Laser welding top cover outer plate forming process and structure

By using drawing, trimming and flanging shaping processes in the laser welding process of the top cover outer plate, combined with movable punch and double parting line technology, the cracking, wrinkling and cracking of the top cover outer plate during laser welding are solved. The problem of springback deformation is improved, the forming accuracy and production efficiency are improved, and the manufacturing cost is reduced.

CN118808446APending Publication Date: 2024-10-22ANHUI JIANGHUAI AUTOMOBILE GRP CORP LTD

Patent Information

Application Number
CN202410860005.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-28
Publication Date
2024-10-22

AI Technical Summary

Technical Problem

The existing top cover outer plate has cracking, wrinkling and rebound deformation problems during the laser welding process, and the production process is complex, which increases costs and equipment requirements.

Method used

The drawing process is used to design the convex and concave fillet structures, the trimming process is used to remove excess material, the flanging shaping process uses a movable punch structure and a double parting mold line to form double press materials, and the tail shaping process is optimized to reduce springback and lifting. wrinkles to improve forming accuracy and stability.

Benefits of technology

By optimizing the process and structure, the phenomenon of springback and wrinkling is reduced, the accuracy of the tail seam and the shaping stability are improved, the production cost is reduced, and the equipment requirements and mold design are simplified.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118808446A_ABST
    Figure CN118808446A_ABST
Patent Text Reader

Abstract

The invention discloses a laser welding top cover outer plate forming process and structure. The laser welding top cover outer plate forming process comprises the following steps that (1) a blank is provided, and a blank line is marked; (2) drawing: setting a draw bead to control the feeding speed, and designing and forming a convex fillet and concave fillet structure at the edge of the A surface of the product to reduce springback; (3) trimming is conducted, all waste materials are trimmed at a time, and material blocking is avoided through deformation and shrinkage of shrinkage ribs; and (4) performing a flanging and shaping process, including front side positive shaping, tail side shaping, two-side shaping and skylight positive shaping, designing and using a movable male die structure to perform negative angle surface forming, reducing machining and assembling accumulated tolerance, and finally performing accurate flanging and shaping on the product to ensure the tail precision and stability. The problems of cracking, wrinkling, springback deformation and the like in the prior art are solved, the forming precision and the production efficiency are improved by optimizing the product structure and the technological process, the manufacturing cost is reduced, and therefore important application value and market prospects are achieved in the automobile manufacturing industry.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of automobiles, and in particular to a laser welding top cover outer panel forming process and structure. Background Art

[0002] With the rapid development of the automobile manufacturing industry, higher requirements have been placed on the welding process of body structural parts. Laser welding technology has been widely used in the field of automobile body welding and has been successfully applied to the welding of key parts such as roofs, trunks and frames, showing advantages that traditional welding technology cannot match.

[0003] However, despite the great potential of laser welding technology in automobile body manufacturing, the existing roof outer panel product structure and stamping process solutions still have some limitations. For example, the traditional roof outer panel usually adopts a flange structure on both sides and is connected to the side outer panel by spot welding. This structure has certain limitations in the laser welding process, because the flange structure is not suitable for laser welding, and it is easy to produce problems such as drawing cracking during the stamping process. At the same time, the front sunroof area of ​​the roof outer panel in the prior art is prone to wave wrinkling during flanging due to the large change in curvature, which affects the appearance and structural strength of the product. In addition, the bending surface of the water flow channel at the tail of the roof under the existing process has a large impact on the feeding due to the small side shaping pressing area, resulting in a large impact on the side pressure effect on the feeding, resulting in poor rebound deformation surface after shaping, high difficulty in controlling the stopper precision, and poor process stability. These problems not only increase production costs, but also affect the performance and quality of the final product.

[0004] Moreover, the laser welding of the top cover outer panel usually requires multiple processes, which not only increases the equipment requirements of the production line, but also increases the complexity and cost of tooling development. In particular, the tail side lower punch is a large active part, and the accumulated tolerances during its processing and assembly process have an adverse effect on the final assembly and commissioning.

[0005] In view of these shortcomings of the prior art, the present invention provides an improved automotive laser welding roof outer panel stamping forming process and a tail precision stability control method. The present invention aims to solve the problems of cracking, wrinkling, springback deformation, etc. in the prior art, and improves the forming precision and production efficiency and reduces the manufacturing cost by optimizing the product structure and process flow, thus having important application value and market prospects in the automotive manufacturing industry. Summary of the invention

[0006] The technical problem to be solved by the present invention is to provide a laser welding top cover outer panel forming process and structure, which solves the problems of cracking, wrinkling, springback deformation and the like in the prior art, improves the forming accuracy and production efficiency, and reduces the manufacturing cost by optimizing the product structure and process flow, thereby having important application value and market prospects in the automobile manufacturing industry.

[0007] The technical problem to be solved by the present invention is achieved through the following technical solutions:

[0008] A laser welding top cover outer panel forming process, the process comprising the following steps:

[0009] (1) Providing the blank and marking the blank line;

[0010] (2) Execute the drawing process, set draw ribs to control the feed speed, design and form the convex and concave fillet structures on the edge of the A surface of the product to reduce springback, and form a step surface at the tail for feed control in subsequent processes and to improve the deformation resistance of the product;

[0011] (3) Trimming process: All waste materials are trimmed at one time, including removing excess material from the edge of the top cover outer panel and trimming the front and rear skylights and discharging waste materials, and avoiding material jamming by shrinking the shrink ribs;

[0012] (4) Perform flanging shaping processes, including front positive shaping, tail side shaping, both side shaping, and sunroof positive shaping. Design and use a movable punch structure to perform negative angle surface forming to reduce the cumulative tolerance of processing and assembly. Finally, perform precise flanging shaping on the product to ensure the accuracy and stability of the tail.

[0013] Preferably, step (2) specifically comprises the following steps:

[0014] (21) at least four upward-turned circular holes are provided on the front and rear sides for precise positioning in the subsequent process; the drawing is performed with the circumferential parting line as the dividing line, and the flanging is performed with the upward-turned parting line as the boundary to form the preliminary shape of the top cover outer panel; a bottom mark is provided on the process supplementary surface of the diagonal non-product area to confirm whether the drawing is closed to the bottom; and draw ribs are used to control the feeding speed of the blank during the forming process;

[0015] (22) an over-drawing convex fillet, a transition convex fillet connected to the side wall of the tail, and a reverse concave fillet connecting the over-drawing convex fillet and the transition convex fillet are arranged on the outer side of the edge of the A surface of the tail product of the drawing die face; after drawing, the stress direction of the reverse concave fillet is opposite to the stress direction of the over-drawing convex fillet;

[0016] (23) A step surface is provided at the tail end for feeding control and work hardening deformation in the subsequent process to improve the stability of the plane structure.

[0017] Preferably, in step (23), the root of the R angle of the step surface retains a width of 10-15 mm from the tail trimming stop line.

[0018] Preferably, step (3) comprises the following steps:

[0019] (31) All the waste materials of the outer ring are removed along the peripheral trimming line, and the waste cutter is designed to cut the waste materials on the front and rear sides into small sections and discharge them from the mold. The large-sized slipped waste materials are cut into multiple small-sized waste materials by the secondary cutting waste cutter and then discharged;

[0020] (32) The front and rear skylights are cut off as a whole along the skylight perimeter trimming line, and the waste is cut into two sections by a skylight waste cutter and discharged.

[0021] Preferably, the flanging shaping in step (4) includes:

[0022] 1) Perform positive shaping on the anterior segment;

[0023] 2) The front sections on both sides are subjected to side shaping. The transition section is first subjected to positive flanging through the intersection sinking part of the positive shaping insert, and then subjected to side shaping transition through the side intersection part of the front section side shaping insert;

[0024] 3) The rear sections on both sides are subjected to positive flanging shaping and triangular positioning waste removal, wherein the overlapping part uses the rear section orthogonal sinking part to first contact the plane after drawing and cutting for positive flanging, and then the side intersection of the front section side shaping insert is used for side shaping;

[0025] 4) Perform side shaping on the rear corner sections on both sides, wherein the overlapping parts are first shaped orthogonally by the sunken parts, and then shaped by the side shaping inserts.

[0026] Preferably, step (4) further includes flange shaping for preventing the front side skylight flange from wrinkling, which includes the following steps:

[0027] 1) The double parting line and double pressing forming process is used for the flanging shaping of the front sunroof;

[0028] 2) The upper A-surface circumference is set as the upper pressing parting line of the front skylight, which is used to press the A-surface of the skylight circumference;

[0029] 3) Design the front sunroof lower pressing parting line 4mm inside the upper pressing parting line of the front sunroof as the boundary line of the lower pressing block;

[0030] 4) During the flanging process of the front skylight, the upper mold main body pressing core is used to press the product surface around the skylight, and at the same time, the flanging shaping insert moves downward and works together with the inner pressing ring to press the skylight surface to be flanging;

[0031] 5) As the flanging shaping insert moves downward, the sheet metal gradually completes the flanging shaping. During this process, the sheet metal of the skylight to be flanging is subjected to a quasi-drawing forming process through the inner pressure ring.

[0032] Preferably, the design of step (4) and the use of a movable punch structure for negative angle surface forming are specifically as follows:

[0033] 1) Select an appropriate movable punch structure to adapt to the negative angle surface forming;

[0034] 2) defining a forming area A between the upper parting line of the movable punch and the side shaping parting line, wherein the area is formed by the movable punch;

[0035] 3) In the forming area A, a movable punch is arranged, and the movable punch can be moved according to the forming needs to adapt to the forming requirements of different parts;

[0036] 4) The side shaping area and the pressing part between the lower parting line of the movable punch and the side pressing parting line are designed as an integral structure and fixedly mounted on the lower die base to reduce the active area of ​​the side shaping, thereby avoiding the problem of difficult control of forming accuracy and poor stability of the double active structure of the upper side shaping movable concave die and the lower movable punch, thereby improving the forming accuracy and stability;

[0037] 5) During the forming process, by controlling the movement of the active punch, the sheet metal after drawing is precisely formed with a negative angle surface to ensure that the formed sheet metal meets the design requirements.

[0038] Preferably, step (4) further comprises: performing side shaping on the front corner transition portion until it is in place and performing side shaping on the remaining positive shaping portions of the rear sections on both sides.

[0039] A laser-welded roof outer panel product structure is suitable for laser welding of automobile bodies, comprising a roof outer panel, wherein an A surface is arranged on the top of the roof outer panel, an inwardly buckled negative angle bevel is arranged on the lower side of the A surface, the negative angle bevel and the A surface form a rounded welding fillet surface, and notches are respectively arranged on the front corner, rear section and rear corner of the negative angle bevel, wherein the length of the notch is 60 mm, and the distance between the edge of the notch and the root of the R angle is 2 mm.

[0040] Preferably, a step surface is provided at the tail of the top cover outer panel drawing die surface, and the step surface and the V-shaped groove of the side shaping process surface constitute a reinforcing raised ridge for controlling the side pressure effect and improving the forming stability; the root of the R angle of the step surface is kept 10-15mm away from the tail trimming stop line, which is used for side shaping feed control and work hardening deformation in the subsequent process to improve the stability of the plane structure after forming; the front and rear sides of the top cover outer panel drawing die surface are provided with upturned circular holes for precise positioning in the subsequent process.

[0041] The above technical solution of the present invention has the following beneficial effects:

[0042] (1) The present application provides a top cover outer panel product structure to realize laser welding of the top cover outer panel; through the tail reinforcement raised ridge structure, the side pressure effect is controlled, and the stability of the plane structure after forming is improved through work hardening deformation, the rebound is reduced, and the accuracy and stability of the tail stop are improved.

[0043] (2) Through the tail movable punch structure and the side shaping punch process design, the cumulative tolerance of processing and assembly is reduced, and the difficulty of assembly and debugging is reduced. The side shaping area and the pressing part between the lower parting line 305 of the movable punch and the side pressing parting line 306 are designed as an integral structure and fixedly installed on the lower die base. This design effectively reduces the active area of ​​the side shaping and avoids the problem of difficult control of forming accuracy and poor stability of the double active structure of the upper side shaping movable concave die and the lower movable punch. When the mold reaches the bottom, it can be effectively fixed to ensure the shaping effect and improve the accuracy and quality of the mold surface. At the same time, it can also improve the pressing effect and improve wrinkling through effective fixing.

[0044] (3) The negative angle surfaces on both sides of the present application adopt a process scheme in which the drawing plane is directly side-shaped to achieve the product state. At the same time, the front and rear sections on both sides are segmented and side-shaped and positively shaped to ensure the feasibility of the mold structure. Then, in the final process, the corners are side-shaped in place, effectively completing more complex process contents in four processes, reducing the use of machine tools and equipment, and reducing the cost of mold tooling development.

[0045] (4) For the front sunroof, the double-pressing process of the inner edge ring is used to solve the problem of wrinkling on the flange.

[0046] (5) Reduce rebound and inhibit cracking through the design of tail R1, R2, and R3. BRIEF DESCRIPTION OF THE DRAWINGS

[0047] The accompanying drawings, which are incorporated in and constitute a part of the specification, illustrate embodiments of the invention and, together with the description, serve to explain the principles of the invention.

[0048] Figure 1 Existing top cover outer panel product structure diagram.

[0049] Figure 2 A partial enlarged view of both sides of the existing top cover outer panel.

[0050] Figure 3 This application is for the laser welding of the top cover outer panel product structure.

[0051] Figure 4 This application is for the laser welding of the local structure of the top cover outer panel product.

[0052] Figure 5 This is the process mold surface diagram of the laser welding top cover outer panel OP10 for this application.

[0053] Figure 6 This is the local process mold surface diagram of the tail of the laser-welded top cover outer panel OP10 for this application.

[0054] Figure 7 This is the process mold surface diagram of the laser welding top cover outer panel OP20 for this application.

[0055] Figure 8 This is the process mold surface diagram of the laser welding top cover outer panel OP30 for this application.

[0056] Fig. 9A This application provides a laser welding negative angle surface forming process for the front end of the laser welding top cover outer panel OP30.

[0057] Fig. 9B Schematic diagram of the front positive shaping insert.

[0058] Fig. 10A This is the laser welding negative angle surface forming process scheme for the rear end laser welding of the OP30 top cover outer panel for this application.

[0059] Fig. 10B It is a schematic diagram of the orthogonal sinking part.

[0060] Fig.11 This is the laser welding top cover outer panel OP30 tail forming process solution for this application.

[0061] Fig.12 This is a partial enlarged view of the laser welding top cover outer panel OP30 tail forming process scheme for this application.

[0062] Fig.13 This is the process mold surface diagram of the laser welding top cover outer panel OP40 for this application.

[0063] Among them: 106-upward parting line, 107-step surface, 201-circumferential trimming line, 202-waste knife, 203-secondary cutting waste knife, 205-skylight circumferential trimming line, 206-skylight waste knife, 3011-front skylight upper pressing parting line, 3012-front skylight lower pressing parting line, 302-rear skylight parting line, 303-active punch upper parting line, 304-side shaping parting line, 305-active punch lower parting line, 306-side pressing parting line, 307-triangle positioning, 308-side shaping stamping direction, 309-front side positive shaping insert, 3091-intersection sunken part, 310-front section side plastic insert, 3101-side intersection, 311-rear section positive plastic insert, 3111-orthogonal intersection sunken part, 312-reinforced raised ridge, 3121-small plane, 401-skylight side integral parting line, 402-front section side integral parting line, 403-rear section side integral parting line, R1-over-drawing convex fillet, 5-top cover outer panel, 6-A surface, 7-negative angle bevel, 8-welding fillet surface, 9-notch, R2-reverse concave fillet, R3-transition convex fillet, A-movable punch area, B-fixed punch area, C-side pressing area. DETAILED DESCRIPTION

[0064] Various exemplary embodiments of the present invention will now be described in detail with reference to the accompanying drawings. It should be noted that the relative arrangement of components and steps, numerical expressions and numerical values ​​set forth in these embodiments do not limit the scope of the present invention unless otherwise specifically stated.

[0065] Example 1

[0066] like Figure 3 and Figure 4 As shown, in the technical solution of the present invention, the flange structure in the prior art solution is cancelled on both sides of the laser-welded top cover outer panel. A laser-welded top cover outer panel product structure of the present application is suitable for laser welding of automobile bodies, including a top cover outer panel 5, and the top cover outer panel 5 is provided with A surfaces 6 on the left and right sides, and an inward-buckling negative angle bevel 7 is provided on the lower side of the A surface 6. The negative angle bevel 7 and the A surface 6 form a chamfered welding fillet surface 8, and notches 9 are respectively provided on the front corner, rear section and rear corner of the negative angle bevel 7. The length of the notch 9 is preferably 60 mm, and the distance between the edge of the notch 9 and the root of the R angle is 2 mm.

[0067] A step surface 107 is provided at the tail of the drawing die surface of the top cover outer panel 5. The step surface 107 and the V-shaped groove of the side shaping process surface constitute a reinforcing raised step 312 for controlling the side pressure effect and improving the forming stability; a width of 10-15mm is reserved between the root of the R angle of the step surface and the tail trimming stop line, which is used for side shaping feed control and work hardening deformation in the subsequent process to improve the stability of the plane structure after forming; upturned circular holes are provided on the front and rear sides of the drawing die surface of the top cover outer panel 5 for precise positioning in the subsequent process.

[0068] Example 2

[0069] A laser welding top cover outer panel forming process, the process comprising the following steps:

[0070] (1) Blank positioning: Place the blank on the punch press and perform initial positioning, with reference to the blank line position.

[0071] (2) Drawing forming: pressure is applied to the blank through a drawing die to form a roof outer panel with a predetermined shape.

[0072] OP10 drawing process:

[0073] like Figure 5 As shown, four upward-turned circular holes are provided on the front and rear sides for precise positioning in the later process. Drawing is performed with the circumferential parting line as the dividing line, and flanging is performed with the upward-turned parting line 106 as the boundary. A bottom mark is provided on the process supplementary surface of the diagonal non-product area to confirm whether the drawing forming is closed to the bottom in the later production process. The draw ribs are used to control the speed of the blank feeding in the forming process;

[0074] like Figure 6As shown, the outer side of the edge of the A surface of the tail product of the drawing die surface is provided with an over-drawing convex fillet R1, a transition convex fillet R3 connected to the side wall of the tail, and a reverse concave fillet R2 connecting the over-drawing convex fillet R1 and the transition convex fillet R3. By designing a stepped double fillet structure, the radius of the over-drawing convex fillet R1 can be ensured to be relatively small, so that it is as close to the product radius as possible to reduce the amount of subsequent shaping, thereby reducing shaping springback. At the same time, after drawing, the stress direction of the reverse concave fillet R2 is opposite to the stress direction of the over-drawing convex fillet R1, which can offset and improve certain springback. On the other hand, the radius of the transition convex fillet R3 can be designed to be relatively large, and the risk of cracking due to the relatively small radius of the over-drawing convex fillet R1 can be reduced through the step structure.

[0075] like Figure 6 As shown, the tail is also designed with a step surface 107, which is mainly used for the side shaping feed control of the later process OP30 and the work hardening deformation to improve the stability of the plane structure after forming. The step feature is drawn out in OP10, and the root of the R angle of the step surface is kept 10-15mm away from the trimming stop line of the tail.

[0076] (3) Trimming: remove excess material from the edge of the top cover outer panel to ensure a smooth edge.

[0077] OP20 trimming process:

[0078] like Figure 7 As shown, the trimming process adopts a process scheme that completes all trimming and cutting in one process. First, all the waste materials of the outer ring are completely removed along the peripheral trimming line 201, wherein waste cutters 202 are designed on the front and rear sides to cut the waste materials on the front and rear sides into small sections and discharge them from the mold; the large-sized sliding waste materials on both sides are made to slide down a certain distance as a whole, and then cut into multiple small-sized waste materials by the secondary cutting waste cutter 203, and then discharged; this waste discharge method can effectively improve the problem of iron chips.

[0079] The front and rear skylights are cut off as a whole along the skylight perimeter trimming line 205, and then cut into two ends respectively by the middle skylight waste cutter 206, and then discharged from the mold from the bottom inside the mold. Since the skylight perimeter waste is cut similar to punching, the waste is easy to get stuck on the cutting edge of the perimeter after cutting, especially the end of the waste cut in the middle. Therefore, in the technical solution of the present invention, the two ends of the OP20 lower mold skylight waste cutter 206 are respectively designed with raised shrinkage ribs at a distance of about 10mm from the end, so that the waste is deformed and shrunk by the shrinkage ribs after cutting, thereby forming a gap with the skylight perimeter cutting edge to avoid the waste being stuck.

[0080] OP30 flanging shaping process:

[0081] like Figure 8 As shown, this process mainly shapes the front side, the tail side, the front section side and the rear section on both sides, and at the same time, the front and rear skylights are shaped respectively.

[0082] Specifically, the front side bagh segment is positively shaped, and the abcd segment and the ghij segment are side shaped, wherein the overlapping parts of the ab segment and the gh segment are the intersection transition segments, and the intersection transition segments are first positively flanging the trimmed rear side through the intersection sinking part 3091 of the front side positive shaping insert 309, and then side shaping and transitioning through the side intersection part 3101 of the front section side shaping insert 310.

[0083] like Fig. 9A and Fig. 9B As shown, the intersection sinking part 3091 of the front positive shaping insert 309 is lower than the side intersection part 3101 to ensure the order of the forming process. As shown in the figure, in the technical solution of the present invention, the plane of the front section of abcd and the front section of ghij formed by drawing is directly subjected to side shaping to achieve the laser welding surface product state.

[0084] like Fig. 10A and Fig. 10B As shown, the cdef rear section and ijkl rear section on both sides are subjected to positive flanging shaping + triangular positioning 307 waste removal by the rear section positive shaping insert 311, wherein the cd section and the ij section are overlapping parts, similar to the front section structure, and the overlapping part of this area also adopts the rear section orthogonal connection sinking part 311-1 to first contact the plane after drawing and cutting for positive flanging, and then the side intersection part 310-1 of the front section side shaping insert is subjected to side flanging shaping. The same process scheme is used for the rear corners on both sides.

[0085] like Fig. 10A , Fig. 10B , Fig.11 As shown, the eflk segment is the side shaping portion, and the overlapping portion of the ef segment and the kl segment is first shaped positively by the orthogonal sinker 311-1 and then shaped sideways by the side shaping insert.

[0086] like Fig. 10A , Fig. 10B , Fig.11 , Fig.12 As shown in FIG. 1 , the tail negative angle product structure adopts side shaping, and the area between the upper parting line 303 of the movable punch and the lower parting line 305 of the movable punch is recorded as the movable punch area A, which is set as a negative angle movable punch, wherein the upper parting line 303 of the movable punch is the boundary line between the lower punch and the movable punch, and the lower parting line 305 of the movable punch is located in the bottom R angle area, as shown in FIG. Figure 8There is just no negative angle in the Z direction, and the distance from the side shaping parting line 304 is about 10mm (the distance of the Z-direction projection) to ensure that there is no interference in the operation of picking up and placing parts. The step 107 after drawing and forming forms a reinforcing convex ridge 312 with the V-shaped groove on the side shaping process surface. The front R angle intersection of the reinforcing convex ridge 312 is the side pressure material parting line 306, which is the boundary between the side pressure material core and the side shaping area; the reinforcing convex ridge 312 is about 2-3mm high, and a small plane 3121 about 5mm wide is set in the middle of the top, which can ensure that the sheet metal flows in slowly and deforms during the side shaping process to avoid excessive hardening or curling. At the same time, the sheet metal flows in and deforms through the reinforcing convex ridge 312 and then is side-shaped to form a V-shaped structural surface. The rigidity of the sheet metal in the corresponding area is increased after forming, with less rebound deformation and more stability.

[0087] On the other hand, during side shaping, the rear side of the side pressing parting line 306 is the side pressing area C. After the pressing core is pressed, the convex rib step structure can effectively form feeding resistance, improve the pressing effect, and improve the stability of the feeding process.

[0088] The area between the side shaping parting line 304 and the side pressing parting line 306 is all the side shaping area. In the technical solution of the present invention, only the negative angle part of the side shaping area (i.e., area A) is designed as the active punch area, and the side shaping area (fixed punch area B) and the pressing part between the movable punch lower parting line 305 and the side pressing parting line 306 are designed as an integral structure (fixed punch area C), which is fixedly installed on the lower die base. This design effectively reduces the active area of ​​the side shaping, avoids the problem of difficult control of forming accuracy and poor stability of the double active structure of the upper side shaping active concave die and the lower active punch. When the mold reaches the bottom, it can be effectively pierced to ensure the shaping effect, improve the accuracy and quality of the shaping die surface, and at the same time, the pressing effect can be improved by effectively piercing to improve wrinkling.

[0089] like Figure 8 As shown, in order to address the wrinkling of the front skylight flange, the technical solution of the present invention adopts a double-parting line and double-pressing forming process solution, in which the upper A-surface circle is the upper pressing parting line 3011 of the front skylight, which presses the A-surface of the A skylight circle; about 4mm inside the lower pressing parting line 3011 of the front skylight, there is a front skylight lower pressing parting line 3012, which is the boundary line of the lower pressing block. When the front skylight is flanged, the upper mold main body pressing core presses the product surface of the skylight circle, and the flanging shaping insert moves downward and works together with the inner pressing ring to press the skylight surface to be flanging. Then, as the upper mold flanging shaping insert moves downward, the sheet material gradually completes the flanging shaping. In this process, the sheet material of the skylight to be flanging is subjected to the inner pressing ring to achieve quasi-drawing forming of the sheet material, the forming process is stable, and the sheet material is overall flat and deformed under the action of the inner pressing ring, which can completely eliminate the problem of flanging wrinkles.

[0090] like Fig.11As shown, the side shaping stamping direction 308 of the tail movable punch movement direction, the side shaping oblique wedge shaping movement direction, and the side pressure core movement direction are the same angle stamping direction.

[0091] (4) Flanging and shaping: Flanging and shaping the edges of the top cover outer panel to form the desired final shape.

[0092] OP40 flanging shaping process: Fig.13 As shown, this process mainly performs side flanging shaping on the front sunroof along the sunroof side integral parting line 401, performs side shaping on the transition part of the front corner OP30 along the front section side integral parting line 402, and performs side shaping on the remaining positive shaping parts of OP30 on both sides of the rear section along the rear section side integral parting line 403 to achieve the product state.

[0093] The present application provides a laser welded top cover outer panel product structure for conventional spot-welded flange-type top cover outer panels; provides a stamping process and a mold structure to solve the problem of corrugated waves on the flanging of the skylight; provides a process mold surface and a stamping process solution to solve the problem of unstable rebound surface difference accuracy of the tail water flow groove surface, unstable side shaping feeding affecting the water flow groove surface difference and stop accuracy, rubber strip clamping and drainage effect; solves the problem that the product structure of the negative angle surfaces on both sides of the laser welded top cover outer panel can still be realized in four steps by a stamping process solution; solves the problem that the tail side shaping lower punch is an overall movable part with a large area, and there are accumulated tolerances in processing and assembly, which affects the assembly debugging and poor stability of the production process.

[0094] Although the present invention has been disclosed as above by the embodiments, it is not intended to limit the present invention. Any person skilled in the art may make various choices and modifications without departing from the spirit and scope of the present invention. Therefore, the protection scope of the present invention is limited by the claims and their equivalents.

Claims

1. A laser welding roof outer panel forming process, characterized in that: The process comprises the following steps: (1) Providing the blank and marking the blank line; (2) Execute the drawing process, set draw ribs to control the feed speed, design and form the convex and concave fillet structures on the edge of the A surface of the product to reduce springback, and form a step surface at the tail for feed control in subsequent processes and to improve the deformation resistance of the product; (3) Perform trimming process to trim all waste materials at one time, including removing excess material from the edge of the top cover outer panel and trimming the front and rear skylights and removing waste materials, and avoiding material jamming by shrinking the shrink ribs; (4) Perform flanging shaping processes, including front positive shaping, tail side shaping, both side shaping, and sunroof positive shaping. Design and use a movable punch structure to perform negative angle surface forming to reduce processing and assembly tolerances. Finally, perform precise flanging shaping on the product to ensure tail accuracy and stability.

2. The laser welding top cover outer panel forming process according to claim 1 is characterized in that: Step (2) specifically includes the following steps: (21) at least four upward-turned circular holes are provided on the front and rear sides for precise positioning in the subsequent process; the drawing is performed with the circumferential parting line as the dividing line, and the flanging is performed with the upward-turned parting line as the boundary to form the preliminary shape of the top cover outer panel; a bottom mark is provided on the process supplementary surface of the diagonal non-product area to confirm whether the drawing is closed to the bottom; and draw ribs are used to control the feeding speed of the blank during the forming process; (22) an over-drawing convex fillet, a transition convex fillet connected to the side wall of the tail, and a reverse concave fillet connecting the over-drawing convex fillet and the transition convex fillet are arranged on the outer side of the edge of the A surface of the tail product of the drawing die face; after drawing, the stress direction of the reverse concave fillet is opposite to the stress direction of the over-drawing convex fillet; (23) A step surface is provided at the tail end for feeding control and work hardening deformation in the subsequent process to improve the stability of the plane structure.

3. The laser welding top cover outer panel forming process according to claim 2 is characterized in that: In step (23), the root of the R angle of the step surface is kept 10-15 mm wide from the tail trimming stop line.

4. The laser welding top cover outer panel forming process according to claim 1 is characterized in that: Step (3) comprises the following steps: (31) All the waste materials of the outer ring are removed along the peripheral trimming line, and the waste cutter is designed to cut the waste materials on the front and rear sides into small sections and discharge them from the mold. The large-sized slipped waste materials are cut into multiple small-sized waste materials by the secondary cutting waste cutter and then discharged; (32) The front and rear skylights are cut off as a whole along the skylight perimeter trimming line, and the waste is cut into two sections by a skylight waste cutter and discharged.

5. The laser welding top cover outer panel forming process according to claim 1 is characterized in that: The flanging shaping described in step (4) includes: 1) Perform positive shaping on the anterior segment; 2) The front sections on both sides are subjected to side shaping. The transition section is first subjected to positive flanging through the intersection sinking part of the positive shaping insert, and then subjected to side shaping transition through the side intersection part of the front section side shaping insert; 3) The rear sections on both sides are subjected to positive flanging shaping and triangular positioning waste removal, wherein the overlapping part uses the rear section orthogonal sinking part to first contact the plane after drawing and cutting for positive flanging, and then the side intersection of the front section side shaping insert is used for side shaping; 4) Perform side shaping on the rear corner sections on both sides, wherein the overlapping parts are first shaped orthogonally by the sunken parts, and then shaped by the side shaping inserts.

6. The laser welding top cover outer panel forming process according to claim 1 is characterized in that: Step (4) also includes flange shaping for preventing the front side skylight flange from wrinkling, which includes the following steps: 1) The double parting line and double pressing forming process is used for the flanging shaping of the front sunroof; 2) The upper A-surface circumference is set as the upper pressing parting line of the front skylight, which is used to press the A-surface of the skylight circumference; 3) Design the front sunroof lower pressing parting line 4mm inside the upper pressing parting line of the front sunroof as the boundary line of the lower pressing block; 4) During the flanging process of the front skylight, the upper mold main body pressing core is used to press the product surface around the skylight, and at the same time, the flanging shaping insert moves downward and works together with the inner pressing ring to press the skylight surface to be flanging; 5) As the flanging shaping insert moves downward, the sheet metal gradually completes the flanging shaping. During this process, the sheet metal of the skylight to be flanging is subjected to a quasi-drawing forming process through the inner pressure ring.

7. The laser welding top cover outer panel forming process according to claim 1 is characterized in that: The design of step (4) and the use of a movable punch structure for negative angle surface forming are specifically as follows: 1) Select an appropriate movable punch structure to adapt to the negative angle surface forming; 2) defining a forming area A between the upper parting line of the movable punch and the side shaping parting line, wherein the area is formed by the movable punch; 3) In the forming area A, a movable punch is arranged, and the movable punch can be moved according to the forming needs to adapt to the forming requirements of different parts; 4) The side shaping area and the pressing part between the lower parting line of the movable punch and the side pressing parting line are designed as an integral structure and fixedly mounted on the lower die base to reduce the active area of ​​the side shaping, thereby avoiding the problem of difficult control of forming accuracy and poor stability of the double active structure of the upper side shaping movable concave die and the lower movable punch, thereby improving the forming accuracy and anti-deformation stability; 5) During the forming process, by controlling the movement of the active punch, the sheet metal after drawing is precisely formed with a negative angle surface to ensure that the formed sheet metal meets the design requirements.

8. The laser welding top cover outer panel forming process according to claim 1 is characterized in that: Step (4) also includes: performing side shaping on the front corner transition portion until it is in place and performing side shaping on the remaining positive shaping portions of the rear sections on both sides.

9. A laser welded roof outer panel product structure, suitable for laser welding of automobile bodies, characterized in that: It includes a top cover outer plate, the top of which is provided with an A surface, the lower side of which is provided with an inwardly buckled negative angle bevel, the negative angle bevel and the A surface form a rounded welding fillet surface, and notches are respectively provided on the front corner, rear section and rear section corner of the negative angle bevel.

10. The laser welded roof outer panel product structure according to claim 9, characterized in that: A step surface is arranged on the outer side of the tail of the drawing die surface of the outer panel of the top cover, and the step surface and the V-shaped groove of the side shaping process surface constitute a reinforcing raised ridge, which is used to control the side pressure effect and improve the forming stability; the root of the R angle of the step surface retains a width of 10-15mm from the tail trimming stop line, which is used for the side shaping feed control and work hardening deformation of the subsequent process to improve the stability of the plane structure after forming.

Citation Information

Patent Citations

  • Stamping and molding process of automobile roof covers and stamping die

    CN105382126A

  • Three-compartment automobile top cover tail flanging and shaping die

    CN110976649A

  • Automobile top cover shaping die and forming method

    CN113083941A

  • Automobile fender side flanging, side shaping and side punching composite die

    CN113695460A

  • Wedge shaping method, electronic equipment and storage medium

    CN115464049A

Cited By

  • Cold stamping part drawing forming structure, die and springback control method

    CN121198928A