Processing method of erbium-doped optical fiber preform

By filling the mixed solution in the reaction tube and using the pressing and take-off mechanism of the tooling table, the problem of waste and low efficiency in the existing erbium-doped fiber preforming rod process is solved, and efficient doping and resource saving is achieved, making high-quality production Quality fiber prefabricated rods.

CN118908557APending Publication Date: 2024-11-08JIANGSU FASTEN OPTOELECTRONICS TECH CO LTD
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202410792426.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-19
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

In the offline liquid phase doping process of existing erbium-doped fiber preforms, the Er and Yb content of the mixed solution is reduced, resulting in poor adsorption efficiency and adsorption amount, and serious waste of solution, affecting process efficiency and resource utilization.

Method used

A new tooling table is designed to fill the reaction tube with mixed solution for offline doping, and use a pressing mechanism and a take-over mechanism to ensure that the solution fully acts on the loose core layer, and a single-model master rod is made by drying, dehydrating and vitrification. Reduce solution waste and working time.

Benefits of technology

It greatly reduces solution waste, improves work efficiency and adsorption uniformity, saves the use of mixed solutions, reduces resource waste, and ensures doping effect and efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118908557A_ABST
    Figure CN118908557A_ABST
Patent Text Reader

Abstract

The invention discloses a processing method of an erbium-doped optical fiber preform, and relates to the technical field of erbium-doped optical fiber processing. The device comprises a tool table, a high supporting seat and a low supporting seat are fixed to the top of the tool table, the top of the high supporting seat and the top of the low supporting seat are each of an inclined face structure, pressing mechanisms are arranged on the high supporting seat and the low supporting seat, a solution input mechanism is arranged on the side, close to the low supporting seat, of the tool table, and a solution collecting mechanism is arranged on the other side of the tool table. The solution input mechanism and the solution collection mechanism are connected with outer joints through hoses; and the processing method of the preform rod comprises the following steps: SS01, manufacturing of a reaction tube, SS02, offline liquid phase doping, SS03, dehydration, drying and vitrification, and SS04, embedding and assembling to form the rod. According to the invention, the reaction tube is filled with the solution for off-line doping by designing a novel method, and all the solutions can completely act on the loose core layer of the reaction tube, so that the solution waste and the working time can be greatly reduced, the use of the mixed solution can be saved, and the resource waste is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of erbium-doped optical fiber processing, and in particular relates to a processing method of an erbium-doped optical fiber preform. Background Art

[0002] For the processing of erbium-doped optical fiber preform, a loose core layer is first deposited on the substrate tube, and then offline liquid phase doping, drying and dehydration, and vitrification processes are performed to produce a single-mode mother rod. Subsequently, a stress mother rod is produced, symmetrical side holes are opened on the single-mode mother rod, and finally the stress mother rod is installed in the side holes to realize the production of panda-type optical fiber preform.

[0003] As for the offline liquid phase doping process, the entire substrate tube is immersed in the mixed solution, and the offline liquid phase doping is carried out at room temperature. The Er and Yb in the solution will be adsorbed in the loose core layer of the reaction tube. After the process is completed, the Er and Yb content in the solution in the container will be reduced, which is not conducive to subsequent reuse and affects the adsorption efficiency and adsorption amount. At the same time, the entire tube needs to be immersed in the container each time, which will cause waste of the mixed solution itself.

[0004] Therefore, designing a preform processing method that can save mixed solution is a problem that needs to be solved by those skilled in the art. Summary of the invention

[0005] The purpose of the present invention is to provide a processing method for an erbium-doped optical fiber preform. By designing a new method, a solution is filled in a reaction tube for offline doping, and all the solution can completely act on the loose core layer of the reaction tube, thereby greatly reducing solution waste and working time, greatly improving work efficiency and effect, and saving the use of mixed solution and reducing resource waste.

[0006] In order to solve the above technical problems, the present invention is achieved through the following technical solutions:

[0007] The present invention is a method for processing an erbium-doped optical fiber preform, comprising a tooling table;

[0008] A high support seat and a low support seat are fixed on the top of the workbench, the tops of the high support seat and the low support seat are both inclined structures, and a clamping mechanism is provided on the high support seat and the low support seat;

[0009] A solution input mechanism is provided on one side of the workbench close to the low support seat, and a solution collection mechanism is provided on the other side of the workbench. Both the solution input mechanism and the solution collection mechanism are connected to an external joint through a hose;

[0010] The processing method of the preform comprises the following steps:

[0011] Production of SS01 reaction tube: The barrier layer and the loose core layer are deposited and formed in sequence in the substrate tube, and a connecting mechanism with a switch valve is installed at both ends of the reaction tube;

[0012] SS02 offline liquid phase doping: The reaction tube is clamped and fixed on the top of the high support and the low support by a clamping mechanism, with one end of the reaction tube at a high level and the other end at a low level. The solution input mechanism and the solution collection mechanism are respectively connected to the two connecting mechanisms, and the mixed liquid is input into the reaction tube until liquid falls from the solution collection mechanism, indicating that the reaction tube is full of mixed liquid. The two connecting mechanisms are closed to seal the two ends of the reaction tube, and the reaction tube is removed from the workbench and moved to the tube rack for offline doping at room temperature;

[0013] After the loose core layer of SS03 is adsorbed, the reaction tube is placed in a drying device, and a mixed gas of high-purity chlorine and oxygen is input into the reaction tube for drying and dehydration at a suitable temperature. At this time, the mixed gas is input by a connecting mechanism and output by another connecting mechanism. After the drying and dehydration is completed, the connecting mechanism is removed, and the reaction tube after drying and dehydration is subsequently vitrified at a high temperature;

[0014] SS04 shrinks the vitrified reaction tube into a rod and a sleeve in turn to make a single-mode mother rod, opens two symmetrical side holes on the single-mode mother rod, and installs a stress mother rod in the side holes to make a panda-shaped optical fiber preform rod.

[0015] Furthermore, the top surfaces of the high support seat and the low support seat are both provided with lower arc grooves, and the lower arc grooves on the tops of the high support seat and the low support seat are concentric and linearly distributed.

[0016] Furthermore, the clamping mechanism includes a clamping cylinder, which is arranged on the rear side of the high support seat and the low support seat, the output end of the clamping cylinder faces upward and is fixed with a material clamping seat through a pressure plate, and the bottom surface of the material clamping seat is provided with an upper arc groove, and the upper arc groove is located directly above the lower arc groove and a clamping groove body is formed therebetween.

[0017] Furthermore, the solution input mechanism comprises a solution tank, the solution tank is connected to a pump body, and the hose is connected to an output end of the pump body.

[0018] Furthermore, the solution collecting mechanism comprises a transparent chamber, a hose on the transparent chamber is connected to the top of the transparent chamber, and a drainage pipe is provided on the transparent chamber.

[0019] Furthermore, the connecting pipe mechanism comprises a straight pipe, a switch valve is arranged on the straight pipe, one end of the straight pipe is fixedly connected with an end sleeve, and the end sleeve is sleeved on the end of the base pipe and fixed to the base pipe.

[0020] Furthermore, an inner joint is provided at one end of the straight pipe away from the end sleeve, and the inner joint cooperates with the outer joint.

[0021] Furthermore, the mixed solution is a mixed solution of ErCl3 and YbCl3.

[0022] The present invention has the following beneficial effects:

[0023] 1. The present invention designs a novel method to fill the solution into the reaction tube for offline doping. All the solution can completely act on the loose core layer of the reaction tube, thereby greatly reducing solution waste and working time, greatly improving work efficiency and effect, saving the use of mixed solution, and reducing resource waste.

[0024] 2. The present invention designs a new type of workbench for inputting mixed solutions into reaction tubes. After the reaction tubes are clamped on the workbench, the reaction tubes are in an inclined state, and the mixed solutions are input from the low point end and output from the high point end. After the solution flows out from the high point end, the reaction tubes are ensured to be in a full load state without bubbles, thereby ensuring the solution content and improving the doping uniformity and effect.

[0025] 3. The present invention is designed with a take-over mechanism, which is installed at the end of the reaction tube, which is convenient for positioning, installation and disassembly. It also has the function of a switch. After the mixed solution is filled, both ends of the reaction tube can be blocked to ensure the subsequent doping effect and efficiency.

[0026] Of course, any product implementing the present invention does not necessarily need to achieve all of the advantages described above at the same time. BRIEF DESCRIPTION OF THE DRAWINGS

[0027] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the accompanying drawings required for describing the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other accompanying drawings can be obtained based on these accompanying drawings without paying creative work.

[0028] Figure 1 It is a structural schematic diagram of the tooling table of the present invention;

[0029] Figure 2 It is a structural cross-sectional view of the connection between the connecting pipe mechanism and the reaction tube of the present invention;

[0030] Figure 3 It is a schematic diagram of the structure after the reaction tube of the present invention is connected with the solution input mechanism and the solution collection mechanism;

[0031] In the accompanying drawings, the components represented by the reference numerals are listed as follows:

[0032] 1-tooling table, 2-pressing mechanism, 3-solution input mechanism, 4-solution collecting mechanism, 5-base pipe, 6-taking over mechanism, 101-high support seat, 102-low support seat, 103-lower arc groove, 201-pressing cylinder, 202-pressing plate, 203-clamping seat, 204-upper arc groove, 301-solution tank, 302-pump body, 501-barrier layer, 502-loose core layer, 601-straight pipe, 602-switch valve, 603-end sleeve, 604-inner joint. DETAILED DESCRIPTION

[0033] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0034] See also Figure 1-3 As shown, the present invention is a method for processing an erbium-doped optical fiber preform, comprising a tooling table 1;

[0035] A high support seat 101 and a low support seat 102 are fixed on the top of the workbench 1. The tops of the high support seat 101 and the low support seat 102 are both inclined structures. A clamping mechanism 2 is provided on the high support seat 101 and the low support seat 102.

[0036] A solution input mechanism 3 is provided on one side of the workbench 1 close to the low support seat 102, and a solution collection mechanism 4 is provided on the other side of the workbench 1. Both the solution input mechanism 3 and the solution collection mechanism 4 are connected to external joints through hoses.

[0037] The processing method of the preform comprises the following steps:

[0038] Production of SS01 reaction tube: Deposition and molding of barrier layer 501 and loose core layer 502 are carried out in sequence in substrate tube 5, and connecting mechanism 6 with switch valve 602 is installed at both ends of the reaction tube;

[0039] SS02 offline liquid phase doping: The reaction tube is clamped and fixed on the top of the high support seat 101 and the low support seat 102 by the clamping mechanism 2, with the height of the two ends of the reaction tube being one high and one low. The solution input mechanism 3 and the solution collection mechanism 4 are respectively connected to the two connecting mechanisms 6, and the mixed liquid is input into the reaction tube until liquid falls from the solution collection mechanism 4, indicating that the reaction tube is full of mixed liquid. The two connecting mechanisms 6 are closed to seal the two ends of the reaction tube, and the reaction tube is separated from the tooling table 1 and moved to the tube rack for offline doping at room temperature;

[0040] After the loose core layer 502 has finished adsorbing SS03, the reaction tube is placed in a drying device, a mixed gas of high-purity chlorine and oxygen is input into the reaction tube, and a drying and dehydration treatment is performed at a suitable temperature. At this time, the mixed gas is input by a connecting mechanism 6 and output by another connecting mechanism 6. After the drying and dehydration is completed, the connecting mechanism 6 is removed, and the reaction tube after drying and dehydration is subsequently vitrified at a high temperature;

[0041] SS04 shrinks the vitrified reaction tube into a rod and a sleeve in turn to make a single-mode mother rod, opens two symmetrical side holes on the single-mode mother rod, and installs a stress mother rod in the side holes to make a panda-shaped optical fiber preform rod.

[0042] Among them Figure 1 and Figure 3 As shown, the top surfaces of the high support seat 101 and the low support seat 102 are both provided with lower arc grooves 103 , and the lower arc grooves 103 on the tops of the high support seat 101 and the low support seat 102 are concentric and linearly distributed.

[0043] Among them Figure 1 As shown, the clamping mechanism 2 includes a clamping cylinder 201, which is arranged at the rear side of the high support seat 101 and the low support seat 102. The output end of the clamping cylinder 201 faces upward and is fixed with a clamping seat 203 through a pressure plate 202. An upper arc groove 204 is provided on the bottom surface of the clamping seat 203. The upper arc groove 204 is located directly above the lower arc groove 103 and a clamping groove body is formed therebetween.

[0044] Among them Figure 3 As shown, the solution input mechanism 3 includes a solution tank 301 , a pump body 302 is connected to the solution tank 301 , and a hose is connected to the output end of the pump body 302 .

[0045] Among them Figure 3 As shown, the solution collecting mechanism 4 comprises a transparent chamber, a hose on the transparent chamber is connected to the top of the transparent chamber, and a drainage pipe is provided on the transparent chamber.

[0046] Among them Figure 2 As shown, the connecting mechanism 6 includes a straight pipe 601 , on which a switch valve 602 is provided. One end of the straight pipe 601 is fixedly connected to an end sleeve 603 , which is sleeved on the end of the base pipe 5 and fixed to the base pipe 5 .

[0047] Among them Figure 2 As shown, an inner joint 604 is provided at one end of the straight pipe 601 away from the end sleeve 603, and the inner joint 604 cooperates with the outer joint.

[0048] Wherein, the mixed solution is a mixed solution of ErCl3 and YbCl3.

[0049] In the description of this specification, the description with reference to the terms "one embodiment", "example", "specific example", etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described can be combined in any one or more embodiments or examples in a suitable manner.

[0050] The preferred embodiments of the present invention disclosed above are only used to help illustrate the present invention. The preferred embodiments do not describe all the details in detail, nor do they limit the invention to the specific implementation methods described. Obviously, many modifications and changes can be made according to the content of this specification. This specification selects and specifically describes these embodiments in order to better explain the principles and practical applications of the present invention, so that those skilled in the art can understand and use the present invention well. The present invention is limited only by the claims and their full scope and equivalents.

Claims

1. A method for processing an erbium-doped optical fiber preform, characterized in that: The utility model comprises a tooling table (1); A high support seat (101) and a low support seat (102) are fixed on the top of the workbench (1); the tops of the high support seat (101) and the low support seat (102) are both inclined structures; and a clamping mechanism (2) is provided on the high support seat (101) and the low support seat (102); A solution input mechanism (3) is provided on one side of the workbench (1) close to the low support seat (102), and a solution collection mechanism (4) is provided on the other side of the workbench (1). Both the solution input mechanism (3) and the solution collection mechanism (4) are connected to external joints via hoses; The processing method of the preform comprises the following steps: Production of SS01 reaction tube: depositing and molding a barrier layer (501) and a loose core layer (502) in sequence in a base tube (5), and installing a connecting mechanism (6) with a switch valve (602) at both ends of the reaction tube; SS02 offline liquid phase doping: The reaction tube is clamped and fixed on the top of the high support seat (101) and the low support seat (102) by a clamping mechanism (2), with the height of the two ends of the reaction tube being one high and one low. The solution input mechanism (3) and the solution collection mechanism (4) are respectively connected to the two connecting mechanisms (6), and the mixed liquid is input into the reaction tube until liquid falls from the solution collection mechanism (4), indicating that the reaction tube is full of the mixed liquid. The two connecting mechanisms (6) are closed to seal the two ends of the reaction tube, and the reaction tube is separated from the tooling table (1) and moved to the tube rack to perform offline doping under normal temperature environment; After the SS03 is adsorbed on the loose core layer (502), the reaction tube is placed in a drying device, a mixed gas of high-purity chlorine and oxygen is input into the reaction tube, and a drying and dehydration treatment is performed at a suitable temperature. At this time, the mixed gas is input through a connecting mechanism (6) and output through another connecting mechanism (6). After the drying and dehydration is completed, the connecting mechanism (6) is removed, and the reaction tube after drying and dehydration is subsequently vitrified at a high temperature; SS04 shrinks the vitrified reaction tube into a rod and a sleeve in turn to make a single-mode mother rod, opens two symmetrical side holes on the single-mode mother rod, and installs a stress mother rod in the side holes to make a panda-shaped optical fiber preform rod.

2. The method for processing an erbium-doped optical fiber preform according to claim 1, characterized in that: The top surfaces of the high support seat (101) and the low support seat (102) are both provided with lower arc grooves (103), and the lower arc grooves (103) on the tops of the high support seat (101) and the low support seat (102) are concentric and linearly distributed.

3. The method for processing an erbium-doped optical fiber preform according to claim 2, characterized in that: The clamping mechanism (2) comprises a clamping oil cylinder (201), the clamping oil cylinder (201) being arranged at the rear side of the high support seat (101) and the low support seat (102), the output end of the clamping oil cylinder (201) facing upward and being fixed with a clamping seat (203) via a pressing plate (202), the bottom surface of the clamping seat (203) being provided with an upper arc groove (204), the upper arc groove (204) being located directly above the lower arc groove (103) and forming a clamping groove body therebetween.

4. The method for processing an erbium-doped optical fiber preform according to claim 1, characterized in that: The solution input mechanism (3) comprises a solution tank (301), the solution tank (301) is connected to a pump body (302), and the hose is connected to the output end of the pump body (302).

5. The method for processing an erbium-doped optical fiber preform according to claim 1, characterized in that: The solution collecting mechanism (4) comprises a transparent chamber, a hose on the transparent chamber is connected to the top of the transparent chamber, and a liquid discharge pipe is provided on the transparent chamber.

6. The method for processing an erbium-doped optical fiber preform according to claim 1, characterized in that: The connecting pipe mechanism (6) comprises a straight pipe (601), on which a switch valve (602) is provided, and one end of the straight pipe (601) is fixedly connected to an end sleeve (603), which is sleeved on the end of the base pipe (5) and fixed to the base pipe (5).

7. The method for processing an erbium-doped optical fiber preform according to claim 6, characterized in that: An inner joint (604) is provided at one end of the straight pipe (601) away from the end sleeve (603), and the inner joint (604) cooperates with the outer joint.

8. The method for processing an erbium-doped optical fiber preform according to claim 1, characterized in that: The mixed solution is a mixed solution of ErCl3 and YbCl3.

Citation Information

Patent Citations

  • Method for manufacturing doped optical fibre preform by MCVD (modified chemical vapour deposition)

    CN102515501A

  • Large-core-diameter rare earth doped optical fiber preform and preparation method thereof

    CN110606657A

  • Online doping method and device for preparing active optical fiber preform

    CN115180817A

  • Ytterbium-doped optical fiber preform, ytterbium-doped active optical fiber and preparation method thereof

    CN117185644A

  • High-concentration and high-uniformity rare earth doped optical fiber and preparation method thereof

    CN117361868A