Casting pouring equipment and pouring method for engine cylinder block
By automatically adding anti-adhesive agent in the cylinder block casting equipment of automobile engines, and using water to absorb heat to maintain lubricity, the problem of leakage and disassembly of mold joint joints is solved, and higher sealing is achieved and casting quality.
Patent Information
- Application Number
- CN202410930329.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-11
- Publication Date
- 2024-11-05
AI Technical Summary
During the casting process of existing automobile engine cylinder block casting equipment, mold damage and casting quality problems due to leakage at the mold joint joints, and the lack of effective sealing measures leads to difficulty in disassembly.
A casting casting device including hydraulic cylinders and sliding tubes is designed to enhance sealing by automatically adding anti-adhesive agent at the mold connection and to maintain anti-adhesive lubricity with water absorbing heat, reducing friction and wear.
It effectively prevents metal melt leakage, protects molds and castings, simplifies the disassembly process, extends the service life of the mold, and improves the quality of castings.
Smart Images

Figure CN118893202A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of molten metal pouring, in particular to a casting pouring device and a pouring method for an engine cylinder body. Background Art
[0002] The engine block of a car is generally cast from materials such as cast iron and aluminum alloy. The key link in the casting process is the mold making of the casting. For casting the engine block of a car, first of all, it is necessary to make a corresponding mold according to the shape of the cylinder block. The mold is generally a metal mold or a sand mold. Then, liquid metal is poured into the cavity of the mold to form the shape of the cylinder block. Finally, the cylinder block is separated from the mold.
[0003] At present, in the process of using the existing automobile engine cylinder casting equipment, since the equipment directly pours the smelted molten metal into the interior of the melting furnace, when the molten metal gradually fills the mold, the melting furnace is closed, the injection of molten metal into the mold is stopped, and the upper mold is used to cover the lower mold to complete the sealing, and then the mold is left to stand and wait for the molten metal to cool down. Since the mold is assembled from an upper mold and a lower mold, there will be a slight connection seam between the upper mold and the lower mold during the pouring process. At this time, the molten metal will penetrate into the connection seam between the upper mold and the lower mold, and then when the molten metal cools at the connection seam, it will cause the upper mold and the lower mold to be connected together, resulting in the need to forcibly remove the upper mold and the lower mold, which may cause damage to the mold itself, and may also cause damage to the cast cylinder.
[0004] To this end, the present invention provides a casting pouring device and a casting method for an engine cylinder block. Summary of the invention
[0005] In order to make up for the deficiencies of the prior art, at least one technical problem raised in the background technology is solved.
[0006] The technical solution adopted by the present invention to solve its technical problems is as follows: a casting pouring equipment for an engine cylinder block described in the present invention comprises a workbench, a melting box is fixedly connected to one side of the workbench, a positioning box is fixedly connected to the upper surface of the workbench, a mold is fixedly connected to the positioning box, a discharge port is provided on one side of the melting box, and a discharge pipe is fixedly connected to the position of the melting box corresponding to the discharge port; a first guide rail is fixedly connected to the top wall of the workbench, two guide blocks are slidably connected in the first guide rail, a first hydraulic cylinder is fixedly connected to the lower surface of one of the guide blocks, a blanking frame is fixedly connected to the output end of the first hydraulic cylinder, and a plurality of fixing holes are provided on the lower surface of the blanking frame; a second hydraulic cylinder is fixedly connected to the lower surface of the other guide block, and a fixed box is fixedly connected to the output end of the second hydraulic cylinder; a first cavity is provided in the fixed box, an anti-sticking agent is installed in the first cavity, a plurality of rotating plates are rotatably provided on the bottom wall of the first cavity, a first slot body is provided in the fixed box corresponding to the position of each rotating plate, a sliding pipe is slidably connected in the first slot body, and a sealing groove is provided on the upper surface of the mold.
[0007] Preferably, sliding grooves are provided on both sides of the first groove body, and a sliding block is fixedly connected to a position of the sliding tube corresponding to each second sliding groove.
[0008] Preferably, a plurality of limiting rings are fixedly connected to the upper surface of the mold, a limiting groove is provided on the surface of each limiting ring, and a positioning ring is fixedly connected to the bottom end of each sliding tube, and the positioning ring is plugged into the limiting ring.
[0009] Preferably, a second cavity is provided between the fixed box and the first cavity, the second cavity is used to store water, and the partition between the first cavity and the second cavity is a copper partition.
[0010] Preferably, a protective plate is fixedly connected to one side of the blanking frame close to the first hydraulic cylinder, and the cross-section of the blanking frame is larger than the discharge pipe.
[0011] Preferably, a first collecting frame is provided on the upper surface of the workbench, the first collecting frame is located directly below the unloading frame, and a second collecting frame is provided directly below the fixed box.
[0012] Preferably, the outer wall of the fixed box corresponding to the second cavity is threadedly connected to two rotating covers, and the outer wall of the fixed box corresponding to the first cavity is threadedly connected to one rotating cover.
[0013] A casting method for an engine cylinder block, the specific steps comprising:
[0014] Step 1: Raw material preparation: The raw materials for smelting are mainly metal materials, such as iron, copper and aluminum. Prepare iron, copper and aluminum, and then crush, screen and dry these materials to ensure the smooth progress of smelting;
[0015] Step 2: Smelting and pretreatment: Put the raw materials into the smelting furnace for smelting, and add a pretreatment agent to the molten iron after smelting to improve the performance of the molten iron;
[0016] Step 3: Pouring: First, start the guide block to move along the first guide rail, and the guide block can drive the first hydraulic cylinder to move toward the top of the mold. The first hydraulic cylinder will drive the blanking frame fixed to its output end to move to the bottom of the discharge pipe, and then the blanking frame will abut against the discharge pipe, and then open the discharge port on one side of the melting box, and then the molten metal in the melting box will flow into the blanking frame along the discharge pipe, and then the molten metal will be injected into the mold through the funnel-shaped blanking frame. When the molten metal is injected to the specified height, stop adding the molten metal, and then make the guide The guide block drives the first hydraulic cylinder to move to the top of the first collection frame for subsequent cleaning, and then another guide block is started to drive the second hydraulic cylinder on its lower surface to move to the top of the mold. The guide block drives the second hydraulic cylinder and at the same time drives the fixed box on the lower surface of the second hydraulic cylinder to move to the top of the mold. Then the second hydraulic cylinder is started to drive the fixed box at its output end to abut and seal against the mold, and then the anti-sticking agent in the fixed box is released to increase the sealing between the mold and the fixed box. Finally, it solidifies to form a casting, and then the casting is taken out to obtain a rough engine cylinder block casting.
[0017] Preferably, the smelting and pretreatment are specifically as follows: first, the metal materials iron, copper and aluminum are loaded into a heating furnace to melt the iron, copper and aluminum, and then flux coke is added. Coke can accelerate the melting speed and reduce the furnace temperature. Silicon nitride is added to reduce the melting point of the metal. Then coal powder is added to reduce the burning of the ore, reduce environmental pressure, and help reduce defects such as pores and shrinkage.
[0018] Preferably, the casting is removed by starting the second hydraulic cylinder to move the fixed box upward after the molten metal in the mold has cooled down, thereby separating the fixed box from the casting, and then taking the casting out of the mold, and then performing heat treatment, cleaning, cutting and grinding processes to improve the quality of the casting cylinder body.
[0019] The beneficial effects of the present invention are as follows:
[0020] 1. The casting pouring equipment and pouring method for an engine cylinder block described in the present invention, during the downward movement of the fixed box, the sliding tube slidingly arranged on the lower surface of the fixed box will abut against the sealing groove on the upper surface of the mold, and then the sliding tube will slide upward along the first groove body to push several rotating plates on the bottom wall of the first cavity. The rotation of the rotating plate will cause the anti-sticking agent in the first cavity to flow into the sliding tube, and flow along the sliding cavity inside the sliding tube to the sealing groove on the surface of the mold, and then the gradual upward movement of the sliding tube will finally abut against the top wall of the first cavity, at which time the anti-sticking agent cannot continue to flow out, and the fixed box is also completely abutted against the mold. By releasing the anti-sticking agent in the fixed box, the sealing between the mold and the fixed box is increased, thereby achieving protection of the fixed box and the mold, and making disassembly more convenient. Finally, a casting is formed after cooling and solidification, and then the casting is taken out to obtain a rough engine cylinder block casting.
[0021] 2. The present invention relates to a casting equipment and method for an engine cylinder block. A second cavity is provided between the first cavity and the fixed box inside the fixed box. A certain amount of water is stored in the second cavity. The bottom plate of the fixed box and the partition between the first cavity and the second cavity are all copper plates. Therefore, when the fixed box seals the mold, the gradually released heat will be absorbed by the water in the second cavity. Since the temperature gradually increases, the temperature of the water will rise to a higher temperature. Then the heat of the water will be conducted to the anti-sticking agent, so that the anti-sticking agent can maintain lubricity, because the lubricity of the anti-sticking agent can reduce the friction and wear of the mold during the pouring process and extend the service life of the mold. If the paste lacks lubricity, it may cause the mold to stick or generate resistance during the pouring process, affecting the smooth progress of the pouring process and the quality of the casting. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] The present invention will be further described below in conjunction with the accompanying drawings.
[0023] Figure 1 is a three-dimensional diagram of the first embodiment of the present invention;
[0024] Figure 2 It is a front view of the main body of the present invention;
[0025] Figure 3 is a bottom view of the main body of the present invention;
[0026] Figure 4 is a schematic structural diagram of the first guide rail of the present invention;
[0027] Figure 5 It is a structural schematic diagram of the raw material ore of the present invention;
[0028] Figure 6 is a cross-sectional view of a fixed box of the present invention;
[0029] Figure 7The present invention Figure 6 The enlarged view of point A in the middle;
[0030] Figure 8 It is a schematic diagram of the internal structure of the fixed box of the present invention;
[0031] Fig. 9 It is a structural schematic diagram of the mold of the present invention;
[0032] In the figure: 1, workbench; 11, first guide rail; 12, guide block; 13, first hydraulic cylinder; 14, second hydraulic cylinder; 15, blanking frame; 16, protective plate; 17, fixed box; 18, first cavity; 19, second cavity; 110, rotating plate; 111, first trough; 112, slide groove; 113, sliding tube; 114, slider; 115, positioning ring; 116, fixing hole; 117, limiting ring; 118, limiting groove; 119, sealing groove; 120, rotating cover;
[0033] 2. Melting box; 21. Discharge port; 22. Discharge pipe;
[0034] 3. Positioning box; 31. Mould;
[0035] 4. The first collection box;
[0036] 5. The second collection box. DETAILED DESCRIPTION
[0037] In order to make the technical means, creative features, objectives and effects achieved by the present invention easy to understand, the present invention is further explained below in conjunction with specific implementation methods.
[0038] Embodiment 1
[0039] like Figures 1 to 9As shown, a casting pouring device for an engine cylinder block according to an embodiment of the present invention comprises a workbench 1, a melting box 2 is fixedly connected to one side of the workbench 1, a positioning box 3 is fixedly connected to the upper surface of the workbench 1, a mold 31 is fixedly connected to the positioning box 3, a discharge port 21 is opened on one side of the melting box 2, and a discharge pipe 22 is fixedly connected to the position of the melting box 2 corresponding to the discharge port 21; a first guide rail 11 is fixedly connected to the top wall of the workbench 1, two guide blocks 12 are slidably connected in the first guide rail 11, a first hydraulic cylinder 13 is fixedly connected to the lower surface of one of the guide blocks 12, and the output end of the first hydraulic cylinder 13 is fixedly connected to A blanking frame 15 is provided with a plurality of fixing holes 116 on its lower surface; a second hydraulic cylinder 14 is fixedly connected to the lower surface of another guide block 12, and a fixed box 17 is fixedly connected to the output end of the second hydraulic cylinder 14; a first cavity 18 is provided in the fixed box 17, and an anti-sticking agent is contained in the first cavity 18, and a plurality of rotating plates 110 are rotatably provided on the bottom wall of the first cavity 18, and a first groove 111 is provided in the fixed box 17 corresponding to the position of each rotating plate 110, and a sliding tube 113 is slidably connected in the first groove 111, and a sealing groove 119 is provided on the upper surface of the mold 31.
[0040] Specifically, in the process of using the existing automobile engine cylinder casting equipment, since the equipment directly pours the smelted molten metal into the interior of the molten metal furnace, when the molten metal gradually fills the mold 31, the smelting furnace is closed, the injection of molten metal into the mold 31 is stopped, and the upper mold 31 is used to cover the lower mold 31 to complete the sealing, and then the mold 31 is left to stand and wait for the molten metal to cool down. Since the mold 31 is assembled from the upper mold 31 and the lower mold 31, during the pouring process, there will be a slight connection seam between the upper mold 31 and the lower mold 31. At this time, the molten metal will penetrate into the connection seam between the upper mold 31 and the lower mold 31, and then when the molten metal cools at the connection seam, it will cause the upper mold 31 and the lower mold 31 to be connected together, resulting in the need to forcibly remove the upper mold 31 and the lower mold 31, which may cause damage to the mold 31 itself, and may also cause damage to the cast cylinder body;
[0041] Therefore, the present invention solves this problem by automatically adding an anti-sticking agent at the sealing part. First, the guide block 12 at the top of the workbench 1 is started to move along the first guide rail 11, and the guide block 12 can drive the first hydraulic cylinder 13 to move directly above the mold 31. The first hydraulic cylinder 13 will drive the blanking frame 15 fixed to its output end to move to the bottom of the discharge pipe 22, and then the blanking frame 15 will abut against the discharge pipe 22, and then open the discharge port 21 on one side of the melting box 2, and then the molten metal in the melting box 2 will flow into the blanking frame 15 along the discharge pipe 22. Then, the molten metal is injected into the mold 31 through the funnel-shaped blanking frame 15. Because a plurality of through fixing holes 116 are provided on the lower surface of the blanking frame 15, when the molten metal is injected into the mold 31 to a specified height, the injection of the molten metal is stopped, and then the guide block 12 drives the first hydraulic cylinder 13 and the blanking frame 15 to move to one side of the mold 31, and then another guide block 12 is started to drive the second hydraulic cylinder 14 on its lower surface to move to the top of the mold 31. When the guide block 12 drives the second hydraulic cylinder 14, it also drives the second hydraulic cylinder 13 to move to the lower surface of the mold 31. The fixed box 17 on the lower surface of the cylinder 14 moves to the top of the mold 31, and then the second hydraulic cylinder 14 is started to drive the fixed box 17 at its output end to abut and seal with the mold 31. During the downward movement of the fixed box 17, the sliding tube 113 slidingly arranged on the lower surface of the fixed box 17 will abut with the sealing groove 119 on the upper surface of the mold 31, and then the sliding tube 113 will slide upward along the first groove body 111 to push the several rotating plates 110 on the bottom wall of the first cavity 18. The rotation of the rotating plate 110 will cause the anti-sticking agent in the first cavity 18 to flow into the sliding tube 113, and along the The sliding cavity inside the sliding tube 113 flows into the sealing groove 119 on the surface of the mold 31, and then the sliding tube 113 gradually moves upward and finally abuts against the top wall of the first cavity 18. At this time, the anti-adhesive agent cannot continue to flow out. At this time, the fixed box 17 is also completely abutted against the mold 31. By releasing the anti-adhesive agent in the fixed box 17, the sealing between the mold 31 and the fixed box 17 is increased, and the protection of the fixed box 17 and the mold 31 is achieved. It is also more convenient to disassemble. Finally, after cooling and solidification, a casting is formed. Then, the casting is taken out to obtain a rough engine cylinder casting.
[0042] The problem that during the pouring process, there will be a slight connection gap between the upper mold 31 and the lower mold 31, and the molten metal will penetrate into the connection gap between the upper mold 31 and the lower mold 31. Then, when the molten metal cools down at the connection gap, the upper mold 31 and the lower mold 31 will be connected together, which will require the upper mold 31 and the lower mold 31 to be forcibly removed, which may cause damage to the mold 31 itself and may also cause damage to the cast cylinder.
[0043] like Figure 4As shown, in this embodiment, two sides of the first slot body 111 are provided with sliding grooves 112 , and a sliding block 114 is fixedly connected to the position of the sliding tube 113 corresponding to each second sliding groove 112 .
[0044] Specifically, when the sliding tube 113 slides along the first groove body 111, sliders 114 are fixedly connected to both sides of the sliding tube 113, and then sliding grooves 112 are opened in the first groove body 111 at positions corresponding to the sliders 114. The sliding tube 113 can stably slide upward along the first groove body 111 through the sliders 114, thereby achieving the effect of allowing the anti-sticking agent to stably flow out of the sliding tube 113.
[0045] like Figure 4 As shown, a plurality of limit rings 117 are fixedly connected to the upper surface of the mold 31 of this embodiment, and a limit groove 118 is provided on the surface of each limit ring 117. A positioning ring 115 is fixedly connected to the bottom end of each sliding tube 113, and the positioning ring 115 is plugged into the limit ring 117.
[0046] Specifically, when the sliding tube 113 abuts against the mold 31, the positioning ring 115 at the bottom end of each sliding tube 113 will be inserted into the limiting ring 117 on the upper surface of the mold 31. Then, after the anti-sticking agent flows into the sliding tube 113, it will not flow out of the limiting ring 117, but will flow along the limiting ring 117 to the sealing groove 119 on the upper surface of the mold 31, thereby preventing the anti-sticking agent from flowing out and saving the anti-sticking agent.
[0047] Embodiment 2
[0048] like Figures 2 to 9 As shown, in contrast to Example 1, another embodiment of the present invention is that a second cavity 19 is provided between the fixed box 17 and the first cavity 18, the second cavity 19 is used to store water, and the partition between the first cavity 18 and the second cavity 19 is a copper partition.
[0049] Specifically, inside the fixed box 17, a second cavity 19 is opened between the first cavity 18 and the fixed box 17, and a certain amount of water is stored in the second cavity 19. Then the bottom plate of the fixed box 17 and the partition between the first cavity 18 and the second cavity 19 are all copper plates. Therefore, when the fixed box 17 seals the mold 31, the gradually released heat will be absorbed by the water in the second cavity 19. Due to the gradually higher temperature, the temperature of the water will rise to a higher temperature, and then the heat of the water will be conducted to the anti-sticking agent, so that the anti-sticking agent can maintain lubricity, because the lubricity of the anti-sticking agent can reduce the friction and wear of the mold 31 during the pouring process, and extend the service life of the mold 31. If the paste lacks lubricity, it may cause the mold 31 to stick or generate resistance during the pouring process, affecting the smooth progress of the pouring process and the quality of the casting.
[0050] like Figure 4 As shown, in this embodiment, a protective plate 16 is fixedly connected to one side of the blanking frame 15 close to the first hydraulic cylinder 13 , and the cross-section of the blanking frame 15 is larger than the discharge pipe 22 .
[0051] Specifically, when using the blanking frame 15 for unloading, a protective plate 16 is fixedly connected to one side of the blanking frame 15 to prevent the metal liquid from splashing onto the first hydraulic cylinder 13 and affecting the operation of the first hydraulic cylinder 13, and the blanking frame 15 is set larger than the discharge pipe 22, so that unloading can be carried out better.
[0052] like Figure 2 As shown, a first collecting frame 4 is disposed on the upper surface of the workbench 1 of this embodiment. The first collecting frame 4 is located directly below the blanking frame 15 , and a second collecting frame 5 is disposed directly below the fixed box 17 .
[0053] Specifically, after the pouring of the cylinder casting is completed, when the blanking frame 15 and the mold 31 need to be cleaned, the blanking frame 15 is moved to the top of the first collecting frame 4, and then the blanking frame 15 is rinsed with water. There is no need to disassemble the blanking frame 15 for flushing, which achieves a more convenient effect. At the same time, the anti-sticking agent attached to the surface of the sliding tube 113 and the positioning ring 115 can also be cleaned, and the cleaned sewage is collected by the second collecting frame 5.
[0054] like Figure 4 As shown, in this embodiment, the outer wall of the fixed box 17 corresponding to the second cavity 19 is threadedly connected to two rotating covers 120 , and the outer wall of the fixed box 17 corresponding to the first cavity 18 is threadedly connected to one rotating cover 120 .
[0055] Specifically, by threading a rotating cover 120 at the position of the fixed box 17 corresponding to the first cavity 18, the effect of facilitating the addition of anti-sticking agent into the first cavity 18 is achieved. At the same time, the fixed box 17 is threadedly connected to two rotating covers 120 at the outer wall corresponding to the second cavity 19, and one of the rotating covers 120 is higher than the other rotating cover 120. One of the rotating covers 120 is used for adding water, and the other rotating cover 120 is used for taking the heated water in the second cavity 19. Hot water can be used to clean the positioning ring 115 or the blanking frame 15, and hot water can more effectively remove the anti-sticking agent on the surface of the positioning ring 115.
[0056] A casting method for an engine cylinder block, the specific steps comprising:
[0057] Step 1: Raw material preparation: The raw materials for smelting are mainly metal materials, such as iron, copper and aluminum. Prepare iron, copper and aluminum, and then crush, screen and dry these materials to ensure the smooth progress of smelting;
[0058] Step 2: Smelting and pretreatment: Put the raw materials into the smelting furnace for smelting, and add a pretreatment agent to the molten iron after smelting to improve the performance of the molten iron;
[0059] Step 3: Pouring: First, start the guide block 12 to move along the first guide rail 11, and the guide block 12 can drive the first hydraulic cylinder 13 to move toward the top of the mold 31. The first hydraulic cylinder 13 will drive the blanking frame 15 fixed to its output end to move to the bottom of the discharge pipe 22, and then the blanking frame 15 will abut against the discharge pipe 22, and then open the discharge port 21 on one side of the melting box 2, and then the molten metal in the melting box 2 will flow into the blanking frame 15 along the discharge pipe 22, and then the molten metal will be injected into the mold 31 through the funnel-shaped blanking frame 15. When the molten metal is injected to the specified height, stop adding the molten metal, and then make the guide The guide block 12 drives the first hydraulic cylinder 13 to move to the top of the first collecting frame 4 for subsequent cleaning, and then another guide block 12 is started to drive the second hydraulic cylinder 14 on its lower surface to move to the top of the mold 31. The guide block 12 drives the second hydraulic cylinder 14 and at the same time drives the fixed box 17 on the lower surface of the second hydraulic cylinder 14 to move to the top of the mold 31. Then the second hydraulic cylinder 14 is started to drive the fixed box 17 at its output end to abut and seal with the mold 31, and then the anti-sticking agent in the fixed box 17 is released to increase the sealing between the mold 31 and the fixed box 17. Finally, it solidifies to form a casting, and then the casting is taken out to obtain a rough engine cylinder block casting.
[0060] The specific smelting and pretreatment are as follows: first, the metal materials iron, copper and aluminum are loaded into the heating furnace. After the iron, copper and aluminum are melted, flux coke is added. Coke can speed up the melting speed and lower the furnace temperature. Silicon nitride is added to lower the melting point of the metal. Then coal powder is added to reduce the burning of the ore, reduce environmental pressure, and help reduce defects such as pores and shrinkage.
[0061] Specifically, when the molten metal in the mold 31 is cooled, the second hydraulic cylinder 14 is started to drive the fixed box 17 to move upward, so that the fixed box 17 is separated from the casting, and then the casting in the mold 31 is taken out, and then heat treatment, cleaning, cutting and grinding processes are carried out to improve the quality of the casting cylinder body.
[0062] Working principle: first, start the guide block 12 on the top of the workbench 1 to move along the first guide rail 11, and the guide block 12 can drive the first hydraulic cylinder 13 to move toward the top of the mold 31. The first hydraulic cylinder 13 will drive the blanking frame 15 fixed to its output end to move to the bottom of the discharge pipe 22, and then the blanking frame 15 will abut against the discharge pipe 22, and then open the discharge port 21 on one side of the melting box 2, and then the molten metal in the melting box 2 will flow into the blanking frame 15 along the discharge pipe 22, and then the molten metal will be injected into the mold 31 through the funnel-shaped blanking frame 15, because a plurality of penetrating fixing holes 116 are opened on the lower surface of the blanking frame 15;
[0063] When the molten metal is injected into the mold 31 to a specified height, the injection of the molten metal is stopped, and then the guide block 12 drives the first hydraulic cylinder 13 and the blanking frame 15 to move to one side of the mold 31, and then another guide block 12 is started to drive the second hydraulic cylinder 14 on its lower surface to move to just above the mold 31. When the guide block 12 drives the second hydraulic cylinder 14, it also drives the fixed box 17 on the lower surface of the second hydraulic cylinder 14 to move to just above the mold 31, and then the second hydraulic cylinder 14 is started to drive the fixed box 17 at its output end to abut against the mold 31 for sealing;
[0064] When the fixed box 17 moves downward, the sliding tube 113 slidingly arranged on the lower surface of the fixed box 17 will abut against the sealing groove 119 on the upper surface of the mold 31. When the sliding tube 113 abuts against the mold 31, the positioning ring 115 at the bottom end of each sliding tube 113 will be inserted into the limiting ring 117 on the upper surface of the mold 31, and then the sliding tube 113 will slide upward along the first groove body 111 to push the several rotating plates 110 on the bottom wall of the first cavity 18. When the sliding tube 113 slides along the first groove body 111, the sliding blocks 114 are fixedly connected to both sides of the sliding tube 113, and the sliding grooves 112 are opened at the positions corresponding to the sliding blocks 114 in the first groove body 111. The sliding tube 113 can stably slide upward along the first groove body 111 through the sliding blocks 114, so that the anti-sticking agent can stably flow out of the sliding tube 113.
[0065] Then, the rotation of the rotating plate 110 causes the anti-adhesive in the first cavity 18 to flow into the sliding tube 113, and flows along the sliding cavity inside the sliding tube 113 to the sealing groove 119 on the surface of the mold 31. Then, the sliding tube 113 gradually moves upward and finally abuts against the top wall of the first cavity 18. At this time, the anti-adhesive cannot continue to flow out. At this time, the fixed box 17 also completely abuts against the mold 31. By releasing the anti-adhesive in the fixed box 17, the sealing between the mold 31 and the fixed box 17 is increased, so that the fixed box 17 and the mold 31 are protected, and it is more convenient to disassemble. Finally, after cooling and solidification, a casting is formed. Then, the casting is taken out to obtain a rough engine cylinder casting.
[0066] In addition, inside the fixed box 17, a second cavity 19 is opened between the first cavity 18 and the fixed box 17, and a certain amount of water is stored in the second cavity 19. Then the bottom plate of the fixed box 17 and the partition between the first cavity 18 and the second cavity 19 are all copper plates. Therefore, when the fixed box 17 seals the mold 31, the gradually released heat will be absorbed by the water in the second cavity 19. Due to the gradually higher temperature, the temperature of the water will rise to a higher temperature, and then the heat of the water will be conducted to the anti-sticking agent, so that the anti-sticking agent can maintain lubricity, because the lubricity of the anti-sticking agent can reduce the friction and wear of the mold 31 during the pouring process, and extend the service life of the mold 31. If the paste lacks lubricity, it may cause the mold 31 to stick or generate resistance during the pouring process, affecting the smooth progress of the pouring process and the quality of the casting.
[0067] The above shows and describes the basic principles, main features and advantages of the present invention. It should be understood by those skilled in the art that the present invention is not limited to the above embodiments. The above embodiments and descriptions are only for explaining the principles of the present invention. Without departing from the spirit and scope of the present invention, the present invention may have various changes and improvements, which fall within the scope of the present invention. The scope of protection of the present invention is defined by the attached claims and their equivalents.
Claims
1. A casting pouring equipment for an engine block, characterized in that: The invention comprises a workbench (1), a melting box (2) is fixedly connected to one side of the workbench (1), a positioning box (3) is fixedly connected to the upper surface of the workbench (1), a mold (31) is fixedly connected inside the positioning box (3), a discharge port (21) is opened on one side of the melting box (2), and a discharge pipe (22) is fixedly connected to the melting box (2) at a position corresponding to the discharge port (21); The top wall of the workbench (1) is fixedly connected to a first guide rail (11), two guide blocks (12) are slidably connected inside the first guide rail (11), a first hydraulic cylinder (13) is fixedly connected to the lower surface of one of the guide blocks (12), an output end of the first hydraulic cylinder (13) is fixedly connected to a blanking frame (15), and a plurality of fixing holes (116) are provided on the lower surface of the blanking frame (15); A second hydraulic cylinder (14) is fixedly connected to the lower surface of the other guide block (12), and a fixed box (17) is fixedly connected to the output end of the second hydraulic cylinder (14); A first cavity (18) is provided in the fixed box (17), and an anti-sticking agent is contained in the first cavity (18). A plurality of rotating plates (110) are rotatably provided on the bottom wall of the first cavity (18). A first groove (111) is provided in the fixed box (17) at a position corresponding to each rotating plate (110), and a sliding tube (113) is slidably connected in the first groove (111). A sealing groove (119) is provided on the upper surface of the mold (31).
2. The casting pouring equipment for an engine block according to claim 1, characterized in that: Slide grooves (112) are provided on both sides of the first groove body (111), and a sliding block (114) is fixedly connected to the position of each second slide groove (112) of the sliding tube (113).
3. The casting pouring equipment for an engine block according to claim 1, characterized in that: A plurality of limiting rings (117) are fixedly connected to the upper surface of the mold (31), and a through limiting groove (118) is provided on the surface of each limiting ring (117). A positioning ring (115) is fixedly connected to the bottom end of each sliding tube (113), and the positioning ring (115) is plugged into the limiting ring (117).
4. The casting pouring equipment for an engine block according to claim 1, characterized in that: A second cavity (19) is provided between the fixed box (17) and the first cavity (18); the second cavity (19) is used to store water; and a partition between the first cavity (18) and the second cavity (19) is a copper partition.
5. The casting pouring equipment for an engine block according to claim 1, characterized in that: A protective plate (16) is fixedly connected to one side of the material discharge frame (15) close to the first hydraulic cylinder (13), and the cross section of the material discharge frame (15) is larger than the material discharge pipe (22).
6. The casting pouring equipment for an engine block according to claim 1, characterized in that: A first collecting frame (4) is arranged on the upper surface of the workbench (1), and the first collecting frame (4) is located directly below the unloading frame (15). A second collecting frame (5) is arranged directly below the fixed box (17).
7. The casting pouring equipment for an engine block according to claim 1, characterized in that: The fixed box (17) is threadedly connected to two rotating covers (120) on the outer wall corresponding to the second cavity (19), and the fixed box (17) is threadedly connected to one rotating cover (120) on the outer wall corresponding to the first cavity (18).
8. A casting method for an engine cylinder block, characterized in that: The specific steps include: Step 1: Raw material preparation: crush, screen and dry iron, copper and aluminum to obtain raw materials; Step 2: Smelting and pretreatment: Put the raw materials into the smelting furnace for smelting, and add the pretreatment agent to the molten iron for treatment after smelting; Step 3: Pouring: First, start the guide block (12) to move along the first guide rail (11), and the guide block (12) can drive the first hydraulic cylinder (13) to move toward the top of the mold (31). The first hydraulic cylinder (13) will drive the discharge frame (15) fixed to its output end to move to the bottom of the discharge pipe (22), and then the discharge frame (15) will abut against the discharge pipe (22), and then open the discharge port (21) on one side of the melting box (2), and then the molten metal in the melting box (2) will flow into the discharge frame (15) along the discharge pipe (22), and then the molten metal will be injected into the mold (31) through the funnel-shaped discharge frame (15). When the molten metal is injected to a specified height, stop adding the molten metal, and then make the guide block (12) move to the bottom of the mold (31). The guide block (12) drives the first hydraulic cylinder (13) to move to the top of the first collecting frame (4) for subsequent cleaning, and then another guide block (12) is started to drive the second hydraulic cylinder (14) on its lower surface to move to the top of the mold (31). The guide block (12) drives the second hydraulic cylinder (14) and at the same time drives the fixed box (17) on the lower surface of the second hydraulic cylinder (14) to move to the top of the mold (31). Then the second hydraulic cylinder (14) is started to drive the fixed box (17) at its output end to abut against the mold (31) for sealing, and then the anti-sticking agent in the fixed box (17) is released to increase the sealing between the mold (31) and the fixed box (17). Finally, the casting is solidified to form a casting, and then the casting is taken out to obtain a rough engine cylinder casting.
9. A casting method for an engine cylinder block according to claim 8, characterized in that: The smelting and pretreatment are specifically as follows: first, the metal materials iron, copper and aluminum are loaded into a heating furnace to melt the iron, copper and aluminum, and then flux coke is added. Coke can accelerate the melting speed and reduce the furnace temperature. Silicon nitride is added to reduce the melting point of the metal, and then coal powder is added to reduce the burning of the ore.
10. A casting method for an engine cylinder block according to claim 8, characterized in that: Specifically, the casting is taken out by starting the second hydraulic cylinder (14) to drive the fixed box (17) to move upward after the molten metal in the mold (31) has cooled down, so that the fixed box (17) is separated from the casting, and then the casting in the mold (31) is taken out, and then heat treatment, cleaning, cutting and grinding processes are performed.