Electrode plate and method for manufacturing electrode plate

In the manufacture of electrode plates of lithium-ion batteries, the end and bending points of metal foil are used to solve the wrinkle problem caused by the difference in the ductility of lithium foil and copper foil, and the electrode plate that is not easy to produce wrinkles is realized, which improves the battery Stability and safety.

CN118901148APending Publication Date: 2024-11-05PANASONIC INTELLECTUAL PROPERTY MANAGEMENT CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202380027857.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-03-28
Filing Date
2023-03-23
Publication Date
2024-11-05

AI Technical Summary

Technical Problem

In lithium-ion batteries, wrinkles are easily caused due to the difference in the ductility of lithium foil and copper foil.

Method used

During the manufacturing process of the electrode plate, the ends of the first metal foil and the second metal foil are arranged and a bending point is formed at a specific position, so that the second metal foil overlaps the surface of the first metal foil, thereby at the bending point. Bending both to form electrode plates that are not prone to wrinkles.

Benefits of technology

The electrode plate is realized that is not easy to generate wrinkles, which improves the manufacturing stability of the battery and the strength of the electrode, reduces the internal resistance, and improves the safety of the battery and the high-current discharge characteristics.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118901148A_ABST
    Figure CN118901148A_ABST
Patent Text Reader

Abstract

The first metal foil (200) has a first surface (400) and a second surface (402), and has a first end portion (410) and a second end portion (412) disposed at both ends in one direction. In the second metal foil (202), a third end portion (420) and a fourth end portion (422) are disposed at both ends in one direction. The second end portion (412) is aligned with the fourth end portion (422), and the second metal foil (202) overlaps the first surface (400) of the first metal foil (200). A bending point (440) is disposed between the central position (430) and the second end portion (412), and the first metal foil (200) and the second metal foil (202) are bent at the central position (430) so as to contact the second surface (402) of the first metal foil (200). The second surface (402) of the first metal foil (200) is exposed between the first end portion (410) and the second end portion (412).
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to an electrode plate composed of two kinds of metal foils and a method for manufacturing the electrode plate. Background Art

[0002] The negative electrode current collector in a secondary battery such as a lithium ion battery is manufactured by placing a lithium foil as a negative electrode active material in a copper foil as a current collector. For example, the lithium foil and the copper foil are pressed by a relatively weak pressing roller and a relatively strong pressing roller in sequence (for example, refer to Patent Document 1).

[0003] Prior art literature

[0004] Patent Literature

[0005] Patent Document 1: Japanese Patent Application Laid-Open No. 3-93156 Summary of the invention

[0006] Technical problem to be solved by the invention

[0007] In secondary batteries such as lithium ion batteries, lithium foil is sometimes pressed against both surfaces of copper foil. In this case, wrinkles are easily generated in the foil due to the difference in elongation between the lithium foil and the copper foil.

[0008] The present disclosure has been made in view of such circumstances, and one object of the present disclosure is to provide an electrode plate that is less likely to wrinkle.

[0009] Methods used to solve technical problems

[0010] In order to solve the above technical problems, an electrode plate of one solution of the present disclosure includes: a first metal foil having a first surface and a second surface facing the opposite side of the first surface, with a first end and a second end configured at both ends in one direction; and a second metal foil having a third end and a fourth end configured at both ends in one direction. The second end of the first metal foil is aligned with the fourth end of the second metal foil, the second metal foil overlaps the first surface of the first metal foil, a bending point is configured between the center position of the first end and the second end of the first metal foil and the second end, the first metal foil and the second metal foil are bent at the bending point in a manner of contacting the second surface of the first metal foil, and the second surface of the first metal foil is exposed between the first end and the second end.

[0011] Another scheme of the present disclosure is a method for manufacturing an electrode plate. The method includes: a step of forming a laminated body for a first metal foil having a first surface and a second surface facing the opposite side of the first surface, and having a first end and a second end configured at both ends in one direction, and a second metal foil having a third end and a fourth end configured at both ends in one direction, wherein the laminated body is a structure in which the second end of the first metal foil and the fourth end of the second metal foil are aligned, and the second metal foil overlaps the first surface of the first metal foil; and a step of configuring a bending point between the center position of the first end and the second end of the first metal foil and the second end, and bending the first metal foil and the second metal foil at the bending point in a manner that the bending point contacts the second surface of the first metal foil.

[0012] Effects of the Invention

[0013] According to the present disclosure, it is possible to provide an electrode plate that is less likely to wrinkle. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] Figure 1 This is a longitudinal sectional view showing the structure of the battery of Example 1.

[0015] Figure 2 It is shown Figure 1 A cross-sectional view of an example of the configuration of an electrode body.

[0016] Figure 3 (a)-(b) shows Figure 2 A diagram of an example of the structure of a negative electrode.

[0017] Figure 4 (a) to (e) are diagrams showing the manufacturing process of the electrode plate of Example 1.

[0018] Figure 5 is shown for manufacturing Figure 4 (b) to (c) are side views of the structure of the manufacturing device.

[0019] Figure 6 (a)-(d) show Figure 4 (e) Diagram of the manufacturing process.

[0020] Figure 7 (a) to (e) are diagrams showing the manufacturing process of the electrode plate of Example 2.

[0021] Figure 8 (a)-(h) shows Figure 7 (c) is a diagram of the structure of a stacked body. DETAILED DESCRIPTION

[0022] (Example 1)

[0023] Below, the present disclosure is described with reference to the accompanying drawings based on preferred embodiments. The embodiments do not limit the present disclosure but are illustrative, and all the features or combinations thereof recorded in the embodiments do not necessarily represent the essential content of the present disclosure. The same or equivalent components, parts, and processes shown in the drawings are marked with the same figure marks, and repeated descriptions are appropriately omitted. In addition, the scales or shapes of the various parts shown in the drawings are conveniently set for easy description, and are not interpreted restrictively unless otherwise mentioned. In addition, when the terms "first", "second", etc. are used in this specification or claims, unless otherwise mentioned, the terms do not indicate any order or importance, but are used to distinguish one structure from other structures. In addition, in the drawings, a part of the unimportant parts is omitted for display when describing the embodiments.

[0024] The following describes in the order of (1) the structure of the battery and (2) the manufacturing process of the electrode plate.

[0025] (1) Battery structure

[0026] use Figure 1 , the structure of a non-aqueous electrolyte secondary battery (hereinafter also referred to as a “battery”) 10 will be described. Figure 1 : is a longitudinal cross-sectional view showing the structure of the battery 10. The battery 10 includes: a wound electrode body 14 in which a positive electrode 30 and a negative electrode 40 are spirally wound via a gasket 50; a non-aqueous electrolyte (not shown); and a metal battery case (external body) that accommodates the electrode body 14 and the non-aqueous electrolyte. A predetermined amount of the non-aqueous electrolyte is injected into the battery case to impregnate the electrode body 14.

[0027] The positive electrode 30 and the negative electrode 40 have a structure in which an electrode active material layer is stacked on a current collector. For example, if the current collector is a positive electrode, it is composed of aluminum foil or the like, and if it is a negative electrode, it is composed of copper foil or the like. The electrode active material layer can be formed by coating an electrode composite material on the surface of the current collector with a known coating device, and by drying and rolling. The electrode composite material is obtained by kneading materials such as electrode active materials, adhesive materials, and conductive materials in a dispersion medium to uniformly disperse them. For example, if the electrode active material is a positive electrode, it is lithium cobalt oxide or lithium iron phosphate, and if it is a negative electrode, it is graphite or the like.

[0028] The shell body 15 is, for example, a metal container in a bottomed cylindrical shape. A gasket 27 is provided between the shell body 15 and the sealing body 16 to ensure the sealing property inside the battery case. The shell body 15 preferably has, for example, an extension 21 formed by pressing the side surface from the outside and supporting the sealing body 16.

[0029] The sealing body 16 has a filter 22 having a filter opening 22a formed therein, and a valve body disposed on the filter 22. The valve body blocks the filter opening 22a of the filter 22, and breaks when the internal pressure of the battery 10 rises due to heat generated by an internal short circuit or the like. In this embodiment, a lower valve body 23 and an upper valve body 25 are provided as valve bodies, and an insulating member 24 disposed between the lower valve body 23 and the upper valve body 25, and a cover 26 having a cover opening 26a are also provided. The components constituting the sealing body 16 have, for example, a disc shape or a ring shape, and the components except the insulating member 24 are electrically connected to each other. Specifically, the filter 22 and the lower valve body 23 are joined to each other at their respective peripheral portions, and the upper valve body 25 and the cover 26 are also joined to each other at their respective peripheral portions. The lower valve body 23 and the upper valve body 25 are connected to each other at their respective central portions, and an insulating member 24 is present between the respective peripheral portions.

[0030] The battery 10 includes an insulating plate 17 and an insulating plate 18 disposed above and below the electrode body 14, respectively. Figure 1 In the example shown, the positive lead 19 mounted on the positive electrode 30 passes through the through hole of the insulating plate 17 and extends to the sealing body 16 side. For example, the positive lead 19 is connected to the lower surface of the filter 22 as the bottom plate of the sealing body 16 by welding, etc., and the cover 26 as the top plate of the sealing body 16 electrically connected to the filter 22 becomes the positive terminal. In this embodiment, a current cutoff mechanism (CID) and a gas exhaust mechanism (safety valve) are provided in the sealing body 16. In addition, a gas exhaust valve (not shown) is preferably provided at the bottom of the shell body 15.

[0031] Figure 2 1 shows a partial cross-sectional view of the electrode body 14 contained in the battery 10. The strip-shaped positive electrode 30 constituting the electrode body 14 includes a positive electrode collector 31 (positive electrode collector), a positive electrode active material layer 32 (positive electrode active material layer) formed on both sides of the positive electrode collector 31, and a positive electrode lead 19. One end of the positive electrode lead 19 is joined to a region where the positive electrode active material layer 32 is not formed and the positive electrode collector 31 is exposed.

[0032] The strip-shaped negative electrode 40 constituting the electrode body 14 includes a negative electrode current collector 41 (current collector of the negative electrode) and a negative electrode active material layer 42 (electrode active material layer of the negative electrode) formed on the negative electrode current collector 41. Figure 1 and Figure 2 As shown, negative electrode 40 is arranged on the outer peripheral surface of electrode body 14 housed in the battery case, and an exposed portion 43 is provided on the outer peripheral side of negative electrode 40 arranged at the outermost periphery where negative electrode collector 41 is exposed and contacts the inner peripheral surface of the battery case. Figure 3 (a) to (b) schematically show an example of the structure of the negative electrode 40 . Figure 3(a) is a top view observed from one main side surface of the negative electrode 40, Figure 3 (b) is along Figure 3 The cross-sectional view of the line X-X in (a). Figure 3 As shown in (a) to (b) of FIG. 1 , the negative electrode 40 includes a negative electrode current collector 41 and negative electrode active material layers 42 formed on both sides of the negative electrode current collector 41. Figure 3 As shown in (a) and (b) of FIG. 1 , the exposed portion 43 provided in the negative electrode 40 is provided on one main surface of the negative electrode 40 and is located at one end in the longitudinal direction of the outermost peripheral portion of the electrode body 14 .

[0033] The exposed portion 43 is provided on the outer peripheral surface of the electrode body 14, and the exposed portion 43 is brought into contact with the inner peripheral surface of the battery case which also serves as the negative electrode terminal, thereby achieving electrical conduction between the negative electrode 40 and the battery case. Furthermore, since the exposed portion 43 of the negative electrode 40 is in wide contact with the inner peripheral surface of the battery case, the internal resistance of the battery 10 can be reduced. As a result, a battery having excellent large current discharge characteristics can be realized, and current concentration during an external short circuit can be prevented, so that a battery with high safety can be realized.

[0034] like Figures 1 to 3 As shown in (a)-(b), at the innermost circumference of the negative electrode 40, there is a portion where both surfaces of the negative electrode collector 41 are exposed, and the negative electrode lead 20 is connected to this portion. The negative electrode lead 20 is connected to the bottom inner surface of the shell body 15 by welding or the like. By separating the negative electrode lead 20 from the exposed portion 43 connected to the inner circumference of the battery case and connecting it to the battery case, the current collection efficiency is improved, and the internal resistance of the battery can be further reduced. In addition, when an external short circuit occurs, local heat generation can be suppressed by dispersing the short-circuit current, and internal short circuits caused by gasket melting can be prevented. In addition, the position where the negative electrode lead 20 is provided in the negative electrode 40 is not limited to the innermost circumference ( Figure 3 The negative electrode 40 may not be provided with the negative electrode lead 20 .

[0035] In addition, if Figures 1 to 3 As shown in (a) to (b) of FIG. 1 , the negative electrode 40 has a negative electrode active material layer 42 formed on the main surface opposite to the exposed portion 43 of the negative electrode current collector 41. Thus, the battery has a high capacity, and the strength of the region where the exposed portion 43 is formed in the negative electrode 40 can be maintained, making it easier to accommodate the electrode body 14 in the case body 15, relative to the positive electrode active material layer 32 of the positive electrode 30.

[0036] (2) Manufacturing process of electrode plates

[0037] Next, a procedure for manufacturing the negative electrode 40 as a negative electrode plate is described. In the negative electrode 40, the copper foil needs to be exposed. When the lithium foil is intermittently pressed against the copper foil, wrinkles are easily generated in the lithium foil due to the difference in elongation between the lithium foil and the copper foil. In this embodiment, after the lithium foil is pressed against the front surface of one side of the copper foil, it is bent at a position deviated from the center position in one direction, thereby forming a metal lithium layer on both sides of the copper foil and forming a portion of the copper foil exposed.

[0038] Figure 4 (a) to (e) show the manufacturing process of the electrode plate 280 . Figure 4 (a) shows the first metal foil 200 . Figure 4 The upper part of (a) is a top view. Figure 4 The lower part of (a) is a side view. The first metal foil 200 is a copper foil (about 13 μm) serving as a negative electrode current collector 41. The first metal foil 200 has a first surface 400 facing upward and a second surface 402 facing downward opposite to the first surface 400. In the left-right direction of the first metal foil 200, a first end 410 is arranged at the left end, and a second end 412 is arranged at the right end.

[0039] Figure 4 (b) shows Figure 4 (a) after the processing. Figure 4 The upper part of (b) is a top view. Figure 4 The lower part of (b) is a side view. A stack is formed by overlapping the second metal foil 202 on the first surface 400 of the first metal foil 200. The second metal foil 202 is a lithium foil (about 10 μm) that becomes the negative electrode active material layer 42. In the left and right directions of the second metal foil 202, a third end 420 is arranged at the left end, and a fourth end 422 is arranged at the right end. When the first metal foil 200 and the second metal foil 202 are overlapped, the second end 412 of the first metal foil 200 is aligned with the fourth end 422 of the second metal foil 202, and the first end 410 of the first metal foil 200 is also aligned with the third end 420 of the second metal foil 202. Here, the width of the second metal foil 202 is larger than the width of the first metal foil 200.

[0040] Figure 4 (c) shows Figure 4 (b) The subsequent processing. Figure 4 The upper part of (c) is a top view. Figure 4 The lower part of (c) is a side view. As described above, the width of the second metal foil 202 is greater than the width of the first metal foil 200. In order to make the width of the second metal foil 202 consistent with the width of the first metal foil 200, a part of the second metal foil 202 is cut.

[0041] Below, we will explain in more detail Figure 4 Production of a laminate of (b) to (c). Figure 5 is shown for manufacturing Figure 4 1 and 2 are side views of the structure of the manufacturing apparatus 180 of (b) to (c). The first metal foil roll 100 is wound around the first metal foil 200. The second metal foil roll 102 is wound around the second metal foil 202.

[0042] The first metal foil 200 is pulled out from the first metal foil roll 100, and the second metal foil 202 is pulled out from the second metal foil roll 102. The first metal foil 200 and the second metal foil 202 face the first pressing roller 110 and the second pressing roller 112, which are a pair of pressing rollers. At this time, the second metal foil 202 and the first metal foil 200 are overlapped in this order from above.

[0043] The first crimping roller 110 and the second crimping roller 112 are arranged in the up-down direction. Specifically, the first crimping roller 110 is arranged on the second metal foil 202 side, and the second crimping roller 112 is arranged on the first metal foil 200 side. The overlapping first metal foil 200 and the second metal foil 202 are inserted between the first crimping roller 110 and the second crimping roller 112. The first crimping roller 110 and the second crimping roller 112 have a cylindrical shape and can rotate. The first crimping roller 110 and the second crimping roller 112 rotate, so that the first metal foil 200 and the second metal foil 202 are crimped. As a laminate of the first metal foil 200 and the second metal foil 202 after crimping Figure 4 (b) is cut off.

[0044] Figure 4 (d) shows Figure 4 (c) The subsequent processing. Figure 4 The upper part of (d) is a top view. Figure 4 The lower part of (d) is a side view. The center between the first end 410 and the second end 412 of the first metal foil 200 is shown as a center position 430. In addition, a bending point 440 is arranged between the center position 430 and the second end 412.

[0045] Figure 4 (e) shows Figure 4 (d) The subsequent processing. Figure 4 The upper part of (e) is a top view. Figure 4 The middle part of (e) is a top view. Figure 4The lower part of (e) is a side view. The first metal foil 200 and the second metal foil 202 are bent at the bending point 440 in such a manner as to contact the second surface 402 of the first metal foil 200. That is, the first metal foil 200 and the second metal foil 202 are bent in such a manner that the second end 412 and the fourth end 422 face downward. On the surface on the lower side, the second surface 402 of the first metal foil 200 is exposed between the first end 410 and the second end 412. On the other hand, on the upper side, the first surface 400 of the first metal foil 200 is not exposed. Figure 4 (e) is an electrode plate 280 , which is used as the negative electrode 40 , for example.

[0046] Figure 6 (a)-(d) show Figure 4 (e) The manufacturing process. Figure 6 In (a), a stack of the first metal foil 200 and the second metal foil 202 and an inflection point 440 in the stack are shown. In addition, an ejector pin 450 is arranged near the inflection point 440. Figure 6 In (b), the ejector pin 450 is lifted up, and the ejector pin 450 pushes up the bending point 440. Therefore, the laminated body of the first metal foil 200 and the second metal foil 202 is lifted up from the bending point 440. Figure 6 In (c), the ejector pin 450 returns to its original position. The bending point 440 remains in the state after being raised. Figure 6 In (d), the stacked body of the first metal foil 200 and the second metal foil 202 is lifted from the bending point 440 .

[0047] According to the present embodiment, the first metal foil 200 and the second metal foil 202 are bent at the bending point 440 in such a manner that the second metal foil 202 overlaps the first surface 400 of the first metal foil 200 and contacts the second surface 402, so that the first metal foil 200 can be exposed with a simple structure. In addition, by exposing the first metal foil 200 with a simple structure, an electrode plate 280 that is not prone to wrinkles can be provided. In addition, the second end 412 of the first metal foil 200 is aligned with the fourth end 422 of the second metal foil 202, so that the first metal foil 200 can be exposed on one side and not exposed on the opposite side. In addition, by adjusting the position of the bending point 440, the exposed area of ​​the first metal foil 200 can be adjusted. In addition, the exposed area of ​​the first metal foil 200 is adjusted, so that design changes can be easily made.

[0048] (Example 2)

[0049] Next, Example 2 is described. In the electrode plate 280 of Example 1, the first metal foil 200 is exposed from the second metal foil 202 on one surface side, and the opposite side is covered only by the second metal foil 202. When the second metal foil 202 includes a surplus portion, the surplus portion causes a reduction in the surplus space in the battery 10. Here, the description will be centered on the differences from Example 1.

[0050] Figure 7 (a) to (e) show the manufacturing process of the electrode plate 282. Figure 7 (a) and Figure 4 The same as (a). Figure 7 (b) shows Figure 7 (a) after the processing. Figure 7 The upper part of (b) is a top view. Figure 7 The lower part of (b) is a side view. A laminate is formed by overlapping the second metal foil 202 on the first surface 400 of the first metal foil 200. When overlapping the first metal foil 200 and the second metal foil 202, the second end 412 of the first metal foil 200 is aligned with the fourth end 422 of the second metal foil 202. In addition, the third end 420 of the second metal foil 202 is aligned with a position closer to the second end 412 side than the first end 410 of the first metal foil. As described above, the width of the second metal foil 202 is larger than the width of the first metal foil 200.

[0051] Figure 7 (c) shows Figure 7 (b) The subsequent processing. Figure 7 The upper part of (c) is a top view. Figure 7 As described above, the width of the second metal foil 202 is greater than that of the first metal foil 200 , and therefore, in order to make the width of the second metal foil 202 consistent with that of the first metal foil 200 , a portion of the second metal foil 202 is cut.

[0052] Figure 8 (a) to (h) show the structure of the laminate. Figure 8 (a) is a plan view of the second metal foil 202 and the first metal foil 200 (not shown) that are crimped together, as viewed from the second metal foil 202 side. A first boundary 300 and a second boundary 302 are formed.

[0053] The gap 212 is formed between the first boundary 300 and the second boundary 302 . On the other hand, the portions other than the gap 212 are subjected to crimping. The crimping force of the gap 212 is weaker than the crimping force of the portions other than the gap 212 .

[0054] Figure 8 (b) is Figure 8The cross-sectional view taken along the AA′ direction of (a) is a cross-sectional view of the intermittent portion 212. A weakly pressed portion 220 is disposed between the first metal foil 200 and the second metal foil 202. The weakly pressed portion 220 is a portion where the pressing force is weak.

[0055] like Figure 8 As shown in (a), the portion of the second metal foil 202 that is connected to one end of the first metal foil 200 is the third boundary 304, and the portion that is connected to the other end of the first metal foil 200 is the fourth boundary 306. The portion outside the third boundary 304 is the first remaining portion 210a, and the portion outside the fourth boundary 306 is the second remaining portion 210b. The first remaining portion 210a and the second remaining portion 210b are collectively referred to as the remaining portion 210. The remaining portion 210 is a portion extending from the first metal foil 200 and is a portion that is not bonded to the first metal foil 200.

[0056] Figure 8 (d) is Figure 8 A cross-sectional view taken along the BB′ direction of (a) The first metal foil 200 and the second metal foil 202 overlap each other, and the weakly pressed portion 220 is not provided. Figure 8 (d) is Figure 8 As described above, the weak crimping portion 220 is disposed only in the intermittent portion 212 , and the weak crimping portion 220 is not disposed in the portion other than the intermittent portion 212 .

[0057] Figure 8 (e) shows the portion peeled off from the second metal foil 202. As shown in the figure, the remaining portion 210 and the intermittent portion 212 are peeled off. Figure 8 (f) shows Figure 8 The electrode plate 280 is a remaining laminated body in which the second metal foil 202 is peeled off as shown in (e). The first metal foil 200 is exposed from a part of the second metal foil 202. Figure 8 (g) is Figure 8 The DD′ cross-sectional view of (f) includes only the first metal foil 200 . Figure 8 (h) is Figure 8 The EE' cross-sectional view of (f) shows a first metal foil 200 and a second metal foil 202 stacked. The stacked body cut into a plurality of Figure 7 (c).

[0058] Figure 7 (d) shows Figure 7 (c) The subsequent processing. Figure 7 The upper part of (d) is a top view. Figure 7The lower part of (d) is a side view. The center of the first end 410 and the second end 412 of the first metal foil 200 shows a center position 430. In addition, a bending point 440 is arranged between the center position 430 and the second end 412.

[0059] Figure 7 (e) shows Figure 7 (d) The subsequent processing. Figure 7 The upper part of (e) is a top view. Figure 7 The middle part of (e) is a bottom view. Figure 7 The lower part of (e) is a side view. The first metal foil 200 and the second metal foil 202 are bent at the bending point 440 in a manner that the second surface 402 of the first metal foil 200 is contacted. That is, the first metal foil 200 and the second metal foil 202 are bent in a manner that the second end 412 and the fourth end 422 face downward. In the lower surface, the second surface 402 of the first metal foil 200 is exposed between the first end 410 and the second end 412. In addition, in the upper surface, the first surface 400 of the first metal foil 200 is exposed between the first end 410 and the third end 420. Figure 7 (e) is an electrode plate 282 , which is used as the negative electrode 40 , for example.

[0060] According to this embodiment, the third end 420 of the second metal foil 202 is aligned to a position closer to the second end 412 than the first end 410 of the first metal foil 200, so that the first metal foil 200 is exposed between the first end 410 and the third end 420, thereby providing an electrode plate 282 with the first metal foil 200 exposed on both sides.

[0061] The embodiments of the present disclosure have been described in detail above. The aforementioned embodiments merely illustrate specific examples for implementing the present disclosure. The contents of the embodiments do not limit the technical scope of the present disclosure, and various design changes such as changes, additions, and deletions of constituent elements can be made without departing from the scope of the idea of ​​the invention defined in the claims. The new embodiments with design changes have the respective effects of the combined embodiments and deformations. In the aforementioned embodiments, the contents that can be subjected to such design changes are emphasized by expressions such as "in this embodiment", "in this embodiment", etc., and design changes are allowed even without such expressions. In addition, any combination of the constituent elements contained in the embodiments is also valid as a scheme of the present disclosure. The hatching marked on the cross-section of the accompanying drawings does not limit the material of the object marked with the hatching.

[0062] The embodiments can also be determined by the items described below.

[0063] [First item]

[0064] An electrode plate (280, 282), comprising:

[0065] A first metal foil (200) has a first surface (400) and a second surface (402) facing the opposite side of the first surface (400), and is provided with a first end (410) and a second end (412) at both ends in one direction, and

[0066] The second metal foil (202) is provided with a third end portion (420) and a fourth end portion (422) at both ends in the one direction;

[0067] The second end (412) of the first metal foil (200) is aligned with the fourth end (422) of the second metal foil (202), and the second metal foil (202) overlaps the first surface (400) of the first metal foil (200).

[0068] A bending point (440) is arranged between a central position (430) of the first end (410) and the second end (412) of the first metal foil (200) and the second end (412), and the first metal foil (200) and the second metal foil (202) are bent at the bending point (440) in such a manner as to contact the second surface (402) of the first metal foil (200).

[0069] The second surface (402) of the first metal foil (200) is exposed between the first end (410) and the second end (412).

[0070] [Second item]

[0071] The electrode plate (280) as described in the first item,

[0072] The first end (410) of the first metal foil (200) and the third end (420) of the second metal foil (202) are also aligned, and the second metal foil (202) overlaps the first surface (400) of the first metal foil (200).

[0073] The first surface (400) of the first metal foil (200) is not exposed.

[0074] [Third Item]

[0075] The electrode plate (282) as described in the first item,

[0076] The third end portion (420) of the second metal foil (202) is aligned at a position closer to the second end portion (412) than the first end portion (410) of the first metal foil (200), and the second metal foil (202) overlaps the first surface (400) of the first metal foil (200).

[0077] The first surface (400) of the first metal foil (200) is exposed between the first end (410) and the third end (420).

[0078] [Fourth Item]

[0079] A method for manufacturing an electrode plate (280, 282), comprising:

[0080] A step of forming a laminated body for a first metal foil (200) having a first surface (400) and a second surface (402) facing the opposite side of the first surface (400), and having a first end (410) and a second end (412) arranged at both ends in one direction, and a second metal foil (202) having a third end (420) and a fourth end (422) arranged at both ends in the one direction, wherein the laminated body has a structure in which the second end (412) of the first metal foil (200) and the fourth end (422) of the second metal foil (202) are aligned and the second metal foil (202) overlaps the first surface (400) of the first metal foil (200); and

[0081] A step of configuring a bending point (440) at a central position (430) between the first end (410) and the second end (412) of the first metal foil (200) and between the second end (412), and bending the first metal foil (200) and the second metal foil (202) at the bending point (440) in such a manner as to contact the second surface (402) of the first metal foil (200).

[0082] [Fifth Item]

[0083] The method for manufacturing the electrode plate (280) as described in the fourth item,

[0084] In the step of forming the laminate, the first end (410) of the first metal foil (200) and the third end (420) of the second metal foil (202) are also aligned, and the second metal foil (202) overlaps the first surface (400) of the first metal foil (200).

[0085] [Sixth Item]

[0086] The method for manufacturing the electrode plate (282) as described in the fourth item,

[0087] In the step of forming the stack, the third end (420) of the second metal foil (202) is aligned to a position closer to the second end (412) than the first end (410) of the first metal foil (200), and the second metal foil (202) overlaps the first surface (400) of the first metal foil (200).

[0088] Industrial Applicability

[0089] According to the present disclosure, it is possible to provide an electrode plate that is less likely to wrinkle.

[0090] Description of Reference Numerals

[0091] 10 battery, 14 electrode body, 15 case body, 16 sealing body, 17, 18 insulating plate, 19 positive electrode lead, 20 negative electrode lead, 21 extension portion, 22a filter opening, 22 filter, 23 lower valve body, 24 insulating member, 25 upper valve body, 26a cover opening, 26 cover, 27 gasket, 30 positive electrode, 31 positive electrode collector, 32 positive electrode active material layer, 40 negative electrode, 41 negative electrode collector, 42 negative electrode active material layer, 43 exposed portion, 50 gasket, 100 first metal foil roll, 102 second metal foil Roller material, 110 first crimping roller, 112 second crimping roller, 180 manufacturing device, 200 first metal foil, 202 second metal foil, 210 remaining part, 212 intermittent part, 220 weak crimping part, 280, 282 electrode plates, 300 first boundary, 302 second boundary, 304 third boundary, 306 fourth boundary, 400 first surface, 402 second surface, 410 first end, 412 second end, 420 third end, 422 fourth end, 430 central position, 440 bending point, 450 ejector pin.

Claims

1. An electrode plate, comprising: The first metal foil has a first surface and a second surface facing the opposite side of the first surface, and has a first end and a second end disposed at both ends in one direction, and The second metal foil is provided with a third end portion and a fourth end portion at both ends in the one direction; The second end of the first metal foil is aligned with the fourth end of the second metal foil, and the second metal foil overlaps the first surface of the first metal foil. A bending point is arranged between a central position of the first end and the second end of the first metal foil and the second end, and the first metal foil and the second metal foil are bent at the bending point so as to contact the second surface of the first metal foil. The second surface of the first metal foil is exposed between the first end and the second end.

2. The electrode plate according to claim 1, The first end of the first metal foil is also aligned with the third end of the second metal foil, and the second metal foil overlaps the first surface of the first metal foil. The first surface of the first metal foil is not exposed.

3. The electrode plate according to claim 1, The third end of the second metal foil is aligned at a position closer to the second end than the first end of the first metal foil, and the second metal foil overlaps the first surface of the first metal foil. The first surface of the first metal foil is exposed between the first end and the third end.

4. The method for manufacturing an electrode plate according to claim 1, comprising: A step of forming a laminated body with a first metal foil having a first surface and a second surface facing the opposite side of the first surface and having a first end and a second end arranged at both ends in one direction, and a second metal foil having a third end and a fourth end arranged at both ends in the one direction, wherein the second end of the first metal foil and the fourth end of the second metal foil are aligned and the second metal foil overlaps the first surface of the first metal foil; as well as A step of arranging a bending point between a center position between the first end and the second end of the first metal foil and the second end, and bending the first metal foil and the second metal foil at the bending point so as to contact the second surface of the first metal foil.

5. The method for manufacturing an electrode plate according to claim 4, In the step of forming the stacked body, the first end of the first metal foil and the third end of the second metal foil are also aligned, and the second metal foil overlaps the first surface of the first metal foil.

6. The method for manufacturing an electrode plate according to claim 4, In the step of forming the laminated body, the third end portion of the second metal foil is aligned closer to the second end portion than the first end portion of the first metal foil, and the second metal foil overlaps the first surface of the first metal foil.