Preparation method of water-soluble oxide wound dressing
Through the manufacturing method of water-soluble oxide wound dressings, a heated electrolysis method and a magnetization reactor are used to prepare a dilute oxide salt aqueous solution, which is combined with polymers such as sodium alginate to form a sustained-release closed moisturizing environment, solving the problems in the existing technology. Rapid healing and infection control are achieved without the problems of long wound recovery times and damage during dressing changes.
Patent Information
- Application Number
- CN202410462994.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-04-17
- Filing Date
- 2024-04-17
- Publication Date
- 2024-10-22
Smart Images

Figure CN118806972A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a method for manufacturing a water-soluble oxide wound dressing, and in particular to a method for manufacturing a water-soluble oxide wound dressing capable of protecting active ingredients and achieving a sustained-release effect. Background Art
[0002] The skin is the largest organ in the human body. It is the soft layer that covers the vertebrates. The skin blocks foreign invasion and retains moisture. It has the functions of warmth, insulation and sensation. Therefore, when there are wounds on the skin, such as those caused by general trauma or bedsores, the skin will be adversely affected and unable to perform its normal functions.
[0003] There are many types of wound dressings available on the market. Usually, appropriate wound dressings are selected according to the different properties of the wound, and a good healing environment is provided for the wound, foreign matter is blocked, and various bacteria and viruses in the environment are prevented from invading the wound and causing infection. Secondly, the current treatment method for the wound is to first disinfect the wound and then apply ointment and wrap it with gauze, wait for the wound to heal on its own, and then remove the gauze and other external coating fixing materials. However, this method is for large-area wounds or wounded people (such as diabetic patients) who are difficult to recover due to physical problems. The recovery time of the wound is long and the dressing needs to be changed many times. When the gauze is removed during the dressing change, the wound is often subjected to external force and torn again due to the adhesion and combination of the covering materials such as gauze and the tissue fluid of the wound, causing the wound to be damaged again, and a longer healing time is required.
[0004] In view of this, the inventor is committed to combining moisturizing dressings with negative oxygen ions to form ionic gels to facilitate rapid wound healing. The inventor has invested a lot of energy and spirit in research and development, constantly making breakthroughs and innovations in this field, hoping to solve the shortcomings of existing methods with novel technical means, bring better products to society, and promote industrial development. Summary of the invention
[0005] The main purpose of the present invention is to provide a method for manufacturing a water-soluble oxide wound dressing. The water-soluble oxide wound dressing prepared by the manufacturing method is conducive to the dissolution of necrotic tissue and fibrin, and can promote the release of multiple growth factors in the exudate, thereby achieving the purpose of local moisturizing, reducing scab formation, avoiding mechanical damage to new granulation tissue, and reducing damage and pain when changing dressings. Secondly, the water-soluble oxide wound dressing of the present invention can form a closed moisturizing environment. The dressing forms a barrier to reduce the chance of wound infection, protect the nerve endings of the wound surface to reduce pain, and at the same time maintain a constant temperature of the wound surface, accelerate cell division to promote wound healing. The water-soluble oxide wound dressing can protect the active ingredients and achieve a sustained release effect.
[0006] To achieve the above-mentioned purpose of the present invention, the present invention provides a method for manufacturing a water-soluble oxide wound dressing, which comprises the following steps: first, providing distilled water or mineral water, and adding an oxide salt aqueous solution into the distilled water or the mineral water to form a diluted oxide salt aqueous solution, wherein the oxide salt aqueous solution is formed by passing high pressure oxygen into a crystalline salt solution by heating electrolysis, the oxide salt aqueous solution has a pH value of 5.5 to 8 and a volume molar concentration of 5 to 50 mol / L, and the heating temperature of the heating electrolysis method is controlled between 40 and 80°C. Secondly, the diluted oxide salt aqueous solution is passed through an activated carbon adsorption filter to remove trace hydrophobic harmful substances. Furthermore, the diluted oxide salt aqueous solution is introduced into a magnetization reactor through a flow control valve for a synthesis reaction, the magnetization reactor has a magnetic field of 0.1 to 1 Tesla and an electric field of 10 to 100 volts / cm, the synthesis temperature of the magnetization reactor is controlled between 10°C and 55°C, and the synthesis pressure is controlled between 6kg / cm 2 Up to 9kg / cm 2 The high pressure between 200°C and 250°C, and the synthesis time is 30 to 90 minutes to form concentrated active oxide water. In addition, the concentrated active oxide water is heated to 65 to 70°C, and the water-soluble polymer and the distilled water or the mineral water are added and stirred for 3.5 to 4.5 hours, and the stirring speed is controlled at 600 to 650 rpm, and then stirred for 5 to 6 hours under a vacuum state to form a water-soluble oxide wound dressing; wherein, based on the total weight percentage of the water-soluble oxide wound dressing, the water-soluble oxide wound dressing comprises: 45.0 to 55.0% of the distilled water or the mineral water, 15.0 to 25.0% of the oxide salt aqueous solution and 30.0 to 35.0% of the water-soluble polymer.
[0007] In the method for manufacturing the water-soluble oxide wound dressing of the present invention, preferably, the oxide salt aqueous solution has a volume molar concentration of 10-40 mol / L.
[0008] In the method for manufacturing the water-soluble oxide wound dressing of the present invention, preferably, the water-soluble polymer is sodium alginate, polyvinyl pyrrolidone, sodium carboxymethyl cellulose, hyaluronic acid or any combination thereof.
[0009] In the method for manufacturing the water-soluble oxide wound dressing of the present invention, preferably, based on the total weight percentage of the water-soluble oxide wound dressing, the water-soluble polymer comprises: 1.0-30.0% sodium alginate, 1.0-25.0% polyvinyl pyrrolidone and 1.0-25.0% sodium carboxymethyl cellulose.
[0010] In the method for manufacturing the water-soluble oxide wound dressing of the present invention, preferably, it further comprises an additive adding step, wherein the diluted oxide salt aqueous solution is introduced into an additive tank, and ozone is added into the additive tank for sterilization.
[0011] In the method for manufacturing the water-soluble oxide wound dressing of the present invention, preferably, the oxide salt aqueous solution is an aqueous solution composed of metal element cations and carbonate, sulfate, chromate, tungstate, molybdate, phosphate, arsenate or vanadate.
[0012] In the method for manufacturing the water-soluble oxide wound dressing of the present invention, preferably, the metal element cation comprises at least one divalent or trivalent metal cation, which is Fe 2+ , Cu 2+ 、Zn 2+ , Pb 2+ , Mn 2+ 、Bi 3+ or any combination thereof.
[0013] In the method for manufacturing the water-soluble oxide wound dressing of the present invention, preferably, the thickness of the water-soluble oxide wound dressing is greater than or equal to 0.1 mm and less than or equal to 4 mm.
[0014] In the method for manufacturing the water-soluble oxide wound dressing of the present invention, preferably, the flow control valve controls the flow rate of the small molecule water to 500-8000 L / min.
[0015] To achieve the above another object of the present invention, the present invention provides a water-soluble oxide wound dressing prepared by the above method for preparing the water-soluble oxide wound dressing. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 The present invention is a flow chart of a method for manufacturing a water-soluble oxide wound dressing;
[0017] Figure 2 A system for preparing the water-soluble oxide wound dressing according to Example 1 of the present invention;
[0018] Figure 3 A preparation system for the water-soluble oxide wound dressing according to Example 2 of the present invention;
[0019] Figure 4A This is a photo of the affected part of diabetic foot taken when the water-soluble oxide wound dressing of the present invention is not applied;
[0020] Figure 4B A photograph of the affected part of diabetic foot taken 2 days after applying the water-soluble oxide wound dressing of the present invention; and
[0021] Figure 4C This is a photo of the affected part of diabetic foot taken 7 days after the water-soluble oxide wound dressing of the present invention was applied.
[0022] Explanation of symbols
[0023] 11. Storage tank
[0024] 12 Activated carbon adsorption filter
[0025] 13 Electrolytic magnetization device
[0026] 14 Flow Control Valve
[0027] 15. Magnetization Reactor
[0028] 151 Water-soluble polymer
[0029] 16 Additive Slots DETAILED DESCRIPTION
[0030] The following is an explanation of the implementation of the present invention by means of specific embodiments. Those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. In addition, the present invention can also be implemented or applied by means of other different specific embodiments, and various modifications and changes can be made without departing from the spirit of the present invention.
[0031] Example 1
[0032] Please refer to Figure 1 and Figure 2 , Figure 1 is a flow chart of a method for manufacturing a water-soluble oxide wound dressing of the present invention; and Figure 2 This is a system for preparing the water-soluble oxide wound dressing according to Example 1 of the present invention.
[0033] like Figure 1 and Figure 2As shown, the present invention provides a method for manufacturing a water-soluble oxide wound dressing, the method comprising: step S101: providing distilled water or mineral water in a containing tank 11; step S102: adding an oxide salt aqueous solution into the distilled water or the mineral water to form a diluted oxide salt aqueous solution; wherein the oxide salt aqueous solution is formed by passing high pressure oxygen into a crystalline salt solution by heating electrolysis, and the oxide salt aqueous solution has a pH value of 5.5 to 8 and a volume molar concentration of 5 to 50 mol / L; the oxide salt aqueous solution is preferably The oxide salt aqueous solution preferably has a volume molar concentration of 10 to 40 mol / L, and the oxide salt aqueous solution preferably has a volume molar concentration of 15 to 35 mol / L, and the heating temperature of the heating electrolysis method is controlled between 40 and 80° C.; wherein the oxide salt aqueous solution is an aqueous solution composed of metal element cations and carbonate, sulfate, chromate, tungstate, molybdate, phosphate, arsenate or vanadate, and the metal element cations include at least one divalent or trivalent metal cation or any combination thereof, and the metal element cation is preferably Fe 2+ , Cu 2+ 、Zn 2+ , Pb 2+ , Mn 2+ Or Bi 3+ . Step S103: Pass the diluted oxide salt aqueous solution mixed with the aqueous solution through the activated carbon adsorption filter 12 to remove trace hydrophobic harmful substances. Step S104: Introduce the diluted oxide salt aqueous solution into the magnetization reactor 15 through the flow control valve 14 for synthesis reaction. The magnetization reactor has a magnetic field between 0.1 and 1 Tesla and an electric field between 10 and 100 volts / cm. Therefore, when the diluted oxide salt aqueous solution passes through the magnetization reactor 15, the charged particles in the water molecules will be affected by the magnetic field and the electric field and move, thereby breaking the hydrogen bonds in the water molecules and making the hydrogen bonds cover the oxide salts. In addition, the synthesis temperature of the magnetization reactor 15 is controlled between 10°C and 55°C, and the synthesis pressure is controlled between 6kg / cm 2 Up to 9kg / cm 2The synthesis time is 30 to 90 minutes to form diluted active oxide water. Step S105: Heat the diluted active oxide water to 65 to 70°C, add the water-soluble polymer 151 and the distilled water or the mineral water and stir for 3.5 to 4.5 hours, control the stirring speed at 600 to 650 rpm, and then stir for 5 to 6 hours under vacuum to form a water-soluble oxide wound dressing; wherein, based on the total weight percentage of the water-soluble oxide wound dressing, it comprises: 45.0 to 55.0% of the distilled water or the mineral water, 15.0 to 25.0% of an aqueous solution of oxide salts and 30.0-35.0% of a water-soluble polymer 151, wherein the water-soluble polymer 151 is sodium alginate, polyvinyl pyrrolidone, sodium carboxymethyl cellulose, hyaluronic acid or any combination thereof; based on the total weight percentage of the water-soluble oxide wound dressing, the water-soluble polymer 151 comprises: 1.0-30.0% of sodium alginate, 1.0-25.0% of polyvinyl pyrrolidone and 1.0-25.0% of sodium carboxymethyl cellulose, and the thickness of the water-soluble oxide wound dressing is greater than 0.1 mm and less than 4 mm.
[0034] The water-soluble oxide wound dressing of the present invention adopts three-dimensional mesh water-based gel molecular technology, which is characterized in that hydrogel macromolecules are interconnected to form a spatial mesh structure, and the pores of the mesh structure are filled with liquid. The gel undergoing cross-linking reaction forms a covalent cross-linking network, and the gel characteristic is swelling but not dissolving. Due to the large number of hydrophilic groups in the hydrogel, a large amount of water can be absorbed and retained. Therefore, the active oxide gel of the present invention has excellent biocompatibility, biodegradability, is easy to synthesize, and has good permeability to low molecular weight solutes.
[0035] Wound healing test
[0036] Experimental Animals 1
[0037] The experiment used 8-week-old male New Zealand white rabbits weighing about 2000-2500g. All experimental animals were kept in an independently air-conditioned animal room with a room temperature maintained at 22°C and a relative humidity maintained at 45%, and water and feed were fully supplied. Before the experiment, the animals were given at least 4 weeks to adapt to the environment. The feeding environment, treatment and all experimental procedures of the experimental animals were in accordance with the Guide for the Care and Use of Laboratory Animals.
[0038] Skin wound formation
[0039] The back of the New Zealand rabbit was shaved and then disinfected with iodine and 70% alcohol. A skin wound with an area of about 2 cm×2 cm and a depth of about 2-3 mm was cut on the back of the New Zealand rabbit using a scalpel.
[0040] Content of water-soluble oxide wound dressing ingredients
[0041] Experimental Group 1: Based on the total weight percentage of the water-soluble oxide wound dressing, the water-soluble oxide wound dressing comprises: 55% of the distilled water or the mineral water, 15.0% of an aqueous solution of oxide salts, 3.0% of sodium alginate, 2.0% of polyvinyl pyrrolidone and 25.0% of sodium carboxymethyl cellulose.
[0042] Experimental Group 2: Based on the total weight percentage of the water-soluble oxide wound dressing, the water-soluble oxide wound dressing comprises: 55.0% of the distilled water or the mineral water, 20.0% of the oxide salt aqueous solution, 3.0% of sodium alginate, 2.0% of polyvinyl pyrrolidone and 20.0% of sodium carboxymethyl cellulose.
[0043] Control group 1: Based on the total weight percentage of the water-soluble oxide wound dressing, the water-soluble oxide wound dressing comprises: 55% of the distilled water or the mineral water, 15.0% of an aqueous solution of oxide salts, 3.0% of sodium alginate, 2.0% of polyvinyl pyrrolidone and 25.0% of sodium carboxymethyl cellulose.
[0044] Control group 2: Based on the total weight percentage of the water-soluble oxide wound dressing, the water-soluble oxide wound dressing comprises: 55.0% of the mineral water or distilled water, 20.0% of an aqueous solution of oxide salts, 3.0% of sodium alginate, 2.0% of polyvinyl pyrrolidone and 20.0% of sodium carboxymethyl cellulose.
[0045] Application of water-soluble oxide wound dressings
[0046] New Zealand white rabbits were randomly divided into 2 experimental groups and 2 control groups, wherein skin wounds were formed in each group of New Zealand white rabbits according to the above method; then, the skin wounds of the New Zealand white rabbits in experimental groups 1 and 2 were respectively applied with the water-soluble oxide wound dressings according to the above experimental groups 1 and 2, and the wounds of the animals were covered with a polyurethane (PU) waterproof film to keep them moist. Skin wounds were formed in the New Zealand white rabbits in control groups 1 and 2 according to the above method; then, the skin wounds of the New Zealand white rabbits in control groups 1 and 2 were respectively applied with the water-soluble oxide wound dressings according to the above control groups 1 and 2. The experiment was conducted for a total of 14 days, and the wound areas of each group of New Zealand white rabbits were measured on the 2nd, 6th, 10th and 14th days after the application of the dressings, and the results are shown in Table 1 below.
[0047] Table 1
[0048] 2 days after administration 6 days after administration 10th day after administration 14 days after administration Experimental Group 1 <![CDATA[3.87cm 2 ]]> <![CDATA[3.45cm 2 ]]> <![CDATA[2.95cm 2 ]]> <![CDATA[2.51cm 2 ]]> Experimental Group 2 <![CDATA[3.79cm 2 ]]> <![CDATA[3.32cm 2 ]]> <![CDATA[2.76cm 2 ]]> <![CDATA[2.34cm 2 ]]> Control group 1 <![CDATA[3.77cm 2 ]]> <![CDATA[3.33cm 2 ]]> <![CDATA[2.69cm 2 ]]> <![CDATA[2.13cm 2 <!-- 4 -->]]> Control group 2 <![CDATA[3.63cm 2 ]]> <![CDATA[3.10cm 2 ]]> <![CDATA[2.44cm 2 ]]> <![CDATA[2.09Cm 2 ]]>
[0049] The difference between experimental group 1 and experimental group 2 lies in the oxygen content. The oxygen content of experimental group 2 is higher than that of experimental group 1. As can be seen from the above table, high oxygen content improves the wound closure rate. Secondly, experimental group 1 and experimental group 2 covered the animal's wound with a polyurethane waterproof film to keep the wound moist, while control group 1 and control group 2 did not cover the animal's wound with a polyurethane waterproof film. As can be seen from the above table, the wound heals faster in a wet environment. In summary, moist wound healing has the following advantages. First, it is conducive to the dissolution of necrotic tissue and fibrin. In a wet environment, the tissue protein lytic enzyme in the wound exudate can promote the dissolution and absorption of necrotic tissue. Secondly, it regulates the oxygen tension of the wound surface and promotes the formation of capillaries. The hypoxic environment stimulates capillary proliferation, which is conducive to the formation of epithelial cells and collagen. Furthermore, it promotes the release of various growth factors in the exudate, and the exudate retained in the wound surface releases and activates various enzymes and enzyme activation factors. The exudate can also effectively maintain cell survival, promote the release of various growth factors, and stimulate cell proliferation. In addition, it maintains a constant temperature on the wound surface, accelerates cell division, promotes wound healing, moisturizes the wound surface, reduces scab formation, avoids mechanical damage to new granulation tissue, reduces damage and pain when changing dressings, protects nerve endings on the wound surface, and reduces pain. In addition, the closed moisturizing environment forms a barrier for the dressing, reduces the chance of infection, and the slightly acidic environment in the closed state inhibits bacterial growth and is conducive to the reproduction and function of white blood cells.
[0050] Experimental Animals 2
[0051] Experimental animals 2 were C57BL / 6J Narl mice purchased from the Experimental Animal Center, weighing 40-45 g and aged 8 weeks. All experimental animals 2 were kept in an independently air-conditioned animal room with a room temperature maintained at 18-26°C and a relative humidity maintained at 30-70%, a light cycle of 12 hours of light and 12 hours of darkness, and sufficient water and feed were provided. The feeding environment, treatment and all experimental procedures of the experimental animals were in accordance with the experimental animal feeding management and use regulations.
[0052] Non-infected wound care
[0053] Before the operation, the mice were given 0.6 / kg of anesthetic by intraperitoneal injection. After the mice were anesthetized, the hair on their backs was shaved, and a skin wound with an area of about 1.2 cm×1.2 cm was cut on the backs of the mice. Secondly, the mice were divided into a blank control group, a vaseline group and an experimental group. The blank control group did not treat the wound; the vaseline group used a cotton swab to dip an appropriate amount of vaseline and evenly applied it on the wound; the experimental group used a cotton swab to dip an appropriate amount of water-soluble oxide wound dressing and evenly applied it on the wound.
[0054] Infected wound management
[0055] Before the operation, the mice were given 0.6 / kg of anesthetic by intraperitoneal injection. After the mice were anesthetized, the hair on their backs was shaved and a skin wound of about 1.2 cm × 1.2 cm was cut on the backs of the mice. Staphylococcus aureus was diluted to 10 5 CFU / 150μl, and 150μl of bacterial solution was added to each mouse, allowing the bacterial solution to completely penetrate the skin for about 5 minutes. Secondly, the mice were divided into a blank control group, a vaseline group and an experimental group. The blank control group did not treat the wound; the vaseline group used a cotton swab to dip an appropriate amount of vaseline and evenly applied it on the wound; the experimental group used a cotton swab to dip an appropriate amount of water-soluble oxide wound dressing (based on the total weight percentage of the water-soluble oxide wound dressing, the water-soluble oxide wound dressing contains: 55.0% of the distilled water or the mineral water, 20.0% of the oxide salt aqueous solution, 3.0% of sodium alginate, 2.0% of polyvinyl pyrrolidone and 20.0% of sodium carboxymethyl cellulose.) and evenly applied it on the wound.
[0056] Wound tissue bacterial content test
[0057] On the seventh day of the mouse experiment, the purulent tissues of the wounds on the backs of the traumatized mice were collected. The tissues were cut into pieces and crushed with an ultrasonic cell crusher. After centrifugation at 1,500 rpm for 8 minutes at 4°C, the supernatant was collected. The supernatant was serially diluted, and the bacterial solution was evenly spread on agar. After incubation in a 37°C incubator for about 16 hours, the number of colonies was calculated. The number of bacteria per gram of tissue (CFU / g) = (number of colonies * dilution factor * 10 / number of grams of tissue).
[0058] result
[0059] The changes in the appearance of the wounds of non-infected mice were evaluated. After the wounds were opened on the back skin of the mice, the wounds were cleaned and the medicine was changed every two days. Compared with other groups, the wounds of non-infected wounds treated with water-soluble oxide wound dressings had better healing efficiency. On the 8th to 10th day, the wounds of the blank control group and the vaseline group did not heal significantly. In contrast, the appearance of the wounds of the water-soluble oxide wound dressings had obviously begun to heal. The results in Table 2 show that after treatment with water-soluble oxide wound dressings, non-infected wounds can heal in about 8 to 10 days.
[0060] Table 2
[0061] Day 2 Day 5 Day 8 Day 10 Blank control group <![CDATA[1.35cm 2 ]]> <![CDATA[1.29cm 2 ]]> <![CDATA[1.26cm 2 ]]> <![CDATA[1.28cm 2 ]]> Vaseline Group <![CDATA[1.27cm 2 ]]> <![CDATA[1.20cm 2 ]]> <![CDATA[1.17cm 2 ]]> <![CDATA[1.20cm 2 ]]> Experimental Group <![CDATA[1.05cm 2 ]]> <![CDATA[0.82cm 2 ]]> <![CDATA[0.49cm 2 ]]> <![CDATA[0.11cm 2 ]]>
[0062] The changes in the appearance of the wounds of infected mice were evaluated. The wounds were infected with Staphylococcus aureus. After the seventh day of infection, the wounds were cleaned and the medicine was changed every two days. Compared with other groups, the wounds of infected wounds treated with water-soluble oxide wound dressings showed a significant shrinkage trend. On the 6th day, the wounds treated with water-soluble oxide wound dressings had achieved more than 60% wound healing. On the 6th day, the wounds of the blank control group and the vaseline group had not yet begun to heal. In contrast, the appearance of the wounds of the water-soluble oxide wound dressings had begun to heal significantly. The results in Table 3 show that after the water-soluble oxide wound dressings were given to the infected mouse wounds, the wounds could heal about 8 to 12 days earlier.
[0063] Table 3
[0064] Day 3 Day 6 Day 8 Day 12 Blank control group <![CDATA[1.32cm 2 ]]> <![CDATA[1.34cm 2 ]]> <![CDATA[1.32cm 2 ]]> <![CDATA[1.28cm 2 ]]> Vaseline Group <![CDATA[1.30cm 2 ]]> <![CDATA[1.29cm 2 ]]> <![CDATA[1.27cm 2 ]]> <![CDATA[1.27cm 2 ]]> Experimental Group <![CDATA[1.13cm 2 ]]> <![CDATA[0.57cm 2 ]]> <![CDATA[0.29cm 2 ]]> <![CDATA[0.05cm 2 ]]>
[0065] Antibacterial test
[0066] In addition, inhibiting the growth of wound bacteria and protecting the wound from infection are the key points of care. The antibacterial test of Staphylococcus aureus and Aggregatibacter was carried out using the ASTM E2315 method. The steps are as follows.
[0067] Step 1: Take Staphylococcus aureus and culture it for an appropriate period of time, prepare 20 ml of bacterial solution, and adjust the concentration of the bacterial solution to 5x105 CFU / mL.
[0068] Step 2: Divide the bacterial solution of step 1 into five groups, and the five groups are respectively acted for 0 hours, 0.5 hours, 1.0 hours, 2.0 hours and 4.0 hours. Each group includes 3 samples, and the 3 samples include a blank group, an experimental group 1 and an experimental group 2. The blank group is a wound dressing without adding a water-soluble oxide; the experimental group 1 is a wound dressing with a water-soluble oxide, which includes, based on the total weight percentage of the water-soluble oxide wound dressing: 55% of the distilled water or the mineral water, 15.0% of an aqueous solution of oxide salts, 3.0% of sodium alginate, 2.0% of polyvinyl pyrrolidone and 25.0% of sodium carboxymethyl cellulose; Experimental Group 2: adding a water-soluble oxide wound dressing, which, based on the total weight percentage of the water-soluble oxide wound dressing, comprises: 55.0% of the mineral water or the distilled water, 20.0% of an aqueous solution of oxide salts, 3.0% of sodium alginate, 2% of polyvinyl pyrrolidone and 20.0% of sodium carboxymethyl cellulose.
[0069] Step 3: Take 0.1 ml of bacterial solution from each sample and evenly spread it on the culture medium. Prepare two replicates of culture medium for each sample, and then culture at 37°C for 24 hours.
[0070] Step 4: Count the amount of bacteria and calculate the inhibition rate according to the following formula: Inhibition rate = original inoculation amount (Log10) - bacterial amount after sample treatment (Log10) / original inoculation amount (Log10) x 100%.
[0071] As mentioned above, the difference between experimental group 1 and experimental group 2 lies in the oxygen content. The oxygen content of experimental group 2 is higher than that of experimental group 1. As shown in Table 4, high oxygen content improves the antibacterial rate. The antibacterial effect on Staphylococcus aureus can reach an inhibition rate of 99.9%. Secondly, the antibacterial test method of Aggregatibacter is the same as that of Staphylococcus aureus, and its inhibition rate can also reach 99.9%.
[0072] Table 4
[0073]
[0074]
[0075] Blood oxygen partial pressure
[0076] Whether it is venous blood oxygen or arterial blood oxygen in the same individual, blood pH and pCO 2 , pO 2 The values of O in the blood will increase after the application of water-soluble oxide wound dressings. 2 Content and reduce blood CO 2The content can increase the oxygen content in the organism to promote the speed of wound healing.
[0077] The water-soluble oxide wound dressing made by the manufacturing method of the water-soluble oxide wound dressing of the present invention has the characteristics of sodium carboxymethyl cellulose, polyvinyl pyrrolidone and sodium alginate, which can form a high-viscosity colloid, forming a network polymer colloid containing a large amount of water, with adhesion and good water absorption; the colloid can undergo repeated hydration when in contact with the body surface, and has the dual functions of providing moisture to the surface and absorbing exudate, thereby controlling bleeding or loss of body fluids. After absorbing water, the hydrophilic group of sodium carboxymethyl cellulose becomes gel-like and adheres to the vascular wound surface, and forms a gel layer after expansion to achieve wound hemostasis. Secondly, the water-soluble oxide wound dressing forms a protective layer on the wound surface, which is colorless, transparent and has a high water content; it can keep the wound moist, avoid friction and irritation of the wound, do not damage the new granulation tissue, and reduce secondary damage. Because sodium carboxymethyl cellulose has an acidic carboxyl group and Fe in hemoglobin 2+ Combined, forming a brown sticky block, to achieve the purpose of sealing the end of the capillary and stopping bleeding. In addition, the gel also has an adhesion and aggregation effect on platelets, which can accelerate coagulation.
[0078] Example 2
[0079] Please refer to Figure 3 , Figure 3 This is a system for preparing the water-soluble oxide wound dressing according to Example 2 of the present invention.
[0080] like Figure 3 As shown, the steps of Example 2 are substantially the same as those of Example 1, except that: in Example 2, before the step of passing the diluted oxide salt solution through the activated carbon adsorption filter 12, a step of adding ozone is further included, wherein the diluted oxide salt solution is introduced into the additive tank 16, and the ozone is added into the additive tank 15, and the ozone can sterilize the diluted oxide salt solution.
[0081] Human Experiments
[0082] See also Figures 4A to 4C , Figure 4A This is a photograph of the affected part of diabetic foot taken when the water-soluble oxide wound dressing of the present invention is not applied; Figure 4B is a photograph of the affected part of diabetic foot taken 2 days after applying the water-soluble oxide wound dressing of the present invention; and Figure 4C This is a photograph of the affected part of diabetic foot taken 7 days after the water-soluble oxide wound dressing of the present invention was applied.
[0083] like Figures 4A to 4CAs shown, the test subject is a diabetic foot, the tendon and ligament tissue of the test subject has been ruptured, and purulent secretions and necrotic tissue have increased. The water-soluble oxide wound dressing of the present invention is applied to the affected part of the patient and the wound healing is observed from 0 to 7 days; after 2 days of use, the ulcer condition is improved, and after 7 days of use, the wound slowly heals and the wound area is reduced.
[0084] In summary, the water-soluble oxide wound dressing made by the manufacturing method of the water-soluble oxide wound dressing of the present invention puts the wound in a moist environment, so the tissue protein lytic enzyme in the wound exudate can promote the dissolution and absorption of necrotic tissue; the hypoxic environment stimulates capillary proliferation, which is beneficial to the production of epithelial cells and collagen. Secondly, the water-soluble oxide wound dressing of the present invention puts the wound in a closed moisturizing environment, and the dressing forms a barrier to reduce the chance of infection. The slightly acidic environment in a closed state inhibits bacterial growth, which is beneficial to the reproduction and function of white blood cells. Furthermore, the water-soluble oxide wound dressing of the present invention helps the exudate retained in the wound surface to release and activate a variety of enzymes and enzyme activation factors. The exudate can also effectively maintain cell survival, promote the release of a variety of growth factors to stimulate cell proliferation. By this, the water-soluble oxide wound dressing of the present invention has anti-inflammatory response and wound smoothing effects, thereby achieving the purpose of accelerating wound healing.
[0085] However, the above description is only a preferred embodiment of the present invention and is not intended to limit the patent protection scope of the present invention. Therefore, all equivalent changes made using the contents of the present invention's description and drawings are also included in the scope of protection of the present invention and are hereby stated.
Claims
1. A method for manufacturing a water-soluble oxide wound dressing, It is characterized in that The method comprises the following steps: Provide distilled or mineral water; Adding an oxide salt aqueous solution into the distilled water or the mineral water to form a diluted oxide salt aqueous solution, wherein the oxide salt aqueous solution is formed by passing high pressure oxygen into a crystalline salt solution by a heating electrolysis method, the oxide salt aqueous solution has a pH value of 5.5 to 8 and a volume molar concentration of 5 to 50 mol / L, and the heating temperature of the heating electrolysis method is controlled between 40 and 80° C.; Passing the diluted oxide salt aqueous solution through an activated carbon adsorption filter to remove trace hydrophobic harmful substances; and The diluted oxide salt aqueous solution is introduced into a magnetized reactor through a flow control valve for synthesis reaction, and the magnetized reactor has a magnetic field of 0.1 to 1 Tesla and an electric field of 10 to 100 volts / cm. The synthesis temperature of the magnetized reactor is controlled between 10° C. and 55° C., and the synthesis pressure is controlled between 6 kg / cm 2 Up to 9kg / cm 2 The synthesis time is 30 to 90 minutes to form concentrated active oxide water; The concentrated active oxide water is heated to 65-70° C., a water-soluble polymer and the distilled water or the mineral water are added and stirred for 3.5-4.5 hours, the stirring speed is controlled at 600-650 rpm, and then stirred for 5-6 hours under vacuum to form a water-soluble oxide wound dressing; Wherein, based on the total weight percentage of the water-soluble oxide wound dressing, the water-soluble oxide wound dressing comprises: 45.0-55.0% of the distilled water or the mineral water, 15.0-25.0% of the oxide salt aqueous solution and 30.0-35.0% of the water-soluble polymer.
2. The method for producing the water-soluble oxide wound dressing according to claim 1, It is characterized in that The oxide salt aqueous solution has a volume molar concentration of 10 to 40 mol / L.
3. The method for producing the water-soluble oxide wound dressing according to claim 1, It is characterized in that The water-soluble polymer is sodium alginate, polyvinyl pyrrolidone, sodium carboxymethyl cellulose, hyaluronic acid or any combination thereof.
4. The method for producing the water-soluble oxide wound dressing according to claim 3, It is characterized in that Calculated by the total weight percentage of the water-soluble oxide wound dressing, the water-soluble polymer comprises: 1.0-30.0% of sodium alginate, 1.0-25.0% of polyvinyl pyrrolidone and 1.0-25.0% of sodium carboxymethyl cellulose.
5. The method for producing the water-soluble oxide wound dressing according to claim 1, It is characterized in that The method further comprises an additive adding step, wherein the diluted oxide salt aqueous solution is introduced into an additive tank, and ozone is added into the additive tank for sterilization.
6. The method for producing the water-soluble oxide wound dressing according to claim 1, It is characterized in that The oxide salt aqueous solution is an aqueous solution formed by the mutual combination of metal element cations and carbonate, sulfate, chromate, tungstate, molybdate, phosphate, arsenate or vanadate.
7. The method for producing the water-soluble oxide wound dressing according to claim 6, It is characterized in that The metal element cation includes at least one divalent or trivalent metal cation, which is Fe 2+ , Cu 2+ 、Zn 2+ , Pb 2+ , Mn 2+ 、Bi 3+ or any combination thereof.
8. The method for producing the water-soluble oxide wound dressing according to claim 1, It is characterized in that The water-soluble oxide wound dressing has a thickness of not less than 0.1 mm and not more than 4 mm.
9. The method for producing the water-soluble oxide wound dressing according to claim 1, It is characterized in that The flow control valve controls the flow rate of the small molecule water to 500-8000 L / min.
10. A water-soluble oxide wound dressing prepared by the method according to any one of claims 1 to 9.