Preparation method of heating type graphene fabric
By surface grafting modification of graphene oxide fibers and treatment of sulphon extract, combined with electric heating wire mesh, the problem of thermal conductivity and antibacterial properties of heated graphene fabrics is solved, and the fabric is realized after multiple use Efficient heating and antibacterial effects.
Patent Information
- Application Number
- CN202410947274.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-16
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2044-07-16
AI Technical Summary
After many wear and use of existing heated graphene fabrics, their thermal conductivity and antibacterial properties will be significantly reduced, resulting in a decrease in the use effect.
By preparing modified graphene oxide fibers, surface grafting modification was performed using N-aminoethyl-3-aminopropylmethyldimethoxysilane, and soaking it in the roshurica extract to enhance the fibers The binding ability and antibacterial properties are laid in the graphene fiber layer with an electric heating wire mesh to form a stable heating graphene fabric.
It significantly improves the thermal conductivity and antibacterial properties of the fabric, so that it can maintain efficient heating and antibacterial effects after multiple wear and use.
Smart Images

Figure BDA0004946047320000081 
Figure BDA0004946047320000082 
Figure BDA0004946047320000091
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of fabric preparation, and in particular to a method for preparing a heated graphene fabric. Background Art
[0002] Graphene is an emerging material that has been widely studied in recent years. It is ultra-thin, has excellent conductivity, super hardness, and is light and soft. It has great application prospects in aerospace, weapons and equipment, major infrastructure, as well as new energy, new energy vehicles, energy conservation and environmental protection, and electronic information.
[0003] Research shows that graphene materials can be applied to textile fabrics because they also have excellent thermal conductivity and certain antibacterial properties. Among them, high thermal conductivity can make the fabric processed into heating fabrics and applied to human protection products used in some specific environments, while antibacterial properties can increase the antibacterial and deodorizing properties of the fabrics. However, the existing heating-type graphene fabrics with antibacterial properties encountered a technical difficulty during the research and development process, that is, after multiple wearing and use, the thermal conductivity and antibacterial properties of the graphene fabric will be significantly reduced. The reason for this is that the wearing process has a certain impact on the structure and distribution of graphene, thereby reducing its thermal conductivity and antibacterial effects. Summary of the invention
[0004] The object of the present invention is to provide a method for preparing a heating type graphene fabric, which solves the problem that the thermal conductivity and antibacterial properties of the existing heating type graphene fabric are significantly reduced after being worn and used for many times.
[0005] The present invention achieves the above-mentioned purpose through the following technical solutions:
[0006] A method for preparing a heated graphene fabric, comprising the steps of:
[0007] S1. Preparing a base fabric layer: blending cotton fiber and bamboo fiber to obtain a base fabric layer;
[0008] S2, preparing an electric heating layer: preparing graphene oxide fiber, using N-aminoethyl-3-aminopropylmethyldimethoxysilane to perform surface grafting modification treatment on it, and then soaking it with a strychnos nux vomica extract, taking the treated graphene oxide fiber and cotton fiber to blend to obtain a graphene fiber layer, and then taking a double-layer graphene fiber layer and laying an electric heating wire mesh in the interlayer to obtain an electric heating layer;
[0009] S3, preparing a heat-insulating protective layer: taking polyester fiber, nylon fiber and glass fiber and blending them to obtain a heat-insulating protective layer;
[0010] S4, taking the prepared base fabric layer, electric heating layer, and heat-insulating protective layer and bonding them in sequence to obtain the heating type graphene fabric.
[0011] A further improvement is that the mass ratio of cotton fiber to bamboo fiber in the base fabric layer is 1-3:1.
[0012] A further improvement is that the specific operation of preparing graphene oxide fibers is:
[0013] Preparing a spinning solution: taking a graphene oxide solution, adjusting the pH to 6-10, and obtaining a spinning solution;
[0014] Preparing raw fibers: taking the spinning solution through a 0.5-1 mm spinneret and injecting it into a coagulation bath at a speed of 0.2-1 mL / min, and then drying to obtain raw fibers;
[0015] Stretching and shaping: placing the original fiber in a protective atmosphere furnace, controlling the temperature to 200-400° C., and applying tension to the original fiber to make the fiber length stretching rate 28-32%;
[0016] Reduction: Take the original fibers after stretching and shaping, place them in a reducing agent for reduction for 1-5 hours, wash and dry to obtain graphene oxide fibers.
[0017] A further improvement is that the reducing agent is selected from one of hydrazine hydrate, hydrobromic acid, sodium borohydride or hydroiodic acid.
[0018] A further improvement is that the specific operation of the surface grafting modification treatment is: dispersing N-aminoethyl-3-aminopropylmethyldimethoxysilane in 4-8 times the mass of ethanol to obtain a dispersion, then immersing the graphene oxide fiber in the dispersion, ultrasonically oscillating for 40-60 minutes, taking out the graphene oxide fiber, washing and drying.
[0019] A further improvement is that the specific operation of the soaking treatment is: take the dried stems of the vines of the wisteria, crush them to 120-150 mesh, soak them in 70% ethanol with 15-20 times the mass for 24-48 hours, then stir and extract them at 60-70°C for 100-150 minutes, filter the residue to obtain the extract, immerse the graphene oxide fiber in the extract for 1-3 hours, take out the graphene oxide fiber, wash and dry it.
[0020] A further improvement is that the mass ratio of polyester fiber, nylon fiber and glass fiber in the heat-insulating protective layer is 0.5-4:1-2:1.
[0021] A further improvement is that the base fabric layer, the electric heating layer and the heat-insulating protective layer are bonded together by an adhesive, and the adhesive is selected from one of polyvinyl alcohol, polyacrylate, epoxy resin or carboxymethyl cellulose.
[0022] A further improvement is that the warp density of the base fabric layer is 200-250 strands / 10cm, and the weft density is 160-200 strands / 10cm, the warp density of the graphene fiber layer is 150-180 strands / 10cm, and the weft density is 150-180 strands / 10cm, and the warp density of the heat insulation protective layer is 180-220 strands / 10cm, and the weft density is 150-180 strands / 10cm.
[0023] The beneficial effects of the present invention are:
[0024] (1) The modified graphene oxide fiber of the present invention has been subjected to a surface grafting modification treatment with N-aminoethyl-3-aminopropylmethyldimethoxysilane, so that the amino group of N-aminoethyl-3-aminopropylmethyldimethoxysilane reacts with the functional groups (such as hydroxyl, carboxyl, etc.) on the fiber surface to form a stable chemical bond. At the same time, the silane group can also form a covalent bond with the carbon atoms on the fiber surface, thereby enhancing the grafting modification effect, significantly improving the fiber's binding ability, chemical stability and biocompatibility, strengthening the structure and distribution of graphene, and reducing the impact of the wearing process on the thermal conductivity of the fabric; then the fiber is soaked in a vine extract, so that a large amount of vine bioactive ingredients are infiltrated and locked into the fiber, so that the antibacterial and antioxidant properties of the fiber are significantly improved, so that the overall antibacterial effect of the fabric can still be effectively maintained after multiple wearing and use;
[0025] (2) The present invention arranges the electric heating wire in the graphene fiber layer, and utilizes its high thermal conductivity to quickly and evenly spread the heat, and transfer it inward from the base fabric layer to provide a stable heating effect. DETAILED DESCRIPTION
[0026] The present application is further described in detail below in conjunction with specific embodiments. It is necessary to point out that the following specific implementation methods are only used to further illustrate the present application and cannot be understood as limiting the scope of protection of the present application. Technical personnel in this field can make some non-essential improvements and adjustments to the present application based on the above application content.
[0027] 1. Main Materials
[0028] (1) Graphene oxide solution: 100 g of graphite powder and 50 g of sodium nitrate were placed in a glass container, and 2.3 L of concentrated sulfuric acid was slowly added to the container. The mixture was stirred in an ice bath for 2.5 h. 600 g of potassium permanganate was weighed and slowly added to the container. The temperature was maintained at no more than 20 °C and the mixture was stirred for 1 h. The ice bath was removed and the container was placed in a 35 °C water bath. The mixture was stirred for 2.5 h to obtain a dark brown paste. 4.8 L of hot water was added to the mixture and stirred. After the temperature reached 98 °C, the mixture was quickly transferred to a 98 °C hot water bath and stirred at a constant temperature for 5 min. The hot water bath was removed and the mixture was transferred to an ordinary water bath and stirred for 30 min. 1.4 L of 50 °C deionized water and 1 L of 20 °C deionized water were added to the mixture in sequence. 30% hydrogen peroxide, the reactant changes from brown to yellow, and after stirring for another 12 minutes, the reactant is taken out and filtered, and the filter cake is washed and centrifuged 3 times with 3% hydrochloric acid, and then redispersed in deionized water to obtain a brown suspension. After dialysis for 3 days, the graphene oxide solution is obtained.
[0029] (2) N-aminoethyl-3-aminopropylmethyldimethoxysilane: purchased from Nanjing Quanxi New Materials Co., Ltd.
[0030] (3) Rhizoma Dioscoreae: purchased from Qingping Medicinal Materials Market in Guangdong Province, and identified by the School of Traditional Chinese Medicine of Guangdong Pharmaceutical University as the dried vine stem of Rhizoma Dioscoreae of the subgenus Thick-discus of the genus Bauhinia in the family Fabaceae.
[0031] (4) Electric heating wire mesh: A mesh structure composed of multiple insulated electric heating wires vertically interwoven. The diameter of the heating wire is 0.5 mm. The mesh is smaller than and connected to a rechargeable power source.
[0032] 2. Implementation of the experiment
[0033] Example 1
[0034] A method for preparing a heated graphene fabric, comprising the steps of:
[0035] S1. Preparing a base fabric layer: blending cotton fiber and bamboo fiber to obtain a base fabric layer, wherein the mass ratio of the cotton fiber to the bamboo fiber is 1:1, and the warp density of the base fabric layer is 200 strands / 10 cm, and the weft density is 160 strands / 10 cm.
[0036] S2, prepare electric heating layer: prepare graphene oxide fiber, adopt N-aminoethyl-3-aminopropylmethyldimethoxysilane to carry out surface grafting modification treatment, adopt spatholobi spatholobi extract to soak it, take the treated graphene oxide fiber and cotton fiber blending (blending mass ratio 1:2) to obtain graphene fiber layer, the warp density of graphene fiber layer is 150 roots / 10cm, the weft density is 150 roots / 10cm, then take double-layer graphene fiber layer and lay electric heating wire mesh in the interlayer to obtain electric heating layer;
[0037] The specific operation of preparing graphene oxide fiber is as follows: preparing spinning solution: taking graphene oxide solution, adjusting pH to 6, and obtaining spinning solution; preparing protofibrils: taking the spinning solution through a 0.5 mm spinneret, and injecting it into a coagulation bath at a speed of 0.2 mL / min, and then drying to obtain protofibrils; stretching and shaping: taking the protofibrils and placing them in a nitrogen protective atmosphere furnace, controlling the temperature to 200° C., and applying tension to the protofibrils so that the fiber length stretching rate is 28%; reducing: taking the protofibrils after stretching and shaping, placing them in a hydrazine hydrate reducing agent for reduction for 1 h, washing and drying, and obtaining graphene oxide fiber.
[0038] The specific operation of the surface grafting modification treatment is: dispersing N-aminoethyl-3-aminopropylmethyldimethoxysilane in 4 times the mass of ethanol to obtain a dispersion, then immersing the graphene oxide fiber in the dispersion (the fiber accounts for 1 / 5 of the mass of the dispersion, the same below), ultrasonically oscillating for 40 minutes, taking out the graphene oxide fiber, washing and drying.
[0039] The specific operation of the soaking treatment is: take the dried stems of Glechoma longituba, crush them into 120 mesh, soak them in 15 times the mass of 70% ethanol for 24 hours, then stir and extract them at 60°C for 150 minutes, filter the residue to obtain the extract, immerse the graphene oxide fiber in the extract for 1 hour (the fiber accounts for 1 / 5 of the mass of the extract, the same below), take out the graphene oxide fiber, wash and dry it.
[0040] S3. Prepare a heat-insulating protective layer: blend polyester fiber, nylon fiber and glass fiber to obtain a heat-insulating protective layer, the mass ratio of polyester fiber, nylon fiber and glass fiber is 0.5:1:1, and the warp density of the heat-insulating protective layer is 180 strands / 10 cm, and the weft density is 150 strands / 10 cm.
[0041] S4. Take the prepared base fabric layer, electric heating layer, and heat-insulating protective layer and bond them in sequence to obtain the heating type graphene fabric, and use polyvinyl alcohol as the adhesive.
[0042] Example 2
[0043] A method for preparing a heated graphene fabric, comprising the steps of:
[0044] S1. Preparing a base fabric layer: blending cotton fiber and bamboo fiber to obtain a base fabric layer, wherein the mass ratio of the cotton fiber to the bamboo fiber is 2:1, and the warp density of the base fabric layer is 220 strands / 10 cm, and the weft density is 180 strands / 10 cm.
[0045] S2, prepare electric heating layer: prepare graphene oxide fiber, adopt N-aminoethyl-3-aminopropylmethyldimethoxysilane to carry out surface grafting modification treatment, adopt spatholobi spatholobi extract to soak it, take the treated graphene oxide fiber and cotton fiber blending (blending mass ratio 1:1) to obtain graphene fiber layer, the warp density of graphene fiber layer is 160 roots / 10cm, the weft density is 160 roots / 10cm, then take double-layer graphene fiber layer and lay electric heating wire mesh in the interlayer to obtain electric heating layer;
[0046] Among them, the specific operation of preparing graphene oxide fiber is as follows: preparing spinning solution: taking graphene oxide solution, adjusting pH to 8, and obtaining spinning solution; preparing protofibrils: taking the spinning solution through a 0.7mm spinneret, and injecting it into a coagulation bath at a speed of 0.6mL / min, and then drying to obtain protofibrils; stretching and shaping: taking the protofibrils and placing them in a nitrogen protective atmosphere furnace, controlling the temperature to 300°C, and applying tension to the protofibrils so that the fiber length stretching rate is 30%; reducing: taking the protofibrils after stretching and shaping, placing them in a sodium borohydride reducing agent for reduction for 3h, washing and drying, and obtaining graphene oxide fibers.
[0047] The specific operation of the surface grafting modification treatment is: dispersing N-aminoethyl-3-aminopropylmethyldimethoxysilane in 6 times the mass of ethanol to obtain a dispersion, then immersing the graphene oxide fiber in the dispersion, ultrasonically oscillating for 50 minutes, taking out the graphene oxide fiber, washing and drying.
[0048] The specific operation of the soaking treatment is: take the dried stems of Glechoma longituba, crush them into 140 mesh, soak them in 70% ethanol with 18 times the mass for 36 hours, then stir and extract them at 65°C for 120 minutes, filter the residue to obtain the extract, immerse the graphene oxide fiber in the extract for 2 hours, take out the graphene oxide fiber, wash and dry it.
[0049] S3. Prepare a heat-insulating protective layer: blend polyester fiber, nylon fiber and glass fiber to obtain a heat-insulating protective layer, the mass ratio of polyester fiber, nylon fiber and glass fiber is 2:1.5:1, and the warp density of the heat-insulating protective layer is 200 strands / 10 cm, and the weft density is 160 strands / 10 cm.
[0050] S4. The prepared base fabric layer, electric heating layer, and heat-insulating protective layer are sequentially bonded to obtain the heating type graphene fabric, and the adhesive is polyacrylate.
[0051] Example 3
[0052] A method for preparing a heated graphene fabric, comprising the steps of:
[0053] S1. Preparing a base fabric layer: blending cotton fiber and bamboo fiber to obtain a base fabric layer, wherein the mass ratio of the cotton fiber to the bamboo fiber is 3:1, and the warp density of the base fabric layer is 250 strands / 10 cm, and the weft density is 200 strands / 10 cm.
[0054] S2, prepare electric heating layer: prepare graphene oxide fiber, adopt N-aminoethyl-3-aminopropylmethyldimethoxysilane to carry out surface grafting modification treatment, adopt spatholobi spatholobi extract to soak it, take the treated graphene oxide fiber and cotton fiber blending (blending mass ratio 1:3) to obtain graphene fiber layer, the warp density of graphene fiber layer is 180 roots / 10cm, the weft density is 180 roots / 10cm, then take double-layer graphene fiber layer and lay electric heating wire mesh in the interlayer to obtain electric heating layer;
[0055] Among them, the specific operation of preparing graphene oxide fiber is as follows: preparing spinning solution: taking graphene oxide solution, adjusting pH to 10, and obtaining spinning solution; preparing protofibrils: taking the spinning solution through a 1mm spinneret, and injecting it into a coagulation bath at a speed of 1mL / min, and then drying to obtain protofibrils; stretching and shaping: taking the protofibrils and placing them in a nitrogen protective atmosphere furnace, controlling the temperature to 400°C, and applying tension to the protofibrils so that the fiber length stretching rate is 32%; reducing: taking the protofibrils after stretching and shaping, placing them in a hydrobromic acid reducing agent for reduction for 5h, washing and drying, and obtaining graphene oxide fibers.
[0056] The specific operation of the surface grafting modification treatment is: dispersing N-aminoethyl-3-aminopropylmethyldimethoxysilane in ethanol of 8 times the mass to obtain a dispersion, then immersing the graphene oxide fiber in the dispersion, ultrasonically oscillating for 60 minutes, taking out the graphene oxide fiber, washing, and drying.
[0057] The specific operation of the soaking treatment is: take the dried stems of the vines of the dragon's beard vine, crush them into 150 meshes, soak them in 70% ethanol with 20 times the mass for 48 hours, then stir and extract them at 70°C for 100 minutes, filter the residue to obtain the extract, immerse the graphene oxide fiber in the extract for 3 hours, take out the graphene oxide fiber, wash and dry it.
[0058] S3. Prepare a heat-insulating protective layer: blend polyester fiber, nylon fiber and glass fiber to obtain a heat-insulating protective layer, the mass ratio of polyester fiber, nylon fiber and glass fiber is 4:2:1, and the warp density of the heat-insulating protective layer is 220 strands / 10 cm, and the weft density is 180 strands / 10 cm.
[0059] S4. Take the prepared base fabric layer, electric heating layer, and heat-insulating protective layer and bond them in sequence to obtain the heating type graphene fabric, and the adhesive is epoxy resin.
[0060] Comparative Example 1
[0061] A method for preparing a heated graphene fabric, comprising the steps of:
[0062] S1. Preparing a base fabric layer: blending cotton fiber and bamboo fiber to obtain a base fabric layer, wherein the mass ratio of the cotton fiber to the bamboo fiber is 2:1, and the warp density of the base fabric layer is 220 strands / 10 cm, and the weft density is 180 strands / 10 cm.
[0063] S2, prepare electric heating layer: prepare graphene oxide fiber, adopt elaiocarpus sylvestris extract to soak it, take the treated graphene oxide fiber and cotton fiber blending (blending mass ratio 1: 1) to obtain a graphene fiber layer, the warp density of the graphene fiber layer is 160 / 10cm, and the weft density is 160 / 10cm, then take a double-layer graphene fiber layer and lay an electric heating wire mesh in the interlayer to obtain an electric heating layer;
[0064] Among them, the specific operation of preparing graphene oxide fiber is as follows: preparing spinning solution: taking graphene oxide solution, adjusting pH to 8, and obtaining spinning solution; preparing protofibrils: taking the spinning solution through a 0.7mm spinneret, and injecting it into a coagulation bath at a speed of 0.6mL / min, and then drying to obtain protofibrils; stretching and shaping: taking the protofibrils and placing them in a nitrogen protective atmosphere furnace, controlling the temperature to 300°C, and applying tension to the protofibrils so that the fiber length stretching rate is 30%; reducing: taking the protofibrils after stretching and shaping, placing them in a sodium borohydride reducing agent for reduction for 3h, washing and drying, and obtaining graphene oxide fibers.
[0065] The specific operation of the soaking treatment is: take the dried stems of Glechoma longituba, crush them into 140 mesh, soak them in 70% ethanol with 18 times the mass for 36 hours, then stir and extract them at 65°C for 120 minutes, filter the residue to obtain the extract, immerse the graphene oxide fiber in the extract for 2 hours, take out the graphene oxide fiber, wash and dry it.
[0066] S3. Prepare a heat-insulating protective layer: blend polyester fiber, nylon fiber and glass fiber to obtain a heat-insulating protective layer, the mass ratio of polyester fiber, nylon fiber and glass fiber is 2:1.5:1, and the warp density of the heat-insulating protective layer is 200 strands / 10 cm, and the weft density is 160 strands / 10 cm.
[0067] S4. The prepared base fabric layer, electric heating layer, and heat-insulating protective layer are sequentially bonded to obtain the heating type graphene fabric, and the adhesive is polyacrylate.
[0068] Comparative Example 2
[0069] A method for preparing a heated graphene fabric, comprising the steps of:
[0070] S1. Preparing a base fabric layer: blending cotton fiber and bamboo fiber to obtain a base fabric layer, wherein the mass ratio of the cotton fiber to the bamboo fiber is 2:1, and the warp density of the base fabric layer is 220 strands / 10 cm, and the weft density is 180 strands / 10 cm.
[0071] S2, prepare electric heating layer: prepare graphene oxide fiber, adopt N-aminoethyl-3-aminopropylmethyldimethoxysilane to carry out surface grafting modification treatment, take the treated graphene oxide fiber and cotton fiber blending (blending mass ratio 1:1) to obtain graphene fiber layer, the warp density of graphene fiber layer is 160 roots / 10cm, and the weft density is 160 roots / 10cm, then take double-layer graphene fiber layer and lay electric heating wire mesh in the interlayer to obtain electric heating layer;
[0072] Among them, the specific operation of preparing graphene oxide fiber is as follows: preparing spinning solution: taking graphene oxide solution, adjusting pH to 8, and obtaining spinning solution; preparing protofibrils: taking the spinning solution through a 0.7mm spinneret, and injecting it into a coagulation bath at a speed of 0.6mL / min, and then drying to obtain protofibrils; stretching and shaping: taking the protofibrils and placing them in a nitrogen protective atmosphere furnace, controlling the temperature to 300°C, and applying tension to the protofibrils so that the fiber length stretching rate is 30%; reducing: taking the protofibrils after stretching and shaping, placing them in a sodium borohydride reducing agent for reduction for 3h, washing and drying, and obtaining graphene oxide fibers.
[0073] The specific operation of the surface grafting modification treatment is: dispersing N-aminoethyl-3-aminopropylmethyldimethoxysilane in 6 times the mass of ethanol to obtain a dispersion, then immersing the graphene oxide fiber in the dispersion, ultrasonically oscillating for 50 minutes, taking out the graphene oxide fiber, washing and drying.
[0074] S3. Prepare a heat-insulating protective layer: blend polyester fiber, nylon fiber and glass fiber to obtain a heat-insulating protective layer, the mass ratio of polyester fiber, nylon fiber and glass fiber is 2:1.5:1, and the warp density of the heat-insulating protective layer is 200 strands / 10 cm, and the weft density is 160 strands / 10 cm.
[0075] S4. Take the prepared base fabric layer, electric heating layer, and heat-insulating protective layer and bond them in sequence to obtain the heating type graphene fabric, and the adhesive is polyacrylate.
[0076] 3. Performance Test
[0077] (1) Heating effect:
[0078] The heated graphene fabrics prepared in Examples 1-3 and Comparative Examples 1-2 were taken and cut into samples of 30 cm × 30 cm. Five positions were randomly marked on the side of the base fabric layer of each sample as temperature measuring points. After the electric heating screen was connected to the power supply for 10 seconds, the surface temperature values at the five positions were read with a thermometer, and the average temperature values and variance values at the five positions on each sample were calculated. Each sample was first curled (using a cylinder with a diameter of 5 cm, connecting one edge of the sample to the cylinder wall, pulling the other opposite edge of the sample, so that the sample was completely rolled up and attached to the surface of the cylinder and then unfolded, and the operation was repeated 1000 times), and then extruded (using a pressing plate with the same area as the sample, driving the pressing plate to press against the surface of the fabric through a driving device, controlling the pressure to 500 N, and then driving the pressing plate to separate from the fabric, and repeating the operation 1000 times), and then the average temperature value and variance of each sample were measured and calculated again in the same way, and the test results were statistically obtained in the following Tables 1-1 and 1-2.
[0079] (2) Antibacterial properties:
[0080] The heated graphene fabrics prepared in Examples 1-3 and Comparative Examples 1-2 were cut into samples of 10 cm × 10 cm. According to GB / T 20944.2-2007 "Evaluation of Antibacterial Properties of Textiles Part 2: Absorption Method", the antibacterial rate of these fabric samples was tested; each sample was first curled (using a cylinder with a diameter of 5 cm, connecting one edge of the sample to the cylinder wall, pulling the other opposite edge of the sample, so that the sample was completely rolled up and attached to the surface of the cylinder and then unfolded, and the operation was repeated 1000 times), and then squeezed (using a pressing plate with the same area as the sample, driving the pressing plate to press the surface of the fabric through a driving device, controlling the pressure to 500 N, and then driving the pressing plate to separate from the fabric, and repeating the operation 1000 times), and then the antibacterial rate of these fabric samples was tested again in the same way, and the test results were statistically obtained in the following Table 2.
[0081] IV. Results Analysis
[0082] Table 1-1: Test results of heating effect before treatment
[0083]
[0084] Table 1-2: Test results of heating effect after curling and extrusion
[0085]
[0086]
[0087] Table 2: Antibacterial rate test results
[0088]
[0089] From Table 1-1, Table 1-2 and Table 2 above, it can be seen that the temperature values of the heating graphene fabrics prepared in Examples 1-3 of the present invention at each test point in the heating test are generally high, the heat conduction is fast, and the distribution is uniform, the heating effect is outstanding, and there is no obvious downward trend after treatment; in the antibacterial test, the antibacterial rates of Examples 1-3 for three kinds of bacteria all performed well, and there was no obvious downward trend after treatment. However, since Comparative Example 1 did not undergo surface grafting modification treatment with N-aminoethyl-3-aminopropylmethyldimethoxysilane, the temperature value after treatment was generally reduced, and the distribution was uneven, the heating effect was significantly deteriorated, and the antibacterial rate was also significantly reduced. However, since Comparative Example 2 did not undergo soaking treatment with the extract of the dragon beard vine, the antibacterial rate before treatment was also reduced to a certain extent, and the antibacterial rate after treatment was further reduced. This shows that the surface grafting modification treatment with N-aminoethyl-3-aminopropylmethyldimethoxysilane and the soaking treatment with the extract of the dragon beard vine are both indispensable, and the synergistic effect can reduce the influence of wearing and use on the heating effect and antibacterial effect.
[0090] The above-mentioned embodiments only express several implementation methods of the present invention, and the description thereof is relatively specific and detailed, but it cannot be understood as limiting the scope of the present invention. It should be pointed out that, for ordinary technicians in this field, several variations and improvements can be made without departing from the concept of the present invention, which all belong to the protection scope of the present invention.
Claims
1. A method for preparing a heated graphene fabric, characterized in that the steps include: S1. preparing a base fabric layer: blending cotton fiber and bamboo fiber to obtain a base fabric layer; S2, preparing an electric heating layer: preparing graphene oxide fiber, using N-aminoethyl-3-aminopropylmethyldimethoxysilane to perform surface grafting modification treatment on it, and then soaking it with a strychnos nux vomica extract, taking the treated graphene oxide fiber and cotton fiber to blend to obtain a graphene fiber layer, and then taking a double-layer graphene fiber layer and laying an electric heating wire mesh in the interlayer to obtain an electric heating layer; S3, preparing a heat-insulating protective layer: taking polyester fiber, nylon fiber and glass fiber and blending them to obtain a heat-insulating protective layer; S4, taking the prepared base fabric layer, electric heating layer, and heat-insulating protective layer and bonding them in sequence to obtain the heating type graphene fabric.
2. The method for preparing a heated graphene fabric according to claim 1, characterized in that: The mass ratio of cotton fiber to bamboo fiber in the base fabric layer is 1-3:
1.
3. The method for preparing a heated graphene fabric according to claim 1, characterized in that: The specific operation of preparing graphene oxide fiber is as follows: Preparing a spinning solution: taking a graphene oxide solution, adjusting the pH to 6-10, and obtaining a spinning solution; Preparing raw fibers: taking the spinning solution through a 0.5-1 mm spinneret and injecting it into a coagulation bath at a speed of 0.2-1 mL / min, and then drying to obtain raw fibers; Stretching and shaping: placing the original fiber in a protective atmosphere furnace, controlling the temperature to 200-400° C., and applying tension to the original fiber to make the fiber length stretching rate 28-32%; Reduction: Take the original fibers after stretching and shaping, place them in a reducing agent for reduction for 1-5 hours, wash and dry to obtain graphene oxide fibers.
4. The method for preparing a heated graphene fabric according to claim 3, characterized in that: The reducing agent is selected from one of hydrazine hydrate, hydrobromic acid, sodium borohydride or hydroiodic acid.
5. The method for preparing a heated graphene fabric according to claim 1, characterized in that: The specific operation of the surface grafting modification treatment is: dispersing N-aminoethyl-3-aminopropylmethyldimethoxysilane in 4-8 times the mass of ethanol to obtain a dispersion, then immersing the graphene oxide fiber in the dispersion, ultrasonically oscillating for 40-60 minutes, taking out the graphene oxide fiber, washing, and drying.
6. The method for preparing a heated graphene fabric according to claim 1, characterized in that: The specific operation of the soaking treatment is: take the dried stems of Glechoma longituba, crush them into 120-150 mesh, soak them in 70% ethanol with 15-20 times the mass for 24-48 hours, then stir and extract them at 60-70°C for 100-150 minutes, filter the residue to obtain the extract, immerse the graphene oxide fiber in the extract for 1-3 hours, take out the graphene oxide fiber, wash and dry it.
7. The method for preparing a heated graphene fabric according to claim 1, characterized in that: The mass ratio of polyester fiber, nylon fiber and glass fiber in the heat insulation protective layer is 0.5-4:1-2:
1.
8. The method for preparing a heated graphene fabric according to claim 1, characterized in that: The base fabric layer, the electric heating layer and the heat-insulating protective layer are all bonded together by an adhesive, and the adhesive is selected from one of polyvinyl alcohol, polyacrylate, epoxy resin or carboxymethyl cellulose.
9. The method for preparing a heated graphene fabric according to claim 1, characterized in that: The warp density of the base fabric layer is 200-250 strands / 10cm, and the weft density is 160-200 strands / 10cm. The warp density of the graphene fiber layer is 150-180 strands / 10cm, and the weft density is 150-180 strands / 10cm. The warp density of the heat-insulating protective layer is 180-220 strands / 10cm, and the weft density is 150-180 strands / 10cm.
Citation Information
Patent Citations
Graphene electric conduction composite and preparation method thereof
CN109096752A
Durable antibacterial composite clothing fabric based on graphene
CN111705509A
Preparation method of high-performance graphene fiber and graphene fiber
CN114959948A
Antibacterial and warm-keeping graphene composite fiber fabric and preparation method thereof
CN117754930A
Graphene knitted fabric and preparation method thereof
CN118109956A
Cited By
Graphene heating garment fabric and preparation method thereof
CN119932744A
A graphene-based thermal clothing fabric and its preparation method
CN119932744B