WO3 / g-C3N4 / Ni-foam photocatalytic film as well as preparation method and application thereof

By loading g-C3N4 on the foam nickel film and growing WO3, forming WO3/g-C3N4/Ni-foam photocatalytic film, the high cost of electrocatalytic method and difficulty in recycling are solved, and can efficient degradation of dodecyl groups be achieved? and protect the salt lake environment.

CN118874509AActive Publication Date: 2024-11-01HUAQIAO UNIVERSITY

Patent Information

Application Number
CN202410907270.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-08
Publication Date
2024-11-01
Estimated Expiration
2044-07-08

AI Technical Summary

Technical Problem

The existing electrocatalytic methods are costly and have secondary pollution problems when treating industrial wastewater containing dodecylmorpholine. The powder material of the photocatalyst is difficult to recover, and there are few methods for degrading the flotation agent in the salt lake brine.

Method used

g-C3N4 was supported on a foam nickel film by gel method, and WO3 was grown by hydrothermal method to form a WO3/g-C3N4/Ni-foam photocatalytic film, improving photocatalytic activity and degrading dodecylmorpholine.

Benefits of technology

It improves the degradation efficiency of dodecylmorpholine, avoids water pollution, realizes easy recycling and reuse of photocatalysts, reduces operating costs, and protects the salt lake environment.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118874509A_ABST
    Figure CN118874509A_ABST
Patent Text Reader

Abstract

The invention provides a WO3 / g-C3N4 / Ni-foam photocatalytic film as well as a preparation method and application of the WO3 / g-C3N4 / Ni-foam photocatalytic film. The WO3 / g-C3N4 photocatalyst is loaded on the surface of the foamed nickel film mainly according to a gel method and a hydrothermal method, the photocatalyst forms a composite photocatalytic material on the surface of the foamed nickel film, effective degradation of dodecyl morpholine in a water body is realized, and no redundant energy consumption is caused by using sunlight as an energy source; the method is suitable for treating the dodecylmorpholine in the water body, and is simple, remarkable in effect, safe, environmentally friendly and easy to recycle. The method disclosed by the invention has important significance on low-energy-consumption and pollution-free treatment of the flotation agent dodecyl morpholine in the salt lake brine.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the field of salt lake brine treatment and environmental protection, and specifically relates to a WO 3 / gC 3 N 4 / Ni-foam photocatalytic film and its preparation method and application. Background Art

[0002] The main preparation method of potassium salt is to enrich the potassium element in the salt lake brine. It is necessary to add flotation agents to the salt lake brine to float the potassium salt. Dodecylmorpholine (DMP) is one of the most commonly used flotation agents today. However, adding a large amount of flotation agents to the salt lake will damage the ecological environment of the salt lake. Therefore, it is necessary to promptly deal with the residual flotation agents in the salt lake water.

[0003] At present, most factories use electrocatalytic methods to treat industrial wastewater containing DMP, that is, the dielectric barrier discharge plasma method, but this method has the following disadvantages: first, the electrocatalytic method is more expensive, and the electrocatalytic process continuously increases the current to the wastewater, consuming a lot of energy; second, a large amount of Cr-containing 3+ , Fe 3+ solution, causing secondary pollution.

[0004] In view of the shortcomings of electrocatalytic reactions, photocatalysis, a semiconductor photodegradation technology that utilizes solar energy, is widely considered to be a promising technology for removing organic pollutants in water because of its advantages such as non-toxicity, recyclability, green and renewable energy. The mechanism of photocatalytic redox is mainly that the catalyst is exposed to light, absorbs light energy, undergoes electron transition, generates electron-hole pairs, directly redoxes pollutants adsorbed on the surface, or oxidizes the surface OH- to generate strong oxidizing hydroxyl radicals (·OH) or superoxide radicals (·O2 - ), oxidizing the pollutants.

[0005] Most of the photocatalysts prepared today are powder materials, which are difficult to recycle after being put into water to degrade pollutants, and the recovery loss rate is high. Therefore, preparing the photocatalytic material as a membrane material is conducive to recycling and reuse after the catalytic reaction. The recovery method is simple and the loss rate is low. Although photocatalytic degradation of pollutants in water bodies has been applied in many fields, there are very few methods for using photocatalysis to treat the flotation agent dodecylmorpholine in salt lake brine. If photocatalysis is used to degrade dodecylmorpholine, how to synthesize a photocatalyst that can efficiently degrade dodecylmorpholine is the key to the technology. Summary of the invention

[0006] The inventors found in the process of implementing the present invention that gC 3 N 4Unique properties such as high stability (even in strong acid and base solutions), low cost, and a band gap of 2.7 eV make gC 3 N 4 It has become a promising candidate material for photocatalytic processes using solar energy as a light source. However, pure gC 3 N 4 The photogenerated carriers recombine quickly and have poor absorption in the visible light region, resulting in low photocatalytic activity under visible light irradiation. Therefore, it is necessary to explore gC with enhanced photocatalytic activity. 3 N 4 Photocatalysts are becoming increasingly important. 3 N 4 In order to improve the photocatalytic activity, strategies such as doping with metal or non-metal elements, increasing the surface area, and coupling with other semiconductors were adopted.

[0007] Tungsten trioxide (WO 3 ) has good visible light absorption performance due to its suitable band gap, high chemical stability and good electron transport behavior. 3 It is a non-toxic, light-stable semiconductor with a band gap of 2.6-2.8 eV and can absorb visible light, but due to its insufficient conduction band potential, WO 3 It is impossible to generate superoxide radicals in the photocatalytic reaction. 3 N 4 with WO 3 After constructing a Z-type heterojunction, the efficiency of electron separation and migration can be effectively improved, and the photocatalytic ability can be enhanced.

[0008] Nickel foam is a typical three-dimensional porous material, due to its low density, high mechanical strength, good thermal stability and chemical stability. In addition, its large specific surface area provides a large number of active catalytic sites, which is conducive to improving the photocatalytic activity. Therefore, nickel foam is an ideal carrier material for photocatalysts.

[0009] Based on the above considerations, the present invention uses a gel method to convert powdered 3 N 4 The modified WO was loaded on the nickel foam material and then hydrothermally treated. 3 Grown on the surface of the film, the composite WO 3 / gC 3 N 4 / Ni-foam photocatalytic film.

[0010] Specifically, the preparation method comprises the following steps:

[0011] (1) Weigh rosin resin, morpholine, ammonia water and deionized water into a beaker;

[0012] (2) placing the material obtained in step (1) in an oil bath and stirring to react to obtain rosin water gel;

[0013] (3) calcining dicyandiamide to obtain gC 3 N 4 ;

[0014] (4) the gC 3 N 4 After grinding until there are no obvious particles, add it into the rosin water gel and mix evenly to obtain a hydrogel;

[0015] (5) applying the hydrogel obtained in step (4) on the surface of the nickel foam film;

[0016] (6) placing the nickel foam film coated with hydrogel obtained in step (5) in a tubular furnace and calcining the nickel foam film loaded with gC 3 N 4 Nickel foam film;

[0017] (7) Put Na 2 WO 4 ·H 2 O was dissolved in water, HCl solution was added dropwise to adjust the pH value to 1.9-2.1, and then water was added to obtain solution A;

[0018] (8) Add glacial acetic acid dropwise to solution A to adjust the pH value to 2.2 to 2.4, and stir evenly to obtain solution B;

[0019] (9) The nickel foam film obtained in step (6) is placed vertically in solution B, subjected to hydrothermal reaction at 155-165° C. for 14-18 h, and then taken out after cooling to room temperature, washed, and vacuum dried to obtain WO 3 / gC 3 N 4 / Ni-foam photocatalytic film.

[0020] Preferably, in step (2), the temperature of the oil bath is 50-60° C., and the stirring rate is 150-250 r / min.

[0021] Preferably, in step (3), the heating rate of calcination is 4-6°C / min, and after heating to 545-555°C, the temperature is maintained for 3-5h.

[0022] Preferably, the concentration of the HCl solution in step (7) is 1-2 mol / L.

[0023] Preferably, in step (8), the stirring rate is 150-250 r / min, and the stirring time is 20-40 min.

[0024] Preferably: in step (9), the washing method is to wash repeatedly with water and alcohol alternately; in step (9), the vacuum drying temperature is 45-55°C, and the vacuum drying time is 22-26 hours.

[0025] A WO prepared according to the above preparation method 3 / gC 3 N 4 / Ni-foam photocatalytic film.

[0026] A WO as described above 3 / gC 3 N 4 / Application of Ni-foam photocatalytic film in degradation of dodecylmorpholine in water.

[0027] Preferably: including:

[0028] The WO 3 / gC 3 N 4 / Ni-foam photocatalytic film is added into water containing dodecylmorpholine, stirred in a dark place for 25 to 35 minutes, and then reacted under light conditions for 50 to 70 minutes.

[0029] Among them, a 300W xenon lamp plus a filter can be used to simulate sunlight to provide a light source.

[0030] Preferably: the WO 3 / gC 3 N 4 The ratio of the / Ni-foam photocatalytic film to the water containing dodecylmorpholine is 0.08-0.12 g: 90-110 mL, the concentration of dodecylmorpholine in the water is 7-9 mmol / L, and the pH value of the water is 3.0-3.2.

[0031] Unless otherwise specified, the equipment, reagents, processes, parameters, etc. involved in the present invention are conventional equipment, reagents, processes, parameters, etc. and are not given as embodiments.

[0032] All ranges recited herein include all point values ​​within the range.

[0033] In the present invention, the "room temperature" refers to the normal ambient temperature, which may be 10 to 30°C.

[0034] Compared with the prior art, the present invention has the following beneficial effects:

[0035] The present invention targets dodecylmorpholine in water and utilizes modified WO 3 and graphite type gC 3 N 4The composite photocatalyst constructs a Z-type heterojunction to improve the catalytic performance of the material, thereby increasing the degradation efficiency of dodecylmorpholine, without causing any excess pollutants to pollute the water body. It can effectively degrade a small amount of dodecylmorpholine in the water body, prevent dodecylmorpholine from damaging and polluting the mineral deposits in the water body, and achieve the purpose of protecting the environment.

[0036] In addition, the preparation method of the present invention is simple to operate, high in quality, and good in repeatability. Compared with the existing DMP degradation technology, it has higher efficiency and no secondary pollution, and the catalyst is easy to recover and reuse. BRIEF DESCRIPTION OF THE DRAWINGS

[0037] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the drawings required for use in the embodiments are briefly introduced below. It should be understood that the following drawings only show certain embodiments of the present invention and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without creative work.

[0038] Figure 1 WO in Example 1 of the present invention 3 / gC 3 N 4 / X-ray diffraction pattern of Ni-foam photocatalytic film.

[0039] Figure 2 a)- Figure 2 f) is WO in Example 1 of the present invention 3 / gC 3 N 4 / Scanning electron microscope photograph of Ni-foam photocatalytic film.

[0040] Figure 3 WO in Example 1 of the present invention 3 / gC 3 N 4 Performance curve of photocatalytic degradation of dodecylmorpholine solution of / Ni-foam photocatalytic film.

[0041] picture Figure 4(a)-Figure 4(c) WO in Example 1 of the present invention 3 / gC 3 N 4 / Ni-foam photocatalytic film degradation of dodecylmorpholine solution cyclic degradation spectrum.

[0042] Figure 5 WO in Example 2 of the present invention 3 / gC 3 N 4Performance curve of photocatalytic degradation of dodecylmorpholine solution of / Ni-foam photocatalytic film. Specific implementation plan

[0043] In order to make the purpose, technical solutions and advantages of the present invention more clearly understood, the present invention is described in more detail below with reference to the accompanying drawings and specific embodiments, but the protection scope of the present invention is not limited to these embodiments.

[0044] Example 1

[0045] A WO 3 / gC 3 N 4 / The preparation method of Ni-foam photocatalytic film is as follows:

[0046] (1) Weigh 12 g of rosin resin, 1 g of morpholine, 3.5 g of ammonia water and 83.5 g of deionized water into a beaker;

[0047] (2) placing the material obtained in step (1) in an oil bath and stirring at 60° C. to obtain rosin water gel;

[0048] (3) Dicyandiamide was placed in a muffle furnace and calcined at 550°C for 4 h to prepare gC 3 N 4 ;

[0049] (4) The gC obtained in step (3) 3 N 4 After grinding until there are no obvious particles, weigh 0.9g and add it to 15g of rosin water gel and mix well;

[0050] (5) applying the hydrogel obtained in step (4) on the surface of the nickel foam film;

[0051] (6) The nickel foam film coated with hydrogel obtained in step (5) was placed in a tube furnace and heated to 320° C. at a heating rate of 5° C. / min under a nitrogen atmosphere and maintained for 2 h to obtain a nickel foam film loaded with gC 3 N 4 Nickel foam film;

[0052] (7) 1.65 g Na 2 WO 4 ·H 2 O was dissolved in water, 1 mol / L HCl solution was added dropwise to adjust the pH value to 1.9-2.1, and then water was added to obtain solution A;

[0053] (8) Add glacial acetic acid dropwise to solution A to adjust the pH value to 2.2 to 2.4, and stir evenly to obtain solution B;

[0054] (9) The nickel foam film obtained in step (6) was placed vertically in solution B, subjected to hydrothermal reaction at 160° C. for 16 h, and then taken out after cooling to room temperature, washed, and vacuum dried at 50° C. to obtain WO 3 / C 3 N 4 / Ni-foam photocatalytic film.

[0055] The prepared WO 3 / C 3 N 4 / Ni-foam photocatalytic film, its X-ray diffraction pattern is as follows Figure 1 As shown in the figure, it can be seen that there are three obvious characteristic peaks in the XRD spectrum of the nickel foam film, which are located at 44.94°, 52.32° and 76.76° respectively. 3 N 4 After loading and conducting XRD test on the surface of nickel foam film, it can be observed that a broad peak appears at 28.18° in the film after reaction. This characteristic peak is gC 3 N 4 The characteristic peaks of gC 3 N 4 The film was successfully loaded on the surface of the film, and the characteristic peak of the film after calcination was shifted to the right, indicating that the crystal plane spacing of the nickel foam became smaller after calcination. 3 / C 3 N 4 / Ni-foam samples were subjected to XRD test. The results show that the characteristic peak intensity of nickel foam is significantly reduced after the hydrothermal reaction. This is due to the 3 Growth on the film surface weakens the characteristic peak of nickel foam film. And it is observed that all samples have sharp peaks at 28.65°, 37.62°, and 49.95°. 3 Standard card (PDF#75-2187) is compared to WO here 3 The (1 0 1), (2 1 0), and (2 2 0) crystal planes of WO 3 Successfully grown in g- / C 3 N 4 / Ni-foam film surface.

[0056] to WO 3 / C 3 N 4 The surface morphology of Ni-foam photocatalytic film was observed by scanning electron microscopy. Figure 2 a)- Figure 2b) is nickel foam, which presents a sponge-like porous structure with a pore size between 100 μm and 400 μm. The width of the nickel foam on the film is about 60 μm. 3 N 4 gC obtained after powder 3 N 4 / Ni-foam morphology is Figure 2 c)- Figure 2 d), a large number of blocky gC 3 N 4 Loaded on the film surface, block gC 3 N 4 The size of the negative powder is between 20μm and 100μm. After loading, the cavities of nickel foam on the film surface have been replaced by blocky gC 3 N 4 Negative filling, indicating that gC was successfully filled after calcination. 3 N 4 Negative load on the film surface. WO 3 Grown on the film surface, it presents a flower-like structure such as Figure 2 e)- Figure 2 f), tightly bonded to the film surface, flake WO 3 The length of WO is between 20 μm and 30 μm, which is relatively uniform. 3 Successfully grown on the film surface; 3 / gC 3 N 4 / Ni-foam photocatalytic film was used to degrade dodecyl morpholine, and the degradation effect was measured by UV spectrophotometer. Figure 3 As shown, under the irradiation of a light source simulating sunlight, it can be observed that the degradation efficiency of DMP by the nickel foam film is 21.03% in 60 minutes. Taking into account a part of the natural degradation effect, it is shown that the degradation effect of the nickel foam film on DMP is poor.

[0057] G C 3 N 4 After the hydrogel was loaded on the surface of nickel foam film, the degradation effect of DMP reached 33.37% in 60 minutes, which was a certain improvement compared with the monomer substance. 3 N 4 Loading on the film surface has a certain improvement in catalytic ability, not just simply loading on the film surface but there is an interaction between the two. Under the same test conditions, WO 3 / gC 3 N 4 / Ni-foam photocatalytic film has a significant improvement in the degradation efficiency of DMP. The degradation efficiency of DMP by the photocatalytic film can reach 49.3% in 60 minutes. 3 / gC 3 N 4 / Ni-foam photocatalytic film has a significant degradation effect on dodecylmorpholine, achieving the effect of removing dodecylmorpholine in water.

[0058] like Figure 4(a)-Figure 4(c) As shown, this embodiment also 3 / gC 3 N 4 / Ni-foam photocatalytic film was subjected to stability experiments to test its degradation ability after multiple degradations. After 5 cycles, the catalytic performance of the photocatalytic film did not decrease significantly, indicating that the stability of the photocatalytic film was good when the number of cycles was small. After 6-15 cycles of experiments, the catalytic performance of the photocatalytic film decreased by 12% overall, indicating that the photocatalytic film can still maintain about 80% of its catalytic performance in a high number of cycles, with good stability and easy recycling.

[0059] Example 2

[0060] The difference from Example 1 is that in the preparation of WO 3 / gC 3 N 4 / Ni-foam photocatalytic film changes gC 3 N 4 The amount added was 1.0 g.

[0061] After the catalyst synthesis is completed, the synthesized WO 3 / gC 3 N 4 / Ni-foam photocatalytic film was added to 100ml8mmol / L dodecylmorpholine solution and stirred in a dark reactor for 30min to allow the catalyst and solution to reach adsorption equilibrium. Then the solution was placed under a light source and the light source was turned on to stir and react for 60min under light conditions. Samples were taken every 10min to test the concentration of dodecylmorpholine in the current solution and calculate the degradation rate. The results are shown in Figure 5 As shown, the composite WO 3 / gC 3 N 4 / The Ni-foam photocatalytic film has a degradation efficiency of 45% for dodecylmorpholine in the solution, which is significantly improved compared with the monomer and has a significant effect on the degradation of dodecylmorpholine in a short time.

[0062] The embodiments described above are part of the embodiments of the present invention, rather than all of the embodiments. The detailed description of the embodiments of the present invention is not intended to limit the scope of the invention claimed for protection, but merely represents selected embodiments of the present invention. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

Claims

1. A method for preparing a WO3 / g-C3N4 / Ni-foam photocatalytic film, characterized in that: include: (1) Weigh rosin resin, morpholine, ammonia water and deionized water into a beaker; (2) placing the material obtained in step (1) in an oil bath and stirring to react to obtain rosin water gel; (3) calcining dicyandiamide to obtain g-C3N4; (4) grinding the g-C3N4 until there are no obvious particles, adding it to the rosin water gel and mixing it evenly to obtain a hydrogel; (5) applying the hydrogel obtained in step (4) on the surface of the nickel foam film; (6) placing the nickel foam film coated with the hydrogel obtained in step (5) in a tubular furnace and calcining it to obtain a nickel foam film loaded with g-C3N4; (7) dissolving Na2WO4·H2O in water, adding HCl solution dropwise to adjust the pH value to 1.9-2.1, and then adding water to obtain solution A; (8) Add glacial acetic acid dropwise to solution A to adjust the pH value to 2.2 to 2.4, and stir evenly to obtain solution B; (9) The nickel foam film obtained in step (6) is placed vertically in solution B, subjected to hydrothermal reaction at 155-165° C. for 14-18 h, and taken out after cooling to room temperature, washed and vacuum dried to obtain a WO3 / g-C3N4 / Ni-foam photocatalytic film.

2. The preparation method according to claim 1, characterized in that: In step (2), the temperature of the oil bath is 50-60° C., and the stirring rate is 150-250 r / min.

3. The preparation method according to claim 1, characterized in that: In the step (3), the heating rate of calcination is 4 to 6°C / min, and the temperature is maintained for 3 to 5 hours after being heated to 545 to 555°C; in the step (6), the heating rate of calcination is 4 to 6°C / min in a tubular furnace under a nitrogen atmosphere, and the temperature is maintained for 2 to 3 hours after being heated to 305 to 330°C.

4. The preparation method according to claim 1, characterized in that: The concentration of the HCl solution in step (7) is 1-2 mol / L, and the amount of water added is 4-6 times the amount of water used to dissolve Na2WO4·H2O.

5. The preparation method according to claim 1, characterized in that: In the step (8), the stirring rate is 150 to 250 r / min, and the stirring time is 20 to 40 min.

6. The preparation method according to claim 1, characterized in that: In the step (9), the washing method is to wash repeatedly with water and alcohol alternately; in the step (9), the vacuum drying temperature is 45 to 55°C, and the vacuum drying time is 22 to 26 hours.

7. A WO3 / g-C3N4 / Ni-foam photocatalytic film prepared according to the preparation method according to any one of claims 1 to 6.

8. Use of the WO3 / g-C3N4 / Ni-foam photocatalytic film prepared according to claim 7 in degrading dodecylmorpholine in water.

9. The use according to claim 8, characterized in that: The WO3 / g-C3N4 / Ni-foam photocatalytic film is added into a water body containing dodecylmorpholine, and stirred in a dark place for 25 to 35 minutes, and then reacted under light conditions for 50 to 70 minutes.

10. The use according to claim 8, characterized in that: The ratio of the WO3 / g-C3N4 / Ni-foam photocatalytic film to the water containing dodecylmorpholine is 0.08-0.12 g: 90-110 mL, the concentration of dodecylmorpholine in the water is 7-9 mmol / L, and the pH value of the water is 3.0-3.2.

Citation Information

Patent Citations

  • Photocatalytic material of nano WO3-g-C3N4-rGO heterojunction loaded foamed nickel and preparation method of the photocatalytic material

    CN111644191A

  • Bi5O7I / WO3 / Ni foam photocatalytic membrane for deeply purifying VOCs (volatile organic compounds) and preparation method of Bi5O7I / WO3 / Ni foam photocatalytic membrane

    CN114849742A

  • Rod-like WO3 / flaky g-C3N4 photocatalyst, preparation method and method for degrading dodecyl morpholine in salt lake brine

    CN116603557A

  • Ni-MOF thin-film photocatalyst grown in-situ on foamed nickel surface, preparation method therefor, and use thereof

    WO2022041852A1

Cited By

  • Supported BiVO4 / NF photocatalyst as well as preparation method and application thereof

    CN119608175A

  • A supported BiVO4 / NF photocatalyst, its preparation method and application

    CN119608175B