I-shaped cutting knife machining method
Through metal powder injection molding and laser quenching technology, the problems of complex processing and insufficient edge sharpness of the I-shaped cutting knife are solved, cost savings and performance improvement are achieved, and the efficient use of the cutting knife is ensured.
Patent Information
- Application Number
- CN202410828345.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-25
- Publication Date
- 2024-10-22
AI Technical Summary
The existing I-shaped cutting knife has complex mechanical processing and high cost during the manufacturing process. The cutting edge of the cutting knife is not sharp enough, resulting in uneven tissue cutting. The cutting force may be large and the incision may be uneven. It is also easy to break or be pushed poorly during use, resulting in Stapler failure.
The cutting knife body is prepared by metal powder injection molding, and the edge hardness is increased by laser partial quenching, combined with magnetic polishing and passivation treatment to reduce friction.
The processing cost is reduced, the sharpness and tensile strength of the cutting blade are improved, the friction resistance is reduced, and the efficient use of the cutting blade is ensured.
Smart Images

Figure BDA0004911142220000061 
Figure HDA0004911142230000011
Abstract
Description
Technical Field
[0001] The invention belongs to the field of tool processing, and in particular relates to a method for processing an I-shaped cutting tool. Background Art
[0002] Currently, the I-shaped cutting blades of staplers on the market are mostly manufactured by integral machining and sharpening. Due to the limitations of the machining methods of the cutting blades, the following problems are prone to occur: (1) The machining methods of the cutting blades are complex and the machining costs are high; (2) The cutting blade edge is not sharp enough (hard enough), which affects tissue cutting. In severe cases, the cutting force is large, resulting in uneven tissue incisions, which in turn causes tissue lesions; (3) The cutting blade slides along the slide grooves provided on the staple magazine seat and the staple anvil seat. During the expected use, the free ends of the staple magazine and the staple anvil seat will gradually close or open, and the clamped tissue will generate large radial reaction forces and frictional forces, which may cause the cutting blade to break in a place with a small cross-sectional area or the cutting blade to be pushed poorly, which may easily cause stapler failure during surgery and normal cutting and anastomosis cannot be effectively implemented. Summary of the invention
[0003] The purpose of the present invention is to provide a method for processing an I-shaped cutting knife, which is easy to implement and simple to operate, and solves the technical problems raised in the above-mentioned background technology.
[0004] To achieve the above object, the present invention provides the following technical solutions:
[0005] A method for processing an I-shaped cutting knife comprises the following steps:
[0006] A. Metal powder injection molding is used to prepare the cutting blade body: martensitic stainless steel 440C powder is used as the raw material, mixed with a binder and injected into a molding mold. After molding, it is catalytically degreased, sintered, aged, and magnetically polished to form an unsharpened cutting blade blank;
[0007] B. Then, laser local quenching is performed on the 1.5mm width of the cutting edge, the quenching temperature is 1010-1070℃, and oil cooling (oil temperature is 20-25℃) is performed to obtain fine-grained martensite at the cutting edge; then, the cutting edge is sharpened on an automatic sharpening machine and then passivated.
[0008] Preferably, the fine-grained martensite comprises the following components in mass percentage: C: 0.9-1.2%, Cr: 16-18%, Nb: ≤3.5%, and the rest is iron.
[0009] Preferably, the catalytic degreasing includes mechanical degreasing, acid washing and high-pressure water washing degreasing.
[0010] Preferably, the sintering temperature is 1300-1350° C., and the sintering time is 100 minutes.
[0011] Preferably, the aging treatment method is: heating the cutting knife blank to 800-850°C, keeping it warm for one hour, and cooling it in air (air cooling to 20-25°C).
[0012] Preferably, during the magnetic polishing, an abrasive is first selected, and then the selected abrasive is placed in a polishing container of a magnetic polishing machine, an appropriate amount of polishing liquid is added to the container of the magnetic polishing machine, and a surfactant is provided, the cutting knife blank is placed in the magnetic polishing machine, the machine is started, a rotating magnetic field is generated, and the abrasive is rubbed against the surface of the cutting knife blank, and the polishing time is controlled to be 5-15 minutes; after the polishing is completed, the cutting knife blank is taken out for inspection, and the surface is cleaned in preparation for the next step.
[0013] Preferably, during the laser local quenching, the heating rate is controlled to be 980°C / s-1010°C / s.
[0014] Preferably, during the passivation treatment, the I-shaped cutting knife is placed in a passivation solution for full contact reaction to form a passivation film.
[0015] Through the above technical measures: the cutting knife adopts metal powder injection molding to prepare the body. Compared with the machining process, the powder metallurgy process has high material utilization rate and good processing performance, which can greatly reduce the cost. The body has good mechanical properties (tensile strength, yield strength), sintering temperature of 1300-1350℃, sintering time of 100 minutes, through this process condition, it provides conditions for the mutual flow, diffusion, melting, recrystallization and other processes of the powder particles in the green embryo, eliminates part or all of the pores, and makes the powder body more dense; aging treatment of 800-850℃, heat preservation for one hour, greatly reduces the internal stress of the product. Laser local quenching increases the hardness of the edge and the sharpness of the edge. It mainly reduces the processing cost, improves the sharpness of the edge and the strength of the body, and reduces the technical problems of friction resistance in the movement of the cutting knife.
[0016] Compared with the prior art, the present invention has the following beneficial effects:
[0017] The present invention adopts a new processing method, which can not only save processing costs, but also ensure the sharpness (hardness) and tensile strength and yield strength of the cutting blade, and can reduce friction to a certain extent. The present invention adopts a metal powder injection molding method to produce the product, and the cost is 30-35% of the mechanical processing method; local laser quenching at the edge can make the hardness of the edge reach 650-700HV, while the main body can still provide high tensile strength and yield strength; the surface roughness after magnetic polishing is less than 0.8, which meets the product use requirements. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1 It is a quenching schematic diagram of the present invention; DETAILED DESCRIPTION
[0019] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0020] Embodiment 1:
[0021] refer to Figure 1 , a method for processing an I-shaped cutting knife, comprising the following steps:
[0022] A. Metal powder injection molding is used to prepare the cutting blade body: martensitic stainless steel 440C powder is used as the raw material, mixed with a binder and injected into a molding mold. After molding, it is catalytically degreased, sintered, aged, and magnetically polished to form an unsharpened cutting blade blank;
[0023] B. Then, laser local quenching is performed on the cutting blade with a width of 1.5 mm at a quenching temperature of 1010, 1030, 1050 or 1070°C, and oil cooling is performed to obtain fine-grained martensite at the cutting blade edge; then, the cutting blade is sharpened on an automatic sharpening machine and then passivated.
[0024] The fine-grained martensite includes the following components in mass percentage: C: 0.9%, Cr: 16%, Nb: ≤3.5%, and the rest is iron.
[0025] Wherein, the catalytic degreasing includes mechanical degreasing, acid washing and high-pressure water washing degreasing.
[0026] Wherein, the sintering temperature is 1300°C.
[0027] Wherein, the aging treatment method is: heating the cutting knife blank to 810 or 820 or 830 or 840 or 850° C., and cooling in air (air cooling to 20-25° C.).
[0028] During the magnetic polishing, an abrasive is first selected, and then the selected abrasive is placed in a polishing container of a magnetic polishing machine, an appropriate amount of polishing liquid is added to the container of the magnetic polishing machine, and a surfactant is provided, and a cutting knife blank is placed in the magnetic polishing machine, and the machine is started to generate a rotating magnetic field, so that the abrasive and the surface of the cutting knife blank are rubbed, and the polishing time is controlled to be 5 or 7 or 9 or 13 or -15 minutes; after the polishing is completed, the cutting knife blank is taken out for inspection, and the surface is cleaned in preparation for the next step.
[0029] Wherein, during the laser local quenching, the heating rate is controlled to be 980°C / s.
[0030] Wherein, during the passivation treatment, the I-shaped cutting knife is placed in the passivation solution for full contact reaction to form a passivation film.
[0031] Among them, the present invention adopts a new processing method, which can not only save processing costs, but also ensure the sharpness (hardness) and tensile strength and yield strength of the cutting blade, and can reduce friction to a certain extent. The present invention adopts the method of metal powder injection molding to make the product, and the cost is 30-35% of the mechanical processing method; local laser quenching at the edge can make the hardness of the edge reach 650-700HV, while the main body can still provide high tensile strength and yield strength; the surface roughness after magnetic polishing is less than 0.8, which meets the product use requirements.
[0032] The powder and the binder are mixed at a stirring speed of 130-150 rpm, a stirring temperature of 60-70°C, and a stirring time of 30-50 minutes;
[0033] The injection molding method is to control the injection pressure to 132 MPa, control the injection temperature to 165-171° C., inject the material to be injected into the molding mold to obtain a green body;
[0034] The catalyst concentrated nitric acid is introduced into the degreasing furnace, and the temperature in the furnace chamber is 95-125℃
[0035] The green body is heated to 1300-1350° C. under a vacuum degree of 0.003-0.005 MPa, kept warm for 100 minutes, and then cooled to 20-25° C. to obtain a cutting blade blank;
[0036] Heat the cutting blade blank to 800-850℃, keep it warm for one hour, and cool it in air (air cooling to 20-25℃).
[0037] Put the selected abrasive into the polishing container of the magnetic polisher, add an appropriate amount of polishing liquid into the container of the magnetic polisher, and provide a surfactant, put the cutting knife blank into the magnetic polisher, start the machine, generate a rotating magnetic field, make the abrasive rub against the surface of the cutting knife blank, and control the polishing time to be 5-15 minutes; after the polishing is completed, take out the cutting knife blank for inspection and clean the surface;
[0038] The laser is used to heat the local surface of the cutting tool to above the phase change point. The laser power is 2kW, the scanning speed is 2cm / s, the surface temperature of the workpiece is controlled at about 1010-1070℃, and the oil is cooled at 20-25℃.
[0039] During the passivation treatment, the I-shaped cutting knife is placed in the passivation liquid for full contact reaction to form a passivation film.
[0040] Embodiment 2:
[0041] refer to Figure 1A method for processing an I-shaped cutting knife comprises the following steps: preparing a cutting knife body by metal powder injection molding: using martensitic stainless steel 440C powder as raw material, mixing with a binder and injecting it into a molding mold, and then catalytically degreasing, sintering, aging, and magnetic polishing are performed to make an unsharpened cutting knife blank after molding; then laser local quenching is performed on the cutting knife edge with a width of 1.5 mm, the quenching temperature is 1010 or 1030 or 1050 or 1070°C, and oil cooling is performed to obtain fine-grained martensite at the cutting knife edge; then, the cutting knife is sharpened on an automatic sharpening machine and then passivated.
[0042] The fine-grained martensite includes the following components in mass percentage: C: 1.2%, Cr: 18%, Nb: ≤3.5%, and the rest is iron.
[0043] Wherein, the catalytic degreasing includes mechanical degreasing, acid washing and high-pressure water washing degreasing.
[0044] Wherein, the sintering temperature is 1300 or 1320 or 1340 or 1350° C., and the sintering time is 100 minutes.
[0045] Wherein, the aging treatment method is: heating the cutting knife blank to 850°C and cooling it in air.
[0046] During the magnetic polishing, an abrasive is first selected, and then the selected abrasive is placed in a polishing container of a magnetic polishing machine, an appropriate amount of polishing liquid is added to the container of the magnetic polishing machine, and a surfactant is provided, and a cutting knife blank is placed in the magnetic polishing machine, and the machine is started to generate a rotating magnetic field, so that the abrasive and the surface of the cutting knife blank are rubbed, and the polishing time is controlled to be 5-15 minutes; after the polishing is completed, the cutting knife blank is taken out for inspection, and the surface is cleaned in preparation for the next step.
[0047] Wherein, during the laser local quenching, the heating rate is controlled to be 1010°C / s.
[0048] Wherein, during the passivation treatment, the I-shaped cutting knife is placed in the passivation solution for full contact reaction to form a passivation film.
[0049] Among them, the present invention adopts a new processing method, which can not only save processing costs, but also ensure the sharpness (hardness) and tensile strength and yield strength of the cutting blade, and can reduce friction to a certain extent. The present invention adopts the method of metal powder injection molding to make the product, and the cost is 30-35% of the mechanical processing method; local laser quenching at the edge can make the hardness of the edge reach 650-700HV, while the main body can still provide high tensile strength and yield strength; the surface roughness after magnetic polishing is less than 0.8, which meets the product use requirements.
[0050] Table 1: Chemical composition (%)
[0051] C Cr Nb Fe 0.9-1.2 16-18 ≤3.5 Bal.
[0052] Table 2: Performance comparison
[0053]
[0054] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A method for processing an I-shaped cutting knife, characterized in that: The following steps are involved: A. Metal powder injection molding is used to prepare the cutting blade body: martensitic stainless steel 440C powder is used as the raw material, mixed with a binder and injected into a molding mold. After molding, it is catalytically degreased, sintered, aged, and magnetically polished to form an unsharpened cutting blade blank; B. Then, laser local quenching is performed on the cutting blade with a width of 1.5 mm, with a quenching temperature of 1010-1070°C and oil cooling: the oil temperature is 20-25°C, so that the cutting blade obtains fine-grained martensite; then, the cutting blade is sharpened on an automatic sharpening machine and then passivated; The fine-grained martensite comprises the following components by mass percentage: C: 0.9-1.2%, Cr: 16-18%, Nb: ≤3.5%, and the rest is iron; The sintering temperature is 1300-1350° C. and the sintering time is 100 minutes; The aging treatment method is as follows: heating the cutting blade blank to 800-850°C, keeping the temperature for one hour, and cooling it to 20-25°C in air; During the magnetic polishing, an abrasive is first selected, and then the selected abrasive is placed in a polishing container of a magnetic polishing machine, an appropriate amount of polishing liquid is added to the container of the magnetic polishing machine, a surfactant is provided, and the cutting knife blank is placed in the magnetic polishing machine, the machine is started, a rotating magnetic field is generated, and the abrasive is rubbed against the surface of the cutting knife blank, and the polishing time is controlled to be 5-15 minutes; After polishing, take out the cutting knife blank for inspection and clean the surface in preparation for the next step.
2. The method for processing an I-shaped cutting blade according to claim 1, characterized in that: During the laser local quenching, the heating rate is controlled to be 980°C / s-1010°C / s.
3. The method for processing an I-shaped cutting knife according to claim 1, characterized in that: During the passivation treatment, the I-shaped cutting knife is placed in the passivation solution for full contact reaction to form a passivation film.
Citation Information
Cited By
Ice breaker blade injection molding method
CN121104101A