High-stripping acrylate adhesive for motor train unit and preparation process of high-stripping acrylate adhesive
Through specific acrylic glue ratio and process, the problem of insufficient anti-fatigue performance and peel strength in EMUs is solved, the odor is reduced, and high bonding strength and anti-fatigue performance are achieved, ensuring that the glue layer is not sticky and suitable for Used in high-speed EMUs.
Patent Information
- Application Number
- CN202411108437.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-13
- Publication Date
- 2024-10-25
AI Technical Summary
The existing two-component structural bonding acrylate adhesive has insufficient fatigue resistance and peeling strength caused by high-frequency vibration in high-speed EMU applications. At the same time, it contains methyl methacrylate and has a strong pungent odor, which is opposed by workers. .
The main agent component and the curing agent component are used in a ratio of 10:1 by mass, and raw materials such as methacrylate monomers, polyurethane modified acrylates and tougheners are used to prepare EMU components through specific process steps. High-release acrylic glue reduces odor and improves bonding strength and fatigue resistance, ensuring that the glue layer does not become sticky after curing.
An acrylic adhesive with excellent bonding properties to metal materials, high peel strength, excellent fatigue resistance and low odor has been realized to ensure that the adhesive layer does not become sticky after curing and meets the safety requirements of EMU parts.
Smart Images

Figure SMS_1
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of adhesives, and in particular to a high-peeling acrylic adhesive for electric train sets and a preparation process thereof. Background Art
[0002] Two-component structural bonding acrylic adhesive is widely used in structural bonding in the automotive, machinery, electronics, furniture, instrumentation, railway vehicles, civil engineering and other industries due to its rapid curing at room temperature, high strength, good toughness and easy operation.
[0003] When high-speed EMU vehicles are running, their parts are in a state of high-frequency vibration for a long time, such as the elastic support of the floor and the anti-pullout parts of the seats. In order to ensure their safety, the fatigue resistance and peel strength of the parts have become key indicators. And with the progress of the times, the continuous improvement of policies and regulations, and the continuous improvement of consumers' quality requirements. Two-component structural bonding acrylic glue has a strong pungent odor due to the large amount of methyl methacrylate, and is increasingly rejected by workers.
[0004] Therefore, it is urgent to develop an acrylic adhesive that has excellent bonding properties to metal materials, high peel strength, excellent fatigue resistance and can reduce odor. Summary of the invention
[0005] Therefore, in view of the above-mentioned problems, the present invention provides a high-peeling acrylic adhesive for EMUs and a preparation process thereof. The high-peeling acrylic adhesive for EMUs of the present invention has the advantages of low odor, excellent bonding strength to metal materials, high peeling strength, excellent fatigue resistance, and the surface of the adhesive layer will not become sticky after curing.
[0006] In order to solve this technical problem, the present invention adopts the following scheme: a high-peeling acrylic adhesive for EMU, which is composed of a main agent component and a curing agent component in a ratio of 10:1 by mass. The main agent component is composed of the following raw materials by mass percentage: (A) 25% to 50% wt methacrylate monomer; (B) 1% to 10% wt epoxy resin; (C) 35% to 55% wt polyurethane modified acrylate; (D) 5% to 15% Wt toughening agent; (E) 0.1%~2%Wt fully refined paraffin; (F) 5% to 10% Wt filler; (G) 0.01%~5%Wt stabilizer; (H) 0.1%~2%Wt accelerator; (I) 1% to 10% wt adhesion promoter; (J) 1% to 5% Wt coupling agent; Wherein, the methacrylate monomer is one of hydroxyethyl methacrylate, hydroxypropyl methacrylate, lauryl methacrylate, isobornyl methacrylate, 2-phenoxyethyl methacrylate, tetrahydrofuran methacrylate, ethoxylated bisphenol A dimethacrylate, trimethylolpropane trimethacrylate or a mixture thereof, and the polyurethane modified acrylate is a polyurethane acrylate obtained by polymerization of hydrogenated bisphenol A, polyethylene glycol and isocyanate and capped with a methacrylate monomer; The curing agent component is composed of the following raw materials by mass percentage: (A) 30% to 60% Wt plasticizer; (B) 5% to 15% Wt toughening agent; (C) 0.1% to 2% Wt pigment; (D) 15% to 30% wt oxidant; (E) 5% to 10% Wt filler; The fillers in the main agent component and the curing agent component are calcium carbonate, silicon micropowder, hollow glass microspheres, polyethylene powder or a mixture thereof.
[0007] Furthermore, the epoxy resin is one of 828EL epoxy resin and 128E epoxy resin or a mixture thereof.
[0008] Furthermore, the toughening agent is MBS, ABS high rubber powder or a mixture thereof.
[0009] Furthermore, the fully refined paraffin wax is one of WAX-120, WAX-145, WAX-156 or a mixture thereof.
[0010] Furthermore, the stabilizer is one of phenolic compounds, quinone compounds, oxalic acid, sodium salt, phenothiazine or a mixture thereof.
[0011] Furthermore, the accelerator is one of N,N-dimethyl-p-toluidine, N,N-diethyl-p-toluidine, N,N-diethyl-m-toluidine, N,N-dihydroxyethyl-p-methylaniline, zinc dimethacrylate or a mixture thereof.
[0012] Furthermore, the coupling agent is a silane coupling agent or a mixture thereof, and the oxidant is benzoyl peroxide.
[0013] Furthermore, the plasticizer is one of DOP, DIDP, DEHP or a mixture thereof.
[0014] Furthermore, the pigment is iron blue, milori blue or a mixture thereof.
[0015] The method for preparing the high-peeling acrylic adhesive for EMUs comprises the following steps: (1) Preparation of polyurethane modified acrylate: IBOMA and isocyanate are added into a reaction bottle, the temperature in the reaction bottle is raised to 80-90°C, and stirred for 30-60 minutes; hydrogenated bisphenol A is then added into the reaction bottle and the temperature in the reaction bottle is controlled at 80-90°C, and stirred for 120-150 minutes; then PTMG is added into the reaction bottle and the temperature is controlled at 75-85°C, and stirred for 120-150 minutes; finally, monofunctional methacrylate monomer is added into the reaction bottle and the temperature is controlled at 70-80°C, and stirred for 120-150 minutes to obtain polyurethane modified acrylate; (2) Main agent component: put methacrylate monomer, epoxy resin and fully refined paraffin into a reaction kettle, heat to 70°C-75°C, add polyurethane modified acrylate and toughening agent, stir until completely dissolved, stop heating, add filler, stir until completely dissolved, add stabilizer, stir evenly, cool to below 30°C, add accelerator, adhesion promoter and coupling agent, stir evenly to obtain the main agent component; (3) Curing agent component: put the plasticizer and oxidant into the reaction kettle, add the toughening agent, stir until completely dissolved, add the pigment and filler, stir evenly, control the material temperature below 30°C during the stirring process, and vacuum degassing to obtain the curing agent component; (4) The main agent component prepared in step (2) and the curing agent component prepared in step (3) are mixed evenly in a mass ratio of 10:1 to obtain a high-peeling acrylic adhesive for EMUs.
[0016] By adopting the above technical scheme, the beneficial effects of the present invention are as follows: compared with the existing acrylic adhesives on the market, the present invention adopts methacrylic acid higher esters to replace methyl methacrylate, so that the product has low odor and the surface of the adhesive layer will not be sticky after curing. At the same time, methacrylate monomers, polyurethane modified acrylates and toughening agents react under the action of oxidants and promoters to improve the chemical bond and mechanical bonding force between the acrylic adhesive of the present invention and the substrate. At the same time, by making homemade polyurethane modified acrylates and introducing special fillers, the acrylic adhesive of the present invention has very good bonding strength to metal materials, high peel strength and excellent fatigue resistance. By introducing adhesion promoters such as phosphate esters, the bonding strength of the acrylic adhesive of the present invention to metal materials is further improved, so that it can produce very good bonding performance and bonding strength with metal materials. In addition, by introducing methacrylate monomers of different types and proportions, and cooperating with the introduction of fully refined paraffin wax, the adhesive layer will not be sticky after curing. DETAILED DESCRIPTION
[0017] The present invention will now be further described in conjunction with specific implementation methods. Embodiment 1:
[0018] The preferred high-peeling acrylic adhesive for EMUs is composed of a main agent component and a curing agent component in a ratio of 10:1 by mass: Embodiment 1:
[0019] Modification of polyurethane modified acrylate: 1. Put IBOMA and isocyanate into the reaction bottle; 2. Raise the temperature to 80-90°C and stir for 30-60 minutes; 3. Add hydrogenated bisphenol A into the reaction bottle; 4. Control the temperature at 80-90°C and stir for 120-150 minutes; 5. Add PTMG into the reaction bottle, control the temperature at 75-85°C, and stir for 120-150 minutes; 6. Add the monofunctional methacrylate monomer into the reaction bottle, control the temperature at 70-80°C, and stir for 120-150 minutes; Main ingredients: 2-Phenoxyethyl Methacrylate 16.75%Wt Hydroxypropyl Methacrylate 15.00%Wt 828EL Epoxy Resin 2.00%Wt WAX-156 1.00%Wt MBS 13.00%Wt Polyurethane modified acrylate 35.00%Wt Hollow Glass Microspheres 4.00%Wt BHT 0.20%Wt Hydroquinone 0.05%Wt N, N-Dimethyl-p-toluidine 1.00%Wt PM1500 5.00%Wt Methacrylic acid 5.00%Wt KH-560 2.00%Wt; Curing agent components: DIDP 43.00%Wt DOA 15.80%Wt MBS 10.00%Wt Polyethylene powder 8.00%Wt BPO 23.00%Wt Milori Blue 0.20%Wt
[0020] Preparation method: (1) Main agent component: put methacrylate monomer, epoxy resin and fully refined paraffin into a reaction kettle, heat to 70°C-75°C, add polyurethane modified acrylate and toughening agent, stir until completely dissolved, stop heating, add filler, stir until completely dissolved, add stabilizer, stir evenly, cool to below 30°C, add accelerator, adhesion promoter and coupling agent, stir evenly to obtain the main agent component; (2) Curing agent component: Put the plasticizer and oxidant into the reaction kettle, add the toughening agent, stir until completely dissolved, add the pigment and filler, stir evenly. During the stirring process, control the material temperature below 30°C, and vacuum degassing to obtain the curing agent component.
[0021] Performance Testing: 1. Test method for tensile shear strength The bonded test pieces were cured for 24 hours and then subjected to a tensile shear strength test using a universal tensile testing machine in accordance with GB / T7124-2008.
[0022] 2. Test method for T-peel strength Determine according to the method specified in GB / T 2791. Each sample shall be tested in parallel at least 5 times and the average value shall be taken.
[0023] 3. Vibration fatigue The test was carried out according to the method specified in ISO 9664. Embodiment 2:
[0024] Main ingredients: 2-Phenoxyethyl Methacrylate 11.75%Wt Isobornyl Methacrylate 15.00%Wt 828EL Epoxy Resin 2.00%Wt WAX-156 1.00%Wt MBS 8.00%Wt Polyurethane modified acrylate 45.00%Wt Hollow Glass Microspheres 4.00%Wt MEHQ 0.20%Wt Phenothiazine 0.05%Wt N, N-Dimethyl-p-toluidine 1.00%Wt P-2M 5.00%Wt Methacrylic acid 5.00%Wt KH-560 2.00%Wt; Curing agent components: DOA 55.80%Wt MBS 10.00%Wt Polyethylene powder 5.00%Wt BPO 29.00%Wt Iron blue 0.20%Wt
[0025] The preparation method and performance test are the same as those in Example 1. Embodiment 3:
[0026] Main ingredients: Tetrahydrofuran Methacrylate 10.75%Wt Hydroxypropyl Methacrylate 15.00%Wt 128E Epoxy Resin 2.00%Wt WAX-120 0.50%Wt WAX-145 0.50%Wt MBS 3.00%Wt Polyurethane modified acrylate 50.00%Wt Hollow Glass Microspheres 3.00%Wt Calcium carbonate 2.00%Wt MEHQ 0.20%Wt Phenothiazine 0.05%Wt N, N-Dimethyl-p-toluidine 1.00%Wt P-2M 5.00%Wt Methacrylic acid 5.00%Wt KH-550 2.00%Wt; Curing agent components: DIDP 55.80%Wt MBS 13.00%Wt Polyethylene powder 5.00%Wt BPO 26.00%Wt Milori Blue 0.20%Wt
[0027] The preparation method and performance test are the same as those in Example 1.
[0028] Comparative Example 1: Main ingredients: Methyl Methacrylate 45.75%Wt Lauryl Methacrylate 4.00%Wt WAX-156 1.00%Wt Nitrile rubber 13.00%Wt MBS 16.00%Wt SBS 8.00%Wt Silica powder 4.00%Wt BHT 0.20%Wt Hydroquinone 0.05%Wt N, N-Diethyl-p-toluidine 1.00%Wt KH-560 2.00%Wt Methacrylic acid 5.00%Wt Curing agent components: Epoxy resin 23.00%Wt MBS 21.00%Wt BBP 22.00%Wt BPO 23.00%Wt Ferrosinic Oxide 7.00%Wt Titanium Dioxide 4.00% wt.
[0029] The preparation method and performance test are the same as those in Example 1.
[0030] The performance test of high-peeling acrylic adhesive for EMU prepared in Example 1 to Example 3 and Comparative Example 1 is as follows:
[0031] The performance test comparison of Examples 1 to 3 and Comparative Example 1 shows that compared with the acrylic adhesive currently on the market, the product of the present invention has the advantages of low odor, excellent bonding strength to metal materials, high peel strength, excellent fatigue resistance, and no stickiness on the surface after the adhesive layer is cured.
[0032] The weight percentage ratio of each raw material of the main agent component in the present invention is preferably the following ratio: main agent component: (A) 25% to 50% wt methacrylate monomer; (B) 1% to 10% wt epoxy resin; (C) 35% to 55% wt polyurethane modified acrylate; (D) 5% to 15% wt toughening agent; (E) 0.1% to 2% wt fully refined paraffin; (F) 5% to 10% wt filler; (G) 0.01%~5%Wt stabilizer; (H) 0.1%~2%Wt accelerator; (I) 1%~10%Wt adhesion promoter; (J) 1%~5%Wt coupling agent; curing agent components: (A) 30%~60%Wt plasticizer; (B) 5%~15%Wt toughening agent; (C) 0.1%~2%Wt pigment; (D) 15%~30%Wt oxidant; (E) 5%~10%Wt filler.
[0033] The methacrylate monomers in the main component and the curing agent component can also be hydroxyethyl methacrylate, hydroxypropyl methacrylate, lauryl methacrylate, isobornyl methacrylate, 2-phenoxyethyl methacrylate, tetrahydrofuran methacrylate, ethoxylated bisphenol A dimethacrylate, trimethylolpropane trimethacrylate or a mixture thereof; the epoxy resin can also be 828EL epoxy resin, 128E epoxy resin or a mixture thereof; the polyurethane modified acrylate is a polyurethane acrylate obtained by polymerization of hydrogenated bisphenol A, polyethylene glycol and isocyanate and end-capped with a methacrylate monomer; the toughening agent can also be MBS, ABS high-rubber powder or a mixture thereof; the fully refined paraffin can also be WAX-120, WAX-145, WAX-156 or a mixture thereof The filler may be one or a mixture of calcium carbonate, silicon powder, hollow glass microspheres, polyethylene powder; the stabilizer may be one or a mixture of phenolic compounds, quinone compounds, oxalic acid, sodium salt, phenothiazine; the promoter may be one or a mixture of N,N-dimethyl-p-toluidine, N,N-diethyl-p-toluidine, N,N-diethyl-m-toluidine, N,N-dihydroxyethyl-p-methylaniline, zinc dimethacrylate; the adhesion promoter may be one or a mixture of phosphate monomer, acrylated polyester adhesion promoter, methacrylic acid; the coupling agent may be a silane coupling agent or a mixture thereof; the plasticizer may be one or a mixture of DOP, DIDP, DEHP; the pigment may be one or a mixture of iron blue and milori blue; the oxidant may be benzoyl peroxide.
[0034] It should be noted that, in this article, words such as "include", "comprises" or any other variations thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of more restrictions. The phrase "including an element defined by ..." does not exclude the existence of other identical elements in the process, method, article or device including the element".
[0035] The above embodiments are only preferred embodiments of the present invention, and the present invention may also have other embodiments. For those of ordinary skill in the art, it will be appreciated that various changes, modifications, substitutions and variations may be made to these embodiments without departing from the principles and spirit of the present invention, and the scope of the present invention is limited by the appended claims and their equivalents.
Claims
1. A high-peeling acrylic adhesive for EMUs, Features: It is composed of the main agent component and the curing agent component in a mass ratio of 10:
1. The main component is composed of the following raw materials by mass percentage: (A) 25% to 50% wt methacrylate monomer; (B) 1% to 10% wt epoxy resin; (C) 35% to 55% wt polyurethane modified acrylate; (D) 5% to 15% Wt toughening agent; (E) 0.1%~2%Wt fully refined paraffin; (F) 5% to 10% Wt filler; (G) 0.01%~5%Wt stabilizer; (H) 0.1%~2%Wt accelerator; (I) 1% to 10% wt adhesion promoter; (J) 1% to 5% Wt coupling agent; Wherein, the methacrylate monomer is one of hydroxyethyl methacrylate, hydroxypropyl methacrylate, lauryl methacrylate, isobornyl methacrylate, 2-phenoxyethyl methacrylate, tetrahydrofuran methacrylate, ethoxylated bisphenol A dimethacrylate, trimethylolpropane trimethacrylate or a mixture thereof, and the polyurethane modified acrylate is a polyurethane acrylate obtained by polymerization of hydrogenated bisphenol A, polyethylene glycol and isocyanate and capped with a methacrylate monomer; The curing agent component is composed of the following raw materials by mass percentage: (A) 30% to 60% Wt plasticizer; (B) 5% to 15% Wt toughening agent; (C) 0.1% to 2% Wt pigment; (D) 15% to 30% wt oxidant; (E) 5% to 10% Wt filler; The fillers in the main agent component and the curing agent component are calcium carbonate, silicon micropowder, hollow glass microspheres, polyethylene powder or a mixture thereof.
2. The high-peeling acrylic adhesive for train sets according to claim 1, Features: The epoxy resin is one of 828EL epoxy resin and 128E epoxy resin or a mixture thereof.
3. The high-peeling acrylic adhesive for EMU according to claim 1, Features: The toughening agent is MBS, ABS high rubber powder or a mixture thereof.
4. The high-peeling acrylic adhesive for train sets according to claim 1, Features: The fully refined paraffin wax is one of WAX-120, WAX-145, WAX-156 or a mixture thereof.
5. The high-peeling acrylic adhesive for train sets according to claim 1, Features: The stabilizer is one of phenolic compounds, quinone compounds, oxalic acid, sodium salt, phenothiazine or a mixture thereof.
6. The high-peeling acrylic adhesive for train sets according to claim 1, Features: The accelerator is one of N,N-dimethyl-p-toluidine, N,N-diethyl-p-toluidine, N,N-diethyl-m-toluidine, N,N-dihydroxyethyl-p-methylaniline and zinc dimethacrylate or a mixture thereof.
7. The high-peeling acrylic adhesive for train sets according to claim 1, Features: The coupling agent is a silane coupling agent or a mixture thereof, and the oxidizing agent is benzoyl peroxide.
8. The high-peeling acrylic adhesive for train sets according to claim 1, Features: The plasticizer is one of DOP, DIDP, DEHP or a mixture thereof.
9. The high-peeling acrylic adhesive for train sets according to claim 1, Features: The pigment is iron blue, milori blue or a mixture thereof.
10. A method for preparing the high-peeling acrylic adhesive for EMUs as claimed in any one of claims 1 to 9, Features: The following steps are involved: (1) Preparation of polyurethane modified acrylate: IBOMA and isocyanate are added into a reaction bottle, the temperature in the reaction bottle is raised to 80-90°C, and stirred for 30-60 minutes; hydrogenated bisphenol A is then added into the reaction bottle and the temperature in the reaction bottle is controlled at 80-90°C, and stirred for 120-150 minutes; then PTMG is added into the reaction bottle and the temperature is controlled at 75-85°C, and stirred for 120-150 minutes; finally, monofunctional methacrylate monomer is added into the reaction bottle and the temperature is controlled at 70-80°C, and stirred for 120-150 minutes to obtain polyurethane modified acrylate; (2) Main agent component: put methacrylate monomer, epoxy resin and fully refined paraffin into a reaction kettle, heat to 70°C-75°C, add polyurethane modified acrylate and toughening agent, stir until completely dissolved, stop heating, add filler, stir until completely dissolved, add stabilizer, stir evenly, cool to below 30°C, add accelerator, adhesion promoter and coupling agent, stir evenly to obtain the main agent component; (3) Curing agent component: put the plasticizer and oxidant into the reaction kettle, add the toughening agent, stir until completely dissolved, add the pigment and filler, stir evenly, control the material temperature below 30°C during the stirring process, and vacuum degassing to obtain the curing agent component; (4) The main agent component prepared in step (2) and the curing agent component prepared in step (3) are mixed evenly in a mass ratio of 10:1 to obtain a high-peeling acrylic adhesive for EMUs.
Citation Information
Patent Citations
High peel strength acrylate adhesive
CN103834307A
High-elongation two-component acrylic ester binding agent and preparation method thereof
CN105419658A
Two-component acrylate adhesive
CN110205081A
Ultraviolet cured structure adhesive membrane and preparation method thereof
CN110396390A
Low-odor acrylate adhesive for bonding metal materials and preparation process of low-odor acrylate adhesive
CN115627136A