Alkali metal doped and alkaline earth metal doped positive electrode materials and methods of making same
By doping alkali metals or alkaline earth metals in the positive electrode material of cyclic lithium-ion electrochemical cells, a layered structure of Li1.2-xAx[Mn0.8-x-y-zNiyMez]O2 is formed, which solves the problem of high-temperature problems in existing LMR materials. The problem of phase change under voltage improves electrochemical performance and capacity retention.
Patent Information
- Application Number
- CN202311387043.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-04-25
- Filing Date
- 2023-10-24
- Publication Date
- 2024-10-25
AI Technical Summary
Existing layered lithium- and manganese-rich oxide (LMR) positive electrode materials exhibit voltage fading, low Coulombic efficiency, and irreversible capacity loss during cyclic charging, mainly due to their irreversible phase transformation at high voltages. It leads to the formation of spinel structure and hinders the diffusion of lithium ions.
A doped layered lithium- and manganese-rich oxide material Li1.2-xAx[Mn0.8-x-y-zNiyMez]O2 was developed by calcining transition metal carbonates, dopant metals in an oxygen-containing environment The mixture of carbonate and lithium source forms a layered crystal structure with a transition metal layer, an oxygen layer and a lithium layer, and the presence of alkali metal or alkaline earth metal in the lithium layer inhibits the formation of the spinel phase.
The electrochemical performance, especially the capacity retention, is improved, and the layered structure and electrochemical performance characteristics are maintained by inhibiting the formation of spinel phase.
Smart Images

Figure CN118841528A_ABST
Abstract
Description
Technical Field
[0001] The present invention discloses a positive electrode material and a method for manufacturing the positive electrode material. Background Art
[0002] The information provided in this section is for the purpose of generally presenting the background of the present disclosure. The work of the presently named inventors (to the extent it is described in this section) and the various aspects of the description (which would not otherwise constitute prior art at the time of filing) are neither explicitly nor implicitly admitted to be prior art to the present disclosure.
[0003] The present disclosure relates to positive electrode materials for electrochemical cells that cycle lithium ions, and more particularly to positive electrode materials comprising lithium-rich and manganese-rich oxides doped with alkali metals and / or alkaline earth metals.
[0004] Layered lithium- and manganese-rich oxides (LMRs) are attractive candidates for positive electrode materials for cycling lithium-ion electrochemical cells due to their relatively high capacity (e.g., >250 mAh / g), thermal stability, and relatively low cost. However, LMRs have been found to exhibit voltage decay, low coulombic efficiency, and irreversible capacity loss after repeated charge and discharge cycles. One proposed mechanism for the observed performance degradation is that the LMR undergoes an irreversible phase transition from a layered structure to a spinel structure when a large amount of lithium is removed from the LMR during electrochemical charging. This layered to spinel phase transition has been found to be detrimental to the electrochemical performance of lithium batteries, which may be due to the relatively poor electrochemical properties of the spinel phase and because the presence of the spinel phase in the layered crystal structure of the LMR hinders the diffusion of lithium ions during cycling.
[0005] It would be desirable to develop layered lithium-rich and manganese-rich oxide materials with improved resistance to phase transformation during cycling, especially at high voltages. Summary of the invention
[0006] A positive electrode material for an electrochemical cell for circulating lithium ions is disclosed. The positive electrode material comprises an oxide represented by formula (1):
[0007] Li 1.2-x A x [Mn 0.8-x-y-z Ni y Me z ]O2, (1)
[0008] wherein A is an alkali metal, an alkaline earth metal or a combination thereof, Me is a transition metal, 0<x≤0.12, 0.1≤y≤0.5, and 0≤z≤0.2.
[0009] In some aspects, A can be a metal selected from sodium (Na), potassium (K), rubidium (Rb), cesium (Cs), magnesium (Mg), calcium (Ca), strontium (Sr), barium (Ba), and combinations thereof.
[0010] In some aspects, A can be a metal selected from rubidium (Rb), cesium (Cs), and combinations thereof.
[0011] In some aspects, Me can be a transition metal selected from cobalt (Co), aluminum (Al), and combinations thereof.
[0012] In some aspects, z=0, x is greater than or equal to about 0.001 and less than or equal to about 0.05, and y is greater than or equal to about 0.2 and less than or equal to about 0.3.
[0013] The oxide may have a layered crystal structure including a transition metal layer, an oxygen layer, and a lithium layer. In this case, A may exist at an octahedral site within the lithium layer.
[0014] A method for making a positive electrode material for an electrochemical cell for cycling lithium ions is disclosed. In the method, a mixture comprising a transition metal carbonate, a dopant metal carbonate and a lithium source is prepared and calcined to form an oxide represented by formula (1):
[0015] Li 1.2-x A x [Mn 0.8-x-y-z Ni y Me z ]O2, (1)
[0016] Wherein A is a dopant metal, Me is a metal selected from cobalt (Co), aluminum (Al) and combinations thereof, 0<x≤0.12, 0.1≤y≤0.5, and 0≤z≤0.2.
[0017] The transition metal carbonate comprises nickel and manganese. The dopant metal carbonate comprises a dopant metal selected from the group consisting of sodium (Na), potassium (K), rubidium (Rb), cesium (Cs), magnesium (Mg), calcium (Ca), strontium (Sr), barium (Ba), and combinations thereof.
[0018] The molar ratio of the dopant metal to lithium in the mixture may be greater than or equal to about 0.005 and less than or equal to about 0.1.
[0019] The transition metal carbonate may include manganese nickel carbonate. The molar ratio of manganese to nickel in the transition metal carbonate may be greater than or equal to about one (1) to less than or equal to about 5.
[0020] The dopant metal may include rubidium (Rb), cesium (Cs), or a combination thereof.
[0021] The transition metal carbonate may further include cobalt (Co), aluminum (Al), or a combination thereof.
[0022] The lithium source may include lithium metal, lithium salts, or a combination thereof.
[0023] The mixture may be calcined by heating the mixture in an oxygen-containing environment at a temperature of about 700 degrees Celsius to about 1000 degrees Celsius for about 12 hours to about 36 hours.
[0024] The mixture may be calcined by heating the mixture from ambient temperature to a temperature of about 900° C. at a ramp rate of about 2° C. / minute in an oxygen-containing environment, and then maintaining the mixture at a temperature of about 900° C. for about 12 hours.
[0025] The method may further include grinding the transition metal carbonate, the dopant metal carbonate, and the lithium source together to form a powder prior to calcining the mixture.
[0026] The method may further include preparing a precursor solution comprising a metal salt in a solvent. The metal salt may include nickel and manganese. The ammonium carbonate solution may be introduced into the precursor solution to form a slurry comprising a liquid phase and a solid precipitation phase, the solid precipitation phase comprising a transition metal carbonate. The method may further include separating the solid precipitation phase from the liquid phase.
[0027] The metal salt may further comprise a dopant metal. In this case, the solid precipitated phase may further comprise a dopant metal carbonate.
[0028] The metal salt may include carbonates, nitrates, sulfates, acetates, oxalates, or combinations thereof. The solvent may include water.
[0029] The precursor solution may include metal cations, and the ammonium carbonate solution may include ammonium cations ([NH4] + In this case, a molar ratio of the metal cations in the precursor solution to the ammonium cations in the ammonium carbonate solution may be greater than or equal to about 0.03 and less than or equal to about 0.04.
[0030] The method may further include adjusting the pH of the slurry such that the slurry exhibits a pH of greater than or equal to about 7 and less than or equal to about 9.
[0031] The present invention discloses the following embodiments:
[0032] 1. A positive electrode material comprising:
[0033] The oxide represented by formula (1):
[0034] Li 1.2-x A x [Mn 0.8-x-y-z Ni y Me z ]O2, (1)
[0035] wherein A is an alkali metal, an alkaline earth metal or a combination thereof, Me is a transition metal, 0<x≤0.12, 0.1≤y≤0.5, and 0≤z≤0.2.
[0036] 2. The positive electrode material according to Embodiment 1, wherein A is a metal selected from sodium (Na), potassium (K), rubidium (Rb), cesium (Cs), magnesium (Mg), calcium (Ca), strontium (Sr), barium (Ba) and combinations thereof.
[0037] 3. The positive electrode material according to embodiment 1, wherein A is a metal selected from rubidium (Rb), cesium (Cs) and a combination thereof.
[0038] 4. The positive electrode material according to Embodiment 3, wherein Me is a transition metal selected from cobalt (Co), aluminum (Al) and a combination thereof.
[0039] 5. The positive electrode material according to Embodiment 3, wherein z=0, x is greater than or equal to about 0.001 and less than or equal to about 0.05, and y is greater than or equal to about 0.2 and less than or equal to about 0.3.
[0040] 6. The positive electrode material according to Embodiment 1, wherein the oxide has a layered crystal structure comprising a transition metal layer, an oxygen layer, and a lithium layer, and wherein A is present at an octahedral site in the lithium layer.
[0041] 7. A method for producing a positive electrode material, the method comprising:
[0042] preparing a mixture comprising a transition metal carbonate comprising nickel and manganese, a dopant metal carbonate comprising a dopant metal selected from the group consisting of sodium (Na), potassium (K), rubidium (Rb), cesium (Cs), magnesium (Mg), calcium (Ca), strontium (Sr), barium (Ba), and combinations thereof; and
[0043] The mixture is calcined to form an oxide represented by formula (1):
[0044] Li l.2-x A x [Mn 0.8-x-y-z Ni y Me z ]O2, (1)
[0045] Wherein A is a dopant metal, Me is a metal selected from cobalt (Co), aluminum (Al) and combinations thereof, 0<x≤0.12, 0.1≤y≤0.5, and 0≤z≤0.2.
[0046] 8. The method of embodiment 7, wherein the molar ratio of the dopant metal to lithium in the mixture is greater than or equal to about 0.005 and less than or equal to about 0.1.
[0047] 9. The method of embodiment 7, wherein the transition metal carbonate comprises manganese nickel carbonate, and wherein the molar ratio of manganese to nickel in the transition metal carbonate is greater than or equal to about one (1) to less than or equal to about 5.
[0048] 10. The method of embodiment 7, wherein the dopant metal comprises rubidium (Rb), cesium (Cs), or a combination thereof.
[0049] 11. The method according to embodiment 7, wherein the transition metal carbonate further comprises cobalt (Co), aluminum (Al) or a combination thereof.
[0050] 12. The method according to Embodiment 7, wherein the lithium source comprises lithium metal, a lithium salt or a combination thereof.
[0051] 13. The method of embodiment 7, wherein the mixture is calcined by heating the mixture at a temperature of about 700 degrees Celsius to about 1000 degrees Celsius in an oxygen-containing environment for about 12 hours to about 36 hours.
[0052] 14. A method according to embodiment 7, wherein the mixture is calcined by heating the mixture from ambient temperature to a temperature of about 900 degrees Celsius in an oxygen-containing environment at a heating rate of about 2 degrees Celsius per minute, and then maintaining the mixture at a temperature of about 900 degrees Celsius for about 12 hours.
[0053] 15. The method according to embodiment 7 further comprises:
[0054] The transition metal carbonate, dopant metal carbonate and lithium source are ground together to form a powder prior to calcining the mixture.
[0055] 16. The method according to embodiment 7 further comprises:
[0056] preparing a precursor solution comprising a metal salt comprising nickel and manganese in a solvent;
[0057] introducing an ammonium carbonate solution into the precursor solution to form a slurry comprising a liquid phase and a solid precipitation phase comprising a transition metal carbonate; and
[0058] The solid precipitate phase is separated from the liquid phase.
[0059] 17. A method according to embodiment 16, wherein the metal salt further comprises a dopant metal, and wherein the solid precipitated phase further comprises a dopant metal carbonate.
[0060] 18. The method of embodiment 16, wherein the metal salt comprises a carbonate, a nitrate, a sulfate, an acetate, an oxalate, or a combination thereof, and wherein the solvent comprises water.
[0061] 19. The method of embodiment 16, wherein the precursor solution comprises metal cations and the ammonium carbonate solution comprises ammonium cations ([NH4] + ), and wherein the molar ratio of the metal cations in the precursor solution to the ammonium cations in the ammonium carbonate solution is greater than or equal to about 0.03 and less than or equal to about 0.04.
[0062] 20. The method according to embodiment 16, further comprising:
[0063] The pH of the slurry is adjusted such that the slurry exhibits a pH greater than or equal to about 7 and less than or equal to about 9.
[0064] Other areas of applicability of the present disclosure will become apparent from the detailed description, claims and drawings.The detailed description and specific examples are for illustrative purposes only and are not intended to limit the scope of the present disclosure. BRIEF DESCRIPTION OF THE DRAWINGS
[0065] The present disclosure will be more fully understood from the detailed description and accompanying drawings, in which:
[0066] Figure 1 is a schematic cross-sectional view of an electrochemical cell that circulates lithium ions and includes a positive electrode, a negative electrode, a porous separator, and an electrolyte.
[0067] Among the drawings, reference numerals may be repeated to identify similar and / or identical elements. Specific implementation plan
[0068] The positive electrode material according to the present disclosure comprises a layered lithium-rich and manganese-rich nickel oxide (LMR) that has been doped with an alkali metal and / or an alkaline earth metal (doped-LMR). It has been found that an electrochemical cell comprising the doped-LMR positive electrode material of the present disclosure exhibits improved electrochemical performance, such as improved capacity retention, compared to an electrochemical cell in which an undoped LMR is used as a positive electrode material.
[0069] LMR has a layered crystal structure with repeated transition metal (TM) layers, oxygen layers, and lithium (Li) layers. During electrochemical charging, LMR delithiation, and Li ions are removed from the Li layer, leaving vacancies in the Li layer. In some cases, the formation of three adjacent Li vacancies (Li trivacancies) in the Li layer can create opportunities for TM ions (e.g., manganese ions) located at octahedral sites in the TM layer to migrate to face-sharing tetrahedral sites in the Li layer at the position of the Li trivacancies. The migration of TM ions from the TM layer to the tetrahedral sites in the Li layer can promote the formation of undesirable spinel phases. Without intending to be bound by theory, it is believed that in the doped-LMR positive electrode material of the present disclosure, alkali metal and / or alkaline earth metal ions can replace some Li ions in the Li layer. And the relatively large ionic radius of the alkali metal and / or alkaline earth metal ions can inhibit the migration of TM ions from octahedral sites in the TM layer to tetrahedral sites in the Li layer, even when there is a high concentration of Li ion vacancies in the Li layer. In this manner, doping the LMR with an alkali metal and / or alkaline earth metal is believed to suppress the formation of a spinel phase during electrochemical charging and delithiation of the doped-LMR and may thus help maintain the layered structure and electrochemical performance characteristics of the doped-LMR.
[0070] As used herein, the phrase "alkali metals" refers to elements in Group 1 of the Periodic Table of Chemical Elements as designated by the International Union of Pure and Applied Chemistry (IUPAC), and includes, for example, sodium (Na), potassium (K), rubidium (Rb), and cesium (Cs). As used herein, the phrase "alkaline earth metals" refers to elements in Group 2 of the Periodic Table of Chemical Elements, as designated by IUPAC, and includes, for example, magnesium (Mg), calcium (Ca), strontium (Sr), and barium (Ba).
[0071] Figure 1 A schematic side cross-sectional view of an electrochemical cell 10 for cycling lithium ions is depicted. The electrochemical cell 10 includes a positive electrode 12, a negative electrode 14, a separator 16, and an electrolyte 18. The positive electrode 12 is disposed on a major surface of a positive electrode current collector 20, and the negative electrode 14 is disposed on a major surface of a negative electrode current collector 22. In practice, the positive and negative electrode current collectors 20, 22 may be electrically connected to a power source or load 24 via an external circuit 26.
[0072] Electrochemical cell 10 can be used in secondary lithium batteries, as non-limiting examples, for vehicle or automotive transportation applications (e.g., motorcycles, boats, tractors, buses, motorbikes, mobile homes, campers, and tanks), as well as for a wide variety of other industries and applications, including aerospace parts, consumer products, devices, buildings (e.g., houses, offices, sheds, and warehouses), office equipment and furniture, and industrial equipment machinery, agricultural or farm equipment, or heavy machinery. In certain aspects, electrochemical cell 10 can be used in secondary lithium batteries for hybrid electric vehicles (HEVs) and / or electric vehicles (EVs).
[0073] The positive electrode 12 is configured to store and release lithium ions during the discharge and charge processes of the electrochemical cell 10, and may be in the form of a continuous porous layer disposed on a major surface of the positive electrode current collector 20. The positive electrode 12 includes at least one electrochemically active (electroactive) material that can promote the storage and release of lithium ions by undergoing a reversible redox reaction with lithium. The at least one electroactive material of the positive electrode 12 comprises a layered lithium-rich and manganese-rich nickel oxide (doped-LMP) that has been doped with an alkali metal and / or an alkaline earth metal. The alkali metal and / or alkaline earth metal doped-LMR electroactive material of the positive electrode 12 is represented by formula (1):
[0074] Li 1.2-x A x [Mn 0.8-x-y-z Ni y Me z ]O2, (1)
[0075] Wherein A is an alkali metal, an alkaline earth metal, or a combination thereof, Me is a transition metal, 0<x≤0.12, 0.1≤y≤0.5, and 0≤z≤0.2. For example, A can be a metal selected from sodium (Na), potassium (K), rubidium (Rb), cesium (Cs), magnesium (Mg), calcium (Ca), strontium (Sr), barium (Ba), and combinations thereof, and Me can be a transition metal selected from cobalt (Co), aluminum (Al), and combinations thereof. In some aspects, A can be Rb and / or Cs. In some aspects, x can be greater than or equal to about zero (0), optionally about 0.001, or optionally about 0.005, and less than or equal to about 0.12, optionally about 0.1, or optionally about 0.05. For example, in various aspects, x can be about 0.01. In other words, the molar ratio of A to Li in the doped-LMR electroactive material of formula (1) may be greater than or equal to about 0.005, optionally about 0.008, or optionally about 0.01 and less than or equal to about 0.1, or optionally about 0.05. In some aspects, y may be greater than or equal to about 0.1, or optionally about 0.2 and less than or equal to about 0.5, or optionally about 0.3. For example, in some aspects, y may be about 0.24. In other words, the molar ratio of Mn to Ni in the doped-LMR electroactive material of formula (1) may be greater than or equal to about one (1), optionally about 2, or optionally about 3, and less than or equal to about 5, or optionally about 4. In some aspects, z may be greater than or equal to 0 and less than or equal to about 0.2. For example, in some aspects, z may be 0. In this case, the doped-LMR electroactive material of formula (1) may be substantially free of Co and / or Al. In some aspects, manganese (Mn) and nickel (Ni) can be the only transition metals in the doped-LMR electroactive material of formula (1).
[0076] The doped-LMR electroactive material of formula (1) may have a layered crystal structure having repeating transition metal (TM) layers, oxygen layers, and lithium (Li) layers. The TM layers may contain Mn ions, Ni ions, and optionally Me ions (Co and / or Al). In some aspects, the TM layers may also include Li ions. Alkali metal and / or alkaline earth metal (A) ions may be present in the layered crystal structure of the doped-LMR electroactive material of formula (1). For example, the A metal ions may be present at octahedral sites within the Li layer. In other words, the LMR may be substitutionally doped with A metal ions, wherein the A metal ions replace the Li ions in the Li layer. As another example, the A metal ions may be present at octahedral sites within the TM layer. In other words, the LMR may be substitutionally doped with A metal ions, wherein the A metal ions replace the Li ions in the TM layer.
[0077] In some aspects, the doped-LMR electroactive material of formula (1) can be in particle form. In this case, the particles of the doped-LMR electroactive material of formula (1) can be substantially spherical and can have an aspect ratio close to one (1). For example, the particles of the doped-LMR electroactive material of formula (1) can be substantially spherical and can have an aspect ratio of less than 10.
[0078] The doped-LMR electroactive material of formula (1) may be present in the positive electrode 12 in an amount by weight of greater than or equal to about 30 wt %, greater than or equal to about 40 wt %, greater than or equal to about 50 wt %, greater than or equal to about 60 wt %, greater than or equal to about 70 wt %, greater than or equal to about 80 wt %, greater than or equal to about 90 wt %, greater than or equal to about 96 wt %, or about 98 wt %; or from about 30 wt % to about 98 wt %, from about 40 wt % to about 98 wt %, from about 40 wt % to about 96 wt %, from about 40 wt % to about 90 wt %, from about 40 wt % to about 80 wt %, from about 40 wt % to about 70 wt %, from about 40 wt % to about 60 wt %, or from about 40 wt % to about 50 wt %.
[0079] In some embodiments, in addition to the doped -LMR electroactive material of formula (1), the electroactive material of the positive electrode 12 may include a material that can undergo lithium insertion and deinsertion or can undergo transformation by reacting with lithium. In some aspects, the electroactive material of the positive electrode 12 may include an intercalation host material that is capable of undergoing reversible insertion or insertion of lithium ions. In such cases, the electroactive material of the positive electrode 12 may include a layered oxide represented by the formula LiMeO2, an olivine-type oxide represented by the formula LiMePO4, a monoclinic-type oxide represented by the formula Li3Me2(PO4)3, a spinel-type oxide represented by the formula LiMe2O4, a hydroxyphosphite represented by one or two of the following formulas LiMeSO4F or LiMePO4F, or a combination thereof, wherein Me is a transition metal (e.g., Co, Ni, Mn, Fe, Al, V, or a combination thereof). In some aspects, the electroactive material of the positive electrode 12 may include lithium manganese iron phosphate (LMFP), such as LiMn 0.7 Fe 0.3 PO4, lithium iron phosphate (LFP), lithium manganese oxide (LMO), such as LiMn2O4, and combinations thereof.
[0080] The electroactive material of the positive electrode 12 may be a particulate material, and the particles of the electroactive material of the positive electrode 12 may be mixed with, for example, a polymer binder to provide a positive electrode 12 having structural integrity. Examples of polymer binders include polyvinylidene fluoride (PVDF), polytetrafluoroethylene (PTFE), ethylene propylene diene monomer (EPDM) rubber, styrene butadiene rubber (SBR), carboxymethyl cellulose (CMC), nitrile rubber (NBR), styrene-butadiene rubber (SBR), styrene ethylene butylene styrene copolymer (SEBS), polyacrylate, alginate, polyacrylic acid, and combinations thereof. In some aspects, the positive electrode 12 may include a polymer binder containing polyvinylidene fluoride.
[0081] Positive electrode 12 optionally may include particles of conductive material. Examples of conductive materials include carbon-based materials, metals (e.g., nickel) and / or conductive polymers. Examples of conductive carbon-based materials include carbon black (CB) (e.g., acetylene black), graphite, graphene (e.g., graphene nanosheets GNP), graphene oxide, carbon nanotubes (CNTs) and / or carbon fibers (e.g., carbon nanofibers). Examples of conductive polymers include polyaniline, polythiophene, polyacetylene and / or polypyrrole. In some aspects, the conductive material of positive electrode 12 may include carbon black.
[0082] The negative electrode 14 is configured to store and release lithium ions during the charge and discharge process of the electrochemical cell 10, and can be in the form of a continuous porous or non-porous material layer disposed on the major surface of the negative electrode current collector 24. The negative electrode 14 includes one or more electroactive materials that can promote the storage and release of lithium ions by undergoing a reversible redox reaction with lithium at a lower electrochemical potential than the electroactive material of the positive electrode 12, so that an electrochemical potential difference exists between the positive and negative electrodes 12, 14. Examples of electroactive materials for the negative electrode 14 include lithium, lithium alloys (e.g., alloys of lithium and silicon, aluminum, indium, tin, or combinations thereof), graphite, activated carbon, carbon black, hard carbon, soft carbon, graphene, silicon, silicon-based materials (e.g., alloys of silicon and tin, iron, aluminum, cobalt, or combinations thereof and / or composites of silicon and / or silicon oxide and carbon), tin oxide, aluminum, indium, zinc, germanium, silicon oxide, lithium silicon oxide, lithium silicide, titanium oxide, lithium titanate, and combinations thereof. In some aspects, negative electrode 22 can be in the form of a non-porous metal film or foil, such as a lithium metal film or a lithium-containing foil. In other aspects, the electroactive material of negative electrode 14 can be a particulate material, and the particles of the electroactive material of negative electrode 14 can be mixed with particles of a polymer binder and / or a conductive material. The same polymer binder and / or conductive material disclosed above for positive electrode 12 can be used for negative electrode 14.
[0083] The separator 16 physically separates and electrically isolates the positive electrode from the negative electrode 12, 14 while allowing lithium ions to pass therethrough. The separator 16 exhibits an open microporous structure and may include organic and / or inorganic materials that can physically separate and electrically isolate the positive electrode from the negative electrode 12, 14 while allowing ions to flow freely therebetween. For example, the separator 16 may include a nonwoven material, such as an artificial sheet, web or felt of oriented or randomly oriented fibers. As another example, the separator 16 may include a microporous membrane or film. The nonwoven material and / or microporous membrane of the separator 16 may include a polymer material. For example, the separator 16 may include a polymer having the general formula (CH2CH R ) n A polyolefin-based material, wherein R is an alkyl group. In some aspects, the separator 16 may include a single polyolefin or a combination of polyolefins. Examples of polyolefins include polyethylene (PE), polypropylene (PP), polyamide (PA), poly(tetrafluoroethylene) (PTFE), polyvinylidene fluoride (PVdF), poly(vinyl chloride) (PVC) and / or polyacetylene. Examples of other polymer materials that may be included in the separator 16 or may be used to form the separator 16 include cellulose, polyimide, copolymers of polyolefins and polyimides, polyethylene coated with poly(lithium 4-styrene sulfonate), polyetherimide (PEI), bisphenol-acetone diphthalic anhydride (BPADA), p-phenylenediamine, polyisophthalamide (PMIA) and / or expanded polytetrafluoroethylene-reinforced polyvinylidene fluoride-hexafluoropropylene.
[0084] The electrolyte 18 provides a medium for conducting lithium ions across the electrochemical cell 10 between the positive and negative electrodes 12, 14, and can be in the form of a solid, liquid, or gel. In some aspects, the electrolyte 18 can include a non-aqueous liquid electrolyte solution comprising a lithium salt dissolved in a non-aqueous aprotic organic solvent or a mixture of non-aqueous aprotic organic solvents. Non-limiting examples of lithium salts include lithium hexafluorophosphate (LiPF6), lithium perchlorate (LiClO4), lithium tetrachloroaluminate (LiAlCl4), lithium iodide (LiI), lithium bromide (LiBr), lithium thiocyanate (LiSCN), lithium tetrafluoroborate (LiBF4), lithium tetraphenylborate (LiB(C6H5)4), lithium bis(oxalato)borate (LiB(C2O4)2) (LiBOB), lithium difluorooxalatoborate (LiBF2(C2O4)), lithium hexafluoroarsenate (LiAsF6), Lithium trifluoromethanesulfonate (LiCF3SO3), lithium bis(trifluoromethanesulfonyl)imide (LiN(CF3SO2)2), lithium bis(fluorosulfonyl)imide (LiN(FSO2)2) (LiSFI), lithium (triethylene glycol dimethyl ether) bis(trifluoromethanesulfonyl)imide (Li(G3)(TFSI)), lithium bis(trifluoromethanesulfonyl)azanide (LiTFSA) and combinations thereof. Non-limiting examples of non-aqueous aprotic organic solvents include cyclic carbonates (e.g., ethylene carbonate (EC), propylene carbonate (PC), butylene carbonate (BC), fluoroethylene carbonate (FEC)), linear carbonates (e.g., dimethyl carbonate (DMC), diethyl carbonate (DEC), ethyl methyl carbonate (EMC)), aliphatic carboxylates (e.g., methyl formate, methyl acetate, methyl propionate), γ-lactones (e.g., γ-butyrolactone, γ-valerolactone), chain structure ethers (e.g., 1,2-dimethoxyethane, 1-2-diethoxyethane, ethoxymethoxyethane), cyclic ethers (e.g., tetrahydrofuran, 2-methyltetrahydrofuran), and 1,3-dioxolane.
[0085] The positive and negative electrode current collectors 20, 22 are electrically conductive and provide electrical connections between the external circuit 26 and their respective positive and negative electrodes 12, 14. In some aspects, the positive and negative electrode current collectors 20, 22 may be in the form of non-porous metal foils, perforated metal foils, porous metal meshes, or combinations thereof. The negative electrode current collector 22 may be made of copper, nickel, or alloys thereof, stainless steel, or other suitable conductive materials. The positive electrode current collector 20 may be made of aluminum (Al) or another suitable conductive material.
[0086] method
[0087] The doped-LMR electroactive material of formula (1) can be prepared by a two-step process. In the first stage, a metal carbonate precursor can be prepared by a carbonate co-precipitation method. In the second stage, a solid mixture containing a metal carbonate precursor and a lithium source is calcined to form a doped-LMR electroactive material of formula (1). The first and second stages may include one or more of the following steps.
[0088] In the first step, a precursor aqueous solution of a mixture of metal salts contained in a solvent can be prepared. The solvent can include water. In the preparation process of the doped-LMR electroactive material of formula (1), the metal salt is a source of Mn, Ni, alkali metal and / or alkaline earth metal (A metal) and optionally one or more transition metals (Me metal) such as Co and / or Al. Therefore, the metal salt can include cations of Mn and Ni. In some aspects, the metal salt can include cations of one or more alkali metals and / or alkaline earth metals (A metal) and optionally one or more transition metals (Me metal) such as Co and / or Al. The metal salt can be in the form of carbonate, nitrate, sulfate, acetate, oxalate or a combination thereof. In some aspects, one or more metal salts can be in the form of a hydrate. Examples of metal salts include manganese nitrate (Mn(NO3)2), nickel nitrate (Ni(NO3)2), manganese sulfate (MnSO4), manganese sulfate tetrahydrate (MnSO4·4H2O), nickel sulfate (NiSO4), nickel sulfate hexahydrate (NiSO4·6H2O), rubidium nitrate (RbNO3), rubidium sulfate (Rb2SO4), cesium nitrate (CsNO3), cesium sulfate (Cs2SO4), cobalt nitrate hexahydrate (Co(NO3)2·6H2O), hydrated cobalt sulfate (CoSO4·xH2O), aluminum nitrate (Al(NO3)3), aluminum sulfate (Al2(SO4)3), and combinations thereof. The metal salt may be present in the precursor solution at a concentration of greater than or equal to about 1 molar to less than or equal to about 2 molar. For example, the metal salt may be present in the precursor solution at a concentration of about 1.5 molar.
[0089] In the second step, an ammonium carbonate solution is prepared. The ammonium carbonate solution contains carbonate anions [CO3] 2- and ammonium cation [NH4] +. The ammonium carbonate solution may include a mixture of a carbonate precipitant and a base dissolved in a solvent, which may include water. Examples of carbonate precipitants include sodium carbonate (Na2CO3), ammonium bicarbonate (NH4HCO3), ammonium carbonate ((NH4)2CO3), and combinations thereof. The base is included in the ammonium carbonate solution to control and / or adjust the pH of the ammonium carbonate solution to promote precipitation of metal carbonates. Examples of bases include sodium hydroxide (NaOH) and ammonium hydroxide (NH4OH). In one form, the ammonium carbonate solution may include a mixture of sodium carbonate (Na2CO3) and ammonium hydroxide (NH4OH) in an aqueous solvent (e.g., water). The ammonium cations [NH4] in the ammonium carbonate solution + The concentration of can be greater than or equal to about 0.01 molar, or optionally about 0.05 molar, to less than or equal to about 0.5 molar, or optionally about 0.2 molar. For example, in ammonium carbonate solution [NH4] + The concentration may be about 0.09 molar.
[0090] In the third step, ammonium carbonate solution can be introduced into the precursor solution to form a slurry comprising a solid precipitation phase and a liquid phase. Ammonium carbonate solution can be introduced into the precursor solution at a temperature of greater than or equal to about 50°C to less than or equal to about 70°C or about 60°C. Ammonium carbonate solution can be introduced into the precursor solution at a stirring speed of about 1000rpm and optionally in an inert gas atmosphere (e.g., N2). In some aspects, ammonium carbonate solution can be introduced into the precursor solution by simultaneously introducing ammonium carbonate solution and the precursor solution into a reactor comprising a certain volume (e.g., 850mL) of water. For example, ammonium carbonate solution can be introduced into the reactor at a feed rate of about 2.1 milliliters per hour (mL / hr), and the precursor solution can be introduced into the reactor at a feed rate of about 8.4mL / hr. The amount of ammonium carbonate solution introduced into the precursor solution can be selected so that the molar ratio of the metal cation in the precursor solution to the ammonium cation in the ammonium carbonate solution is greater than or equal to about 0.03 and less than or equal to about 0.04. The pH of the ammonium carbonate solution, precursor solution, and / or slurry may be controlled or adjusted (e.g., by adding an alkaline or acidic solution) such that during the formation of the precipitation phase the slurry exhibits a pH of greater than or equal to about 7, or optionally about 7.7, and less than or equal to about 9, or optionally about 8. After the ammonium carbonate solution is introduced into the precursor solution, the slurry may be maintained at a temperature of greater than or equal to about 50° C. to less than or equal to about 70° C. or about 60° C. while stirring for about 8 hours.
[0091] The solid precipitated phase will contain metal carbonates, such as manganese nickel carbonate (MnNiCO3). In various aspects, the solid precipitated phase may contain carbonates of Mn, Ni, and one or more Me metals, i.e., carbonates represented by the formula MnNiMeCO3. Additionally or alternatively, the solid precipitated phase may contain carbonates of one or more A metals, i.e., carbonates represented by the formula ACO3 (e.g., RbCO3 and / or CsCO3).
[0092] In the fourth step, the solid precipitate phase can be separated from the liquid phase, for example, by vacuum filtration, washed with deionized water to remove reaction byproducts (e.g., Na ions and other water-soluble ions) therefrom, and then dried. The solid precipitate is dried, for example, in a vacuum oven set at 80° C. for 24 hours. The solid precipitate can include substantially spherical particles having an average particle size of greater than or equal to about 1 micron (μm) (or optionally about 5 μm) to less than or equal to about 20 μm, or optionally about 15 μm.
[0093] In the fifth step, a metal carbonate precursor mixture can be prepared, which includes carbonates of Mn, Ni and / or A and optionally Me in the same molar ratio as described in the doped-LMR electroactive material of formula (1). In some aspects, the above-mentioned coprecipitation method can be used to prepare a metal carbonate precursor mixture comprising Mn, Ni, A and optionally Me in a desired ratio, for example by controlling the respective amounts of Mn, Ni, A and optionally Me in the precursor solution. For example, the respective amounts of Mn and Ni in the precursor solution can be controlled to achieve a molar ratio of Mn to Ni in the precursor solution (and in the resulting metal carbonate precipitate) greater than or equal to about one (1), optionally about 2, or optionally about 3 and less than or equal to about 5, or optionally about 4. In other aspects, carbonates of Mn, Ni, A and / or optionally Me can be prepared separately and then mixed together to achieve the same molar ratio as described in the doped-LMR electroactive material of formula (1). For example, MnNiCO3 or MnNiMeCO3 can be prepared by the above-described coprecipitation method, and one or more A metal carbonates (ACO3) can be prepared separately by the above-described coprecipitation method or by another suitable method. Then, MnNiCO3 or MnNiMeCO3 and ACO3 can be mixed together to form a metal carbonate precursor mixture, wherein Mn, Ni, A and optionally Me are present in the mixture in the same molar ratio as described in the doped-LMR electroactive material of formula (1).
[0094] In the sixth step, the metal carbonate precursor mixture is combined with a lithium source to form a solid mixture. The lithium source may include lithium metal and / or a lithium salt. The lithium salt may include lithium and a thermally unstable anion (e.g., nitrate ([NO3] 2- ), carbonate ([CO3] 2-), and combinations thereof). In some aspects, the lithium source may include lithium carbonate (Li2CO3). The metal carbonate precursor mixture and the lithium source are calcined to form a doped-LMR electroactive material of formula (1). The metal carbonate precursor mixture and the lithium source may be mixed together in suitable amounts to achieve the molar ratios of Li, Mn, Ni, A, and optionally Me described in the doped-LMR electroactive material of formula (1). For example, the metal carbonate precursor mixture and the lithium source may be mixed together such that the molar ratio of A to Li in the mixture is greater than or equal to about 0.005, optionally about 0.008, or optionally about 0.01 and less than or equal to about 0.1, or optionally about 0.05.
[0095] The mixture of the metal carbonate precursor mixture and the lithium source may be ground together to form a substantially homogeneous mixture.
[0096] The mixture of the metal carbonate precursor mixture and the lithium source is calcined to form the doped-LMR electroactive material of formula (1). The mixture of the metal carbonate precursor mixture and the lithium source can be calcined by heating the mixture at a temperature of about 700°C to about 1000°C for a duration of about 12 hours to about 36 hours in an oxygen-containing environment (e.g., air). During the calcination of the metal carbonate precursor mixture and the lithium source, gaseous reaction byproducts of oxygen (O2) and carbon dioxide (CO2) can be released therefrom. In some aspects, the mixture of the metal carbonate precursor mixture and the lithium source can be calcined in a stepwise manner. For example, the mixture of the metal carbonate precursor mixture and the lithium source can be calcined by heating the mixture from ambient temperature (e.g., about 25°C) to a temperature of about 500°C (about 4 hours) at a heating rate of about 2°C / minute, heating the mixture to a temperature of about 900°C (about 3 hours) at a heating rate of about 2°C / minute, and then keeping the mixture at a temperature of about 900°C for about 12 hours. As another example, a mixture of a metal carbonate precursor mixture and a lithium source can be calcined by heating the mixture from ambient temperature to a temperature of about 500°C (about 4 hours) at a heating rate of about 2°C / min, heating the mixture to a temperature of about 700°C (about 1.5 hours) at a heating rate of about 2°C / min, heating the mixture to a temperature of about 900°C (about 1.5 hours) at a heating rate of about 2°C / min, and then maintaining the mixture at a temperature of about 900°C for about 12 hours.
[0097] The foregoing description is merely illustrative, and is by no means intended to limit the present disclosure, its application or use. The broad teachings of the present disclosure can be implemented in various forms. Therefore, although the present disclosure includes specific examples, the true scope of the present disclosure should not be so limited, because after studying the drawings, the specification and the appended claims, other modifications will become apparent. It should be understood that, without changing the principles of the present disclosure, one or more steps in the method can be performed in different orders (or simultaneously). In addition, although each embodiment is described above as having certain features, any one or more of those features described in any embodiment of the present disclosure can be implemented in any of other embodiments and / or combined with any feature in other embodiments, even if the combination is not explicitly described. In other words, the embodiments described are not mutually exclusive, and the replacement of one or more embodiments with each other remains within the scope of the present disclosure.
[0098] The terms used herein are only for describing exemplary embodiments and are not intended to be limiting. Unless the context clearly indicates otherwise, as used herein, the singular forms "a", "an" and "the" may be intended to also include plural forms. The terms "comprising", "including", "covering" and "having" are compatible, and therefore specify the presence of the features, elements, compositions, steps, integers, operations and / or components, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, components and / or their groups. Although the open-ended terms "comprising", "including" and "having" should be understood as non-limiting terms for describing and claiming the various embodiments described herein, in some respects, the terms may be understood as alternatively more restrictive and limited terms, such as "consisting of" or "consisting essentially of". Thus, for any given embodiment reciting compositions, materials, components, elements, ingredients, features, integers, operations, and / or method steps, the present disclosure also specifically includes embodiments consisting of or consisting essentially of such recited compositions, materials, components, elements, ingredients, features, integers, operations, and / or method steps. In the case of "consisting of", alternative embodiments exclude any additional compositions, materials, components, elements, ingredients, features, integers, operations, and / or method steps, while in the case of "consisting essentially of", any additional compositions, materials, components, elements, ingredients, features, integers, operations, and / or method steps that materially affect the basic and novel characteristics are excluded from such embodiments, but any compositions, materials, components, elements, ingredients, features, integers, operations, and / or method steps that do not materially affect the basic and novel characteristics may be included in the embodiments.
[0099] Any method steps, processes, and operations described herein should not be construed as necessarily requiring their performance in the order discussed or illustrated, unless expressly identified as an order of performance. It is also understood that additional or alternative steps may be employed unless otherwise specified.
[0100] Although the terms first, second, third, etc. can be used to describe various steps, elements, components, regions, layers and / or sections in this article, unless otherwise specified, these steps, elements, components, regions, layers and / or sections should not be limited by these terms. These terms can only be used to distinguish a step, element, component, region, layer or section from another step, element, component, region, layer or section. Unless the context clearly indicates, terms such as "first", "second" and other numerical terms do not imply order or sequence when used in this article. Therefore, the first step, element, component, region, layer or section discussed below can be referred to as the second step, element, component, region, layer or section without departing from the teaching of exemplary embodiments.
[0101] Throughout this disclosure, numerical values represent approximate measurements or range limits and encompass slight deviations from given values and embodiments having approximately the values mentioned as well as embodiments having exactly the values mentioned. In addition to the working examples provided at the end of the detailed description, all numerical values of (e.g., amounts or conditions) parameters in this specification should be understood to be modified by the term "about" in all cases, regardless of whether "about" actually appears before the numerical value. The numerical values of the parameters in the attached claims should be understood to be modified by the term "about" only when the term "about" appears before the numerical value. "Approximately" means that the numerical value allows a certain slight imprecision (close to the exact value of the value to a certain extent; roughly or reasonably approximate the value; almost). If the imprecision provided by "about" is not otherwise understood in this ordinary meaning in the art, then "about" as used herein refers to at least the deviation that can be caused by the ordinary methods of measuring and using such parameters. For example, "about" can include deviations of less than or equal to 5%, optionally less than or equal to 4%, optionally less than or equal to 3%, optionally less than or equal to 2%, optionally less than or equal to 1%, optionally less than or equal to 0.5%, and optionally less than or equal to 0.1% in some aspects. Furthermore, the disclosure of a range includes disclosure of all values within the entire range and further subdivided ranges, including disclosure of endpoints and sub-ranges given for the range.
[0102] As used herein, unless otherwise indicated, the terms "composition" and "material" are used interchangeably to refer generally to materials that contain at least a preferred chemical constituent, element, or compound, but may also contain additional elements, compounds, or substances, including trace impurities. An "X-based" composition or material broadly refers to a composition or material in which "X" is the largest single component of the composition or material on a weight percent (%) basis. This can include compositions or materials having greater than 50% X by weight, as well as those having less than 50% X by weight - as long as X is the largest single component of the composition or material based on its total weight. When a composition or material is referred to as being "substantially free" of a substance, the composition or material may contain less than 5% by weight, optionally less than 3% by weight, optionally less than 1% by weight, or optionally less than 0.1% by weight of the substance.
[0103] As used herein, the term "metal" may refer to a pure elemental metal or an alloy of an elemental metal with one or more other metals or nonmetallic elements, referred to as "alloying" elements. Alloying elements may be selected to impart certain desired properties to the alloy that the base metal element cannot exhibit.
Claims
1. A positive electrode material comprising: The oxide represented by formula (1): Li 1.2-x A x [Mn 0.8-x-y-z Ni y Me z ]O2, (1) Where 0<x≤0.12, 0.1≤y≤0.5, 0≤z≤0.2, wherein A is a metal selected from the group consisting of sodium (Na), potassium (K), rubidium (Rb), cesium (Cs), magnesium (Mg), calcium (Ca), strontium (Sr), barium (Ba), and combinations thereof, and wherein Me is a transition metal selected from cobalt (Co), aluminum (Al) and combinations thereof, and wherein the oxide has a layered crystal structure including a transition metal layer, an oxygen layer, and a lithium layer, and wherein A exists at an octahedral site in the lithium layer. 2 . The positive electrode material according to claim 1 , wherein A is a metal selected from rubidium (Rb), cesium (Cs) and combinations thereof. 3 . The positive electrode material according to claim 3 , wherein z=0, x is greater than or equal to 0.001 and less than or equal to 0.05, and y is greater than or equal to 0.2 and less than or equal to 0.
3.
4. A method for producing a positive electrode material, the method comprising: preparing a mixture comprising a transition metal carbonate comprising nickel and manganese, a dopant metal carbonate comprising a dopant metal selected from the group consisting of sodium (Na), potassium (K), rubidium (Rb), cesium (Cs), magnesium (Mg), calcium (Ca), strontium (Sr), barium (Ba), and combinations thereof, and wherein the molar ratio of manganese to nickel in the transition metal carbonate is greater than or equal to about one (1) to less than or equal to about 5; and The mixture is calcined to form an oxide represented by formula (1): Li 1.2-x A x [Mr 0.8-x-y-z Ni y Along with z ]O2, (1) Wherein A is a dopant metal, Me is a metal selected from cobalt (Co), aluminum (Al) and combinations thereof, 0<x≤0.12, 0.1≤y≤0.5, and 0≤z≤0.
2. 5 . The method of claim 4 , wherein a molar ratio of the dopant metal to lithium in the mixture is greater than or equal to 0.005 and less than or equal to 0.
1. The method of claim 4 , wherein the dopant metal comprises rubidium (Rb), cesium (Cs), or a combination thereof.
7. The method of claim 4, wherein the mixture is calcined by heating the mixture at a temperature of about 700 degrees Celsius to about 1000 degrees Celsius for about 12 hours to about 36 hours in an oxygen-containing environment.
8. The method according to claim 4, further comprising: A precursor solution is prepared comprising a metal salt in a solvent, the metal salt comprising nickel and manganese, the precursor solution comprising metal cations, and the ammonium carbonate solution comprising ammonium cations ([NH4] + ), and wherein the molar ratio of the metal cations in the precursor solution to the ammonium cations in the ammonium carbonate solution is greater than or equal to about 0.03 and less than or equal to about 0.04; introducing an ammonium carbonate solution into the precursor solution to form a slurry having a pH of 7 to 9, the slurry comprising a liquid phase and a solid precipitated phase, the solid precipitated phase comprising a transition metal carbonate; as well as The solid precipitate phase is separated from the liquid phase.
9. The method of claim 8, wherein the metal salt further comprises a dopant metal, and wherein the solid precipitated phase further comprises a dopant metal carbonate.
10. The method of claim 8, wherein the metal salt comprises a carbonate, a nitrate, a sulfate, an acetate, an oxalate, or a combination thereof, and wherein the solvent comprises water.