Five-axis laser shock die-free forming equipment and path optimization algorithm thereof

Through the five-axis laser shock mold-less forming equipment and its path optimization algorithm, the problems of low laser shock forming efficiency and difficult parameter control in the existing technology are solved, achieving efficient and precise forming of complex shapes, and enhancing the adaptability and adaptability of the equipment. reliability.

CN118808916AActive Publication Date: 2024-10-22NANJING UNIV OF AERONAUTICS & ASTRONAUTICS
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202410802417.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-20
Publication Date
2024-10-22
Estimated Expiration
2044-06-20

AI Technical Summary

Technical Problem

Existing laser shock forming technology has low efficiency when processing large-area complex structures, and the selection and control of laser parameters is demanding, which may cause material damage.

Method used

Using five-axis laser impact moldless forming equipment and its path optimization algorithm, by obtaining the current laser parameters, calculating the laser impact pressure and strain, judging the forming conditions, using the path optimization algorithm for path planning, adjusting the laser parameters, and building an optimization model to Improves impact path efficiency and accuracy.

Benefits of technology

It improves the accuracy and efficiency of complex shape manufacturing, enhances the adaptability and reliability of equipment, and reduces the risk of material damage.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118808916A_ABST
    Figure CN118808916A_ABST
Patent Text Reader

Abstract

The invention provides five-axis laser shock die-free forming equipment and a path optimization algorithm thereof. The method comprises the path optimization algorithm based on an XYZAC five-degree-of-freedom control system. Laser shock is carried out by adjusting laser parameters, and micro-forming experiments are carried out on different metal materials; a five-axis laser shock path optimization model is constructed, and laser parameter optimization is used for controlling microstructure forming of the metal surface; the influence of laser parameters and impact paths on the forming quality is studied, optimization experiments are carried out for different metal materials, and the forming quality and repeatability are remarkably improved. The method has wide application prospects in the field of metal micro-forming, the precision and efficiency of complex shape manufacturing are improved, and meanwhile the adaptability and reliability of equipment are enhanced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to laser shock processing technology, and in particular to a five-axis laser shock mold-free forming device and a path optimization algorithm thereof. Background Art

[0002] Metal microforming technology is particularly important in modern manufacturing, especially in high-tech fields such as microelectronics, aerospace and biomedicine. With the increasing demand for miniaturization and high precision, traditional mechanical processing methods can no longer meet complex manufacturing needs, which has promoted the development of new processing technologies.

[0003] As an emerging processing method, high-energy laser shock forming uses the shock wave generated by high-energy laser pulses to impact the metal surface, causing the material to undergo plastic deformation and achieve the formation of complex microstructures. This technology has the following significant advantages: non-contact processing, avoiding tool wear and workpiece deformation; concentrated energy, achieving high-precision microstructure forming; adjustable laser parameters, with high flexibility and controllability.

[0004] However, the existing technology still has some shortcomings, such as the local heat accumulation caused by energy concentration during laser shock process may damage the material, the selection and control of laser parameters require high standards, and the existing equipment has low efficiency when processing large-area complex structures.

[0005] Our research aims to solve these problems, optimize the laser shock forming process, improve efficiency and processing quality, and promote the application of this technology in industrial production. By deeply studying the influence of laser parameters on microstructure forming, we can provide a solid theoretical and practical foundation for the application of high-energy laser shock forming technology in metal microforming. Summary of the invention

[0006] In view of the defects of the prior art, the present invention provides a five-axis laser shock moldless forming device and a path optimization algorithm thereof. The present invention improves the precision and efficiency of complex shape manufacturing and enhances the adaptability and reliability of the device.

[0007] To achieve the purpose of the present invention, the technical solution adopted by the present invention is:

[0008] A five-axis laser shock mold-free forming device and a path optimization algorithm thereof, wherein the method comprises the following specific steps:

[0009] S1. Obtain current laser parameters (energy, frequency, pulse width);

[0010] S2, calculate laser shock pressure and strain based on material properties;

[0011] S3, judging the forming conditions, using the path optimization algorithm for path planning for rapid forming conditions, and adjusting the laser parameters for micro-forming experiments for fine forming conditions;

[0012] S4, judging the operation mode, building a path optimization model for the normal operation mode to optimize the control microstructure, and adjusting the laser parameters and path optimization forming quality for the abnormal processing mode;

[0013] S5, obtaining the best impact path by constructing an optimization model based on the parameters;

[0014] S6. Perform laser shock forming according to the optimal path and laser parameters.

[0015] Furthermore, the acquisition of current laser parameters in step S1 includes real-time measurement of laser energy, frequency and pulse width.

[0016] Furthermore, the calculation of laser shock pressure and strain in step S2 includes: calculating the pressure and strain generated by laser shock according to material properties and laser parameters to determine appropriate process parameters.

[0017] Furthermore, the working condition judgment in step S3 includes: rapid prototyping working condition and fine prototyping working condition; the rapid prototyping working condition performs path planning through a path optimization algorithm; the fine prototyping working condition performs micro-forming experiments by adjusting laser parameters;

[0018] The basic equation of laser-induced shock wave is derived from the law of conservation of energy, mass and momentum. Its one-dimensional plane expression is as follows:

[0019] Energy Conservation Equation: PU P =1 / 2ρ0U S Up 2 +ρ0U S (E-E0)

[0020] Mass conservation equation: ρ0U S =ρ(U S -U p )

[0021] Momentum conservation equation: (P-P0) = ρ0U S U P

[0022] Among them, ρ0 is the density before the wavefront, P0 is the pressure before the wavefront, and E0 is the energy before the wavefront; after the wavefront, ρ is the density of the medium after the wavefront, P is the shock wave pressure after the wavefront, and U S is the diffusion velocity of the wavefront behind the wavefront, E is the shock wave energy behind the wavefront; U p is the particle speed on and behind the wavefront, assuming that Up is zero, then the combined equation can be expressed as follows:

[0023]

[0024] The various parameters of the laser-induced shock wave can be solved by combining the above equations;

[0025] In the process of laser shock forming, the relationship between laser power density I0, pulse width τ, pulse energy E and spot diameter d can be expressed by the following formula:

[0026]

[0027] In order to increase the peak pressure of the shock wave, we proposed an innovative constraint model. In the laser shock forming process, by covering the metal surface with an absorption layer and a constraint layer, the peak pressure of the shock wave can be significantly increased. This paper mainly introduces our method for estimating the peak pressure of laser-induced shock waves under the constraint model, as well as the macroscopic equation of plasma motion proposed based on the law of conservation of energy and the theory of macroscopic gas expansion. According to the law of conservation of energy and the theory of macroscopic gas expansion, the macroscopic equation of plasma motion is given:

[0028]

[0029] Where: I(t) is the laser power density, P(t) is the laser-induced shock wave pressure, L(t) is the absorption layer thickness, V(t) is the plasma expansion velocity, Z1 is the acoustic impedance of the impacted target, and Z2 is the acoustic impedance of the confinement layer. The calculation formula for the peak pressure of the laser-induced shock wave can be obtained from the above two formulas:

[0030]

[0031] In the above formula, P max is the peak pressure, I0 is the laser power density, α is the efficiency of the laser and the metal material, and α is usually 0.1-0.2; in the formula, Z1 is the acoustic impedance of the laser-impacted material, Z2 is the acoustic impedance of the constrained layer, and Z is the composite acoustic impedance of Z1 and Z2; there are some ideal assumptions in the above Fabbro model, assuming that the surface of the impacted material is heated uniformly within the laser irradiation range; the constrained layer and the impacted material are isotropic; the plasma gasification state is regarded as an ideal gas; the plasma diffusion direction is only in the axial direction; in summary, the Fabbro formula fully considers the influence of the acoustic impedance of the absorption layer and the constrained layer on the induced shock wave, and also considers the efficiency of the laser and the metal foil, and the formula parameters are relatively easy to select, which can accurately estimate the peak pressure of the nanosecond laser-induced shock wave;

[0032] The strain rate estimation of laser shock induced plastic deformation is an important step in understanding the behavior of materials under laser shock. The strain rate describes the rate at which a material deforms per unit time. Usually, during high-energy laser shock, the strain rate is very high, reaching more than 10^6s^-1. The following is a method and steps for estimating the strain rate of laser shock induced plastic deformation:

[0033] Laser shock wave pressure: When a laser pulse acts on the surface of a material, it generates an instantaneous high-pressure shock wave. This pressure is usually calculated by the energy density of the laser.

[0034] Strain rate It is defined as the rate of change of strain ε with time t, and the formula is:

[0035]

[0036] The laser shock wave pressure (P) can be estimated by the following formula:

[0037]

[0038] I is the energy density of the laser, c is the sound velocity of the material, and R is the reflectivity of the material;

[0039] Calculate the plastic strain rate: Plastic strain rate It can be estimated by the shock wave pressure, material density and wave speed, the formula is:

[0040]

[0041] ρ is the density of the material.

[0042] Furthermore, the operation mode judgment in step S4 includes: a normal operation mode and an abnormal processing mode; in the normal operation mode, a path optimization model is constructed to optimize and control the metal surface microstructure forming; in the abnormal processing mode, laser parameters and impact paths are adjusted, and optimization experiments are performed to improve the forming quality;

[0043] Among them, only linear interpolation is used, that is, the cutting path is formed by connecting discrete points one by one. In the case of five-axis cladding, it is also necessary to specify the AC angle for the discrete points on the path, that is, the definition format of the printing path for a discrete point is:

[0044] X_Y_Z_A_C

[0045] In the above formula, the horizontal line represents the coordinate value or rotation angle. For two adjacent points, their X, Y, and Z coordinate values ​​are usually very close. In the case of unreasonable path normal vector planning, the deviation of the AC rotation angle of adjacent points will be large.

[0046] Suppose there are two adjacent points with similar X, Y, and Z coordinate values and When the normal line of a workpiece impact point coincides with the beam, the cladding surface is the top area of ​​the sphere, and the X, Y, and Z coordinate values ​​of P_1 and P_2 are very different. Due to data noise, Δθ and The difference is larger in the top area of ​​the surface (Δθ may be close to π, It may be close to π / 4). The control system interpolates according to the travel distance in the axis direction corresponding to a pulse signal. Therefore, for some coordinate positions between P_1 and P_2, the interpolation of the three axes X, Y, and Z may stop, that is, the coordinates remain stationary while waiting for the two axes AC to continue to rotate significantly. At this time, interference may occur;

[0047] In Δθ and In the case of a large diameter, it is necessary to raise the laser emitter to rotate the workpiece into position and then lower the laser emitter to continue cladding, or to perform point interpolation and densification processing on the path represented by line segments P_1 and P_2 to protect the workpiece. Although such processing can avoid damage to the workpiece, it still cannot avoid damage to the optical fiber caused by heat accumulation under long-term heating.

[0048] Furthermore, the step S5 of obtaining the best impact path by constructing an optimization model based on the parameters includes: calculating the best laser impact path by using laser parameters and a path optimization algorithm;

[0049] Since the normal vector is just a direction vector, we can assume that for n = (n x ,n y ,n z ) T For example, the center of rotation is the origin of the coordinate system. In order to make n coincide with the positive direction of the Z axis, the specific process is as follows:

[0050] ①The workpiece rotates around the Z axis by an angle θ so that the normal vector is located on the yOz plane;

[0051] ②The workpiece rotates around the X-axis by an angle φ so that the normal vector coincides with the positive direction of the Z-axis;

[0052] In this way, we can first calculate the vector [n x ,n y ] and the positive direction of the Y axis, and then the vector Calculating Angles According to the processing conditions, due to n z ≥0, that is, the normal vector must point to the side where the nozzle is located, and the value range does not need to be considered when optimizing the two corners A and C based on the normal vector. Therefore, by The normal vector defined can be written as

[0053]

[0054] The above formula is used to estimate Normal vector defined The deviation from the target surface normal vector, i.e., the objective function used to construct the optimization model;

[0055] For the AC angle obtained by the above method, there may be a situation where the C angle deviation of the adjacent points is close to ±2π. Because when the optimization iteration method is used to optimize each angle in the subsequent process, the initial value of the iteration needs to be as close to the optimal value as possible. Therefore, in order to make the deviation of the adjacent point angle as small as possible, the C angle of each point is optimized according to the 2π periodicity of the trigonometric function. Assume that the points on the discrete path are arranged in sequence [p0, p1, ... p i , p n ], where p i =[x i ,y i , z i , a i , c i ] Then use the following formula to calculate each c i To update:

[0056]

[0057] After the first round of optimization of the C angle of each point using the above formula, the difference between the C angles of any two adjacent points can be made no greater than π;

[0058] Assume that all C corners are arranged in the sequence C = [c0, c1, ... c n ],|C|=[|c0|,|c1|…|c n |], ΔC=[…, C i -c i-1 ] Then you can use

[0059] min(max(|ΔC|))

[0060] Indicates that the deviation of the corner near point C is as small as possible. Similarly,

[0061] min(max(|ΔA|))

[0062] It means that the deviation of the corner near point A is as small as possible;

[0063] Let n i and n(a i , c i ) represent the normal vector of the ith discrete point in the theoretical path and the normal vector of the ith point in the corner optimization defined by the AC corner according to the formula,

[0064] V (A, C) = [acos (n0n (a0, c0), acos (n1n (a1, c1)), ..., acos (n n n(α n , c n ))],then,

[0065] min(max(|V(A,C)|))

[0066] Indicates that the deviation between the normal vector defined by the current AC angle of each point and the normal vector of the theoretical path is as small as possible;

[0067] The mathematical model for optimizing each point on the machining path can be obtained:

[0068]

[0069] In the above optimization model, t = α + β + γ, A = (a0 + a1, ..., a n ), C=(c0,c1,…,c n ) respectively represent the vectors formed by the A and C angles of each point, and Δ represents the forward difference operator; the first two constraints are determined according to the software algorithm and actual working conditions. The first constraint is that the A axis always deflects in the positive direction and does not exceed 90°; the second constraint means that the maximum deviation between the nozzle axis and the normal vector of the cladding surface does not exceed 45°; there is no constraint on C, which means the angle of the C axis C∈(-∞,∞); the last two constraints are the constraints on the starting angle when the vector formed by the AC angles of each point on each row is iterated as an individual. There is no constraint on the first row, and the deviation of the angle between the end point of the subsequent row and the starting point of the current row cannot be greater than the threshold of the angle deviation of the adjacent points. The αβγ in the objective function represent the weights of each sub-optimization target respectively; since the sensitivity of C to the error is much greater than that of A in the two angles A and C, β>α≥γ, and β>0, α>0, γ>0 are taken to ensure that the values ​​of the three sub-targets are as small as possible when f(A,C) reaches the optimal value.

[0070] Furthermore, the step S6 of performing laser shock forming according to the optimal path and laser parameters includes: performing a laser shock forming process according to the optimized laser shock path and laser parameters to improve forming accuracy and repeatability.

[0071] Compared with the prior art, the present invention adopts the above technical solution and has the following beneficial effects: the present invention proposes a five-axis laser shock mold-free forming device and its path optimization algorithm, which improves the precision and efficiency of complex shape manufacturing, and at the same time enhances the adaptability and reliability of the equipment. BRIEF DESCRIPTION OF THE DRAWINGS

[0072] Figure 1 It is a flow chart of a five-axis laser shock mold-free forming device and a path optimization algorithm thereof of the present invention;

[0073] Figure 2 This is a schematic diagram of the five-axis laser shock machining path and the beam irradiation direction of the present invention;

[0074] Figure 3 A flow chart of the process of generating a theoretical tool path with a normal vector to a cladding processing instruction of the present invention;

[0075] Figure 4 It is a schematic diagram of the steps of calculating the AC angle from the normal vector of the present invention. DETAILED DESCRIPTION

[0076] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0077] like Figure 1 As shown, a five-axis laser shock mold-free forming device and a path optimization algorithm thereof specifically include the following steps:

[0078] S1. Obtain current laser parameters (energy, frequency, pulse width);

[0079] S2, calculate laser shock pressure and strain based on material properties;

[0080] S3, judging the forming conditions, using the path optimization algorithm for path planning for rapid forming conditions, and adjusting the laser parameters for micro-forming experiments for fine forming conditions;

[0081] S4, judging the operation mode, building a path optimization model for the normal operation mode to optimize the control microstructure, and adjusting the laser parameters and path optimization forming quality for the abnormal processing mode;

[0082] S5, obtaining the best impact path by constructing an optimization model based on the parameters;

[0083] S6. Perform laser shock forming according to the optimal path and laser parameters.

[0084] Furthermore, the acquisition of current laser parameters in step S1 includes real-time measurement of laser energy, frequency and pulse width.

[0085] Furthermore, the calculation of laser shock pressure and strain in step S2 includes: calculating the pressure and strain generated by laser shock according to material properties and laser parameters to determine appropriate process parameters.

[0086] Furthermore, the working condition judgment in step S3 includes: rapid prototyping working condition and fine prototyping working condition; the rapid prototyping working condition performs path planning through a path optimization algorithm; the fine prototyping working condition performs micro-forming experiments by adjusting laser parameters;

[0087] The basic equation of laser-induced shock wave is derived from the law of conservation of energy, mass and momentum. Its one-dimensional plane expression is as follows:

[0088] Energy Conservation Equation: PU P =1 / 2ρ0U S Up 2 +ρ0U S (E-E0)

[0089] Mass conservation equation: ρ0U S =ρ(U S -U p )

[0090] Momentum conservation equation: (P-P0) = ρ0U S U P

[0091] Among them, ρ0 is the density before the wavefront, P0 is the pressure before the wavefront, and E0 is the energy before the wavefront; after the wavefront, ρ is the density of the medium after the wavefront, P is the shock wave pressure after the wavefront, and U S is the diffusion velocity of the wavefront behind the wavefront, E is the shock wave energy behind the wavefront; U p is the particle speed on and behind the wavefront, assuming that U p is zero, then the combined equation can be expressed as follows:

[0092]

[0093] The various parameters of the laser-induced shock wave can be solved by combining the above equations;

[0094] In the process of laser shock forming, the relationship between laser power density I0, pulse width τ, pulse energy E and spot diameter d can be expressed by the following formula:

[0095]

[0096] In order to increase the peak pressure of the shock wave, we proposed an innovative constraint model. In the laser shock forming process, by covering the metal surface with an absorption layer and a constraint layer, the peak pressure of the shock wave can be significantly increased. This paper mainly introduces our method for estimating the peak pressure of laser-induced shock waves under the constraint model, as well as the macroscopic equation of plasma motion proposed based on the law of conservation of energy and the theory of macroscopic gas expansion. According to the law of conservation of energy and the theory of macroscopic gas expansion, the macroscopic equation of plasma motion is given:

[0097]

[0098] Where: I(t) is the laser power density, P(t) is the laser-induced shock wave pressure, L(t) is the absorption layer thickness, V(t) is the plasma expansion velocity, Z1 is the acoustic impedance of the impacted target, and Z2 is the acoustic impedance of the confinement layer. The calculation formula for the peak pressure of the laser-induced shock wave can be obtained from the above two formulas:

[0099]

[0100] In the above formula, P max is the peak pressure, I0 is the laser power density, α is the efficiency of the laser and the metal material, and α is usually 0.1-0.2; in the formula, Z1 is the acoustic impedance of the laser-impacted material, Z2 is the acoustic impedance of the constrained layer, and Z is the composite acoustic impedance of Z1 and Z2; there are some ideal assumptions in the above Fabbro model, assuming that the surface of the impacted material is heated uniformly within the laser irradiation range; the constrained layer and the impacted material are isotropic; the plasma gasification state is regarded as an ideal gas; the plasma diffusion direction is only in the axial direction; in summary, the Fabbro formula fully considers the influence of the acoustic impedance of the absorption layer and the constrained layer on the induced shock wave, and also considers the efficiency of the laser and the metal foil, and the formula parameters are relatively easy to select, which can accurately estimate the peak pressure of the nanosecond laser-induced shock wave;

[0101] The strain rate estimation of laser shock induced plastic deformation is an important step in understanding the behavior of materials under laser shock. The strain rate describes the rate at which a material deforms per unit time. Usually, during high-energy laser shock, the strain rate is very high, reaching more than 10^6s^-1. The following is a method and steps for estimating the strain rate of laser shock induced plastic deformation:

[0102] Laser shock wave pressure: When a laser pulse acts on the surface of a material, it generates an instantaneous high-pressure shock wave. This pressure is usually calculated by the energy density of the laser.

[0103] Strain rate It is defined as the rate of change of strain ε with time t, and the formula is:

[0104]

[0105] The laser shock wave pressure (P) can be estimated by the following formula:

[0106]

[0107] I is the energy density of the laser, c is the sound velocity of the material, and R is the reflectivity of the material;

[0108] Calculate the plastic strain rate: Plastic strain rate It can be estimated by the shock wave pressure, material density and wave speed, the formula is as follows,

[0109]

[0110] ρ is the density of the material.

[0111] like Figure 2 As shown in the figure, the line tangent path, the light beam reciprocates along the line tangent. In this study, only linear interpolation is used, that is, discrete points are connected point by point to represent Figure 2 In the case of five-axis cladding, it is also necessary to specify the AC angle for discrete points on the path, that is, the definition format of the print path for a discrete point is:

[0112] X_Y_Z_A_C

[0113] In the above formula, the horizontal line represents the coordinate value or rotation angle. For two adjacent points, their X, Y, and Z coordinate values ​​are usually very close. In the case of unreasonable path normal vector planning, the deviation of the AC rotation angle of the adjacent points will be large. Suppose there are two adjacent points with similar X, Y, and Z coordinate values and When the normal line of a workpiece impact point coincides with the beam, the cladding surface is the top area of ​​the sphere, and the X, Y, and Z coordinate values ​​of P_1 and P_2 are very different. Due to data noise, Δθ and The difference is larger in the top area of ​​the surface (Δθ may be close to π, It may be close to π / 4). The control system interpolates according to the travel distance in the axis direction corresponding to a pulse signal. Therefore, for some coordinate positions between P_1 and P_2, the interpolation of the three axes X, Y, and Z may stop, that is, the coordinates remain stationary while waiting for the two axes AC to continue to rotate significantly. At this time, interference may occur;

[0114] In Δθ and In the case of a large diameter, it is necessary to raise the laser emitter to rotate the workpiece into position and then lower the laser emitter to continue cladding, or to perform point interpolation and densification processing on the path represented by line segments P_1 and P_2 to protect the workpiece. Although such processing can avoid damage to the workpiece, it still cannot avoid damage to the optical fiber caused by heat accumulation under long-term heating.

[0115] like Figure 3 As shown in the figure, the process of generating the theoretical tool path with normal vector to the cladding processing instruction is to first convert the normal vector to the AC angle. On this basis, the AC angle of each point on the path is initially optimized, and the optimization model is constructed on the basis of the initial optimization to make the deviation of the AC angle of any two adjacent points as small as possible.

[0116] like Figure 4 As shown, since the normal vector is just a direction vector, we can assume that for n = (n x ,n y ,n z ) T For example, the center of rotation is the origin of the coordinate system, so in order to make n coincide with the positive direction of the Z axis:

[0117] ①The workpiece rotates around the Z axis by an angle θ so that the normal vector is located on the yOz plane;

[0118] ②The workpiece rotates around the X-axis by an angle φ so that the normal vector coincides with the positive direction of the Z-axis.

[0119] In this way, we can first calculate the vector [n x ,n y ] and the positive direction of the Y axis, and then the vector

[0120]

[0121] Calculating Angles According to the processing conditions, due to n z ≥0, that is, the normal vector must point to the side where the nozzle is located, and the value range does not need to be considered when optimizing the two corners A and C based on the normal vector. Therefore, by The normal vector defined can be written as

[0122]

[0123] The formula is used to estimate Normal vector defined The deviation from the target surface normal vector is the objective function used to construct the optimization model.

[0124] In addition, for Figure 3The AC angle obtained by the method shown may have a C angle deviation of the adjacent points close to ±2π. Because when the optimization iteration method is used to optimize each angle in the future, the initial value of the iteration needs to be as close to the optimal value as possible. Therefore, in order to minimize the deviation of the adjacent point angle, the C angle of each point is optimized according to the 2π periodicity of the trigonometric function. According to 2a, it is assumed that the points on the discrete path are arranged in a sequence [p0, p1, ... p i , p n ], where p i =[x i ,y i , z i , a i , c i ] Then use the following formula to calculate each c i To update:

[0125]

[0126] After the first round of optimization of the C angle of each point using the above formula, the difference between the C angles of any two adjacent points can be made no greater than π.

[0127] Assume that all C corners are arranged in the sequence C = [c0, c1, ... c n ],|C|=[|c0|,|c1|…|c n |], ΔC=[…, c i -c i-1 ], then you can use

[0128] min(max(|ΔC|))

[0129] Indicates that the deviation of the corner near point C is as small as possible. Similarly,

[0130] min(max(|ΔA|))

[0131] It means that the deviation of the corner near point A is as small as possible.

[0132] Let n i and n(a i , c i ) represent the normal vector of the ith discrete point in the theoretical path and the normal vector of the ith point in the corner optimization defined by the AC corner according to the above formula,

[0133] V(A,C)=[acos(n0n(a0,c0), acos(n1n(a1,c1)),…acos(n n n(a n , c n ))],then,

[0134] min(max(|V(A,C)|))

[0135] It means that the deviation between the normal vector defined by the current AC angle of each point and the normal vector of the theoretical path is as small as possible.

[0136] A mathematical model for optimizing each point on the machining path can be obtained

[0137]

[0138] In the above optimization model, t = α + β + γ, A = (a0 + a1, ..., a n ), C=(c0,c1,…,c n ) respectively represent the vectors formed by the A and C angles of each point, and Δ represents the forward difference operator. The first two constraints are determined according to the software algorithm and actual working conditions. The first constraint is that the A axis always deflects in the positive direction and does not exceed 90°. The second constraint indicates that the maximum deviation between the nozzle axis and the normal vector of the cladding surface does not exceed 45°. There is no constraint on C, which means that the angle of the C axis is C∈(-∞,∞). The last two constraints are the constraints on the starting angle when the vector formed by the AC angles of each point on each row is iterated as an individual. There is no constraint on the first row, and the deviation of the angle between the end point of the subsequent row and the starting point of the current row cannot be greater than the threshold of the angle deviation of the adjacent points. αβγ in the objective function represent the weights of each sub-optimization target. Since the sensitivity of C to the error is much greater than that of A in the two angles A and C, β>α≥γ, and β>0, α>0, γ>0 are taken to ensure that the values ​​of the three sub-targets are as small as possible when f(A,C) reaches the optimal value.

Claims

1. A five-axis laser shock mold-free forming device and its path optimization algorithm, characterized in that: The specific steps of the method are: S1. Obtain current laser parameters, including energy, frequency, and pulse width; S2, calculate laser shock pressure and strain based on material properties; S3, judging the forming conditions, using the path optimization algorithm for path planning for rapid forming conditions, and adjusting the laser parameters for micro-forming experiments for fine forming conditions; S4, judging the operation mode, building a path optimization model for the normal operation mode to optimize the control microstructure, and adjusting the laser parameters and path optimization forming quality for the abnormal processing mode; S5, obtaining the best impact path by constructing an optimization model based on the parameters; S6. Perform laser shock forming according to the optimal path and laser parameters.

2. According to claim 1, a five-axis laser shock mold-free forming device and a path optimization algorithm thereof are characterized in that: The acquisition of current laser parameters in step S1 includes real-time measurement of laser energy, frequency and pulse width.

3. According to claim 1, a five-axis laser shock mold-free forming device and a path optimization algorithm thereof are characterized in that: The calculation of laser shock pressure and strain in step S2 includes: calculating the pressure and strain generated by laser shock according to material properties and laser parameters to determine appropriate process parameters.

4. According to claim 1, a five-axis laser shock mold-free forming device and a path optimization algorithm thereof are characterized in that: The working condition judgment in step S3 includes: rapid prototyping working condition and fine prototyping working condition; the rapid prototyping working condition performs path planning through a path optimization algorithm; the fine prototyping working condition performs micro-forming experiments by adjusting laser parameters; The basic equation of laser-induced shock wave is derived from the law of conservation of energy, mass and momentum. Its one-dimensional plane expression is as follows: Energy Conservation Equation: PU P =1 / 2ρ0U S Up 2 +ρ0U S (E-E0) Mass conservation equation: ρ0U S =ρ(U S -U p ) Momentum conservation equation: (P-P0) = ρ0U S U P Among them, ρ0 is the density before the wavefront, P0 is the pressure before the wavefront, and E0 is the energy before the wavefront; after the wavefront, ρ is the density of the medium after the wavefront, P is the shock wave pressure after the wavefront, and U S is the diffusion velocity of the wavefront behind the wavefront, E is the shock wave energy behind the wavefront; U p is the particle speed on and behind the wavefront, assuming that U p is zero, then the combined equation can be expressed as follows: The various parameters of the laser-induced shock wave can be solved by combining the above equations; In the process of laser shock forming, the relationship between laser power density I0, pulse width τ, pulse energy E and spot diameter d can be expressed by the following formula: In order to increase the peak pressure of the shock wave, we proposed an innovative constraint model. During the laser shock forming process, by covering the metal surface with an absorption layer and a constraint layer, the peak pressure of the shock wave can be significantly increased. This paper mainly introduces our method for estimating the peak pressure of the laser-induced shock wave under the constraint model, as well as the macroscopic equation of plasma motion proposed based on the law of conservation of energy and the theory of macroscopic gas expansion. According to the law of conservation of energy and the theory of macroscopic gas expansion, the macroscopic equation of plasma motion is given: Where: I(t) is the laser power density, P(t) is the laser-induced shock wave pressure, L(t) is the absorption layer thickness, V(t) is the plasma expansion velocity, Z1 is the acoustic impedance of the impacted target, and Z2 is the acoustic impedance of the confinement layer. The calculation formula for the peak pressure of the laser-induced shock wave can be obtained from the above two formulas: In the above formula, P max is the peak pressure, I0 is the laser power density, α is the efficiency of the laser and the metal material, and α is usually 0.1-0.2; in the formula, Z1 is the acoustic impedance of the laser-impacted material, Z2 is the acoustic impedance of the constrained layer, and Z is the composite acoustic impedance of Z1 and Z2; there are some ideal assumptions in the above Fabbro model, assuming that the surface of the impacted material is heated uniformly within the laser irradiation range; the constrained layer and the impacted material are isotropic; the plasma gasification state is regarded as an ideal gas; the plasma diffusion direction is only in the axial direction; in summary, the Fabbro formula fully considers the influence of the acoustic impedance of the absorption layer and the constrained layer on the induced shock wave, and also considers the efficiency of the laser and the metal foil, and the formula parameters are relatively easy to select, which can accurately estimate the peak pressure of the nanosecond laser-induced shock wave; The strain rate estimation of laser shock induced plastic deformation is an important step in understanding the behavior of materials under laser shock. The strain rate describes the rate at which a material deforms per unit time. Usually, during high-energy laser shock, the strain rate is very high, reaching more than 10^6s^-1. The following is a method and steps for estimating the strain rate of laser shock induced plastic deformation: Laser shock wave pressure: When a laser pulse acts on the surface of a material, it generates an instantaneous high-pressure shock wave. This pressure is usually calculated by the energy density of the laser. Strain rate It is defined as the rate of change of strain ε with time t, and the formula is: The laser shock wave pressure (P) can be estimated by the following formula: I is the energy density of the laser, c is the sound velocity of the material, and R is the reflectivity of the material; Calculate the plastic strain rate, Plastic strain rate It can be estimated by the shock wave pressure, material density and wave speed, the formula is: ρ is the density of the material.

5. The five-axis laser shock mold-free forming equipment and path optimization algorithm thereof according to claim 1, characterized in that: The operation mode determination in step S4 includes: a normal operation mode and an abnormal processing mode; in the normal operation mode, a path optimization model is constructed to optimize and control the metal surface microstructure forming; in the abnormal processing mode, laser parameters and impact paths are adjusted, and optimization experiments are performed to improve the forming quality; Among them, only linear interpolation is used, that is, the cutting path is formed by connecting discrete points one by one. In the case of five-axis cladding, it is also necessary to specify the AC angle for the discrete points on the path, that is, the definition format of the printing path for a discrete point is: X_Y_Z_A_C In the above formula, the horizontal line represents the coordinate value or rotation angle. For two adjacent points, their X, Y, and Z coordinate values ​​are usually very close. In the case of unreasonable path normal vector planning, the deviation of the AC rotation angle of the adjacent points will be large. Suppose there are two adjacent points with similar X, Y, and Z coordinate values and When the normal of a workpiece impact point coincides with the beam, the cladding surface is the top area of ​​the sphere, and the X, Y, and Z coordinate values ​​of P_1 and P_2 are very different. Due to data noise, Δθ and The difference is larger in the top area of ​​the surface (Δθ may be close to π, It may be close to π / 4). The control system interpolates according to the travel distance in the axis direction corresponding to a pulse signal. Therefore, for some coordinate positions between P_1 and P_2, the interpolation of the three axes X, Y, and Z may stop, that is, the coordinates remain stationary while waiting for the two axes AC to continue to rotate significantly. At this time, interference may occur; It can be seen that in Δθ and In the case of a larger error, it is necessary to raise the laser emitter to allow the workpiece to rotate into place and then lower the laser emitter to continue cladding, or to perform point interpolation and densification processing on the path represented by line segments P_1 and P_2. Although such processing can avoid damage to the workpiece, it still cannot avoid damage to the optical fiber caused by heat accumulation under long-term heating.

6. The five-axis laser shock mold-free forming equipment and path optimization algorithm thereof according to claim 1, characterized in that: The step S5 of obtaining the best impact path by constructing an optimization model based on the parameters includes: calculating the best laser impact path by using laser parameters and a path optimization algorithm; Since the normal vector is only a direction vector, we can assume that for n = (n x ,n y ,n z ) T For example, the center of rotation is the origin of the coordinate system. In order to make n coincide with the positive direction of the Z axis, the specific process is as follows: ①The workpiece rotates around the Z axis by an angle θ so that the normal vector is located on the yOz plane; ②The workpiece rotates around the X-axis by an angle φ so that the normal vector coincides with the positive direction of the Z-axis; In this way, we can first calculate the vector [n x ,n y ] and the positive direction of the Y axis, and then the vector Calculating Angles According to the processing conditions, due to n z ≥0, that is, the normal vector must point to the side where the nozzle is located, and the value range does not need to be considered when optimizing the two corners A and C based on the normal vector. Therefore, by The normal vector defined can be written as The above formula is used to estimate Normal vector defined The deviation from the target surface normal vector, i.e., the objective function used to construct the optimization model; For the AC angle obtained by the above method, there may be a situation where the C angle deviation of the adjacent points is close to ±2π. Because when the optimization iteration method is used to optimize each angle in the subsequent optimization, it is also necessary to iterate the initial value as close to the optimal value as possible. Therefore, in order to make the deviation of the adjacent point angle as small as possible, the C angle of each point is optimized according to the 2π periodicity of the trigonometric function. Assume that the points on the discrete path are arranged in sequence [p0, p1, ... p i ,p n ], where p i =[x i ,y i , z i , a i , c i ] Then use the following formula to calculate each c i Make an update After the first round of optimization of the C angle of each point using the above formula, the difference between the C angles of any two adjacent points can be made no greater than π; Assume that all C corners are arranged in the sequence C = [c0, c1, ... c n ],|C|=[|c0|,|c1|,…|c n |],ΔC=[…,c i -c i-1 ], then you can use min(max(|ΔC|)) Indicates that the deviation of the corner near point C is as small as possible. Similarly, min(max(|ΔA|)) It means that the deviation of the corner near point A is as small as possible; Let n i and n(a i ,c i ) represent the normal vector of the ith discrete point in the theoretical path and the normal vector of the ith point in the corner optimization defined by the AC corner according to the formula, V(A,C)=[acos(n0n(a0,c0), acos(n1n(a1,c1)),…, acos(n n n(a n , c n ))]then, min(max(|V(A,C)|)) Indicates that the deviation between the normal vector defined by the current AC angle of each point and the normal vector of the theoretical path is as small as possible; The mathematical model for optimizing each point on the machining path can be obtained: In the above optimization model, t = α + β + γ, A = (a0 + a1, ..., a n ), C=(c0,c1,…,c n ) respectively represent the vectors formed by the A and C angles of each point, and Δ represents the forward difference operator; the first two constraints are determined according to the software algorithm and actual working conditions. The first constraint is that the A axis always deflects in the positive direction and does not exceed 90°; the second constraint means that the maximum deviation between the nozzle axis and the normal vector of the cladding surface does not exceed 45°; there is no constraint on C, which means the angle of the C axis C∈(-∞,∞); the last two constraints are the constraints on the starting angle when the vector formed by the AC angles of each point on each row is iterated as an individual. There is no constraint on the first row, and the deviation of the angle between the end point of the subsequent row and the starting point of the current row cannot be greater than the threshold of the angle deviation of the adjacent points. The αβγ in the objective function represent the weights of each sub-optimization target respectively; since the sensitivity of C to the error is much greater than that of A in the two angles A and C, β>α≥γ, and β>0, α>0, γ>0 are taken to ensure that the values ​​of the three sub-targets are as small as possible when f(A,C) reaches the optimal value.

7. The five-axis laser shock mold-free forming equipment and path optimization algorithm thereof according to claim 1, characterized in that: The step S6 of performing laser shock forming according to the optimal path and laser parameters includes: performing a laser shock forming process according to the optimized laser shock path and laser parameters to improve forming accuracy and repeatability.

Citation Information

Patent Citations

  • Accurate three-dimensional printing

    CN108883575A

  • AC corner optimization method for five-axis 3D printing line cutting path planning

    CN113119450A

  • Method for determining laser strengthening area and strengthening parameters of blade

    CN117438006A

  • Method, Control Unit and Laser Cutting System for Combined Path and Laser Process Planning for Highly Dynamic Real-Time Systems

    US20230271276A1

  • Multi-axis linkage laser superfinishing method and device

    WO2024032054A1