Coating manufacturing process of photoresist
Through the precise steps and position control of the nozzles of two robotic arms, the problem of high photoresist usage in semiconductor manufacturing is solved, the cost reduction and the integrity of the coating area is achieved, and the photoresist liquid is ensured. Evenly covering and pure ingredients.
Patent Information
- Application Number
- CN202310509955.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-08
- Publication Date
- 2024-11-08
AI Technical Summary
In the semiconductor manufacturing process, it is difficult for the prior art to effectively save the amount of photoresist, while ensuring the integrity of the coating area, resulting in high production costs.
Two mechanical arms are used to control the first nozzle and the second nozzle respectively. The first nozzle is used to spray wetting liquid and the second nozzle is used to spray photoresist liquid. Through precise spraying steps and position control, the photoresist is reduced. The amount of resist liquid used.
It is achieved without affecting the integrity of the coating area, reducing the use of photoresist, reducing production costs, and ensuring uniform coverage of the photoresist liquid and purifying the composition.
Smart Images

Figure CN118904670A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a coating and manufacturing process of a photoresist, and in particular to coating the photoresist in a manner of respectively controlling a first nozzle and a second nozzle by two mechanical arms. Background Art
[0002] Photoresist is a key material used in the semiconductor manufacturing process. It is a photosensitive polymer applied to a substrate, which is selectively exposed to the patterned photoresist, and then an etching process is used to remove the substrate using the patterned photoresist as a mask to leave a pattern layer on the substrate. The use of photoresist is essential in the production of integrated circuits and other semiconductor components. It allows for the precise patterning of complex circuits and structures on a microscopic scale, enabling the production of smaller and more powerful electronic devices.
[0003] Therefore, photoresist is an important part of the semiconductor manufacturing process. It can accurately compose complex circuits and structures on a microscopic scale. Its use is crucial to the production of advanced electronic equipment and technology. Photoresist is used in multiple semiconductor manufacturing processes. Therefore, if the amount of photoresist can be saved but still achieve the predetermined coating area, the production cost can be reduced. Summary of the invention
[0004] In view of this, the present invention provides a photoresist coating process, which uses two mechanical arms to respectively control a first nozzle to spray a wetting liquid and a second nozzle to spray a photoresist liquid, so as to reduce the usage of the photoresist liquid.
[0005] According to a preferred embodiment of the present invention, a photoresist coating process comprises first providing a wafer rotating table, a wafer being arranged on the wafer rotating table, a first nozzle being suspended from a first mechanical arm, a second nozzle being suspended from a second mechanical arm, wherein the first nozzle is used to spray a wetting liquid, and the second nozzle is used to spray a photoresist liquid, and then performing a photoresist coating process, wherein the photoresist coating process comprises the following operations from step 1 to step 4, step 1 comprises moving the first nozzle to the center of the wafer and starting to spray a wetting liquid; The method comprises the steps of: step 1, moving the first nozzle to a predetermined position toward the edge of the wafer, and moving the second nozzle to the center of the wafer and starting to spray the photoresist liquid onto the upper surface of the wafer after the first nozzle leaves the center of the wafer. The method comprises the steps of: stopping spraying the wetting liquid before the photoresist liquid flows to the bottom of the first nozzle. The method comprises the steps of: moving the second nozzle out of the wafer after the photoresist liquid completely covers the upper surface of the wafer. The photoresist coating process is performed in the order of step 1, step 2, and step 3 to step 4.
[0006] In order to make the above-mentioned objectives, features and advantages of the present invention more clearly understood, the following is a detailed description of the preferred embodiments and the accompanying drawings. However, the following preferred embodiments and drawings are only for reference and explanation, and are not intended to limit the present invention. BRIEF DESCRIPTION OF THE DRAWINGS
[0007] Figures 1 to 6 A schematic diagram of a photoresist coating process according to a preferred embodiment of the present invention;
[0008] Figure 7 A schematic diagram of a baking process.
[0009] Main component symbols
[0010] 10: Wafer Rotation Table
[0011] 12: Chip
[0012] 12a: semiconductor substrate
[0013] 12b: Material layer
[0014] 14a: First nozzle
[0015] 14b: Second nozzle
[0016] 16a: The first robotic arm
[0017] 16b: Second Robotic Arm
[0018] 18: Wetting fluid
[0019] 20: Photoresist liquid
[0020] 22: Photoresist layer DETAILED DESCRIPTION
[0021] like Figure 1 As shown, a wafer rotating platform 10 is provided, a wafer 12 is disposed on the wafer rotating platform 10, a first nozzle 14a is suspended from a first mechanical arm 16a, and a second nozzle 14b is suspended from a second mechanical arm 16b, wherein the first nozzle 14a is used to spray a wetting liquid, and the second nozzle 14b is used to spray a photoresist liquid. The wafer 12 may only include a semiconductor substrate 12a, or the wafer 12 may be a semiconductor substrate 12a stacked with a material layer 12b, such as a semiconductor substrate 12a stacked with silicon oxide, silicon nitride, semiconductor material or dielectric material.
[0022] Next, a photoresist coating process will be performed. The photoresist coating process includes step 1, step 2, step 3 and step 4. The coating process is performed in the order of step 1, step 2, step 3 and step 4. During the process of step 1 to step 4, the wafer rotating table 10 rotates continuously, so the wafer 12 placed on the wafer rotating table 10 also rotates continuously during the process of step 1 to step 4. The following will explain step 1, step 2, step 3 to step 4 in sequence with the help of the diagram.
[0023] like Figure 2 As shown, step one of the photoresist coating process is performed. Step one includes moving the first nozzle 12a to the center of the wafer 12 and starting to spray the wetting liquid 18, so that the wetting liquid 18 contacts the material layer 12b and is coated on the material layer 12b. However, if the wafer 12 is only composed of the semiconductor substrate 12a, the wetting liquid 18 will directly contact the semiconductor substrate 12a. In the subsequent description of the present invention, the wafer 12 includes the semiconductor substrate 12a and the material layer 12b as an example. Step one is preferably performed for several seconds, such as 3 to 5 seconds, at which time the wetting liquid 18 has at least been coated directly above the center of the wafer 12. In step one, the second nozzle 16b has not been activated, that is, the photoresist liquid has not been sprayed out. According to a preferred embodiment of the present invention, the second nozzle 16b does not overlap with the wafer 12 in step one.
[0024] like Figure 3 As shown, the second step of the photoresist coating process is performed. The second step includes moving the first nozzle 14a to a predetermined position toward the edge of the wafer 12. The predetermined position is between the center of the wafer 12 and the edge of the wafer 12. When the first nozzle 14a leaves the center of the wafer 12, the second nozzle 14b is moved to the center of the wafer 12 and begins to spray the photoresist liquid 20. The first nozzle 14a continues to spray the wetting liquid 18 during the movement, and the photoresist liquid 20 flows from the center of the wafer 12 to the edge of the wafer 10 and is coated on the wetting liquid 18. The second step is preferably performed for several seconds, for example, 3 to 5 seconds. Figure 4As shown, step 3 in the photoresist coating process is performed. Step 3 is preferably performed for several seconds, for example, 3 to 5 seconds. As the total number of rotations of the wafer 12 increases, before the photoresist liquid 20 flows to the bottom of the first nozzle 14a, the first nozzle 14a is closed, that is, the spraying of the wetting liquid 18 is stopped. Then, depending on the manufacturing process design, the first nozzle 14a can be selectively moved out of the top of the wafer 12 so that the first nozzle 14a and the wafer 12 do not overlap, that is, the first nozzle 14a can continue to stay above the wafer 12 in the closed state. In this embodiment, the first nozzle 14a is removed from the top of the wafer 12 as an example. According to another preferred embodiment of the present invention, before the photoresist liquid 20 flows to the bottom of the first nozzle 14a, the first nozzle 14a may not be closed, that is, the first nozzle 14a is moved out of the top of the wafer 12 while the wetting liquid 18 is continuously sprayed. If the first nozzle 14a is not moved out from above the wafer 12 or the first nozzle 14a is not closed, the wetting liquid 18 sprayed from the first nozzle 14a will be sprayed directly above the photoresist liquid 20, causing the photoresist liquid 20 and the wetting liquid 18 to mix, causing the composition of the photoresist liquid 20 to change, thereby affecting subsequent exposure results.
[0025] like Figure 5 and Figure 6 As shown, after closing the first nozzle 14a or moving the first nozzle 14a out, the photoresist liquid 20 and the wetting liquid 18 continue to flow toward the edge of the wafer 12 until the photoresist liquid 20 and the wetting liquid 18 completely cover the upper surface of the wafer 12. At this time, step four is performed. When the photoresist liquid 20 completely covers the upper surface of the wafer 12, the second nozzle 14b is closed, and the second nozzle 14b is selectively moved out of the top of the wafer 12 to end the photoresist coating process. According to another preferred embodiment of the present invention, the second nozzle 14b may not be closed, that is, the second nozzle 14b is moved out of the top of the wafer 12 while the photoresist liquid 20 is continuously sprayed. The operation time of step four is preferably between 10 and 30 seconds. Figure 7 As shown, a baking process is performed to solidify the photoresist liquid 20 into a photoresist layer 22. After the baking process, the wetting liquid 18 is essentially completely volatile, and then an exposure and development process can be performed.
[0026] According to a preferred embodiment of the present invention, the wetting liquid 18 includes deionized water, cyclohexanone, propylene glycol monomethyl ether or propylene glycol monomethyl ether acetate. The function of the wetting liquid 18 is to wet the surface of the wafer 12 so that the photoresist liquid 20 is easy to apply and the amount of the photoresist liquid 20 used can be reduced. In the present invention, the wetting liquid 18 and the photoresist liquid 20 are sprayed from two nozzles suspended on different robotic arms, so the positions where the wetting liquid 18 and the photoresist liquid 20 are sprayed can be operated independently. If the two nozzles are suspended on the same robotic arm, the positions of the two nozzles will be very close. Therefore, when spraying the photoresist liquid 20, the spraying of the wetting liquid 18 must be stopped, otherwise the wetting liquid 18 will be mixed into the photoresist liquid 20, which will cause the edge of the wafer 12 to be unable to be completely covered by the wetting liquid 18, thereby affecting the application of the photoresist liquid 20. The method of the present invention reduces the problem of the wetting liquid 18 being mixed into the photoresist liquid 20 and also enables the wetting liquid 18 to completely cover the wafer 12 .
[0027] The above descriptions are only preferred embodiments of the present invention. All equivalent changes and modifications made according to the claims of the present invention should fall within the scope of the present invention.
Claims
1. A photoresist coating process, comprising: A wafer rotating platform is provided, on which a wafer is arranged, a first nozzle is suspended from a first mechanical arm, and a second nozzle is suspended from a second mechanical arm, wherein the first nozzle is used for spraying a wetting liquid, and the second nozzle is used for spraying a photoresist liquid; A photoresist coating process is performed, wherein the photoresist coating process comprises: Step 1: Move the first nozzle directly above the center of the wafer and start spraying the wetting liquid; Step 2: moving the first nozzle to a predetermined position toward the edge of the wafer, and when the first nozzle leaves the position directly above the center of the wafer, moving the second nozzle to the position directly above the center of the wafer and starting to spray the photoresist liquid onto the upper surface of the wafer; Step 3: before the photoresist liquid flows to the bottom of the first nozzle, closing the first nozzle; Step 4: When the photoresist liquid completely covers the upper surface of the wafer, the second nozzle is closed; wherein the photoresist coating process is performed in the order of step 1, step 2, step 3 to step 4. 2 . The photoresist coating process as claimed in claim 1 , wherein in step 1 and step 2, the first nozzle continuously sprays the wetting liquid. 3 . The photoresist coating process as claimed in claim 1 , wherein during the photoresist coating process, the second nozzle continuously sprays the photoresist liquid. 4 . The photoresist coating process as claimed in claim 1 , wherein during the photoresist coating process, the wafer rotating stage continuously rotates the wafer. 5 . The photoresist coating process as claimed in claim 1 , wherein the wetting solution comprises deionized water, cyclohexanone, propylene glycol monomethyl ether or propylene glycol monomethyl ether acetate. 6 . The photoresist coating process as claimed in claim 1 , wherein the first robot arm and the second robot arm operate independently of each other. 7 . The photoresist coating process as claimed in claim 1 , wherein the predetermined position is located between the center of the wafer and the edge of the wafer.
8. The photoresist coating process as claimed in claim 1, wherein after the step 4, a baking process is performed to solidify the photoresist liquid into a photoresist layer. 9 . The photoresist coating process as claimed in claim 1 , wherein the step three further comprises moving the first nozzle out from above the wafer after closing the first nozzle.
10. The photoresist coating process as claimed in claim 1, wherein the step 4 further comprises moving the second nozzle out of the wafer after closing the second nozzle.