Profile surface coating device and process for aluminum alloy door frame

By using auxiliary components in the aluminum alloy door frame profile surface coating device to realize the circulating flow and separation of the electroplating liquid, the problem of poor fluidity of the electroplating liquid is solved, and the corrosion resistance and welding effect are improved.

CN118835302AInactive Publication Date: 2024-10-25CHENGDU JINZHIBANG METAL DOOR & WINDOW CO LTD

Patent Information

Application Number
CN202411330980.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-24
Publication Date
2024-10-25
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

During the profile electroplating process of aluminum alloy door frames, due to the existence of internal chambers in the profiles, the fluidity of the plating solution is poor, resulting in a low coating thickness, affecting the corrosion resistance effect, and the components of the plating solution cannot be quickly replenished, affecting the overall performance.

Method used

A profile surface coating device for aluminum alloy door frames is designed. Through auxiliary components such as a moving trolley and a pump body, the circulating flow of the electroplating liquid in the profile cavity is realized to ensure the consistency of the electroplating liquid components. The liquid dispensing assembly and the rotating assembly are used to After the coating is completed, separate the plating solution to prevent residues from affecting the welding effect.

Benefits of technology

It improves the fluidity of the electroplating solution in the profile cavity, ensuring corrosion resistance and welding effect. It also avoids the residue of the electroplating solution on the profile, ensuring the quality of subsequent welding.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118835302A_ABST
    Figure CN118835302A_ABST
Patent Text Reader

Abstract

The invention discloses a profile surface coating device and process for an aluminum alloy door frame, and relates to the technical field of coating. Comprising a frame, an electroplating pool used for electroplating profiles is installed at the bottom end in the frame, a guide rail used for assisting in moving the profiles is fixedly connected to the top end of the frame, and a moving assembly used for moving is slidably connected to the top end of the guide rail. Through the arrangement of the auxiliary assembly, when a profile is subjected to film plating, the movable trolley can pass through an inner cavity of the profile or reach the innermost position of the inner cavity, in the electroplating process, materials are supplied to the inner cavity of the profile through the pump body, the fluidity of electroplating liquid in the cavity is improved, and meanwhile the pump body is started, so that the electroplating efficiency is improved. The circulation of the electroplating liquid inside the cavity and the electroplating liquid outside the profile is realized, the consistency between the electroplating components of the electroplating liquid inside the cavity and the electroplating components of the electroplating liquid outside the cavity is ensured, and meanwhile, the circulation flow of the electroplating liquid inside the cavity is ensured, so that the overall corrosion resistance of the profile is ensured.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of coating technology, in particular to a surface coating device and process for a profile used in an aluminum alloy door frame. Background Art

[0002] Aluminum alloy door frames have been widely used in the field of building doors and windows due to their lightness, corrosion resistance, and beautiful appearance. Electroplating is a surface coating process for aluminum alloy door frame profiles. Electroplating forms a layer of metal coating on the surface of the profile, which not only enhances the corrosion resistance of the aluminum alloy door frame, but also improves its decorativeness.

[0003] For example, the patent publication number is "CN112981295A", and the name is "A surface coating device for aluminum alloy products", which includes a base plate, the upper end of which is fixedly connected to a coating pool, a push plate is slidably connected to the coating pool, and a driving mechanism for driving the push plate is provided on the coating pool. This invention can automatically clean the oxide layer on the surface of the coating pool, has a good galvanizing effect on the aluminum alloy pipe and will not change the inner diameter of the aluminum alloy pipe.

[0004] When electroplating the profile in the above invention, it is necessary to connect the profile and the cathode of the power supply so that the plating material in the plating solution is deposited on the surface of the profile. Since the profile and the power supply are connected, the profile is immersed in the plating solution, so that a plating layer is also formed inside the cavity inside the profile. However, due to the existence of the internal cavity of the profile, the flow effect of the plating liquid in the inner cavity of the profile is low. The plating material in the plating liquid will be consumed during the electroplating process, resulting in the gradual decrease of the internal components of the plating liquid. However, due to the poor fluidity of the plating liquid, the components of the plating liquid inside the cavity cannot be quickly replenished, resulting in a low thickness of the plating layer formed in the inner cavity of the profile, which directly affects the overall corrosion resistance of the profile. For this purpose, a profile surface coating device and process for aluminum alloy door frames are invented. Summary of the Invention

[0005] The purpose of the present invention is to provide a surface coating device and process for aluminum alloy door frame profiles to solve the problems raised in the above background technology.

[0006] To achieve the above objectives, the present invention provides the following technical solutions: a surface coating device for an aluminum alloy door frame profile, comprising a frame, a plating tank for plating the profile installed at the bottom end of the frame, a guide rail for assisting in moving the profile fixedly connected to the top end of the frame, a moving assembly for movement slidably connected to the top end of the guide rail, a clamping assembly for clamping the profile installed at the moving end of the moving assembly, and an auxiliary assembly for assisting in electroplating the inner cavity of the profile installed on one side of the clamping assembly;

[0007] The cam is secured to the chassis and has a pivotal connection to the chassis, and the pivotal connection to the chassis has a latching mechanism that engages the chassis and engages the chassis to engage the chassis.

[0008] Furthermore, a detection device for detecting whether the fixing component is clamping the moving trolley is installed inside the fixing component, and the telescopic control component includes a limiting ring, which is fixedly installed on the outer wall of the telescopic tube, and one end of the movable frame is rotatably connected to a limiting gear for contacting the limiting ring, and a stepping motor for controlling the rotation of the limiting gear is fixedly connected inside the movable frame.

[0009] Furthermore, the fixing assembly includes a No. 2 telescopic part, which is fixedly mounted on one side of the mobile frame. A No. 2 clamp is installed on the telescopic end of the No. 2 telescopic part. The outside of the mobile trolley is fixedly connected to a No. 1 telescopic part for squeezing the inner cavity of the profile. One side of the mobile frame is fixedly connected to a No. 1 clamp for clamping the profile.

[0010] Furthermore, the recycling component includes a No. 1 motor, which is fixedly mounted on the mobile frame. The telescopic end of the No. 1 motor is fixedly connected to a winding drum. A connecting rope is wrapped around the outside of the winding drum. One end of the connecting rope passes through the telescopic tube and is fixed to one end of the mobile trolley.

[0011] Furthermore, the moving assembly includes a moving frame, the inner wall of the moving frame is slidably connected to the outer wall of the guide rail, a motor drive device is installed inside the moving frame for realizing the movement of the moving frame on the guide rail, a lifting device is installed on the top of the moving frame, the moving end of the lifting device is fixedly connected to the moving body, a telescopic rod that can be extended and retracted is fixedly connected between the top of the moving body and the bottom end of the moving frame, the inner wall of the moving body and the outer wall of the moving frame are rotatably connected, and a liquid separation component is fixedly connected to the top of the frame for realizing phase separation of the plating liquid and the profile after the coating is completed.

[0012] Furthermore, a rotating assembly is installed on one side of the mobile frame, and the rotating assembly includes a No. 3 motor, which is fixedly mounted on the mobile frame. A No. 3 telescopic part is fixedly connected to the mobile frame, and the telescopic end of the No. 3 telescopic part is rotatably connected to a transmission shaft, and the inner wall of the transmission shaft and the outer wall of the output end of the No. 3 motor are slidably connected.

[0013] Furthermore, the liquid separation component includes a semi-ring cover, both ends of the semi-ring cover are rotatably connected to both ends inside the frame, one side of the semi-ring cover is rotatably connected to connecting rod No. 1, and one end of connecting rod No. 1 is rotatably connected to one side of the movable frame.

[0014] A surface coating process for an aluminum alloy door frame profile adopts the above-mentioned surface coating device for an aluminum alloy door frame profile. The coating process includes:

[0015] Pretreatment: Clean the surface of the profile, and then activate the surface of the profile after pretreatment;

[0016] One-time water washing: Use deionized water to clean the profile;

[0017] Electroplating: Electroplating includes surface electroplating and internal electroplating. The fixture holds the profile, and the moving component immerses the profile in the plating solution in the plating tank. The auxiliary component controls the flow of the plating solution in the profile cavity and realizes the circulation flow between the plating solution in the profile cavity and the plating solution outside the profile to achieve electroplating.

[0018] Centrifugal separation: remove the profile from the electroplating solution, control the rotation of the profile, and perform centrifugal motion on the profile to achieve rapid separation of the profile and the electroplating solution;

[0019] Secondary water washing: move the profile to the cleaning tank and wash the profile through the cleaning tank.

[0020] Furthermore, the cleaning treatment includes degreasing and deoxidation, the deoxidation includes cleaning the profile surface with a sodium hydroxide solution, the secondary water washing includes cleaning the profile with an ultrasonic method, and during the electroplating process, a flow meter is used to respectively detect the flow rate of the electroplating liquid on the outer surface of the profile and the flow rate of the electric fluid in the inner cavity of the profile, adjust the power of the pump body, and control the flow rate of the electric fluid in the inner cavity of the profile. The difference between the flow rate of the electric fluid in the inner cavity of the profile and the flow rate of the electroplating liquid on the outer surface of the profile does not exceed five percent of the flow rate of the electroplating liquid on the outer surface of the profile.

[0021] Compared with the prior art, the present invention has the following beneficial effects:

[0022] The surface coating device and process for the profile for aluminum alloy door frames, through the arrangement of auxiliary components, enables a mobile carriage to pass through the inner cavity of the profile or reach the innermost part of the inner cavity when the profile is coated. During the electroplating process, the inner cavity of the profile is supplied by a pump body, thereby improving the fluidity of the electroplating solution inside the chamber. Simultaneously, the start-up of the pump body enables the electroplating solution inside the chamber and the electroplating solution outside the profile to circulate, thereby ensuring the consistency between the electroplating components of the electroplating solution inside the chamber and the electroplating components of the external electroplating solution, and simultaneously enabling the circulation of the electroplating solution inside the chamber, thereby ensuring the overall corrosion resistance of the profile.

[0023] At the same time, through the setting of the liquid separation component and the rotating component, after the electroplating is completed, the lifting device lifts the profile, and then the rotating component contacts the movable frame and causes the movable frame and its profile to rotate. The rotation of the profile can move the remaining electroplating liquid on the profile to the semi-ring cover and the electroplating tank, thereby avoiding the electroplating liquid losing water on the profile and causing residual electroplating material on the profile. The presence of electroplating material will affect the subsequent welding between aluminum alloy door frames, thereby ensuring the subsequent aluminum alloy door frame welding effect.

[0024] Through the setting of the telescopic control component, the telescopic control component will control the telescopic tube's telescopic extension and contraction to prevent the telescopic tube from moving too far out of the mobile frame and causing a bending effect, which in turn affects the discharge effect of the through hole on the telescopic tube. The telescopic tube is exerted with force by the movement of the mobile trolley, and the rotation speed of the gear is limited by the stepper motor control. After the detection device detects that the No. 2 clamp is in contact with the mobile trolley, the stepper motor stops running. At this time, the telescopic tube can be in the best telescopic position, so that the through hole on the telescopic tube can discharge smoothly, ensuring the feasibility of the auxiliary component. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] Figure 1 is an isometric view of the present invention;

[0026] Figure 2 It is a partial cross-sectional view of the present invention;

[0027] Figure 3 is an isometric view of the mobile assembly of the present invention;

[0028] Figure 4 is an isometric view of the rotating assembly of the present invention;

[0029] Figure 5 is an isometric view of the clamping assembly of the present invention;

[0030] Figure 6 is an isometric view of the liquid dispensing assembly of the present invention;

[0031] Figure 7 is an isometric view of the auxiliary components of the present invention;

[0032] Figure 8is a cross-sectional view of the auxiliary component of the present invention;

[0033] Figure 9 is an internal cross-sectional view of the mobile frame of the present invention;

[0034] Figure 10 Flow chart of the process of the present invention.

[0035] In the figure: 1. Frame; 2. Electroplating pool; 3. Clamping assembly; 301. Moving frame; 302. Clamp No. 1; 303. Telescopic part No. 2; 304. Clamp No. 2; 4. Auxiliary assembly; 401. Telescopic tube; 402. Moving trolley; 403. Telescopic part No. 1; 404. Limiting ring; 405. Limiting gear; 406. Stepping motor; 407. Pump body; 5. Recovery assembly; 501. Winding drum; 502. Connecting rope; 6. Moving assembly; 601. Moving frame; 602. Lifting device; 603. Moving body; 604. Telescopic rod; 7. Rotating assembly; 701. Motor No. 3; 702. Telescopic part No. 3; 703. Drive shaft; 8. Liquid separation assembly; 801. Half ring cover; 802. Connecting rod No. 1. DETAILED DESCRIPTION

[0036] The following will clearly and completely describe the technical solutions in the embodiments of the present invention in conjunction with the accompanying drawings. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. All other embodiments obtained by ordinary technicians in this field based on the embodiments of the present invention without making any creative efforts shall fall within the scope of protection of the present invention.

[0037] like Figure 1 - Figure 10 As shown, the present invention provides a technical solution: a surface coating device for an aluminum alloy door frame profile, comprising a frame 1, a plating tank 2 for plating the profile installed at the bottom end of the frame 1, a guide rail for assisting in moving the profile fixedly connected to the top end of the frame 1, a moving assembly 6 for movement slidably connected to the top end of the guide rail, a clamping assembly 3 for clamping the profile installed at the moving end of the moving assembly 6, and an auxiliary assembly 4 for assisting in electroplating the inner cavity of the profile installed on one side of the clamping assembly 3;

[0038] The clamping assembly 3 includes a mobile frame 301, the outer wall of the mobile frame 301 is rotatably connected to the mobile end of the mobile assembly 6, the auxiliary assembly 4 includes a telescopic tube 401, one end of the telescopic tube 401 is fixed to one side of the mobile frame 301, a telescopic control assembly for limiting the telescopic extension of the telescopic tube 401 is installed between the mobile frame 301 and the telescopic tube 401, one end of the telescopic tube 401 is fixedly connected to a mobile trolley 402 for entering the inner cavity of the profile, and a fixing assembly for clamping and fixing the position of the mobile trolley 402 is installed on one side of the mobile frame 301. The interior of the movable frame 301 is fixedly connected to a pump body 407 for supplying material to the interior of the telescopic tube 401. The feed end of the pump body 407 penetrates the inner wall of the movable frame 301 to realize communication between the internal chamber of the pump body 407 and the outside world. A recovery component 5 for controlling the mobile carriage 402 to leave the inner cavity of the profile is installed between the movable carriage 402 and the movable frame 301. The interior of the movable carriage 402 is fixedly connected to a connecting hole, and the outer wall of the telescopic tube 401 is provided with a through hole for moving the electroplating liquid inside the telescopic tube 401 to the area between the telescopic tube 401 and the inner cavity of the profile.

[0039] A detection device for detecting whether the fixed component is clamping the mobile cart 402 is installed inside the fixed component. The telescopic control component includes a limiting ring 404, which is fixedly installed on the outer wall of the telescopic tube 401. One end of the mobile frame 301 is rotatably connected to a limiting gear 405 for contacting the limiting ring 404. The inside of the mobile frame 301 is fixedly connected to a stepping motor 406 for controlling the rotation of the limiting gear 405.

[0040] The fixed component includes a No. 2 telescopic part 303, which is fixedly installed on one side of the mobile frame 301. The telescopic end of the No. 2 telescopic part 303 is installed with a No. 2 clamp 304. The outside of the mobile trolley 402 is fixedly connected to the No. 1 telescopic part 403 for squeezing the inner cavity of the profile, and one side of the mobile frame 301 is fixedly connected to the No. 1 clamp 302 for clamping the profile.

[0041] The recycling component 5 includes motor No. 1, which is fixedly mounted on the mobile frame 301. The telescopic end of motor No. 1 is fixedly connected to the winding drum 501. A connecting rope 502 is wrapped around the outside of the winding drum 501. One end of the connecting rope 502 passes through the telescopic tube 401 and is fixed to one end of the mobile trolley 402.

[0042] The moving component 6 includes a moving frame 601, the inner wall of the moving frame 601 is slidably connected to the outer wall of the guide rail, and a motor drive device for realizing the movement of the moving frame 601 on the guide rail is installed inside the moving frame 601. A lifting device 602 is installed on the top of the moving frame 601, and the moving end of the lifting device 602 is fixedly connected to the moving body 603. The top of the moving body 603 is fixedly connected to the telescopic rod 604, and the top of the telescopic rod 604 is fixed to the bottom end of the moving frame 601. The inner wall of the moving body 603 is rotatably connected to the outer wall of the moving frame 301, and the top of the frame 1 is fixedly connected to a liquid separation component 8 for realizing the separation of the plating solution and the profile after the coating is completed.

[0043] A rotating assembly 7 is installed on one side of the mobile frame 601, and the rotating assembly 7 includes a No. 3 motor 701. The No. 3 motor 701 is fixedly installed on the mobile frame 601. The No. 3 telescopic member 702 is fixedly connected to the mobile frame 601. The telescopic end of the No. 3 telescopic member 702 is rotatably connected to the transmission shaft 703, and the inner wall of the transmission shaft 703 and the outer wall of the output end of the No. 3 motor 701 are slidably connected.

[0044] The liquid separation component 8 includes a semi-ring cover 801, both ends of the semi-ring cover 801 are rotatably connected to both ends inside the frame 1, one side of the semi-ring cover 801 is rotatably connected to a connecting rod No. 1 802, and one end of the connecting rod No. 1 is rotatably connected to one side of the movable frame 601.

[0045] A surface coating process for aluminum alloy door frame profiles, using the above-mentioned surface coating device for aluminum alloy door frame profiles, the coating process includes:

[0046] Pretreatment: Clean the surface of the profile, and then activate the surface of the profile after pretreatment;

[0047] One-time water washing: Use deionized water to clean the profile;

[0048] Electroplating: Electroplating includes surface plating and internal plating. The first fixture 302 clamps the profile, and the moving component 6 immerses the profile in the plating solution in the plating tank 2. The auxiliary component 4 controls the flow rate of the plating solution in the profile cavity and realizes the circulation flow between the plating solution in the profile cavity and the plating solution outside the profile to achieve electroplating.

[0049] Centrifugal separation: The profile is removed from the electroplating solution, and the rotating assembly 7 controls the rotation of the profile to perform centrifugal motion on the profile, and the electroplating solution on the profile is moved to the electroplating tank 2 and the semi-ring cover 801;

[0050] Secondary water washing: move the profile to the cleaning tank and wash the profile through the cleaning tank.

[0051] The cleaning process includes degreasing and deoxidation. Deoxidation includes cleaning the profile surface with sodium hydroxide solution. The secondary water washing includes cleaning the profile with ultrasonic wave. During the electroplating process, a flow meter is used to detect the flow rate of the electroplating liquid on the outer surface of the profile and the flow rate of the electric fluid in the inner cavity of the profile, respectively. The power of the pump body 407 is adjusted to control the flow rate of the electric fluid in the inner cavity of the profile. The difference between the flow rate of the electric fluid in the inner cavity of the profile and the flow rate of the electroplating liquid on the outer surface of the profile does not exceed five percent of the flow rate of the electroplating liquid on the outer surface of the profile.

[0052] The present application is to electroplate the profiles before they are combined into aluminum alloy door frames. After the electroplating is completed, the various profiles are combined into aluminum alloy door frames. The electroplating solution includes but is not limited to cyanide zinc plating and zincate zinc plating, which are used according to the actual manufacturer's choice. The electroplating tank 2 is equipped with a stirring device for stirring the electroplating solution and a replenishing device for replenishing the electroplating material in the electroplating tank 2. Both the stirring device and the replenishing device exist in the existing technology. During the electroplating process, the stirring device stirs the electroplating solution to ensure that the electroplating solution in the electroplating tank 2 and on the outer wall of the profile flows. However, the fluidity of the electroplating solution inside the chamber is poor due to the presence of the profile. At this time, the auxiliary component 4 can increase the flow of the electroplating solution in the chamber inside the profile, so as to ensure the uniformity of the coating inside the profile. Through the auxiliary component Due to the arrangement of component 4, when the profile is coated, the mobile trolley 402 can pass through the inner cavity of the profile or reach the innermost part of the inner cavity. During the electroplating process, the inner cavity of the profile is supplied with material through the pump body 407, thereby improving the fluidity of the electroplating liquid inside the chamber. At the same time, the start-up of the pump body 407 enables the electroplating liquid inside the chamber and the electroplating liquid outside the profile to circulate, thereby ensuring the consistency between the electroplating components of the electroplating liquid inside the chamber and the electroplating components of the external electroplating liquid. At the same time, the circulation of the electroplating liquid inside the chamber ensures the overall corrosion resistance of the profile. There is a significant difference between the existence of the auxiliary component 4 and directly supplying material to the chamber through the pump body 407. The supply of material to the chamber by the pump body 407 will cause the inner coating of the chamber to be thicker the closer it is to the pump body 407, thereby directly leading to uneven coating.

[0053] The detection device detects whether the fixed component is clamping the mobile trolley 402. After the fixed component has clamped the mobile trolley 402, the mobile trolley 402 will no longer move. Both the No. 1 clamp 302 and the No. 2 clamp 304 have existing devices, which can clamp the profile. The No. 1 clamp 302 and the No. 2 clamp 304 can be controlled electrically and hydraulically. The No. 1 clamp 302 clamps the profile. At the same time, the contact position between the No. 1 clamp 302 and the profile is made of non-conductive material. A feeding pipe is installed on the mobile frame 301. The feeding pipe is fixed to the discharge end of the pump body 407. The pump body 407 is started. , the material is fed into the telescopic tube 401 through the feeding pipe, and the electroplating liquid inside the telescopic tube 401 comes into contact with the cavity inside the profile through the through hole, and the electroplating liquid between the outer wall of the telescopic tube 401 and the inside of the profile is moved out of the cavity due to the subsequent squeezing of the electroplating liquid, thereby completing the circulation of the electroplating liquid in the cavity opened on the inner wall, ensuring the uniformity of the electric layer inside the profile, and then ensuring the overall corrosion resistance of the profile. The No. 1 clamp 302 clamps the profile, and the No. 2 clamp 304 clamps the mobile trolley 402. Then the telescopic end of the No. 2 telescopic part 303 contracts, so that the mobile trolley 402 can contact with the feeding pipe.

[0054] like Figure 9 As shown, the feed pipe and the discharge end of the pump body 407 in the movable rack 301 are not fixed to each other. Since the recovery component 5 needs to be installed, a sealed space is formed inside the movable rack 301. The pump body 407 feeds material into the interior to increase the pressure of the electroplating liquid inside the sealed space, thereby moving the electroplating liquid inside the sealed space into the telescopic tube 401 and reaching the interior of the chamber through the through hole on the telescopic tube 401.

[0055] For the open chambers inside the profile, the open chambers include one type of interconnected chambers and one type of chamber with only one opening inside. At the same time, for the interconnected chambers, there are chambers with two open pipes at right angles, which are regarded as chambers with only one opening. As for the closed chambers inside the profile, the electroplating liquid cannot enter, and naturally electroplating cannot be carried out. For the interconnected chambers, a wheel device can be installed on the mobile trolley 402, which contacts the chamber inside the profile through the wheel device and rotates the wheel to move the mobile trolley 402, and the mobile trolley 402 contacts the second clamp 304, and the detection device When the device detects that the moving trolley 402 and the No. 2 clamp 304 are in contact, the No. 2 clamp 304 clamps the moving trolley 402, and the telescopic end of the No. 2 telescopic part 303 contracts, so that the moving trolley 402 can contact the feeding tube. For the chamber with only one opening, the moving trolley 402 moves. When the moving trolley 402 moves to the innermost part of the chamber, the telescopic end of the No. 1 telescopic part 403 moves and applies force to the inner wall of the profile. The position of the moving trolley 402 on the profile is fixed by the reaction force, and the part of the telescopic end of the No. 1 telescopic part 403 that is used to contact the inner wall of the profile is provided with anti-conductive material.

[0056] The movement of the mobile carriage 402 causes the telescopic tube 401 to extend, exerting force on the restriction ring 404 to generate a moving tendency. Under the action of the restriction gear 405, the restriction ring 404 cannot move. The output top of the stepper motor 406 rotates, and the restriction gear 405 rotates. At this time, the restriction ring 404 in contact with the restriction gear 405 can move due to the rotation of the restriction gear 405. The next restriction ring 404 will be restricted by the restriction gear 405 again. Through the setting of the telescopic control component, the telescopic control component will control the extension and retraction of the telescopic tube 401 , to avoid the telescopic tube 401 from moving too much out of the mobile frame 301 and causing a bending effect, which in turn affects the discharge effect of the through hole on the telescopic tube 401, the mobile trolley 402 moves to apply force to the telescopic tube 401, and the stepper motor 406 controls the rotation speed of the limiting gear 405. After the detection device detects that the second clamp 304 and the mobile trolley 402 are in contact, the stepper motor 406 stops running. At this time, the telescopic tube 401 can be in the best telescopic position, so that the through hole on the telescopic tube 401 can discharge smoothly, ensuring the feasibility of the auxiliary component 4.

[0057] After the electroplating is completed, the telescopic end of the No. 2 telescopic part 303 is extended, the No. 2 clamp 304 removes the restriction on the moving trolley 402, and the winding drum 501 rotates, causing the connecting rope 502 to move. The connecting rope 502 applies force to the moving trolley 402, causing the telescopic tube 401 to expand and contract, and the distance between the limiting rings 404 becomes closer, thereby causing the limiting rings 404 to gradually move to the inside of the moving frame 301. At this time, the output end of the stepper motor 406 and the limiting gear 405 rotate in opposite directions, so that the limiting ring 404 can smoothly enter the inside of the moving frame 301.

[0058] There is an existing device for the lifting device 602. The lifting device 602 causes the movable body 603 and the telescopic rod 604 to retract, so that the movable frame 301 moves to the set position. At this position, the telescopic end of the No. 3 telescopic member 702 and the transmission shaft 703 move. A transmission groove for transmission is opened on one side of the movable frame 301. The transmission shaft 703 moves and contacts the inner wall of the transmission groove. The output end of the No. 3 motor 701 and the transmission shaft 703 rotate, thereby causing the movable frame 301, the auxiliary component 4 and the profile to rotate, thereby centrifugally throwing out the electroplating liquid on the profile. Due to the design of the semi-ring cover 801, the thrown-out electroplating liquid will fall on the semi-ring cover 801 and the electroplating pool 2.

[0059] There is prior art for the motor drive device, which can realize the movement of the movable frame 601 on the guide rail. The movement of the movable frame 601 causes the No. 1 connecting rod 802 to move and rotate. Due to the setting of its connecting rod, the semi-ring cover 801 is rotated by the movement of the movable frame 601. One side of the semi-ring cover 801 is designed with an opening, so that the profile can be moved to the interior of the semi-ring cover 801 through the opening of the semi-ring cover 801. When the profile moves to the middle area of ​​the semi-ring cover 801, the opening of the semi-ring cover 801 will face the electroplating pool 2. After the electroplating is completed, the lifting device 602 will retract the profile, and the motor drive device causes the movable frame 601 to move in the opposite direction, and the No. 1 connecting rod 802 rotates and moves, thereby causing the semi-ring cover 801 and its opening position to rotate, so that the profile can rotate from the opening position of the semi-ring cover 801, and the electroplating liquid on the profile will be thrown to the inner wall position of the semi-ring cover 801, and the electroplating liquid will fall into the electrolytic pool through the opening of the semi-ring cover 801. In the pool, since the semi-ring cover 801 is at the top position of the electrolytic cell, the liquid on the semi-ring cover 801 will only fall into the electrolytic cell under the action of gravity. After the electroplating is completed, the profile is rotated by the rotating component 7 to throw out the electroplating liquid adhering to the profile, so as to avoid the electroplating liquid losing water on the profile and causing residual electroplating material on the profile. The presence of electroplating material will affect the subsequent welding between aluminum alloy door frames. Through the arrangement of the liquid separation component 8 and the rotating component 7, after the electroplating is completed, the lifting device 602 lifts the profile, and then the rotating component 7 contacts the movable frame 301 and causes the movable frame 301 and its profile to rotate. The rotation of the profile can move the residual electroplating liquid on the profile to the semi-ring cover 801 and the electroplating pool 2, so as to avoid the electroplating liquid losing water on the profile and causing residual electroplating material on the profile. The presence of electroplating material will affect the subsequent welding between aluminum alloy door frames, thereby ensuring the subsequent aluminum alloy door frame welding effect.

[0060] Through activation treatment, tiny bumps are produced on the surface of the aluminum material to enhance the adhesion of the coating. Degreasing includes using a degreasing agent or alkaline solution to thoroughly clean the aluminum alloy profile to remove grease and dirt on the surface. Deoxidation includes using sodium hydroxide solution to clean the profile surface to remove oxides on the aluminum alloy surface and reduce the oxides on the aluminum alloy surface. Sodium hydroxide will react chemically with the oxides to generate water-soluble compounds, and then the oxides will be completely removed from the profile surface by rinsing to remove the oxides on the profile surface to ensure the quality of subsequent electroplating.

[0061] Although embodiments of the present invention have been shown and described, it will be understood by those skilled in the art that various changes, modifications, substitutions and variations may be made to these embodiments without departing from the principles and spirit of the invention, and that the scope of the invention is limited by the accompanying embodiments and their equivalents.

Claims

1. A profile surface coating device for an aluminum alloy door frame, comprising a frame (1), Features: The bottom end of the frame (1) is provided with an electroplating pool (2) for electroplating the profile, the top end of the frame (1) is fixedly connected with a guide rail for assisting in moving the profile, the top end of the guide rail is slidably connected with a moving component (6) for movement, the moving end of the moving component (6) is provided with a clamping component (3) for clamping the profile, and one side of the clamping component (3) is provided with an auxiliary component (4) for assisting in electroplating the inner cavity of the profile; The clamping assembly (3) comprises a moving frame (301), the outer wall of the moving frame (301) is rotatably connected to the moving end of the moving assembly (6), the auxiliary assembly (4) comprises a telescopic tube (401), one end of the telescopic tube (401) is fixed to one side of the moving frame (301), a telescopic control assembly for limiting the telescopic extension of the telescopic tube (401) is installed between the moving frame (301) and the telescopic tube (401), one end of the telescopic tube (401) is fixedly connected to a moving trolley (402) for entering the inner cavity of the profile, and one side of the moving frame (301) is installed with a fixing assembly for clamping and fixing the position of the moving trolley (402). The interior of the movable frame (301) is fixedly connected to a pump body (407) for supplying material to the interior of the telescopic tube (401); the feed end of the pump body (407) penetrates the inner wall of the movable frame (301) to achieve communication between the internal chamber of the pump body (407) and the outside; a recovery component (5) for controlling the movable frame (402) to leave the inner cavity of the profile is installed between the movable trolley (402) and the movable frame (301); the interior of the movable trolley (402) is fixedly connected to a connecting hole; and the outer wall of the telescopic tube (401) is provided with a through hole for moving the electroplating solution inside the telescopic tube (401) to the area between the telescopic tube (401) and the inner cavity of the profile.

2. A surface coating device for aluminum alloy door frame profile according to claim 1, Features: A detection device for detecting whether the fixing component is clamping the moving trolley (402) is installed inside the fixing component, and the telescopic control component comprises a limiting ring (404), the limiting ring (404) is fixedly installed on the outer wall of the telescopic tube (401), one end of the moving frame (301) is rotatably connected to a limiting gear (405) for contacting the limiting ring (404), and the inside of the moving frame (301) is fixedly connected to a stepping motor (406) for controlling the rotation of the limiting gear (405).

3. The surface coating device for aluminum alloy door frame profile according to claim 1, Features: The fixing assembly comprises a No. 2 telescopic member (303), the No. 2 telescopic member (303) being fixedly mounted on one side of the moving frame (301), a No. 2 clamp (304) being mounted on the telescopic end of the No. 2 telescopic member (303), a No. 1 telescopic member (403) for squeezing the inner cavity of the profile being fixedly connected to the outside of the moving trolley (402), and a No. 1 clamp (302) for clamping the profile being fixedly connected to one side of the moving frame (301).

4. The surface coating device for aluminum alloy door frame profile according to claim 1, Features: The recycling assembly (5) comprises a No. 1 motor, which is fixedly mounted on the moving frame (301); the telescopic end of the No. 1 motor is fixedly connected to a winding drum (501); a connecting rope (502) is wound around the outside of the winding drum (501); one end of the connecting rope (502) passes through the telescopic tube (401) and is fixed to one end of the moving trolley (402).

5. The surface coating device for aluminum alloy door frame profile according to claim 1, Features: The moving assembly (6) comprises a moving frame (601), the inner wall of the moving frame (601) and the outer wall of the guide rail being slidably connected, a motor drive device for realizing movement of the moving frame (601) on the guide rail being installed inside the moving frame (601), a lifting device (602) being installed at the top of the moving frame (601), a moving body (603) being fixedly connected to the moving end of the lifting device (602), a telescopic rod (604) being fixedly connected between the top of the moving body (603) and the bottom of the moving frame (601) to realize telescopic movement, the inner wall of the moving body (603) and the outer wall of the moving frame (301) being rotatably connected, and a liquid separation assembly (8) for realizing phase separation of electroplating liquid and profile after coating is completed being fixedly connected to the top of the frame (1).

6. The surface coating device for aluminum alloy door frame profile according to claim 5, Features: A rotating assembly (7) is installed on one side of the moving frame (601), and the rotating assembly (7) comprises a No. 3 motor (701). The No. 3 motor (701) is fixedly installed on the moving frame (601), and a No. 3 telescopic member (702) is fixedly connected to the moving frame (601). The telescopic end of the No. 3 telescopic member (702) is rotatably connected to a transmission shaft (703), and the inner wall of the transmission shaft (703) is slidably connected to the outer wall of the output end of the No. 3 motor (701).

7. The surface coating device for aluminum alloy door frame profile according to claim 5, Features: The liquid separation assembly (8) comprises a semi-ring cover (801), two ends of the semi-ring cover (801) being rotatably connected to two ends inside the frame (1), one side of the semi-ring cover (801) being rotatably connected to a No. 1 connecting rod (802), and one end of the No. 1 connecting rod (802) being rotatably connected to one side of the moving frame (601).

8. A process for coating the surface of an aluminum alloy door frame profile, using the device for coating the surface of an aluminum alloy door frame profile according to any one of claims 1 to 7, It is characterized in that The coating process comprises: Pretreatment: Clean the profile surface, and then activate the profile surface after pretreatment; One-time water washing: Use deionized water to clean the profile; Electroplating: Electroplating includes surface electroplating and internal electroplating. The fixture clamps the profile, and the moving component (6) immerses the profile in the electroplating liquid in the electroplating tank (2). The auxiliary component (4) controls the flow of the electroplating liquid in the inner cavity of the profile and realizes the circulation flow between the electroplating liquid in the inner cavity of the profile and the electroplating liquid outside the profile, thereby realizing electroplating; Centrifugal separation: Take the profile out of the electroplating solution, control the rotation of the profile, and make centrifugal motion on the profile to achieve rapid separation of the profile and the electroplating solution; Secondary water washing: moving the profile to a cleaning tank and washing the profile through the cleaning tank.

9. The surface coating process for aluminum alloy door frame profile according to claim 8, Features: The cleaning treatment includes degreasing and oxide removal, the oxide removal includes cleaning the profile surface with a sodium hydroxide solution, the secondary water washing includes cleaning the profile with an ultrasonic method, and during the electroplating process, a flow meter is used to detect the flow rate of the electroplating liquid on the outer surface of the profile and the flow rate of the electric fluid in the inner cavity of the profile, respectively, and the power of the pump body (407) is adjusted to control the flow rate of the electric fluid in the inner cavity of the profile, and the difference between the flow rate of the electric fluid in the inner cavity of the profile and the flow rate of the electroplating liquid on the outer surface of the profile does not exceed 5% of the flow rate of the electroplating liquid on the outer surface of the profile.

Citation Information

Patent Citations

  • Surface coating device for aluminum alloy product

    CN112981295A

  • Forged aluminum alloy hub electroplating equipment and electroplating process

    CN115182026A

  • Special engineering plastic cavity coating film device

    CN207062398U

  • Film plating machine and electroplating production line

    US20240003039A1

  • Electroplating device for automobile plastic parts

    WO2024087141A1

Cited By

  • Construction method of double-sided local spraying electroplating model, electroplating system and electroplating method

    CN120654649A

  • A method for constructing a double-sided local jet electroplating model, an electroplating system and an electroplating method

    CN120654649B