Method for improving electroplating sheet taking

By opening thin grooves on the outer wall of the seal and setting appropriate pressure and robotic parameters, the problem of wafer chip failure is solved, the success rate of wafer picking is improved and liquid leakage is avoided, and a stable electroplating chip picking process is achieved.

CN118880422APending Publication Date: 2024-11-01QULIANG ELECTRONICS CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411346204.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-26
Publication Date
2024-11-01

AI Technical Summary

Technical Problem

During the wafer removal process of electroplating in high-temperature plating solution, the vacuum effect at the connection of the lip seal is greater than the torque of the equipment's blade removal, resulting in the failure of the chip removal, and the prior art has failed to effectively solve this problem.

Method used

By opening a thin groove on the outer wall of the seal to increase the roughness, setting the pressure at the connection of the seal to 2.4PSI, using a robot to pick up the wafer, and increasing the speed of the wafer to at least 900rpm during the drying process, setting the robot to set up the robot to a pressure of 2.4PSI, using a robot to pick up the wafer, and increasing the speed of the wafer to at least 900rpm during the drying process. The torque and height thresholds are used to avoid failure of the tablet and leakage of fluid.

Benefits of technology

It effectively reduces the vacuum degree at the seal connection, improves the success rate of sheet removal, and avoids failure during the robotic sheet removal process and liquid leakage during electroplating.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118880422A_ABST
    Figure CN118880422A_ABST
Patent Text Reader

Abstract

The invention provides a method for improving electroplating wafer taking, which comprises the following steps of: providing an electroplated wafer, and positioning and fixing the wafer through a sealing element; carrying out spin-drying on the electroplated wafer so as to blow-dry the water film; setting the pressure at the connecting part of the sealing element to be 2.4 PSI so as to reduce the vacuum degree at the connecting part of the sealing element; taking the wafer through a robot arm; a thin groove is formed in the outer wall of the sealing piece so that the roughness of the connecting position of the sealing piece can be increased. The thin groove extends towards the edge of the sealing element, and the two ends of the thin groove are kept separated from the edge of the wafer, so that the roughness of the connecting part of the sealing element can be effectively improved by arranging the thin groove in the outer wall of the sealing element, and the vacuum degree of the connecting part of the sealing element can be further reduced; therefore, the condition that the manipulator fails to take the wafers in the wafer taking process can be effectively avoided.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application belongs to the technical field of wafers, and in particular, relates to a method for improving wafer extraction during electroplating. Background Art

[0002] In the prior art, wafers are electroplated in high-temperature plating solution for a long time, and a vacuum effect occurs at the contact surface of the lip seal. After the electroplating is completed, the vacuum suction at the lip seal connection is greater than the device's wafer removal torque, resulting in wafer removal failure. The wafer removal failure rate reaches 100%, causing material abnormalities.

[0003] To address the above problems, no effective solution has been proposed yet.

[0004] It should be noted that the above introduction to the technical background is only for the convenience of providing a clear and complete description of the technical solutions of the present invention and for the convenience of understanding by those skilled in the art. It cannot be considered that the above technical solutions are well known to those skilled in the art simply because these solutions are described in the background technology section of the present invention. Summary of the invention

[0005] The purpose of the present application is to provide a method for improving electroplating wafer retrieval to solve the problem of wafer retrieval failure caused by vacuum effect.

[0006] The present application provides a method for improving electroplating film taking, comprising: Providing a wafer that has been electroplated, wherein the wafer is positioned and fixed by a sealing member; The electroplated wafers are spun dry to dry the water film; The pressure at the seal connection is set to 2.4 PSI to reduce the vacuum at the seal connection; Taking the wafer by a robot; Wherein, a fine groove is opened on the outer wall of the seal to increase the roughness of the connection of the seal; the fine groove extends toward the edge of the seal, and the two ends of the fine groove are kept separated from the edge of the wafer.

[0007] Preferably, the connection of the seal is etched to form the fine groove at the connection of the seal.

[0008] Preferably, the seal is subjected to a mold opening to form the fine groove at the connection of the seal.

[0009] Preferably, in the step of "taking the wafer by a robot arm", the torque of the robot arm is set to 46N, and the threshold of the height of the robot arm is set to 3.5mm.

[0010] Preferably, the energy of the wafer exposure is set to 260+460 / -150mj.

[0011] Preferably, the thin groove is configured to be wavy.

[0012] Preferably, in the process of "spinning the electroplated wafer to dry the water film", the rotation speed of the wafer is set to at least 900 rpm.

[0013] Compared with the prior art, the present invention has the following beneficial effects: 1. The present invention can effectively improve the roughness of the sealing connection by arranging fine grooves on the outer wall of the sealing, and further reduce the vacuum degree of the sealing connection, thereby effectively avoiding the failure of the robot arm to take the film during the film taking process.

[0014] 2. The present invention can effectively prevent liquid leakage from occurring during the electroplating process of the wafer by arranging the fine groove to extend toward the edge of the seal, and keeping both ends of the fine groove separated from the edge of the seal.

[0015] 3. The present invention sets the pressure at the sealing connection to 2.4PSI, the torque of the robot to 46N, the threshold of the height of the robot to 3.5mm, the energy of wafer exposure to 260+460 / -150mj and the rotation speed of the wafer to at least 900rpm, so that the robot can remove the wafer stably. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments recorded in the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.

[0017] Figure 1 It is a flow chart of a method for improving electroplating wafer retrieval provided in an embodiment of the present application. DETAILED DESCRIPTION

[0018] In order to enable those skilled in the art to better understand the technical solutions in this application, the technical solutions in the embodiments of this application will be clearly and completely described below in conjunction with the drawings in the embodiments of this application. Obviously, the described embodiments are only part of the embodiments of this application, not all of them. Based on the embodiments in this application, all other embodiments obtained by ordinary technicians in this field without creative work should fall within the scope of protection of this application.

[0019] In the description of the present invention, it should be noted that the orientations or positional relationships indicated by the terms "upper", "middle", "lower", "inner", "outer", "front", "back", etc. are based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or component referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. The terms "first", "second", and "third" are only used for descriptive purposes and cannot be understood as indicating or implying relative importance. For those of ordinary skill in the art, the specific meanings of the above terms in the present invention can be understood according to specific circumstances. The following describes an implementation method of the present invention based on its overall structure.

[0020] Reference Figure 1 As shown, the embodiment of the present application provides a method for improving electroplating film taking, comprising: Providing a wafer that has been electroplated, wherein the wafer is positioned and fixed by a sealing member; The electroplated wafers are spun dry to dry the water film; The pressure at the seal connection is set to 2.4 PSI to reduce the vacuum at the seal connection; Taking the wafer by a robot; Wherein, a fine groove is opened on the outer wall of the seal to increase the roughness of the connection of the seal; the fine groove extends toward the edge of the seal, and the two ends of the fine groove are kept separated from the edge of the wafer.

[0021] According to the above steps, a person skilled in the art may transfer the wafer by a robot during the process of taking out the wafer after electroplating.

[0022] It is understandable that the wafer needs to be completely immersed in the high-temperature plating solution during the electroplating process. In the structure for fixing the wafer, a seal needs to be installed on the wafer, and the seal can not only fix the wafer but also position the wafer. The aforementioned seal is a commonly used component in the art, and the shape of the wafer is fixed, and the seal is contoured to the shape of the wafer.

[0023] In the process of processing the wafer, the wafer can be dried after the electroplating is completed. That is, the water film on the wafer can be blown dry during the process of drying the wafer.

[0024] In order to significantly improve the effect of blowing off the water film, those skilled in the art may increase the speed of spinning the wafer. In this embodiment, the rotation speed of the wafer during spinning may be set to at least 900 rpm.

[0025] Furthermore, those skilled in the art can set the connection of the seal, that is, reduce the pressure at the connection of the seal.

[0026] It is understandable that the pressure at the seal connection is reduced, which can reduce the vacuum at the seal connection. In this embodiment, the pressure at the seal connection can be set to 2.4PSI. Under the aforementioned set pressure, not only can the seal be maintained with good connection strength and positioning ability, but the vacuum at the seal connection can also be effectively reduced.

[0027] On the basis of the above arrangement, the outer wall of the seal may be further provided with fine grooves. It is understandable that if the connection of the seal is too smooth, it will lead to a high vacuum degree at the connection of the seal, and then the film taking failure may occur during the process of the robot taking the film.

[0028] In this embodiment, the fine grooves provided on the outer wall of the seal can effectively increase the roughness of the seal connection, thereby further reducing the vacuum degree of the seal connection, thereby effectively avoiding the failure of the robot arm to take the film during the film taking process.

[0029] In summary, technicians in this field spin-dry the wafers to blow off the water film on the wafers and reduce the pressure at the sealing connection, and then open fine grooves on the outer wall of the seal, thereby improving the robot's ability to stably remove the electroplated wafers during the wafer removal process.

[0030] In the above arrangement, the thin groove arranged by those skilled in the art extends toward the edge of the sealing member, and both ends of the thin groove remain separated from the edge of the sealing member.

[0031] The above structure can effectively prevent the wafer from leaking during the electroplating process. That is, if both ends of the fine groove extend to the edge of the seal, during the connection of the seal, the plating solution will flow into the portion where the seal is connected through the fine groove, thereby causing the wafer to leak.

[0032] In summary, on the basis of providing the fine groove to increase the roughness of the seal, the two ends of the fine groove are kept separated from the edge of the seal, thereby preventing the wafer from leaking during the electroplating process.

[0033] In one embodiment, preferably, the fine groove is configured to be wavy. The wavy fine groove can significantly increase the roughness of the connection of the sealing member, thereby further increasing the probability of successful film removal.

[0034] According to the above arrangement, a person skilled in the art can open a thin groove at the connection of the seal. In this embodiment, preferably, the connection of the seal is etched to form a thin groove at the connection of the seal. That is, a person skilled in the art can open a thin groove on the seal by etching.

[0035] It is worth noting that both ends of all the fine grooves formed by etching are kept separate from the edge of the sealing member, thereby achieving the above-mentioned situation of avoiding liquid leakage during the electroplating process of the wafer.

[0036] In an optional embodiment, preferably, the seal is molded to form a fine groove at the connection of the seal. That is, in this embodiment, the seal can be made by mold opening. The mold used for mold opening is specially configured to keep the two ends of the fine groove separated from the edge of the seal, thereby preventing the wafer from leaking during the electroplating process.

[0037] In the above-mentioned process of taking the wafer, preferably, in the step of "taking the wafer by the robot", the thresholds of the torque and height of the robot are increased. It is understandable that the torque of the robot is set to 46N. And the threshold of the height of the robot is set to 3.5mm.

[0038] In another embodiment, preferably, the energy of the wafer exposure is set to 260+460 / -150mj. That is, those skilled in the art can increase the energy of the wafer exposure to 260+460 / -150mj, which can change the contact condition of the sealing connection, so that the wafer can be stably removed when the robot takes the wafer. It can be understood that the above 260+460 / -150mj is 260-150mj~260+460mj.

[0039] Although different specific embodiments are mentioned in the content of this application, this application is not limited to the situations described in the industry standards or embodiments, etc. Some industry standards or slightly modified implementation plans based on the implementation of the custom methods or embodiments can also achieve the same, equivalent or similar, or predictable implementation effects after deformation of the above embodiments. The embodiments of data acquisition, processing, output, judgment methods, etc. after these modifications or deformations can still fall within the scope of the optional implementation plans of this application.

Claims

1. A method for improving electroplating film taking, characterized in that: include: Providing a wafer that has been electroplated, wherein the wafer is positioned and fixed by a sealing member; The electroplated wafers are spun dry to dry the water film; The pressure at the seal connection is set to 2.4 PSI to reduce the vacuum at the seal connection; Taking the wafer by a robot; Wherein, a fine groove is opened on the outer wall of the seal to increase the roughness of the connection of the seal; the fine groove extends toward the edge of the seal, and the two ends of the fine groove are kept separated from the edge of the wafer.

2. The method for improving electroplating film taking according to claim 1, characterized in that: The seal connection is etched to form the fine groove at the seal connection.

3. The method for improving electroplating film taking according to claim 1, characterized in that: The seal is molded to form the fine groove at the connection of the seal.

4. The method for improving electroplating film taking according to claim 1, characterized in that: In the step of "taking the wafer by a robot arm", the torque of the robot arm is set to 46N, and the threshold of the height of the robot arm is set to 3.5mm.

5. The method for improving electroplating film taking according to claim 1, characterized in that: The energy of the wafer exposure is set to 260-150mj~260+460mj.

6. The method for improving electroplating film taking according to claim 1, characterized in that: The thin grooves are arranged in a wave shape.

7. The method for improving electroplating film extraction according to claim 1, characterized in that: In the process of "spinning the electroplated wafer to dry the water film", the rotation speed of the wafer is set to at least 900 rpm.