Novel wear-resistant environment-friendly CMP (chemical mechanical polishing) pad and preparation method thereof

By using the main layer and multi-layer structure design of environmentally friendly materials such as polyurethane and alumina mixture in the CMP polishing pad, combined with technologies such as self-healing and high-temperature resistant layers, the problems of short polishing pad life, insufficient wear resistance and poor environmental protection are solved , achieving a more stable, environmentally friendly and durable polishing pad.

CN118809435APending Publication Date: 2024-10-22SUZHOU RUNDE NEW MATERIAL
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202410843151.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-27
Publication Date
2024-10-22

AI Technical Summary

Technical Problem

Existing CMP polishing pads have short service life, insufficient wear resistance, not environmentally friendly materials, and unstable self-adhesive connections during use, resulting in loose bonding and difficulty in cleaning up disassembly residues.

Method used

It uses a mixture of polyurethane and alumina as the main layer, combines the coating, lubricating layer, elastic layer, stabilizing layer and filler layer, sets positioning grooves and ring grooves, and adds a self-repairing layer, high temperature resistant layer, The nanolayer and connection layer use environmentally friendly materials and detachable connection designs, and are prepared through vacuum degassing and thermal curing processes.

Benefits of technology

Significantly improves the wear resistance, service life and stability of the polishing pad, reduces environmental pollution, enhances connection stability, reduces residues and extends the use time when used under high temperature conditions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118809435A_ABST
    Figure CN118809435A_ABST
Patent Text Reader

Abstract

The invention provides a novel wear-resistant environment-friendly CMP polishing pad and a preparation method thereof, and relates to the field of polishing pads. The novel wear-resistant environment-friendly CMP polishing pad comprises a main body structure, a bonding structure is connected to the lower end of the main body structure in a bonding mode, the main body structure comprises a body layer, an elastic layer and a stable layer are arranged at the upper end and the lower end of the body layer respectively, and a lubricating layer and a filler layer are arranged on the other side of the elastic layer and the other side of the stable layer respectively. The surface of the lubricating layer is coated with a coating, a positioning groove is formed in the center of the end face of the main body structure, a plurality of wide grooves are formed in the upper end face of the main body structure, and a plurality of annular grooves are formed between every two adjacent wide grooves. By adding related materials of the coating, the lubricating layer, the elastic layer, the stable layer and the filler layer in the main body structure, the wear resistance, the hardness and the stability of the whole body during use are greatly improved, the safety during use is ensured, and the service life of the whole body is effectively prolonged.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of polishing pads, in particular to a novel wear-resistant and environmentally friendly CMP polishing pad and a preparation method thereof. Background Art

[0002] CMP (Chemical Mechanical Polishing) polishing pad is an important auxiliary material used in semiconductor manufacturing process. It is used in the planarization process in semiconductor chip manufacturing, mainly used to remove the unevenness of silicon wafer surface, so that its surface becomes smooth. CMP polishing pad is usually made of polyurethane material, with certain softness and wear resistance. There are tiny particles on its surface, which can play a grinding role together with chemical solution in the polishing process, and remove the protrusion and defect of silicon wafer surface by mechanical force and chemical reaction at the same time. CMP polishing pad plays a key role in semiconductor manufacturing, and its performance directly affects the quality and output of chip. With the continuous advancement of chip manufacturing process, the requirements for CMP polishing pad are also getting higher and higher, and it is necessary to have better polishing effect, longer service life and more stable performance.

[0003] However, the existing CMP polishing pads still have some shortcomings and areas for improvement during actual use. The existing CMP polishing pads will have certain wear during use, resulting in a limited lifespan and poor overall wear resistance. During the polishing process, particles, chemicals and waste liquids generated by wear may cause pollution to the environment. At the same time, the overall materials used in the preparation process of the existing CMP polishing pads are not environmentally friendly, and most of the existing polishing pads are installed and connected with self-adhesive glue during installation, which can easily lead to unstable bonding and loosening during long-term use. At the same time, residues are easily generated during disassembly, which is not easy to clean. Therefore, technicians in this field provide a new type of wear-resistant and environmentally friendly CMP polishing pad and a preparation method thereof to solve the problems raised in the above background technology. Summary of the invention

[0004] 1. Technical issues to be resolved

[0005] In view of the deficiencies in the prior art, the present invention provides a new type of wear-resistant and environmentally friendly CMP polishing pad and a preparation method thereof, which solves the problems of the existing polishing pad having a short service life, insufficient overall wear resistance, environmentally unfriendly materials, and insufficient stability when connected with self-adhesive glue.

[0006] (II) Technical solution

[0007] To achieve the above objectives, the present invention is implemented through the following technical solutions: a new type of wear-resistant and environmentally friendly CMP polishing pad, including a main structure, the lower end of the main structure is bonded to a bonding structure, the main structure includes a body layer, the upper and lower ends of the body layer are respectively provided with an elastic layer and a stabilizing layer, the other sides of the elastic layer and the stabilizing layer are respectively provided with a lubricating layer and a filler layer, the surface of the lubricating layer is coated with a coating, a positioning groove is provided at the center of the end face of the main structure, a plurality of wide grooves are provided on the upper end face of the main structure, and a plurality of annular grooves are respectively provided between each adjacent two wide grooves.

[0008] Preferably, the bonding structure includes a connecting layer, and a high-temperature resistant layer and a nano layer are respectively provided at the upper and lower ends of the connecting layer, and a self-healing layer and a release paper are respectively provided on the other side of the high-temperature resistant layer and the nano layer, and a through hole is provided at the center of the lower end surface of the bonding structure, and the upper end of the through hole passes through the lower end surface of the bonding structure and reaches the upper end, and the position of the through hole corresponds to the positioning groove up and down.

[0009] Preferably, the release paper and the adhesive structure are detachably connected.

[0010] Preferably, the material of the body layer is a mixture of polyurethane and aluminum oxide.

[0011] Preferably, the coating is made of carbon nanotubes, the lubricating layer is made of silicone oil or polyethylene glycol, the elastic layer is made of polyester resin, the stabilizing layer is made of antioxidant or UV absorber, and the filler layer is made of one or more of biodegradable plastics, plant fibers, calcium carbonate, cellulose fibers and starch particles.

[0012] Preferably, the self-healing layer is made of microcapsules, the high temperature resistant layer is made of polyetheretherketone or polyimide, the connecting layer is made of charged polymer film, and the nano layer is made of nano-silicon dioxide or nano-aluminum oxide.

[0013] A method for preparing a novel wear-resistant and environmentally friendly CMP polishing pad, characterized in that it comprises the following steps:

[0014] S1. Select a suitable substrate, select a substrate with high wear resistance and environmental protection characteristics, and ensure that the selected material has good mechanical properties and chemical stability;

[0015] S2. Pretreatment: clean the surface of the selected material to remove possible impurities and contaminants. Solvent cleaning and surface activation methods can be used for pretreatment to ensure that the material surface is clean;

[0016] S3. Prepare a slurry, mix the selected substrate with the solvent and add the material required for the body layer inside, then add the coating, lubricating layer, elastic layer, stabilizing layer and filler layer to mix the materials used inside, and stir them thoroughly according to the formula ratio;

[0017] S4. Mixing and pouring: prepare the mold, ensure that the mold surface is smooth and apply mold release agent, pour the mixed material into the mold for pouring;

[0018] S5. Vacuum degassing, vacuum degassing treatment of the cast material in the above step to remove bubbles and ensure uniformity after casting;

[0019] S6. Curing and molding, heat curing or ultraviolet curing can be used, the cast material is placed in a curing device for curing, and after curing, the cured polishing pad is removed and demolded;

[0020] S7. Surface treatment: Surface treatment is performed on the cured polishing pad to improve its surface smoothness and compatibility with the polishing liquid.

[0021] (III) Beneficial effects

[0022] The present invention provides a novel wear-resistant and environmentally friendly CMP polishing pad and a preparation method thereof. It has the following beneficial effects:

[0023] 1. In the present invention, by adding relevant materials such as coating, lubricating layer, elastic layer, stabilizing layer and filling layer inside the main structure, the wear resistance, hardness and stability of the whole during use are greatly improved, the safety during use is ensured, the service life of the whole is effectively improved, the use time is extended, and the materials used inside are all environmentally friendly materials, which can be recycled and reused, while reducing pollution to the environment.

[0024] 2. In the present invention, by setting the bonding structure to be composed of the materials required for the self-repairing layer, the high temperature resistant layer, the nano layer and the connecting layer, the stability of the connection with the main structure is ensured, while the overall bonding degree during the connection is improved, and the scope of application is expanded. It can be operated under high temperature conditions, and the residue is reduced during disassembly, and the bonding is more stable.

[0025] 3. In the present invention, by providing a plurality of wide grooves and annular grooves on the upper end surface of the main structure, it is convenient to add polishing liquid inside during polishing, thereby improving the use effect during polishing, and the positioning groove at the lower end is convenient for positioning during installation. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] Figure 1 It is an axonometric diagram of the overall structure of the present invention;

[0027] Figure 2It is a front view of the present invention;

[0028] Figure 3 It is a partial axonometric cross-sectional view of the main structure of the present invention;

[0029] Figure 4 It is an axonometric drawing from another perspective in the present invention;

[0030] Figure 5 A top view of the present invention;

[0031] Figure 6 It is a partial axonometric cross-sectional view of the bonding structure in the present invention.

[0032] Among them, 1. main structure; 101. wide groove; 102. annular groove; 103. coating; 104. lubricating layer; 105. elastic layer; 106. main body layer; 107. stabilizing layer; 108. packing layer; 109. positioning groove; 2. bonding structure; 201. through hole; 202. self-healing layer; 203. high temperature resistant layer; 204. connecting layer; 205. nano layer; 206. release paper. DETAILED DESCRIPTION

[0033] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0034] Embodiment 1:

[0035] like Figure 1-6 As shown, an embodiment of the present invention provides a novel wear-resistant and environmentally friendly CMP polishing pad, including a main structure 1, the lower end of the main structure 1 is bonded to a bonding structure 2, the main structure 1 includes a body layer 106, the upper and lower ends of the body layer 106 are respectively provided with an elastic layer 105 and a stabilizing layer 107, the other sides of the elastic layer 105 and the stabilizing layer 107 are respectively provided with a lubricating layer 104 and a filler layer 108, the surface of the lubricating layer 104 is coated with a coating 103, a positioning groove 109 is provided at the center of the end face of the main structure 1, a plurality of wide grooves 101 are provided on the upper end face of the main structure 1, and a plurality of annular grooves 102 are respectively provided between each two adjacent wide grooves 101.

[0036] The bonding structure 2 includes a connecting layer 204, and a high-temperature resistant layer 203 and a nano layer 205 are respectively provided at the upper and lower ends of the connecting layer 204, and a self-repairing layer 202 and a release paper 206 are respectively provided on the other sides of the high-temperature resistant layer 203 and the nano layer 205. A through hole 201 is provided at the center of the lower end surface of the bonding structure 2, and the upper end of the through hole 201 passes through the lower end surface of the bonding structure 2 and reaches the upper end, and the through hole 201 corresponds to the position of the positioning groove 109 up and down.

[0037] The release paper 206 is detachably connected to the adhesive structure 2. The main body layer 106 is made of a mixture of polyurethane and aluminum oxide to enhance the overall wear resistance. The coating 103 is made of carbon nanotubes, which have high wear resistance, corrosion resistance, antibacterial properties, and optical properties. The lubricating layer 104 is made of silicone oil or polyethylene glycol, which can reduce the friction coefficient between the polishing pad and the workpiece, reduce energy loss and improve polishing efficiency. The elastic layer 105 is made of polyester resin, which is a type of organic matter soluble in the base material, and can improve the softness, elasticity and ductility of the polishing pad, thereby increasing its service life and improving the polishing effect. The stabilizing layer 107 is made of antioxidants or ultraviolet absorbers, which are additives that can improve the stability and anti-aging ability of the polishing pad, and can slow down the hardening, aging and deformation speed of the polishing pad during use, thereby extending its service life. The filler layer 108 is made of one or more of biodegradable plastics, plant fibers, calcium carbonate, cellulose fibers and starch particles, which can improve the polishing effect while being degradable to reduce pollution to the environment.

[0038] The self-healing layer 202 is made of microcapsules filled with repair agents. When the material is damaged, the microcapsules can rupture and release the repair agents, thereby achieving self-repair of the material. The high-temperature resistant layer 203 is made of polyetheretherketone or polyimide, which has high temperature resistance, high strength and good chemical stability. The connecting layer 204 is made of a charged polymer film, and the connecting layer 204 is also the base layer, which provides the necessary mechanical strength and durability for the back glue. The nanolayer 205 is made of nano-silicon dioxide or nano-alumina, which mainly serves to increase the bonding strength.

[0039] A method for preparing a novel wear-resistant and environmentally friendly CMP polishing pad comprises the following steps:

[0040] S1. Select a suitable substrate, select a substrate with high wear resistance and environmental protection characteristics, and ensure that the selected material has good mechanical properties and chemical stability;

[0041] S2. Pretreatment: clean the surface of the selected material to remove possible impurities and contaminants. Solvent cleaning and surface activation methods can be used for pretreatment to ensure that the material surface is clean;

[0042] S3. Prepare a slurry, mix the selected substrate with the solvent and add the material required for the body layer 106 inside, then add the coating 103, the lubricating layer 104, the elastic layer 105, the stabilizing layer 107 and the filler layer 108 to mix the materials used inside, and stir them thoroughly according to the formula ratio;

[0043] S4. Mixing and pouring: prepare the mold, ensure that the mold surface is smooth and apply mold release agent, pour the mixed material into the mold for pouring;

[0044] S5. Vacuum degassing, vacuum degassing treatment of the cast material in the above step to remove bubbles and ensure uniformity after casting;

[0045] S6. Curing and molding, heat curing or ultraviolet curing can be used, the cast material is placed in a curing device for curing, and after curing, the cured polishing pad is removed and demolded;

[0046] S7. Surface treatment: Surface treatment is performed on the cured polishing pad to improve its surface smoothness and compatibility with the polishing liquid.

[0047] Working principle: This application is a new type of wear-resistant and environmentally friendly CMP polishing pad and its preparation method.

[0048] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A novel wear-resistant and environmentally friendly CMP polishing pad, comprising a main structure (1), characterized in that: The lower end of the main structure (1) is bonded to an adhesive structure (2), the main structure (1) comprises a main body layer (106), the upper and lower ends of the main body layer (106) are respectively provided with an elastic layer (105) and a stabilizing layer (107), the other sides of the elastic layer (105) and the stabilizing layer (107) are respectively provided with a lubricating layer (104) and a filler layer (108), the surface of the lubricating layer (104) is coated with a coating (103), a positioning groove (109) is provided at the center of the end face of the main structure (1), a plurality of wide grooves (101) are provided on the upper end face of the main structure (1), and a plurality of annular grooves (102) are respectively provided between each two adjacent wide grooves (101).

2. A novel wear-resistant and environmentally friendly CMP polishing pad according to claim 1, characterized in that: The bonding structure (2) comprises a connecting layer (204), wherein the upper and lower ends of the connecting layer (204) are respectively provided with a high temperature resistant layer (203) and a nano layer (205), and the other sides of the high temperature resistant layer (203) and the nano layer (205) are respectively provided with a self-repairing layer (202) and a release paper (206), and a through hole (201) is provided at the center of the lower end surface of the bonding structure (2), and the upper end of the through hole (201) passes through the lower end surface of the bonding structure (2) and reaches the upper end, and the position of the through hole (201) corresponds to that of the positioning groove (109) in the upper and lower directions.

3. A new type of wear-resistant and environmentally friendly CMP polishing pad according to claim 2, characterized in that: The release paper (206) and the adhesive structure (2) are detachably connected.

4. The novel wear-resistant and environmentally friendly CMP polishing pad according to claim 1, characterized in that: The material of the main body layer (106) is a mixture of polyurethane and aluminum oxide.

5. The novel wear-resistant and environmentally friendly CMP polishing pad according to claim 1, characterized in that: The coating (103) is made of carbon nanotubes, the lubricating layer (104) is made of silicone oil or polyethylene glycol, the elastic layer (105) is made of polyester resin, the stabilizing layer (107) is made of an antioxidant or an ultraviolet absorber, and the filler layer (108) is made of one or more of biodegradable plastics, plant fibers, calcium carbonate, cellulose fibers and starch particles.

6. The novel wear-resistant and environmentally friendly CMP polishing pad according to claim 2, characterized in that: The material of the self-repairing layer (202) is microcapsules, the material of the high temperature resistant layer (203) is polyetheretherketone or polyimide, the material of the connecting layer (204) is a charged polymer film, and the material of the nano layer (205) is nano silicon dioxide or nano aluminum oxide.

7. A method for preparing a novel wear-resistant and environmentally friendly CMP polishing pad, characterized in that: The following steps are involved: S1. Select a suitable substrate, select a substrate with high wear resistance and environmental protection characteristics, and ensure that the selected material has good mechanical properties and chemical stability; S2. Pretreatment: clean the surface of the selected material to remove possible impurities and contaminants. Solvent cleaning and surface activation methods can be used for pretreatment to ensure that the material surface is clean; S3. Prepare a slurry, mix the selected substrate with a solvent and add the material required for the body layer (106) therein, then add the materials used for the coating layer (103), the lubricating layer (104), the elastic layer (105), the stabilizing layer (107) and the filler layer (108) therein, mix them, and stir them thoroughly according to the formula ratio; S4. Mixing and pouring: prepare the mold, ensure that the mold surface is smooth and apply mold release agent, pour the mixed material into the mold for pouring; S5. Vacuum degassing, vacuum degassing treatment of the cast material in the above step to remove bubbles and ensure uniformity after casting; S6. Curing and molding, heat curing or ultraviolet curing can be used, the cast material is placed in a curing device for curing, and after curing, the cured polishing pad is removed and demolded; S7. Surface treatment: Surface treatment is performed on the cured polishing pad to improve its surface smoothness and compatibility with the polishing liquid.

Citation Information

Patent Citations

  • Special CMP (chemical mechanical polishing) pad for 12-inch wafer and manufacturing method of special CMP pad

    CN115401624A

  • Olefinic thermoplastic elastomer sheet, process for production thereof, and laminates

    CN1745113A

  • Chemical mechanical polishing pad for wafer

    CN213999050U

  • Method of manufacturing grooved polishing pad and polishing process

    JP2004314215A

  • Polishing pad with improved fluidity of slurry and process for preparing the same

    JP2019217627A