.

[0025] Figure 8 Schematic diagram of the second vacuum lamination step of the method for manufacturing the gold finger structure according to an embodiment of the present invention.

[0026] Fig. 9 Schematic diagram of etching steps of a method for manufacturing a gold finger structure according to an embodiment of the present invention.

[0027] Fig.10 It is a schematic diagram of the second removing step of the method for manufacturing the gold finger structure according to an embodiment of the present invention. DETAILED DESCRIPTION

[0028] The following is an explanation of the implementation method of the "method for manufacturing a gold finger structure" disclosed in the present invention through specific embodiments. Those skilled in the art can understand the advantages and effects of the present invention from the contents disclosed in this specification. The present invention can be implemented or applied through other different specific embodiments, and the details in this specification can also be modified and changed based on different viewpoints and applications without departing from the concept of the present invention. In addition, the drawings of the present invention are only simple schematic illustrations and are not depicted according to actual dimensions. It is stated in advance. The following implementation methods will further explain the relevant technical contents of the present invention in detail, but the disclosed contents are not intended to limit the scope of protection of the present invention.

[0029] It should be understood that, although the terms "first", "second", "third", etc. may be used herein to describe various components or signals, these components or signals should not be limited by these terms. These terms are mainly used to distinguish one component from another component, or one signal from another signal. In addition, the term "or" used herein may include any one or more combinations of the associated listed items depending on the actual situation.

[0030] See also Figures 1 to 10 It should be noted that the numbers and shapes mentioned in the accompanying drawings are only used to specifically illustrate the implementation of the present invention, so as to facilitate understanding of the content of the present invention, and are not used to limit the protection scope of the present invention.

[0031] This embodiment discloses a method S100 for manufacturing a gold finger structure, which manufactures a gold finger structure 100. The gold finger structure 100 includes a board 1, an insulating outer layer 2 formed on the board 1, a circuit layer 3 formed on the board 1, and a plurality of gold-plated films 4 covering a portion of the circuit layer 3.

[0032] See also Figure 1 and Figure 2 As shown, in this embodiment, the board body 1 is a multi-layer circuit board, but the present invention is not limited thereto. The board body 1 is, for example, a rectangle, but the present invention is not limited thereto. For example, in other embodiments not shown in the present invention, the board body 1 may also be a square, etc. The edge of the board body 1 includes two first short sides A1 facing each other and two first long sides B1 facing each other. For the convenience of explanation, the gold finger structure 100 is defined as a lateral direction W parallel to the two first short sides A1 and a longitudinal direction L parallel to the two first long sides B1. In actual application, the main function of the board body 1 is to support the insulating outer layer 2, the circuit layer 3 and other components, etc. Therefore, the appearance, size, material and other related properties of the board body 1 can be changed according to needs, and are not limited in this embodiment.

[0033] In addition, the plate 1 is close to Figure 1 The lower end is defined as a free end 1a. In practical applications, the free end 1a of the plate body 1 can be used to plug into a matching component, a slot or other related components. It should be noted that the gold finger structure 100 disclosed in this embodiment can also be matched with related components, and relevant personnel can also adjust the related components of the gold finger structure 100 accordingly. In other words, the gold finger structure 100 of this embodiment does not limit the matching with related components or the corresponding adjustment of the structure.

[0034] like Figure 1 and Figure 2 As shown, the insulating outer layer 2 is formed on the plate body 1. In the present embodiment, the insulating outer layer 2 is, for example, a rectangle, but the present invention is not limited thereto. For example, in other embodiments not shown in the present invention, the insulating outer layer 2 may also be a square, etc. The insulating outer layer 2 includes two second short sides A2 facing each other and two second long sides B2 facing each other. In addition, the two second short sides A2 of the insulating outer layer 2 are parallel to the longitudinal direction L and the two second long sides B2 of the insulating outer layer 2 are parallel to the transverse direction W. In detail, in the present embodiment, the insulating outer layer 2 is formed on the plate body 1 and adjacent to Figure 1 above.

[0035] In addition, the shape, size, quantity, material, position formed on the board 1 and other related properties of the insulating outer layer 2 can be changed according to design requirements. For example, the insulating outer layer 2 can be a resin material, such as polyimide, polyester, polyethylene glycol, polytetrafluoroethylene, epoxy resin or aramid.

[0036] The circuit layer 3 is formed on the board 1. In this embodiment, the material of the circuit layer 3 can be a conductive material, such as copper or silver, but the present invention is not limited thereto. For example, the material of the circuit layer 3 can be changed according to actual design requirements.

[0037] In addition, the circuit layer 3 includes a plurality of metal circuits 31 arranged along the transverse direction W. Specifically, the plurality of metal circuits 31 are generally parallel to the longitudinal direction L. However, the plurality of metal circuits 31 are not limited to being parallel to the longitudinal direction L and the arrangement direction of the plurality of metal circuits 31 can be changed according to actual design requirements, not limited to this embodiment. In addition, the plurality of metal circuits 31 are arranged spaced apart from each other along the transverse direction W, and the distance between any two adjacent metal circuits 31 can be changed according to design requirements.

[0038] Furthermore, in this embodiment, each metal line 31 is rectangular in shape, but the present invention is not limited thereto. For example, in other embodiments not shown in the present invention, the shape of each metal line 31 can be square, trapezoidal, or can be changed according to actual design requirements.

[0039] In this embodiment, the circuit layer 3 may also include a plurality of inner circuits 32. The plurality of inner circuits 32 are buried in the insulating outer layer 2, and the plurality of inner circuits 32 are arranged at intervals from each other in the attached drawings of this embodiment and are electrically connected to the plurality of metal circuits 31, respectively. The plurality of inner circuits 32 are generally parallel to the longitudinal direction L, but the present invention is not limited thereto. For example, in other embodiments not shown in the present invention, the plurality of inner circuits 32 can be tilted 45 degrees respectively and electrically connected to other components in the board body 1. In detail, the plurality of inner circuits 32 can be changed according to actual design requirements.

[0040] In this embodiment, the circuit layer 3 may also include a transverse circuit 33. In the drawings of this embodiment, the transverse circuit 33 is generally parallel to the transverse direction W and is buried in the insulating outer layer 2. However, the transverse circuit 33 is not limited to being parallel to the transverse direction W and the direction of the transverse circuit 33 can be changed according to needs and is not limited to this embodiment. In addition, the transverse circuit 33 connects the plurality of metal circuits 31 arranged at intervals along the transverse direction W. In detail, the transverse circuit 33 is electrically connected to the plurality of inner circuits 32 arranged at intervals along the transverse direction W, and the plurality of inner circuits 32 are electrically connected to the plurality of metal circuits 31 respectively.

[0041] Please refer to Figure 1 and Figure 2 Each of the metal lines 31 includes a connecting line segment 311 , a main line segment 312 electrically connected to the connecting line segment 311 , and an end line segment 313 electrically connected to the main line segment 312 .

[0042] The connecting line segment 311 is electrically connected to the inner line 32. Specifically, the connecting line segment 311 is electrically connected to the inner line 32 along the longitudinal direction L. The connecting line segment 311 is rectangular in this embodiment, but the present invention is not limited thereto. For example, in other embodiments not shown in the present invention, the shape of the connecting line segment 311 may also be square or may be changed according to actual design requirements.

[0043] In this embodiment, the connection line segment 311 includes a first connection line portion 3111 and a second connection line portion 3112 electrically connected to the first connection line portion 3111. The first connection line portion 3111 is buried in the gold-plated film 4. In other words, the second connection line portion 3112 is covered by the gold-plated film 4. The second connection line portion 3112 is electrically connected to the inner circuit 32 and is exposed to the insulating outer layer 2 and the gold-plated film 4.

[0044] like Figure 1 and Figure 2 As shown, in this embodiment, the main line segment 312 is electrically connected to the first connection line portion 3111 of the connection line segment 311 on one side adjacent to the insulating outer layer 2. The main line segment 312 is in a rectangular shape, but the present invention is not limited thereto. For example, in other embodiments not shown in the present invention, the shape of the main line segment 312 may also be a square, or may be changed according to actual design needs. The main line segment 312 is buried in the gold-plated film 4. In other words, the main line segment 312 is covered by the gold-plated film 4.

[0045] In this embodiment, the end line segment 313 is electrically connected to the main line segment 312. Specifically, the end line segment 313 is electrically connected to the main line segment 312 along the longitudinal direction L. The shape of the end line segment 313 in this embodiment is a rectangle, but the present invention is not limited thereto. For example, in other embodiments not shown in the present invention, the shape of the end line segment 313 may also be a square or may be changed according to actual design requirements.

[0046] In detail, the end circuit section 313 includes a first end circuit portion 3131 and a second end circuit portion 3132 electrically connected to the first end circuit portion 3131. The first end circuit portion 3131 is electrically connected to the main circuit section 312, and the first end circuit portion 3131 is buried in the gold-plated film 4. In other words, the first end circuit portion 3131 is covered by the gold-plated film 4. The second end circuit portion 3132 is exposed from the gold-plated film 4.

[0047] like Figure 1 and Figure 2As shown, the plurality of gold-plated films 4 are respectively plated on the outer surfaces of the first connecting line portion 3111, the main line segment 312, and the first terminal line portion 3131 of the plurality of metal lines 31. In this embodiment, the plurality of gold-plated films 4 are separated from each other, and the surface size of any one of the gold-plated films 4 can be equal to the outer surface size of the first connecting line portion 3111, the outer surface size of the main line segment 312, and the outer surface size of the first terminal line portion 3131 on which it is plated. Furthermore, the number of the plurality of gold-plated films 4 is equal to the number of the plurality of metal lines. However, the size and number of the plurality of gold-plated films 4 can be adjusted and changed according to actual design requirements, and are not limited to this embodiment.

[0048] See also Figures 3 to 10 As shown, this embodiment discloses a method S100 for manufacturing a gold finger structure, and the method S100 for manufacturing a gold finger structure includes a pre-step S110, a first vacuum lamination step S120, a gold plating step S130, a first removal step S140, a second vacuum lamination step S150, an etching step S160, and a second removal step S170. However, the gold finger structure 100 of this embodiment can be manufactured by the above-mentioned manufacturing method, but the present invention is not limited thereto. Furthermore, when implementing the method S100 for manufacturing a gold finger structure, the present invention is not limited to the content and order of the above-mentioned steps.

[0049] The following will describe the various steps of the gold finger structure manufacturing method S100 of this embodiment. For the structure of each part of the gold finger structure 100 or other related features, please refer to the related introduction of the first embodiment, which will not be described in detail below.

[0050] It should be noted that, in order to facilitate the understanding of this embodiment, the accompanying drawings only present a single gold finger structure in the gold finger structure 100, so as to clearly present the various steps in the gold finger structure manufacturing method, but the present invention is not limited to the accompanying drawings. The various steps of the gold finger structure manufacturing method S100 will be introduced separately below.

[0051] like Figure 3 and Figure 4 As shown, the pre-step S110 provides the board body 1 and the circuit layer 3 (such as Figure 2 ). The circuit layer 3 includes a plurality of metal circuits 31. Each of the metal circuits 31 includes a connecting circuit segment 311, a main circuit segment 312 connected to the connecting circuit segment 311, and an end circuit segment 313 connected to the main circuit segment 312.

[0052] It should be noted that the preceding step S110 further provides the insulating outer layer 2 covering a portion of the circuit layer 3. Each of the metal circuits 31 includes the inner circuit 32 buried in the insulating outer layer 2, and the inner circuit 32 is electrically coupled to the connecting circuit segment 311.

[0053] like Figure 3 and Figure 5 As shown, the first vacuum lamination step S120 is to vacuum laminate a first masking film 5a on a portion of the connecting line segment 311 and a portion of the terminal line segment 313 of each metal line 31. That is, a portion of the connecting line segment 311 is vacuum laminated by the first masking film 5a, so that the connecting line segment 311 of each metal line 31 includes the first connecting line portion 3111 connected to the main line segment 312 and the second connecting line portion 3112 connected to the first connecting line portion 3111. The second connecting line portion 3112 is covered by the first masking film 5a. A portion of the terminal line segment 313 is vacuum laminated by the first masking film 5a, so that the terminal line segment 313 of each metal line 31 includes the first terminal line portion 3131 connected to the main line segment 312 and the second terminal line portion 3132 connected to the first terminal line portion 3131. Wherein, the second terminal line portion 3132 is covered by the first masking film 5a.

[0054] It should be noted that in the first vacuum lamination step S120, a laminator (not shown) is used to pressurize the first masking film 5a on the second connection circuit portion 3112 and the second terminal circuit portion 3132 of the metal circuit 31 by vacuum heating. The laminator is used in the vacuum lamination process at a lamination temperature between 60 degrees and 70 degrees, a pressurization time between 15 seconds and 20 seconds, and a vacuuming time between 10 seconds and 30 seconds, so as to optimize the lamination effect and avoid the problem of gold penetration in the subsequent gold plating step S130.

[0055] In addition, in the first vacuum lamination step S120, the present embodiment is not limited to vacuum laminating the first masking film 5a on the second connection circuit portion 3112 of the metal circuit 31. In other words, the first masking film 5a may not be vacuum laminating on the second connection circuit portion 3112 of the metal circuit 31 according to design requirements.

[0056] like Figure 3 and Figure 6As shown, in the gold plating step S130, the gold plating film 4 is plated on the outer surface of the first connecting line portion 3111 of the connecting line segment 311 of each of the metal lines 31, the outer surface of the main line segment 312, and the outer surface of the first end line portion 3131 of the end line segment 313.

[0057] like Figure 3 and Figure 7 As shown, the first removing step S140 removes the first shielding film 5a so that the second terminal circuit portion 3132 is exposed to the gold-plated film 4. It should be particularly noted that in order for the gold-plating step S130 to plate the gold-plated film 4 on the predetermined position on the metal circuit 31, the first shielding film 5a is used to cover the position on the metal circuit 31 that does not need to be plated with gold, so as to avoid being plated with the gold-plated film 4. For this reason, after the gold-plating step S130, the first shielding film 5a must be removed by the first removing step S140.

[0058] like Figure 3 and Figure 8 As shown, the second vacuum lamination step S150 is to vacuum laminate a second masking film 5b on the connecting line segment 311, the main line segment 312 and the end line segment 313 of each of the metal lines 31, so that the second end line portion 3132 of the end line segment 313 of each of the metal lines 31 is exposed to the second masking film 5b.

[0059] Specifically, the second masking film 5b covers a portion of the second end line portion 3132 of the end line segment 313 of each of the metal lines 31, so that the portion of the second end line portion 3132 exposed by the second masking film 5b is defined as a sacrificial portion 3132' for removal in the subsequent etching step S160.

[0060] It should be noted that in the second vacuum lamination step S150, a laminator is used to pressurize the second masking film 5b on the connecting line segment 311, the main line segment 312 and the terminal line segment 313 of the metal line 31 by vacuum heating. The laminator is used in the vacuum lamination process at a lamination temperature of 60 to 70 degrees, a pressurization time of 15 to 20 seconds, and a vacuuming time of 10 to 30 seconds, so as to optimize the lamination effect and avoid the problem of gold penetration in the subsequent gold plating step S130.

[0061] like Figure 3 and Fig. 9As shown, the etching step S160 removes the portion of the second terminal line portion 3132 exposed to the second shielding film 5b. In other words, the etching step S160 removes the sacrificial portion 3132' of the second terminal line portion 3132. It should be particularly noted that after the etching step S160, the length of the terminal line segment 313 in the longitudinal direction L is 0.1 mm to 0.15 mm, but the present invention is not limited thereto.

[0062] In addition, in this embodiment, after the etching step S160 , there is a distance along the longitudinal direction L between the end line segment 313 of each of the metal lines 31 and the edge of the board 1 (ie, the free end 1 a ).

[0063] like Figure 3 and Fig.10 As shown, the second removing step S170 removes the second masking film 5 b to form the gold finger structure 100 .

[0064] [Technical Effects of Embodiments of the Invention]

[0065] In summary, the manufacturing method of the gold finger structure disclosed in the embodiment of the present invention is improved compared to the existing manufacturing method of the gold finger structure through a first vacuum lamination step and a second vacuum lamination step, and the execution of the wet film step can be completely omitted, thereby providing a manufacturing method of the gold finger structure that can shorten the process and save production time, thereby reducing production costs.

[0066] The contents disclosed above are only preferred feasible embodiments of the present invention, and are not intended to limit the patent scope of the present invention. Therefore, all equivalent technical changes made using the contents of the present invention's specification and drawings are included in the patent scope of the present invention.

Claims

1. A method for manufacturing a gold finger structure, characterized in that: The manufacturing method of the gold finger structure comprises: A pre-step: providing a board and a circuit layer formed on the board; wherein the circuit layer comprises: a plurality of metal circuits, each of the metal circuits comprises a main circuit segment and an end circuit segment connected to the main circuit segment; a first vacuum lamination step: vacuum laminating a first shielding film on the end line segment of each metal line, so that the end line segment of each metal line includes a first end line portion connected to the main line segment and a second end line portion connected to the first end line portion; wherein the second end line portion is covered by the first shielding film; a gold plating step: plating a gold plating film on the outer surface of the main line segment of each of the metal lines and the outer surface of the first end line portion of the end line segment; a first removing step: removing the first shielding film to expose the second terminal circuit portion to the gold-plated film; a second vacuum lamination step: vacuum laminating a second masking film on the main line segment and the end line segment of each of the metal lines, so that the second end line portion of the end line segment of each of the metal lines is exposed to the second masking film; and An etching step is to remove the portion of the second end circuit portion exposed by the second shielding film to form a gold finger structure.

2. The method for manufacturing a gold finger structure according to claim 1, characterized in that: In the preceding step, each of the metal circuits also includes a connecting circuit segment; and in the first vacuum lamination step, the first shielding film is also vacuum-laminated to cover a portion of the connecting circuit segment of each of the metal circuits, so that the connecting circuit segment of each of the metal circuits includes a first connecting circuit portion connected to the main circuit segment and a second connecting circuit portion connected to the first connecting circuit portion; wherein the second connecting circuit portion is covered by the first shielding film.

3. The method for manufacturing a gold finger structure according to claim 2, characterized in that: In the gold plating step, the gold plating film is also plated on the outer surface of the first connecting line portion of the connecting line segment of each of the metal lines.

4. The method for manufacturing a gold finger structure according to claim 3, characterized in that: In the first removing step, the first shielding film is removed to expose the second connecting circuit portion and the second terminal circuit portion to the gold-plated film.

5. The method for manufacturing a gold finger structure according to claim 4, characterized in that: In the second vacuum lamination step, the second masking film is also vacuum-laminated to cover the connecting line segment of each of the metal lines.

6. The method for manufacturing a gold finger structure according to claim 1, characterized in that: A second removing step is also included after the etching step, and the second removing step removes the second shielding film.

7. The method for manufacturing a gold finger structure according to claim 2, characterized in that: In the preceding step, an insulating outer layer covering a portion of the circuit layer is also provided; wherein each of the plurality of metal circuits includes an inner circuit buried in the insulating outer layer, and the inner circuit is electrically coupled to the connecting circuit segment.

8. The method for manufacturing a gold finger structure according to claim 1, characterized in that: After the etching step, the end line segment of each of the metal lines is spaced from the edge of the board along a longitudinal direction.

9. The method for manufacturing a gold finger structure according to claim 1, characterized in that: After the etching step, the length of the end line segment in a longitudinal direction is 0.1 mm to 0.15 mm.

10. The method for manufacturing a gold finger structure according to claim 1, characterized in that: In the first vacuum lamination step, the first masking film is vacuum-laminated at a lamination temperature of 60 to 70 degrees at the end line segment of each of the metal lines, a pressurization time is between 15 seconds and 20 seconds, and a vacuuming time is between 10 seconds and 30 seconds.

11. The method for manufacturing a gold finger structure according to claim 1, characterized in that: In the second vacuum lamination step, the second masking film is vacuum laminated on the main line segment and the end line segment of each of the metal lines at a lamination temperature of 60 to 70 degrees, a pressurization time of 15 to 20 seconds, and a vacuuming time of 10 to 30 seconds.

Citation Information

Patent Citations

  • Film removing method for leadless gilt plate

    CN104582287A

  • Fabrication method of gold-plated finger board

    CN105451454A

  • Structure for manufacturing multi-sectional gold finger of circuit board

    TWM602294U