Linear frictional engagement method, linear frictional engagement joint, and engagement structure

By applying a preparatory pressure higher than the joining pressure in linear friction joining and work-hardening the joined interface, the problem of joining materials of different materials and shapes is solved, and the homogeneity of the joint part and accurate temperature control are achieved, improving The reliability and efficiency of the joint are improved.

CN118829508APending Publication Date: 2024-10-22OSAKA UNIVERSITY
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202380025470.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-03-04
Filing Date
2023-01-17
Publication Date
2024-10-22

AI Technical Summary

Technical Problem

The existing linear friction joining method is difficult to form a good joint on materials to be joined of different materials, shapes and sizes, and it is difficult to accurately control the joining temperature, and is prone to problems such as cracks, unjoined parts and temperature unevenness.

Method used

By applying a preparatory pressure higher than the joining pressure in the early stage of joining and work-hardening the joined interface during the joining process, the linear friction behavior in the early stage of joining is ensured to be uniform and stable, thereby suppressing cracks and temperature non-uniformity, and achieving jointing Accurate control of temperature.

Benefits of technology

It achieves a good joint that does not depend on the material, shape and size of the joined materials, ensures the homogeneity and high reliability of the joint, avoids the problems of cracks and temperature unevenness, and obtains an efficient linear friction joint effect.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118829508A_ABST
    Figure CN118829508A_ABST
Patent Text Reader

Abstract

The present invention provides a simple and efficient linear friction bonding method capable of forming a good bonding portion without depending on the material, shape, and size of a material to be bonded, and a linear friction bonded structure obtained by the linear friction bonding method. Provided are a simple and efficient linear frictional bonding method capable of accurately controlling the bonding temperature without depending on the material, shape, and size of the material to be bonded, and a linear frictional bonded structure obtained by the linear frictional bonding method. This linear frictional joining method is characterized by comprising: a first step for forming an interface to be joined by bringing one member into contact with the other member; a second step for applying a preliminary pressure substantially perpendicularly to the interface to be joined; a third step for repeatedly sliding the one member and the other member on the same trajectory while applying a bonding pressure to the interface to be bonded, and discharging burrs from the interface to be bonded; and a fourth step in which the sliding is stopped and the joining surface is formed. The preliminary pressure in the second step is set to a value higher than the joining pressure.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a linear friction joining method for metal materials, a linear friction joining joint obtained by the linear friction joining method, and a joining structure having the linear friction joining joint. Background Art

[0002] With the increasing strength of metal materials such as steel and aluminum alloys, the strength reduction at the joint that determines the mechanical properties of the jointed structure has become a serious problem. In contrast, in recent years, the solid phase joining method, which has a maximum achievable temperature that does not reach the melting point of the joined materials and has a smaller strength reduction at the joint than conventional fusion welding, has attracted attention and is being rapidly put into practical use.

[0003] In particular, linear friction welding (LFW: Linear Friction Welding) that makes metal parts slide along linear tracks does not require the use of tools like friction stir welding (FSW: Friction Stir Welding), so it can be easily applied to high-melting-point metals and is expected to be put into practical use in various industries.

[0004] However, the materials, shapes and sizes of the materials to be joined that are the objects of linear friction joining are diverse, and the appropriate joining conditions, joining mechanisms, etc. corresponding to the combination of each material to be joined are not necessarily clear. The actual situation is optimized based on a large number of preliminary tests and experience.

[0005] In contrast, for example, in patent document 1 (Japanese Patent Gazette No. 2015-164738), there is disclosed a friction engagement device for frictionally engaging one component with another component by repeatedly moving them relative to each other on the same trajectory while the components are in abutment with each other. The friction engagement device is characterized in that it is provided with a stopping means for stopping the relative movement of the one component with respect to the other component in accordance with a stop instruction for the relative movement of the one component with respect to the other component during a period from the generation of the stop instruction until the one component moves relative to the other component once along the trajectory.

[0006] The purpose of the friction engagement device described in the above-mentioned patent document 1 is to be able to easily determine: when one component is frictionally engaged with another component by repeatedly moving relative to each other on the same trajectory in a state where they are in contact with each other, at what timing a stop command for relative movement is generated so that the relative movement of the two components can be stopped exactly when the two components are in an appropriate engagement state.

[0007] In addition, the inventor of the present invention disclosed a linear friction joining method in patent document 2 (Japanese Patent Gazette No. 2018-122344), which is characterized in that it has: a first step of making one component abut against another component to form a joined interface; a second step of repeatedly sliding one component and another component on the same trajectory while applying pressure approximately vertically to the joined interface to remove burrs from the joined interface; and a third step of stopping the sliding to form a joining surface, and setting the pressure to be greater than the yield stress and less than the tensile strength of one component and / or the other component at the desired joining temperature.

[0008] The linear friction joining method described in Patent Document 2 can provide a linear friction joining method that can achieve accurate control of the joining temperature and lower the joining temperature by setting the joining pressure to a level greater than the yield stress and less than the tensile strength of the materials to be joined at the desired joining temperature. Prior art literature Patent Literature

[0009] Patent Document 1: Japanese Patent Application Publication No. 2015-164738 Patent Document 2: Japanese Patent Application Publication No. 2018-122344 Summary of the invention Problems to be solved by the invention

[0010] It is extremely complicated and difficult to find the joining conditions for forming a good joint for each of the joined materials that are the objects of linear friction joining. In contrast, the friction joining method disclosed in the above-mentioned patent document 1 is a method for controlling the friction joining amount by shortening the period required from the generation of the stop command to the stop of the actuator. Although it helps to improve the basic joining process control of linear friction joining, it does not mean that it is a preferred joining method for linear friction joining of joined materials of different materials, sizes and shapes.

[0011] In addition, especially when the joining temperature is accurately controlled, it is difficult to optimize the joining conditions compared to simply joining the materials to be joined. Although the joining temperature can be controlled by using the linear friction joining method described in the above-mentioned patent document 2, for example, a higher joining pressure than that when low temperature is achieved needs to be applied. Here, in the case where the joined interface is large, it is difficult to make the behavior of the entire joined interface in the joining uniform (stabilize), and the formation of cracks, unjoined parts, and the occurrence of location dependence of temperature history changes become problems.

[0012] In view of the above problems in the prior art, the object of the present invention is to provide a simple and efficient linear friction joining method that can form a good joint without depending on the material, shape and size of the materials to be joined, and a linear friction joining structure obtained by using the linear friction joining method. In addition, the object of the present invention is to provide a simple and efficient linear friction joining method that can accurately control the joining temperature without depending on the material, shape and size of the materials to be joined, and a linear friction joining structure obtained by using the linear friction joining method. Methods used to solve problems

[0013] In order to achieve the above-mentioned purpose, the inventors of the present invention have repeatedly conducted in-depth research on the linear friction joining method and found that it is extremely effective to apply a pressure higher than the joining pressure to the materials to be joined as a preparatory step for applying the joining pressure, thereby completing the present invention.

[0014] That is, the present invention provides a linear friction joining method, characterized in that it comprises: a first step of making one component abut against another component to form a joined interface; a second step of applying a preliminary pressure approximately vertically to the above-mentioned joined interface; a third step of repeatedly sliding the above-mentioned one component and the above-mentioned other component on the same trajectory while applying the joining pressure to the above-mentioned joined interface to remove burrs from the above-mentioned joined interface; and a fourth step of stopping the above-mentioned sliding and forming a joining surface, so that the above-mentioned preliminary pressure in the above-mentioned second step is a value higher than the above-mentioned joining pressure.

[0015] The most significant feature of the linear friction joining method of the present invention is that a second process is provided for applying a preliminary pressure approximately perpendicularly to the joined interface, so that the preliminary pressure in the second process is a value higher than the joining pressure. The non-uniformity and instability of the linear friction behavior are largely caused by the state at the beginning of the joining, and this state is further strengthened as the joining time passes. In contrast, by applying a preliminary pressure higher than the joining pressure, the linear friction behavior at the beginning of the joining can be made uniform and stabilized, and the suppression of unjoined defects and the uniformity of the joining temperature distribution can be achieved. In addition, by applying a preliminary pressure higher than the joining pressure, cracks caused by the high joining pressure can also be suppressed.

[0016] In addition, in the linear friction joining method of the present invention, it is preferred that the joined interface is work-hardened in the second step. Although the effect of the present invention can be obtained by applying a preparatory pressure higher than the joining pressure, by work-hardening the joined interface, the linear friction behavior in the early stage of joining can be more reliably uniformed and stabilized, and the suppression of unjoined defects and the uniformity of the joining temperature distribution can be achieved.

[0017] In addition, in the linear friction joining method of the present invention, it is preferred that the thickness of the joined interface is 3 mm or more. In the linear friction joining method of the present invention, since the linear friction behavior at the initial stage of joining can be made uniform and stabilized, the unjoined defects can be suppressed and the joining temperature distribution can be made uniform, a good and homogeneous joint can be obtained even when the thickness of the joined interface is 3 mm or more.

[0018] In addition, in the linear friction joining method of the present invention, it is preferred that the one component and / or the other component is made of steel. The microstructure and mechanical properties of steel are sensitive to temperature history changes, so that the joining temperature distribution of the entire joining interface can be uniformed in the linear friction joining of the present invention, thereby also obtaining a good and homogeneous joint.

[0019] In addition, in the linear friction joining method of the present invention, it is preferred to determine the desired joining temperature and set the joining pressure to be greater than the yield stress and less than the tensile strength of the one or the other member at the joining temperature. By setting the joining pressure to be greater than the yield stress and less than the tensile strength of the one or the other member at the desired joining temperature, the joining temperature can be accurately controlled. In addition, although compressive stress is mainly applied near the joined interface, deformation begins when a joining pressure greater than the compressive strength of the one or the other member at the joining temperature is applied, in fact, the joining temperature can be accurately controlled by setting the joining pressure to be greater than the yield stress and less than the tensile strength of the one or the other member at the desired joining temperature.

[0020] Furthermore, in the linear friction joining method of the present invention, it is preferred that the one member and / or the other member is the steel material, and the joining temperature is set to be below the A1 point of the steel material. By setting the joining temperature to be below the A1 point of the steel material, the formation of a brittle metamorphic phase at the joining portion can be suppressed, and a joining portion with high reliability can be obtained.

[0021] In addition, the present invention also provides a linear friction joint, which has a linear friction joint portion in which one component and another component are integrated through a linear friction joint interface, the one component and / or the other component are steel, the thickness of the steel forming the linear friction joint interface is greater than 3 mm, the entire area of ​​the linear friction joint interface is metallurgically joined, and martensite is not formed in the steel in the entire area of ​​the linear friction joint interface.

[0022] In the linear friction joint of the present invention, the entire linear friction joint interface having a thickness of 3 mm or more is free of defects and martensite is not formed, thereby forming a joint having extremely high reliability and mechanical properties.

[0023] In the linear friction joint of the present invention, the steel is preferably weathering steel. Weathering steel contains a relatively large amount of P, etc., which makes it difficult to suppress welding cracks. Therefore, solid phase bonding is urgently needed. By using the linear friction bonding method of the present invention, a good joint can be obtained.

[0024] Furthermore, the present invention also provides a joint structure having the linear friction joint of the present invention. The joint portion of the joint structure of the present invention is in a state where there are no defects and no martensite is formed in the entire area of ​​the linear friction joint interface, and the joint structure is highly reliable. In particular, the joint structure of the linear friction joint of weathering steel has excellent corrosion resistance and mechanical properties, and can therefore be preferably used for applications requiring reliability in a corrosive environment. Effects of the Invention

[0025] According to the present invention, a simple and efficient linear friction joining method capable of forming a good joint portion independently of the material shape and size of the materials to be joined and a linear friction joining structure obtained by using the linear friction joining method can be provided. In addition, by using the present invention, a simple and efficient linear friction joining method capable of accurately controlling the joining temperature independently of the material, shape and size of the materials to be joined and a linear friction joining structure obtained by using the linear friction joining method can be provided. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] Figure 1 It is a schematic diagram showing the state of linear friction engagement. Figure 2 A schematic diagram showing one embodiment of the linear friction joining method of the present invention. Figure 3 It is a graph showing the tensile strength of various stainless steel materials at various temperatures. Figure 4 This is a schematic cross-sectional view showing an example of the linear friction joint of the present invention. Figure 5 This is a macro photograph of the cross section of the joint obtained in Example 1. Figure 6 yes Figure 5 The microstructure of the center of the bonding interface (center in the vibration direction). Figure 7 This is the microstructure of the central portion (central portion in the vibration direction) of the bonding interface obtained in Example 2. Figure 8 This is a macro photograph of a cross section of the linear friction joint obtained in Comparative Example 1. Fig. 9 These are macro photographs of cross sections of each linear friction joint obtained in Comparative Example 2. Fig.10This is the surface temperature history change of the bonding interface during bonding in Comparative Example 2. DETAILED DESCRIPTION

[0027] The following describes in detail representative embodiments of the linear friction joining method, the linear friction joining joint, and the joining structure of the present invention with reference to the accompanying drawings, but the present invention is not limited thereto. In addition, in the following description, the same reference numerals are sometimes used to mark the same or corresponding parts, and repeated descriptions are omitted. In addition, the drawings are only used to conceptually illustrate the present invention, so there are cases where the dimensions of the components shown and their ratios are different from the actual ones.

[0028] (1) Linear friction engagement method Figure 1 is a schematic diagram showing the state of linear friction engagement, Figure 2 Schematic diagram showing the joining process of the linear friction joining method of the present invention. The linear friction joining method of the present invention comprises: a first process of making one component 2 abut against another component 4 to form a joined interface 6; a second process of applying a preliminary pressure P2 approximately perpendicularly to the joined interface 6; a third process of making one component 2 and another component 4 slide repeatedly on the same track while applying a joining pressure P3 approximately perpendicularly to the joined interface 6, and removing burrs 8 from the joined interface 6 approximately parallel to and approximately perpendicular to the sliding direction; and a fourth process of stopping the sliding to form a joining surface. Each process is described in detail below.

[0029] (1-1) First step The first step is a step of bringing one member 2 into contact with another member 4 to form a joined interface 6. One member 2 and / or another member 4 is moved to a position where a desired joint is to be formed, and the joined surfaces are brought into contact with each other to form a joined interface 6. The value of the pressure P1 applied to the joined interface 6 in the first step is not particularly limited as long as the effect of the present invention is not impaired, and a pressure of a degree such that at least one member 2 and another member 4 are brought into contact to form a joined interface 6 may be applied.

[0030] The materials of one member 2 and the other member 4 are not particularly limited as long as they do not impair the effects of the present invention, and any of the conventionally known materials to be joined may be used. The joined material is preferably a metal material, but one member 2 or the other member 4 may also be a ceramic material or a resin material.

[0031] Here, as the metal material, steel is preferably used, and weathering steel is more preferably used. The microstructure and mechanical properties of steel are sensitive to temperature history changes, and the bonding temperature distribution of the entire bonding interface can be uniformed in the linear friction bonding of the present invention, so a good and homogeneous bonding portion can also be obtained. In addition, by using weathering steel, a linear friction bonding joint (bonding structure) having excellent corrosion resistance and mechanical properties can be obtained, which can be preferably used for applications requiring reliability in a corrosive environment.

[0032] In addition, the size and shape of one component 2 and the other component 4 are not particularly limited as long as they do not impair the effect of the present invention, and can be of a desired size and shape, but it is preferred that the thickness of the bonded interface 6 be 3 mm or more. In the linear friction bonding method of the present invention, the linear friction behavior at the initial stage of bonding can be made uniform and stabilized, and the suppression of unbonded defects and the uniformity of bonding temperature distribution can be achieved. Therefore, even when the thickness of the bonded interface 6 is 3 mm or more, a good and homogeneous bond can be obtained.

[0033] (1-2) Second process The second step is a step of applying a preliminary pressure P2 substantially vertically to the interface 6 to be joined, and is the most important step in the linear friction joining of the present invention.

[0034] The biggest feature of the second process is that the preparatory pressure P2 is set to a value higher than the bonding pressure P3 of the third process. The non-uniformity and instability of the linear friction behavior are largely caused by the state at the beginning of bonding, and this state is further strengthened as the bonding time passes. In contrast, by applying a preparatory pressure P2 higher than the bonding pressure P3, the linear friction behavior at the beginning of bonding can be made uniform and stabilized, and the non-bonding defect can be suppressed and the bonding temperature distribution can be made uniform.

[0035] In addition, it is preferred that the interface 6 to be joined is work-hardened by applying a preliminary pressure P2. Although the effect of the present invention can be obtained by applying a preliminary pressure P2 higher than the joining pressure P3, by work-hardening the interface 6 to be joined, the linear friction behavior at the initial stage of joining can be more reliably uniformed and stabilized, and the suppression of unjoined defects and the uniformity of the joining temperature distribution can be achieved. Here, the presence or absence of work hardening of the interface 6 to be joined can be easily determined by measuring the hardness of the interface 6 to be joined.

[0036] The upper limit of the preliminary pressure P2 is not particularly limited as long as a linear friction engagement portion is obtained, but is preferably a value such that the protrusions of one member 2 and the other member 4 (areas protruding forward from the gripping portion of the linear friction engagement device) are not significantly plastically deformed as a whole.

[0037] (1-3) The third step The third step is a step of applying a joining pressure P3 approximately perpendicularly to the joined interface 6, causing one component 2 and another component 4 to slide repeatedly on the same trajectory, thereby removing burrs 8 from the joined interface 6 approximately parallel to and approximately perpendicular to the sliding direction.

[0038] The method of making one member 2 and the other member 4 repeatedly slide on the same trajectory is not particularly limited as long as the effects of the present invention are not impaired. Both members may be vibrated together, or one member may be fixed and the other vibrated.

[0039] Here, the joining temperature can be controlled by setting the joining pressure P3 during linear friction joining to a value greater than the yield stress of one component 2 and / or the other component 4 and less than the tensile strength at the desired joining temperature. By setting the joining pressure P3 to a value greater than the yield stress of the joined material, the discharge of the burr 8 from the joined interface 6 begins, and when the joining pressure P3 is increased until the tensile strength is reached, the discharge of the burr 8 is accelerated. Like the yield stress, the tensile strength at a specific temperature is also approximately constant depending on the joined material, so a joining temperature corresponding to the set joining pressure P3 can be achieved. From the viewpoint of suppressing the rise in the joining temperature, it is preferred to set the joining pressure P3 to a value less than the tensile strength.

[0040] As a specific example, Figure 3 Indicates the tensile strength of carbon steel and various stainless steel materials at various temperatures. Figure 3 This is the curve graph published in "Sanyo Technical Report Vol.21(2014)No.1". Figure 3 As shown in FIG. 1 , the tensile strength at a specific temperature is substantially constant depending on the material. That is, by making such data about the materials to be joined into a database, it is possible to efficiently and easily perform joining at any temperature.

[0041] When the joining pressure P3 is set high during joining, the joined material (steel material) with higher yield strength and tensile strength can be discharged as burrs, and the joining temperature can be lowered. Figure 3 As shown, since the tensile strength (and yield stress) at a specific temperature is substantially constant depending on the material, the joining temperature (maximum achievable temperature) of the steel can be controlled very accurately by setting the joining pressure P3 based on the temperature dependence of the strength of the steel.

[0042] In the third step, it is also necessary to set the bonding parameters other than the bonding pressure P3 (frequency and amplitude of the bonded materials vibrating, bonding time and approach margin, etc.), but these values ​​are not limited as long as they do not impair the effect of the present invention, and can be appropriately set according to the material, shape and size of the bonded materials. Here, by increasing the amplitude and frequency of the bonded materials sliding, the heating rate and the cooling rate after bonding will increase, but the maximum achievable temperature (bonding temperature) will not change.

[0043] The maximum achievable temperature of the bonded portion can be basically determined by the bonding pressure P3. However, when the bonding temperature exceeds a desired value due to overshoot caused by an excessively large temperature increase rate, it is preferable to reduce the frequency and / or amplitude.

[0044] (1-4) Fourth step The fourth step is a step of stopping the sliding of the third step to form a joining surface. In the linear friction joining method of the present invention, a good joint body can be obtained by stopping the sliding after removing the burr 8 from the entire surface of the joined interface 6. In addition, the joining pressure P3 (P3=P4) applied to the joined material in the third step can be directly maintained, and a higher value (P3<P4) can be adopted in order to make the newly formed surface more strongly contact while removing the burr 8. Although there is a case where the pressure P decreases when the joining area increases during the joining process, and the joining temperature rises unexpectedly, this phenomenon can be suppressed by increasing the pressure P.

[0045] Here, as long as the burr 8 is discharged from the entire surface of the bonded interface 6, the timing of stopping the sliding is not limited, but by observing the bonded interface 6 from a direction substantially perpendicular to the sliding direction, the sliding is stopped at the moment when the burr 8 is discharged substantially parallel to the sliding direction, and the discharge amount of the burr 8 can be suppressed to a minimum (the consumption of the bonded material can be suppressed to a minimum), thereby forming a good bond. In addition, "a direction substantially perpendicular to the sliding direction" and "a direction substantially parallel to the sliding direction" are both directions substantially perpendicular to the applied pressure.

[0046] (2) Linear friction joint Figure 4 1 is a schematic cross-sectional view showing an example of a linear friction joint according to the present invention. The linear friction joint 10 is a member that linearly frictionally joins one member 2 and another member 4, and at least one of the one member 2 and the other member 4 is made of steel.

[0047] In addition, the thickness of the steel material forming the linear friction joint interface 12 is 3 mm or more, the entire region of the linear friction joint interface 12 is metallurgically joined, and martensite is not formed in the steel material in the entire region of the linear friction joint interface 12. The entire region of the linear friction joint interface 12 having a thickness of 3 mm or more is free of defects and martensite is not formed, and a joint having extremely high reliability and mechanical properties is formed.

[0048] It is preferred that at least one of the one member 2 and the other member 4 is made of weathering steel. Since weathering steel contains a relatively large amount of P and the like, it is difficult to suppress welding cracks, and therefore it is highly desirable to apply solid phase bonding, and a good joint can be obtained by using the linear friction bonding method of the present invention. The type of weathering steel is not particularly limited as long as it does not impair the effect of the present invention, and not only various weathering steels known in the art can be used, but also weathering steels developed in the future can be used.

[0049] also, Figure 4 The linear friction joint 10 shown is a butt joint, but the joint shape is not limited thereto, and can be a cross joint, an overlap joint, or any other known joint shape. In addition, the size and shape of the materials to be joined are not particularly limited as long as they do not impair the effects of the present invention.

[0050] (3) Joint structures The joint structure of the present invention is a joint structure having a linear friction joint 10 , and particularly, since it has excellent corrosion resistance and mechanical properties when a weather-resistant steel material is used, it can be preferably used for applications requiring high reliability in a corrosive environment.

[0051] The joint structure of the present invention is not particularly limited as long as it does not impair the effect of the present invention, and can be various joint structures known in the art. As the joint structure, for example, automobile parts, railway vehicle parts, ship parts, aircraft parts, building structures, various infrastructure structures, mechanical structure parts, and chemical industry equipment parts can be listed.

[0052] As mentioned above, although the representative embodiments of the present invention have been described, the present invention is not limited to these embodiments, and various design changes can be made, and all of these design changes are included in the technical scope of the present invention. Example

[0053] <Example 1> Highly weather-resistant rolled steel SPA-H (JIS G 3125) was used as the material to be joined, and the highly weather-resistant rolled steels were butted linearly friction joined. The highly weather-resistant rolled steels had a thickness of 3.2 mm and a width of 30 mm, and the end faces of 3.2 mm × 30 mm were brought into contact with each other to form a joined interface (first step).

[0054] Next, after applying a preliminary pressure of 500 MPa approximately vertically to the interface to be joined (second step), it is made to slide linearly under the conditions of a joining pressure of 250 MPa, a frequency of 15 Hz, and an amplitude of ±1.5 mm (third step), and the joining step is terminated when a margin of approximately 2.5 mm is reached (fourth step).

[0055] Figure 5 A cross-sectional macrophotograph of the obtained linear friction joint is shown. It can be seen that metallurgical bonding is achieved over the entire bonding interface, and there are no defects or unbonded areas. Figure 6 express Figure 5 The microstructure of the center of the joint interface (the center of the vibration direction) in the joint is shown in Figure 1. A structure composed of ferrite and fine cementite was formed, and the formation of martensite was not confirmed. This result shows that the maximum achievable temperature in linear friction joining is below the A1 point of high weather-resistant rolled steel. In addition, a Figure 6 The microstructure shown.

[0056] <Example 2> A linear friction joint was obtained in the same manner as in Example 1 except that the preliminary pressure was changed to 200 MPa. Macroscopic observation of the cross section of the obtained linear friction joint revealed that metallurgical joining was achieved over the entire joint interface, and no defects or unjoined portions were observed. Figure 7 Represents the microstructure of the center of the bonding interface (center of the vibration direction). It indicates that a structure composed of ferrite and martensite is formed, and the highest achievable temperature in linear friction bonding is above the A1 point of high weather-resistant rolled steel. This result shows that bonding defects and unbonded parts can be suppressed by applying preliminary pressure, and a relatively high preliminary pressure is required to homogenize the bonding temperature. In addition, the surface temperature history near the bonding interface during bonding was measured using a thermal imaging camera (CPA-T640) (emissivity: 0.78), and the temperature was below the A1 point. Without preliminary pressurization, there is an area of ​​uneven temperature inside, and it is believed that the A1 point is exceeded in this area.

[0057] <Comparative Example 1> A linear friction joint was obtained in the same manner as in Example 1 except that no preliminary pressure was applied to the interface to be joined. Figure 8The cross-sectional macrophotograph of the obtained linear friction joint is shown. It can be seen that defects are formed at the joint interface and a good joint is not obtained. It is believed that this is because the joining pressure of 250 MPa is excessive for the room temperature strength of the joined materials, and the material near the interface undergoes large plastic deformation at the initial stage of joining.

[0058] <Comparative Example 2> Linear friction joints were obtained in the same manner as in Example 1 except that no preliminary pressure was applied to the interface to be joined and the joining pressures were set to 100 MPa, 150 MPa, and 200 MPa. Fig. 9 The cross-sectional macrophotographs of the obtained linear friction joints are shown. Although there were no defects or unjoined portions at the joint interface, formation of martensite was confirmed in all regions.

[0059] The surface temperature history changes near the bonding interface during bonding in Comparative Examples 1 and 2 were measured using a thermal imaging camera (CPA-T640) (emissivity: 0.78). The measurement position was the center portion of the bonding interface in the vibration direction. Fig.10 The obtained measurement results are shown in FIG. 1 . It can be seen that the maximum achievable temperature decreases with the increase of the joining pressure. Here, although the maximum achievable temperature becomes below the A1 point of the high weather-resistant rolled steel when the joining pressure is set to 250 MPa, there is actually a region where martensite is formed at the obtained joining interface. Description of Reference Numerals

[0060] 2: A component 4: Another component 6: Bonded interface 8: Burr 10: Linear friction joint 12: Linear friction interface

Claims

1. A linear friction engagement method, characterized in that: have: In a first step, one member is brought into contact with another member to form a joined interface; The second step is to apply a preliminary pressure substantially vertically to the interface to be joined; A third step is to repeatedly slide the one member and the other member on the same trajectory while applying a bonding pressure to the bonded interface, thereby removing burrs from the bonded interface; and The fourth step is to stop the sliding and form a joint surface. The preliminary pressure in the second step is set to a value higher than the bonding pressure.

2. The linear friction joining method according to claim 1, wherein: In the second step, the joined interface is work-hardened.

3. The linear friction joining method according to claim 1 or 2, characterized in that: The thickness of the bonded interface is set to be greater than 3 mm.

4. The linear friction joining method according to claim 1 or 2, characterized in that: The one component and / or the other component is made of steel.

5. The linear friction joining method according to claim 1 or 2, characterized in that: Determine the desired bonding temperature, The joining pressure is set to be equal to or higher than the yield stress and equal to or lower than the tensile strength of the one member or the other member at the joining temperature.

6. The linear friction joining method according to claim 4 or 5, characterized in that: The one component and / or the other component is the steel material, The joining temperature is set to be equal to or lower than the A1 point of the steel material.

7. A linear friction joint, characterized in that: A linear friction joint portion in which one member is integrated with another member via a linear friction joint interface, The one component and / or the other component is made of steel, The thickness of the steel material forming the linear friction joint interface is 3 mm or more, The full-area metallurgical bonding of the linear friction joint interface, Martensite is not formed in the steel material over the entire area of ​​the linear friction joint interface.

8. The linear friction joint according to claim 7, characterized in that: The steel material is weather-resistant steel.

9. A joint structure, characterized in that: A linear friction joint according to claim 7 or 8.