Preparation method of high-molecular polymer all-plastic simulation wood material based on waste plastic recovery
Through the preparation process of polymer recycled materials, fixture demand and recycling problems in the production of plastic wood materials are solved, and the preparation of high-performance fully plastic simulated wood materials is realized, with environmentally friendly and circular economy characteristics and traditional woodworking usability.
Patent Information
- Application Number
- CN202411283237.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-13
- Publication Date
- 2024-11-01
AI Technical Summary
The existing plastic wood materials require special fixing or support fixtures during the production process. The construction method is different from the traditional wooden working method. Due to the addition of non-plastic substances, the recycling and recycling of materials cannot be achieved.
Using polymer recycled materials as raw materials, the preparation of polystyrene composite plastic elastomers and the preparation process of fully plastic simulated wood materials include hot press reaction, tower reactor cooling, kneading machine kneading, granulator treatment , special-shaped extruder press, temperature control mold setting and thermal transfer embossing, etc., to prepare high-performance fully plastic simulated wood materials.
It realizes the high performance of the material, pressure resistance, weight resistance, non-brittle cracking, and is recyclable and recyclable. It has the characteristics of environmental protection and emission reduction and circular economy. It can be used by traditional woodworking methods without special working methods and accessories.
Smart Images

Figure CN118879093A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to imitation wood building materials, and in particular relates to a preparation method of a high molecular polymer all-plastic imitation wood material based on recycled waste plastics. Background Art
[0002] Wood-Plastic Composites (WPC) is a new type of composite material that has been booming in recent years at home and abroad. It refers to the use of polyethylene, polypropylene and polyvinyl chloride to replace the usual resin adhesives, mixed with more than 50% of waste plant fibers such as wood powder, rice husks, straws, etc. to form new wood materials, and then produced through plastic processing processes such as extrusion, molding, injection molding, etc., to produce boards or profiles. It is mainly used in building materials, furniture, logistics packaging and other industries. The board formed by hot extrusion after mixing plastic and wood powder in a certain proportion is called extruded wood-plastic composite board. At present, all plastic wood materials on the market need to use special fixing or supporting fixtures to complete the process, and the construction methods and tools are different from traditional wood construction methods, which cannot allow users to quickly get started, and can only be used in conjunction with the installation methods of plastic wood manufacturers. In addition, after these plastic wood materials are used, because non-plastic substances such as sawdust, rice stalks, expanders, curing agents, catalysts and adhesives are added to the materials, it is impossible to recycle the plastic wood for production and use. Summary of the invention
[0003] The purpose of the present invention is to provide a preparation method of a polymer all-plastic simulated wood material based on the recycling of waste plastics. The preparation process is reasonable and the design is ingenious. The polymer recycled material is used as the raw material. The developed polymer all-plastic simulated wood material has high wood properties, good compression and weight resistance, no brittle cracking, can be recycled and reused, and is highly practical.
[0004] In order to solve the above problems, the present invention relates to a method for preparing a polymer all-plastic simulated wood material based on waste plastic recycling, comprising the following steps: (1) Preparation of polystyrene composite plastic elastomer Weigh the raw materials according to the following weight proportions: 50-60 parts of polystyrene material, 5-10 parts of polyisoprene, and 10-20 parts of polyacrylate; react all the weighed materials in an autoclave at a reaction temperature of 150-180° C. and a reaction time of 5-10 min. The reacted materials enter a tower reactor, and then enter a kneading machine for kneading after cooling to room temperature at a kneading temperature of about 110-120° C. and a kneading time of 5-8 min. The kneaded materials are then passed through a granulator to form a polystyrene composite plastic elastomer in small granules; (2) Preparation of all-plastic simulated wood materials Weigh the following raw materials in parts by weight: 80 parts of high molecular polymer recycled material and 20 parts of polystyrene composite plastic elastomer, put the high molecular polymer recycled material and the polystyrene composite plastic elastomer into a kneading machine for kneading at a temperature of 200° C. for 10-15 minutes to obtain material A; Material A is put into a special-shaped extruder for processing to obtain material B; A single screw or twin screw is used to extrude material B onto a temperature-controlled mold. The mold temperature is 200°C and the molding time is 30 seconds. After molding, the material is cooled and shaped to obtain a finished product D. A circulating water cooling system is used for cooling and shaping. The cooling temperature is 60-90°C. The finished product D is put into the heat transfer embossing equipment for embossing treatment at a temperature of 60°C. After embossing, it is cut to a fixed length to become a full plastic simulated wood product, which is then packaged and shipped after passing the inspection; Unqualified products and scraps from the preparation process are put into the crusher for processing.
[0005] Preferably, during the preparation of the polystyrene composite plastic elastomer, the raw materials are weighed according to the following weight proportions: 55 parts of polystyrene material, 8 parts of polyisoprene, and 15 parts of polyacrylate.
[0006] Compared with the prior art, the technical solution of the present invention has the following advantages: 1. The essence of the production technology of all-plastic simulated wood materials is the integration, circulation and reuse of resources. It has extremely high economic and social value and is characterized by environmental protection, emission reduction and circular economy.
[0007] 2. There are many types of high molecular polymer recycled materials (single material, such as PS, PP, HDPE, PET, PC, PA, ABS and other plastics). Compared with other plastic wood materials that only use raw materials such as HDPE, PS, PP, the production cost is very different, and the market potential is unlimited.
[0008] 3. The all-plastic simulated wood material can be used with traditional woodworking methods, without the need for additional special methods and accessories such as clamps or support frames. BRIEF DESCRIPTION OF THE DRAWINGS
[0009] Figure 1 It is a process flow chart of an embodiment.
[0010] Figure 2 It is a schematic cross-sectional view of product D. DETAILED DESCRIPTION
[0011] In order to make the technical purpose, technical solution and beneficial effects of the present invention clearer, the technical solution of the present invention is further described below in conjunction with specific embodiments.
[0012] Example 1: A method for preparing a polymer all-plastic simulated wood material based on recycled waste plastics, such as Figure 1-2 As shown, the following steps are included: (1) Preparation of polystyrene composite plastic elastomer Weigh the raw materials according to the following weight proportions: 50 parts of polystyrene material, 5 parts of polyisoprene, and 10 parts of polyacrylate; react all the weighed materials in an autoclave at a reaction temperature of 150° C. and a reaction time of 5 minutes. The reacted materials enter a tower reactor, and then enter a kneading machine for kneading after cooling to room temperature at a kneading temperature of about 110° C. and a kneading time of 5 minutes. The kneaded materials are then passed through a granulator to form small granular polystyrene composite plastic elastomer; (2) Preparation of all-plastic simulated wood materials Weigh the following raw materials in parts by weight: 80 parts of high molecular polymer recycled material and 20 parts of polystyrene composite plastic elastomer, put the high molecular polymer recycled material and the polystyrene composite plastic elastomer into a kneading machine for kneading at a temperature of 200° C. for 10-15 minutes to obtain material A; Material A is put into a special-shaped extruder for processing to obtain material B; A single screw or twin screw is used to extrude material B onto a temperature-controlled mold. The mold temperature is 200°C and the molding time is 30 seconds. After molding, the material is cooled and shaped to obtain a finished product D. The cooling and shaping process uses a circulating water cooling system at a cooling temperature of 60°C. The finished product D is put into the heat transfer embossing equipment for embossing treatment at a temperature of 60°C. After embossing, it is cut to a fixed length to become a full plastic simulated wood product, which is then packaged and shipped after passing the inspection; Unqualified products and scraps from the preparation process are put into the crusher for processing.
[0013] Embodiment 2: A method for preparing a polymer all-plastic simulated wood material based on waste plastic recycling, comprising the following steps: (1) Preparation of polystyrene composite plastic elastomer Weigh the raw materials according to the following weight proportions: 60 parts of polystyrene material, 10 parts of polyisoprene, and 20 parts of polyacrylate; react all the weighed materials in an autoclave at a reaction temperature of 180° C. and a reaction time of 10 minutes. The reacted materials enter a tower reactor, and then enter a kneading machine for kneading after cooling to room temperature at a kneading temperature of about 120° C. and a kneading time of 8 minutes. The kneaded materials are then passed through a granulator to form a polystyrene composite plastic elastomer in small granules; (2) Preparation of all-plastic simulated wood materials Weigh the following raw materials in parts by weight: 80 parts of high molecular polymer recycled material and 20 parts of polystyrene composite plastic elastomer, put the high molecular polymer recycled material and the polystyrene composite plastic elastomer into a kneading machine for kneading at a temperature of 200° C. for 15 minutes to obtain material A; Material A is put into a special-shaped extruder for processing to obtain material B; A single screw or twin screw is used to extrude material B onto a temperature-controlled mold. The mold temperature is 200°C and the molding time is 30 seconds. After molding, the material is cooled and shaped to obtain a finished product D. The cooling and shaping process uses a circulating water cooling system at a cooling temperature of 90°C. The finished product D is put into the heat transfer embossing equipment for embossing treatment at a temperature of 60°C. After embossing, it is cut to a fixed length to become a full plastic simulated wood product, which is then packaged and shipped after passing the inspection; Unqualified products and scraps from the preparation process are put into the crusher for processing.
[0014] Embodiment 3: A method for preparing a polymer all-plastic simulated wood material based on waste plastic recycling, comprising the following steps: (1) Preparation of polystyrene composite plastic elastomer Weigh the raw materials according to the following weight proportions: 50 parts of polystyrene material, 10 parts of polyisoprene, and 10 parts of polyacrylate; react all the weighed materials in an autoclave at a reaction temperature of 180° C. and a reaction time of 5 minutes. The reacted materials enter a tower reactor, and then enter a kneading machine for kneading after cooling to room temperature at a kneading temperature of about 120° C. and a kneading time of 5 minutes. The kneaded materials are then passed through a granulator to form a polystyrene composite plastic elastomer in small granules; (2) Preparation of all-plastic simulated wood materials Weigh the following raw materials in parts by weight: 80 parts of high molecular polymer recycled material and 20 parts of polystyrene composite plastic elastomer, put the high molecular polymer recycled material and the polystyrene composite plastic elastomer into a kneading machine for kneading at a temperature of 200° C. for 15 minutes to obtain material A; Material A is put into a special-shaped extruder for processing to obtain material B; A single screw or twin screw is used to extrude material B onto a temperature-controlled mold. The mold temperature is 200°C and the molding time is 30 seconds. After molding, the material is cooled and shaped to obtain a finished product D. The cooling and shaping process uses a circulating water cooling system at a cooling temperature of 60°C. The finished product D is put into the heat transfer embossing equipment for embossing treatment at a temperature of 60°C. After embossing, it is cut to a fixed length to become a full plastic simulated wood product, which is then packaged and shipped after passing the inspection; Unqualified products and scraps from the preparation process are put into the crusher for processing.
[0015] Embodiment 4: A method for preparing a polymer all-plastic simulated wood material based on waste plastic recycling, comprising the following steps: (1) Preparation of polystyrene composite plastic elastomer The raw materials are weighed according to the following weight proportions: 55 parts of polystyrene material, 8 parts of polyisoprene, and 15 parts of polyacrylate; all the weighed materials are reacted in an autoclave at a reaction temperature of 160° C. and a reaction time of 8 minutes. The reacted materials enter a tower reactor, and then enter a kneading machine for kneading after cooling to room temperature at a kneading temperature of about 115° C. and a kneading time of 6 minutes. The kneaded materials are then passed through a granulator to form a polystyrene composite plastic elastomer in small granules; (2) Preparation of all-plastic simulated wood materials Weigh the following raw materials in parts by weight: 80 parts of high molecular polymer recycled material and 20 parts of polystyrene composite plastic elastomer, put the high molecular polymer recycled material and the polystyrene composite plastic elastomer into a kneading machine for kneading at a temperature of 200° C. for 12 minutes to obtain material A; Material A is put into a special-shaped extruder for processing to obtain material B; A single screw or twin screw is used to extrude material B onto a temperature-controlled mold. The mold temperature is 200°C and the molding time is 30 seconds. After molding, the material is cooled and shaped to obtain a finished product D. The cooling and shaping process uses a circulating water cooling system with a cooling temperature of 75°C. The finished product D is put into the heat transfer embossing equipment for embossing treatment at a temperature of 60°C. After embossing, it is cut to a fixed length to become a full plastic simulated wood product, which is then packaged and shipped after passing the inspection; Unqualified products and scraps from the preparation process are put into the crusher for processing.
[0016] Preferably, during the preparation of the polystyrene composite plastic elastomer, the raw materials are weighed according to the following weight parts: Among the above embodiments, Embodiment 4 is the best embodiment.
[0017] Finally, it should be noted that the above embodiments are only used to illustrate but not limit the technical solutions of the present invention, and any equivalent substitutions of the present invention and any modifications or partial substitutions that do not depart from the spirit and scope of the present invention should be included in the scope of protection of the claims of the present invention.
Claims
1. A method for preparing a polymer all-plastic simulated wood material based on waste plastic recycling, characterized in that: The following steps are involved: (1) Preparation of polystyrene composite plastic elastomer Weigh the raw materials according to the following weight proportions: 50-60 parts of polystyrene material, 5-10 parts of polyisoprene, and 10-20 parts of polyacrylate; react all the weighed materials in an autoclave at a reaction temperature of 150-180° C. and a reaction time of 5-10 min. The reacted materials enter a tower reactor, and then enter a kneading machine for kneading after cooling to room temperature at a kneading temperature of about 110-120° C. and a kneading time of 5-8 min. The kneaded materials are then passed through a granulator to form a polystyrene composite plastic elastomer in small granules; (2) Preparation of all-plastic simulated wood materials Weigh the following raw materials in parts by weight: 80 parts of high molecular polymer recycled material and 20 parts of polystyrene composite plastic elastomer, put the high molecular polymer recycled material and the polystyrene composite plastic elastomer into a kneading machine for kneading at a temperature of 200° C. for 10-15 minutes to obtain material A; Material A is put into a special-shaped extruder for processing to obtain material B; A single screw or twin screw is used to extrude material B onto a temperature-controlled mold. The mold temperature is 200°C and the molding time is 30 seconds. After molding, the material is cooled and shaped to obtain a finished product D. A circulating water cooling system is used for cooling and shaping. The cooling temperature is 60-90°C. The finished product D is put into the heat transfer embossing equipment for embossing treatment at a temperature of 60°C. After embossing, it is cut to a fixed length to become a full plastic simulated wood product, which is then packaged and shipped after passing the inspection; Unqualified products and scraps from the preparation process are put into the crusher for processing.
2. The method for preparing a polymer all-plastic simulated wood material based on recycling of waste plastics according to claim 1, characterized in that: During the preparation of the polystyrene composite plastic elastomer, raw materials are weighed according to the following weight proportions: 55 parts of polystyrene material, 8 parts of polyisoprene, and 15 parts of polyacrylate.