Forming mold and forming method for double-layer panel box
By using a forming mold and method that combines gas and rigid media, the problems of low efficiency, high cost, and poor quality in the double-layer plate forming process have been solved. This has enabled efficient and simple liquid-cooled flow channel forming and box forming, thereby improving the overall quality and reliability of the product.
Patent Information
- Application Number
- CN202410977678.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-19
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2044-07-19
AI Technical Summary
Existing double-layer plate forming processes are complex to operate, have poor quality, are difficult to guarantee sealing performance, have low production efficiency, high costs, and poor product reliability.
The forming die, which includes a concave die structure, a convex die structure, and a pressure ring structure, achieves global deep drawing and local gas expansion through the synergistic effect of gas and rigid medium, forming a liquid cooling channel, simplifying the forming process, and ensuring welding accuracy and the fit of the liquid cooling channel.
It improves forming efficiency, reduces the number and cost of molds, ensures precise forming of liquid cooling channels and surface quality of the housing, reduces leakage, and enhances the overall quality and reliability of the product.
Smart Images

Figure CN118832055B_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of electrical equipment technology, and more specifically, to a forming mold and forming method for a double-layer panel box. Background Technology
[0002] Some existing electronic products rely on air convection to dissipate heat generated by heat-generating components within the casing. This method is not only energy-intensive and noisy, but also limited by low density in equipment layout. During operation, the coolant in liquid cooling systems remains separate from the components being cooled, avoiding direct contact. Instead, the coolant flows into the unit for efficient heat exchange, carrying away heat from the heat-generating components and maintaining the product within a predetermined temperature range. Providing coolant circulation to heat-generating components through liquid cooling eliminates the need for air heat exchange and significantly reduces the energy consumption of the refrigeration system. More importantly, by directly guiding the coolant to the heat source, and given that liquids have a higher specific heat capacity than air, their heat dissipation rate is far greater, resulting in significantly higher cooling efficiency than traditional air cooling. This highly efficient heat dissipation technology not only effectively solves the unit's heat dissipation problem but also significantly reduces noise during product operation. Given the significant advantages of liquid cooling technology in terms of heat dissipation efficiency, energy consumption, and noise control, the electronics industry is widely researching and applying liquid cooling technology to improve product performance and optimize energy efficiency.
[0003] During the efficient operation of electronic products, significant heat accumulation occurs, necessitating advanced cooling technologies to transfer excess heat to the external environment. Liquid cooling technology is an advanced solution to this problem, achieving efficient heat conduction and removal by precisely channeling coolant into the internal flow channels of the electronic product's casing. Electronic product casings typically employ a double-layer structure to ensure coolant circulation. However, current mainstream double-layer forming processes primarily involve separately forming the inner and outer layers and then welding them together. This process is not only complex but can also lead to poor flow channel quality and difficulty in guaranteeing sealing performance, making traditional solutions insufficient to meet the stringent requirements of modern electronic products for lightweight casings and efficient heat dissipation.
[0004] Existing technology involves forming the outer layer into separate parts and then welding them together to obtain a box-shaped integral part with boss and flow channel features. Specifically, the outer layer is formed using a dedicated mold (such as...). Figure 1 As shown), the inner layer is formed using a different set of molds (such as...). Figure 2(As shown in the figure). The components in the figure are described as follows: 1- Upper working platform of the hydraulic press; 2- Upper mold heating platform; 3- Upper mold; 4- Pressure ring; 5- Aluminum alloy sheet; 6- Lower mold; 7- Lower mold heating platform; 8- Lower working platform of the hydraulic press. In the separate forming processes of the outer and inner layers, firstly, the upper mold 3, pressure ring 4, and lower mold 6 are preheated to a preset temperature through a heating furnace. Next, the aluminum alloy sheet 5 is placed on the upper surface of the lower mold 6, and simultaneously the mold (upper mold 3, pressure ring 4, and lower mold 6) and the aluminum alloy sheet 5 are heated to the target forming temperature and maintained for a period of time to ensure uniform temperature. Subsequently, under the pressure of the upper mold 3, the aluminum alloy sheet 5 gradually flows into the cavity of the lower mold 6, and finally, the mold is closed to obtain the formed part. Finally, the corresponding areas of the outer layer formed part and the inner layer formed part are welded to form a double-layer box with flow channels. By introducing coolant into the flow channels, the heat generated by the electronic components is carried away, achieving the purpose of liquid cooling.
[0005] However, existing technologies have the following drawbacks: (1) The accuracy of the product shape depends heavily on the precise design of the convex and concave dies. The product is formed by the close fit of the convex and concave dies. Therefore, the precision and structural design of the mold are required to be high, and the mold structure is relatively complex.
[0006] (2) During the deep drawing process, the rigid contact between the sheet metal and the die will cause friction, which will form scratches on the surface of the blank. This rigid impact can also easily cause forming defects such as tearing and wrinkling, which seriously affect the final quality of the product; in addition, the wear on the die is relatively large, which increases the cost of maintenance and replacement of the die.
[0007] (3) Existing forming methods often require multiple processes to complete, which not only increases the number of molds, but also leads to complicated mold preparation work; at the same time, this process also faces problems such as long design and debugging cycle, high labor production cost and low overall efficiency.
[0008] In summary, existing forming methods face core problems such as low production efficiency, high cost, poor forming quality, and poor product reliability. Summary of the Invention
[0009] The main objective of this invention is to provide a forming mold and forming method for a double-layer plate box, so as to solve the core problems faced by the forming methods in the prior art, such as low production efficiency, high cost, poor forming quality and poor product reliability.
[0010] To achieve the above objectives, according to one aspect of the present invention, a forming mold for a double-layer plate box is provided, comprising a concave mold structure, a convex mold structure, and a pressure ring structure, wherein a portion of the upper surface of the concave mold structure is recessed to form a mold cavity, and the bottom surface of the mold cavity has 2N spaced groove cavities, and the concave mold structure has a first vent pipe, the first end of the first vent pipe being connected to an external air source, and the second end of the first vent pipe being connected to the mold cavity, with the connection point between the two located at a position on the bottom surface of the mold cavity that avoids the groove cavities; the convex mold structure is vertically and flexibly disposed above the concave mold structure, and the side surface of the convex mold structure facing the mold cavity has M protrusions, where M=N, such that the M protrusions... The die body is arranged in a one-to-one correspondence with N groove cavities. The protruding die body extends into the groove cavities to stamp out the boss structure on the double-layer plate. The pressure ring structure is located on the outer periphery of the punch structure and can be raised and lowered. The pressure ring structure is arranged opposite to the outer circumferential surface of the die cavity, and the pressure ring structure has a second vent pipe. The first end of the second vent pipe is connected to an external air source, and the second end of the second vent pipe is used to connect to the air inlet on the double-layer plate to punch the non-diffusion soldering area of the outer layer of the double-layer plate that is not coated with solder resist into the remaining N groove cavities to form liquid cooling channels. The N groove cavities used to form the boss structure and the N groove cavities used to form the liquid cooling channels are arranged alternately.
[0011] Furthermore, the first ventilation pipe includes a first sub-pipe and a second sub-pipe that are connected to each other, wherein the first end of the first sub-pipe extends radially along the die structure and penetrates the circumferential outer surface of the die structure to form the first end of the first ventilation pipe; the first end of the second sub-pipe is connected to the second end of the first sub-pipe, and the second end of the second sub-pipe extends axially along the die structure and penetrates the bottom surface of the mold cavity to form the second end of the first ventilation pipe.
[0012] Furthermore, the second venting duct includes a third sub-duct and a fourth sub-duct that are connected to each other. The first end of the third sub-duct extends radially along the pressure ring structure and penetrates the circumferential outer surface of the pressure ring structure to form the first end of the second venting duct. The first end of the fourth sub-duct is connected to the second end of the third sub-duct, and the second end of the fourth sub-duct extends axially along the pressure ring structure and penetrates the end surface of the pressure ring structure facing the die structure to form the second end of the second venting duct.
[0013] Furthermore, the punch structure includes, in its radial direction from the outside to the inside, a first punch heating zone, a second punch heating zone, and a third punch heating zone, wherein the protruding body is located in the second punch heating zone; in the radial direction of the punch structure, the forming die also includes, in its radial direction from the outside to the inside, a first punch heating structure, a second punch heating structure, and a third punch heating structure, wherein the first punch heating structure is used to heat the first punch heating zone, the second punch heating structure is used to heat the second punch heating zone, and the third punch heating structure is used to heat the third punch heating zone.
[0014] Furthermore, the die structure includes, in its radial direction from the outside to the inside, a first die heating area, a second die heating area, and a third die heating area, wherein the groove cavity is located in the second die heating area; in the radial direction of the die structure, the forming mold also includes, in its radial direction from the outside to the inside, a first die heating structure, a second die heating structure, and a third die heating structure, wherein the first die heating structure is used to heat the first die heating area, the second die heating structure is used to heat the second die heating area, and the third die heating structure is used to heat the third die heating area.
[0015] According to another aspect of the present invention, a method for forming a double-layer panel box is provided. The forming method is based on the forming mold described above, and the forming method includes: Step S1: Wire cut the plate substrate to cut out two plate structures of the required size, and perform zoning preprocessing on each plate structure. Step S2: Stack the two plate structures that have completed the partitioning preprocessing together, and perform edge sealing and butt welding on the outer periphery of the two plate structures to form a closed double-layer plate. Reserve an air inlet on one of the plate structures in the double-layer plate, and use the plate structure with the air inlet as the inner plate and the plate structure without the air inlet as the outer plate. Step S3: Place the double-layer plate that has completed step S2 on the cavity structure of the forming mold. Heat the punch structure and cavity structure of the forming mold through the upper heating structure and the lower heating structure respectively. At the same time, under the heat conduction of the punch structure and the cavity structure, heat the double-layer plate to the target forming temperature. Step S4: After the double-layer plate is heated to the target forming temperature and kept at that temperature for a first preset time, the pressure ring structure of the forming mold moves downward to the mold closing position and presses the non-deformable area of the double-layer plate firmly under the action of constant pressure force, so that a closed space is formed between the surface of the outer layer plate facing the concave mold structure and the cavity wall of the concave mold structure. Step S5: After the enclosed space is formed, the punch structure moves downward at a constant speed while gas at a first preset pressure is injected into the mold cavity through the first ventilation pipe on the die structure, so that the double-layer plate is gradually stretched under the combined action of the rigid pressure of the punch structure and the flexible pressure of the gas until the die structure and the punch structure are closed. Step S6: After the double-layer plate is tightly attached to the punch structure, stop filling the mold cavity with gas and unload the air pressure. The punch structure continues to apply the second preset pressure to perform diffusion welding on the area of the double-layer plate that is not coated with solder resist. Step S7: After the diffusion welding process is completed, gas at a third preset pressure is injected into the area of the double-layer plate that is not coated with solder resist through the second vent pipe and the gas inlet on the pressure ring structure. Under the action of gas pressure, the material of the inner layer plate continues to be tightly attached to the punch structure, and the local material of the outer layer plate that has not participated in the diffusion welding process gradually flows to the groove cavity of the die structure until the outer layer plate and the die structure are completely attached. The pressure is maintained for a second preset time to allow the liquid cooling channel to expand and take shape. Step S8: After completing the forming operation of the double-layer plate, turn off the power, slowly cool down to below the preset temperature, and then open the furnace door for natural cooling so that the punch structure, die structure, and formed part cool down to room temperature with the furnace. Then, take out the formed part and test its quality and performance.
[0016] Further, in step S1, the partition pretreatment includes first performing a surface pretreatment to retain the oxide layer on the non-diffusion soldering area of the board structure, and then applying solder resist to the non-diffusion soldering area after the surface pretreatment to retain the oxide layer is completed; then performing a surface pretreatment to remove the oxide layer on the diffusion soldering area of the board structure, and then polishing the diffusion soldering area with sandpaper after the surface pretreatment to remove the oxide layer is completed.
[0017] Furthermore, before applying solder resist to the non-diffusion soldering area, the flow path of material deformation during the forming process of the double-layer plate is simulated using simulation technology, and the positions of the expansion channel and the inter-plate air filling path are determined. The corresponding positions of the expansion channel and the inter-plate air filling path are found on the plate structure. The positions of the expansion channel and the inter-plate air filling path are both regarded as the non-diffusion soldering area, and the area of the double-layer plate other than the non-diffusion soldering area is regarded as the diffusion soldering area.
[0018] Furthermore, in step S3, during the heating of the punch structure and die structure of the forming mold by the upper heating structure and the lower heating structure respectively, the temperature provided to the area of the double-layer plate that promotes material thinning is higher than the temperature provided to the area of the double-layer plate that inhibits material thinning.
[0019] Furthermore, in step S3, the heating method for heating the punch structure and die structure of the forming mold through the upper heating structure and the lower heating structure respectively includes: The first punch heating structure heats the first punch heating area to a first preset temperature T1; The second punch heating structure heats the second punch heating area to a second preset temperature T2; The third punch heating structure heats the third punch heating zone to a third preset temperature T3; wherein, T1 = T3 < T2; and / or, The first die heating structure heats the first die heating zone to the fourth preset temperature T4; The second die heating structure heats the second die heating zone to the fifth preset temperature T5; The third die heating structure heats the third die heating zone to a sixth preset temperature T6; where T4 = T6 < T5.
[0020] Applying the technical solution of this invention, a forming mold for a double-layer plate box body is provided, including a concave mold structure, a convex mold structure, and a pressure ring structure. The concave mold structure has 2N spaced groove cavities on its bottom surface, and a first end of a first vent pipe connected to an external air source, while the second end of the first vent pipe is connected to the mold cavity. Further, the convex mold structure has M protruding shapes on one side of its surface facing the mold cavity, where M=N, so that the M protruding shapes correspond one-to-one with the N groove cavities. The protruding shapes extend into the groove cavities to stamp out the double-layer plate. The boss structure; further, the pressure ring structure is located on the outer periphery of the punch structure and can be raised and lowered. The pressure ring structure is opposite to the outer circumferential surface of the mold cavity, and the pressure ring structure has a second vent pipe. The first end of the second vent pipe is connected to an external air source, and the second end of the second vent pipe is used to connect to the air inlet on the double-layer plate to flush the non-diffusion solder area of the outer layer plate of the double-layer plate without solder resist into the remaining N groove cavities to form liquid cooling channels; further, the N groove cavities used to form the boss structure and the N groove cavities used to form the liquid cooling channels are staggered.
[0021] The specific method for forming the double-layer plate provided in this application is as follows: Step S1: Wire cut the plate substrate to cut out two plate structures of the required size, and perform zoning preprocessing on each plate structure. Step S2: Stack the two plate structures that have completed the partitioning preprocessing together, and perform edge sealing and butt welding on the outer periphery of the two plate structures to form a closed double-layer plate. Reserve an air inlet on one of the plate structures in the double-layer plate, and use the plate structure with the air inlet as the inner plate and the plate structure without the air inlet as the outer plate. Step S3: Place the double-layer plate that has completed step S2 on the cavity structure of the forming mold. Heat the punch structure and cavity structure of the forming mold through the upper heating structure and the lower heating structure respectively. At the same time, under the heat conduction of the punch structure and the cavity structure, heat the double-layer plate to the target forming temperature. Step S4: After the double-layer plate is heated to the target forming temperature and kept at that temperature for a first preset time, the pressure ring structure of the forming mold moves downward to the mold closing position and presses the non-deformable area of the double-layer plate firmly under the action of constant pressure force, so that a closed space is formed between the surface of the outer layer plate facing the concave mold structure and the cavity wall of the concave mold structure. Step S5: After the enclosed space is formed, the punch structure moves downward at a constant speed while gas at a first preset pressure is injected into the mold cavity through the first ventilation pipe on the die structure, so that the double-layer plate is gradually stretched under the combined action of the rigid pressure of the punch structure and the flexible pressure of the gas until the die structure and the punch structure are closed. Step S6: After the double-layer plate is tightly attached to the punch structure, stop filling the mold cavity with gas and unload the air pressure. The punch structure continues to apply the second preset pressure to perform diffusion welding on the area of the double-layer plate that is not coated with solder resist. Step S7: After the diffusion welding process is completed, gas at a third preset pressure is injected into the area of the double-layer plate that is not coated with solder resist through the second vent pipe and the gas inlet on the pressure ring structure. Under the action of gas pressure, the material of the inner layer plate continues to be tightly attached to the punch structure, and the local material of the outer layer plate that has not participated in the diffusion welding process gradually flows to the groove cavity of the die structure until the outer layer plate and the die structure are completely attached. The pressure is maintained for a second preset time to allow the liquid cooling channel to expand and take shape. Step S8: After completing the forming operation of the double-layer plate, turn off the power, slowly cool down to below the preset temperature, and then open the furnace door for natural cooling so that the punch structure, die structure, and formed part cool down to room temperature with the furnace. Then, take out the formed part and test its quality and performance.
[0022] This application combines the synergistic effect of a flexible gas medium and a rigid punch medium to achieve the dual objectives of global deep drawing of double-layer plates and local gas expansion to form liquid cooling channels. The forming method provided in this application first involves butt welding the edges of a double-layer plate, and then, under the synergistic effect of gas and a punch structure, globally deep drawing is performed to form the basic shape of the box. Subsequently, under specific pressure and temperature conditions, the double-layer plate is welded in sections to ensure the welding accuracy and reliability of the diffusion welding area. Finally, under the action of gas, the local non-diffusion welding area is formed into the desired shape of the liquid cooling channel. The forming method provided in this application fully utilizes the process advantages of the flexible gas medium, which not only ensures the precise forming of the liquid cooling channel features, but also has significant advantages such as simple forming process, high box surface quality, excellent fitting effect of the liquid cooling channel, and low risk of leakage. In addition, the forming method provided in this application only requires one set of forming molds to complete the entire production process, significantly reducing the number of forming molds, thereby reducing the processing and manufacturing costs, labor costs, and material costs of forming molds. Furthermore, the forming method provided in this application also helps to shorten the product forming cycle, improve forming efficiency, and further enhance the overall quality of the product. Attached Figure Description
[0023] The accompanying drawings, which form part of this application, are used to provide a further understanding of the invention. The illustrative embodiments of the invention and their descriptions are used to explain the invention and do not constitute an undue limitation of the invention. In the drawings: Figure 1 A schematic diagram of the forming process of the outer layer plate in the prior art is shown. In this diagram, the forming process of the outer layer plate is shown. Figure 1 (a) Figure 1 (b) Figure 1 (c) in the figure represents the forming step of the outer layer plate; Figure 2 A schematic diagram of the forming process of the inner layer plate in the prior art is shown. In this diagram, the forming process of the inner layer plate is shown. Figure 2 (a) Figure 2 (b) Figure 2 (c) in the figure represents the forming step of the inner layer plate; Figure 3 A cross-sectional structural schematic diagram of a double-layered panel box according to an optional embodiment of the present invention is shown; Figure 4 A schematic diagram of a forming die according to an optional embodiment of the present invention is shown, in which both the punch structure and the die structure are heated to heat the double-layer plate; Figure 5 It shows Figure 4 A schematic diagram showing the state in which the pressure ring structure of the forming mold moves downward and presses the outer periphery of the double-layer plate tightly; Figure 6 It shows Figure 5 A schematic diagram of the deep drawing process using a forming die. Figure 7 It shows Figure 6 A schematic diagram showing the state after the forming operation of the forming mold is completed and the diffusion welding process is completed in a local area; Figure 8 It shows Figure 7 A schematic diagram showing the completed forming state of the liquid cooling channel of the double-layer plate box body using the forming mold. Figure 9 It shows Figure 8 A schematic diagram of the air inlet on the inner layer of the double-layered plate; Figure 10 A schematic flowchart of a method for forming a double-layer plate box according to an optional embodiment of the present invention is shown.
[0024] The above figures include the following reference numerals: 01. Double-layer panel; 010. Inner panel; 011. Outer panel; 02. Boss structure; 03. Air inlet; 04. Liquid cooling channel; 05. Housing; 10. Die structure; 11. Mold cavity; 12. Groove cavity; 13. First vent pipe; 131. First sub-pipe; 132. Second sub-pipe; 14. First die heating zone; 15. Second die heating zone; 16. Third die heating zone; 20. Punch structure; 21. First punch heating zone; 22. Second punch heating zone; 23. Third punch heating zone; 24. Protruding shape; 30. Pressure ring structure; 31. Second vent pipe; 311. Third sub-pipe; 312. Fourth sub-pipe; 40. Heating structure; 41. First punch heating structure; 42. Second punch heating structure; 43. Third punch heating structure; 44. First die heating structure; 45. Second die heating structure; 46. Third die heating structure. Detailed Implementation
[0025] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. The following description of at least one exemplary embodiment is merely illustrative and is in no way intended to limit the present invention or its application or use. All other embodiments obtained by those skilled in the art based on the embodiments of the present invention without creative effort are within the scope of protection of the present invention.
[0026] To address the core problems of existing forming methods, such as low production efficiency, high cost, poor forming quality, and poor product reliability, this invention provides a forming mold and forming method for a double-layer plate box.
[0027] like Figure 1 and Figure 2 The figures shown are schematic diagrams illustrating the forming methods of the outer and inner layers in the prior art.
[0028] like Figures 3 to 9As shown, the forming mold for the double-layer panel box includes a concave mold structure 10, a convex mold structure 20, and a pressure ring structure 30. A portion of the upper surface of the concave mold structure 10 is recessed to form a mold cavity 11. The bottom surface of the mold cavity 11 has 2N spaced grooved cavities 12. The concave mold structure 10 has a first ventilation pipe 13. The first end of the first ventilation pipe 13 is connected to an external air source, and the second end of the first ventilation pipe 13 is connected to the mold cavity 11. The connection point between the two is located on the bottom surface of the mold cavity 11, away from the grooved cavities 12. The convex mold structure 20 is vertically and flexibly positioned above the concave mold structure 10. The side surface of the convex mold structure 20 facing the mold cavity 11 has M protruding shapes 24, where M=N, so that the M protruding shapes 24 correspond one-to-one with the N grooved cavities 12. The protruding body 24 extends into the groove cavity 12 to stamp out the boss structure 02 on the double-layer plate 01; the pressure ring structure 30 is located on the outer periphery of the punch structure 20 and can be raised and lowered. The pressure ring structure 30 is arranged opposite to the outer periphery of the mold cavity 11, and the pressure ring structure 30 has a second vent pipe 31. The first end of the second vent pipe 31 is connected to an external air source, and the second end of the second vent pipe 31 is used to connect to the air inlet 03 on the double-layer plate 01 to punch the non-diffusion soldering area of the outer layer plate 011 of the double-layer plate 01 that is not coated with solder resist into the remaining N groove cavities 12 to form liquid cooling channels 04; wherein, the N groove cavities 12 used to form the boss structure 02 and the N groove cavities 12 used to form the liquid cooling channels 04 are staggered.
[0029] Applying the technical solution of this invention, a forming mold for a double-layer plate box body is provided, including a concave mold structure 10, a convex mold structure 20, and a pressure ring structure 30. The concave mold structure 10 has 2N spaced groove cavities 12 on the bottom surface of its cavity 11. The first end of the first ventilation pipe 13 of the concave mold structure 10 is connected to an external air source, and the second end of the first ventilation pipe 13 is connected to the cavity 11. Further, the convex mold structure 20 has M protruding shapes 24 on one side surface facing the cavity 11, where M=N, so that the M protruding shapes 24 correspond one-to-one with the N groove cavities 12. The protruding shapes 24 extend into the groove cavities 12 to stamp protrusions onto the double-layer plate 01. Structure 02; Further, the pressure ring structure 30 is located on the outer periphery of the punch structure 20 and can be raised and lowered. The pressure ring structure 30 is opposite to the outer periphery of the mold cavity 11, and the pressure ring structure 30 has a second vent pipe 31. The first end of the second vent pipe 31 is connected to an external air source, and the second end of the second vent pipe 31 is used to connect to the air inlet 03 on the double-layer plate 01, so as to push the non-diffusion soldering area of the outer layer plate 011 of the double-layer plate 01 without solder resist into the remaining N groove cavities 12 to form a liquid cooling channel 04; Further, the N groove cavities 12 used to form the boss structure 02 and the N groove cavities 12 used to form the liquid cooling channel 04 are staggered.
[0030] The specific method for forming the double-layer plate provided in this application is as follows: Step S1: Wire cut the plate substrate to cut out two plate structures of the required size, and perform zoning preprocessing on each plate structure. Step S2: Stack the two plate structures that have completed the partitioning preprocessing together, and perform edge sealing and butt welding on the outer periphery of the two plate structures to form a closed double-layer plate 01. Reserve an air inlet 03 on one of the plate structures in the double-layer plate 01, and use the plate structure with the air inlet 03 as the inner plate 010, and the plate structure without the air inlet 03 as the outer plate 011. Step S3: Place the double-layer plate 01, which has completed step S2, on the cavity structure 10 of the forming mold. Heat the punch structure 20 and the cavity structure 10 of the forming mold through the upper heating structure and the lower heating structure respectively. At the same time, under the heat conduction of the punch structure 20 and the cavity structure 10, the double-layer plate 01 is heated to the target forming temperature. Step S4: After the double-layer plate 01 is heated to the target forming temperature and kept at that temperature for a first preset time, the pressure ring structure 30 of the forming mold moves downward to the mold closing position and presses the non-deformable area of the double-layer plate 01 under the action of constant pressure force, so that the surface of the outer plate 011 facing the cavity structure 10 and the cavity wall surface of the cavity 11 of the cavity structure 10 form a closed space. Step S5: After the enclosed space is formed, while the punch structure 20 moves downward at a constant speed, gas with a first preset pressure is injected into the mold cavity 11 through the first ventilation pipe 13 on the die structure 10, so that the double-layer plate 01 is gradually stretched under the combined action of the rigid pressure of the punch structure 20 and the flexible pressure of the gas until the die structure 10 and the punch structure 20 are closed. Step S6: After the double-layer plate 01 is tightly attached to the punch structure 20, stop filling the mold cavity 11 with gas and unload the air pressure. The punch structure 20 continues to apply the second preset pressure to perform diffusion welding on the area of the double-layer plate 01 that is not coated with solder resist. Step S7: After the diffusion welding process is completed, gas at a third preset pressure is injected into the area of the double-layer plate 01 where no solder resist is applied through the second vent pipe 31 and the air inlet 03 on the pressure ring structure 30. Under the action of gas pressure, the material of the inner layer plate 010 continues to be tightly attached to the punch structure 20, and the local material of the outer layer plate 011 that has not participated in the diffusion welding process gradually flows to the groove cavity 12 of the die structure 10 until the outer layer plate 011 is completely attached to the die structure 10. The pressure is maintained for a second preset time so that the liquid cooling channel 04 expands and takes shape. Step S8: After completing the forming operation of the double-layer plate 01, turn off the power, slowly cool down to below the preset temperature, and then open the furnace door for natural cooling so that the punch structure 20, the die structure 10, and the formed part cool down to room temperature with the furnace. Then, take out the formed part and test its quality and performance.
[0031] This application combines the synergistic effect of a flexible gas medium and a rigid punch medium to achieve the dual objectives of global deep drawing of double-layer plates and local gas expansion to form liquid cooling channels. The forming method provided in this application first involves butt welding the edges of a double-layer plate, and then, under the synergistic effect of gas and a punch structure, globally deep drawing is performed to form the basic shape of the box. Subsequently, under specific pressure and temperature conditions, the double-layer plate is welded in sections to ensure the welding accuracy and reliability of the diffusion welding area. Finally, under the action of gas, the local non-diffusion welding area is formed into the desired shape of the liquid cooling channel. The forming method provided in this application fully utilizes the process advantages of the flexible gas medium, which not only ensures the precise forming of the liquid cooling channel features, but also has significant advantages such as simple forming process, high box surface quality, excellent fitting effect of the liquid cooling channel, and low risk of leakage. In addition, the forming method provided in this application only requires one set of forming molds to complete the entire production process, significantly reducing the number of forming molds, thereby reducing the processing and manufacturing costs, labor costs, and material costs of forming molds. Furthermore, the forming method provided in this application also helps to shorten the product forming cycle, improve forming efficiency, and further enhance the overall quality of the product.
[0032] like Figure 4 As shown, the first ventilation conduit 13 includes a first sub-conduit 131 and a second sub-conduit 132 that are connected to each other. The first end of the first sub-conduit 131 extends radially along the die structure 10 and penetrates the circumferential outer surface of the die structure 10 to form the first end of the first ventilation conduit 13. The first end of the second sub-conduit 132 is connected to the second end of the first sub-conduit 131, and the second end of the second sub-conduit 132 extends axially along the die structure 10 and penetrates the bottom surface of the mold cavity 11 to form the second end of the first ventilation conduit 13. Thus, by configuring the first ventilation conduit 13 with a structure including the connected first sub-conduit 131 and the second sub-conduit 132, the ventilation reliability of the first ventilation conduit 13 is ensured.
[0033] like Figure 4As shown, the second venting duct 31 includes a third sub-duct 311 and a fourth sub-duct 312 that are connected to each other. The first end of the third sub-duct 311 extends radially along the pressure ring structure 30 and penetrates the circumferential outer surface of the pressure ring structure 30 to form the first end of the second venting duct 31. The first end of the fourth sub-duct 312 is connected to the second end of the third sub-duct 311, and the second end of the fourth sub-duct 312 extends axially along the pressure ring structure 30 and penetrates the end surface of the pressure ring structure 30 facing the die structure 10 to form the second end of the second venting duct 31. Thus, by configuring the second venting duct 31 with a structure including the connected third sub-duct 311 and fourth sub-duct 312, the venting reliability of the second venting duct 31 is ensured.
[0034] Optionally, the gas introduced into the mold cavity 11 through the first ventilation pipe 13 is nitrogen, and the gas introduced through the second ventilation pipe 31 and the air inlet 03 is also nitrogen.
[0035] like Figure 4 As shown, the punch structure 20 includes, in its radial direction from the outside in, a first punch heating zone 21, a second punch heating zone 22, and a third punch heating zone 23, wherein the protruding body 24 is located in the second punch heating zone 22. In the radial direction of the punch structure 20, the forming die also includes, in its radial direction from the outside in, a first punch heating structure 41, a second punch heating structure 42, and a third punch heating structure 43. The first punch heating structure 41 is used to heat the first punch heating zone 21, the second punch heating structure 42 is used to heat the second punch heating zone 22, and the third punch heating structure 43 is used to heat the third punch heating zone 23. This facilitates the temperature control of different areas of the punch structure 20, thereby enabling corresponding temperature control of different areas of the double-layer plate 01.
[0036] like Figure 4 As shown, the die structure 10 includes, in its radial direction from the outside in, a first die heating zone 14, a second die heating zone 15, and a third die heating zone 16, wherein the groove cavity 12 is located in the second die heating zone 15. In the radial direction of the die structure 10, the forming mold also includes, in its radial direction from the outside in, a first die heating structure 44, a second die heating structure 45, and a third die heating structure 46. The first die heating structure 44 is used to heat the first die heating zone 14, the second die heating structure 45 is used to heat the second die heating zone 15, and the third die heating structure 46 is used to heat the third die heating zone 16. This facilitates the temperature control of different areas of the die structure 10, thereby enabling corresponding temperature control of different areas of the double-layer plate 01.
[0037] Optionally, the press of this application integrates a high-precision thermocouple, which is used to monitor in real time and ensure that the forming temperature accurately reaches the preset value, thereby ensuring the accuracy and reliability of forming.
[0038] Optionally, the plate substrate described above and below in this application is an aluminum alloy substrate.
[0039] It should be noted that the forming mold in this application integrates a high-precision gas pressure control module and an advanced heating temperature control module to ensure the forming reliability of the forming mold. Applying boron nitride to the forming surface of the forming mold helps to improve the lubricity of the forming mold and can also effectively prevent oxidation reactions, laying a solid foundation for the subsequent forming process.
[0040] like Figure 10 As shown, the forming method of the double-layer panel box body is based on the forming molds described above and below, and the forming method includes: Step S1: Wire cut the plate substrate to cut out two plate structures of the required size, and perform zoning preprocessing on each plate structure. Step S2: Stack the two plate structures that have completed the partitioning preprocessing together, and perform edge sealing and butt welding on the outer periphery of the two plate structures to form a closed double-layer plate 01. Reserve an air inlet 03 on one of the plate structures in the double-layer plate 01, and use the plate structure with the air inlet 03 as the inner plate 010, and the plate structure without the air inlet 03 as the outer plate 011. Step S3: Place the double-layer plate 01, which has completed step S2, on the cavity structure 10 of the forming mold. Heat the punch structure 20 and the cavity structure 10 of the forming mold through the upper heating structure and the lower heating structure respectively. At the same time, under the heat conduction of the punch structure 20 and the cavity structure 10, the double-layer plate 01 is heated to the target forming temperature. Step S4: After the double-layer plate 01 is heated to the target forming temperature and kept at that temperature for a first preset time, the pressure ring structure 30 of the forming mold moves downward to the mold closing position and presses the non-deformable area of the double-layer plate 01 under the action of constant pressure force, so that the surface of the outer plate 011 facing the cavity structure 10 and the cavity wall surface of the cavity 11 of the cavity structure 10 form a closed space. Step S5: After the enclosed space is formed, while the punch structure 20 moves downward at a constant speed, gas with a first preset pressure is injected into the mold cavity 11 through the first ventilation pipe 13 on the die structure 10, so that the double-layer plate 01 is gradually stretched under the combined action of the rigid pressure of the punch structure 20 and the flexible pressure of the gas until the die structure 10 and the punch structure 20 are closed. Step S6: After the double-layer plate 01 is tightly attached to the punch structure 20, stop filling the mold cavity 11 with gas and unload the air pressure. The punch structure 20 continues to apply the second preset pressure to perform diffusion welding on the area of the double-layer plate 01 that is not coated with solder resist. Step S7: After the diffusion welding process is completed, gas at a third preset pressure is injected into the area of the double-layer plate 01 where no solder resist is applied through the second vent pipe 31 and the air inlet 03 on the pressure ring structure 30. Under the action of gas pressure, the material of the inner layer plate 010 continues to be tightly attached to the punch structure 20, and the local material of the outer layer plate 011 that has not participated in the diffusion welding process gradually flows to the groove cavity 12 of the die structure 10 until the outer layer plate 011 is completely attached to the die structure 10. The pressure is maintained for a second preset time so that the liquid cooling channel 04 expands and takes shape. Step S8: After completing the forming operation of the double-layer plate 01, turn off the power, slowly cool down to below the preset temperature, and then open the furnace door for natural cooling so that the punch structure 20, the die structure 10, and the formed part cool down to room temperature with the furnace. Then, take out the formed part and test its quality and performance.
[0041] Further, in step S1, the partition pretreatment includes first performing a surface pretreatment to retain the oxide layer on the non-diffusion soldering area of the board structure, and then applying solder resist to the non-diffusion soldering area after the surface pretreatment to retain the oxide layer is completed; then performing a surface pretreatment to remove the oxide layer on the diffusion soldering area of the board structure, and then polishing the diffusion soldering area with sandpaper after the surface pretreatment to remove the oxide layer is completed, so that the surface roughness of the diffusion soldering area is within a preset roughness range.
[0042] Preferably, 800# sandpaper is used.
[0043] Specifically, in the non-diffusion soldering area, only surface cleaning is performed, retaining the oxide layer to act as a bonding inhibitor. Solder resist is precisely applied to the non-diffusion soldering area. In the diffusion soldering area, a rigorous surface cleaning operation is required. Ultrasonic cleaning is used to remove surface oil, and mechanical processing is used to remove the oxide film in the diffusion soldering area. At the same time, the surface roughness is kept at the optimal level, and sandpaper is used to finely polish the diffusion soldering area.
[0044] Furthermore, before applying solder resist to the non-diffusion soldering area, the flow path of material deformation during the forming process of the double-layer plate 01 is simulated using simulation technology, and the positions of the expansion channel and the inter-plate air filling path are determined. The corresponding positions of the expansion channel and the inter-plate air filling path are found on the plate structure. The positions of the expansion channel and the inter-plate air filling path are both taken as the non-diffusion soldering area, and the area of the double-layer plate 01 other than the non-diffusion soldering area is taken as the diffusion soldering area.
[0045] Optionally, the simulation technology is finite element simulation technology.
[0046] Furthermore, in step S3, during the heating of the punch structure 20 and die structure 10 of the forming mold by the upper and lower heating structures respectively, the temperature provided to the area of the double-layer plate 01 that promotes material thinning is higher than the temperature provided to the area of the double-layer plate 01 that inhibits material thinning. This facilitates the realization of regional temperature forming of the product, ensures uniform distribution of product wall thickness, and improves product quality and performance.
[0047] It should be noted that, in this application, the heating method for heating the punch structure 20 and the die structure 10 of the forming mold through the upper heating structure and the lower heating structure respectively includes: The first punch heating structure 41 heats the first punch heating zone 21 to a first preset temperature T1; The second punch heating structure 42 heats the second punch heating zone 22 to the second preset temperature T2; The third punch heating structure 43 heats the third punch heating zone 23 to a third preset temperature T3; wherein, T1 = T3 < T2; and / or, The first die heating structure 44 heats the first die heating zone 14 to the fourth preset temperature T4; The second die heating structure 45 heats the second die heating zone 15 to the fifth preset temperature T5; The third die heating structure 46 heats the third die heating zone 16 to a sixth preset temperature T6; where T4 = T6 < T5.
[0048] This application proposes a forming mold and forming method for a double-layer plate box with flow channels. The target forming part is a double-layer plate box with a boss structure 02 at the bottom and a liquid cooling flow channel 04 on the outer layer to achieve efficient liquid cooling heat dissipation. The forming method integrates the synergistic effect of gas pressure and mold pressure. By precisely controlling the gas pressure acting on the outer plate, it is made to accurately fit the surface of the punch structure 20 to form the required shape. Subsequently, with the help of the mold closing pressure of the die structure 10 and the punch structure 20, under specific temperature and other conditions, the double-layer plate material outside the expansion flow channel area and the inter-plate air filling path area is ensured to be firmly welded. After the double-layer plate is welded, by carefully controlling the gas pressure and combining the fine design of the die structure 10 and the punch structure 20, the required shape of the liquid cooling flow channel 04 is further formed between the double-layer plates. The shape of the liquid cooling flow channel 04 is mainly determined by the expansion pressure and the precise position and shape of the die structure 10.
[0049] Furthermore, the development of heating rods with independent temperature control (i.e., heating structure 40) allows for zoned temperature control of the heating zone on each heating rod, ensuring precise temperature control across all parts of the mold and enabling zoned temperature forming of aluminum alloy sheets. The hydraulic press forming equipment used is equipped with a zoned temperature control system for the mold. This system overcomes the limitation of uniform temperature in the forming zone of traditional forming machines, allowing for independent temperature adjustment at specific locations within the mold. Simultaneously, high-precision thermocouples are integrated inside the mold to monitor and ensure the forming temperature accurately reaches the preset value in real time, thereby ensuring the precision and reliability of the forming process.
[0050] Step 1: In the preliminary preparation stage, the forming mold integrates key components such as a high-precision gas pressure control module and an advanced heating temperature control module to ensure the reliability of the forming process. Applying boron nitride to the forming surface of the mold not only improves its lubrication performance but also effectively prevents oxidation, laying a solid foundation for the subsequent forming process.
[0051] Step Two: In the pretreatment stage of the aluminum alloy double-layer plate, the substrate is first cut into the required plate structure dimensions using high-precision wire cutting technology. The plate structure has clearly defined diffusion and non-diffusion welding zones. In the non-diffusion welding area, only routine surface cleaning is performed, retaining the oxide layer as a bonding agent. However, in the diffusion welding area, a rigorous surface cleaning process is required. Ultrasonic cleaning removes surface oil, and mechanical treatment removes the oxide film from the diffusion welding area, ensuring optimal surface roughness, as the interface roughness of the diffusion welding process is beneficial for joint bonding. Therefore, 800# sandpaper is used for fine polishing of the diffusion welding area of the plate structure. Solder resist is precisely applied to the non-diffusion welding area. The location of the solder resist relies on advanced finite element simulation technology, which simulates the material deformation and flow path of the plate structure throughout the forming process, locating the positions of the expansion channels and the inter-plate inflation paths. By reverse engineering, the positions of the required expansion channels on the original plate and the inter-plate inflation paths are found, and solder resist is applied at the corresponding locations. Subsequently, to ensure stable and effective air expansion pressure during the forming process, the edges of the plate structure are sealed by butt welding to form a well-sealed system with good airtightness. At the same time, to connect the air inlet path, air inlets are reserved at the edges to provide the required vacuum environment and air inlet channel during diffusion welding to expand and form the bottom flow channel characteristics.
[0052] Step 3: In the furnace heating stage, the pre-treated plate structure is first placed at a suitable position on the upper surface of the die structure 10. Then, the temperature of the heating rods is adjusted through the upper and lower die heating platforms to raise the mold temperature, and the mold temperature is transferred to the plate structure through heat conduction. Alternatively, the heating device can be upgraded to achieve independent temperature control at specific locations on the mold. This involves using individually adjustable heating rods, allowing independent temperature zone control for each heating zone. This zoned temperature control technology enables precise temperature control for different areas of the plate structure. Higher temperatures are provided in areas where material thinning is desired to enhance deformation capacity, while lower temperatures are maintained in areas where thinning is inhibited to limit deformation. This achieves zoned temperature forming of the product, ensuring uniform wall thickness distribution and improving product quality and performance.
[0053] Step 4: Deep drawing stage of the box-shaped part. After the sheet structure is heated to the target forming temperature of about 480℃ and held at that temperature for a period of time, the press is started, and the load is precisely controlled to drive the blank holder structure 30 downward until the mold closes. Under the action of constant blank holder force, the blank holder structure 30 tightly presses the sheet structure, ensuring that the mold cavity space between the sheet structure and the die structure 10 is in a sealed state, preparing for the subsequent gas-assisted deep drawing process. Next, under the precise control of the hydraulic press, the upper die 3 moves downward at a constant speed of about 5mm / min, gradually drawing and deforming the sheet structure. Under the pressure of the upper die 3, the sheet structure enters the mold cavity of the die structure 10. At the same time, nitrogen gas of about 2MPa is introduced through the first vent pipe 13 on the die structure 10. Under the action of gas pressure, the sheet structure gradually flows towards the punch structure 20 and gradually fits into the punch structure 20. Under the combined action of the rigid pressure of the punch structure 20 and the flexible pressure of the gas, the plate structure gradually flows into the mold cavity of the die structure 10 until the upper and lower dies are completely closed, and the plate structure is completely attached to the punch structure 20. At this time, the pressure is maintained for about 20 minutes to ensure the forming effect. Subsequently, the air pressure is released, and the double-layer plate 01 is tightly attached to the upper die, with the shape of the inner plate consistent with the punch structure 20. The boss is formed mainly by the precise closing of the upper and lower dies. Afterward, the press equipment applies a pressure of about 10 MPa to perform diffusion welding on the parts of the plate structure that are not coated with solder resist, so that the joint surface can fully contact and produce slight plastic deformation. Throughout the welding process, the mechanical vacuum pump maintains the vacuum level of the internal environment and ensures that the welding interface is kept at a temperature of about 500°C for about 2 hours to allow sufficient reaction time for the joint interface to ensure the connection quality.
[0054] Step 5: Flow channel bulging stage. After the diffusion welding process is completed, approximately 1 MPa of nitrogen gas is introduced through a gas storage cylinder into the second vent pipe 31 on the pressure ring structure 30, and then flows into the inflation port 03 pre-installed on the outer edge of the plate structure flange. Under the action of gas pressure, the inner layer material continues to adhere tightly to the upper mold, while the material in the outer layer that did not participate in the diffusion welding process gradually flows towards the pre-set flow channel groove cavity feature at the bottom of the die structure 10, until the outer layer and the die structure 10 are completely adhered. Pressure is maintained for approximately 10 minutes, at which point the flow channel is bulged out. That is, single-plate flow channel bulging is achieved by gas pressure, and the shape of the outer layer precisely matches the surface of the die structure 10, thus obtaining a complete double-layer box-shaped part with flow channels.
[0055] Step Six: Post-processing of the formed part. After the forming process is complete, the power is turned off, and the heating equipment is stopped. A precise control system gradually unloads the gas pressure and mold pressure, ensuring a smooth and safe unloading process. To avoid deformation caused by sudden cooling, the material must be slowly cooled to below 150°C before the furnace door can be opened for natural cooling. The mold and formed part slowly cool to room temperature inside the furnace. This step not only ensures uniform cooling of the material but also avoids potential performance loss due to excessive temperature differences. Finally, the formed part with the double-layer structure is removed and carefully inspected according to strict process standards to ensure that the quality and performance of the formed part meet the preset standards.
[0056] The beneficial effects of the technical solution of this invention are as follows: (1) Good surface quality and high forming accuracy. The use of inert gas flexible medium to replace the traditional rigid die in stamping allows the sheet metal to undergo flexible deformation, reducing the impact on the die and alleviating the rigid hard contact friction between the sheet metal and the die during deep drawing, thereby avoiding scratches caused by friction between the sheet metal and the rigid die. During the forming process, the sheet metal is pressed tightly against the punch by the gas pressure, and the inner layer is pressed tightly against the punch. The shape of the inner layer of the product mainly depends on the punch, and the inner layer size is consistent with the punch size. The shape of the outer layer of the product mainly depends on the die. Through the gas expansion forming of the flow channel groove feature, the outer layer size is consistent with the die size. The production stability is better than the traditional rigid die deep drawing process, effectively avoiding wrinkling and cracking defects. In addition, the presence of the gas flexible medium can also help the sheet metal flow and improve the sheet metal fluidity. At the same time, it can also enhance the beneficial friction effect between the sheet metal and the die, improve the deep drawing limit, and help improve the overall forming quality of the product.
[0057] (2) Low production cost. Traditional forming methods often require multiple processes, while this process, through the synergistic effect of gas pressure and mold, forms the box-shaped part in one step. After diffusion welding, the flow channel is expanded, achieving rigid punch rigid medium forming and gas flexible medium forming in one thermal cycle. Compared with traditional methods, there are fewer forming processes, and only one set of molds is needed to complete the entire production process. Therefore, the mold development work is also reduced accordingly, which not only saves mold development time and reduces mold cost, but also reduces mold wear and avoids the need for frequent mold replacement. In addition, this process has lower tonnage requirements for forming equipment, thereby reducing equipment investment costs, reducing the consumption of human and material resources, and improving production efficiency, resulting in considerable economic benefits.
[0058] (3) By adjusting the temperature parameters of the heating rod and the distribution position of the heating zone, the aluminum alloy sheet can be heated in different areas to obtain a more ideal material distribution flow trend and wall thickness distribution form, so as to realize the material distribution on demand, improve the material utilization rate, improve the wall thickness uniformity, and improve the mechanical properties.
[0059] Applying the forming process of this invention to the processing and production of double-layer plate boxes that require liquid cooling can solve the problems of poor quality, low yield, low efficiency, and high cost caused by traditional forming methods, ultimately achieving the effects of high efficiency, energy saving, cost reduction and efficiency improvement.
[0060] This invention provides a forming mold and forming method for a double-layer plate box with flow channels, cleverly combining the coordinated forming technology of rigid and flexible media to precisely manufacture double-layer structural components. It fully utilizes the improved wall thickness uniformity characteristics of zoned heating, sequentially completing the forming of complex feature areas of the double-layer plate and the zoned connection within a single mold. This effectively controls the forming effect of the aluminum alloy double-layer plate, avoiding the process defects of traditional forming technologies. It aims to improve product forming quality, enhance product structural strength, increase product forming efficiency, reduce product processing and manufacturing costs, and achieve lightweight product structure.
[0061] It should be noted that the terminology used herein is for the purpose of describing particular embodiments only and is not intended to limit the exemplary embodiments according to this application. As used herein, the singular form is intended to include the plural form as well, unless the context clearly indicates otherwise. Furthermore, it should be understood that when the terms "comprising" and / or "including" are used in this specification, they indicate the presence of features, steps, operations, devices, components, and / or combinations thereof.
[0062] Unless otherwise specifically stated, the relative arrangement, numerical expressions, and values of the components and steps set forth in these embodiments do not limit the scope of the invention. It should also be understood that, for ease of description, the dimensions of the various parts shown in the drawings are not drawn to actual scale. Techniques, methods, and devices known to those skilled in the art may not be discussed in detail, but where appropriate, such techniques, methods, and devices should be considered part of the specification. In all examples shown and discussed herein, any specific values should be interpreted as merely exemplary and not as limitations. Therefore, other examples of exemplary embodiments may have different values. It should be noted that similar reference numerals and letters in the following figures denote similar items; therefore, once an item is defined in one figure, it need not be further discussed in subsequent figures.
[0063] For ease of description, spatial relative terms such as "above," "on top of," "on the upper surface of," "above," etc., are used herein to describe the spatial positional relationship of a device or feature as shown in the figures to other devices or features. It should be understood that spatial relative terms are intended to encompass different orientations in use or operation beyond the orientation of the device as described in the figures. For example, if the device in the figures were inverted, a device described as "above" or "on top of" other devices or structures would subsequently be positioned as "below" or "under" other devices or structures. Thus, the exemplary term "above" can include both "above" and "below." The device may also be positioned in other different ways (rotated 90 degrees or in other orientations), and the spatial relative descriptions used herein will be interpreted accordingly.
[0064] It should be noted that the terminology used herein is for the purpose of describing particular embodiments only and is not intended to limit the exemplary embodiments according to this application. As used herein, the singular form is intended to include the plural form as well, unless the context clearly indicates otherwise. Furthermore, it should be understood that when the terms "comprising" and / or "including" are used in this specification, they indicate the presence of features, steps, operations, devices, components, and / or combinations thereof.
[0065] It should be noted that the terms "first," "second," etc., used in the specification, claims, and accompanying drawings of this application are used to distinguish similar objects and are not necessarily used to describe a specific order or sequence. It should be understood that such data can be interchanged where appropriate so that the embodiments of this application described herein can be implemented in sequences other than those illustrated or described herein.
[0066] The above description is merely a preferred embodiment of the present invention and is not intended to limit the invention. Various modifications and variations can be made to the present invention by those skilled in the art. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of the present invention should be included within the scope of protection of the present invention.
Claims
1. A forming mold for a double-layer panel box, characterized in that, include: A concave mold structure (10) has a portion of its upper surface recessed to form a mold cavity (11), and the bottom surface of the mold cavity (11) has 2N spaced groove cavities (12), and the concave mold structure (10) has a first ventilation pipe (13), the first end of the first ventilation pipe (13) is connected to an external air source, the second end of the first ventilation pipe (13) is connected to the mold cavity (11), and the connection point between the two is located at a position on the bottom surface of the mold cavity (11) that avoids the groove cavities (12); A punch structure (20) is vertically and flexibly disposed above the die structure (10). The punch structure (20) has M protruding bodies (24) on one side surface facing the mold cavity (11), and M=N, so that the M protruding bodies (24) are arranged in a one-to-one correspondence with the N groove cavities (12). The protruding bodies (24) extend into the groove cavities (12) to stamp out boss structures (02) on the double-layer plate (01). A pressure ring structure (30) is located on the outer periphery of the punch structure (20) and can be raised and lowered. The pressure ring structure (30) is arranged opposite to the outer periphery of the mold cavity (11). The pressure ring structure (30) has a second ventilation pipe (31). The first end of the second ventilation pipe (31) is connected to an external air source. The second end of the second ventilation pipe (31) is used to connect to the air inlet (03) on the double-layer plate (01) so as to flush the non-diffusion soldering area of the outer layer plate (011) of the double-layer plate (01) without solder resist into the remaining N groove cavities (12) to form a liquid cooling channel (04). The N groove cavities (12) used to form the boss structure (02) are staggered with the N groove cavities (12) used to form the liquid cooling channel (04).
2. The forming mold according to claim 1, characterized in that, The first ventilation conduit (13) includes a first sub-conduit (131) and a second sub-conduit (132) that are connected to each other, wherein, The first end of the first sub-pipe (131) extends radially along the concave mold structure (10) and penetrates the circumferential outer surface of the concave mold structure (10) to form the first end of the first ventilation pipe (13); The first end of the second sub-pipe (132) is connected to the second end of the first sub-pipe (131), and the second end of the second sub-pipe (132) extends along the axial direction of the concave mold structure (10) and penetrates the bottom surface of the mold cavity (11) to form the second end of the first ventilation pipe (13).
3. The forming mold according to claim 1, characterized in that, The second ventilation duct (31) includes a third sub-duct (311) and a fourth sub-duct (312) that are connected to each other, wherein, The first end of the third sub-pipe (311) extends radially along the pressure ring structure (30) and penetrates the circumferential outer surface of the pressure ring structure (30) to form the first end of the second ventilation pipe (31); The first end of the fourth sub-pipe (312) is connected to the second end of the third sub-pipe (311). The second end of the fourth sub-pipe (312) extends along the axial direction of the pressure ring structure (30) and penetrates the end surface of the pressure ring structure (30) on the side facing the die structure (10) to form the second end of the second ventilation pipe (31).
4. The forming mold according to claim 1, characterized in that, The punch structure (20) includes a first punch heating zone (21), a second punch heating zone (22), and a third punch heating zone (23) in a radial direction from the outside to the inside, wherein the protruding body (24) is located in the second punch heating zone (22). In the radial direction of the punch structure (20), the forming mold also includes a first punch heating structure (41), a second punch heating structure (42), and a third punch heating structure (43) in sequence from the outside to the inside. The first punch heating structure (41) is used to heat the first punch heating area (21), the second punch heating structure (42) is used to heat the second punch heating area (22), and the third punch heating structure (43) is used to heat the third punch heating area (23).
5. The forming mold according to claim 1, characterized in that, The die structure (10) includes a first die heating area (14), a second die heating area (15), and a third die heating area (16) in a radial direction from the outside to the inside, wherein the groove cavity (12) is located in the second die heating area (15). In the radial direction of the die structure (10), the forming mold also includes a first die heating structure (44), a second die heating structure (45), and a third die heating structure (46) in sequence from the outside to the inside. The first die heating structure (44) is used to heat the first die heating area (14), the second die heating structure (45) is used to heat the second die heating area (15), and the third die heating structure (46) is used to heat the third die heating area (16).
6. A method for forming a double-layered panel box, characterized in that, The forming method is based on the forming mold according to any one of claims 1 to 5, and the forming method includes: Step S1: Wire cut the plate substrate to cut out two plate structures of the required size, and perform partition preprocessing on each of the plate structures. Step S2: Stack the two plate structures that have completed the partitioning preprocessing together, and perform edge sealing and butt welding on the outer periphery of the two plate structures to form a closed double-layer plate (01). Reserve an air inlet (03) on one of the plate structures in the double-layer plate (01), and use the plate structure with the air inlet (03) as the inner plate (010), and the plate structure without the air inlet (03) as the outer plate (011). Step S3: The double-layer plate (01) after completing step S2 is placed on the cavity structure (10) of the forming mold. The upper heating structure and the lower heating structure heat the punch structure (20) and the cavity structure (10) of the forming mold respectively. At the same time, under the heat conduction of the punch structure (20) and the cavity structure (10), the double-layer plate (01) is heated to the target forming temperature. Step S4: After the double-layer plate (01) is heated to the target forming temperature and kept at that temperature for a first preset time, the pressure ring structure (30) of the forming mold moves downward to the mold closing position and presses the non-deformable area of the double-layer plate (01) under the action of constant pressure force, so that the surface of the outer plate (011) facing the cavity structure (10) and the cavity wall of the cavity (11) of the cavity structure (10) form a closed space. Step S5: After the sealed space is formed, the punch structure (20) moves downward at a constant speed while the first ventilation pipe (13) on the die structure (10) fills the mold cavity (11) with a first preset pressure of gas, so that the double plate (01) is gradually stretched under the combined action of the rigid pressure of the punch structure (20) and the flexible pressure of the gas until the die structure (10) and the punch structure (20) are closed. Step S6: After the double-layer plate (01) is tightly attached to the punch structure (20), stop filling the mold cavity (11) with gas and unload the gas pressure. The punch structure (20) continues to apply a second preset pressure to perform diffusion welding on the area of the double-layer plate (01) that is not coated with solder resist. Step S7: After the diffusion welding process is completed, gas at a third preset pressure is injected into the area of the double-layer plate (01) without solder resist through the second vent pipe (31) on the pressure ring structure (30) and the air inlet (03). Under the action of gas pressure, the material of the inner layer plate (010) continues to be tightly attached to the punch structure (20), and the local material of the outer layer plate (011) that has not participated in the diffusion welding process gradually flows to the groove cavity (12) of the die structure (10) until the outer layer plate (011) and the die structure (10) are completely attached. The pressure is maintained for a second preset time so that the liquid cooling channel (04) expands and takes shape. Step S8: After completing the forming operation of the double-layer plate (01), turn off the power, slowly cool down to below the preset temperature, open the furnace door for natural cooling, so that the punch structure (20), the die structure (10), and the formed part are cooled to room temperature with the furnace, then take out the formed part and test the quality and performance of the formed part.
7. The forming method according to claim 6, characterized in that, In step S1, the partition preprocessing includes: The non-diffusion soldering area of the plate structure is first subjected to surface pretreatment to retain the oxide layer. After the surface pretreatment to retain the oxide layer is completed, solder resist is applied to the non-diffusion soldering area. The diffusion welding area of the plate structure is subjected to surface pretreatment to remove the oxide layer. After the surface pretreatment to remove the oxide layer is completed, the diffusion welding area is polished with sandpaper.
8. The forming method according to claim 7, characterized in that, Before applying solder resist to the non-diffusion soldering area, the flow path of material deformation of the double-layer plate (01) during the forming process is simulated by simulation technology, and the positions of the expansion channel and the inter-plate air filling path are determined. The corresponding positions of the expansion channel and the inter-plate air filling path are found on the plate structure. The positions of the expansion channel and the inter-plate air filling path are both used as the non-diffusion soldering area, and the area of the double-layer plate (01) other than the non-diffusion soldering area is used as the diffusion soldering area.
9. The forming method according to claim 6, characterized in that, In step S3, during the process of heating the punch structure (20) and die structure (10) of the forming mold by the upper heating structure and the lower heating structure respectively, the temperature provided to the area of the double-layer plate (01) that promotes material thinning is higher than the temperature provided to the area of the double-layer plate (01) that inhibits material thinning.
10. The forming method according to claim 9, characterized in that, In step S3, the heating method for heating the punch structure (20) and die structure (10) of the forming mold through the upper heating structure and the lower heating structure respectively includes: The first punch heating structure (41) heats the first punch heating area (21) to the first preset temperature T1; The second punch heating structure (42) heats the second punch heating area (22) to the second preset temperature T2; The third punch heating structure (43) heats the third punch heating zone (23) to a third preset temperature T3; wherein, T1=T3<T2; and / or, The first die heating structure (44) heats the first die heating area (14) to the fourth preset temperature T4; The second die heating structure (45) heats the second die heating zone (15) to the fifth preset temperature T5; The third die heating structure (46) heats the third die heating zone (16) to the sixth preset temperature T6; where T4=T6<T5.
Citation Information
Patent Citations
Lock latch type rigid and plastic compound bulging device for t-branch pipe
CN105234243A
Liquid-filling forming mold
CN106799424A