Manufacturing method of semiconductor structure, semiconductor structure and semiconductor joint structure
By forming a passivation layer and trenches on the metal layer in semiconductor manufacturing, and processing the dielectric material layer with the top surface of the passivation layer as the grinding end point, the problem of voids on the joint surface of the semiconductor structure is solved, and the quality and joint strength of the semiconductor structure are improved. .
Patent Information
- Application Number
- CN202310385935.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-04-07
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2043-04-07
AI Technical Summary
During the semiconductor manufacturing process, bumps are easily formed on the top surface of the wafer, resulting in gaps on the joint surface when the wafers are bonded and unable to be tightly bonded, affecting the quality and bonding strength of the semiconductor structure.
Form a passivation layer on the metal layer, and through the steps of forming trenches and filling the dielectric material layer, optimize the process sequence with the top surface of the passivation layer as the grinding stop end point, remove the height difference part of the dielectric material layer, and reduce the film layer The thickness and groove depth improve the flatness of the joint surface.
By adjusting the process sequence and processing steps, the manufacturing process is optimized, the quality of the semiconductor structure and the tightness of the joint surface are improved, void defects are avoided, and the solid connection between the semiconductor structure and other structures is enhanced.
Smart Images

Figure CN118824940A_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to the field of semiconductor technology, and in particular to a method for manufacturing a semiconductor structure, a semiconductor structure, and a semiconductor bonding structure. Background Art
[0002] With the development of integrated circuit manufacturing technology, the integration of integrated circuits continues to increase, and the requirements for the precision of various components in integrated circuits are also increasing. In the semiconductor manufacturing process, it is easy for protrusions to form on the top surface of the wafer in the back-end process, and a large height difference is produced on the top surface of the wafer, resulting in gaps on the bonding surface after the wafer is bonded to other wafers, and the wafers cannot be tightly bonded. Summary of the invention
[0003] The following is a summary of the subject matter of the detailed description of the present disclosure. This summary is not intended to limit the scope of the claims.
[0004] The present disclosure provides a method for manufacturing a semiconductor structure, a semiconductor structure, and a semiconductor bonding structure.
[0005] A first aspect of the present disclosure provides a method for manufacturing a semiconductor structure, the method comprising:
[0006] providing a metal layer;
[0007] forming a passivation layer, the passivation layer covering the top surface of the metal layer;
[0008] forming at least one groove, wherein the groove at least penetrates the passivation layer;
[0009] forming a dielectric material layer, wherein the dielectric material layer fills the groove and covers the top surface of the passivation layer;
[0010] The dielectric material layer is ground with the top surface of the passivation layer as a grinding stop point, and the dielectric material layer retained by grinding forms a dielectric layer in the groove.
[0011] Optionally, the metal layer is formed on the interlayer dielectric layer, and forming at least one trench comprises:
[0012] A first trench is formed, wherein the first trench penetrates the passivation layer and the metal layer, and the first trench exposes a top surface of the interlayer dielectric layer.
[0013] Optionally, the manufacturing method comprises:
[0014] Depositing a dielectric material to fill the first trench and cover the top surface of the passivation layer to form a first dielectric material layer;
[0015] The first dielectric material layer is ground with the top surface of the passivation layer as a grinding stop point, and the ground first dielectric material layer forms a first dielectric layer, which is located in the first groove and divides the metal layer into a metal circuit layer.
[0016] Optionally, forming at least one trench comprises:
[0017] A second trench is formed, wherein the second trench penetrates the passivation layer, and the second trench exposes a top surface of the metal layer.
[0018] Optionally, the manufacturing method comprises:
[0019] Depositing a dielectric material to fill the second trench and cover the top surface of the passivation layer to form a second dielectric material layer;
[0020] The second dielectric material layer is ground with the top surface of the passivation layer as a grinding stop point to form a second dielectric layer in the second groove.
[0021] Optionally, the manufacturing method further comprises:
[0022] removing a portion of the second dielectric layer to form a first through hole in the second dielectric layer, wherein the first through hole exposes a top surface of the metal layer;
[0023] A metal interconnect structure is formed in the first via.
[0024] Optionally, forming a metal interconnection structure in the first through hole includes:
[0025] forming a first metal material layer, the first metal material layer filling the first through hole and covering the top surface of the passivation layer;
[0026] The first metal material layer is ground with the top surface of the passivation layer as a grinding stop point, and the ground first metal material layer forms the metal interconnection structure.
[0027] A second aspect of the present disclosure provides a semiconductor structure, the semiconductor structure comprising:
[0028] Metal layer;
[0029] a passivation layer, the passivation layer covering a top surface of the metal layer;
[0030] at least one groove, the groove at least passing through the passivation layer;
[0031] a dielectric layer, located in the groove;
[0032] The semiconductor structure includes a first surface including a top surface of the dielectric layer and a top surface of the passivation layer.
[0033] Optionally, the metal layer is disposed on the interlayer dielectric layer, and the semiconductor structure includes:
[0034] A first trench, penetrating the passivation layer and the metal layer;
[0035] The dielectric layer includes a first dielectric layer, the first dielectric layer fills the first trench, the first dielectric layer is connected to the interlayer dielectric layer, and the first dielectric layer divides the metal layer into metal circuit layers.
[0036] Optionally, the semiconductor structure comprises:
[0037] A second groove, penetrating the passivation layer;
[0038] The dielectric layer includes a second dielectric layer, the second dielectric layer fills the second trench, and the second dielectric layer covers a portion of the top surface of the metal layer.
[0039] Optionally, the semiconductor structure further includes:
[0040] The metal interconnection structure is arranged in the second dielectric layer, and the metal interconnection structure penetrates the second dielectric layer and is in contact with the metal layer.
[0041] Optionally, the first surface also includes a top surface of the metal interconnect structure
[0042] Optionally, the first dielectric layer has an air gap therein, and a top surface of the air gap is lower than the first surface.
[0043] A third aspect of the present disclosure provides a semiconductor bonding structure, comprising a first semiconductor structure and a second semiconductor structure, wherein the first semiconductor structure and the second semiconductor structure both adopt the semiconductor structure as described in the second aspect of the present disclosure;
[0044] The first surface of the first semiconductor structure and the first surface of the second semiconductor structure are arranged opposite to each other, the first surface of the first semiconductor structure and the first surface of the second semiconductor structure are connected together, and at the connection surface between the first semiconductor structure and the second semiconductor structure, the dielectric layer of the first semiconductor structure and the dielectric layer of the second semiconductor structure are bonded and connected, and the passivation layer of the first semiconductor structure and the passivation layer of the second semiconductor structure are bonded and connected.
[0045] In the semiconductor structure manufacturing method, semiconductor structure, and semiconductor bonding structure provided by the embodiments of the present disclosure, a passivation layer is formed on the entire metal layer before the metal layer is etched by adjusting the process sequence, thereby reducing the thickness of the film layer formed on the metal layer, and then performing the steps of forming a groove and forming a dielectric material layer to fill the groove. The dielectric material layer is ground with the top surface of the passivation layer as the grinding stop point, thereby optimizing the process, improving the processing efficiency, and improving the quality of the formed semiconductor structure.
[0046] Other aspects will be apparent upon reading and understanding the drawings and detailed description. BRIEF DESCRIPTION OF THE DRAWINGS
[0047] The accompanying drawings incorporated into the specification and constituting a part of the specification illustrate embodiments of the present disclosure and are used together with the description to explain the principles of the embodiments of the present disclosure. In these drawings, similar reference numerals are used to represent similar elements. The drawings described below are some embodiments of the present disclosure, rather than all embodiments. For those skilled in the art, other drawings can be obtained based on these drawings without paying creative work.
[0048] Figure 1 is a schematic diagram of a metal layer formed in the related art.
[0049] Figure 2 It is a schematic diagram after a metal circuit layer is formed in the related art.
[0050] Figure 3 It is a schematic diagram after forming a dielectric material layer and a passivation layer in the related art.
[0051] Figure 4 It is a schematic diagram of grinding the top surface of the passivation layer into a plane in the related art.
[0052] Figure 5 It is a schematic diagram after the second trench is formed in the related art.
[0053] Figure 6 It is a schematic diagram of forming a polymer layer to fill the second trench in the related art.
[0054] Figure 7 It is a schematic diagram of a metal interconnection structure formed in the related art.
[0055] Figure 8 is a schematic diagram of a semiconductor structure formed in the related art.
[0056] Fig. 9 It is a schematic diagram of the bonding connection between a semiconductor structure and other structures in the related art.
[0057] Fig.10The invention is a flow chart of a method for manufacturing a semiconductor structure according to an exemplary embodiment.
[0058] Fig.11 The invention is a flow chart of a method for manufacturing a semiconductor structure according to an exemplary embodiment.
[0059] Fig.12 is a schematic diagram of a metal layer according to an exemplary embodiment.
[0060] Fig.13 is a schematic diagram showing a passivation layer formed according to an exemplary embodiment.
[0061] Fig.14 is a schematic diagram showing a groove formed according to an exemplary embodiment.
[0062] Fig.15 is a schematic diagram showing a dielectric material layer after being formed according to an exemplary embodiment.
[0063] Fig.16 is a schematic diagram showing a dielectric layer formed according to an exemplary embodiment.
[0064] Fig.17 is a schematic diagram showing a groove formed according to an exemplary embodiment.
[0065] Fig.18 is a schematic diagram showing a dielectric material layer after being formed according to an exemplary embodiment.
[0066] Fig.19 is a schematic diagram showing a dielectric layer formed according to an exemplary embodiment.
[0067] Fig. 20 is a schematic diagram showing a first trench formed according to an exemplary embodiment.
[0068] Fig.21 is a schematic diagram showing a first dielectric material layer after being formed according to an exemplary embodiment.
[0069] Fig. 22 is a schematic diagram showing a first dielectric layer after being formed according to an exemplary embodiment.
[0070] Fig.23 is a schematic diagram showing a second trench formed according to an exemplary embodiment.
[0071] Fig.24 is a schematic diagram showing a second dielectric material layer after being formed according to an exemplary embodiment.
[0072] Fig.25 is a schematic diagram showing a second dielectric layer after being formed according to an exemplary embodiment.
[0073] Fig.26 is a schematic diagram showing a first through hole formed according to an exemplary embodiment.
[0074] Fig. 27 is a schematic diagram showing a first metal material layer after being formed according to an exemplary embodiment.
[0075] Fig.28 is a schematic diagram showing a metal interconnection structure after being formed according to an exemplary embodiment.
[0076] Fig.29 is a schematic diagram showing a semiconductor bonding structure according to an exemplary embodiment.
[0077] Reference numerals:
[0078] 10. metal layer; 11. first barrier layer; 12. second barrier layer; 20. passivation layer; 21. groove; 121. first groove; 221. second groove; 30. dielectric material layer; 130. first dielectric material layer; 230. second dielectric material layer; 40. dielectric layer; 140. first dielectric layer; 141. air gap; 240. second dielectric layer; 241. first through hole; 50. interlayer dielectric layer; 60. metal interconnect structure; 61. metal wire; 62. contact pad; 70. first metal material layer; 80. metal line layer; 100a. first surface;
[0079] h1, first preset height; h2, second preset height;
[0080] 110, first semiconductor structure; 210, second semiconductor structure; 110a, first surface of the first semiconductor structure; 210a, first surface of the second semiconductor structure; 120, passivation layer of the first semiconductor structure; 220, passivation layer of the second semiconductor structure; 160, metal interconnection structure of the first semiconductor structure; 260, metal interconnection structure of the second semiconductor structure;
[0081] 10', metal layer; 20', passivation layer; 121', first trench; 221', second trench; 30', dielectric material layer; 50', interlayer dielectric layer; 60', metal interconnect structure; 80', metal circuit layer; 90', polymer layer. DETAILED DESCRIPTION
[0082] In order to make the purpose, technical solutions and advantages of the embodiments of the present disclosure clearer, the technical solutions in the disclosed embodiments will be clearly and completely described below in conjunction with the drawings in the embodiments of the present disclosure. Obviously, the described embodiments are part of the embodiments of the present disclosure, rather than all of the embodiments. Based on the embodiments in the present disclosure, all other embodiments obtained by those skilled in the art without making creative work are within the scope of protection of the present disclosure. It should be noted that the embodiments in the present disclosure and the features in the embodiments can be arbitrarily combined with each other without conflict.
[0083] In the related art, metal circuit layers and metal interconnect structures are formed in the semiconductor back-end process, using the following implementation methods:
[0084] like Figure 1 As shown, after forming the metal layer 10' on the interlayer dielectric layer 50', the metal layer 10' is patterned, as shown in FIG. Figure 2 As shown, a first trench 121' is formed in the metal layer 10', and the first trench 121' divides the metal layer 10' into a metal line layer 80'. Then, as shown in FIG. Figure 3 As shown, the dielectric material is deposited to fill the first trench 121' and cover the top surface of the metal wiring layer 80' to form a dielectric material layer 30'. The thickness of the dielectric material layer 30' on the top surface of the metal wiring layer 80' is generally between 850nm and 1000nm. However, in the process of depositing the dielectric material, the first trench 121' may not be fully filled, resulting in the height of the top surface of the dielectric material layer 30' in the area filling the first trench 121' being higher than the height of the top surface of the dielectric material layer 30' in other areas, resulting in a height difference on the top surface of the dielectric material layer 30'.
[0085] Then, if Figure 3 As shown, a passivation layer 20' is formed on the top surface of the dielectric material layer 30'. The thickness of the passivation layer 20' is generally 850nm-1000nm. Affected by the height difference of the top surface of the dielectric material layer 30', the top surface of the passivation layer 20' also has a height difference.
[0086] like Figure 4 As shown, the passivation layer 20' is processed by chemical mechanical polishing (CMP) to grind the top surface of the passivation layer 20' into a flat surface. After grinding, the total thickness of the dielectric material layer 30' and the passivation layer 20' on the metal circuit layer 80' is about 1700nm-2000nm. Then, as Figure 5As shown, the passivation layer 20' and the dielectric material layer 30' located on the top surface of the metal wiring layer 80' are etched to form a second groove 221'. The second groove 221' layer penetrates the passivation layer 20' and the first dielectric layer 140' located on the top surface of the metal wiring layer 80'. The second groove 221' exposes the top surface of the metal wiring layer 80'. The depth of the second groove 221' is 1700nm-2000nm.
[0087] Then, if Figure 6 As shown, refer to Figure 5 , a polymer layer 90' is formed, and the polymer layer 90' fills the second trench 221' and covers the top surface of the passivation layer 20'. Figure 7 As shown, a metal interconnection structure 60 ′ is formed in the second trench 221 ′.
[0088] Since the second groove 221' is very deep, after the polymer layer 90' is formed, the top surface of the polymer layer 90' in the second groove 221' is lower than the top surface of the polymer layer 90' on the passivation layer 20', and the polymer layer 90' is usually soft and not suitable for semiconductor structures and other structures. It is necessary to use a chemical mechanical polishing process to polish and remove the polymer layer 90' on the top surface of the passivation layer 20', but the polymer layer 90' is soft and it is impossible to polish the polymer layer 90' and the dielectric material layer 30' at the same polishing rate. Figure 8 As shown in FIG. 1 , even after grinding, the height difference of the top surface of the semiconductor structure cannot be completely eliminated, that is, the top surface of the finally formed semiconductor structure still has a height difference. Fig. 9 As shown, voids are likely to appear at the connection surfaces between the semiconductor structure and other semiconductor structures. Especially when the semiconductor structure is bonded to other semiconductor structures using a hybrid bonding (HB) process, the void problem will become more serious.
[0089] In view of this, an exemplary embodiment of the present disclosure provides a method for manufacturing a semiconductor structure, comprising the following steps: providing a metal layer; forming a passivation layer, the passivation layer covers the top surface of the metal layer, the passivation layer has a first preset height, and the top surface of the passivation layer is a plane; forming at least one groove, the groove at least penetrates the passivation layer; forming a dielectric material layer, the dielectric material layer fills the groove and covers the top surface of the passivation layer; grinding the dielectric material layer with the top surface of the passivation layer as the grinding stop point, and grinding the retained dielectric material layer to form a dielectric layer in the groove. The present disclosure adjusts the process sequence, forms a passivation layer on the entire metal layer before etching the metal layer, reduces the thickness of the film layer formed on the metal layer, and then performs the steps of forming the groove and forming the dielectric material layer to fill the groove, and grinds the dielectric material layer with the top surface of the passivation layer as the grinding stop point, thereby optimizing the process, improving the processing efficiency, and improving the quality of the formed semiconductor structure.
[0090] In an exemplary embodiment of the present disclosure, a method for manufacturing a semiconductor structure is provided. Fig.10 As shown, Fig.10 A flowchart of a method for manufacturing a semiconductor structure provided according to an exemplary embodiment of the present disclosure is shown. Figure 12-Figure 19 The schematic diagram of each stage of the semiconductor structure manufacturing method is shown below. Figure 12-Figure 19 The method of manufacturing semiconductor structures is introduced.
[0091] The present embodiment does not limit the semiconductor structure. The semiconductor structure will be described below by taking a dynamic random access memory (DRAM) as an example, but the present embodiment is not limited thereto. The semiconductor structure in the present embodiment may also be other structures.
[0092] like Fig.10 As shown, a method for manufacturing a semiconductor structure provided by an exemplary embodiment of the present disclosure includes the following steps:
[0093] Step S110: providing a metal layer.
[0094] like Fig.12 As shown, the metal layer 10 can be set on a semiconductor substrate or a semiconductor wafer. The metal layer 10 is a material layer used to form a semiconductor element. The material of the metal layer 10 can include aluminum or aluminum alloy layer, tungsten or tungsten alloy layer, titanium or titanium alloy layer, etc.
[0095] Step S120: forming a passivation layer, wherein the passivation layer covers the top surface of the metal layer.
[0096] like Fig.13As shown, the passivation layer 20 may be formed on the top surface of the metal layer 10 by a deposition process. It is understood that after deposition, the top surface of the passivation layer 20 may be ground by a grinding process to grind the top surface of the passivation layer 20 into a plane.
[0097] Step S130: forming at least one trench, wherein the trench at least penetrates the passivation layer.
[0098] In some examples, such as Fig.14 As shown, the groove 21 may penetrate the passivation layer 20 and the metal layer 10, and the groove 21 exposes the film layer under the metal layer 10. Alternatively, in other examples, such as Fig.17 As shown, a trench 21 may be formed in the passivation layer 20 , the trench 21 penetrating the passivation layer 20 and exposing a top surface of the metal layer 10 .
[0099] Step S140: forming a dielectric material layer, wherein the dielectric material layer fills the trench and covers the top surface of the passivation layer.
[0100] like Fig.15 , reference Fig.14 As shown, or Fig.18 , refer to Fig.17 As shown, a deposition process may be used to deposit dielectric material, and the dielectric material fills the groove 21 and covers the top surface of the passivation layer 20 to form a dielectric material layer 30. The presence of the groove 21 causes a concave defect or a convex defect to be formed on the top surface of the dielectric layer 40 located on the groove 21, and the top surface of the dielectric layer 40 has a height difference.
[0101] Step S150: grinding the dielectric material layer with the top surface of the passivation layer as the grinding stop point, and grinding the retained dielectric material layer to form a dielectric layer in the groove.
[0102] like Fig.16 , reference Fig.15 As shown, or Fig.19 , refer to Fig.18 As shown in the figure, the dielectric material layer 30 is ground with the top surface of the passivation layer 20 as the grinding stop point. For example, white light endpoint detection or advanced process control (APC) technology can be used to detect the top surface of the passivation layer 20. When the top surface of the passivation layer 20 is detected, the grinding is stopped, and the dielectric material layer 30 located on the top surface of the passivation layer 20 is removed. The dielectric material layer 30 located in the groove 21 is retained to form a dielectric layer 40.
[0103] The method for manufacturing the semiconductor structure of the exemplary embodiment adjusts the process sequence. Before etching the metal layer, a passivation layer is formed on the entire metal layer to reduce the thickness of the film layer formed on the metal layer. Then, the steps of forming a groove and forming a dielectric material layer to fill the groove are performed. The portion of the top of the dielectric material layer with a height difference is located above the passivation layer. The dielectric material layer can be ground with the top surface of the passivation layer as the grinding stop point to remove the portion of the dielectric material layer with a height difference. By optimizing the process, the processing efficiency is improved and the quality of the formed semiconductor structure is improved.
[0104] The top surface of the semiconductor structure formed in this embodiment is composed of the top surface of the passivation layer and the top surface of the dielectric layer. The top surface of the semiconductor structure has good bonding ability, ensuring that after the conductor is combined with the other structure, the connection surface of the semiconductor structure and the other structure is tightly connected, and there are no gap defects on the connection surface, so that the semiconductor structure and the other structure can be bonded and connected more firmly.
[0105] In an exemplary embodiment of the present disclosure, a method for manufacturing a semiconductor structure is provided. Fig.11 As shown, Fig.11 A flowchart of a method for manufacturing a semiconductor structure provided according to an exemplary embodiment of the present disclosure is shown. Figure 12-13 , Figure 20-Figure 28 The schematic diagram of each stage of the semiconductor structure manufacturing method is shown below. Figure 12-13 , Figure 20-Figure 28 The method of manufacturing semiconductor structures is introduced.
[0106] like Fig.11 As shown, a method for manufacturing a semiconductor structure provided by an exemplary embodiment of the present disclosure includes the following steps:
[0107] Step S210: providing a metal layer, wherein the metal layer is formed on the interlayer dielectric layer.
[0108] This exemplary embodiment is described by taking a process of forming a metal wiring layer ML (Metal Layer) in a back-end process of a DRAM memory.
[0109] like Fig.12 As shown, the metal layer 10 is a whole film layer covering the interlayer dielectric layer 50, and there is no step of patterning the metal layer 10. The material of the interlayer dielectric layer 50 may include at least one of silicon oxide, silicon nitride or silicon oxynitride. The metal layer 10 is an aluminum metal layer 10 or an aluminum alloy metal layer 10. The thickness of the metal layer 10 is 550nm-700nm, for example, the thickness of the metal layer 10 may be 550nm, 600nm, 650nm or 700nm. In this embodiment, the thickness of the metal layer 10 is 600nm.
[0110] The interlayer dielectric layer 50 is disposed on a semiconductor substrate or a semiconductor wafer (not shown in the figure). The material of the semiconductor substrate or semiconductor wafer may be silicon (Si), germanium (Ge), or silicon germanium (GeSi), silicon carbide (SiC); it may also be silicon on insulator (SOI), germanium on insulator (GOI); or it may also be other materials with semiconductor properties, such as III-V group compounds such as gallium arsenide. The semiconductor substrate or semiconductor wafer may include one or more stacked semiconductor device layers, wherein each semiconductor device layer may be formed with a variety of semiconductor devices and a variety of metal devices. Among them, the semiconductor device may include at least one of a metal oxide semiconductor field effect transistor, a bipolar junction transistor, a resistor, an inductor, a diode, and an optical device.
[0111] like Fig.12 As shown, the bottom surface of the metal layer 10 is covered by the first barrier layer 11, and the top surface of the metal layer 10 is covered by the second barrier layer 12. The first barrier layer 11 and the second barrier layer 12 are used to protect the metal layer 10 to prevent the metal layer 10 from being exposed to the process environment and being oxidized, resulting in degradation of the electrical properties of the metal layer 10. At the same time, the first barrier layer 11 and the second barrier layer 12 are also used to prevent the metal material in the metal layer 10 from diffusing into other film layers, causing contamination of other film layers of the semiconductor structure. The materials of the first barrier layer 11 and the second barrier layer 12 may include titanium or titanium nitride.
[0112] Step S220: forming a passivation layer, wherein the passivation layer covers the top surface of the metal layer.
[0113] like Fig.13 As shown, any one of the deposition processes of chemical vapor deposition (CVD), physical vapor deposition (PVD), atomic layer deposition (ALD) or sputtering can be used to deposit insulating material to cover the top surface of the metal layer 10 to form a passivation layer 20, and then, a chemical mechanical polishing process can be used to polish the top surface of the insulating material layer to grind the top surface of the passivation layer 20 into a plane. The thickness of the passivation layer 20 is between 500nm and 1000nm. For example, the thickness of the passivation layer 20 can be 500nm, 600nm, 700nm, 800nm, 900nm or 1000nm. In this embodiment, the thickness of the passivation layer 20 is 1000nm.
[0114] The material of the passivation layer 20 includes silicon nitride, which is hard and has good grinding resistance. In the subsequent process, the top surface of the passivation layer 20 is used as the grinding stop point, which can avoid damaging the top surface of the passivation layer 20 during the grinding process, forming defects and height differences on the top surface of the passivation layer 20, and ensuring that the top surface of the formed semiconductor structure is flat.
[0115] Step S230: forming a first trench, wherein the first trench penetrates the passivation layer and the metal layer, and the first trench exposes the top surface of the interlayer dielectric layer.
[0116] like Fig. 20 As shown, refer to Fig.13 A first mask layer (not shown) is formed on the top surface of the passivation layer 20, and the first mask layer defines a pattern for forming the first trench 121. The passivation layer 20, the second barrier layer 12, the metal layer 10 and the first barrier layer 11 are sequentially etched (dry or wet etching can be adopted) according to the first mask layer until the top surface of the interlayer dielectric layer 50 is exposed, and the etching is stopped to form the first trench 121.
[0117] It is understandable that the present embodiment does not limit the number, shape and layout of the first trenches 121 formed, and one first trench 121 or multiple first trenches 121 can be formed according to the design and application requirements of the semiconductor structure.
[0118] Step S240: depositing a dielectric material to fill the first trench and cover the top surface of the passivation layer to form a first dielectric material layer.
[0119] like Fig.21 As shown, refer to Fig. 20 , a dielectric material may be deposited by chemical vapor deposition or physical vapor deposition to form a first dielectric material layer 130, the first dielectric material layer 130 fills the first trench 121 and covers the top surface of the passivation layer 20, due to the large depth-width ratio of the first trench 121, the first dielectric material layer 130 may not fill the first trench 121, an air gap 141 is generated in the first trench 121, resulting in a convex defect on the top surface of the first dielectric material layer 130 located on the first trench 121, and a height difference exists on the top surface of the first dielectric material layer 130. In this embodiment, the material of the first dielectric material layer 130 includes silicon oxide.
[0120] Step S250: grinding the first dielectric material layer with the top surface of the passivation layer as the grinding stop point, the ground first dielectric material layer forms a first dielectric layer, the first dielectric layer is located in the first groove and divides the metal layer into a metal circuit layer.
[0121] like Fig. 22 As shown, refer to Fig.21The first dielectric material layer 130 can be ground by chemical mechanical polishing process, and the top surface of the passivation layer 20 is used as the grinding stop point. During the grinding process, the top surface of the passivation layer 20 can be detected by white light endpoint detection or advanced control technology. When the top surface of the passivation layer 20 is detected, the grinding is stopped, and the first dielectric material layer 130 located on the top surface of the passivation layer 20 is removed. The retained first dielectric material layer 130 forms a first dielectric layer 140, and the first dielectric layer 140 is filled in the first groove 121. The top surface of the first dielectric layer 140 is flush with the top surface of the passivation layer 20, and the bottom surface of the first dielectric layer 140 is connected to the interlayer dielectric layer 50 located below the metal layer 10. The first dielectric layer 140 divides the metal layer 10 into a metal circuit layer 80.
[0122] In the method for manufacturing the semiconductor structure of the present embodiment, after forming the passivation layer, the metal layer is patterned to form a metal circuit layer, so as to avoid that a portion of the top of the first dielectric material layer with a height difference is directly formed on the top surface of the metal layer, and the first dielectric material layer located on the top surface of the passivation layer is removed by grinding to form the first dielectric layer. The top surface of the formed semiconductor structure is flat, so as to ensure that there is no gap in the connection surface where the semiconductor structure and other structures are joined and connected, and the semiconductor structure can be firmly connected to other structures.
[0123] According to an exemplary embodiment, the method for manufacturing the semiconductor structure of this embodiment further performs the following steps after forming the first dielectric layer:
[0124] Step S260: forming a second trench, wherein the second trench penetrates the passivation layer and exposes the top surface of the metal layer.
[0125] like Fig.23 As shown, refer to Fig. 22 A second mask layer (not shown) is formed on the top surface of the passivation layer 20, and a pattern for forming the second groove 221 is defined on the second mask layer. The passivation layer 20 and the second barrier layer 12 are sequentially etched according to the second mask layer until the top surface of the metal wiring layer 80 formed by the metal layer 10 is exposed, thereby forming a second groove 221 penetrating the passivation layer 20.
[0126] The present embodiment does not limit the number, shape and layout of the second trenches 221 to be formed, and one or more second trenches 221 may be formed according to the design and application requirements of the semiconductor structure.
[0127] In this embodiment, in the process of forming the second trench 221 , only the passivation layer 20 needs to be etched, which reduces the time cost of forming the second trench 221 and reduces the aspect ratio of the second trench 221 .
[0128] Step S270: depositing a dielectric material to fill the second trench and cover the top surface of the passivation layer to form a second dielectric material layer.
[0129] like Fig.24 As shown, refer to Fig.23 , a dielectric material can be deposited by chemical vapor deposition process or physical vapor deposition process to fill the second groove 221 to form a second dielectric material layer 230. The second dielectric material layer 230 also covers the top surface of the passivation layer 20. The area where the second dielectric material layer 230 fills the second groove 221 is lower than the top surface of the second dielectric material layer 230 in other areas, forming a height difference on the top surface of the second dielectric material layer 230.
[0130] Step S280: grinding the second dielectric material layer with the top surface of the passivation layer as a grinding stop point to form a second dielectric layer in the second trench.
[0131] like Fig.25 As shown, refer to Fig.24 The second dielectric material layer 230 can be ground by chemical mechanical polishing process, and the top surface of the passivation layer 20 is used as the grinding stop point. During the grinding process, the top surface of the passivation layer 20 can be detected by white light endpoint detection or advanced control technology. The top surface of the passivation layer 20 is exposed and the grinding is stopped. The second dielectric material layer 230 located on the top surface of the passivation layer 20 is removed, and the retained second dielectric material layer 230 forms a second dielectric layer 240. The second dielectric layer 240 is filled in the second groove 221. The top surface of the second dielectric layer 240 and the top surface of the passivation layer 20 and the top surface of the first dielectric layer 140 are located in the same plane. The top surface of the semiconductor structure formed in this embodiment is a plane.
[0132] In this embodiment, by adjusting the process sequence of the semiconductor back-end process, the process of forming the first groove patterned metal layer to form the metal circuit layer and the process of forming the second groove on the metal circuit layer are performed after the passivation layer is formed. Only one passivation layer needs to be formed above the metal circuit layer, which reduces the thickness of the film layer located on the metal circuit layer, reduces the thickness of the film layer that needs to be etched to form the second groove on the metal circuit layer, and reduces the depth of the second groove formed on the metal circuit layer, thereby reducing the height difference formed on the top surface of the second dielectric material layer, and reducing the difficulty of removing the height difference on the top surface of the second dielectric material layer. The second dielectric material layer can be ground with the top surface of the passivation layer as the grinding stop point to remove the portion of the second dielectric material layer with the height difference, and at the same time, it is ensured that the top surface of the formed semiconductor structure is flat, and it is ensured that there is no gap in the connection surface where the semiconductor structure and other structures are bonded and connected, and the semiconductor structure and other structures are firmly connected.
[0133] This embodiment reduces the depth of the second trench, which is beneficial to improving the process efficiency of subsequently forming a metal interconnection structure and saving process time.
[0134] According to an exemplary embodiment, the method for manufacturing the semiconductor structure of this embodiment further performs the following steps after forming the second dielectric layer:
[0135] Step S290: removing a portion of the second dielectric layer to form a first through hole in the second dielectric layer, wherein the first through hole exposes the top surface of the metal layer.
[0136] like Fig.26 As shown, refer to Fig.25 , a portion of the second dielectric layer 240 is etched away until the top surface of the metal wiring layer 80 is exposed, and a first through hole 241 is formed in the second dielectric layer 240 .
[0137] Step S300: forming a metal interconnection structure in a first through hole.
[0138] In some examples, reference Fig.28 As shown, a dual damascene process may be used to form a metal interconnect structure 60, the metal interconnect structure 60 penetrates the second dielectric layer 240, the metal interconnect structure 60 includes a metal wire 61 that is in contact with the metal line layer 80 and a contact pad 62 disposed on the metal wire 61, and the top surface of the contact pad 62 is flush with the top surface of the second dielectric layer 240. In other examples, a single damascene process is used to form the metal interconnect structure 60, and the metal structure includes a metal wire that penetrates the second dielectric layer 240 (this example is not shown in the drawings).
[0139] In this embodiment, the metal interconnection structure 60 is formed in the first through hole 241, and the following implementation methods may be adopted:
[0140] First, an atomic layer deposition is used to deposit a diffusion barrier layer (not shown in the figure), and the diffusion barrier layer covers the first through hole 241 (refer to Fig.26 )'s pore wall, the material of the diffusion barrier layer may include tantalum, titanium, tantalum oxide or titanium oxide.
[0141] Then, copper metal is deposited on the diffusion barrier layer by physical vapor deposition to form a seed layer (not shown in the figure). For example, the following implementation can be adopted: the seed layer is pre-annealed for 20 seconds to 40 seconds at a temperature of 180° C. to 250° C. to promote the growth of the copper lattice of the seed layer, fill the gaps between the copper lattices in the seed layer, so that the copper lattice of the seed layer is uniform and continuous, reduce the resistance of the seed layer, and improve the conductivity of the seed layer, so that the formed metal interconnect structure 60 has good conductivity.
[0142] Then, if Fig. 27 As shown, refer to Fig.26A first metal material layer 70 is formed by an electroplating process. The first metal material layer 70 grows on the seed layer. The first metal material layer 70 fills the first through hole 241 and covers the top surface of the passivation layer 20 .
[0143] Then, if Fig.28 As shown, refer to Fig. 27 The first metal material layer 70 is ground with the top surface of the passivation layer 20 as the grinding stop point. During the grinding process, white light end point detection or advanced control technology can be used to detect the top surface of the passivation layer 20. The top surface of the passivation layer 20 is exposed and the grinding is stopped. The first metal material layer 70 located after the passivation layer is ground is removed. The first metal material layer 70 after grinding forms a metal interconnection structure 60. The metal interconnection structure 60 is embedded in the second dielectric layer 240. The peripheral surface of the metal interconnection structure 60 is covered by the seed layer. The metal interconnection structure 60 and the second dielectric layer 240 are separated by a barrier diffusion layer. The barrier diffusion layer is used to prevent the copper element in the metal interconnection structure 60 from diffusing into other structures to cause semiconductor structure pollution.
[0144] The top surface of the metal interconnect structure 60 formed in this embodiment is flush with the top surface of the passivation layer 20 and the top surface of the second dielectric layer 240 .
[0145] The manufacturing method of the semiconductor structure of the present embodiment reduces the process depth of forming the metal interconnection structure, reduces the height of the metal interconnection structure, and reduces the resistance of the metal interconnection structure, which is beneficial to improving the conductivity and response speed of the semiconductor structure, avoiding response delay of the semiconductor structure, and at the same time shortening the process time of forming the metal interconnection structure and improving the process efficiency; the top surface of the semiconductor structure formed in the present embodiment is composed of the first dielectric layer, the second dielectric layer, the passivation layer and the top surface of the metal interconnection structure, the top surface of the semiconductor structure is flat, and the material of the top surface of the semiconductor structure does not contain a polymer material with poor bonding ability. When the semiconductor structure of the present embodiment and other structures are bonded and connected by a hybrid bonding process, the gap between the connection surfaces can be reduced, ensuring that the semiconductor structure and other structures are more firmly connected.
[0146] According to an exemplary embodiment, the difference between this embodiment and the above-mentioned embodiments is that, in this embodiment, after exposing the top surface of the passivation layer 20 during the grinding of the first metal material layer 70, the first metal material layer 70 and the passivation layer 20, the first dielectric layer 140, and the second dielectric layer 240 are ground together to a target height, thereby further reducing the height of the metal interconnect structure, reducing the contact resistance of the metal interconnect structure, improving the conductivity and response speed of the semiconductor structure, and avoiding response delays in the semiconductor structure.
[0147] In this embodiment, the target height is higher than the air gap 141 in the first dielectric layer 140 to avoid exposure of the air gap 141 and adverse effects on the semiconductor structure.
[0148] According to an exemplary embodiment, the present exemplary embodiment provides a semiconductor structure such as Fig.16 , Fig.19 or Fig.28 As shown, the semiconductor structure includes a metal layer 10, a passivation layer 20, and at least one trench 21 (refer to Fig.14 or Fig.17 ) and a dielectric layer 40, the passivation layer 20 covers the top surface of the metal layer 10; the groove 21 at least penetrates the passivation layer 20, and the dielectric layer 40 is located in the groove 21. The semiconductor structure includes a first surface 100a, and the first surface 100a includes the top surface of the dielectric layer 40 and the top surface of the passivation layer 20.
[0149] In some embodiments, Fig.28 As shown, the metal layer 10 (refer to Fig.16 or Fig.19 ) is disposed on the interlayer dielectric layer 50, the semiconductor structure includes a first trench 121, and the first trench 121 penetrates the passivation layer 20 and the metal layer 10. The dielectric layer 40 includes a first dielectric layer 140, the first dielectric layer 140 fills the first trench 121, the first dielectric layer 140 is connected to the interlayer dielectric layer 50, and the first dielectric layer 140 divides the metal layer 10 into a metal line layer 80.
[0150] In some embodiments, Fig.28 As shown, the semiconductor structure includes a second trench 221 penetrating the passivation layer 20 , and the dielectric layer 40 includes a second dielectric layer 240 . The second dielectric layer 240 fills the second trench 221 and covers a portion of the top surface of the metal layer 10 .
[0151] In some embodiments, Fig.28 As shown, the semiconductor structure further includes a metal interconnection structure 60 . The metal interconnection structure 60 is disposed in the second dielectric layer 240 . The metal interconnection structure 60 penetrates the second dielectric layer 240 and is in contact with the metal layer 10 .
[0152] In some embodiments, Fig.28 As shown, the first surface 100 a also includes a top surface of the metal interconnect structure 60 .
[0153] In some embodiments, Fig.28 As shown, the first dielectric layer 140 has an air gap 141 , the top surface of the air gap 141 is lower than the first surface 100 a , and the air gap 141 is sealed in the first dielectric layer 140 , which can improve the insulation effect of the first dielectric layer 140 and prevent the metal layer 10 from short-circuiting.
[0154] In some embodiments, Fig.28 As shown, the first surface 100a is a plane. The first surface 100a of the semiconductor structure of this embodiment is a flat and uniform plane. After the semiconductor structure of this embodiment is bonded and connected with other structures, the first surface 100a is more tightly connected with the other structures, there is no gap between the connection surfaces of the semiconductor structure and the other structures, and the semiconductor structure is more firmly bonded with the other structures.
[0155] According to an exemplary embodiment, Fig.29 As shown, this exemplary embodiment provides a semiconductor bonding structure, and the semiconductor structure of this embodiment includes a first semiconductor structure 100 and a second semiconductor structure 200, and the first semiconductor structure 100 and the second semiconductor structure 200 both adopt the semiconductor structure in the above-mentioned embodiments. Among them, the first semiconductor structure 100 can be a semiconductor chip that adopts the structure in the above-mentioned embodiments, and the second semiconductor structure 200 can be a semiconductor wafer that adopts the structure in the above-mentioned embodiments. The semiconductor bonding structure of this embodiment can be formed in a chip-on-wafer manner (Chip ON Wafer, COW). Alternatively, the semiconductor structure of this embodiment can also be formed in a chip-on-chip (Chip ON Chip, COC) manner, or a wafer-on-wafer (Wafer ON Wafer, WOW) manner.
[0156] like Fig.29 As shown, the first surface 110a of the first semiconductor structure 110 and the first surface 210a of the second semiconductor structure 210 are arranged opposite to each other, the first surface 110a of the first semiconductor structure 110 and the first surface 210a of the second semiconductor structure 210 are connected together, at the connecting surface of the first semiconductor structure 110 and the second semiconductor structure 210, the metal interconnection structure 160 of the first semiconductor structure 110 and the metal interconnection structure 260 of the second semiconductor structure 210 are bonded and connected, and the passivation layer 120 of the first semiconductor structure 110 and the passivation layer 220 of the second semiconductor structure 210 are bonded and connected.
[0157] In the semiconductor bonding structure of the present embodiment, there is no gap between the first surface 110 a of the first semiconductor structure 110 and the bonding surface of the second semiconductor structure 210 , thereby improving the firmness of the semiconductor bonding structure.
[0158] The various embodiments or implementation methods in this specification are described in a progressive manner. Each embodiment focuses on the differences from other embodiments, and the same or similar parts between the various embodiments can be referenced to each other.
[0159] In the description of this specification, reference to the terms "embodiment", "exemplary embodiment", "some embodiments", "illustrative embodiment", "example", etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present disclosure.
[0160] In this specification, the schematic representations of the above terms do not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described can be combined in any one or more embodiments or examples in a suitable manner.
[0161] In the description of the present disclosure, it should be noted that the terms "center", "up", "down", "left", "right", "vertical", "horizontal", "inside", "outside", etc. indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present disclosure and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present disclosure.
[0162] It is to be understood that the terms "first", "second", etc. used in the present disclosure can be used to describe various structures in the present disclosure, but these structures are not limited by these terms. These terms are only used to distinguish a first structure from another structure.
[0163] In one or more of the accompanying drawings, the same elements are represented by similar reference numerals. For the sake of clarity, the parts in the accompanying drawings are not drawn to scale. In addition, some well-known parts may not be shown. For the sake of simplicity, the structure obtained after several steps can be described in one figure. Many specific details of the present disclosure, such as the structure, materials, dimensions, processing technology and technology of the device are described below to more clearly understand the present disclosure. However, as those skilled in the art will appreciate, the present disclosure may not be implemented in accordance with these specific details.
[0164] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present disclosure, rather than to limit them. Although the present disclosure has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein by equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present disclosure.
Claims
1. A method for manufacturing a semiconductor structure, characterized in that: The method for manufacturing the semiconductor structure comprises: providing a metal layer; forming a passivation layer, the passivation layer covering the top surface of the metal layer; forming at least one groove, wherein the groove at least penetrates the passivation layer; forming a dielectric material layer, wherein the dielectric material layer fills the groove and covers the top surface of the passivation layer; The dielectric material layer is ground with the top surface of the passivation layer as a grinding stop point, and the dielectric material layer retained by grinding forms a dielectric layer in the groove.
2. The method for manufacturing a semiconductor structure according to claim 1, characterized in that: The metal layer is formed on the interlayer dielectric layer, and forming at least one trench comprises: A first trench is formed, wherein the first trench penetrates the passivation layer and the metal layer, and the first trench exposes a top surface of the interlayer dielectric layer.
3. The method for manufacturing a semiconductor structure according to claim 2, characterized in that: The production method comprises: Depositing a dielectric material to fill the first trench and cover the top surface of the passivation layer to form a first dielectric material layer; The first dielectric material layer is ground with the top surface of the passivation layer as a grinding stop point, and the ground first dielectric material layer forms a first dielectric layer, which is located in the first groove and divides the metal layer into a metal circuit layer.
4. The method for manufacturing a semiconductor structure according to any one of claims 1 to 3, characterized in that: Forming at least one trench comprises: A second trench is formed, wherein the second trench penetrates the passivation layer, and the second trench exposes a top surface of the metal layer.
5. The method for manufacturing a semiconductor structure according to claim 4, characterized in that: The production method comprises: Depositing a dielectric material to fill the second trench and cover the top surface of the passivation layer to form a second dielectric material layer; The second dielectric material layer is ground with the top surface of the passivation layer as a grinding stop point to form a second dielectric layer in the second groove.
6. The method for manufacturing a semiconductor structure according to claim 5, characterized in that: The production method further comprises: removing a portion of the second dielectric layer to form a first through hole in the second dielectric layer, wherein the first through hole exposes a top surface of the metal layer; A metal interconnect structure is formed in the first via.
7. The method for manufacturing a semiconductor structure according to claim 6, characterized in that: forming a metal interconnection structure in the first through hole, comprising: forming a first metal material layer, the first metal material layer filling the first through hole and covering the top surface of the passivation layer; The first metal material layer is ground with the top surface of the passivation layer as a grinding stop point, and the ground first metal material layer forms the metal interconnection structure.
8. A semiconductor structure, characterized in that: The semiconductor structure comprises: Metal layer; a passivation layer, the passivation layer covering a top surface of the metal layer; at least one groove, the groove at least passing through the passivation layer; a dielectric layer, located in the groove; The semiconductor structure includes a first surface including a top surface of the dielectric layer and a top surface of the passivation layer.
9. The semiconductor structure according to claim 8, characterized in that: The metal layer is arranged on the interlayer dielectric layer, and the semiconductor structure comprises: A first trench, penetrating the passivation layer and the metal layer; The dielectric layer includes a first dielectric layer, the first dielectric layer fills the first trench, the first dielectric layer is connected to the interlayer dielectric layer, and the first dielectric layer divides the metal layer into metal circuit layers.
10. The semiconductor structure according to claim 9, characterized in that: The semiconductor structure comprises: A second groove, penetrating the passivation layer; The dielectric layer includes a second dielectric layer, the second dielectric layer fills the second trench, and the second dielectric layer covers a portion of the top surface of the metal layer.
11. The semiconductor structure according to claim 10, characterized in that: The semiconductor structure further comprises: The metal interconnection structure is arranged in the second dielectric layer, and the metal interconnection structure penetrates the second dielectric layer and is in contact with the metal layer.
12. The semiconductor structure according to claim 11, characterized in that: The first surface also includes a top surface of the metal interconnect structure.
13. The semiconductor structure according to any one of claims 9 to 12, characterized in that: The first dielectric layer has an air gap therein, and a top surface of the air gap is lower than the first surface.
14. A semiconductor bonding structure, characterized in that: comprising a first semiconductor structure and a second semiconductor structure, wherein the first semiconductor structure and the second semiconductor structure both adopt the semiconductor structure according to any one of claims 8 to 12; The first surface of the first semiconductor structure and the first surface of the second semiconductor structure are arranged opposite to each other, the first surface of the first semiconductor structure and the first surface of the second semiconductor structure are connected together, and at the connection surface between the first semiconductor structure and the second semiconductor structure, the dielectric layer of the first semiconductor structure and the dielectric layer of the second semiconductor structure are bonded and connected, and the passivation layer of the first semiconductor structure and the passivation layer of the second semiconductor structure are bonded and connected.
Citation Information
Patent Citations
Silicon based LCD device, silicon based LCD device reflector and manufacture method
CN101311802A
Manufacturing method for ultra-thickness metal
CN103681309A
Method for forming semiconductor device structure
CN109585374A
Manufacturing method of semiconductor device
CN112466810A
Pad manufacturing method and CIS chip packaging method
CN115206815A