Array substrate, manufacturing method thereof and display device
Patent Information
- Application Number
- CN202380008006.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-03-03
- Publication Date
- 2024-11-05
AI Technical Summary
Traditional single-domain LCD displays have problems with low contrast, asymmetric viewing angles, and color shift. Multi-domain display technology will reduce transmittance when increasing the number of domains, and the coupling capacitance between pixel electrodes and data lines causes crosstalk, affecting liquid crystal deflection. .
Design an array substrate. By setting an electrode pattern between the data line and the pixel electrode, the electrode pattern fully covers the data line, reducing the coupling capacitance, avoiding the loss of aperture rate caused by the shielding electrode, and setting transfer electrodes and discharge lines on the same layer. Optimize the voltage difference to achieve multi-domain display effects.
It effectively improves crosstalk, improves display quality, increases aperture ratio, and achieves multi-domain display effects while ensuring transmittance, reducing the risk of static electricity accumulation.
Smart Images

Figure CN118901040A_ABST
Abstract
Description
Array substrate, manufacturing method thereof and display device Technical Field
[0001] The present disclosure relates to the field of display technology, and in particular to an array substrate, a manufacturing method thereof, and a display device. Background Art
[0002] Thin Film Transistor Liquid Crystal Displays (TFT-LCDs) feature compact size, low power consumption, high image quality, zero radiation, and portability. They have experienced rapid development in recent years, gradually replacing traditional cathode ray tube (CRT) displays and dominating the current flat-panel display market. Currently, TFT-LCDs are widely used in a variety of large, medium, and small-sized products, encompassing nearly every major electronic product in today's information society, including LCD TVs, high-definition digital TVs, computers (desktop and laptop), mobile phones, tablets, navigation systems, in-car displays, projection displays, camcorders, digital cameras, electronic watches, calculators, electronic instruments, meters, public displays, and virtual displays.
[0003] Summary of the Invention
[0004] The present disclosure provides an array substrate, a manufacturing method thereof, and a display device, and the specific solutions are as follows:
[0005] In one aspect, the present disclosure provides an array substrate, comprising:
[0006] a base substrate, the base substrate comprising a display area;
[0007] A plurality of data lines extending along a first direction and arranged along a second direction in the display area;
[0008] an electrode pattern located on a side of the layer where the plurality of data lines are located away from the base substrate, the electrode pattern being a block-shaped electrode, and an orthographic projection of at least some of the data lines on the base substrate being located within the orthographic projection of the electrode pattern on the base substrate;
[0009] Multiple pixel electrodes are located on the side of the layer where the electrode pattern is located away from the base substrate. The pixel electrodes are block electrodes. The multiple pixel electrodes are coupled to the multiple data lines. The orthographic projections of the multiple pixel electrodes on the base substrate overlap with the orthographic projections of the electrode pattern on the base substrate.
[0010] In some embodiments, in the above-mentioned array substrate provided by the embodiments of the present disclosure, the orthographic projection of the data line on the base substrate overlaps with the orthographic projection of the pixel electrode on the base substrate.
[0011] In some embodiments, the array substrate provided in the embodiments of the present disclosure further includes a plurality of pixel circuits, wherein the pixel circuits are coupled to the data lines and the pixel electrodes;
[0012] The electrode pattern includes a plurality of hollow structures, and the orthographic projections of the plurality of pixel circuits on the base substrate are located within the orthographic projections of the plurality of hollow structures on the base substrate.
[0013] In some embodiments, the above-mentioned array substrate provided in the embodiments of the present disclosure further includes a plurality of switching electrodes arranged on the same layer as the electrode pattern, the switching electrodes coupling the pixel electrodes and the pixel circuits, and the orthographic projections of the plurality of switching electrodes on the base substrate are located within the orthographic projections of the plurality of hollow structures on the base substrate.
[0014] In some embodiments, the above-mentioned array substrate provided in the embodiments of the present disclosure further includes a plurality of discharge lines arranged in the same layer as the plurality of data lines, and the discharge lines and the data lines are alternately arranged in the second direction; the pixel electrode includes a first pixel electrode and a second pixel electrode arranged side by side in the first direction, and the discharge line is coupled to the second pixel electrode through the pixel circuit.
[0015] In some embodiments, the above-mentioned array substrate provided in the embodiments of the present disclosure further includes a plurality of first voltage lines and a plurality of second voltage lines, the orthographic projection of the first voltage line on the base substrate overlaps with the orthographic projection of the first pixel electrode on the base substrate, the orthographic projection of the second voltage line on the base substrate overlaps with the orthographic projection of the second pixel electrode on the base substrate, and the plurality of first voltage lines and the plurality of second voltage lines are respectively coupled to the electrode patterns.
[0016] In some embodiments, the above-mentioned array substrate provided in the embodiments of the present disclosure further includes a plurality of gate lines extending along the second direction in the display area and arranged along the first direction, the plurality of first voltage lines and the plurality of second voltage lines are arranged in the same layer as the plurality of gate lines, and the gate lines are coupled to the pixel circuit.
[0017] In some embodiments, in the above-mentioned array substrate provided in the embodiments of the present disclosure, the pixel circuit includes a first transistor, a second transistor and a third transistor, wherein the gate of the first transistor, the gate of the second transistor and the gate of the third transistor are reused and integrated with the gate line, the first electrode of the first transistor and the first electrode of the second transistor are reused, the first electrode of the third transistor and the second electrode of the second transistor are reused and coupled to the second pixel electrode, and the second electrode of the first transistor is coupled to the first pixel electrode.
[0018] In some embodiments, in the above-mentioned array substrate provided in the embodiments of the present disclosure, the channel width-to-length ratio of the first transistor is approximately the same as the channel width-to-length ratio of the second transistor, and the channel width-to-length ratio of the first transistor is greater than the channel width-to-length ratio of the third transistor.
[0019] In some embodiments, in the above-mentioned array substrate provided by the embodiments of the present disclosure, the discharge line includes a first section overlapping with the gate line in a direction perpendicular to the base substrate, a second section overlapping with the first voltage line, and a third section overlapping with the second voltage line, wherein the line width of the first section is smaller than the line width of the second section, and the line width of the second section is approximately equal to the line width of the third section.
[0020] In some embodiments, in the array substrate provided by the embodiments of the present disclosure, the gate line includes a narrowing portion, and an orthographic projection of the narrowing portion on the base substrate overlaps with an orthographic projection of the discharge line on the base substrate.
[0021] In some embodiments, in the above-mentioned array substrate provided in the embodiments of the present disclosure, the base substrate further includes a border area located on at least one side of the display area, and the array substrate further includes a frame sealing glue area and multiple routing lines located in the border area, wherein at least part of the routing lines include a main line and multiple protruding structures located on at least one side of the main line, wherein at least one end of the area between adjacent main lines exceeds or roughly coincides with the boundary of the frame sealing glue area, and the protruding structures between adjacent main lines are staggered.
[0022] In some embodiments, in the above-mentioned array substrate provided by the embodiments of the present disclosure, in the extension direction of the area between adjacent main lines, the width of the protruding structure is greater than or equal to 6 μm and less than or equal to 20 μm, and the distance between the two staggered protruding structures is greater than or equal to 15 μm and less than or equal to 20 μm.
[0023] In some embodiments, in the above-mentioned array substrate provided in the embodiments of the present disclosure, the base substrate further includes a border area located on at least one side of the display area, and the array substrate further includes a common electrode line located in the border area, and the common electrode line includes a plurality of conductive structures arranged side by side, and a connecting line integrally arranged with the plurality of conductive structures.
[0024] In some embodiments, in the above-mentioned array substrate provided by the embodiments of the present disclosure, the ratio of the orthographic projection area of the conductive structure on the base substrate to the orthographic projection area of the pixel electrode on the base substrate is greater than or equal to 30 and less than or equal to 50.
[0025] In some embodiments, in the array substrate provided by the embodiments of the present disclosure, in the extension direction of the connecting line, the ratio of the distance between adjacent conductive structures to the size of the conductive structure is greater than or equal to 1 and less than or equal to 3.
[0026] In some embodiments, in the above-mentioned array substrate provided in the embodiments of the present disclosure, the border area includes a sealing glue area, the orthographic projections of the multiple conductive structures on the base substrate and the orthographic projections of the sealing glue area on the base substrate overlap with each other, and the orthographic projections of the connecting lines on the base substrate are located between the orthographic projections of the sealing glue area on the base substrate and the display area.
[0027] In some embodiments, the above-mentioned array substrate provided in the embodiments of the present disclosure further includes a signal line located in the border area, the orthographic projection of the signal line on the base substrate is located between the orthographic projection of the sealing glue area on the base substrate and the display area, and overlaps with the orthographic projection of the connecting line on the base substrate, and the signal line is coupled to the connecting line.
[0028] In some embodiments, the array substrate provided in the embodiments of the present disclosure further includes a plurality of gate lines located in the display area, and an insulating layer located between a layer where the plurality of gate lines are located and a layer where the plurality of pixel electrodes are located;
[0029] The signal line is provided in the same layer as the plurality of gate lines, the connection line is provided in the same layer as the plurality of pixel electrodes, and the signal line is coupled to the connection line through a via hole penetrating the insulating layer.
[0030] On the other hand, an embodiment of the present disclosure provides a method for manufacturing the array substrate, comprising:
[0031] providing a base substrate, the base substrate comprising a display area;
[0032] forming a plurality of data lines extending along a first direction and arranged along a second direction in the display area;
[0033] forming an electrode pattern covering at least a portion of the data lines on the layer where the data lines are located, wherein the electrode pattern is a block electrode;
[0034] A plurality of pixel electrodes are formed on the layer where the electrode pattern is located. The pixel electrodes are block electrodes. The plurality of pixel electrodes are coupled to the plurality of data lines. The orthographic projections of the plurality of pixel electrodes on the base substrate overlap with the orthographic projections of the electrode pattern on the base substrate.
[0035] On the other hand, an embodiment of the present disclosure provides a display device, including an array substrate and an opposing substrate arranged opposite to each other, and a liquid crystal layer located between the array substrate and the opposing substrate, the array substrate is the above-mentioned array substrate provided in the embodiment of the present disclosure, and the opposing substrate includes a common electrode. BRIEF DESCRIPTION OF THE DRAWINGS
[0036] FIG1 is a schematic diagram of an array substrate provided by an embodiment of the present disclosure;
[0037] FIG2 is an enlarged schematic diagram of the Z1 region in FIG1 ;
[0038] FIG3 is a cross-sectional view along line I-II in FIG1 ;
[0039] FIG4 is a schematic structural diagram of the layer where the gate lines are located in FIG2 ;
[0040] FIG5 is a schematic structural diagram of the active layer in FIG2 ;
[0041] FIG6 is a schematic structural diagram of the layer where the data line is located in FIG2;
[0042] FIG7 is a schematic structural diagram of the first passivation layer in FIG2 ;
[0043] FIG8 is a schematic structural diagram of the layer where the electrode pattern is located in FIG2 ;
[0044] FIG9 is a schematic structural diagram of the second passivation layer in FIG2 ;
[0045] FIG10 is a schematic structural diagram of the layer where the pixel electrode is located in FIG2 ;
[0046] FIG11 is an equivalent circuit diagram of a pixel electrode region provided by the present disclosure;
[0047] FIG12 is an enlarged schematic diagram of the Z2 area in FIG1 ;
[0048] FIG13 is an enlarged schematic diagram of the Z3 region in FIG12 ;
[0049] FIG14 is an enlarged schematic diagram of the Z4 region in FIG1 ;
[0050] FIG15 is a cross-sectional view along line III-IV in FIG14;
[0051] FIG16 is a schematic diagram of transmitting a common electrode signal according to an embodiment of the present disclosure;
[0052] FIG17 is another schematic diagram of an array substrate provided by an embodiment of the present disclosure;
[0053] FIG18 is a schematic structural diagram of a display device provided in an embodiment of the present disclosure;
[0054] FIG19 is a schematic diagram of photo-alignment in the related art;
[0055] FIG20 is a schematic diagram of four-domain orientation provided by an embodiment of the present disclosure;
[0056] FIG21 is a schematic diagram of the exposure direction in the four-domain area provided in an embodiment of the present disclosure. DETAILED DESCRIPTION
[0057] To further clarify the objectives, technical solutions, and advantages of the embodiments of the present disclosure, the technical solutions of the embodiments of the present disclosure will be described below in conjunction with the accompanying drawings. It should be noted that, to further clarify the objectives, technical solutions, and advantages of the embodiments of the present disclosure, the technical solutions of the embodiments of the present disclosure will be described below in conjunction with the accompanying drawings. It should be noted that in the accompanying drawings, the thicknesses of layers, films, panels, regions, etc. are exaggerated for clarity. Example embodiments are described in this disclosure with reference to cross-sectional views that are schematic representations of idealized embodiments. As such, deviations from the shapes of the figures as a result of, for example, manufacturing techniques and / or tolerances are to be expected. Therefore, the embodiments described in this disclosure should not be construed as limited to the specific shapes of the regions shown in this disclosure, but rather include deviations in shape resulting from, for example, manufacturing. For example, a region illustrated or described as flat may typically have rough and / or nonlinear features; sharp corners illustrated may be rounded, etc. Therefore, the regions shown in the figures are schematic in nature, and their sizes and shapes are not intended to depict the precise shapes of the regions or reflect true scale. They are intended solely to illustrate the present disclosure. The same or similar reference numerals throughout the text represent the same or similar elements or elements having the same or similar functions. In order to keep the following description of the embodiments of the present disclosure clear and concise, the present disclosure omits detailed descriptions of known functions and known components.
[0058] Unless otherwise defined, the technical or scientific terms used herein shall have the ordinary meaning understood by persons of ordinary skill in the field to which the present disclosure belongs. The words "first", "second" and similar terms used in the present disclosure and the claims do not indicate any order, quantity or importance, but are only used to distinguish different components. Words such as "include" or "comprise" mean that the elements or objects preceding the word include the elements or objects listed after the word and their equivalents, without excluding other elements or objects. Words such as "connect" or "connected" are not limited to physical or mechanical connections, but may include electrical connections, whether direct or indirect. "Inside", "outside", "upper", "lower" and the like are only used to indicate relative positional relationships. When the absolute position of the object being described changes, the relative positional relationship may also change accordingly.
[0059] In the following description, when an element or layer is referred to as being “on” or “connected to” another element or layer, the element or layer may be directly on, directly connected to, the other element or layer, or there may be intermediate elements or intermediate layers. When an element or layer is referred to as being “disposed on one side of” another element or layer, the element or layer may be directly on, directly connected to, the other element or layer, or there may be intermediate elements or intermediate layers. However, when an element or layer is referred to as being “directly on” or “directly connected to” another element or layer, there are no intermediate elements or intermediate layers. The term “and / or” includes any and all combinations of one or more of the associated listed items.
[0060] With the advancement of science and technology, traditional single-domain LCDs can no longer meet people's expectations for LCDs due to shortcomings such as low contrast, asymmetric viewing angles, and color shift when viewing the display at different angles. Multi-domain display technology has gradually developed. Multi-domain display divides a sub-pixel into different regions, with the liquid crystal in each region having different degrees of deflection. When viewing the LCD from different angles, the combined effect of the liquid crystal deflection in each region is seen. This reduces the contrast differences at different angles caused by the same deflection of all liquid crystals in the pixel, thereby reducing color shift and increasing viewing angle.
[0061] The more domains a sub-pixel has, the better it improves color shift. However, increasing the number of domains often reduces transmittance, so comprehensive considerations are required during design to maximize color shift reduction while ensuring transmittance. To effectively reduce color shift, related technologies often use 8-domain sub-pixels.
[0062] However, in the relevant 8-domain display scheme, there is a coupling capacitor Cpd between the pixel electrode and the data line. The coupling capacitor Cpd will cause electric field disorder and affect the normal deflection of the liquid crystal, resulting in crosstalk. To improve the crosstalk problem, a shielding electrode can be provided on the same layer as the pixel electrode, and the shielding electrode can cover the data line to shield the electric field disorder caused by the coupling capacitor Cpd through the shielding electrode, thereby reducing the effect of the coupling capacitor Cpd on the normal deflection of the liquid crystal. However, since at least an exposure distance needs to be retained between the pixel electrode and the shielding electrode to avoid coupling of adjacent pixel electrodes through the shielding electrode, and there is a shielding electrode between adjacent pixel electrodes, it will result in a large loss in aperture ratio; at the same time, during the process, the offset of the shielding electrode may also cause differences in the coupling capacitors Cpd of adjacent pixels, causing electric field disorder, thereby generating crosstalk and failing the shielding effect.
[0063] In order to at least improve the above technical problems existing in the related art, an embodiment of the present disclosure provides an array substrate, as shown in FIG1 to FIG3 , comprising:
[0064] A base substrate 101, the base substrate 101 includes a display area AA. Optionally, the base substrate 101 is a substrate that allows visible light to pass through, such as glass, quartz, plastic, etc.;
[0065] A plurality of data lines 102 extend in the display area AA along a first direction Y and are arranged along a second direction X. Optionally, the data lines 102 may be made of a metal such as molybdenum (Mo), aluminum (Al), titanium (Ti), chromium (Cr), or nickel (Ni). The data lines 102 may have a single-layer structure or a stacked-layer structure. For example, the data lines 102 may have a stacked-layer structure consisting of a titanium metal layer, an aluminum metal layer, and a titanium metal layer.
[0066] The electrode pattern 103 is located on a side of the layer where the multiple data lines 102 are located, away from the base substrate 101. The electrode pattern 103 is a block electrode. The orthographic projections of at least some of the data lines 102 (for example, all of the data lines 102) on the base substrate 101 are located within the orthographic projections of the electrode pattern 103 on the base substrate 101. Optionally, to ensure transmittance, the material of the electrode pattern 103 may include a transparent conductive material such as indium tin oxide (ITO) or indium zinc oxide (IZO).
[0067] A plurality of pixel electrodes 104 are located on a side of the layer where the electrode pattern 103 is located away from the base substrate 101. The pixel electrodes 104 are block electrodes. The plurality of pixel electrodes 104 are coupled to a plurality of data lines 102 (for example, each column of pixel electrodes 104 is coupled to a corresponding data line 102). The orthographic projections of the plurality of pixel electrodes 104 on the base substrate 101 overlap with the orthographic projections of the electrode pattern 103 on the base substrate 101. Optionally, the material of the pixel electrodes 104 includes transparent conductive materials such as indium tin oxide (ITO) and indium zinc oxide (IZO). The "coupling" in the present disclosure can be a direct electrical connection or an indirect electrical connection, for example, an electrical connection is achieved through other circuits or components (transistors, etc.). In a specific implementation, the pixel electrodes 104 are coupled to the data lines 102 through transistors.
[0068] In the above-mentioned array substrate provided in the embodiment of the present disclosure, since the electrode pattern 103 is set between the layer where the data line 102 is located and the layer where the pixel electrode 104 is located, and the electrode pattern 103 fully covers the data line 102, the phenomenon of shielding failure caused by process fluctuations will not occur, thereby effectively improving crosstalk and improving display quality.
[0069] In some embodiments, in the above-mentioned array substrate provided by the embodiment of the present disclosure, since the pixel electrode 104 and the electrode pattern 103 are arranged in different layers, there is no shielding electrode in the related art between adjacent pixel electrodes 104, so the distance between adjacent pixel electrodes 104 of the present disclosure can be reduced, thereby improving the aperture ratio. Optionally, the distance between adjacent pixel electrodes 104 can be greater than the exposure distance and less than the line width of the data line 102. In other words, the orthographic projection of the pixel electrode 104 on the base substrate 101 can overlap with the orthographic projection of the data line 102 on the base substrate 101. In addition, as can be seen from Figure 3, there are two passivation layers, namely the first passivation layer 105 and the second passivation layer 106, between the layer where the data line 102 is located and the layer where the pixel electrode 104 is located, so that the distance between the two is large and the coupling capacitance Cpd is small. Therefore, even if the orthographic projections of the two overlap, the impact on the display effect is not significant.
[0070] In some embodiments, the array substrate provided in the embodiments of the present disclosure, as shown in FIG2 , further includes a plurality of pixel circuits 107, which couple the data lines 102 and the pixel electrodes 104. Optionally, the electrode pattern 103 includes a plurality of hollow structures 1031, and the orthographic projections of the plurality of pixel circuits 107 on the base substrate 101 are located within the orthographic projections of the plurality of hollow structures 1031 on the base substrate 101. This prevents interference of the electrode pattern 103 with the pixel circuits 107, thereby ensuring the stability of the performance of the pixel circuits 107.
[0071] In some embodiments, in the above-mentioned array substrate provided in the embodiments of the present disclosure, as shown in Figures 2, 8 and 10, it may also include a plurality of transfer electrodes 108 arranged in the same layer as the electrode pattern 103, the transfer electrodes 108 couple the pixel electrodes 104 and the pixel circuit 107, and the orthographic projections of the plurality of transfer electrodes 108 on the base substrate 101 are located within the orthographic projections of the plurality of hollow structures 1031 on the base substrate 101. In the present disclosure, "same layer" refers to a layer structure formed by a single patterning process using the same film forming process to form a film layer for making a specific pattern, and then using the same mask. That is, a single patterning process corresponds to a mask (also called a photomask). Depending on the specific pattern, a single patterning process may include multiple exposure, development or etching processes, and the specific patterns in the formed layer structure may be continuous or discontinuous, and these specific patterns may be at the same height or have the same thickness, or at different heights or have different thicknesses. Based on this, by placing the transfer electrode 108, which couples the pixel electrode 104 and the pixel circuit 107, on the same layer as the electrode pattern 103, the number of masking operations can be reduced, production efficiency can be improved, and the number of film layers can be reduced, which is conducive to a thinner and lighter product design. In addition, the transfer electrode 108 is located within the hollow structure 1031 of the electrode pattern 103, preventing short circuits between the electrode pattern 103, the pixel electrode 104, and the pixel circuit 107.
[0072] In some embodiments, in the above-mentioned array substrate provided in the embodiments of the present disclosure, as shown in Figures 2, 6, 10 and 11, it can also include multiple discharge lines 109 arranged in the same layer as the multiple data lines 102. The signal of the discharge line 109 is not a fixed voltage, and the signal voltage difference between it and the data line 102 can be adjusted according to the actual required brightness and darkness effect. The greater the required brightness and darkness contrast, the greater the signal voltage difference between the discharge line 109 and the data line 102; optionally, the discharge line 109 and the data line 102 are alternately arranged in the second direction X; the pixel electrode 104 includes a first pixel electrode 1041 and a second pixel electrode 1042 arranged side by side in the first direction Y, and the discharge line 109 is coupled to the second pixel electrode 104 through the pixel circuit 107. Because the pixel circuit 107 is coupled to the first pixel electrode 1041 and the second pixel electrode 1042 at the same time, and the discharge line 109 is only coupled to the second pixel electrode 1042, the discharge effect of the discharge line 109 can make the voltage difference (Pixel-com) between the pixel voltage of the first pixel electrode 1041 and the common voltage greater than the voltage difference (Pixel-com) between the pixel voltage of the second pixel electrode 1042 and the common voltage. In this way, the brightness of the area where the first pixel electrode 1041 is located is greater than the brightness of the area where the second pixel electrode 1042 is located, thereby adopting a method of combining a smaller domain (for example, 4 domains) orientation with a voltage difference drive to achieve a liquid crystal display effect with more domains (for example, 8 domains).
[0073] In some embodiments, in the above-mentioned array substrate provided by the embodiments of the present disclosure, as shown in Figures 2, 4, 7 to 10, it may also include multiple first voltage lines 110 and multiple second voltage lines 111. The orthographic projection of the first voltage line 110 on the base substrate 101 overlaps with the orthographic projection of the first pixel electrode 1041 on the base substrate 101, and the orthographic projection of the second voltage line 111 on the base substrate 101 overlaps with the orthographic projection of the second pixel electrode 1042 on the base substrate 101. The multiple first voltage lines 110 and the multiple second voltage lines 111 are respectively coupled to the electrode pattern 103. Optionally, the first voltage line 110 is coupled to the electrode pattern 103 through a first via hole h1 penetrating the first passivation layer 105 and the gate insulating layer (GI, located between the layer where the gate line 112 is located and the layer where the data line 102 is located), and the second voltage line 111 is coupled to the electrode pattern 103 through a second via hole h2 penetrating the first passivation layer 105 and the gate insulating layer (GI). Optionally, the gate insulating layer and the passivation layer may be made of at least one inorganic insulating material such as silicon oxide, silicon nitride, or silicon oxynitride.
[0074] As can be seen from Figure 11, the electrode pattern 103 and the first pixel electrode 1041 constitute the first storage capacitor Cst1 of the bright pixel area, and the electrode pattern 103 and the second pixel electrode 1042 constitute the second storage capacitor Cst2 of the dark pixel area. The first voltage line 110 and the second voltage line 111 can be used to provide a fixed voltage, so that the first storage capacitor Cst1 is used to charge the first pixel electrode 1041 and maintain the voltage on the first pixel electrode 1041 during the period when a row of scan lines is closed, and the second storage capacitor Cst2 is used to charge the second pixel electrode 1042 and maintain the voltage on the second pixel electrode 1042 during the period when a row of scan lines is closed.
[0075] In some embodiments, the array substrate provided in the embodiments of the present disclosure, as shown in FIG2 and FIG4 , further includes a plurality of gate lines 112 extending along the second direction Y and arranged along the first direction X in the display area AA, the gate lines 112 being coupled to the pixel circuit 107; a plurality of first voltage lines 110, a plurality of second voltage lines 111, and the plurality of gate lines 112 being disposed in the same layer, the gate lines 112 being located between the first voltage lines 110 and the second voltage lines 111 overlapping the same pixel electrode 104, such that most areas of the gate lines 112 are exposed by the hollow structure 1031, thereby reducing the coupling capacitance between the gate lines 112 and the electrode pattern 103 and reducing the loading of the gate lines 112. Optionally, the material of the gate lines 112 may include metals such as molybdenum (Mo), aluminum (Al), titanium (Ti), chromium (Cr), and nickel (Ni), and the gate lines 112 may be a single-layer structure or a stacked-layer structure, for example, the gate lines 112 may be a single-layer structure composed of a molybdenum metal layer.
[0076] In some embodiments, in the above-mentioned array substrate provided by the embodiments of the present disclosure, as shown in Figures 2, 4 to 11, in order to simplify the layout of the pixel circuit 107 and reduce the non-opening area occupied by the pixel circuit 107, the pixel circuit 107 can be provided to include a first transistor T1, a second transistor T2 and a third transistor T3, wherein the gate g1 of the first transistor T1, the gate g2 of the second transistor T2 and the gate g3 of the third transistor T3 are multiplexed and integrally provided with the gate line 112, the first electrode s1 of the first transistor T1 and the first electrode s2 of the second transistor T2 are multiplexed and integrally provided with the data line 102, the first electrode s3 of the third transistor T3 and the second electrode d2 of the second transistor T2 are multiplexed, And coupled to the second pixel electrode 1042, the second electrode d1 of the first transistor T1 is coupled to the first pixel electrode 1041, and the second electrode d3 of the third transistor T3 is integrally arranged with the discharge line 109; optionally, the second electrode d1 of the first transistor T1 is coupled to the transfer electrode 108 through a third via h3 penetrating the first passivation layer 105, and the transfer electrode 108 is further coupled to the first pixel electrode 1041 through a fourth via h4 penetrating the second passivation layer 106; the first electrode S3 of the third transistor T3 is coupled to the transfer electrode 108 through a fifth via h5 penetrating the first passivation layer 105, and the transfer electrode 108 is further coupled to the second pixel electrode 1042 through a sixth via h6 penetrating the second passivation layer 106.
[0077] As can be seen from FIG11, the common electrode 201 and the first pixel electrode 1041 constitute the first liquid crystal capacitor Cpx1 of the bright pixel area, and the common electrode 201 and the second pixel electrode 1042 constitute the second liquid crystal capacitor Cpx2 of the dark pixel area. When the gate line 112 provides a scanning voltage, the data voltage from the data line 102 can be applied to the first pixel electrode 1041 and the second pixel electrode 1042 respectively through the first transistor T1 and the second transistor T2, so that the electric field between the first pixel electrode 1041 and the common electrode 201 can drive the corresponding liquid crystal molecules in the bright pixel area to rotate, and the electric field between the second pixel electrode 1042 and the common electrode 201 can drive the corresponding liquid crystal molecules in the bright pixel area to rotate. It is able to drive the corresponding liquid crystal molecules in the dark pixel area to rotate; at the same time, the third transistor T3 is turned on, and shares the data voltage from the data line 102 with the second transistor T2, thereby realizing discharge to the second pixel electrode 1042; finally, the voltage difference between the pixel voltage of the first pixel electrode 1041 and the common voltage is greater than the voltage difference between the pixel voltage of the second pixel electrode 1042 and the common voltage, so that the brightness of the area where the first pixel electrode 1041 is located is greater than the brightness of the area where the second pixel electrode 1042 is located, thereby adopting a method of combining a smaller number of domains (for example, 4 domains) with a voltage difference drive orientation to achieve a liquid crystal display effect with more domains (for example, 8 domains).
[0078] In some embodiments, in the array substrate provided by the embodiments of the present disclosure, as shown in FIG5 , considering that the first transistor T1 and the second transistor T2 are used to charge the first pixel electrode 1041 and the second pixel electrode 1042, respectively, to ensure synchronous and rapid charging of the first pixel electrode 1041 and the second pixel electrode 1042, the channel width-to-length ratio of the first transistor T1 and the channel width-to-length ratio of the second transistor T2 can be set to be substantially the same (i.e., the same or within an error range caused by factors such as manufacturing and measurement). In some embodiments, the width-to-length ratio of the active layer a1 of the first transistor T1 and the width-to-length ratio of the active layer a2 of the second transistor T2 can be made the same; the third transistor T3 is used for discharge, and it only needs to have a discharge function. Therefore, the channel width-to-length ratio of the third transistor T3 can be smaller than the channel width-to-length ratio of the first transistor T1, which can be specifically manifested as the width-to-length ratio of the active layer a3 of the third transistor T3 being smaller than the width-to-length ratio of the active layer a1 of the first transistor T1. In addition, because the channel width-to-length ratio of the third transistor T3 is small, the third transistor T3 occupies less wiring space, which is more conducive to improving the aperture ratio. Optionally, the channel width-to-length ratio of the first transistor T1 is between 6:5 and 12:5, such as 6:5, 5:4, 12:5, etc.; the channel width-to-length ratio of the third transistor T3 is between 4:12 and 8:10, such as 4:12, 4:10, 8:10, etc.
[0079] In some embodiments, the transistor may be a P-type transistor or an N-type transistor, and may be a bottom-gate transistor, a top-gate transistor, or a dual-gate transistor, without limitation. The first electrode of the transistor may be a source electrode, and the second electrode may be a drain electrode, or the first electrode of the transistor may be a drain electrode, and the second electrode may be a source electrode. The material of the active layer of the transistor may be amorphous silicon (a-Si), polycrystalline silicon (poly), or an oxide (e.g., indium gallium zinc oxide (IGZO)).
[0080] In some embodiments, in the array substrate provided by the embodiments of the present disclosure, as shown in Figures 4 and 6, the discharge line 109 includes a first subsection 1091 that overlaps with the gate line 112 in a direction perpendicular to the base substrate 101, a second subsection 1092 that overlaps with the first voltage line 110, and a third subsection 1093 that overlaps with the second voltage line 111. The line width of the first subsection 1091 is smaller than the line width of the second subsection 1092, and the line width of the second subsection 1092 is approximately equal to (i.e., equal to or within the error range caused by factors such as manufacturing and measurement) the line width of the third subsection 1093. Because the signals of the first and second voltage lines 111 and 112 are fixed potentials, while the signals of the gate line 112 and the discharge line 109 vary, the gate line 112 may affect the discharge line 109. Therefore, the discharge line 109 is made relatively narrow at the location where it overlaps with the gate line 112, and slightly wider at the location where it overlaps with the voltage lines to reduce the risk of line breakage. Accordingly, the gate line 112 may also include a narrowed portion 1121, where the orthographic projection of the narrowed portion 1121 on the base substrate 101 overlaps with the orthographic projection of the discharge line 109 (specifically, the first sub-portion 1091) on the base substrate 101, thereby reducing the load caused by the gate line 112 on the discharge line 109. Optionally, to reduce mutual interference between the gate line 112 and the data line 102, the width of the gate line 112 and the data line 102 may be reduced at the location where the data line 102 and the gate line 112 overlap.
[0081] In some embodiments, in the above-mentioned array substrate provided in the embodiments of the present disclosure, as shown in Figures 2, 12 and 13, the base substrate 101 also includes a frame area BB located on at least one side of the display area AA, and the array substrate may further include a frame sealant area (for setting the frame sealant 113) and multiple traces 114 (for example, signal lines or dummy lines) located in the frame area BB, wherein at least part of the traces 114 include a main line 1141 and a plurality of protruding structures 1142 located on at least one side of the main line 1141, wherein at least one end of the area between adjacent main lines 1141 exceeds or approximately coincides with the boundary of the frame sealant area (equivalent to the boundary of the frame sealant 113) (i.e., coincides or is within the error range caused by factors such as manufacturing and measurement), and the protruding structures 1142 between adjacent main lines 1141 are staggered to increase the path for water vapor to enter the display area AA along the area between adjacent main lines 1141, thereby reducing the risk of water vapor intrusion.
[0082] It is worth noting that in the present disclosure, the frame sealant 113 may not be set on the array substrate first, but after the array substrate and the opposite substrate (also called the color film substrate) are assembled into a display box containing liquid crystal, a frame sealant 113 is provided between the array substrate and the opposite substrate to surround the liquid crystal.
[0083] In some embodiments, in the array substrate provided by the embodiments of the present disclosure, the line width of the protruding structures 1142 can be the same as the line width of the peripheral slits. For example, the line width of the protruding structures 1142 can be greater than or equal to 6 μm and less than or equal to 20 μm, such as 6 μm, 10 μm, 15 μm, 20 μm, etc. The spacing between the staggered protruding structures 1042 can be designed according to the spacing design rules for signal lines. For example, the distance between two staggered protruding structures 1042 can be greater than or equal to 15 μm and less than or equal to 20 μm, such as 15 μm, 16 μm, 17 μm, 18 μm, 19 μm, 20 μm, etc. This allows the protruding structures 1142 to be manufactured using conventional process parameters, which is more compatible with existing technologies. Optionally, the shape of the protruding structures 1142 is not limited to the rectangle shown in FIG. 13 , but can also be a triangle, trapezoid, etc.
[0084] In some embodiments, in the array substrate provided in the embodiments of the present disclosure, as shown in FIG. 2 and FIG. 14 to FIG. 16 , a common electrode line (COM_TFT) 115 may be further provided in the frame area BB to transmit the common voltage on the array substrate to the common electrode 201 on the opposite substrate via the gold balls (Au) in the sealant 113 (located in the sealant area); the common electrode line 115 (optionally, the common electrode line 115 is provided in the same layer of material as the pixel electrodes in the display area) may include a plurality of conductive structures 1151 arranged side by side, and a connecting line 1152 integrally provided with the plurality of conductive structures 1151. In the related art, large, independently provided electrodes (typically with an area 200 to 500 times that of the pixel electrodes 104) are used to transmit the common voltage. This results in that when electrostatic discharge (ESD) occurs, the static electricity can be quickly discharged from the array substrate at the location of the large electrodes, but the static electricity cannot be quickly discharged between the large electrodes, resulting in excessive static electricity accumulation and burning of the surrounding metal traces. The present disclosure divides a large electrode into a plurality of small conductive structures 1151 and connects the conductive structures 1151 in series with connecting wires 1152. When static electricity occurs, the static electricity will first contact the connecting wires 1152 and then spread to both sides along the connecting wires 1152, preventing the surrounding metal traces from being burned. Optionally, the ratio of the orthographic projection area of the conductive structure 1151 on the substrate 101 to the orthographic projection area of the pixel electrode 104 on the substrate 101 is greater than or equal to 30 and less than or equal to 50. For example, the width of the conductive structure 1151 is 2000μm to 6000μm; the spacing between the conductive structures 1151 can be 1 to 3 times (for example, 2 times) the width of the conductive structure 1151 to facilitate uniform circuit configuration. The larger the size of the conductive structure 1151, the easier it is to manufacture. When the ratio of the orthographic projection area of the conductive structure 1151 on the base substrate 101 to the orthographic projection area of the pixel electrode 104 on the base substrate 101 is greater than or equal to 30, the size of the conductive structure 1151 can be ensured to be large and easy to manufacture. However, an oversized conductive structure 1151 is prone to accumulate more static electricity and burn the surrounding metal traces. Therefore, the present disclosure sets the ratio of the orthographic projection area of the conductive structure 1151 on the base substrate 101 to the orthographic projection area of the pixel electrode 104 on the base substrate 101 to be less than or equal to 50 to ensure that the size of the conductive structure 1151 is moderate and static electricity is not accumulated due to the excessive size of the conductive structure 1151.
[0085] In some embodiments, in the above-mentioned array substrate provided by the embodiments of the present disclosure, as shown in Figure 14, the orthographic projections of the multiple conductive structures 1151 on the base substrate 101 can overlap with the orthographic projections of the sealing glue 113 (equivalent to the sealing glue area) on the base substrate 101, and the orthographic projections of the connecting wires 1152 on the base substrate 101 are located between the orthographic projections of the sealing glue 113 on the base substrate 101 and the display area AA; compared to locating the orthographic projections of the connecting wires 1152 on the base substrate 101 on the side of the orthographic projections of the sealing glue 113 on the base substrate 101 away from the display area AA, in the present disclosure, the length of the connecting wires 1152 is shorter, the resistance of the connecting wires 1152 is reduced, and the loss of the common voltage on the connecting wires 1152 is reduced.
[0086] In some embodiments, in the array substrate provided in the embodiments of the present disclosure, as shown in FIG14 and FIG15 , a signal line 116 may be further provided in the border area BB. The orthographic projection of the signal line 116 on the base substrate 101 is located between the orthographic projection of the sealant 113 (equivalent to the sealant area) on the base substrate 101 and the display area AA, and overlaps with the orthographic projection of the connection line 1152 on the base substrate 101, and the signal line 116 is coupled to the connection line 1152. Optionally, the signal line 116 is provided on the same layer as the plurality of gate lines 114, and the connection line 1152 is provided on the same layer as the plurality of pixel electrodes 104 (equivalent to the common electrode line 115 being provided on the same layer as the pixel electrode 104). The signal line 116 is coupled to the connection line 1152 via a seventh via hole h7 penetrating the insulating layer (including the gate insulating layer GI, the first passivation layer 105, and the second passivation layer 106). The pixel electrode 104 is the top conductive layer in the array substrate, and the common electrode line 115 is in the same layer as the pixel electrode 104, which facilitates the contact and electrical connection between the sealant 113 and the conductive structure 1151 of the common electrode line 115; at the same time, the gate line 112 is made of metal, and the signal line 116 is arranged in the same layer as the gate line 112, which can achieve a lower resistance of the signal line 116, so that the overall resistance on the transmission path of the common voltage is smaller, reducing the loss of the common voltage. In some embodiments, the seventh via h7 can be set at the contact position between at least part of the conductive structure 1151 and the connecting line 1152, and in the extension direction of the connecting line 1152, the size of the seventh via h7 can be approximately the same as the size of the conductive structure 1151 (i.e., the same or within the error range caused by factors such as manufacturing and measurement), so that the seventh via h7 is smaller, reducing the risk of corrosion in large-area vias.
[0087] In some embodiments, in the array substrate provided in the embodiment of the present disclosure, as shown in FIG17 , a ground signal line (GND) 117, a common voltage feedback line (COM_CF_FB) 118, an even column discharge bus (Discharge Even) 119, and an odd column discharge bus (Discharge Odd) 120, voltage bus (Com_TFT) 121, etc.; wherein, the common voltage feedback line 118 can monitor the remote common voltage signal, and then compensate the fluctuating common voltage signal through the common voltage line set in the display panel, and the compensation adopts reverse compensation. When the common voltage signal fluctuates positively relative to the reference voltage (i.e., greater than the reference voltage), compensation for the downward fluctuation relative to the reference voltage (i.e., less than the reference voltage) is performed; the even column discharge bus is coupled to the discharge line 109 of the even column in the display area AA to discharge the second pixel electrode 1042 of the even column and adjust the brightness difference between the first pixel electrode 10421 and the second pixel electrode 1042 of the even column; the odd column discharge bus 120 discharges the second pixel electrode 1042 of the odd column and adjusts the brightness difference between the first pixel electrode 1041 and the second pixel electrode 1042 of the odd column. 42 brightness difference; the voltage bus 121 provides a fixed potential for the first voltage line 110 and the second voltage line 111. It should be noted that odd-numbered columns and even-numbered columns of discharge lines are set in this case. Optionally, the discharge lines corresponding to the odd-numbered columns and the even-numbered columns provide different fixed potentials. With such a design, it is possible to achieve two dark degrees for the dark pixels in the odd-numbered columns and the even-numbered columns of the display panel, which is equivalent to further increasing the domain direction and better improving the display effect; optionally, in this case, the odd-numbered columns and the even-numbered columns of discharge lines provide the same fixed potential; optionally, in this case, the odd-numbered columns and the even-numbered columns of discharge lines are not distinguished, and all discharge lines are given the same potential; optionally, in this case, more than two discharge lines with different voltages are set, for example, three discharge lines are set, the three discharge lines are arranged alternately, and the three discharge lines are given different fixed voltages, so that three pixels with different darkness can be achieved. The specific setting method is not limited in this case. Optionally, in the present disclosure, a printed circuit board (PCB) and a timing control board (TCON) can provide signals to a chip on film (COF IC), and the chip on film (COF IC) can also have the functions of a gate driver chip (Gate IC) and a data signal driver chip (Source IC), so that the pads bonded to the chip on film on the array substrate can transmit the signals provided by the chip on film (COF IC) to the data lines 102, gate lines 112, discharge lines 109, etc. Other components of the array substrate that are well known to those skilled in the art are not described here in detail and are not intended to limit the present disclosure.
[0088] Accordingly, an embodiment of the present disclosure provides a method for manufacturing the above array substrate, which may include the following steps:
[0089] Providing a base substrate, the base substrate including a display area;
[0090] forming a plurality of data lines extending along a first direction and arranged along a second direction in a display area;
[0091] forming an electrode pattern on the layer where the multiple data lines are located, the electrode pattern at least partially covering the multiple data lines, wherein the electrode pattern is a block electrode;
[0092] A plurality of pixel electrodes are formed on the layer where the electrode pattern is located. The pixel electrodes are block electrodes and are coupled to a plurality of data lines. The orthographic projections of the plurality of pixel electrodes on the base substrate overlap with the orthographic projections of the electrode pattern on the base substrate.
[0093] In order to better understand the manufacturing method of the array substrate provided by the present disclosure, the process of the manufacturing method provided by the present disclosure is introduced below:
[0094] The first step is to provide a base substrate 101 having a display area AA;
[0095] In the second step, a plurality of gate lines 112 arranged along the first direction Y and extending along the second direction X, as well as first voltage lines 110 and second voltage lines 111 located on both sides of the gate lines 112 are patterned in the display area AA.
[0096] Step 3: forming a gate insulating layer GI on the layer where the gate line 112 is located;
[0097] In the fourth step, an active layer a1 of the first transistor T1, an active layer a2 of the second transistor T1, and an active layer a3 of the third transistor T3 are patterned on the gate insulating layer GI. The active layer a1 of the first transistor T1, the active layer a2 of the second transistor T1, and the active layer a3 of the third transistor T3 can be integrally provided.
[0098] Step 5: Patterning the active layer a1 of the first transistor T1 to form a first electrode s1 and a second electrode d1 of the first transistor T1, a first electrode s2 and a second electrode d2 of the second transistor T2, a first electrode s3 and a second electrode d3 of the third transistor T3, a plurality of data lines 102, and discharge lines 109 alternately arranged with the data lines 102 in the second direction X.
[0099] In the sixth step, a first passivation layer 105 is patterned on the layer where the data line 102 is located. The first passivation layer 105 has a first via h1 for coupling the first voltage line 110 and the subsequent electrode pattern 103, a second via h2 for coupling the second voltage line 111 and the subsequent electrode pattern 103, a third via h3 for coupling the second electrode d1 of the first transistor T1 and the subsequent transfer electrode 108, and a fifth via h5 for coupling the second electrode d2 of the second transistor T2 and the subsequent transfer electrode 108, and the second electrode d1 of the first transistor T1 and the second electrode d2 of the second transistor T2 are connected to different transfer electrodes 108.
[0100] Step 7: Patterning the first passivation layer 105 to form an electrode pattern 103 and a transfer electrode 108;
[0101] In the eighth step, a second passivation layer 106 is formed on the layer where the electrode pattern 103 is located. The second passivation layer 106 has a fourth via h4 for coupling the transfer electrode 108 and the first pixel electrode 1041 to be subsequently manufactured, and a sixth via h6 for coupling the transfer electrode 108 and the second pixel electrode 1042 to be subsequently manufactured, and the first pixel electrode 1041 and the second pixel electrode 1042 are connected to different transfer electrodes 108.
[0102] In the ninth step, a plurality of pixel electrodes 104 are formed by patterning on the second passivation layer 106 . Each pixel electrode 104 includes a first pixel electrode 1041 and a second pixel electrode 1042 arranged side by side in the first direction Y.
[0103] The tenth step is to form an alignment film on the layer where the pixel electrode 104 is located.
[0104] It should be noted that the above mainly introduces the production order of the components in the display area AA. For the arrangement of each component in the above steps and other components arranged on the same layer (for example, the common electrode line 115 arranged on the same layer as the pixel electrode 104 in the border area BB), please refer to the above content and will not be repeated here.
[0105] Based on the same inventive concept, an embodiment of the present disclosure provides a display device, as shown in FIG18 , comprising an array substrate 001 and an opposing substrate 002 disposed opposite each other, and a liquid crystal layer 003 located between the array substrate 001 and the opposing substrate 002. The array substrate 001 is the aforementioned array substrate provided in the embodiment of the present disclosure, and the opposing substrate 002 comprises a common electrode 201, a color resist 202, and a black matrix 203. The color resist 202 may include a red color resist R, a green color resist G, a blue color resist B, and the like. Because the principles underlying the display device and the aforementioned array substrate are similar, the implementation of the display device may refer to the aforementioned array substrate embodiments, and any repetitive details will not be repeated.
[0106] In some embodiments, in the display device provided by the embodiments of the present disclosure, as shown in Figure 18, a first alignment film 122 is provided on the side of the array substrate 001 close to the liquid crystal layer 003, and a second alignment film 204 is provided on the side of the opposing substrate 002 close to the liquid crystal layer 003. The first alignment film 122 and the second alignment film 204 jointly determine the pretilt angle of the liquid crystal molecules LC in the liquid crystal layer 003.
[0107] As can be seen from Figure 19, the present disclosure adopts a photo-alignment method to enable the first alignment film 122 and the second alignment film 204 to have alignment capabilities. When the first alignment film 122 or the second alignment film 204 is exposed and aligned separately, the tilt (Tilt) direction of the liquid crystal molecule LC is opposite to the exposure direction of the first alignment film 122 or the second alignment film 204. The final pre-tilt direction of the liquid crystal molecule LC depends on the comprehensive alignment effect of the first alignment film 122 and the second alignment film 204.
[0108] In the present disclosure, the region where the first pixel electrode 1041 and the second pixel electrode 1042 are located is divided into four sub-regions ① to ④. The liquid crystal molecules LC have corresponding pretilt directions D1 to D4 within these four sub-regions ① to ④, resulting in a four-domain alignment in the region where the first pixel electrode 1041 and the second pixel electrode 1042 are located, as shown in FIG20 . In some embodiments, as shown in FIG21 , within the first sub-region ①, the first alignment film 122 can be exposed and aligned along the negative direction X2 of the second direction, and the second alignment film 204 can be exposed and aligned along the negative direction Y2 of the first direction. This will cause the liquid crystal molecules LC to tilt along the positive direction X1 of the second direction and the positive direction Y1 of the first direction, resulting in a pretilt direction D1 located between the negative direction X2 of the second direction and the positive direction Y1 of the first direction, as shown in FIG20 . In the second sub-region ②, as shown in FIG21, the first alignment film 122 can be exposed and aligned along the negative direction X2 of the second direction, and the second alignment film 204 can be exposed and aligned along the positive direction Y1 of the first direction; thus, the liquid crystal molecules LC will tilt along the positive direction X1 of the second direction and the negative direction Y2 of the first direction, exhibiting a pretilt direction D2 located between the negative direction X2 of the second direction and the negative direction Y2 of the first direction, as shown in FIG20. In the third sub-region ③, as shown in FIG21, the first alignment film 122 can be exposed and aligned along the positive direction X1 of the second direction, and the second alignment film 204 can be exposed and aligned along the positive direction Y1 of the first direction; thus, the liquid crystal molecules LC will tilt along the negative direction X2 of the second direction and the negative direction Y2 of the first direction, exhibiting a pretilt direction D3 located between the positive direction X1 of the second direction and the negative direction Y2 of the first direction, as shown in FIG20. In the fourth sub-region (4), as shown in FIG21 , the first alignment film 122 can be exposed and aligned along the positive second direction X1, while the second alignment film 204 can be exposed and aligned along the negative first direction Y2. This causes the liquid crystal molecules LC to tilt along the negative second direction X2 and the positive first direction Y1, exhibiting a pretilt direction D4 intermediate between the positive second direction X1 and the positive first direction Y1. This achieves a four-domain alignment in the region where the first pixel electrode 1041 and the second pixel electrode 1042 are located.
[0109] In some embodiments, the above-mentioned display device provided by the embodiments of the present disclosure may further include a backlight module located on the light incident side of the array substrate 001, and the backlight module may be a direct-type backlight module or an edge-entry backlight module. Optionally, the edge-entry backlight module may include a light bar, a reflective sheet stacked, a light guide plate, a diffuser, a prism group, etc., and the light bar is located on one side of the thickness direction of the light guide plate. The direct-type backlight module may include a matrix light source, a reflective sheet stacked on the light emitting side of the matrix light source, a diffuser and a brightening film, etc., and the reflective sheet includes an opening arranged opposite to the position of each lamp bead in the matrix light source. The lamp beads in the light bar and the lamp beads in the matrix light source may be light-emitting diodes (LEDs), such as micro light-emitting diodes (Mini LED, Micro LED, etc.).
[0110] Submillimeter or even micron-scale micro-LEDs are self-luminous devices, just like organic light-emitting diodes (OLEDs). Like organic light-emitting diodes, they have a series of advantages such as high brightness, ultra-low latency, and ultra-large viewing angles. And because inorganic light-emitting diodes emit light based on metal semiconductors with more stable properties and lower resistance, they have the advantages of lower power consumption, greater resistance to high and low temperatures, and longer service life compared to organic light-emitting diodes that emit light based on organic matter. And when micro-LEDs are used as backlight sources, more precise dynamic backlight effects can be achieved. While effectively improving screen brightness and contrast, they can also solve the glare phenomenon caused by traditional dynamic backlighting between bright and dark areas of the screen, thereby optimizing the visual experience.
[0111] In some embodiments, the above-mentioned display device provided in the embodiments of the present disclosure may be: a projector, a 3D printer, a virtual reality device, a mobile phone, a tablet computer, a television, a monitor, a laptop computer, a digital photo frame, a navigator, a smart watch, a fitness wristband, a personal digital assistant, or any other product or component with a display function. Optionally, the display device provided in the present disclosure includes, but is not limited to, components such as a radio frequency unit, a network module, an audio output & input unit, a sensor, a display unit, a user input unit, an interface unit, and a control chip. Optionally, the control chip is a central processing unit, a digital signal processor, a system-on-chip (SoC), etc. For example, the control chip may further include a memory, a power module, etc., and realize power supply and signal input and output functions through additionally provided wires, signal lines, etc. For example, the control chip may further include hardware circuits and computer executable code, etc. The hardware circuit may include conventional very large scale integration (VLSI) circuits or gate arrays and existing semiconductors or other discrete components such as logic chips and transistors; the hardware circuit may also include field programmable gate arrays, programmable array logic, programmable logic devices, etc. In addition, those skilled in the art will understand that the above structure does not constitute a limitation on the above display device provided in the embodiment of the present disclosure. In other words, the above display device provided in the embodiment of the present disclosure may include more or fewer of the above components, or a combination of certain components, or different component arrangements.
[0112] Although the present disclosure has described preferred embodiments, it should be understood that those skilled in the art may make various changes and modifications to the embodiments without departing from the spirit and scope of the embodiments of the present disclosure. Thus, if such modifications and variations of the embodiments of the present disclosure fall within the scope of the claims of the present disclosure and their equivalents, the present disclosure is intended to include such modifications and variations.
Claims
1. An array substrate, wherein: include: A base substrate, the base substrate comprising a display area; A plurality of data lines extending along a first direction and arranged along a second direction in the display area; an electrode pattern, located on a side of the layer where the plurality of data lines are located away from the base substrate, the electrode pattern being a block electrode, and at least a portion of the orthographic projections of the data lines on the base substrate being located within the orthographic projection of the electrode pattern on the base substrate; A plurality of pixel electrodes are located on a side of the layer where the electrode pattern is located away from the base substrate. The pixel electrodes are block electrodes. The plurality of pixel electrodes are coupled to the plurality of data lines. The orthographic projections of the plurality of pixel electrodes on the base substrate overlap with the orthographic projections of the electrode pattern on the base substrate.
2. The array substrate according to claim 1, wherein: The orthographic projection of the data line on the base substrate overlaps with the orthographic projection of the pixel electrode on the base substrate.
3. The array substrate according to claim 1 or 2, wherein: Also included are a plurality of pixel circuits, wherein the pixel circuits are coupled to the data lines and the pixel electrodes; The electrode pattern includes a plurality of hollow structures, and the orthographic projections of the plurality of pixel circuits on the base substrate are located within the orthographic projections of the plurality of hollow structures on the base substrate.
4. The array substrate according to claim 3, wherein: It also includes a plurality of switching electrodes arranged in the same layer as the electrode pattern, the switching electrodes couple the pixel electrode and the pixel circuit, and the orthographic projections of the plurality of switching electrodes on the base substrate are located within the orthographic projections of the plurality of hollow structures on the base substrate.
5. The array substrate according to claim 3 or 4, wherein: It also includes a plurality of discharge lines arranged in the same layer as the plurality of data lines, and the discharge lines and the data lines are alternately arranged in the second direction; the pixel electrode includes a first pixel electrode and a second pixel electrode arranged side by side in the first direction, and the discharge line is coupled to the second pixel electrode through the pixel circuit.
6. The array substrate according to claim 5, wherein: It also includes multiple first voltage lines and multiple second voltage lines, the orthographic projection of the first voltage line on the base substrate overlaps with the orthographic projection of the first pixel electrode on the base substrate, the orthographic projection of the second voltage line on the base substrate overlaps with the orthographic projection of the second pixel electrode on the base substrate, and the multiple first voltage lines and the multiple second voltage lines are respectively coupled to the electrode pattern.
7. The array substrate according to claim 6, wherein: It also includes a plurality of gate lines extending along the second direction in the display area and arranged along the first direction, the plurality of first voltage lines, the plurality of second voltage lines and the plurality of gate lines are arranged in the same layer, and the gate lines are coupled to the pixel circuit.
8. The array substrate according to claim 7, wherein: The pixel circuit includes a first transistor, a second transistor and a third transistor, wherein the gate of the first transistor, the gate of the second transistor and the gate of the third transistor are multiplexed and integrated with the gate line, the first electrode of the first transistor and the first electrode of the second transistor are multiplexed, the first electrode of the third transistor and the second electrode of the second transistor are multiplexed and coupled to the second pixel electrode, and the second electrode of the first transistor is coupled to the first pixel electrode.
9. The array substrate according to claim 8, wherein: The channel width-to-length ratio of the first transistor is substantially the same as the channel width-to-length ratio of the second transistor, and the channel width-to-length ratio of the first transistor is greater than the channel width-to-length ratio of the third transistor.
10. The array substrate according to any one of claims 7 to 9, wherein: The discharge line includes a first section overlapping with the gate line in a direction perpendicular to the substrate, a second section overlapping with the first voltage line, and a third section overlapping with the second voltage line, wherein the line width of the first section is smaller than the line width of the second section, and the line width of the second section is substantially equal to the line width of the third section.
11. The array substrate according to any one of claims 7 to 10, wherein: The gate line includes a narrowing portion, and an orthographic projection of the narrowing portion on the base substrate overlaps with an orthographic projection of the discharge line on the base substrate.
12. The array substrate according to any one of claims 1 to 11, wherein: The base substrate also includes a frame area located on at least one side of the display area, and the array substrate also includes a frame-sealing glue area and multiple routing lines located in the frame area, wherein at least part of the routing lines include a main line and multiple protruding structures located on at least one side of the main line, wherein at least one end of the area between adjacent main lines exceeds or roughly overlaps with the boundary of the frame-sealing glue area, and the protruding structures between adjacent main lines are staggered.
13. The array substrate according to claim 12, wherein: In the extension direction of the region between adjacent main lines, the width of the protruding structure is greater than or equal to 6 μm and less than or equal to 20 μm, and the distance between two staggered protruding structures is greater than or equal to 15 μm and less than or equal to 20 μm.
14. The array substrate according to any one of claims 1 to 13, wherein: The base substrate also includes a frame area located on at least one side of the display area, and the array substrate also includes a common electrode line located in the frame area. The common electrode line includes a plurality of conductive structures arranged side by side and a connecting line integrally arranged with the plurality of conductive structures.
15. The array substrate according to claim 14, wherein: A ratio of an orthographic projection area of the conductive structure on the base substrate to an orthographic projection area of the pixel electrode on the base substrate is greater than or equal to 30 and less than or equal to 50.
16. The array substrate according to claim 14 or 15, wherein: In the extending direction of the connecting line, the ratio of the distance between adjacent conductive structures to the size of the conductive structure is greater than or equal to 1 and less than or equal to 3.
17. The array substrate according to any one of claims 14 to 16, wherein: The frame area includes a sealing glue area, the orthographic projections of the multiple conductive structures on the base substrate overlap with the orthographic projection of the sealing glue area on the base substrate, and the orthographic projection of the connecting line on the base substrate is located between the orthographic projection of the sealing glue area on the base substrate and the display area.
18. The array substrate according to claim 17, wherein: It also includes a signal line located in the border area, the orthographic projection of the signal line on the base substrate is located between the orthographic projection of the sealing glue area on the base substrate and the display area, and overlaps with the orthographic projection of the connecting line on the base substrate, and the signal line is coupled to the connecting line.
19. The array substrate according to claim 18, wherein: It also includes a plurality of gate lines located in the display area, and an insulating layer located between a layer where the plurality of gate lines are located and a layer where the plurality of pixel electrodes are located; The signal line is disposed in the same layer as the plurality of gate lines, the connection line is disposed in the same layer as the plurality of pixel electrodes, and the signal line is coupled to the connection line through a via hole penetrating the insulating layer.
20. A method for manufacturing an array substrate according to any one of claims 1 to 19, wherein: include: providing a substrate substrate, the substrate substrate comprising a display area; forming a plurality of data lines extending along a first direction and arranged along a second direction in the display area; forming an electrode pattern at least partially covering the plurality of data lines on the layer where the plurality of data lines are located, wherein the electrode pattern is a block electrode; A plurality of pixel electrodes are formed on the layer where the electrode pattern is located. The pixel electrodes are block electrodes. The plurality of pixel electrodes are coupled to the plurality of data lines. The orthographic projections of the plurality of pixel electrodes on the base substrate overlap with the orthographic projections of the electrode pattern on the base substrate.
21. A display device, wherein: The invention comprises an array substrate and an opposite substrate which are opposite to each other, and a liquid crystal layer located between the array substrate and the opposite substrate. The array substrate is the array substrate according to any one of claims 1 to 19, and the opposite substrate comprises a common electrode.