Deflection compensation method for double-groove die
By calculating the deflection compensation values of single molds and double groove molds, drawing contour curves and summing compensation, the problem of serious deflection deformation deviation during the double groove mold forming process is solved, and the accuracy of mold processing and product quality are improved.
Patent Information
- Application Number
- CN202411207479.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-30
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2044-08-30
AI Technical Summary
During the molding process, the deflection deformation deviation caused by the forming pressure is severe, which affects the mold research and integration and product quality.
By determining the center point deflection compensation value of single mold and double groove mold, drawing multiple contour curves, calculating the first and second deflection compensation values of the points to be measured, and summing them as the final deflection compensation value, performing Compensation for processing data stages of double-slot molds.
It effectively improves the deformation deviation of the double-slot mold, ensures that the mold processing data is more in line with the actual deflection deformation, and improves the accuracy of mold research and integration and product quality.
Smart Images

Figure CN118905068A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of mold processing, and in particular to a double-groove mold deflection compensation method. Background Art
[0002] The forming pressure of automobile stamping and drawing dies can reach thousands of tons during operation. The dies and worktables will produce deflection deformation. The deflection deformation of the dies will cause the upper and lower model surfaces to be inconsistent and the side walls of the product in the cavity to interfere, which will lead to a large amount of mold grinding. Designers often need to compensate for the deflection of the dies during mold processing and machining. When performing deflection compensation on the mold, designers often perform deformation compensation on the mold during the mold processing data stage. A common mold compensation method is to first select the center point of the mold as the starting point, and then draw multiple contour closed curves with the center point of the mold. The multiple contour closed curves are arranged from the inside to the outside with the center point of the mold as the center; the center point of the mold is the maximum compensation point, the deflection compensation values on the contour curves are equal, and the deflection compensation values of the multiple contour curves decrease in sequence from the direction close to the center point of the mold to the direction away from the center point of the mold.
[0003] The double-slot mold includes two single molds that are fixedly connected. The double-slot mold has two machining centers, which are the center points of the two single molds respectively. The molding force of the double-slot mold is concentrated on the production centers of the two single molds respectively. The center point of the double-slot mold is inconsistent with the machining center of the double-slot mold. If the contour curve of the double-slot mold is directly drawn with the center point of the double-slot mold, the double-slot mold will produce relatively serious deformation deviation. Summary of the invention
[0004] The main purpose of the present invention is to propose a double-groove die deflection compensation method, aiming to improve the problem of serious deformation deviation of the double-groove die.
[0005] To achieve the above object, the present invention proposes the following steps: S1: determining a deflection compensation value of a center point of a single mold, drawing a plurality of first contour curves with the center point of the single mold as the center, and determining a deflection compensation value of any of the first contour curves; S2: determining a deflection compensation value of a center point of the double-groove mold, drawing a plurality of second contour curves with the center point of the double-groove mold, and determining a deflection compensation value of any of the second contour curves; S3: Select any point on the single mold as the point to be tested; S4: Calculating a first deflection compensation value of the point to be measured according to the positional relationship between the point to be measured and the first contour curve; S5: Calculating a second deflection compensation value of the point to be measured according to the positional relationship between the point to be measured and the second contour curve; S6: summing the first deflection compensation value of the point to be measured and the second deflection compensation value of the point to be measured to obtain a final deflection compensation value of the point to be measured; S7: Select other points to be measured and repeat steps S4-S6; S8: In the processing data stage of the double-groove mold, the double-groove mold is deflected and compensated according to the final deflection compensation value of the point to be measured.
[0006] In one embodiment, step S1 further includes the following steps: S11: Use the finite element analysis (FEA) numerical simulation method to perform stress analysis on the single mold, observe the deformation of the single mold under the simulated load, and record the deflection deformation at each position of the single mold; S12: The sum of the deflection deformation of the center point of a single mold and the manufacturing error is used as the deflection compensation value of the center point of the single mold.
[0007] In one embodiment, in step S2, the plurality of second contour curves are a plurality of concentric circles, and the centers of the second contour curves coincide with the center point of the double-groove mold.
[0008] In one embodiment, taking the die of the double-slot mold as the negative direction, the deflection compensation value of the center point of the double-slot mold is -0.40mm; the maximum distance between the center of the double-slot mold and the edge of the die of the double-slot mold is set to L, and the second contour curves are set to three, the radius R1=L*0.2 of the first second contour curve, and the deflection compensation value of the first second contour curve is -0.24mm; the radius R2=L*0.8 of the second second contour curve, and the deflection compensation value of the second second contour curve is 0mm; the radius R3=L*1.4 of the third second contour curve, and the deflection compensation value of the second second contour curve is 0.12mm.
[0009] In one embodiment, step S4 comprises: S41: Taking the center point of the single mold as the starting point, draw a first ray passing through the point to be measured; S42: dividing the first ray into a plurality of first line segments by means of a single mold center point and a plurality of the first contour curves; S43: measuring the length of the first line segment where the point to be measured is located, and then calculating the slope of the first line segment where the point to be measured is located; S44: measuring the distance between the point to be measured and the endpoint of the first line segment where the point to be measured is located, and calculating the first deflection compensation value of the point to be measured according to the slope of the first line segment where the point to be measured is located.
[0010] In one embodiment, step S5 includes: S51: Taking the center point of the double-groove mold as the starting point, draw a second ray passing through the point to be measured; S52: dividing the second ray into a plurality of second line segments through the center point of the double-groove mold and the plurality of second contour curves; S53: measuring the length of the second line segment where the point to be measured is located, and calculating the slope of the second line segment where the point to be measured is located; S54: measuring the distance between the point to be measured and the endpoint of the second line segment where the point to be measured is located, and calculating the second deflection compensation value of the point to be measured according to the slope of the second line segment where the point to be measured is located.
[0011] In one implementation, in step S1, the number of the first contour curves is three.
[0012] In one embodiment, with the concave mold of the double-groove mold as the negative direction, when a single mold is used to process the automobile outer panel, the deflection compensation value of the center point of the single mold is -0.26mm, and the deflection compensation values of the three first contour curves are -0.14mm, 0mm and 0.12mm respectively.
[0013] In one embodiment, with the concave mold of the double-groove mold as the negative direction, when a single mold is used to process the automobile inner panel, the deflection compensation value of the center point of the single mold is -0.32 mm, and the deflection compensation values of the three first contour curves are -0.16 mm, 0 mm and 0.12 mm respectively.
[0014] In one embodiment, when the two single molds are symmetrical to each other, the deflection compensation values at the symmetrical points of the two single molds are equal; Step S7 includes: S71: Calculate the final deflection compensation value of the point to be measured on a single mold: S72: A symmetrical point of the point to be measured on another single mold is obtained by an axisymmetric method, and the deflection compensation value of the symmetrical point is equal to the deflection compensation value of the point to be measured.
[0015] The technical solution of the present invention takes into account that the center of the single mold is a concentrated force point, and draws a first contour curve with the concentrated force point of the single mold as the center point, and then obtains the first deflection compensation value of the point to be measured. The first deflection compensation value can compensate for the deflection deformation of the single mold with the center point of the single mold as the center; taking into account the deflection deformation of the double-slot mold as a whole, a second contour curve is drawn with the center point of the double-slot mold as the center, and the second deflection compensation value of the point to be measured is obtained. The second deflection compensation value is the deflection compensation for the deflection deformation of the double-slot mold as a whole; the first deflection compensation value and the second deflection compensation value are summed to obtain a final deflection compensation value, and the final deflection compensation value is related to both the deflection deformation of the double-slot mold as a whole and the deflection deformation of the single mold itself as a concentrated force point; compensating the double-slot mold with the final deflection compensation value can improve the problem of serious deformation deviation of the double-slot mold. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on the structures shown in these drawings without paying creative work.
[0017] Figure 1 A schematic diagram of the first contour curve in step S1 in an embodiment of the double-groove mold deflection compensation method provided by the present invention; Figure 2 A schematic diagram of the second contour curve in step S2 in the embodiment of the double-groove mold deflection compensation method provided by the present invention; Figure 3 An overall schematic diagram of a first contour curve and a second contour curve in an embodiment of a double-groove die deflection compensation method provided by the present invention; Figure 4 It is a schematic diagram of obtaining the positioning points on a single mold in step S1 in an embodiment of the present invention; Figure 5 It is a schematic diagram of finding the centers of each circle on a single mold in step S1 in an embodiment of the present invention; Figure 6 This is a schematic diagram of obtaining the radius corresponding to each center of a circle on a single mold in step S1 in an embodiment of the present invention; Figure 7 It is a schematic diagram of making circles with the centers of each circle on a single mold in step S1 in an embodiment of the present invention; Figure 8 It is a schematic diagram of connection of definition lines on a single mold in step S1 in an embodiment of the present invention; Fig. 9Schematic diagram of multiple definition lines on a single mold in step S1 in an embodiment of the present invention.
[0018] Description of Figure Numbers: 1. Double-slot mold; 11. Single mold; 2. First contour curve; 3. Second contour curve; 4. First ray; 41. First line segment; 5. Second ray; 51. Second line segment; The realization of the purpose, functional features and advantages of the present invention will be further explained in conjunction with embodiments and with reference to the accompanying drawings. DETAILED DESCRIPTION
[0019] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0020] It should be noted that if the embodiments of the present invention involve directional indications (such as up, down, left, right, front, back, etc.), the directional indications are only used to explain the relative position relationship, movement status, etc. between the components in a certain specific posture. If the specific posture changes, the directional indication will also change accordingly.
[0021] In addition, if there are descriptions involving "first", "second", etc. in the embodiments of the present invention, the descriptions of "first", "second", etc. are only used for descriptive purposes and cannot be understood as indicating or implying their relative importance or implicitly indicating the number of technical features indicated. Therefore, the features limited to "first" and "second" may explicitly or implicitly include at least one of the features. In addition, if "and / or" or "and / or" appears in the full text, its meaning includes three parallel solutions. Taking "A and / or B" as an example, it includes solution A, solution B, or solutions that satisfy both A and B. In addition, the technical solutions between the various embodiments can be combined with each other, but it must be based on the ability of ordinary technicians in this field to implement. When the combination of technical solutions is contradictory or cannot be implemented, it should be deemed that such combination of technical solutions does not exist and is not within the scope of protection required by the present invention.
[0022] The forming pressure of automobile stamping and drawing dies can reach thousands of tons. The dies and workbenches will produce deflection deformation under heavy load. In order to cope with the deflection deformation of the stamping die, the lower side (concave surface) of the die (generally the upper die) will be deflected and compensated. The deflection compensation is carried out with the center point of the single-slot die as the starting point. The deflection compensation amount downward from the center point of the single-slot die is the largest, and the rest is driven by contour curves to deform the die surface. Common double-slot dies include two single dies, which are axially symmetrical and fixedly connected. The double-slot die can complete the production of two parts at the same time. The double-slot die has two production centers, and the center point of the double-slot die is inconsistent with the production center. The double-slot die is only deflected and compensated with the center point of the double-slot die as the starting point. The deflection deformation of the stress point of the single die is not taken into account. The double-slot die will produce a relatively serious deformation deviation.
[0023] The invention provides a double-groove die deflection compensation method to improve the problem of serious deformation deviation of the double-groove die.
[0024] See also Figure 1 , Figure 2 and Figure 3 The double-groove mold 1 includes two single molds 11 fixedly connected, the two single molds 11 are axially symmetrical, the center of the single mold 11 is the center of gravity of the single mold 11, and the center of the double-groove mold 1 is the intersection of the line between the centers of the two single molds 11 and the symmetry plane between the two single molds 11, that is, the center of the double-groove mold 1 is the center of gravity of the double-groove mold 1.
[0025] In the embodiment of the present application, the direction in which the double-slot mold 1 is close to its die is the negative direction, and the plane perpendicular to the negative direction is the working plane. The contour curves are all drawn on the working plane. If not specified, the center point of the single mold 11 is the positive projection of the center of the single mold 11 on the working plane, and the center point of the double-slot mold 1 is the positive projection of the center of the double-slot mold 1 on the working plane. When the deflection compensation value of a point of the double-slot mold 1 is a negative value, it means that the die surface of the double-slot mold 1 is compensated for the protrusion along the negative direction, and the height value of the protrusion compensation is the absolute value of the deflection compensation.
[0026] The method comprises the following steps: Step S1: firstly obtain the deflection compensation value of the center point of the single mold 11 by an analytical method, then select a suitable number of first contour curves 2 according to the requirements, and determine the deflection compensation value corresponding to each first contour curve 2; finally draw the first contour curve 2 on the working plane with the center point of the single mold 11 as the center; Step S2: first determine the deflection compensation value of the center point of the double-groove mold 1, then select a suitable number of second contour curves 3, and select the deflection compensation value corresponding to each second contour curve 3 according to the number of the second contour curves 3; finally, draw the second contour curve 3 on the working plane with the center point of the double-groove mold 1 as the center; Step S3: Select any point on the single mold 11 as a point to be tested; Step S4: Given the deflection compensation value of the center point of the single mold 11 and the deflection compensation value corresponding to each first contour curve 2, the first deflection compensation value of the point to be measured is calculated according to the position and distance relationship between the point to be measured and the plurality of first contour curves 2; Step S5: the deflection compensation value of the center point of the double-groove mold 1 and the deflection compensation value corresponding to each second contour curve 3 are known, and the second deflection compensation value of the point to be measured is calculated according to the position and distance relationship between the point to be measured and the plurality of second contour curves 3; Step S6: obtaining a final deflection compensation value of the point to be measured by summing the first deflection compensation value and the second deflection compensation value of the same point to be measured; Step S7: Select other points to be measured. The selection of multiple points to be measured can be carried out by sampling at equal intervals, and then repeat steps S4-S6 to obtain the final deflection compensation values of other points to be measured; obtain the final deflection compensation values of each point of the double-groove mold 1; Step S8: In the processing data stage of the double-slot mold 1, the final deflection compensation value of each position of the double-slot mold 1 is added to the processing numerical value of the double-slot mold 1, thereby adding deflection compensation to the double-slot mold 1 in the processing data stage of the double-slot mold 1.
[0027] Taking into account that the center point of the single mold 11 is the concentrated force point, the single mold 11 will produce deflection deformation centered on its center point. Taking the concentrated force point of the single mold 11 as the center point, the first deflection compensation value of the point to be measured is obtained. The first deflection compensation value can compensate for the deflection deformation of the single mold 11 centered on the center point of the single mold 11.
[0028] The double-slot mold 1 includes two single molds 11 fixedly connected. When the double-slot mold 1 processes parts, the deflection deformation of the double-slot mold 1 as a whole is taken into consideration. The second deflection compensation value of the point to be measured is obtained with the center point of the double-slot mold 1 as the center. The second deflection compensation value can compensate for the deflection deformation of the double-slot mold 1 as a whole.
[0029] In the technical solution provided by the present invention, the final deflection compensation value is obtained by summing the first deflection compensation value and the second deflection compensation value. The final deflection compensation value is related to the deflection deformation of the double-slot mold 1 as a whole, and also to the deflection deformation of the single mold 11 itself as a concentrated force point. The final deflection compensation value is more in line with the actual deflection deformation of the double-slot mold 1; using the final deflection compensation value to perform deflection compensation on the double-slot mold 1 can improve the problem of serious deformation deviation of the double-slot mold 1.
[0030] In one embodiment, in step S1, the step of determining the deflection compensation value of the center point of the single mold includes: Step S11: using a finite element analysis (FEA) numerical simulation method to perform a stress analysis on the single mold 11, observing the deformation of the single mold 11 under the simulated load, and recording the deflection deformation at each position of the single mold 11, especially recording the value of the deflection deformation at the center point of the single mold 11; Step S12: taking the sum of the deflection deformation of the center point of the single mold 11 and the manufacturing error as the deflection compensation value of the center point of the single mold 11.
[0031] When performing finite element numerical simulation analysis on the single mold 11 , the size of the single mold 11 and the size of the parts corresponding to the single mold 11 will affect the deflection deformation of the single mold 11 .
[0032] When performing force analysis on the single mold 11, the deflection deformation at the center point of the single mold 11 is the largest. After recording the deflection deformation value at the center point of the single mold 11, the deflection compensation value at the center point of the single mold 11 can be calculated. Taking the maximum deformation of the center point of the single mold 11 as 0.24mm as an example, the actual manufacturing process is often 0.02mm larger than the theoretical value, that is, the common manufacturing error is 0.02mm. When performing deflection compensation on the single mold 11, the deflection compensation acts on the concave surface of the single mold 11, and the sum of the maximum deformation of the center point of the single mold 11, 0.24mm, and the manufacturing error of 0.02mm, is used as the absolute value of the deflection compensation value at the center point of the single mold 11, that is, the deflection compensation value at the center point of the single mold 11 is -0.26mm.
[0033] In one embodiment of the present invention, in step S1, the number of first contour curves 2 is set to three, or the number of first contour curves 2 can be set to four, five or more according to requirements.
[0034] In one embodiment of the present invention, in step S1, when the single mold 11 is used to process the automobile outer panel, that is, when the single mold 11 is an outer panel mold, the deflection compensation value of the center point of the single mold 11 is set to -0.26mm, and then the deflection compensation values corresponding to the three first contour curves 2 are set to -0.16mm, 0mm and 0.12mm respectively, and the three first contour curves 2 are successively away from the center point of the single mold 11. Common automobile outer panels include left and right front door outer panels and left and right rear door outer panels. When the single mold 11 is an outer panel mold, the number of first contour curves 2 and the corresponding deflection compensation values of the first contour curves 2 can be directly selected, which reduces the preparation work before drawing the first contour curves 2. It is also possible to select other numbers of first contour curves 2 according to needs, determine the deflection compensation values corresponding to the first contour curves 2, and then draw the first contour curves 2 for the single mold 11.
[0035] In one embodiment of the present invention, in step S1, when the single mold 11 is used to process the inner panel of the automobile, that is, when the single mold 11 is an inner panel mold, the deflection compensation value of the center point of the single mold 11 is set to -32mm, and then the deflection compensation values corresponding to the three first contour curves 2 are set to -0.16mm, 0mm and 0.12mm respectively, and the three first contour curves 2 are successively away from the center point of the single mold 11. Common automobile inner panels include left and right front door inner panels and left and right rear door inner panels. When the single mold 11 is an inner panel mold, the number of first contour curves 2 and the corresponding deflection compensation values of the first contour curves 2 can be directly selected, and then the first contour curves 2 are drawn for the single mold 11, which reduces the preparation work before drawing the first contour curves 2. It is also possible to select other numbers of first contour curves 2 according to needs, determine the deflection compensation values corresponding to the first contour curves 2, and finally draw the first contour curves 2 for the single mold 11.
[0036] See also Figure 1 and Figure 3 In one embodiment of the present invention, step S4 includes: Step S41: Taking the center point of the single mold 11 on the working plane as the starting point, draw a first ray 4 passing through the point to be measured; Step S42: By means of the center point of the single mold 11 and the plurality of first contour curves 2, the first ray 4 can be divided into a plurality of first line segments 41, and any first line segment 41 does not cross any first contour curve 2; Step S43: one end point of the first line segment 41 where the test point is located is located on a first contour curve 2, and the other end point is located on another first contour curve 2 or the center point of the single mold 11, and the deflection compensation values of the two end points of the first line segment 41 where the test point is located are obtained, and the length of the line segment where the test point is located is measured, and the slope of the line segment where the test point is located is calculated; Specifically: assume that the two end points of the first line segment 41 where the test point is located are point N1 and point N2, and point N1 is located on the side of point N2 close to the center point of the single mold 11, the length of the first line segment 41 where the test point is located is set to N2-N1, the deflection compensation value corresponding to the first contour curve 2 where point N1 is located is set to h1, the deflection compensation value corresponding to the first contour curve 2 where point N2 is located is set to h2, and the slope of the first line segment 41 where the test point is located is K1=(h2-h1) / (N2-N1); Step S44: Measure the distance between the point to be measured and point N1 by means of a measuring tool, and set the distance between the point to be measured and point N1 as M-N1, and set the first deflection compensation value of the point to be measured as H1, then the first deflection compensation value of the point to be measured H1=(M-N1)*K1+h1; When the point to be measured is located on a first contour curve 2 , the first deflection compensation value of the point to be measured is equal to the deflection compensation value corresponding to the first contour curve 2 where the point is located.
[0037] When selecting the number of first contour curves 2, the density of the first contour curves 2 can be improved by increasing the number of first contour curves 2 and reducing the distance between the first contour curves 2, which is beneficial to reducing the length of each first line segment 41, and can make the multiple first line segments 41 more closely fit the deflection deformation curve of the single mold 11, so that the first deflection compensation value of the measured point is closer to the deflection deformation value of the measured point when the single mold 11 is deformed.
[0038] A common double-groove mold 1 is symmetrical along a symmetry plane, the symmetry plane of the double-groove mold 1 is perpendicular to the working plane, the double-groove mold 1 is axially symmetrical on the working plane, and the shape of the double-groove mold 1 is relatively regular; for this reason, in one embodiment of the present invention, in step S2, multiple second contour curves 3 are set as concentric circles, and the centers of the multiple second contour curves 3 are all the center points of the double-groove mold 1, which can facilitate the drawing of the second contour curves 3.
[0039] In one embodiment of the present invention, in step S2, the maximum value of the distance between the center point of the double groove mold 1 and the edge of the die of any single mold 11 on the working plane is set to L, and the second contour curve 3 is set to three, the radius R1 of the first second contour curve 3 is R1=L*0.2, and the deflection compensation value of the first second contour curve 3 is -0.24mm; the radius R2 of the second second contour curve 3 is R2=L*0.8, and the deflection compensation value of the second second contour curve 3 is 0mm; the radius R3 of the third second contour curve 3 is R3=L*1.4, and the deflection compensation value of the second second contour curve 3 is 0.12mm. Before drawing the second contour curve 3, the second contour curve 3 can be directly started by selecting the set number of second contour curves 3, which can improve the efficiency of drawing the second contour curve 3.
[0040] See also Figure 2 and Figure 3 In one embodiment of the present invention, step S5 includes: Step S51: Taking the center point of the double-groove mold 1 as the starting point, draw a second ray 5 passing through the point to be measured; Step S52: dividing the second ray 5 into a plurality of second line segments 51 through the center of the double-groove mold 1 and a plurality of second contour curves 3, and any second line segment 51 does not cross any second contour curve 3; Step S53: measuring the length of the second line segment 51 where the point to be measured is located, one end of the second line segment 51 is located on a second contour curve 3, and the other end is located on the second contour curve 3 or the center point of the double-groove mold 1, obtaining the deflection compensation values of the two ends of the second line segment 51 where the point to be measured is located, and calculating the slope of the second line segment 51 where the point to be measured is located; Specifically: Assume that the two end points of the second line segment 51 at both ends of the test point are point N3 and point N4 respectively, point N3 is located on the side of point N4 close to the center point of the double-groove mold 1, the length of the second line segment 51 where the test point is located is set to N4-N3, the deflection compensation value corresponding to the second contour curve 3 where point N3 is located is set to h3, and the deflection compensation value corresponding to the second contour curve 3 where point N4 is located is set to h4, then the slope K2 of the second line segment 51 where the test point is located is (h4-h3) / (N4-N3); Step S54: Measure the distance between the point to be measured and point N3 by means of a tool, and set the distance between the point to be measured and point N3 to be M-N3, and set the second deflection compensation value of the point to be measured to be H2, then the second deflection compensation value of the point to be measured can be obtained as H2=(M-N3)*K2+h3; When drawing the second contour curves 3, the density of the second contour curves can be increased by increasing the number of the second contour curves 3, so that the distance between adjacent second curves can be reduced, and the length of each second line segment 51 can be reduced, so that the plurality of second line segments 51 can be more closely matched to the overall deflection deformation curve of the double-groove mold 1. This makes the second deflection compensation value closer to the deflection compensation value of the deflection deformation of the double-groove mold 1 as a whole.
[0041] The common double-groove mold 1 is an axisymmetric figure, that is, the two single molds 11 on the double-groove mold 1 are axisymmetric to each other, the symmetry axis between the two single molds 11 is the symmetry axis of the double-groove mold 1 itself, the center points of the two single molds 11 are axisymmetric, and the symmetry axis between the two single molds 11 passes through the center point of the double-groove mold 1. When drawing the first contour curves 2 on the two single molds 11 respectively, two groups of first contour curves 2 with equal numbers and equal deflection values are often selected, so that the two groups of first contour curves 2 are axisymmetric about the symmetry axis of the double-groove mold 1.
[0042] The deflection compensation values of the center points of the two single molds 11 are equal, and the two groups of first contour curves 2 are axially symmetrical, so it can be obtained that the first deflection compensation values of two points axially symmetrical to each other on the two single molds 11 are equal.
[0043] The double-groove mold 1 is axially symmetrical, and the center point of the double-groove mold 1 is located on the symmetry line. The second contour curve 3 of the double-groove mold 1 is a concentric circle with the center point of the double-groove mold 1 as the center. It can be obtained that the second deflection compensation values of the two axially symmetrical points on the two single molds 11 are equal.
[0044] The first deflection compensation values of the two axially symmetrical points between the two single molds 11 are equal, and the second deflection compensation values of the two axially symmetrical points between the two single molds 11 are equal, so that the final deflection compensation values of the two axially symmetrical points between the two single molds 11 are equal. When calculating the final deflection compensation values of the points on the double-groove mold 1, the final deflection compensation values of each point on one single mold 11 can be calculated first, and then the corresponding point of the other single mold 11 can be found by the method of axial symmetry, and finally the final deflection compensation value of the corresponding point of the other single mold 11 can be obtained, which can save work intensity.
[0045] In one embodiment of the present invention, when the two single molds 11 are axially symmetrical to each other, the deflection compensation values at the symmetrical points between the two single molds 11 are equal, and step S7 includes: Step S71: Calculate the final deflection compensation value of a point to be measured on a single mold 11: Step S72: The symmetrical point of the point to be measured on another single mold 11 is obtained by axisymmetry, and the deflection compensation value of the symmetrical point is equal to the deflection compensation value of the point to be measured.
[0046] It is only necessary to draw the first contour curve 2 on one single mold 11, and there is no need to draw the first contour curve 2 on two single molds 11 at the same time; it is only necessary to calculate the final deflection compensation values of several points to be measured on one single mold 11, and the final deflection compensation values of the symmetrical points on another single mold 11 can be obtained, which reduces the workload and improves work efficiency.
[0047] The draw ribs are located on the outside of the die edge of the single die 11; the single die 11 of the double-groove die 1 is mostly irregular in shape. When drawing the first contour curve of the single die 11, it is necessary to follow the product characteristics, approach the direction of the product, and finally generate the contour curve.
[0048] In one embodiment of the present invention, taking a fender mold as an example, the fender mold is a single mold 11 of a double-groove mold 1, and step S1 includes the following steps for drawing a first contour curve 2 on the single mold 11, and the value unit is millimeter: Step S11: Please refer to Figure 4, make a point from the edge of the die and the center of the drawbead of the single die 11; Step S12: Please refer to Figure 5 , determine points A, B, C, D and E, and use points A, B, C, D and E as the center of the circle respectively; Step S13: Please refer to Figure 6 and Figure 7 , make circles of radius R(a) with points A, B, C and D as the centers, and then make a circle of radius r(a) with point E as the center; Step S14: Please refer to Figure 8 , use tangents to connect circle A and circle B, circle B and circle D, circle D and circle E, circle E and circle C, circle C and circle A; when the tangent connecting circle A and circle E does not intersect circle C, make a definition line without considering circle C, and connect circle E and circle A through the tangent; connect adjacent tangents, draw a complete definition line, and use the definition line as the first contour curve 2; Step S15: Please refer to Fig. 9 , draw four definition lines and use the four definition lines as the four first contour curves 2 respectively.
[0049] By reserving data in the early stage, the deflection compensation of the double-slot mold 1 can be performed during the data processing stage of the double-slot mold 1, which can reduce the workload during mold grinding, reduce the difficulty of on-site debugging and shorten the debugging period.
[0050] The above description is only an exemplary embodiment of the present invention, and does not limit the patent scope of the present invention. All equivalent structural changes made by using the contents of the present invention specification and drawings under the technical concept of the present invention, or directly / indirectly applied in other related technical fields are included in the patent protection scope of the present invention.
Claims
1. A double-groove die deflection compensation method, It is characterized in that The following steps are involved: S1: determining a deflection compensation value of a center point of a single mold, drawing a plurality of first contour curves with the center point of the single mold as the center, and determining a deflection compensation value of any of the first contour curves; S2: determining a deflection compensation value of a center point of the double-groove mold, drawing a plurality of second contour curves with the center point of the double-groove mold, and determining a deflection compensation value of any of the second contour curves; S3: Select any point on the single mold as the point to be tested; S4: calculating a first deflection compensation value of the point to be measured according to the positional relationship between the point to be measured and the first contour curve; S5: Calculating a second deflection compensation value of the point to be measured according to the positional relationship between the point to be measured and the second contour curve; S6: summing the first deflection compensation value of the point to be measured and the second deflection compensation value of the point to be measured to obtain a final deflection compensation value of the point to be measured; S7: Select other points to be measured and repeat steps S4-S6; S8: In the processing data stage of the double-groove mold, the double-groove mold is deflected and compensated according to the final deflection compensation value of the point to be measured.
2. A double groove die deflection compensation method as claimed in claim 1, It is characterized in that In step S1, the step of determining the deflection compensation finger of the center point of the single mold includes: S11: Use the finite element analysis (FEA) numerical simulation method to perform stress analysis on the single mold, observe the deformation of the single mold under the simulated load, and record the deflection deformation at each position of the single mold; S12: The sum of the deflection deformation of the center point of a single mold and the manufacturing error is used as the deflection compensation value of the center point of the single mold.
3. A double groove die deflection compensation method as claimed in claim 1, It is characterized in that In step S2, the plurality of second contour curves are a plurality of concentric circles, and the centers of the second contour curves coincide with the center point of the double-groove mold.
4. A double groove die deflection compensation method as claimed in claim 3, It is characterized in that Taking the double-groove mold close to its die surface as the negative direction, the deflection compensation value of the center point of the double-groove mold is -0.40mm; the maximum distance between the center of the double-groove mold and the die edge of the double-groove mold is set to L, and the second contour curves are set to three, the radius of the first second contour curve is R1=L*0.2, and the deflection compensation value of the first second contour curve is -0.24mm; the radius of the second second contour curve is R2=L*0.8, and the deflection compensation value of the second second contour curve is 0mm; the radius of the third second contour curve is R3=L*1.4, and the deflection compensation value of the second second contour curve is 0.12mm.
5. A double groove die deflection compensation method as claimed in claim 1, It is characterized in that Step S4 includes: S41: Taking the center point of the single mold as the starting point, draw a first ray passing through the point to be measured; S42: dividing the first ray into a plurality of first line segments by means of a single mold center point and a plurality of the first contour curves; S43: measuring the length of the first line segment where the point to be measured is located, and then calculating the slope of the first line segment where the point to be measured is located; S44: measuring the distance between the point to be measured and the endpoint of the first line segment where the point to be measured is located, and calculating the first deflection compensation value of the point to be measured according to the slope of the first line segment where the point to be measured is located.
6. A double groove die deflection compensation method as claimed in claim 1, It is characterized in that Step S5 includes: S51: Taking the center point of the double-groove mold as the starting point, draw a second ray passing through the point to be measured; S52: dividing the second ray into a plurality of second line segments through the center point of the double-groove mold and the plurality of second contour curves; S53: measuring the length of the second line segment where the point to be measured is located, and calculating the slope of the second line segment where the point to be measured is located; S54: measuring the distance between the point to be measured and the endpoint of the second line segment where the point to be measured is located, and calculating the second deflection compensation value of the point to be measured according to the slope of the second line segment where the point to be measured is located.
7. A double groove die deflection compensation method as claimed in claim 1, It is characterized in that In step S1, three first contour curves are set.
8. A double groove die deflection compensation method as claimed in claim 7, It is characterized in that Taking the double-groove mold close to its concave mold surface as the negative direction, when a single mold is used to process the automobile outer panel, the deflection compensation value of the center point of the single mold is -0.26mm, and the deflection compensation values of the three first contour curves are -0.14mm, 0mm and 0.12mm respectively.
9. A double groove die deflection compensation method as claimed in claim 7, It is characterized in that Taking the double-groove mold close to its concave mold surface as the negative direction, when a single mold is used to process the automobile inner panel, the deflection compensation value of the center point of the single mold is -0.32mm, and the deflection compensation values of the three first contour curves are -0.16mm, 0mm and 0.12mm respectively.
10. A double groove die deflection compensation method as claimed in claim 3, It is characterized in that When two single molds are axially symmetrical to each other, the deflection compensation values at the symmetrical points of the two single molds are equal; Step S7 includes: S71: Calculate the final deflection compensation value of the point to be measured on a single mold: S72: A symmetrical point of the point to be measured on another single mold is obtained by an axisymmetric method, and the deflection compensation value of the symmetrical point is equal to the deflection compensation value of the point to be measured.
Citation Information
Patent Citations
Method for producing a large steel tube
CN102056687A
Method for designing loading track for multi-pass roll bending of wall plate and generating numerical control code
CN102445921A
Molded surface compensation method of large stamping die aiming at deflection deformation of press machine
CN102601194A
Adaptive control of machining process
CN102905847A
Double-piece double-inclined-plane matching type bidirectional deflection compensation device of bending machine
CN103521574A