Technical method for improving rolled steel yield

Through the technology of online weighing and automatic adjustment of billet length, the problems of low production efficiency and safety hazards in the existing technology are solved, the steel rolling yield rate is increased and the cost is reduced, and the production efficiency and safety are improved.

CN118808334APending Publication Date: 2024-10-22YANCHENG LIANXIN IRON & STEEL CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202410962180.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-18
Publication Date
2024-10-22

AI Technical Summary

Technical Problem

When the existing technology improves the steel rolling yield, the production efficiency is low, there are safety hazards, and complete fixed-weight rolling cannot be achieved, resulting in increased costs.

Method used

The billet length is automatically adjusted through online weighing sensors, and the flame cutting system and infrared system are used to achieve precise fixed-weight rolling, reducing manual intervention and reducing calculation errors.

Benefits of technology

It improves the steel rolling yield, reduces production costs, reduces the consumption of steel materials for steelmaking, and improves production efficiency and safety.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118808334A_ABST
    Figure CN118808334A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of metallurgical production, in particular to a technical method for improving rolled steel yield, which comprises the following steps: determining the weight of a steel billet by a steel mill and acquiring sample variables; the steel plant calculates the billet length according to the weight and estimates the theoretical length of the sample; the steel billets are weighed on line, and the weight is transmitted to a flame cutting system; the system adjusts the length required by the sample through a calculation formula and transmits the length to an infrared system; the infrared system automatically adjusts the length of the steel billet for cutting; accurate fixed-weight rolling is achieved, and detection is carried out. The device has the advantages that firstly, steel billets with stable weight can be provided for rolled steel according to different requirements of steel mills, so that the yield of the rolled steel is improved; the problem of weight fluctuation of steel billet fixed-weight rolling is solved, the labor intensity of workers and calculation errors in the previous weighing and adjusting process are avoided, and the cost of the production process is reduced; and thirdly, the consumption of steelmaking steel and iron materials is reduced to 1049.7 from 1050.3 Kg / t by 0.6 Kg / t, so that the production cost is reduced, and contributions are made to cost reduction and benefit improvement of companies.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of metallurgical production, and in particular to a technical method for improving the yield rate of steel rolling. Background Art

[0002] In recent years, the market has been sluggish, and the profit effect of the steel industry has gradually decreased. In order to reduce production costs and increase the survival space of enterprises, various factories are trying to improve the yield rate of steel rolling. At present, fixed weight rolling is mostly used to improve the yield rate. There are two ways of fixed weight rolling used by various factories. One is to randomly weigh the billet through a crane and a hook scale, and then adjust the length of the billet to achieve fixed rolling. The other is to use a rail scale to weigh online, and then adjust the billet length according to the weighing result to achieve fixed weight rolling.

[0003] The above two methods have the following disadvantages: first, they need to be weighed by a hook scale or a rail scale, and then the length of the billet is adjusted manually, which is inefficient and inconvenient, and there are also production safety issues; second, weighing and calibration are required after adjustment, and complete fixed weight rolling cannot be achieved. Summary of the invention

[0004] The purpose of the present invention is to provide a technical method for improving the yield rate of steel rolling to solve the problems existing in the above-mentioned background technology.

[0005] To achieve the above object, the present invention provides the following technical solution: a technical method for improving the yield rate of steel rolling, characterized in that it comprises the following steps:

[0006] (1) The steel mill determines the weight of steel billets of different specifications and obtains sample variables;

[0007] (2) The steel mill calculates the length of the billet based on the weight and estimates the theoretical length of the sample;

[0008] (3) The billet is weighed online and the weight is transmitted to the flame cutting system;

[0009] (4) The system adjusts the required length of the sample through a calculation formula and transmits it to the infrared system;

[0010] (5) The infrared system automatically adjusts the length of the billet for cutting;

[0011] (6) Achieve precise fixed-weight rolling and conduct testing.

[0012] Furthermore, the formula for estimating the theoretical length of the sample in step (2) is: theoretical length of steel billet = steel billet weight / 0.165 / 0.165 / 7.85.

[0013] Furthermore, the formula for the length to be adjusted in step (4) is: length to be adjusted = (actual weighed weight - required set weight) / 0.165 / 0.165 / 7.85.

[0014] Furthermore, the online weighing in step (3) is automatic weighing by a weighing sensor and the information is transmitted to a computing module in the flame cutting system, which performs simulation calculations based on the measured weight and automatically adjusts the length of the billet to ensure stable billet weight.

[0015] Furthermore, the infrared system in step (5) includes an infrared length measuring instrument, which automatically adjusts the actual length required for the billet according to the result of the length to be adjusted calculated in step (4) and performs cutting.

[0016] Compared with the prior art, the beneficial effects of the present invention are: first, it can provide steel billets with stable weight for steel rolling according to the different needs of steel rolling mills, thereby improving the yield rate of steel rolling; second, it solves the weight fluctuation of steel billets during fixed rolling, avoids the labor intensity and calculation errors of workers in the previous weighing and adjustment process, and reduces the cost of the production process; third, the steel consumption of steelmaking is reduced from the original 1050.3Kg / t to 1049.7, a decrease of 0.6Kg / t, and the yield rates of the first, second, third and fourth rolling are increased by 0.4%, 0.3%, 0.3% and 0.31% respectively, thereby reducing production costs and contributing to the company's cost reduction and efficiency improvement. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 It is the work flow chart of the present invention. DETAILED DESCRIPTION

[0018] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0019] The present invention provides a technical solution: a technical method for improving the yield rate of steel rolling, the specific steps are as follows:

[0020] (1) The steel mill determines the weight of steel billets of different specifications and obtains sample variables;

[0021] (2) The steel mill calculates the length of the billet based on the weight and estimates the theoretical length of the sample, which is billet theoretical length = billet weight / 0.165 / 0.165 / 7.85; and the billet is put into the online weighing device for online weighing;

[0022] (3) Billet weighing online. The weighing sensor automatically weighs and transmits the information to the calculation module in the flame cutting system. The module performs simulation calculation based on the measured weight, automatically adjusts the billet length, ensures the billet weight is stable, and transmits the weight to the flame cutting system.

[0023] (4) The system adjusts the required length of the sample through a calculation formula. The formula for the required length adjustment is: required length adjustment = (actual weighing weight - required fixed weight) / 0.165 / 0.165 / 7.85, and transmits the calculated data to the infrared system;

[0024] (5) The infrared system automatically adjusts the length of the billet for cutting;

[0025] (6) Achieve precise weight rolling and inspect the products.

[0026] Furthermore, the infrared system in step (5) includes an infrared length measuring instrument, which automatically adjusts the actual length required for the billet according to the result of the length to be adjusted calculated in step (4) and performs cutting.

[0027] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A technical method for improving the yield rate of steel rolling, characterized in that: The following steps are involved: (1) The steel mill determines the weight of steel billets of different specifications and obtains sample variables; (2) The steel mill calculates the length of the billet based on the weight and estimates the theoretical length of the sample; (3) The billet is weighed online and the weight is transmitted to the flame cutting system; (4) The system adjusts the required length of the sample through a calculation formula and transmits it to the infrared system; (5) The infrared system automatically adjusts the length of the billet for cutting; (6) Achieve precise fixed-weight rolling and conduct testing.

2. The technical method for improving the steel rolling yield rate according to claim 1 is characterized in that: The formula for estimating the theoretical length of the sample in step (2) is: theoretical length of steel billet = steel billet weight / 0.165 / 0.165 / 7.

85.

3. The technical method for improving the steel rolling yield rate according to claim 1 is characterized in that: The formula for the length to be adjusted in step (4) is: length to be adjusted = (actual weighed weight - required fixed weight) / 0.165 / 0.165 / 7.

85.

4. The technical method for improving the steel rolling yield rate according to claim 1 is characterized in that: The online weighing in step (3) is that the weighing sensor automatically weighs and transmits the information to the calculation module in the flame cutting system, performs simulation calculation according to the measured weight, automatically adjusts the length of the steel billet, and ensures the stability of the steel billet weight.

5. The technical method for improving the steel rolling yield rate according to claim 1 is characterized in that: The infrared system in step (5) includes an infrared length measuring instrument, which automatically adjusts the actual length required for the billet according to the result of the length to be adjusted calculated in step (4) and performs cutting.

Citation Information

Patent Citations

  • Fixed-weight blank supply long material production device

    CN108097721A

  • Permanent weight cutting method of continuous casting machine and cutting system thereof

    CN110116194A