Damascene wiring structure, actuating device, and method for manufacturing damascene wiring structure

By setting an inclined surface and a cover layer in the inlaid wiring structure, stress is dispersed, peeling and damage problems caused by stress concentration of the wiring part and metal layer are solved, and the reliability and strength of the inlaid wiring structure are improved.

CN118908143APending Publication Date: 2024-11-08HAMAMATSU PHOTONICS KK
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410971014.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2018-10-31
Filing Date
2019-10-30
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

In the inlaid wiring structure, the concentration of stresses of the wiring part and the metal layer leads to the risk of peeling and damage. Especially when the Lorenz force is applied in the actuation device, the contact part of the stress with the wiring part and the metal layer is prone to stress. concentrated.

Method used

By providing an inclined surface and a cover layer in the inlay wiring configuration, the end of the metal layer enters between the cover layer and the inclined surface, and using the same material in the contact portion of the cover layer and the metal layer, increasing the thickness and contact of the cover layer. The area disperses the stress and reduces the concentration of stress.

Benefits of technology

It effectively improves the reliability of the inlay wiring structure, reduces the risk of damage caused by stress concentration, and enhances the bonding strength between the cover layer and the insulating layer, improving the overall reliability and strength.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118908143A_ABST
    Figure CN118908143A_ABST
Patent Text Reader

Abstract

A damascene wiring structure is provided with: a base having a main surface in which a groove is provided; an insulating layer having: a first portion provided on the inner surface of the groove portion; and a second portion integrally formed with the first portion and provided on the main surface; a metal layer disposed on the first portion of the insulating layer; a wiring part embedded in the groove part and bonded to the metal layer; and a covering layer provided so as to cover the second portion of the insulating layer, the end portion of the metal layer, and the wiring portion. A surface of a boundary portion between the first portion and the second portion of the insulating layer on the opposite side from the substrate includes an inclined surface inclined with respect to a direction perpendicular to the main surface when viewed from an extending direction of the wiring portion. An end portion of the metal layer enters between the cover layer and the inclined surface, and at the end portion, a first surface along the cover layer forms an acute angle with a second surface along the inclined surface.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] This application is filed on October 30, 2019 、Application No. 201980071401.7 、The name of the invention is mosaic Wiring structure, actuator, and method for manufacturing embedded wiring structure A divisional application for a patent application. Technical Field

[0002] One aspect of the present invention relates to a damascene wiring structure, an actuator, and a method of manufacturing the damascene wiring structure. Background Art

[0003] Conventionally, there is known a damascene wiring structure in which a wiring portion is formed by embedding a metal material in a groove portion (see, for example, Patent Document 1). In such a damascene wiring structure, a metal layer is provided on the inner surface of the groove portion, and the wiring portion is bonded to the metal layer.

[0004] Prior art literature

[0005] Patent Literature

[0006] Patent Document 1: Japanese Patent Application Laid-Open No. 6-84896 Summary of the invention

[0007] Technical problem to be solved by the invention

[0008] In the above-mentioned embedded wiring structure, there is a case where stress is applied to the wiring portion and the metal layer. For example, when the embedded wiring structure is applied to the coil of an actuator that utilizes the Lorentz force acting on the coil through interaction with the magnetic field, stress is applied to the wiring portion and the metal layer in a direction perpendicular to the extension direction of the wiring portion. On the other hand, in the above-mentioned embedded wiring structure, there is a case where a covering layer is provided in a manner covering the surface of the wiring portion and the end of the metal layer. In the case where stress is applied to the wiring portion and the metal layer in such an embedded wiring structure, the stress is concentrated in the portion of the covering layer that is in contact with the wiring portion and the metal layer, and there is a risk of peeling and damage in this portion.

[0009] Therefore, an object of one aspect of the present invention is to provide a highly reliable Damascene wiring structure and an actuator device, and a method for manufacturing a Damascene wiring structure capable of obtaining such a Damascene wiring structure.

[0010] Technical methods for solving problems

[0011] An inlaid wiring structure involved in one aspect of the present invention comprises: a substrate having a main surface provided with a groove portion; an insulating layer having: a first portion provided on the inner surface of the groove portion; and a second portion formed integrally with the first portion and provided on the main surface; a metal layer provided on the first portion of the insulating layer; a wiring portion embedded in the groove portion and bonded to the metal layer; and a covering layer provided in a manner covering the second portion of the insulating layer, an end portion of the metal layer, and the wiring portion, wherein a surface of a boundary portion between the first portion and the second portion in the insulating layer on the opposite side to the substrate includes an inclined surface inclined relative to a direction perpendicular to the main surface when viewed from the extension direction of the wiring portion, the end portion of the metal layer enters between the covering layer and the inclined surface, and at the end portion, the first surface along the covering layer forms an acute angle with the second surface along the inclined surface.

[0012] In the embedded wiring structure, the insulating layer has: a first part provided on the inner surface of the groove; and a second part formed integrally with the first part and provided on the main surface, and the covering layer is provided in a manner covering the second part of the insulating layer, the end of the metal layer, and the wiring part. Thus, compared with, for example, a case where the insulating layer has only the first part, the parts where stress is easily concentrated can be reduced. Furthermore, the surface of the boundary part of the first part and the second part in the insulating layer on the opposite side to the base includes an inclined surface, and the end of the metal layer enters between the covering layer and the inclined surface. Furthermore, in the end, the first surface along the covering layer and the second surface along the inclined surface form an acute angle. Thus, it is possible to suppress the stress from acting on the covering layer in a concentrated manner. Based on the above, reliability can be improved in the embedded wiring structure.

[0013] The thickness of the cover layer may be thicker than the thickness of the insulating layer. In this case, the strength of the cover layer can be increased, and the reliability can be further improved.

[0014] Alternatively, the portion of the end of the metal layer in the covering layer that contacts the first surface and the portion of the end of the metal layer in the insulating layer that contacts the second surface may be made of the same material. In this case, the bonding strength between the covering layer and the insulating layer can be increased near the contact portion between the ends of the covering layer and the metal layer, and reliability can be further improved.

[0015] The insulating layer may include a first layer made of an oxide film and a second layer made of a nitride film provided on the first layer. In this case, the first layer made of the oxide film can be easily formed into an inclined shape, so that the formation of the inclined surface can be facilitated.

[0016] A boundary surface that is inclined relative to a direction perpendicular to the main surface when viewed from the extending direction may be provided at the boundary portion between the main surface and the groove portion in the base. In this case, the formation of the inclined surface can be further facilitated.

[0017] The inclined surface may be curved convexly. In this case, it is possible to more reliably suppress the stress from being concentrated on the cover layer.

[0018] Alternatively, the third surface on the opposite side of the second surface in the end of the metal layer is inclined relative to the direction perpendicular to the main surface when viewed from the extension direction, and a portion of the wiring portion enters between the cover layer and the third surface. In this case, the end of the metal layer can be suppressed by the wiring portion, and the stress acting on the cover layer from the metal layer can be reduced. In addition, the thickness of the portion of the wiring portion in the direction perpendicular to the main surface is reduced, so the stress acting on the cover layer from the wiring portion can be reduced.

[0019] Alternatively, the thickness of the end of the metal layer in a direction parallel to the main surface may be thicker than the thickness of the portion other than the end of the metal layer. In this case, the contact area between the end of the metal layer and the covering layer can be increased, and the stress acting on the covering layer from the metal layer can be more appropriately dispersed.

[0020] Alternatively, the thickness of the end of the metal layer in a direction parallel to the main surface gradually increases as it approaches the front end of the end. In this case, the contact area between the end of the metal layer and the covering layer can be further increased, and the stress acting on the covering layer from the metal layer can be further appropriately dispersed.

[0021] Alternatively, the first contact surface in the wiring portion that contacts the covering layer may be located on the bottom side of the groove portion relative to the second contact surface in the insulating layer that contacts the covering layer. In this case, the portion where stress is easily concentrated can be further reduced. Furthermore, the contact area between the end of the metal layer and the covering layer can be further increased, and the stress acting on the covering layer from the metal layer can be further appropriately dispersed.

[0022] The thickness of the cover layer may be greater than the distance between the first contact surface and the second contact surface in the direction perpendicular to the main surface. In this case, the strength of the cover layer can be further improved.

[0023] The thickness of the cover layer may be smaller than the distance between the first contact surface and the second contact surface in the direction perpendicular to the main surface. In this case, the stress acting on the cover layer from the wiring portion can be further reduced.

[0024] The groove may extend spirally when viewed from a direction perpendicular to the main surface. In this case, high reliability can be obtained.

[0025] The interval between adjacent portions of the groove may be smaller than the width of the groove. In this case, the pitch (interval) of the wiring can be narrowed, and space saving can be achieved.

[0026] The width of the groove may be smaller than the depth of the groove. In this case, space saving and low resistance of wiring can be achieved.

[0027] Alternatively, the base may have an opposite surface opposite to the main surface, and the distance between the bottom of the groove in a direction perpendicular to the main surface and the opposite surface is greater than the depth of the groove. In this case, the strength of the base can be increased, and the reliability can be further improved.

[0028] An actuator device according to one aspect of the present invention has the above-mentioned embedded wiring structure, and includes: a support portion; a movable portion supported in the support portion in a swingable manner; a coil having the embedded wiring structure and provided on at least one of the support portion and the movable portion; and a magnetic field generating portion that generates a magnetic field acting on the coil. In the actuator device, stress in a direction perpendicular to the extending direction of the wiring portion acts on the wiring portion and the metal layer, and reliability can be improved for the above-mentioned reasons.

[0029] A method for manufacturing a damascene wiring structure according to one aspect of the present invention comprises: a first step of forming an insulating layer on a substrate having a main surface provided with a groove, the insulating layer comprising: a first portion provided on an inner surface of the groove; and a second portion formed integrally with the first portion and provided on the main surface; a second step of forming a metal layer on the first portion and the second portion of the insulating layer after the first step; a third step of forming a wiring portion on the metal layer after the second step in a manner buried in the groove and bonded to the metal layer; a fourth step of removing the metal layer and the wiring portion on the second portion by chemical mechanical polishing to flatten the wiring portion after the third step in a manner in which the second portion of the insulating layer is exposed; and a fifth step of forming a covering layer after the fourth step in a manner in which the second portion of the insulating layer, an end portion of the metal layer, and the wiring portion are covered, wherein in the first step, the insulating layer is formed, wherein a surface of a boundary portion between the first portion and the second portion in the insulating layer on the opposite side to the substrate includes an inclined surface inclined relative to a direction perpendicular to the main surface when viewed from the extending direction of the wiring portion. According to this method of manufacturing a Damascene wiring structure, the above-mentioned Damascene wiring structure with high reliability can be obtained.

[0030] Alternatively, the metal layer may be formed by sputtering in the second step. In this case, the thickness of the end of the metal layer in a direction parallel to the main surface can be gradually increased toward the tip of the end, thereby increasing the contact area between the end of the metal layer and the cover layer.

[0031] Effects of the Invention

[0032] According to one aspect of the present invention, it is possible to provide a highly reliable Damascene wiring structure and an actuator device, and a method for manufacturing a Damascene wiring structure capable of obtaining such a Damascene wiring structure. BRIEF DESCRIPTION OF THE DRAWINGS

[0033] Figure 1 It is a top view of the actuator device involved in embodiment.

[0034] Figure 2 yes Figure 1 II-II line cross-sectional view.

[0035] Figure 3 yes Figure 2 Magnified image of .

[0036] Figure 4 yes Figure 3 Magnified image of .

[0037] Figure 5 (a) and Figure 5 (b) is a cross-sectional view for explaining a method for manufacturing a damascene wiring structure.

[0038] Figure 6 (a) and Figure 6 (b) is a cross-sectional view for explaining a method for manufacturing a damascene wiring structure.

[0039] Figure 7 (a) and Figure 7 (b) is a cross-sectional view for explaining a method for manufacturing a damascene wiring structure.

[0040] Figure 8 It is a cross-sectional view of a damascene wiring structure according to a first modification.

[0041] Fig. 9 It is a cross-sectional view of a damascene wiring structure according to a second modification.

[0042] Fig.10 (a) is a cross-sectional view of a damascene wiring structure according to a third modification example. Fig.10 (b) is a cross-sectional view of a damascene wiring structure according to a fourth modification. DETAILED DESCRIPTION

[0043] Hereinafter, one embodiment of the present invention will be described in detail with reference to the accompanying drawings. In the following description, the same reference numerals are used for the same or corresponding elements, and repeated descriptions are omitted.

[0044] [Structure of mirror device]

[0045] like Figure 1As shown, the mirror device (actuator) 1 includes: a support portion 2; a first movable portion 3; a second movable portion (support portion) 4; a pair of first connecting portions 5, 6; a pair of second connecting portions 7, 8; and a magnetic field generating portion 9. The support portion 2, the first movable portion 3, the second movable portion 4, the first connecting portions 5, 6, and the second connecting portions 7, 8 are integrally formed by, for example, a semiconductor substrate such as an SOI (Silicon on Insulator) substrate. That is, the mirror device 1 is configured as a MEMS (Micro Electro Mechanical Systems) device.

[0046] In the mirror device 1, a first movable portion 3 having a mirror surface (optical surface) 10 is swung around a first axis X1 and a second axis X2 that are orthogonal to each other. The mirror device 1 can be used, for example, in an optical switch for optical communication, an optical scanner, etc. The magnetic field generating unit 9 is composed of, for example, a permanent magnet having a Halbach array. The magnetic field generating unit 9 generates a magnetic field that acts on coils 21 and 22 described later.

[0047] The support portion 2 has a quadrilateral shape when viewed from above, for example, and is formed in a frame shape. The support portion 2 is arranged on one side in a direction perpendicular to the mirror surface 10 relative to the magnetic field generating portion 9. The first movable portion 3 is arranged on the inner side of the support portion 2 in a state separated from the magnetic field generating portion 9. In addition, "viewed from above" refers to the situation of observing from a direction perpendicular to the mirror surface 10, in other words, the situation of observing from a direction perpendicular to the main surface 31 of the substrate 30 described later.

[0048] The first movable part 3 includes a configuration part 3a, a frame part 3b surrounding the configuration part 3a, and a plurality of (here, for example, 4) connecting parts 3c connecting the configuration part 3a and the frame part 3b. The configuration part 3a is formed, for example, to be circular when viewed from above. On the surface of the configuration part 3a on the opposite side to the magnetic field generating part 9, for example, a circular mirror surface 10 is provided. The mirror surface 10 is formed by a reflective film composed of, for example, aluminum, aluminum alloy, silver, silver alloy, gold, a dielectric multilayer film, etc.

[0049] The frame portion 3b has a quadrilateral shape when viewed from above, and is formed into a frame shape. A plurality of connecting portions 3c are arranged on both sides of the configuration portion 3a on the first axis X1 and on both sides of the configuration portion 3a on the second axis X2, and connect the configuration portion 3a and the frame portion 3b to each other on the first axis X1 or on the second axis X2.

[0050] The second movable portion 4 has a rectangular outer shape in a plan view and is formed in a frame shape. The second movable portion 4 is arranged inside the support portion 2 so as to surround the first movable portion 3 in a state separated from the magnetic field generating portion 9 .

[0051] The first connecting parts 5 and 6 are arranged on both sides of the first movable part 3 on the first axis X1. Each of the first connecting parts 5 and 6 connects the first movable part 3 and the second movable part 4 to each other on the first axis X1 so that the first movable part 3 can swing around the first axis X1. Each of the first connecting parts 5 and 6 extends linearly along the first axis X1, for example.

[0052] The second connecting parts 7 and 8 are arranged on both sides of the second movable part 4 on the first axis X1. Each of the second connecting parts 7 and 8 connects the second movable part 4 and the support part 2 to each other on the second axis X2 so that the second movable part 4 can swing around the second axis X2. Each of the second connecting parts 7 and 8 extends linearly along the second axis X2, for example.

[0053] The mirror device 1 further includes: coils 21, 22; a plurality of wirings 12, 13, 14, 15; and a plurality of electrode pads 25, 26, 27, 28. The coil 21 is embedded in the frame portion 3b of the first movable portion 3, for example, and extends in a spiral shape when viewed from above. The coil 22 is embedded in the second movable portion 4, for example, and extends in a spiral shape when viewed from above. Each of the coils 21, 22 is made of a metal material such as copper, for example.

[0054] A plurality of electrode pads 25, 26, 27, and 28 are provided on the support portion 2. The wiring 12 electrically connects one end of the coil 21 to the electrode pad 25. The wiring 12 extends from one end of the coil 21 to the electrode pad 25 via the first connecting portion 5, the second movable portion 4, and the second connecting portion 7. The wiring 13 electrically connects the other end of the coil 21 to the electrode pad 26. The wiring 13 extends from the other end of the coil 21 to the electrode pad 26 via the first connecting portion 6, the second movable portion 4, and the second connecting portion 8.

[0055] Wiring 14 electrically connects one end of coil 22 to electrode pad 27. Wiring 14 extends from one end of coil 22 to electrode pad 27 via second connection portion 8. Wiring 15 electrically connects the other end of coil 22 to electrode pad 28. Wiring 15 extends from the other end of coil 22 to electrode pad 28 via second connection portion 7.

[0056] In the mirror device 1 configured as described above, when a driving signal for linear motion is input to the coil 22 via the electrode pads 27, 28 and the wirings 14, 15, a Lorentz force acts on the coil 22 by interaction with the magnetic field generated by the magnetic field generating unit 9. By utilizing the balance between the Lorentz force and the elastic force of the second connecting portions 7, 8, the mirror surface 10 (first movable portion 3) and the second movable portion 4 are linearly moved around the second axis X2.

[0057] On the other hand, when a drive signal for resonant operation is input to the coil 21 via the electrode pads 25, 26 and the wirings 12, 13, a Lorentz force acts on the coil 21 by interaction with the magnetic field generated by the magnetic field generating unit 9. In addition to the Lorentz force, the mirror 10 (first movable unit 3) is resonantly operated around the first axis X1 by utilizing the resonance of the first movable unit 3 at the resonant frequency.

[0058] [Inlay wiring structure]

[0059] Reference Figure 2 , Figure 3 and Figure 4 , the inlaid wiring structure 100 of the coils 21 and 22 will be described. Since the coils 21 and 22 have the same structure, the coil 22 will be described below, and the description of the coil 21 will be omitted.

[0060] As described above, the coil 22 is provided on the second movable portion 4. The second movable portion 4 is composed of, for example, the first silicon layer 81 of the substrate (base) 30. The substrate 30 includes, for example, the first silicon layer 81 and the second silicon layer 82, and an insulating layer 83 ( Figure 5 to Figure 7 ). The support portion 2 is composed of a first silicon layer 81, a second silicon layer 82 and an insulating layer 83, and the first movable portion 3, the second movable portion 4, the first connecting portions 5, 6 and the second connecting portions 7, 8 are composed of the first silicon layer 81. The substrate 30 has a main surface 31. In this example, the main surface 31 is a surface of the first silicon layer 81 on the opposite side to the insulating layer 83.

[0061] The main surface 31 is provided with a groove 33. The groove 33 has a shape corresponding to the coil 21, and in this example, extends in a spiral shape when viewed from above. In a cross section perpendicular to the extending direction of the groove 33, the groove 33 is, for example, rectangular in shape. In this example, the inner surface 34 of the groove 33 has a side surface 34a and a bottom surface (bottom) 34b. Figure 2 to Figure 4 Only one cross section is shown in the figure, and for example, the inlaid wiring structure 100 is configured in the same manner with respect to the extension direction of the groove portion 33, and is configured in the same manner in any cross section perpendicular to the extension direction of the groove portion 33. However, the inlaid wiring structure 100 does not necessarily have to be configured in the same manner with respect to the extension direction of the groove portion 33. For example, the inlaid wiring structure 100 may have the shape of the present embodiment in a portion in the extension direction of the groove portion 33, and may have the shape of a modified example described later in another portion in the extension direction of the groove portion 33.

[0062] The inlaid wiring structure 100 includes an insulating layer 40, a metal layer 50, a wiring portion 60, and a cover layer 70 in addition to the substrate 30 as a base. The insulating layer 40 is provided over the main surface 31 and the inner surface 34 of the groove portion 33. More specifically, the insulating layer 40 includes: a first portion 41 provided on the inner surface 34; and a second portion 42 formed integrally with the first portion 41 and provided on the main surface 31. The boundary portion 43 between the first portion 41 and the second portion 42 in the insulating layer 40 is located at the boundary portion between the main surface 31 of the substrate 30 and the groove portion 33.

[0063] The insulating layer 40 is composed of a first layer 44 and a second layer 45. The first layer 44 is composed of an oxide film and is provided on the main surface 31 and the inner surface 34 of the groove portion 33. The oxide film constituting the first layer 44 is, for example, a silicon oxide film (SiO2) formed by thermally oxidizing silicon. The second layer 45 is composed of a nitride film and is provided on the first layer 44. The nitride film constituting the second layer 45 is, for example, a silicon nitride film (SiN) or the like. The first portion 41 and the boundary portion 43 are composed of the first layer 44 and the second layer 45, and the second portion 42 is composed of the first layer 44.

[0064] The metal layer 50 is provided over the first portion 41 of the insulating layer 40. That is, the metal layer 50 is provided on the inner surface 34 of the groove portion 33 via the first portion 41. The metal layer 50 is composed of a metal material such as titanium (Ti), for example. The metal layer 50 can function as a seed layer for stably forming the wiring portion 60 on the semiconductor substrate, and a barrier layer for preventing the metal element contained in the wiring portion 60 from diffusing into the first silicon layer 81.

[0065] The wiring portion 60 is embedded in the groove portion 33 and is bonded to the metal layer 50. That is, the wiring portion 60 is provided in the groove portion 33 via the first portion 41 of the insulating layer 40 and the metal layer 50. The wiring portion 60 is made of a metal material such as copper (Cu), for example. The shape of the metal layer 50 in the cross section perpendicular to the extension direction of the wiring portion 60 (in other words, the extension direction of the groove portion 33) corresponds to the cross-sectional shape of the groove portion 33, and in this example, is substantially rectangular. In addition, as shown in the present embodiment, the wiring portion 60 extends spirally when viewed from above, and the wiring portion 60 has a first portion extending in a direction parallel to the first axis X1 and a second portion extending in a direction parallel to the second axis X2. In the first portion, the extension direction is a direction parallel to the first axis X1, and in the second portion, it is a direction parallel to the second axis X2. Alternatively, in the case where the wiring portion 60 extends in a curved or bent manner, the extension direction of a certain portion of the wiring portion 60 refers to the tangent direction of the portion.

[0066] The cover layer 70 is provided so as to cover the second portion 42 of the insulating layer 40, the end portion 51 of the metal layer 50, and the wiring portion 60. In this example, the cover layer 70 extends in a planar shape parallel to the main surface 31. The thickness T1 of the cover layer 70 is thicker than the thickness T2 of the insulating layer 40. The cover layer 70 is composed of, for example, a silicon nitride film and has insulating properties. That is, the cover layer 70 is composed of the same material as the second layer 45 of the insulating layer 40.

[0067] like Figure 4 As shown, the surface 41a of the first portion 41 of the insulating layer 40 on the side opposite to the substrate 30 is, for example, a flat surface perpendicular to the main surface 31. The surface 42a of the second portion 42 of the insulating layer 40 on the side opposite to the substrate 30 is, for example, a flat surface parallel to the main surface 31. The surface 42a is in contact with the cover layer 70. The surface 43a of the boundary portion 43 on the side opposite to the substrate 30 includes an inclined surface 43b inclined relative to the direction A1 perpendicular to the main surface 31 when viewed from the extending direction of the wiring portion 60. More specifically, the inclined surface 43b is inclined outwardly relative to the surface 41a of the first portion 41 (in a manner that the farther away from the bottom surface 34b of the groove portion 33, the farther away from the center of the groove portion 33). In this example, the inclined surface 43b is curved convexly toward the side opposite to the substrate 30.

[0068] The end portion 51 of the metal layer 50 enters between the cover layer 70 and the inclined surface 43 b . More specifically, the end portion 51 has a portion arranged in a space formed between the cover layer 70 and the inclined surface 43 b in the direction A1 perpendicular to the main surface 31 .

[0069] The end portion 51 has a first surface 51a, a second surface 51b continuous with the first surface 51a, and a third surface 51c continuous with the first surface 51a on the opposite side to the second surface 51b. The first surface 51a is along the cover layer 70 and is bonded to the cover layer 70. In this example, the first surface 51a is a flat surface, and is located on the same plane as the surface 42a of the second portion 42 of the insulating layer 40 and the surface 60a of the wiring portion 60 described later.

[0070] The second surface 51b is along the inclined surface 43b and is bonded to the inclined surface 43b. The second surface 51b is inclined outward relative to the direction A1 perpendicular to the main surface 31, similarly to the inclined surface 43b. The second surface 51b is concavely curved toward the opposite side of the substrate 30. The second surface 51b is in contact with the second layer 45 constituting the boundary portion 43 of the insulating layer 40. That is, the portion of the insulating layer 40 that is in contact with the second surface 51b (in this example, the second layer 45 constituting the boundary portion 43) is made of the same material (silicon nitride film) as the portion of the covering layer 70 that is in contact with the first surface 51a. As described above, in this example, the entire covering layer 70 is made of a silicon nitride film. As a result, the bonding strength between the insulating layer 40 and the covering layer 70 can be improved.

[0071] The third surface 51c is a surface of the end portion 51 on the opposite side to the second surface 51b. The third surface 51c is inclined outward relative to the direction A1 when viewed from the extension direction of the wiring portion 60. The degree of inclination of the third surface 51c relative to the direction A1 is gentler than the degree of inclination of the second surface 51b relative to the direction A1. Thus, the thickness of the end portion 51 in the direction A2 parallel to the main surface 31 gradually increases as it approaches the front end of the end portion 51. A portion 61 of the wiring portion 60 located at the boundary portion with the metal layer 50 and the covering layer 70 enters between the covering layer 70 and the third surface 51c. More specifically, a portion 61 of the wiring portion 60 is arranged in the space formed between the covering layer 70 and the third surface 51c in the direction A1.

[0072] In the end portion 51, the first surface 51a and the second surface 51b form an acute angle. In other words, the angle θ formed by the first surface 51a and the second surface 51b is less than 90 degrees. That is, the thickness of the end portion 51 in the direction A1 perpendicular to the main surface 31 gradually decreases as it approaches the front end of the end portion 51 (for example, the vertex formed by the first surface 51a and the second surface 51b). The angle θ can be, for example, 15 degrees to 88 degrees. The end portion 51 of the metal layer 50 is not disposed on the second portion 42 of the insulating layer 40.

[0073] The thickness (minimum thickness) of the end portion 51 in the direction A2 parallel to the main surface 31 is greater than the thickness of the portion other than the end portion 51 in the metal layer 50 (for example, the portion located in the middle in the direction A1 perpendicular to the main surface 31 in the metal layer 50, or the portion located on the first portion 41 of the insulating layer 40 in the metal layer 50). The thickness (maximum thickness) of the front end portion of the metal layer 50 in the direction A1 is smaller than the thickness T2 of the insulating layer 40. Here, the “front end portion of the metal layer 50” refers to the portion of the metal layer 50 whose thickness in the direction A2 parallel to the main surface 31 is greater than the thickness in the direction A1 perpendicular to the main surface 31.

[0074] In this example, the surface (first contact surface) 60a of the wiring portion 60 in contact with the cover layer 70 is located on the same plane as the surface 42a of the second portion 42 of the insulating layer 40. The surface 42a is the surface (second contact surface) of the insulating layer 40 in contact with the cover layer 70. The surface 70a of the cover layer 70 on the substrate 30 side is a flat surface.

[0075] As described above, the groove portion 33 extends spirally in a plan view. Figure 2 As shown, the groove portion 33 has a plurality of portions 33a adjacent to each other. The interval B between the portions 33a is smaller than the width W of the groove portion 33. The width W of the groove portion 33 is smaller than the depth D of the groove portion 33. The depth D of the groove portion 33 refers to, for example, the distance between the main surface 31 and the bottom surface 34b in the direction A1 perpendicular to the main surface 31. The distance L between the bottom surface 34b of the groove portion 33 and the opposite surface of the substrate 30 on the opposite side to the main surface 31 in the direction A1 perpendicular to the main surface 31 is greater than the depth D of the groove portion 33. In this example, the opposite surface is the surface 81a of the first silicon layer 81 on the insulating layer 83 side (opposite side to the main surface 31).

[0076] [Effect]

[0077] In the Damascene wiring structure 100, the insulating layer 40 includes: a first portion 41 provided on the inner surface 34 of the groove portion 33; and a second portion 42 formed integrally with the first portion 41 and provided on the main surface 31, and the cover layer 70 is provided so as to cover the second portion 42 of the insulating layer 40, the end portion 51 of the metal layer 50, and the wiring portion 60. Thus, compared with, for example, a case where the insulating layer 40 has only the first portion 41, the portion where stress is likely to be concentrated can be reduced. That is, in a case where the insulating layer 40 has only the first portion 41, the end portion of the insulating layer 40 is located near the boundary portion between the main surface 31 and the groove portion 33, and the main surface 31 is in contact with the cover layer 70. In this case, the substrate 30, the end portion of the insulating layer 40, the end portion 51 of the metal layer 50, the wiring portion 60, and the cover layer 70 are in contact at a portion close to each other. Stress is likely to be concentrated at such a portion. In contrast, in the damascene wiring structure 100, since there is no end of the insulating layer 40 near the boundary between the main surface 31 and the groove 33, the stress concentration site can be reduced. In addition, the end 51 of the metal layer 50 extends in contact with the cover layer 70. If the end 51 does not reach the cover layer 70 and stays at a position lower than the surface 60a of the wiring portion 60, a void may be generated in the portion of the wiring portion 60 exposed from the metal layer 50. In contrast, in the damascene wiring structure 100, the generation of such a void can be suppressed, and the peeling of the cover layer 70 caused by the void can be suppressed. In addition, the surface 43a of the boundary portion 43 between the first portion 41 and the second portion 42 of the insulating layer 40 on the opposite side to the substrate 30 includes an inclined surface 43b, and the end 51 of the metal layer 50 enters between the cover layer 70 and the inclined surface 43b. Furthermore, in the end portion 51, the first surface 51a along the cover layer 70 and the second surface 51b along the inclined surface 43b form an acute angle. This can suppress the stress from being concentrated on the cover layer 70. As described above, the reliability of the Damascene wiring structure 100 can be improved.

[0078] In the Damascene wiring structure 100, the thickness T1 of the cover layer 70 is greater than the thickness T2 of the insulating layer 40. This can increase the strength of the cover layer 70 and further improve reliability.

[0079] In the Damascene wiring structure 100, the portion of the cover layer 70 in contact with the first surface 51a of the end portion 51 and the portion of the insulating layer 40 in contact with the second surface 51b of the end portion 51 (the second layer 45 constituting the boundary portion 43) are made of the same material. Thus, the bonding strength between the cover layer 70 and the insulating layer 40 in the vicinity of the contact portion between the cover layer 70 and the end portion 51 of the metal layer 50 can be improved, and reliability can be further improved.

[0080] In the Damascene wiring structure 100, the insulating layer 40 includes a first layer 44 made of an oxide film and a second layer 45 made of a nitride film and provided on the first layer 44. Thus, the first layer 44 made of an oxide film can be easily formed into an inclined shape, so that the inclined surface 43b can be easily formed.

[0081] In the Damascene wiring structure 100 , the inclined surface 43 b is curved in a convex shape. This can more reliably suppress the stress from being concentrated on the cover layer 70 .

[0082] In the damascene wiring structure 100, the third surface 51c of the end 51 of the metal layer 50, which is opposite to the second surface 51b, is inclined, and a portion 61 of the wiring portion 60 enters between the cover layer 70 and the third surface 51c. As a result, the end 51 of the metal layer 50 can be suppressed by the wiring portion 60, and the stress acting on the cover layer 70 from the metal layer 50 can be reduced. Furthermore, since the thickness of the portion 61 of the wiring portion 60 in the direction A1 perpendicular to the main surface 31 is reduced, the stress acting on the cover layer 70 from the wiring portion 60 can be reduced.

[0083] In the Damascene wiring structure 100, the thickness of the end 51 of the metal layer 50 in the direction A2 parallel to the main surface 31 is thicker than the thickness of the portion other than the end 51 of the metal layer 50. Thus, the contact area between the end 51 of the metal layer 50 and the cover layer 70 can be increased, and the stress acting from the metal layer 50 to the cover layer 70 can be more appropriately dispersed.

[0084] In the Damascene wiring structure 100, the thickness of the end 51 of the metal layer 50 in the direction A2 parallel to the main surface 31 gradually increases as it approaches the front end of the end 51. Thus, the contact area between the end 51 of the metal layer 50 and the cover layer 70 can be further increased, and the stress acting from the metal layer 50 to the cover layer 70 can be further appropriately dispersed.

[0085] In the Damascene wiring structure 100, the groove portion 33 extends in a spiral shape. Even when the groove portion 33 extends in a spiral shape in this way, high reliability can be obtained.

[0086] In the Damascene wiring structure 100, the interval B between the adjacent portions 33a of the groove 33 may be smaller than the width W of the groove 33. This can narrow the pitch (interval) of the wiring and achieve space saving.

[0087] In the Damascene wiring structure 100 , the width W of the groove 33 is smaller than the depth D of the groove 33 . This can save space and reduce wiring resistance.

[0088] In the Damascene wiring structure 100, the distance L between the bottom surface 34b of the groove portion 33 and the opposite surface of the substrate 30 opposite to the main surface 31 (the surface 81a of the first silicon layer 81) in the direction A1 perpendicular to the main surface 31 is greater than the depth D of the groove portion 33. Thus, the strength of the substrate 30 can be increased, and the reliability can be further improved.

[0089] [Method for manufacturing a damascene wiring structure]

[0090] Next, refer to Figure 5 , Figure 6 and Figure 7 , a method for manufacturing the embedded wiring structure 100 is described. Figure 5 to Figure 7 In the figure, each part is schematically shown, but in reality, for example, it is formed as follows Figure 4 Shape shown.

[0091] First, if Figure 5 As shown in (a), a substrate 30 having a first silicon layer 81, a second silicon layer 82 and an insulating layer 83 is prepared, and a groove portion 33 is formed on the main surface 31 of the substrate 30. The groove portion 33 is formed, for example, by reactive ion etching (DRIE) using the Bosch process. The thickness of the first silicon layer 81 is, for example, about 30 to 150 μm, and the thickness of the second silicon layer 82 is, for example, about 625 μm. The depth of the groove portion 33 is, for example, about 5 to 30 μm.

[0092] Then, if Figure 5 As shown in (b), an insulating layer 40 is formed on the main surface 31 of the substrate 30 (first step), and the insulating layer 40 includes: a first portion 41 provided on the inner surface 34; and a second portion 42 formed integrally with the first portion 41 and provided on the main surface 31. More specifically, after a first layer 44 composed of a silicon oxide film (thermal oxide film) is formed over the main surface 31 and the inner surface 34 of the groove portion 33, a second layer 45 composed of a silicon nitride film (LP-SiN) is formed on the first layer 44. The thickness of the first layer 44 and the second layer 45 is, for example, about 100 to 1000 nm.

[0093] More specifically, in the first step, the insulating layer 40 is formed, wherein the surface 43a of the boundary portion 43 between the first portion 41 and the second portion 42 of the insulating layer 40, which is opposite to the substrate 30, includes an inclined surface 43b (see FIG. 4B ) inclined with respect to the direction A1 perpendicular to the main surface 31 when viewed from the extending direction of the wiring portion 60. Figure 4). For example, by forming the first layer 44 composed of a silicon oxide film and the second layer 45 composed of a silicon nitride film on the main surface 31 and the inner surface 34 of the groove portion 33, an inclined surface 43b is formed on the surface 43a of the boundary portion 43. This is because the first layer 44 composed of the silicon oxide film is easily formed with an inclined shape.

[0094] Then, if Figure 6 As shown in (a), a metal layer 50 is formed on the first portion 41 and the second portion 42 of the insulating layer 40 (second step). In the second step, a metal layer 55 is formed on the metal layer 50. The metal layer 55 is composed of a metal material such as copper, for example. The metal layer 55 functions as a seed layer together with the metal layer 50. The metal layer 50 and the metal layer 55 are formed, for example, by sputtering, but can also be formed by atomic layer deposition (ALD), chemical growth method (CVD), ion plating or electroless plating. The total thickness of the metal layer 50 and the metal layer 55 is, for example, about 10nm to 3000nm.

[0095] Then, if Figure 6 As shown in (b), the wiring portion 60 is formed in a manner buried in the groove portion 33 and joined to the metal layer 50 (third step). The wiring portion 60 is formed, for example, by plating. The wiring portion 60 is formed, for example, in a manner in which the average thickness of the wiring portion 60 on the main surface 31 is greater than 1 μm. In addition, in this example, since the metal layer 55 is made of the same material as the wiring portion 60, when the wiring portion 60 is formed, there is a situation where the wiring portion 60 and the metal layer 55 are integrated and the interface between the wiring portion 60 and the metal layer 55 disappears. In this case, it can be regarded that the metal layer 55 constitutes the wiring portion 60.

[0096] Then, if Figure 7 As shown in (a), the metal layer 50, the metal layer 55, and the wiring portion 60 on the second portion 42 are removed by chemical mechanical polishing (CMP) to flatten the second portion 42 of the insulating layer 40 so as to expose the second portion 42 (the fourth step). In the fourth step, chemical mechanical polishing is performed on the insulating layer 40, the metal layer 50, the metal layer 55, and the wiring portion 60 from the side opposite to the substrate 30. For each of the insulating layer 40, the metal layer 50, the metal layer 55, and the wiring portion 60, a portion on the opposite side to the main surface 31 or the bottom surface 34b in the direction A1 perpendicular to the main surface 31 is removed, thereby flattening the insulating layer 40, the metal layer 50, the metal layer 55, and the wiring portion 60. At this time, in this example, the portion constituting the second portion 42 in the second layer 45 of the insulating layer 40 is removed.

[0097] Then, if Figure 7As shown in (b), a cover layer 70 is formed in a manner covering the second portion 42 of the insulating layer 40, the end portion 51 of the metal layer 50, and the wiring portion 60 (fifth step). The cover layer 70 is, for example, made of a silicon nitride film (PE-SiN) and is formed to a thickness of about 200 to 3000 nm. Next, the second silicon layer 82 and the insulating layer 83 are removed by etching or the like. Through the above steps, the above-mentioned damascene wiring structure 100 can be obtained.

[0098] [Modifications]

[0099] The present disclosure is not limited to the above-mentioned embodiment. Figure 8 The first modified example is shown in the figure. In the first modified example, a boundary surface 35 is provided at the boundary portion between the main surface 31 of the substrate 30 and the groove portion 33, which is inclined outward relative to the direction A1 perpendicular to the main surface 31 when viewed from the extension direction of the wiring portion 60. The boundary surface 35 is, for example, a flat surface. The boundary portion 43 of the insulating layer 40 is provided on the boundary surface 35, so it extends along the boundary surface 35 and is inclined outward relative to the direction A1 perpendicular to the main surface 31. The inclined surface 43b of the boundary portion 43 and the second surface 51b of the end portion 51 of the metal layer 50 become flat surfaces parallel to the boundary surface 35. The third surface 51c of the end portion 51 also becomes a flat surface inclined outward relative to the direction A1. The inclination angle of the third surface 51c relative to the direction A1 becomes gentler than the inclination angle of the second surface 51b relative to the direction A1. As a result, the thickness of the end portion 51 in the direction A2 parallel to the main surface 31 gradually increases as it approaches the front end of the end portion 51.

[0100] When manufacturing the Damascene wiring structure 100 of the first modified example, for example, the groove 33 is formed by reactive ion etching using a non-Bosch process and a Bosch process. Thus, when the groove 33 is formed, a boundary surface 35 is formed at the boundary between the main surface 31 of the substrate 30 and the groove 33. By combining the non-Bosch process and the Bosch process, reliability can be improved.

[0101] According to the first modification, similarly to the above-mentioned embodiment, reliability can be improved. Furthermore, since the boundary surface 35 is provided at the boundary portion between the main surface 31 and the groove portion 33 in the substrate 30, the formation of the inclined surface 43b can be facilitated. In the first modification, the interval B between the plurality of portions 33a of the groove portion 33 may be smaller than the width W of the groove portion 33. In the case of the first modification, the interval B is the distance between the inner surfaces 34 other than the boundary surface 35 in the plurality of portions 33a (in other words, the distance between the portions of the inner surface 34 extending in the direction A1 perpendicular to the main surface 31).

[0102] The inlaid wiring structure 100 can also be Fig. 9The second variant is constructed in the manner shown. In the second variant, the surface 60a of the wiring portion 60 is located on the bottom surface 34b side of the groove portion 33 relative to the surface 42a of the second portion 42 of the insulating layer 40. The third surface 51c of the end portion 51 of the metal layer 50 is covered by a boundary portion 71 between a portion on the surface 60a and a portion on the surface 42a in the covering layer 70. The boundary portion 71 extends along the third surface 51c and is inclined outward relative to a direction A1 perpendicular to the main surface 31. When manufacturing the embedded wiring structure 100 of the second variant, for example, by adjusting the slurry in the chemical mechanical polishing in the fourth step, the dishing amount of the wiring portion 60 (the amount of the wiring portion 60 removed) is increased. Thereby, it is possible to form Fig. 9 The wiring section 60 has the shape shown.

[0103] According to the second modification, similarly to the above-mentioned embodiment, reliability can be improved. Furthermore, the surface 60a is located on the bottom surface 34b side of the groove portion 33 relative to the surface 42a. Thus, the portion where stress is easily concentrated can be further reduced. Furthermore, since the third surface 51c of the end portion 51 is covered by the boundary portion 71, the contact area between the end portion 51 of the metal layer 50 and the cover layer 70 can be further increased, and the stress acting on the cover layer 70 from the metal layer 50 can be further appropriately dispersed.

[0104] The inlaid wiring structure 100 can also be Fig.10 The third variant is configured in the manner of the third variant shown in (a). In the third variant, as in the second variant, the surface 60a of the wiring portion 60 is located on the bottom surface 34b side of the groove portion 33 relative to the surface 42a of the second portion 42 of the insulating layer 40. In addition, the third surface 51c of the end portion 51 of the metal layer 50 is covered by the boundary portion 71 of the covering layer 70. In the third variant, the thickness T1 of the covering layer 70 is larger than the distance H between the surface 60a and the surface 42a in the direction A1 perpendicular to the main surface 31. According to the third variant, as in the above-mentioned embodiment, the reliability can be improved. In addition, since the thickness T1 of the covering layer 70 is larger than the distance H between the surface 60a and the surface 42a in the direction A1 perpendicular to the main surface 31, the strength of the covering layer 70 can be further improved.

[0105] The inlaid wiring structure 100 can also be Fig.10The fourth modification example is configured in the manner of the fourth modification example shown in (b). In the fourth modification example, as in the second modification example, the surface 60a of the wiring portion 60 is located on the bottom surface 34b side of the groove portion 33 relative to the surface 42a of the second portion 42 of the insulating layer 40. In addition, the third surface 51c of the end portion 51 of the metal layer 50 is covered by the boundary portion 71 of the covering layer 70. In the fourth modification example, the thickness T1 of the covering layer 70 is smaller than the distance H between the surface 60a and the surface 42a in the direction A1 perpendicular to the main surface 31. According to the fourth modification example, the reliability can be improved as in the above-mentioned embodiment. In addition, the thickness T1 of the covering layer 70 is smaller than the distance H between the surface 60a and the surface 42a in the direction A1 perpendicular to the main surface 31, so that the thickness of the wiring portion 60 in the direction A1 can be thinned, and as a result, the stress acting on the covering layer from the wiring portion 60 can be further reduced.

[0106] The shape and configuration of the coils 21 and 22 are not limited to the above-mentioned examples. For example, in the above-mentioned embodiment, the coil 22 only has a portion extending in a direction parallel to the first axis X1 and a portion extending in a direction parallel to the second axis X2, but the coil 22 may also have a portion extending in a direction intersecting the first axis X1 and the second axis X2 when viewed from above. The coil 22 may also have a portion extending at an angle of 45 degrees relative to the first axis X1 when viewed from above. These aspects are the same for the coil 21. In the above-mentioned embodiment, either of the coils 21 and 22 may also be omitted. In the above-mentioned embodiment, the second movable portion 4 may also be regarded as a support portion that can swingably support the first movable portion 3. The second movable portion 4 and the second connecting portions 7 and 8 may also be omitted. In this case, the first movable portion 3 swings only around the first axis X1.

[0107] The materials and shapes of each component are not limited to the above examples. The third surface 51c of the end 51 of the metal layer 50 may also extend along the second surface 51b. For example, the inclination degree (inclination angle) of the third surface 51c may be the same as the inclination degree (inclination angle) of the second surface 51b. The third surface 51c and the second surface 51b may also extend parallel to each other. The second portion 42 may also be composed of the first layer 44 and the second layer 45. In this case, the location where stress is easily concentrated can be further reduced. In the case where the cover layer 70 is composed of the same material as the second layer 45 of the insulating layer 40, the area of ​​the portion where the same materials are bonded to each other becomes larger, so that the adhesion can be improved. The insulating layer 40 may also be composed of a single layer. The insulating layer 40 may be composed of a single layer composed of an oxide film, for example. In this case, the cover layer 70 may also be composed of an oxide film. When viewed from the extension direction of the wiring portion 60, the first surface 51a and the second surface 51b may be connected in a manner that the curvatures of each other are continuous. The inlaid wiring structure 100 may also be applied to structures other than actuators.

[0108] Explanation of symbols

[0109] 1…mirror device (actuator); 2…support portion; 3…first movable portion; 4…second movable portion (support portion); 9…magnetic field generating portion; 21, 22…coils; 30…substrate; 31…main surface; 33…groove portion; 34…inner surface; 34b…bottom surface (bottom); 35…boundary surface; 40…insulating layer; 41…first portion; 42…second portion; 42a…surface (second contact surface); 43…boundary portion; 43a…surface; 43b…inclined surface; 44…first layer; 45…second layer; 50…metal layer; 51…end portion; 51a…first surface; 51b…second surface; 51c…third surface; 60…wiring portion; 60a…surface (first contact surface); 61…part of the wiring portion; 70…covering layer; 81a…surface (opposite surface); 100…inlaid wiring structure.

Claims

1. A mosaic wiring structure, characterized in that: have: a substrate having a main surface provided with a groove portion; an insulating layer having: a first portion provided on the inner surface of the groove portion; and a second portion formed integrally with the first portion and provided on the main surface; a metal layer disposed on the first portion of the insulating layer; a wiring portion embedded in the groove portion and bonded to the metal layer; as well as a covering layer provided so as to cover the second portion of the insulating layer and the wiring portion, A surface of a boundary portion between the first portion and the second portion of the insulating layer on the opposite side to the base includes an inclined surface inclined with respect to a direction perpendicular to the main surface when viewed in the extending direction of the wiring portion.

2. The inlaid wiring structure according to claim 1, wherein: The cover layer is thicker than the insulating layer.

3. The inlaid wiring structure according to claim 1 or 2, characterized in that: The insulating layer includes: a first layer composed of an oxide film; and a second layer composed of a nitride film and provided on the first layer.

4. The inlaid wiring structure according to any one of claims 1 to 3, characterized in that: A boundary surface is provided at a boundary portion between the main surface of the base and the groove portion, the boundary surface being inclined with respect to a direction perpendicular to the main surface when viewed from the extending direction.

5. The inlaid wiring structure according to any one of claims 1 to 4, characterized in that: The inclined surface is convexly curved.

6. The inlaid wiring structure according to any one of claims 1 to 5, characterized in that: The thickness of the end portion of the metal layer in a direction parallel to the main surface is greater than the thickness of a portion of the metal layer other than the end portion.

7. The inlaid wiring structure according to any one of claims 1 to 6, wherein: The thickness of the end portion of the metal layer in a direction parallel to the main surface gradually increases as it approaches a front end of the end portion.

8. The inlaid wiring structure according to any one of claims 1 to 7, wherein: A first contact surface of the wiring portion that is in contact with the cover layer is located on the bottom side of the groove portion with respect to a second contact surface of the insulating layer that is in contact with the cover layer.

9. The inlaid wiring structure according to claim 8, characterized in that: The thickness of the cover layer is greater than a distance between the first contact surface and the second contact surface in a direction perpendicular to the main surface.

10. The inlaid wiring structure according to claim 8, wherein: The thickness of the cover layer is smaller than the distance between the first contact surface and the second contact surface in a direction perpendicular to the main surface.

11. The inlaid wiring structure according to any one of claims 1 to 10, characterized in that: The groove portion extends in a spiral shape when viewed from a direction perpendicular to the main surface.

12. The inlaid wiring structure according to claim 10, wherein: A distance between adjacent portions of the groove is smaller than a width of the groove.

13. The inlaid wiring structure according to any one of claims 1 to 10, characterized in that: The width of the groove portion is smaller than the depth of the groove portion.

14. The inlaid wiring structure according to any one of claims 1 to 13, characterized in that: The base has an opposite surface opposite to the main surface. A distance between a bottom of the groove portion and the opposite surface in a direction perpendicular to the main surface is greater than a depth of the groove portion.

15. The inlaid wiring structure according to any one of claims 1 to 14, characterized in that: The end portion of the metal layer has a first surface along the inclined surface of the insulating layer and a second surface opposite to the first surface. The second surface is tilted more gently with respect to a direction perpendicular to the main surface than the first surface is tilted with respect to the direction perpendicular to the main surface.

16. The inlaid wiring structure according to any one of claims 1 to 15, characterized in that: A thickness of a front end portion of the metal layer in a direction perpendicular to the main surface is smaller than a thickness of the second portion of the insulating layer.

17. An actuating device, characterized in that: A embedded wiring structure having any one of claims 1 to 16, The actuating device has: Supporting part; a movable portion supported in the supporting portion in a swingable manner; a coil having the embedded wiring structure and provided on at least one of the supporting portion and the movable portion; and A magnetic field generating unit generates a magnetic field acting on the coil.